Method for manufacturing an integrated electro-optical device and the electro-optical device thus obtained
By machining the residue of the proton exchange layer between electrodes, the method stabilizes the electro-optical response of integrated devices, addressing unstable responses due to environmental changes and frequency variations.
Patent Information
- Application Number
- FR2023003050
- Authority / Receiving Office
- FR · FR
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-29
- Publication Date
- 2024-10-04
AI Technical Summary
Integrated electro-optical devices manufactured by annealed proton exchange (APE) exhibit unstable electro-optical responses due to temporal drifts and hysteresis under varying environmental conditions such as temperature and vacuum, particularly at low and very low frequencies.
A manufacturing method that includes machining a residue of the layer modified by proton exchange after thermal annealing to form a machined zone between the electrodes, which removes or reduces the degraded crystal structure caused by proton exchange, thereby stabilizing the electro-optical response.
The method significantly reduces temporal and frequency drifts, ensuring a stable electro-optical response independent of environmental variations, with improved performance at low and very low frequencies.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Title of the invention: Method for manufacturing an integrated electro-optical device and electro-optical device thus obtained Technical field of the invention
[0001] The present invention relates to the technical field of electro-optical devices and their manufacturing method.
[0002] It relates in particular to a method of manufacturing an electro-optical device integrated on an electro-optical substrate.
[0003] The invention also relates to an integrated electro-optical device having a stabilized electro-optical response as a function of time and modulation frequency. The invention finds applications in an optical phase modulator, an optical intensity modulator of the Mach-Zehnder interferometer type. The invention also finds applications in an active directional coupler. State of the art
[0004] In the above field, it is known to manufacture and use an electro-optical device integrated on a planar electro-optical substrate, the electro-optical device comprising an optical waveguide and an electrode system adapted to modulate a light beam propagating in the optical waveguide by applying an electrical voltage to the terminals of the electrode system.
[0005] Different materials can be used for the fabrication of integrated electro-optical devices. Lithium niobate (LiNbO3), lithium tantalate (LiTaO3) and lithium antimonate (LiSbO3) are particularly interesting materials because they exhibit an electro-optical Pockels effect. By placing electrodes close to the integrated waveguide, it is possible to modulate the index of the optical waveguide and thus modulate the phase of an optical signal propagating in the waveguide. In an integrated electro-optical device where the electrodes are separated by about ten microns, the application of a voltage of only a few volts is sufficient to generate an electric field and induce the desired phase modulation.
[0006] Different technologies for manufacturing integrated electro-optical devices on lithium niobate substrates have been developed, such as titanium (Ti) diffusion and annealed proton exchange (APE).
[0007] The proton exchange technology comprises a first step in which a birefringent crystal of lithium niobate is placed in a benzoic acid bath heated to a temperature below 250°C (below the boiling point of benzoic acid), to replace lithium ions (Li+) with protons (or H+ ions) from the surface exposed to the acid bath. This proton exchange operation (PE for Proton Exchange in English) leads to the formation of a layer 3 modified by proton exchange extending over the zone exposed to the acid from the surface 2 of the substrate to a small depth P3 in the substrate 1 (see [Fig.l]). Layer 3 has a difference in optical index of refraction of the order of 0.1 with the substrate. The refractive index profile of layer 3 is step-shaped in the X and Z directions. Layer 3 is limited laterally to a width W3 is generally between 1 pm and 10 pm. The depth P3 is less than or equal to 500 nm. Indeed, the temperature being low, the proton exchange phenomenon cannot diffuse very far into the substrate.
[0008] This first step is followed by a thermal annealing step at a temperature below 500°C. During the annealing step, the temperature being higher, the protons, or hydrogen ions, of the layer 3 modified by proton exchange can exchange with the lithium ions in a diffusion zone 4 around the initial location of the layer 3. The annealing makes it possible to create a refractive index gradient in the diffusion zone 4 under the surface of the crystal and thus to form an optical waveguide 5. The diffusion zone 4 extends into the substrate to a great depth P4, which can reach several microns, depending on the temperature and the duration of the annealing (see [Fig.2]). The diffusion zone 4 has a width W4 greater than the width W3 of the layer 3 modified by proton exchange. The width W4 is generally between 1 pm and 10 pm.The width W4 and respectively the depth P4 are measured here at the maximum of the refractive index gradient divided by the number e in the base of the natural logarithms (or exponential (-1)), along the direction Z and respectively X.
