METHOD FOR MANUFACTURED A TENSILE TEST PRODUCT BY DEPOSITTING SUCCESSIVE LAYERS OF MELTED FILAMENTS AND THE TENSILE TEST PRODUCT OBTAINED BY THIS METHOD
The method addresses the issue of unreliable tensile test results in additive manufacturing by creating a tensile specimen with a discontinuous section to isolate filaments, ensuring accurate mechanical behavior characterization and reliable data for material assessment.
Patent Information
- Application Number
- FR2022011297
- Authority / Receiving Office
- FR · FR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-10-28
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2042-10-28
AI Technical Summary
Existing tensile test methods for materials produced via additive manufacturing, particularly FFF technology, are influenced by the structure of molten filaments, making it difficult to accurately characterize the mechanical behavior of the material due to gaps and weaknesses at filament interfaces, leading to unreliable test results.
A method for manufacturing a tensile specimen with a discontinuous section in the narrow portion, where each molten filament is transversely spaced from adjacent filaments, allowing for a pure tensile force application without shearing, using additive manufacturing technology to create a specific geometry.
The method enables characterization of the material's mechanical behavior independently of the filament structure, providing reliable and representative data for part dimensioning.
Smart Images

Figure 00000011_0000 
Figure 00000011_0001 
Figure 00000012_0000
Abstract
Description
Title of the invention: METHOD FOR MANUFACTURED A TENSILE TEST TEST PROTECTION BY LAYER DEPOSIT SUCCESSIVE MELTED FILAMENTS AND TENSILE TEST TEST OBTAINED BY THIS PROCESS TECHNICAL FIELD OF THE INVENTION
[0001] The present invention relates to the field of tensile test specimens used for the characterization of materials.
[0002] The present invention relates more particularly to a method of manufacturing a tensile test specimen by depositing successive layers of molten filaments and a tensile test specimen obtained by the manufacturing process. TECHNOLOGICAL BACKGROUND OF THE INVENTION
[0003] There are manufacturing processes for parts by successively depositing layers of material using, for example, a molten polymer filament or a polyaryletherketone (PAEK) or polyetherimide (PEI) resin filament. An example of this type of manufacturing process is fused filament fabrication (FFF). FFF is an additive manufacturing technology, also called three-dimensional (3D) printing, involving the use of a 3D printer.
[0004] Figure 1 illustrates a 3D printer 2 according to the prior art comprising: • a print head 4 equipped with at least one extrusion nozzle 6, or extruder, • an 8-inch printing plate, and • a spool 9 of filament 14. The filament 14 from spool 9 is heated, melted and then deposited by the extrusion nozzle 6 of the print head 4 onto the print bed 8.
[0005] The print head 4 is mobile in translation along the X, Y and Z directions and its movement is guided along a predefined path so as to draw the part to be manufactured.
[0006] As a general rule, a part produced by a process is considered a homogeneous body. However, in the case of a part made by depositing successive layers of molten filaments, and more particularly using FFF technology, the resulting part is composed of a plurality of filaments deposited against and on top of each other. Spaces are formed between the molten filaments, and the presence of weaknesses at the interfaces of the molten filaments and the layers has a significant impact on the mechanical behavior of the part. For example, a part made of the same material produced by an injection manufacturing process and / or by FFF technology presents a different mechanical behavior for an identical geometry.
[0007] Conventionally, to obtain information on the elastic behavior, plastic behavior, and degree of tensile strength of a material when subjected to stress, a tensile test is performed using a tensile specimen. The tensile test allows the materials to be characterized independently of the shape of the stressed part.
[0008] There are various geometries of tensile test specimens used in additive manufacturing. The most common are standardized and have a continuous cross-section. Figure 2 is an example of a prior art tensile test specimen comprising: • a first and a second large portion 16, 18, • a narrow portion 20, longitudinal, extending along a traction axis X, and • a first and second connecting portions 28, 30 comprising transverse edges 32 connecting the first and second wide portions 16, 18 to the narrow portion 20.
