Realization of a Josephson junction quantum device

A quantum device with a crystalline semiconductor substrate protected by a charge trapping layer addresses the degradation issues during manufacturing, enhancing the quality factor and coherence time of the resonator.

FR3143949B1Active Publication Date: 2024-11-29COMMISSARIAT A LENERGIE ATOMIQUE ET AUX ENERGIES ALTERNATIVES
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
FR2022013899
Authority / Receiving Office
FR · FR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-12-20
Publication Date
2024-11-29
Estimated Expiration
2042-12-20

AI Technical Summary

Technical Problem

Existing quantum devices with Josephson junctions face issues such as degradation of the substrate surface layer due to etching processes, leading to reduced quantum coherence time and resonator quality factor, especially when integrated with CMOS technology.

Method used

A quantum device structure is developed with a crystalline semiconductor substrate protected by a charge trapping layer, such as hydrogenated amorphous silicon or silicon nitride, which prevents defects and maintains the integrity of the surface layer during manufacturing, thereby improving the quality factor and coherence time of the resonator.

Benefits of technology

The proposed structure enhances the quality factor and coherence time of the resonator by preventing defects and maintaining the integrity of the substrate surface, ensuring low-loss operations and improved performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000013_0000
    Figure 00000013_0000
  • Figure 00000013_0001
    Figure 00000013_0001
  • Figure 00000013_0002
    Figure 00000013_0002
Patent Text Reader

Abstract

Fabrication of a structure for a quantum device comprising: - a substrate (10) having a surface layer (102) of crystalline silicon, - a Josephson junction (160) formed of a first metallic portion (132), made of superconducting material (134), coated with an insulating zone (145), the insulating zone itself being coated with a second metallic portion (152) made of superconducting material (134) and enveloping the insulating zone (145) and the first metallic portion (132), the first metallic portion (132) and the second metallic portion (152) being arranged on and in contact with a layer (116) called a "protective" layer arranged on or in the substrate (10). Figure for the abstract: 1I.
Need to check novelty before this filing date? Find Prior Art

Description

Title of the invention: Production of a quantum device with a Josephson junction TECHNICAL FIELD AND PRIOR ART

[0001] The present application relates to the field of quantum devices provided with at least one structure comprising a Josephson junction associated with a resonator as well as to a method of manufacturing such a structure.

[0002] Resonators, in particular superconducting resonators, are components allowing the reading of spin states of quantum devices implementing quantum bits commonly called “qubits” or “Qbits”.

[0003] A resonator of a quantum device is typically in the form of at least one microwave transmission line designed to be the location of resonant oscillations under certain particular conditions.

[0004] Quantum computing requires low-loss operations of the resonators.

[0005] Quantum devices with qubits formed by means of Josephson junctions coupled to a superconducting resonator and in which quantum information can be exchanged via a photon have appeared.

[0006] The document: "Path toward manufacturable superconducting qubits with relaxation times exceeding 0.1 ms", by Verjauw et al., npj Quantum Information volume 8, Article number: 93 (2022) provides for the production of a quantum device with a Josephson junction having a particular arrangement and which is implemented on a substrate compatible with the integration of components in CMOS technology ("Complementary Metal Oxide Semiconductor" or "complementary metal oxide semiconductor"). The production of the Josephson junction includes the deposition of superconducting material such as aluminum on a substrate and then a structuring of this material.

[0007] This embodiment may use etching processes which tend to introduce defects into the substrate on which the junction is made.

[0008] An argon ion beam milling process can be used in particular to remove a native oxide layer which forms on thin aluminum layers due to their exposure to the atmosphere between two lithographic steps. It is generally sought to avoid such oxide layers which can prove harmful to the resonator.

[0009] This step as well as other dry etching steps can lead to degradation of the surface layer of the substrate which can limit the quantum coherence time as well as the quality factor of the resonators formed on the latter.

[0010] One way of improving the performance of such devices when they are produced on a silicon substrate and of protecting against the harmful consequences linked to the cleaning and / or etching processes is, once the resonator structure has been produced, to etch the surface of the silicon substrate in a region located opposite the Josephson junction(s) and the resonator.