[0009] After the thermal annealing step, the manufacturing of the integrated electro-optical device comprises a step of depositing a pair of electrodes. This pair of electrodes makes it possible to apply an electric field in the optical waveguide 5 so as to control the electro-optical device, for example for the electro-optical modulation of an optical wave propagating in the optical waveguide 5.
[0010] Proton exchange on a birefringent lithium niobate crystal has the effect of both increasing the extraordinary index of the crystal, which creates guidance for a wave polarized along the extraordinary axis of the crystal, and reducing the ordinary index of the crystal, so that a wave polarized along the ordinary axis is not guided.
[0011] In electro-optical devices comprising an optical waveguide formed by proton exchange on lithium niobate, the usual configuration is an X-section, the X axis of the uniaxial birefringent lithium niobate crystal being perpendicular to the surface of the substrate, while the Y and Z axes of the crystal are parallel to the surface. The propagation direction of the waveguide is parallel to the Y axis and the TE mode (transverse electric, i.e. electric field parallel to the surface of the substrate) is parallel to the Z direction. In this case, the optical waveguide by proton exchange only guides the TE polarization state, the cross-polarization state TM (transverse magnetic, i.e. magnetic field parallel to the surface of the substrate and therefore electric field perpendicular to the surface of the substrate) propagating freely in the substrate. The proton exchange technique on lithium niobate thus makes it possible to manufacture a polarizing waveguide on an integrated optical circuit. Electrodes arranged on both sides of the optical waveguide 5 make it possible to apply an electric field parallel to the Z axis in the optical waveguide 5.
[0012] There are also electro-optical devices comprising an optical waveguide formed by proton exchange on lithium niobate (or lithium tantalate or lithium antimoniate), along a Z cut, the Z axis of the uniaxial birefringent lithium niobate crystal being perpendicular to the surface of the substrate, while the X and Y axes of the crystal are parallel to the surface. The propagation direction of the waveguide is parallel to the Y axis, and the TE mode (transverse electric, i.e. electric field parallel to the surface of the substrate) is parallel to the Z direction. One electrode covers the waveguide while the other electrode is arranged next to the waveguide or on an opposite face of the substrate. These electrodes make it possible to apply an electric field parallel to the Z axis in the optical waveguide 5.Moreover, in this case, the metal electrode covering the waveguide absorbs the TM mode of electromagnetic radiation propagating in the optical waveguide 5 while it transmits the TE mode parallel to the Z axis.
[0013] However, the behavior of integrated electro-optical devices manufactured in APE is degraded under particular conditions of use such as vacuum and / or temperature. For example, an electro-optical phase modulator manufactured by APE has a transfer function defined by the ratio between a voltage Vm applied to the terminals of the modulator electrodes and the optical phase shift <bm induit, avec Vm / <bm = Vit Ik où le signal Vir est aussi appelé tension demi-onde (Vit). Or ce signal Vir fluctue avec l’environnement, notamment avec la température et / ou le vide.
[0014] Furthermore, the low frequency (between 100 Hz and 1 kHz) and very low frequency (between 0.0 Hz and 100 Hz) response of an electro-optical device manufactured in APE is assimilated in certain applications to a slow drift of the operating points or to a measurable hysteresis in the transfer function of the electro-optical device.
[0015] Various solutions to the time drift of an integrated optical phase modulator have already been proposed. For example, US patent 8,463,081 proposes to combine in series a portion of optical waveguide formed by titanium diffusion and another portion of optical waveguide formed by APE, the two portions having time drifts of opposite sign. However, the compensation is not perfect but depends on the temperature and the frequency of the signal applied at low and very low frequency.
[0016] One of the aims of the invention is to propose a means for stabilizing the electro-optical response of an integrated electro-optical device, as a function of the time and / or the frequency of the modulation signal applied to the electrodes of such an integrated electro-optical device. It is desirable to reduce the slow drift of the operating points at low frequency and very low frequency. It is also desirable to eliminate or limit the hysteresis of the transfer function of such an integrated electro-optical device. In particular, in an electro-optical phase modulator based on an integrated electro-optical device, it is desirable to reduce the fluctuations of the signal Vit with the environment, in particular with the temperature and / or the vacuum.
[0017] Another aim of the invention is to propose a simple manufacturing method for such an integrated electro-optical device having an instantaneous electro-optical response, stable over time and / or as a function of the electrical modulation frequency, and independent of ambient variations in temperature and / or pressure. Presentation of the invention
[0018] In this context, the present invention provides a method of manufacturing an electro-optical device.