[0009] In the case of a tensile test specimen produced by an injection molding process, a tensile test can therefore be considered to characterize the mechanical behavior of the material itself. However, in the case of a tensile test specimen produced by FFF technology, the structure of the deposited molten filaments has too significant an impact on the mechanical behavior of the part to assert that the tensile test characterizes the mechanical behavior of the material itself. Consequently, the result of the mechanical test on such a tensile test specimen is linked to the specific structure of the tensile test specimen tested, particularly to the arrangement of the molten filaments forming the final part. The predetermined geometry of tensile test specimens is therefore not particularly well-suited to a manufacturing process involving the deposition of successive layers of molten filaments.
[0010] Indeed, each parameter of molten filament deposition directly influences the results of the specimen's tensile tests. Consequently, it is difficult to know the actual behavior of the material and therefore to obtain representative data usable for dimensioning a part. Summary of the invention
[0011] The invention offers a solution to the problems mentioned above, by proposing a method for manufacturing a tensile test specimen by depositing successive layers of molten filaments and a tensile test specimen obtained by the manufacturing process and having a particular geometry.
[0012] One aspect of the invention relates to a method for manufacturing a test tube of traction by deposition of successive layers of molten filaments, comprising a step of making a discontinuous section within the tensile specimen, in a single layer, in which each molten filament extends along a traction axis X and is moved transversely away from an adjacent molten filament.
[0013] The creation of a discontinuous section of the tensile test specimen according to the invention makes it possible, thanks to the dissociation of the molten filaments from one another, to avoid any interaction between the filaments. Consequently, the result obtained during a tensile test on a tensile test specimen according to the invention characterizes the mechanical behavior of the material constituting the molten filament itself.
[0014] In addition to the characteristics mentioned in the preceding paragraph, the manufacturing process according to one aspect of the invention may have one or more additional characteristics from among the following, considered individually or in all technically possible combinations: The manufacturing process utilizes additive manufacturing technology through fused filament deposition, and The succession of layers of molten filaments forms the thickness of the tensile test specimen.
[0015] A second aspect of the invention relates to a tensile test specimen comprising: two large portions, and a narrow longitudinal portion extending along a traction axis X and connecting the two wide portions.
[0016] Each portion is geometrically defined by a lower surface and an upper surface, separated by a thickness. The tensile test specimen is obtained by the manufacturing process according to the first aspect of the invention, and the narrow portion comprises a discontinuous section.
[0017] In addition to the characteristics mentioned in the preceding paragraph, the tensile test specimen according to one aspect of the invention may have one or more additional characteristics from among the following, considered individually or in all technically possible combinations: The thickness of the tensile test specimen gradually decreases from the wide portions towards the discontinuous section of the narrow portion. Each molten filament of the discontinuous section is transversely separated from the adjacent molten filament by a distance dl greater than or equal to 0.2 mm, the lower surface of the discontinuous section is in a median plane P3 of each wide portion, parallel to their lower surface, and Each wide portion has a rectangular cross-section.
[0018] The invention and its various applications will be better understood by reading the following description and examining the accompanying figures. BRIEF DESCRIPTION OF THE FIGURES
[0019] Other advantages and features of the invention will become apparent from the following description, illustrated by the figures in which: • Fig. 1 schematically represents a central perspective view of an example of a 3D printer producing a part by depositing successive layers of molten filaments according to the state of the art; • Fig. 2 is a perspective view of a tensile test specimen according to the prior art; • Fig. 3 schematically represents a top view of a tensile test specimen according to the invention; • Fig. 4 schematically represents a partial perspective view of the tensile test specimen according to Fig. 3; • Fig. 5 schematically represents a side view of the tensile test specimen from Fig. 3. DETAILED DESCRIPTION
[0020] An example of an embodiment of a manufacturing process for a tensile test specimen according to the invention and of a tensile test specimen obtained by this manufacturing process are described in detail below, with reference to the accompanying drawings. This example illustrates the features and advantages of the invention.
[0021] Unless otherwise specified, the same element appearing on different figures has a unique reference.
