METHOD FOR PREPARING A POLYMER SEAL SUBJECTED TO FATIGUE PRESSURE

By applying assembly pressure to induce plastic deformation in polymer seals, the process addresses mechanical fatigue issues, enhancing seal durability and extending service life.

FR3138175B1Active Publication Date: 2024-10-11SAFRAN AIRCRAFT ENGINES SAS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
FR2022007426
Authority / Receiving Office
FR · FR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-07-20
Publication Date
2024-10-11
Estimated Expiration
2042-07-20

AI Technical Summary

Technical Problem

Polymer seals in mechanical assemblies experience mechanical fatigue due to minor stress variations during low-cycle fatigue, leading to potential damage despite using materials like PTFE, which are susceptible to stress concentrations.

Method used

Applying an assembly pressure during mechanical assembly that induces plastic deformation in the seals, specifically twice or 2.5 times the maximum operating pressure, to reduce stress variations and enhance durability.

Benefits of technology

The plastic deformation process increases the lifespan of polymer seals by reducing stress concentrations and extending their service life beyond expectations.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000006_0000
    Figure 00000006_0000
  • Figure 00000006_0001
    Figure 00000006_0001
  • Figure 00000007_0000
    Figure 00000007_0000
Patent Text Reader

Abstract

A seal (10, 11) bordering a cavity (12) containing a fluid at variable pressure is subjected, before the mechanical assembly is put into service, to overpressure that allows it to plastically deform at stress concentration points. This reduces the stresses subsequently experienced locally, and the risk of fatigue damage due to fluid pressure variations during the mechanical assembly's service life. This applies to polymer seals, particularly those with low resistance to cyclic loading. See Figure 3 for abbreviations.
Need to check novelty before this filing date? Find Prior Art

Description

Title of the invention: METHOD FOR PREPARING A POLYMER SEAL SUBJECTED TO FATIGUE PRESSURE

[0001] The subject of the invention is a method for preparing a polymer seal subjected to fatigue pressure.

[0002] The seals in question here border cavities of a fluid subject to pressure variations during the operation of a mechanical assembly in which the cavity is included and which comprises the seal. A possible, but not limiting, application concerns the lubrication cavities of bearings supporting pivot shafts of variable-pitch propeller blades, that is to say, the incidence of which relative to the longitudinal axis of the engine can be modified at will, according to the speeds thereof or other operating characteristics. Such a housing cavity for a blade root pivot shaft is described in document FR 21 07066.

[0003] The pressure of the cavity fluid is likely to vary over time, particularly with variations in engine speed and temperature variations. These pressure variations produce mechanical fatigue stresses that can be described as "oligocyclic", since the fatigue cycles are not always numerous. Certain materials that can be considered for the construction of seals, such as certain polymers and in particular PTFE (polytetrafluoroethylene) are however subject to mechanical fatigue, even with small stress variations during oligocyclic fatigue, and they are therefore exposed to damage.

[0004] The object of the invention is to increase the service life of such seals in response to alternating mechanical stresses, even at small numbers of cycles and moderate intensity variations.

[0005] The idea on which the invention is based is to produce a plastic deformation on the seal, or at least on the parts exposed to a stress concentration by the fluid. It has been found that this plastic deformation reduces the stress variations experienced during fatigue cycles. An increase in the service life of the seals, possibly beyond the expected service life of the mechanical assembly in which they are included, is then expected. According to the invention, the overpressure leading to the plastic deformation is produced during the assembly of the mechanical assembly and therefore under the exact service conditions of the seal.

[0006] In a general form, the invention thus relates to a method for preparing a polymer seal bordering a cavity of a fluid subject to variations in pressure during operations of a mechanical assembly in which the cavity is included and which comprises the seal, the method being characterized in that it consists, during an assembly of the mechanical assembly preceding the operations, in applying an assembly pressure in the cavity, said assembly pressure exerting a plastic deformation in at least a part of the seal.