[0019] More particularly, the invention proposes a method for manufacturing an electro-optical device comprising the following steps: manufacturing an optical waveguide in an electro-optical substrate by proton exchange annealing comprising the steps of: a) exposing an area of a surface of the substrate to a proton source so as to create in the substrate a layer modified by proton exchange, said layer extending over said area from the surface of the substrate to a small depth (P3) in the substrate, and b) thermally annealing the substrate so as to diffuse hydrogen ions from said layer into a diffusion zone extending in the substrate around said layer to a large depth (P4) so as to create an optical waveguide in the diffusion zone; and depositing a pair of electrodes, the optical waveguide extending longitudinally between said pair of electrodes.
[0020] According to the invention, the method comprises, after the thermal annealing step, a step of machining a residue of said layer to form a machined zone located at least partly between said pair of electrodes.
[0021] Thus, the machining step makes it possible to at least partially remove a residue from the layer modified by proton exchange, the electro-optical properties of which are damaged by the proton exchange. The removal of this residue makes it possible to reduce or even eliminate time and / or frequency drifts of the electro-optical device, when an electrical voltage is applied between the terminals of the electrodes.
[0022] Other non-limiting and advantageous characteristics of the system according to the invention, taken individually or in all technically possible combinations, are the following: - the machined area extends into the substrate to a depth greater than or equal to the shallow depth; - the machined area extends over at least a portion of a deposition surface of said pair of electrodes; - the machined area extends over an entire width of the substrate taken transversely to a longitudinal direction of the optical waveguide; - the machined area is limited to an area of the waveguide between said pair of electrodes; - the machining step is adapted to form several machined zones arranged in series along a longitudinal direction of the optical waveguide, said several machined zones being located at least partly between said pair of electrodes; - the machined area extends over the entire surface of the substrate; - the machining step is carried out by wet etching, plasma etching, laser etching, lapping or mechanical polishing; - the method comprises a step of depositing a dielectric layer, the dielectric layer being arranged on the machined area on the surface of the substrate and / or between the substrate and at least one electrode of the pair of electrodes.
[0023] The invention also relates to an electro-optical device obtained according to any one of the embodiments described.
[0024] In particular, the invention relates to such an electro-optical device, used in an electro-optical phase modulator, an optical intensity modulator, a Mach-Zehnder interferometer and / or an active directional coupler with evanescent waves.
[0025] Of course, the various features, variants and embodiments of the invention may be combined with each other in various combinations provided that they are not incompatible or mutually exclusive. Brief description of the drawings
[0026] Furthermore, various other characteristics of the invention emerge from the appended description given with reference to the drawings which illustrate non-limiting forms of embodiment of the invention and where:
[0027] [Fig. 1] is a cross-sectional view of an electro-optical substrate within which a proton exchange modified layer is formed before annealing;
[0028] [Fig.2] is a cross-sectional view of the electro-optical substrate after annealing for form a diffusion zone;
[0029] [Fig.3] is a cross-sectional view of an integrated electro-optical device comprising an optical waveguide formed by APE and electrodes;
[0030] [Fig.4] is a graph schematically illustrating the response of an electro-optical modulator manufactured by APE as a function of frequency, according to the prior art (in solid lines) and according to the present disclosure (in dashed lines);
[0031] [Fig.5] is a graph schematically illustrating the half-wave voltage, characteristic of the transfer function of an electro-optical modulator manufactured by APE as a function of the frequency, according to the prior art (in solid lines) and according to the present disclosure (in dashed lines);
[0032] [Fig.6] is a graph schematically illustrating, on the left, the voltage applied to the terminals of an electro-optical modulator manufactured by APE as a function of time, and on the right, an example of phase shift produced respectively according to the prior art (in solid lines) and according to the present disclosure (in dashed lines);
[0033] [Fig.7] is a top view of an integrated electro-optical device comprising an optical waveguide formed by APE, electrodes and a machined area according to a first example;
[0034] [Fig.8] is a top view of an integrated electro-optical device comprising an optical waveguide formed by APE, electrodes and a machined area according to a second example;
[0035] [Fig.9] is a cross-sectional view of an integrated electro-optical device according to the first or second example;
[0036] [Fig. 10] is a top view of an integrated electro-optical device comprising an optical waveguide formed by APE, electrodes and a machined area according to a third example;
[0037] [Fig. 11] is a top view of an integrated electro-optical device comprising an optical waveguide formed by APE, electrodes and a machined area according to a fourth example;
[0038] [Fig. 12] is a top view of an integrated electro-optical device comprising an optical waveguide formed by APE, electrodes and a machined area according to a fifth example;
[0039] [Fig. 13] is a top view of an integrated electro-optical device comprising an optical waveguide formed by APE, electrodes and a machined area according to a sixth example;
[0040] [Fig. 14] is a cross-sectional view of an integrated electro-optical device according to any one of the third to sixth examples;
[0041] [Fig. 15] is a cross-sectional view of an integrated electro-optical device according to a variation of any one of the third to sixth examples;
[0042] [Fig. 16] is a cross-sectional view of an alternative integrated electro-optical device comprising an optical waveguide formed by APE and electrodes;
[0043] [Fig. 17] is a cross-sectional view of another alternative integrated electro-optical device comprising an APE-formed optical waveguide and electrodes.