[0022] For the purposes of understanding the invention, the vertical, longitudinal, and transverse orientations shall be adopted according to the coordinate system V, L, T shown in the figures, whose longitudinal axis L and transverse axis T extend in a horizontal plane LT. The vertical axis V extends along the thickness of the tensile test specimen, the longitudinal axis extends along the length of the specimen, and the transverse axis extends along the width of the specimen. By convention, the longitudinal axis L is oriented from a first wide portion to a second wide portion of the tensile test specimen according to the invention.
[0023] Figures 3, 4 and 5 illustrate a particular example of a tensile test specimen 10 according to the invention comprising: • a first and a second wide portions 16, 18 presenting a continuous cross-section, and • a narrow portion 20, longitudinal, extending along a traction axis X parallel to the longitudinal axis L and connecting the first and second wide portions 16, 18.
[0024] The terms "wide" and "narrow" are not dimensioned; they are defined by comparison with each other for the same test specimen. Thus, the narrow portion of a the test specimen has a transverse dimension (along the T axis) greater than the transverse dimensions of the wide portions of said test specimen, the transverse dimensions of the wide portions being or not identical.
[0025] The tensile test specimen 10 is symmetric with respect to a plane PI parallel to the plane VL of the frame VLT and including the tensile axis X and with respect to a plane P2 parallel to the plane VT of the frame VLT including an axis Y perpendicular to the tensile axis X and passing through the center of the tensile test specimen 10.
[0026] The tensile test specimen 10 is geometrically defined by a lower surface 22 and an upper surface 24, separated by a thickness e of the tensile test specimen. More specifically, the thickness e of the tensile test specimen 10 varies such that each wide portion 16, 18 is defined by a thickness e1, the narrow portion 20 is defined by a thickness e2, and each connecting portion 28, 30 is defined by a thickness e3.
[0027] As shown in Figures 3, 4, and 5, the narrow portion 20 is connected to each of the wide portions 16 and 18 by a connecting portion 28 and 30, respectively. Each of the connecting portions 28 and 30 has a continuous cross-section. The width of each connecting portion 28 gradually decreases from the lateral end adjacent to the wide portion 16 and 18 to the lateral end adjacent to the discontinuous section 26 of the narrow portion 20. As illustrated in Figures 3, 4, and 5, each connecting portion 28 and 30 includes a transverse edge 32 that can form an arc of a circle.
[0028] According to the embodiment illustrated in [Fig.4], each wide portion 16, 18 has a rectangular cross-section. The narrow portion 20, with a rectangular cross-section, includes a discontinuous section 26 which extends over the entire width of said narrow portion 20. The thickness e3 of the connecting portions 28, 30 gradually decreases from the wide portions 16, 18 towards the discontinuous section 26 so as to uniformize the geometry of the tensile test specimen 10. More particularly, the thickness e3 of each connecting portion 28, 30, at the level of the lateral end adjacent to the wide portion 16, 18, is substantially equal to the thickness el of each wide portion 16, 18; and the thickness e3 of each connecting portion 28, 30, at the level of the lateral end adjacent to the discontinuous section 26 of the narrow portion 20, is substantially equal to the thickness e2 of the narrow portion 20.
[0029] The discontinuous section 26 comprises a plurality of dissociated fused filaments 14, also called strands, which extend along the traction axis X and which are arranged parallel to each other along a transverse direction T, all being contained in a median plane P3 parallel to the plane LT and comprising the traction axis X. In contrast, each plane parallel to the plane PI contains only one and the same fused filament 14.
[0030] Furthermore, the molten filaments 14 of the discontinuous section 26 are separated transversely The molten filaments 14 are separated from each other by a distance dl sufficiently large to prevent any contact between them. Preferably, the distance dl is greater than or equal to 0.2 mm (millimeters). The discontinuous section 26 of the tensile test specimen 10 according to the invention therefore has a discontinuous cross-section, shown in dotted lines.
[0031] According to an embodiment as illustrated in figures 3, 4 and 5, the discontinuous section 26 extends over the entire length of the narrow portion 20. The ends of the narrow portion 20 define a first and second junction 34, 36 with the discontinuous section 26 whose thickness corresponds substantially to the thickness e2 of a fused filament 14 of the discontinuous section 26 of the narrow portion 20.