[0007] According to optional, but favorable characteristics:

[0008] - the mounting pressure is equal to at least 2 times a maximum pressure of the fluid during operations;

[0009] - or, even more favorably, 2.5 times this maximum pressure.

[0010] Certain applications of this method, not exclusive of others, may concern:

[0011] - a PTFE seal, virgin or loaded with additives;

[0012] - a seal comprising two sealing lips joined by an intermediate strip and forming a concavity with the intermediate strip, the concavity of the seal belonging to the fluid cavity, said part of the seal comprising connecting portions of the lips to the intermediate strip overlooking the concavity;

[0013] - housing cavities of a variable-pitch propeller blade root journal, the housing also containing pivot bearings for the blade root in the housing, the fluid being lubricant for the bearings.

[0014] The various aspects, characteristics and advantages of the invention will now be described with the aid of the following figures, which describe a particular embodiment which is not exclusive of others:

[0015] [Fig-1]: general view of an aircraft on which the invention can be used;

[0016] [Fig.2]: schematic representation of the installation of the variable-pitch blades;

[0017] [Fig.3]: detailed representation, showing the seals and their location in the mechanical assembly;

[0018] [Fig.4]: section of one of the joints in isolation;

[0019] [Fig.5]: representation of the method of the invention;

[0020] [Fig.6]: mechanical stresses undergone by a portion of the joint without application of the invention;

[0021] [Fig.7]: mechanical stresses undergone by a portion of the joint with application of the invention.

[0022] Figures 1 and 2 will first be described. They partially represent a propeller rotor 1 of an aircraft engine rotating around an axis of rotation XX. The propeller comprises a circle of blades 2 distributed around the axis of rotation XX, and each of the blades 2 comprises a root 3. The propeller rotor extends in front of a main body 4 of the engine, which may comprise a second wheel 5 of fixed (or variable-pitch) blades straightening the air flow, a combustion chamber and expansion turbines. gases. Propeller 1 and wheel 5 lead directly into the outside atmosphere for this unducted engine.

[0023] The embodiment is more fully described in [Fig. 3]. The blades 2 are placed around a ring 6 of the rotor 1, and the ring 6 is provided with holes 7 distributed around its circumference to receive the roots 3 of the blades 2. They pivot around their axis, directed in a direction YY perpendicular or approximately perpendicular to the axis of rotation XX of the engine. The pivoting support of the roots 3 is provided by a pair of bearings 8 and 9, the outer ring of each of which is mounted on the wall of the corresponding hole 7, and the inner ring on the blade root 3.

[0024] From here on, "outer" or "external" on the one hand, "inner" or "internal" on the other hand, will generally be assigned according to opposite positions along the YY direction. Two sealing gaskets 10 and 11, the first 10 placed outside the outer bearing 8, and the second 11 inside the inner bearing 9, isolate a lubrication cavity 12 containing the bearings 8 and 9. Each of the gaskets 10 and 11 is circular with a U-shaped section comprising two essentially parallel and flat lips joined by an intermediate strip located at the largest diameters of the gasket 10 or 11.The outer seal 10 has an intermediate strip 13 which rests on a cylindrical surface of the ring 6; an outer lip 14 which rests on a conical flange 15 hollowed out in the center, the inner edge of which is mounted on the blade root 3, and which contributes to closing the cavity 12 by extending almost to the ring 6; and an inner lip 16 resting on a flat surface of the ring 6.

[0025] The inner seal comprises an intermediate strip 17 and an inner lip 18 which bear respectively on a cylindrical bearing surface and a flat bearing surface of a support ring 19 engaged in the bore 7 and retaining the outer ring of the inner bearing 9; and an outer lip 20 which bears on an inner flange 21. The latter, like the outer flange 15 mentioned above, is of hollow conical shape whose inner edge is mounted on the foot 3, and it contributes to closing the cavity 12 by extending almost as far as the ring 6. The device also comprises in particular a clamping assembly 22, provided with a nut for holding the inner ring of the inner bearing 9 against a flat bearing surface of the foot 3 in the YY direction.To summarize, the cavity 12 is delimited radially between the bore 7 and the blade root 3, axially between the outer 15 and inner 21 flanges; it contains in particular the bearings 8 and 9, as well as the seals 10 and 11, which respectively contribute to perfecting the sealing between the outer ends of the respective flanges 15 and 21 and the wall of the bore 7.