[0044] It should be noted that in these figures the structural and / or functional elements common to the different variants may have the same references. Detailed description
[0045] [Fig. 3] schematically represents an integrated electro-optical device in transverse section view, that is to say perpendicular to the surface 2 of the electro-optical substrate 1 and transversely to a longitudinal direction of the optical waveguide 5. The integrated electro-optical device comprises an optical waveguide 5 formed by APE and electrodes 6, 7.
[0046] The electro-optical substrate 1 is for example a lithium niobate (LiNbO3) substrate. Alternatively, the substrate 1 is a lithium tantalate (LiTaO3) or lithium antimonate (LiSbO3) substrate. By way of non-limiting example, the substrate is in an X-cut configuration, the X axis of the crystal being perpendicular to the surface of the substrate, while the Y and Z axes of the crystal are parallel to the surface, the Y axis being parallel to the propagation direction of the optical waveguide. Alternatively, the substrate is in a Z-cut configuration, the Z axis of the crystal being perpendicular to the surface of the substrate, while the X and Y axes of the crystal are parallel to the surface, the Y axis being parallel to the propagation direction of the optical waveguide (see Figures 16-17).
[0047] As described in connection with Figures 1 and 2, a layer 3 modified by proton exchange is formed in the substrate 1. During thermal annealing, a diffusion zone 4 extends in the substrate 1 around the initial location of the layer 3. The diffusion zone 4 has a refractive index gradient which makes it possible to form an optical waveguide 5. The optical waveguide 5 is limited by the index gradient and by the surface 2 of the substrate 1. The width W4 of the optical waveguide 5 is generally between 1 micrometer (pm) and 10 micrometers (pm). The optical waveguide 5 extends for example longitudinally in the direction Y. In a known manner, the optical waveguide 5 may be rectilinear or comprise a curvature and / or a junction with several branches, for example a Y junction with two branches.The optical waveguide 5 is adapted to guide a single-mode optical wave so that it propagates along the longitudinal direction of the optical waveguide 5, for example here along the Y axis. In [Fig. 3] the spatial extent of the fundamental mode 15 of an optical wave propagating in the optical waveguide 5 is schematically represented.
[0048] The electro-optical device illustrated in [Fig.3] is in an X-cut and Y-propagation configuration. The integrated electro-optical device comprises a system of electrodes comprising at least one pair of conductive electrodes 6, 7. The electrode 6 is deposited on one side of the optical waveguide 5 and the electrode 7 is deposited on an opposite side of the optical waveguide 5. The pair of electrodes 6, 7 is generally deposited on the surface 2 of the substrate 1.
[0049] Alternatively, a dielectric layer 24, for example of silicon dioxide (SiO2) or silicon nitride (SiN), is arranged between the surface 2 of the substrate 1 and each electrode 6, 7. The thickness of the dielectric layer 24 is for example between 100nm and 2pm. The dielectric layer 24 serves to protect the surface of the optical waveguide 5. The dielectric layer 24 also makes it possible to isolate the optical surface from the metal electrodes, for example if the optical waveguide is very close or risks being partly in contact with an electrode, in particular for very wideband electrodes (operating in the range from 0 to several tens of GHz).
[0050] For the sake of clarity, a rectilinear optical waveguide 5 and a pair of rectilinear electrodes 6, 7 are considered. The optical waveguide 5 extends longitudinally between said pair of electrodes 6, 7. The distance between the two electrodes 6, 7 is generally greater than or equal to the width W4 of the optical waveguide 5. For example, the distance D between the two electrodes 6, 7 is between 1 micrometer (pm) and 10 pm. The length L6 of the electrodes in the Y direction is generally between a few millimeters and up to several centimeters. The electrodes have the same width or may have a different width. The optical waveguide 5 is centered or not between the two electrodes 6, 7. Optionally, another electrode is arranged on the rear face 9 of the substrate 1, that is to say the face opposite the front face 2 where the optical waveguide is formed by APE.