[0032] According to another embodiment, not shown, the discontinuous section 26 extends over only part of the length of the narrow portion 20. In this case, the narrow portion 20 comprises a first and a second part whose cross-section is continuous and connected, at one end, to the first and second wide portions 16, 18 and, at the other end, to the discontinuous section 26 defining the first and second junctions 34, 36 and whose thickness corresponds substantially to the thickness e2 of a molten filament 14 of the discontinuous section 26 of the narrow portion 20.
[0033] As illustrated in [Fig.5], the tensile test specimen 10 according to the invention is made by depositing successive layers 12 of molten filaments 14, along a deposition direction Z parallel to the vertical axis V.
[0034] For the production of the tensile test specimen 10, with the exception of the discontinuous section 26 of the narrow portion 20, the molten filaments 14 are joined and assembled to each other so as to form a layer 12 on which a new layer 12 is deposited so as to form the geometry of the test specimen 10.
[0035] Advantageously, the succession of layers 12 of molten filaments 14 forms the thickness e of the tensile test specimen 10. The first layer 12 forms the lower surface 22 and the last layer 12 forms the upper surface 24 of the tensile test specimen 10.
[0036] The discontinuous section 26 of the tensile test specimen 10 is formed in a single layer 12 in which each molten filament 14 extends along the tensile axis X and is transversely separated from an adjacent molten filament 14. In other words, a single layer of molten filaments 14 is deposited in the area of the tensile test specimen 10 intended to form the discontinuous section 26, while several layers 12 of molten filaments 14 are deposited one above the other in the other areas of the tensile test specimen 10.
[0037] During a mechanical tensile test, intended to characterize the material of the tensile specimen 10, for example an extruded polymer, the useful area, i.e. the area that will be mechanically stressed, is the narrow portion 20 of the specimen traction 10, and more specifically the discontinuous section 26.
[0038] The effective area of the tensile test specimen 10 according to the invention is structureless due to the separation of the fused filaments 14 of the discontinuous section 26 from one another. Consequently, during a tensile test, each fused filament 14 is subjected to a pure tensile force, thus avoiding any shearing phenomenon between the fused filaments 14. Furthermore, the fact that the fused filaments 14 are separated from one another by a distance dl allows for meaningful tests to be carried out on the material itself.
[0039] Advantageously, as illustrated in [Fig. 5], the lower surface 22 of the discontinuous section 26 is in the median plane P3 of each wide portion 16, 18, parallel to their lower surface 22. In other words, the single layer 12 of molten filaments of the discontinuous section 26 is in the extension of the intermediate layer 12 of molten filaments located in the median plane P3 of each wide portion 16, 18. Furthermore, each wide portion 16, 18 is symmetrical about the median plane P3, such a feature improving the feasibility of tensile testing of the tensile specimen 10.
[0040] According to a preferred embodiment of the invention, the manufacturing process used to produce the tensile test specimen according to the invention implements additive manufacturing technology by fused filament deposition (FFD). This fused filament 14 can be a polymer filament, for example polylactic acid (PLA) or acrylonitrile butadiene styrene (ABS) or even polyaryl-therketone (PAEK) or polyetherimide (PEI) type resin.
[0041] The manufacturing process comprises the following steps: • deposition of a first layer 12 of molten filaments 14 onto a base such as a plate 8, and • deposition of an additional layer 12 of molten filament 14 on the previous layer in the vertical direction V, this step being repeated until the last layer of molten filaments 14 is deposited, thus forming the tensile test specimen 10.
[0042] The use of this technology for the manufacture of the tensile test specimen 10 according to the invention requires that the printed area of each layer 12 of molten filament, corresponding to a section plane of the test specimen parallel to the LT plane, be supported by a previous printed layer 12.
[0043] The discontinuous section 26 of the narrow portion 20 is made during the deposition of a single layer 12 of molten filaments, the deposition of successive layers being limited to the wide portions 16, 18 and the bonding portions 28, 30. More particularly, the discontinuous section 26 is made during the deposition of the median, or intermediate, layer 12 of molten filaments in the median plane P3 of each wide portion 16, 18.