[0026] Each of the seals 10 and 11 includes a concavity 23 ([Fig.4]) between its lips; each concavity 23 opening into the cavity 12, is bathed by the lubricant contained in the cavity 12, and is subjected to its pressure.

[0027] The portions of the seals 10 and 11 likely to be most strongly stressed by this pressure are the surface connections 24 and 25 of the intermediate strips 13 and 17 to the lips 14, 16, 18 and 20, and more precisely near the surfaces facing the concavity 23. It is at these locations that stress concentrations are observed, and that risks of fatigue failure exist.

[0028] The method of preparing the seals 10 and 11 is shown succinctly in [Fig. 5]. It consists of filling the cavity 12 with a fluid and subjecting this fluid to a pressure sufficient to create plasticization at least at the locations subject to the risk of fatigue damage, therefore firstly at the surface connections 24 and 25. The application of overpressure is carried out during the assembly of the mechanical assembly, therefore before the engine is put into service. It can be carried out by any pressurizing device 26, for example a pump connected to a reservoir, acting through a lubrication orifice 27. It is plausible to use the same lubricant which fills the cavity 12 during service, but the method could possibly be carried out with another fluid.

[0029] Figures 6 and 7 illustrate the result obtained on a concrete configuration. The application of a service pressure on the surface connection 25 not subjected to prior plasticization gives ([Fig.6]) high local stress concentrations at a portion 28 giving onto the bottom of the concavity 23. If the same pressure is applied after plasticization, there is observed ([Fig.7]) an apparent spreading of the surface area of ​​the zone subjected to the stress concentrations, but which is combined with a reduction (up to 20%) of the values ​​of the high stresses in the portion 28, which therefore corresponds to an overall reduction in the stresses on the joint 10 or 11. The variations in the stresses on the joints 10 and 11 during the fatigue cycles will thus be much less significant.

[0030] The preparation pressure of the joints 10 and 11 must therefore be sufficient to plasticize said joints at least at the most constrained locations subsequently, among others at the portions 28 for the joints having the shape shown here. The pressure applied can, for better results, be significantly higher than this minimum value. It is possible to recommend a pressure 2 times, or even better 2.5 times higher than that which will be expected during the harshest conditions of the actual operating cycles.

Claims

Claims

1. Method for preparing a polymer sealing gasket (10, 11) bordering a cavity (12) filled with a fluid capable of being subject to pressure variations during operations of a mechanical assembly in which the cavity is included and which comprises the gasket, the method being characterized in that it consists, during assembly of the mechanical assembly preceding the operating cycles, in applying an assembly pressure in the cavity, said assembly pressure being equal to at least twice a maximum pressure of the fluid during the operating cycles to exert a plastic deformation in at least one portion (28) of the gasket.

2. 2. A preparation method according to claim 1, wherein the mounting pressure is at least 2.5 times the maximum fluid pressure during the operating cycles.

3. 3. The method of claim 1 or 2, wherein the seal is PTFE.

4. 4. Preparation method according to claim 1 to 3, wherein the seal comprises two sealing lips (14, 16; 18, 20) joined by an intermediate strip (13; 17) and forming a concavity (23) with the intermediate strip, the concavity of the seal belonging to the cavity (12) of the fluid, said portion (28) of the seal comprising surface connection parts (24; 25) of the lips to the intermediate strip, which open onto the concavity.

5. 5. Preparation method according to claim 4, in which the cavity is a housing of a root journal (3) of a blade (2) of a variable-pitch propeller, the housing also containing bearings (8, 9) for pivoting the blade root in the housing, the fluid being lubricant for the bearings.