[0051] In connection with Figure 3, we will now explain the electro-optical operation of the integrated electro-optical device. An electrical voltage is applied across the pair of electrodes 6, 7. For example, a positive voltage is applied to the electrode 6 and a negative voltage to the electrode 7. Alternatively, one of the two electrodes is grounded. Lines 14 of electric field E appear between the pair of electrodes 6, 7. In particular, lines 14 of the electric field E oriented parallel to the Z axis pass through the optical waveguide 5. In a known manner, the modulation of the electrical voltage applied between the electrodes 6, 7 makes it possible to modulate the optical phase shift of an optical wave propagating in the optical waveguide 5.
[0052] However, the electro-optical operation of the electro-optical device may exhibit certain deviations, illustrated in Figures 4 to 6.
[0053] In [Fig. 4], a response curve 16 of an electro-optical phase modulator manufactured by APE as a function of the frequency according to the prior art is shown schematically in solid lines. More precisely, curve 16 represents the ratio between the optical phase shift A <1> induced in the optical wave propagating in the guide optical wave 5 and the applied voltage V as a function of the modulation frequency f. At high frequency, for example above 1 kHz, the ratio ± A
[0054] In [Fig. 5], a half-wave voltage curve 18 (or signal Vir) of an electro-optical phase or intensity modulator manufactured by APE is shown schematically in solid lines as a function of frequency, according to the prior art. More precisely, curve 18 represents the signal Vir as a function of the modulation frequency f of the voltage applied to the terminals of the electrodes 6, 7. At high frequency, the signal Vit is constant. On the other hand, at low frequency and very low frequency, the signal Vit increases sharply. This curve 18 also indicates that the response of the electro-optical phase or intensity modulator manufactured by APE according to the prior art depends unfavorably on the modulation frequency f.
[0055] In [Fig.6], a curve 20 of voltage V applied between the electrodes 6,7 as a function of time is shown on the left. The voltage V increases gradually in stages and then also decreases progressively in stages. In [Fig.6], a curve 21 of the optical phase shift A is shown on the right <1> induced in the optical wave propagating in the optical waveguide 5 as a function of time, i.e. as a function of the applied voltage values V. On the curve 21 of the induced optical phase shift, we observe for example a negative exponential step when the voltage increases and a positive exponential step when the voltage decreases. In all cases, with each rising or falling voltage step, a stable value of induced optical phase shift is only reached after a time which can range from one millisecond to several hours and even beyond.
[0056] It follows from the present disclosure that these slow drifts of the operating point of an electro-optical modulator as a function of time and / or modulation frequency can be greatly reduced by machining a portion of the substrate in an area corresponding to a residue of the proton exchange-modified layer 3 located between the pair of electrodes 6, 7.
[0057] Without being bound by theory, a physical interpretation is that during the proton exchange step, a portion of the lithium ions in substrate 1, for example lithium niobate, are substituted by protons or H+ ions to form proton exchange-modified layer 3. In cross-section, along the X axis, proton exchange-modified layer 3 has a step-like refractive index profile down to depth P3. The substitution rate in layer 3 can reach 60% or more of H+ ions. As a result, the crystal structure of proton exchange-modified layer 3 is degraded compared to the structure crystalline layer of substrate 1 around the initial location of layer 3 modified by proton exchange. In the area of layer 3, the high ion exchange rate locally induces a loss of the electro-optical properties of lithium niobate, necessary for any electro-optical modulation. During the thermal annealing step below 500°C, the diffusion zone 4, which forms the optical waveguide 5, extends into the substrate 1. During thermal annealing, H+ ions from layer 3 are exchanged with lithium ions at greater depth, for example up to a depth of several microns depending on the temperature and duration of the annealing. Annealing makes it possible to obtain a gradient of optical refractive index in the substrate and thus to form the optical waveguide 5. In transverse section, along the X axis, the diffusion zone 4 generally has an optical refractive index profile comparable to a semi-Gaussian.The depth P4 corresponds to the maximum divided by the number e in the base of the natural logarithms (or exponential (-1)) of this semi-Gaussian profile along the X axis. Similarly, the width W4 of the optical waveguide 5 corresponds to the maximum divided by the number e of this profile along the Z axis. During thermal annealing, the ion substitution rate in the diffusion zone is lower, generally less than 15%. This low lithium ion substitution rate allows the electro-optical properties of the crystal to be preserved. Following thermal annealing, the lithium ion substitution rate in the zone corresponding to the location of layer 3 modified by proton exchange has decreased. Nevertheless, the crystal structure at the location of layer 3 modified by proton exchange remains degraded.The electro-optical device conventionally manufactured by APE has different crystalline properties in the substrate 1, in the diffusion zone 4 and in the zone corresponding to the layer 3 modified by proton exchange.