[0044] According to certain embodiments, the successive deposition of the first layer to the last layer 12 of molten filaments 14 of the tensile test specimen 10, with the exception of the middle layer 12 of molten filaments 14, includes the deposit: • from the first layer 12 of filaments 14 melted from the first and second wide portions 16, 18, and • of the first layer 12 of filaments 14 melted from a section of the first and second bonding portions 28, 30.
[0045] The successive deposition of the layer 12 of fused filaments 14 in the middle of the tensile test specimen 10 comprises the deposition: • of 12 layers of 14 molten filaments from the first and second wide portions 16, 18, • of layers 12 of molten filaments 14 of the first and second bonding portions 28, 30, and • of the single layer 12 of filaments 14 of the discontinuous section 26 of the narrow portion 20.
[0046] According to some embodiments, the manufacturing process includes a step of manufacturing a support material 40 used during the fabrication of the tensile test specimen 10 in order to create a support structure to support at least the molten filaments 14 of the discontinuous section 26 of the narrow portion 20. Advantageously, the support material 40 is in the form of thinner molten filaments and generally made of a different material than that used for the fabrication of the tensile test specimen 10. According to one embodiment shown in [Fig. 5], the support material 40 is located below the molten filaments 14 of the discontinuous section 26 and below each of the first and second bonding portions 28, 30. According to another embodiment, not shown, the support material 40 is located below the complete tensile test specimen 10.
[0047] The manufacturing process of a tensile test specimen 10 according to the invention offers a solution for characterizing the actual behavior of the material constituting the tensile test specimen 10. Indeed, thanks to the dissociation of the molten filaments 14 of the discontinuous section 26 from each other, the result of a tensile test carried out on a tensile test specimen 10 according to the invention is no longer linked to the particular structure of the tensile test specimen, that is to say to the assembly of the molten filaments 14 forming the final part, but only to the material of the molten filament 14.
[0048] Consequently, the use of a tensile test specimen 10 according to the invention for tensile tests makes it possible to obtain a representative data usable for the dimensioning of the parts to be produced by depositing successive layers of molten filaments.
Claims
Claims
1. Method for manufacturing a tensile test specimen (10) by depositing successive layers (12) of molten filaments (14), comprising a step of producing a discontinuous section (26) of the tensile test specimen (10), in a single layer, in which each molten filament (14) extends along a tensile axis (X) and is transversely spaced from an adjacent molten filament (14).
2. Method for manufacturing a tensile test piece (10) according to claim 1, characterized in that it implements additive manufacturing technology by deposition of fused filaments.
3. Method of manufacturing a tensile test piece (10) according to any one of the preceding claims, characterized in that the succession of layers (12) of melted filaments (14) forms a thickness (e) of the tensile test piece (10).
4. Tensile test piece (10) comprising: - two wide portions (16, 18), and - a longitudinal narrow portion (20) extending along a tensile axis (X) and connecting the two wide portions (16, 18), - each portion (16, 18, 20) being geometrically defined by a lower surface (22) and an upper surface (24), separated by a thickness (e1, e2), characterized in that it is obtained by the manufacturing method according to any one of the preceding claims, and in that the narrow portion comprises a discontinuous section.
5. Tensile test piece (10) according to claim 4, characterized in that the thickness (e) of the tensile test piece (10) decreases progressively from the wide portions (16, 18) towards the discontinuous section (26) of the narrow portion (20).
6. Tensile test piece (10) according to claim 4 or 5, characterized in that each molten filament (14) of the discontinuous section (26) is transversely spaced from the adjacent molten filament (14) by a distance (dl) greater than or equal to 0.2 mm.
7. Tensile test piece (10) according to any one of claims 4 to 6, characterized in that the lower surface (22) of the discontinuous section (26) is in a median plane (P3) of each wide portion
8. (16, 18), parallel to their lower surface (22). Tensile test piece (10) according to any one of claims 4 to 7, characterized in that each wide portion (16, 18) has a rectangular cross-section.