[0011] Such etching must be controlled, particularly in the presence of charges for the performance of the Josephson Junction. In addition, such etching poses a problem, particularly in a case where it is desired to achieve co-integration of the structure with components in the surface layer of the substrate.

[0012] The problem arises of producing a new quantum circuit device which is improved with respect to at least one of the drawbacks mentioned above. Statement of the invention

[0013] It is therefore an object of the present invention to provide a structure for a Josephson junction quantum device comprising:

[0014] - a substrate provided with a surface layer of a semiconductor material crystalline, especially crystalline silicon,

[0015] - at least one Josephson junction, formed of at least a first portion me metal, made of superconducting material, coated with an insulating zone, said insulating zone itself being coated with a second metallic portion made of superconducting material and the second metallic portion covering said insulating zone and said first metallic portion,

[0016] the first metal portion and the second metal portion being arranged on and in contact with a so-called “protective” layer arranged on the substrate or belonging to the substrate, said protective layer being a charge trapping layer.

[0017] With such an arrangement, the presence of crystalline defects in the crystalline surface semiconductor layer is avoided or it is ensured that possible defects in the protective or charge trapping layer are not detrimental to the crystalline surface semiconductor layer and to the operation of the device.

[0018] The Josephson junction is typically coupled or connected to a resonator. With an arrangement as defined above, the quality factor of the resonator is improved in this case.

[0019] The crystalline semiconductor layer is typically a silicon layer.

[0020] Advantageously, the charge trapping layer is a semi- conductive, in particular hydrogenated amorphous silicon (aSi:H) or polysilicon or a layer of dielectric material, in particular silicon nitride.

[0021] An arrangement as defined above can advantageously make it possible to provide a surface layer of the substrate made of crystalline semiconductor material of re- low sistivity.

[0022] By “low” resistivity we mean a resistivity of less than 50 Q.cm and typically between 1 Q.cm and 20 Q.cm, in particular between 10 Q.cm and 20 Q.cm.

[0023] The first metal portion and the second metal portion are made of a given superconducting material, which may in particular be aluminum.

[0024] According to one possible implementation, the first metal portion is arranged on and in contact with a first metal track while the second metal portion is arranged on and in contact with a second metal track, the first metal track and the second metal track being made of a superconducting material different from said given superconducting material, this different superconducting material possibly being in particular Niobium.

[0025] The charge trapping layer may be disposed on the surface layer, the charge trapping layer being made of amorphous semiconductor material or polycrystalline material or a layer of dielectric material such as silicon nitride.

[0026] Advantageously, the protective layer extends entirely in contact with the surface layer of the substrate.

[0027] The first metal track or the second metal track may be connected or coupled to a resonator.

[0028] Preferably, the first metal track and the second metal track are arranged opposite said protective layer or the charge trapping layer.

[0029] According to an alternative embodiment, the charge trapping layer may be provided in a semiconductor base of the substrate, the substrate being a semiconductor-on-insulator substrate provided with an insulating layer arranged between the semiconductor base and the surface layer of crystalline semiconductor material, the insulating layer and the surface layer of crystalline semiconductor material not extending opposite said Josephson junction.

[0030] According to another aspect, the present invention relates to a method of manufacturing a quantum device as defined above.

[0031] More particularly, according to a first possible implementation, the present invention relates to a method of manufacturing a structure as defined above and comprising, in this order, the following steps:

[0032] - providing the substrate with the surface layer of semiconductor material crystalline, then

[0033] - depositing the protective or charge trapping layer on said super layer official, then

[0034] - produce on said protective layer, the first metallic portion, then the zone insulating on the first metal portion, then the second metal portion on the insulating area.

[0035] Advantageously, the insulating zone can be formed by oxidation of the first metal portion.

[0036] According to one possible implementation, the method may comprise in this order, after the deposition of the protective layer and prior to the formation of the first metal portion: the formation of a first metal track and a second metal track on said protective layer by deposition then etching of a first metal layer in a given superconducting material.