[0058] As illustrated in [Fig. 3], the electric field lines 14 pass through not only the diffusion zone 4 but also a zone under the surface of the substrate which corresponds to a residue of the layer 3 modified by proton exchange. The electro-optical response of the electro-optical device depends not only on the electro-optical properties of the diffusion zone 4 but also on the zone corresponding to the location of the layer 3 modified by proton exchange. The crystalline degradation of the zone of the layer 3 leads to an increase in its electrical conductivity when the electro-optical device thus manufactured is placed at a hot temperature, for example about 50°C, this effect being accelerated and amplified when the temperature increases and when the electro-optical device is placed in a hot vacuum.
[0059] The present disclosure provides an additional step in the method of manufacturing an electro-optical device by APE, this additional step, after the thermal annealing step, comprising the machining of at least a part of the residue of the layer 3 in an area located or intended to be placed between the pair of electrodes 6, 7, so as to reduce or eliminate the residue of layer 3 in the machined area. The depth P of the machined area is of the order of the shallow depth P3 of layer 3 modified by proton exchange. In practice, the depth P may be less than, equal to or slightly greater than the shallow depth P3. For example, the depth P of the machined area is such that: 0.02*P3 < P < l.10*P3, and preferably 0.50*P3 < P < l.10*P3 and even more preferably 0.90*P3 < P < l.10*P3. For example, for a depth P3 of 500 nm, the depth P of the machined area is approximately 500 nm ± 50 nm. The machining step is carried out on a small depth P to preserve the majority of the diffusion zone 4.
[0060] This step of machining the residue of said layer 3 can be carried out by different techniques: for example mechanical machining of the lapping type and / or polishing of the surface of the substrate or of a part of the surface of the substrate, surface ablation by laser pulses, wet etching or dry etching by plasma.
[0061] This step of machining the residue of said layer 3 can be carried out on a plate integrating several electro-optical devices manufactured in batches or on an individual chip obtained for example after cutting such a plate, each chip comprising a single electro-optical device. The step of machining the residue of layer 3 can be carried out before or after the deposition of the electrodes 6, 7 on a complete plate or on an individual chip. The step of machining the residue of said layer 3 can be carried out before or after transferring a chip onto a base or into an electronic box.
[0062] Figures 7 to 15 illustrate different embodiments of an electro-optical device according to the present disclosure. Figures 7 to 15 show a machined area 10 or several machined areas 10, 11, 12 on each electro-optical device.
[0063] In [Fig.7], the electro-optical device 50 in top view comprises a guide optical waveguide 5 formed by proton exchange annealed in an electro-optical substrate 1, a pair of electrodes 6, 7 arranged parallel to the two longitudinal sides of the optical waveguide 5. The electro-optical device comprises a machined zone 10 which extends here between the two electrodes 6, 7 over a width W and over a length L. The width W of the machined zone 10 is here less than or equal to the distance D between the two electrodes 6, 7. The length L of the machined zone 10 is here equal to the length L6 of the electrodes 6, 7. Advantageously, the width W is greater than or equal to the initial width W3 of the layer 3 modified by proton exchange. Machining the residue of said layer 3 over this width W and over the entire length L6 of the electrodes 6, 7 makes it possible to completely eliminate the frequency and time drifts of the electro-optical device, as detailed below.In this configuration, the machining of the machined area 10 can be carried out before or after deposition of the electrodes. However, when this machining is carried out after the electrodes have been deposited, precautions are required to avoid damaging the electrodes 6, 7.
[0064] [Fig. 8] shows a second example of an electro-optical device, according to a variant of [Fig. 7]. The machined zone 10 here has a length L less than the length L6 of the electrodes 6, 7, for example such that 0.5*L6 < L < L6. The width W of the machined zone 10 is here less than or equal to the distance D between the two electrodes 6, 7. This example illustrates certain configurations where it is more difficult to machine the zone 10 over the entire length L6 of the electrodes. In this example, the machining of the machined zone 10 can be carried out before or after deposition of the electrodes. In certain applications, the machining of the zone 10 over a portion of the length of the electrodes is sufficient to limit the frequency and time drifts of the electro-optical device. In this case, the time or frequency drift phenomena are reduced proportionally to the machined zone.