[0037] According to a second possible implementation, the present invention relates to a method for manufacturing a structure as defined above and in which the substrate is a semiconductor on insulator provided with a semiconductor base provided with a charge trapping layer, an insulating layer arranged on the charge trapping layer and disposed between the semiconductor base and the surface layer of crystalline semiconductor material, the method comprising steps of:

[0038] - removal of the surface layer and the insulating layer in an area localized from the substrate, so as to reveal the charge trapping layer, then

[0039] - producing in said localized area of ​​the substrate, the first metallic portion on the charge trapping layer, then the insulating area on the first metal portion, then the second metal portion on the insulating area. Brief description of the drawings

[0040] The present invention will be better understood on reading the description of exemplary embodiments given, for purely indicative and non-limiting purposes, with reference to the appended drawings in which:

[0041] Figures 1A, 1B, 1C, 1D, 1E, 1F, 1G, 1H, 1I1 serve to illustrate an exemplary embodiment of a quantum device provided with a structure formed by a Josephson junction coupled to a resonator and in which a protective layer is interposed between the structure and a surface layer of crystalline semiconductor material of a substrate;

[0042] Figures 2A-2B serve to illustrate a particular embodiment of a Josephson junction covering;

[0043] [Fig.3] serves to illustrate an alternative embodiment in which the layer of protection is a dielectric layer, particularly of the pre-metallic type;

[0044] [Fig.4] serves to illustrate an alternative embodiment in which the junction is made on the trapping layer of a semiconductor-on-insulator type substrate provided with a charge trapping layer;

[0045] Identical, similar or equivalent parts of the different figures bear the same numerical references so as to facilitate the transition from one figure to another.

[0046] The different parts represented in the figures are not necessarily on a uniform scale, in order to make the figures more readable.

[0047] DETAILED DESCRIPTION OF PARTICULAR EMBODIMENTS

[0048] We first refer to [Fig.lA] which gives a sectional view of an example of a starting substrate for the implementation of a quantum device, in particular with spin Qbits, and equipped with at least one Josephson junction coupled or connected to a resonator.

[0049] The substrate 10 is provided with a semiconductor surface layer 102 made of crystalline semiconductor material, in particular crystalline silicon. Advantageously, the surface layer 102 may here be a layer made of crystalline semiconductor material of low resistivity, i.e. of resistivity less than 50 Ω.cm and typically between 1 Q.cm and 20 Q.cm.

[0050] According to one possible implementation and as illustrated in the embodiment of [Fig. 1A], the substrate 10 may be of the semiconductor-on-insulator type, in particular SOI (“Silicon On Insulator”, i.e. Silicon on insulator) and in this case comprises a semiconductor base 100, a buried insulating layer 101, typically called BOX (“Buried Oxide” or “buried oxide”), arranged on the semiconductor base 100 and located between the semiconductor surface layer 102 and the semiconductor base 100. The surface layer 102 may be provided with a thickness of, for example, between 10 nm and 10 μm, advantageously between 50 nm and 200 nm.

[0051] According to a particular step of the method, the substrate 10 is coated here ([Fig. 1B]) with a so-called “protective” layer 116. The material of this layer 116 can preferably be chosen so that at the operating frequency of the resonator, the layer 116 has a low intrinsic loss angle δ so that δintrinsic δex 106 is between 0.1 and 1000. The operating frequency of the resonator can be between, for example, 1 and 10 GHz, advantageously between 4 and 8 GHz.

[0052] Advantageously, the protective layer 116 is a free charge trapping layer. The protective layer 116 may be made of amorphous semiconductor material or polycrystalline material and / or porous semiconductor material.

[0053] According to an advantageous embodiment, the protective layer 116 may be provided in amorphous silicon, in particular hydrogenated amorphous silicon (a-SiH). The thickness of the protective layer 116 may, in this case, be provided for example between 10 nm and 10 μm, advantageously between 50 nm and 200 nm.

[0054] Alternatively, a protective layer 116 made of polysilicon and / or porous silicon may be provided. The thickness of this protective layer 116 may in this case be planned for example between 10 nm and 10 pm, advantageously between 50 nm and 200 nm.

[0055] According to another exemplary embodiment, the charge trapping layer 116 may be an insulator, for example a pre-metallic insulator (PMD) such as silicon nitride (SixNy with x 0 and y 0). The thickness of this layer may in this case be provided for example between 10 nm and 10 pm, advantageously between 50 nm and 200 nm.

[0056] In this particular embodiment, the protective layer 116 is advantageously deposited full plate and can cover the surface semiconductor layer 102 entirely. Subsequently, the protective layer 116 is advantageously preserved without subsequent etching of this layer 116 being necessary.

[0057] A metallic layer 121 is then formed ([Fig.lC]) on the protective layer 116, made of a first superconducting material 124, in particular Niobium (Nb) or Tantalum nitride (TaN) on the support layer 116. Alternatively, other superconducting materials may be used, for example a superconductor chosen from the following: TiN, NbTiN, NbN, AIOx, InOx, heavily doped or degenerate silicon, i.e. with a concentration greater than 1019 dopants / cm3, Tungsten, or cobalt silicide (CoSi2).

[0058] A metallic layer 121 of Niobium with a thickness of, for example, between 1 nm and 1000 nm, for example of the order of 150 nm, may in particular be provided.

[0059] An etching ([Fig.lD]) is then carried out in the metal layer 121 so as to form metal tracks, in particular a first metal track 122A and a second metal track 122B.

[0060] Typically, the etching is a dry etching, in particular using a plasma and carried out through a masking (not shown). Dry etching via a plasma can be implemented, for example.

[0061] One of these tracks 122A, 122B, may be connected or coupled to a resonator for example in the form of a microwave transmission line or one or more waveguides, designed to be the location of resonant oscillations and which may also be formed in the metal layer 121.

[0062] A metallic layer 131 is then deposited ([Fig.lE]) in a second superconducting material 134, here different from the first superconducting material 124, and which may be easier to model than the first superconducting material 124. The second superconducting material 134 may for example be aluminum (Al). Alternatively, other superconducting materials may be used, for example a superconductor chosen from the following: TiN, TaN, NbTiN, NbN, AIOx, InOx, heavily doped silicon, Tungsten, or cobalt silicide (CoSi2).

[0063] A metallic layer 131 of Aluminum with a thickness of, for example, between 1 nm and 70 nm, in particular between 1 and 10 nm, may in particular be provided.

[0064] An etching ([Fig.lF]) is then carried out in the metallic layer 131 in such a way to form one or more metal portions, in particular at least a first metal portion 132 arranged on one of the metal tracks 122A, 122B, for example on the first track 122A previously formed. Dry etching using a plasma or wet etching and for example using a chlorinated solution BC13 can be implemented.

[0065] The first metal portion 132 is here arranged so as to overlap a part of the conductive track 122A and thus extends both on an upper face of the conductive track 122A and on its lateral faces. In the particular embodiment illustrated in [Fig. 1F], the metal portion 132 is formed of a region 138 which coats the track 122A and of an end region 137 in the extension of this region 138 for example in the form of a bar and which is narrowed relative to the region 138.

[0066] An insulating zone 145 is then formed on the metal portion 132. The embodiment illustrated in [Fig. 1G] provides in particular for the implementation of this insulating zone 145 by oxidation of the superconducting material 134, in this example aluminum. The oxidation can for example be carried out at a temperature of the order of 300°C and under an atmosphere of the order of 1.33 Pa. The oxidation of the material 134, in particular aluminum, of the metal portion 132 is preferably carried out while preserving the material 124 of the tracks 122A, 122B, in particular niobium. For this, a masking covering the tracks 122A, 122B but comprising at least one opening revealing

[0067] A metallic layer 151 of superconducting material is then deposited ([Fig.lG]), typically based on the second superconducting material 134, here different from the first superconducting material 124, and which may be aluminum (Al).

[0068] A metallic layer 151 of Aluminum with a thickness of, for example, between 2 nm and 70 nm, in particular between 10 nm and 30 nm, may in particular be provided.

[0069] An etching ([Fig.lH]) is then carried out in the metal layer 151 so as to form one or more metal portions, in particular at least one metal portion 152 arranged on the second track 122B, in previously formed superconducting material 124. A dry etching using a plasma or wet etching and for example using a chlorinated solution BC13 can be implemented.