[0065] [Fig. 9] shows a cross-sectional view of the electro-optical device 50 of [Fig. 7] or 8. The machined area 10 corresponds here to a hollow area in the substrate, below the initial surface 2 of the substrate. The machined area 10 has a depth P. For example, the depth P is between 10 nm and 550 nm for a depth P3 of 500 nm. The depth P of the machined area is less than, equal to or slightly greater than the small depth P3 of the layer 3 modified by proton exchange. In all cases, the depth P of the machined area is less than the initial depth P4 of the diffusion area. Consequently, below the machined area between the electrodes 6, 7, the diffusion area 5 has a depth equal to P4-P.
[0066] The machined area 10 of the electro-optical device 50 of [Fig.7], 8 or 9 can be machined before or after the deposition of the electrodes 6, 7.
[0067] [Fig. 10] shows a third example of an electro-optical device 50. The machined area 10 here has a length L less than the length L6 of the electrodes 6, 7. The width W of the machined area 10 is here greater than the total width T of the electrodes 6, 7. The width W of the machined area 10 is for example equal to the width of the substrate 1, which facilitates the use of mechanical machining. The machined area is then shaped before the electrodes are deposited.
[0068] [Fig. 11] shows a fourth example of electro-optical device 50. The machined zone 10 here has a length L equal to the length L6 of the electrodes 6, 7. The width W of the machined zone 10 is here greater than the total width T of the electrodes 6, 7. The width W of the machined zone 10 is for example equal to the width of the substrate 1 which facilitates the use of mechanical machining.
[0069] [Fig. 12] shows a fifth example of electro-optical device 50. The machined zone 10 here has a length L greater than the length L6 of the electrodes 6, 7. The width W of the machined zone 10 is here greater than the total width of the electrodes 6, 7. The machined area 10 extends here, for example, over the entire surface of the substrate 1. The machined area 10 can be shaped by etching, lapping and / or polishing the surface so that the electro-optical device has a flat surface outside the electrodes. Machining the entire surface ensures the removal of all residual parts of the proton exchange-modified layer 3. In addition, machining the entire surface 2 is easy to implement because it is full-plate machining without masking.
[0070] Alternatively, the electro-optical device 50 illustrated in any one of FIGS. 10 to 12 comprises one or more disjointed machined areas located outside the electrodes 6, 7. For example, in [Fig. 10] or 11, the device may also be shaped by forming one machined area located between the two electrodes 6, 7 and two machined areas outside the electrodes 6, 7. In this case, the disjointed machined area or areas may be shaped before or after the electrodes 6, 7 are deposited.
[0071] [Fig. 13] shows a sixth example of an electro-optical device 50 comprising several machined zones 10, 11, 12 arranged in series along the longitudinal direction Y of the optical waveguide 5. More precisely, a machined zone 10 extends over a length L less than the length L6 of the electrodes 6, 7 and over a width W greater than the total width of the electrodes 6, 7, for example over the width of the substrate 1. Another machined zone 11 extends over a length L1 less than the length L6 of the electrodes 6, 7 and over a width W1 less than or equal to the distance D between the two electrodes 6, 7. Yet another machined zone 12 extends longitudinally over a length L2 partly between the electrodes 6, 7 and partly beyond the electrodes 6, 7. The machined zone 12 extends transversely over a width W2 greater than the distance D between the two electrodes 6, 7 and less than or equal to the total width T of the electrodes 6, 7.The machined areas 10, 11, 12 can be machined in one go, using the same machining technique, or can be manufactured sequentially using different machining techniques mentioned above. For example, the machined area 11 can be shaped after the electrodes have been deposited, in the case where time or frequency drifts remain, to further limit these drifts.
[0072] [Fig. 14] shows a cross-sectional view of an electro-optical device 50 such as for example illustrated in one of FIGS. 10 to 13. Advantageously, the machined area 10, 11 and / or 12 is shaped before the deposition of the electrodes 6, 7. The machined area 10, 11 and / or 12 is in this example machined over a width W greater than the total width T of the electrodes, and preferably over the entire width of the substrate 1. For example, the machined area(s) are here formed by removing a layer of thickness P over the entire width of the substrate after the thermal annealing step and before the electrode deposition step. In the cross-section, it can be seen that the machining of the surface has removed a layer of thickness P from the optical waveguide 5, where the residue of the layer 3 modified by proton exchange. Here too, below the machined area between electrodes 6,7, diffusion zone 5 has a depth equal to P4-P.