[0070] The second metal portion 152 is here arranged so as to overlap a portion of the conductive track 122B and thus extends both on an upper face of the conductive track 122B and on its lateral faces. In the particular embodiment illustrated in [Fig. II], the metal portion 152 is formed of a region 158 which overlaps the track 122B and of an end region 157 in the extension of this region 158 for example in the form of a bar and which is narrowed relative to the region 158. The second metal portion 152 here covers, by means of its region end 157, a part of the insulating zone 145 and of the first metal portion 132, in particular the end region 137 of this metal portion 132.

[0071] A Josephson junction structure 160 called “enveloping” or “bridge” as illustrated in the perspective views of Figures II and 2A and the cross-sectional view (the section being made along an axis X'X given in [Fig.2A]) of [Fig.2B] is thus made on the protective layer 116.

[0072] The production of this junction, and in particular of the metal portions 132, 152, may in particular involve one or more steps of stripping by argon milling ("Ar milling" according to English terminology) and / or one or more steps of dry etching.

[0073] The protective layer 116 on which the tracks 122A, 122B and the metal portion 132 rest then makes it possible in particular to protect the surface semiconductor layer 102 of the substrate from such steps, which is made of crystalline semiconductor material.

[0074] This Josephson junction 160 is produced here without having to etch the protective layer 116 and without having to etch parts of the surface layer 102 made of crystalline semiconductor material arranged opposite the Josephson junction.

[0075] This avoids introducing defects or impurities into the surface layer 102 during the manufacturing process and in particular during etching and / or stripping steps implemented during this process, for example to form the metal tracks and / or portions 132, 152, 122A, 122B.

[0076] An advantage of implementing the intermediate layer 116, between the surface layer 102 of the substrate and the metal layers 131, 151 in which the coupled Josephson junction is formed, is that it makes it possible to obtain an improved coherence time of the qubits.

[0077] An advantage of implementing the intermediate layer 116, between the surface layer 102 of the substrate and the metal layer 121 in which the resonator is formed, is that it makes it possible to obtain a resonator with low parasitic losses and an improved quality factor.

[0078] According to a variant of the embodiment described above, a protective layer 216 as described above can be formed, once the tracks 122A, 122B, made of superconducting material 124, for example Niobium, have been formed. Such a variant, however, has the particularity compared to the previous one of requiring, as illustrated in the structure of [Fig. 3], the production of openings 217B in the protective layer 216. Such openings 217B, typically formed after this layer 216, are made to be able to make it possible to implement contact with the conductive portions 132, 152 of the Josephson junction 160. For such a variant, the protective layer 216 can be by example a layer of PMD insulation such as silicon nitride with a thickness of, for example, around 20 nm.

[0079] According to another embodiment variant, it is possible to provide for the Josephson junction to be produced on a charge trapping layer this time belonging to a substrate 10' and in particular a substrate of the semiconductor on insulator type and provided with a charge trapping layer 16' and commonly called "trap rich". Such a layer 16' belongs to the semiconductor base located under the insulating layer 102. This charge trapping layer 16', which may be made of polycrystalline semiconductor material and in particular polysilicon, is typically arranged against and in contact with the insulating layer 101 of the substrate 10'.

[0080] To obtain such an arrangement, it is possible in this case to remove the surface layer 102 of the substrate 10' and the insulating layer 101 in a localized zone Z1 of the substrate 10'. The surface layer 102 of the substrate 10' and the insulating layer 101 are, on the other hand, preserved in other zones Z2 of the substrate 10'.

[0081] In the embodiment illustrated in [Fig.4], both the Josephson junction 160 and the metal layer 121 in which the resonator is made are formed in the localized zone ZI of the substrate 10' without a surface layer 102 or an insulating layer 101. Compared to the method described previously in connection with FIGS. 1A-1I, such a variant has the particularity that it requires additional etching steps.

[0082] Thus, it is possible to start with a substrate 10' of the semiconductor on insulator type and provided with a charge trapping layer 16', for example an RFeSI™ SOI substrate from the company SOITEC, then deposit a masking on a zone Z2 to be protected from the substrate and etch in a localized zone ZI revealed and not covered by the masking the surface layer 12 and the insulating layer 101 of BOX.

[0083] Then, steps are carried out as described previously in connection with FIGS. 1C-1I in order to produce the metal tracks 122A, 122B and the Josephson junction 160 on the charge trapping layer 16'.

Claims

Claims

1. Structure for a quantum device with a Josephson junction comprising: - a substrate (10, 10') provided with a surface layer (102) made of a crystalline semiconductor material, in particular crystalline silicon, - at least one Josephson junction (170), formed of at least a first metal portion (132), made of a superconducting material (134), coated with an insulating zone (145), said insulating zone itself being coated with a second metal portion (152) made of a superconducting material (134) and the second metal portion (152) covering said insulating zone (145) and said first metal portion (132), the first metal portion (132) and the second metal portion (152) being arranged on and in contact with a so-called "protective" layer (116, 16') arranged on the substrate (10) or belonging to the substrate (10'), said layer (116, 16') of protection being a charge trapping layer.

2. The structure of claim 1, wherein the charge trapping layer (116) is hydrogenated amorphous silicon (aSi:H) or polysilicon.

3. The structure of claim 1, wherein the charge trapping layer (116) is based on silicon nitride.

4. Structure according to one of claims 1 to 3, in which the surface layer (102) of the substrate (10) is made of crystalline semiconductor material with low resistivity and between 10 Q.cm and 20 Q.cm.

5. Structure according to one of claims 1 to 4, in which the protective layer (116) extends entirely in contact with the surface layer (102) of the substrate (10).

6. Structure according to one of claims 1 to 5, in which the first metal portion (132) and the second metal portion (152) are made of a given superconducting material (134), in particular aluminum and in which the first metal portion is arranged on and in contact with a first metal track (122A), the second metal portion being arranged on and in contact with a second metal track (122B), the first metal track and the second metal track being made of a superconducting material (124), different from said given superconducting material (134).

7. Structure according to one of claims 1 to 6, the charge trapping layer being arranged on said surface layer (102), the layer of charge trapping being made of amorphous semiconductor material (112) or polycrystalline material or a layer of dielectric material (115) such as silicon nitride.

8. Structure according to one of claims 1 to 6, the charge trapping layer (16') being provided in a semiconductor base (100) of the substrate, the substrate being a semiconductor-on-insulator substrate provided with an insulating layer (101) arranged between the semiconductor base (10) and the surface layer (102) of crystalline semiconductor material, the insulating layer (101) and the surface layer (102) of crystalline semiconductor material not extending opposite said Josephson junction (170).

9. A quantum device comprising a structure according to one of claims 1 to 8, wherein a resonator is coupled to a first metal track (122A) or to a second metal track (122B), the resonator, the first metal track (122A) and the second metal track (122B) being arranged opposite said protective layer (116).

10. Method of manufacturing a structure according to one of claims 1 to 7, comprising, in this order, the following steps: - providing the substrate (10) provided with the surface layer (102) of crystalline semiconductor material, then - depositing the protective layer (116) on said surface layer (102), then - producing on said protective layer (116), the first metal portion (132), then the insulating zone (145) on the first metal portion (132), then the second metal portion (152) on the insulating zone (145).

11. The method of claim 10, wherein the insulating region (145) is formed by oxidation of the first metal portion (132).

12. Method according to one of claims 10 or 11, comprising, in this order, after the deposition of the protective layer (116) and prior to the formation of the first metal portion (132), the formation of a first metal track (122A) and a second metal track (122B) on said protective layer (116) by deposition then etching of a first metal layer (121) in a given superconducting material (124).

13. A method of manufacturing a structure according to claim 8, wherein the substrate (10) is a semiconductor on insulator having a base semiconductor provided with a charge trapping layer (16'), an insulating layer (101) arranged on the charge trapping layer (16') and disposed between the semiconductor base (10) and the surface layer (102) of crystalline semiconductor material, the method comprising steps of: - removal of the surface layer (102) and the insulating layer (101) in a localized area of ​​the substrate (10'), so as to reveal the charge trapping layer (16'), then - producing in said localized zone (Zl) of the substrate, the first metal portion (132) on the charge trapping layer (16'), then the insulating zone (145) on the first metal portion (132), then the second metal portion (152) on the insulating zone (145).