[0073] [Fig. 15] shows a cross-sectional view of an exemplary electro device optical 50 as illustrated in one of figures 10 to 13. Here, the machined area 10, 11 and / or 12 is shaped before or after the deposition of the electrodes 6, 7. The machined area 10, 11 and / or 12 is in this example shaped over a width W less than or equal to the distance D between the electrodes. Optionally, lateral areas are also machined outside the electrodes, between the total width T and the width of the substrate. For example, the machined area(s) are here formed by removing a central strip of thickness P over the entire length or part of the length of the electrodes and possibly two lateral strips after the thermal annealing step and before or after the electrode deposition step. In the cross-section, it is observed that the machining of the surface has removed a layer of thickness P from the optical waveguide 5, where the residue of layer 3 modified by proton exchange was located.After deposition of the electrodes 6, 7, the electro-optical device has a hollow between the electrodes 6, 7 in the machined zone 10. In this example, the electrodes 6, 7 are located at a height greater than P relative to the optical waveguide.
[0074] Optionally, after manufacturing the machined area, the method comprises an additional step of depositing a dielectric layer 24, for example silicon dioxide (SiO2) or silicon nitride (SiN). The dielectric layer 24 is arranged on the surface of the substrate after machining, between each electrode 6, 7 and the substrate 1. Alternatively, the dielectric layer 24 extends not only under the electrodes but over the entire surface of the substrate.
[0075] Alternatively or additionally, the method comprises another step of depositing a dielectric layer 24, for example silicon dioxide (SiO2) or silicon nitride (SiN). The two electrodes 6, 7 are deposited on this dielectric layer 24. The dielectric layer 24 makes it possible to protect the surface of the optical waveguide 5. The dielectric layer 24 also makes it possible to isolate the optical wave circulating in the optical waveguide from the metal electrodes.
[0076] The presence of a residue of the layer corresponding to layer 3 modified by proton exchange after thermal annealing can be detected and measured by different characterization techniques such as: optical or contact profilometry, Raman spectrometry, secondary ion mass spectroscopy (SIMS), X-ray diffraction (X-ray rocking curves), transmission electron microscopy (TEM), Fourier transform spectroscopy (FTIR) or UV ellipsometry. These techniques make it possible to evaluate the machining depth P to be carried out. The machining depth P is generally less than at 500 nm. The control of the machining depth P can be carried out by checking the machined depth during manufacturing or possibly by measuring the surface conductivity before / after etching. In addition, the electro-optical operation of the device is controlled after manufacturing.
[0077] An integrated electro-optical device 50 is thus obtained comprising at least one machined zone 10, 11, 12 over a small depth P, the machined zone 10, 11, 12 being located at least in part between the pair of electrodes 6, 7. The machined zone is adapted to remove at least in part a residue of the layer 3 modified by proton exchange in a zone located at least in part between said pair of electrodes 6, 7. In certain embodiments, the machined zone remains empty and can form a hollow relative to the surface of the substrate. In other embodiments, the machined zone is at least partially filled by a dielectric layer for example. Finally, in other embodiments, the machined zone extends over the entire surface of the substrate which then has the same surface relief as an unmachined electro-optical device.
[0078] The method also applies to an electro-optical device comprising an optical waveguide formed by proton exchange on lithium niobate (or lithium tantalate or lithium antimonate), along a Z cut, as illustrated in Figures 16-17. In this case, one electrode 6 is in contact with the optical waveguide 5. The other electrode 7 is arranged next to the optical waveguide 5 on the same face as the electrode 6 (see [Fig. 16]) or on the opposite face 9 of the substrate 1 (see [Fig. 17]). In this Z cut configuration, an electric potential difference applied between the two electrodes generates an electric field E oriented along the Z axis in the optical waveguide 5.According to the present disclosure, in cutting configuration Z, in a manner analogous to the cutting configuration X, after the thermal annealing step, at least a portion of the residue of layer 3 is machined in an area intended to be placed in contact with the electrode 6, and between the pair of electrodes 6, 7, so as to reduce or eliminate the residue of layer 3 in the machined area. The depth P of the machined area is of the order of the shallow depth P3 of the layer 3 modified by proton exchange. In practice, the depth P may be less than, equal to or slightly greater than the shallow depth P3. For example, the depth P of the machined area is such that: 0.02*P3 < P < 1.10*P3, and preferably 0.50*P3 < P < 1.10*P3 and even more preferably 0.90*P3 < P < 1.10*P3. For example, for a P3 depth of 500 nm, the P depth of the machined area is approximately 500 nm±50 nm.The machining step is carried out on a small depth P to preserve the majority of the diffusion zone 4. .
[0079] In the Z cutting configuration, the machining step is necessarily carried out before the step of depositing the electrode 6. The machining step can be carried out over the entire surface 2 of the substrate, after the thermal annealing step, so as to obtain a flat surface before the deposition of the electrode 6, as for example illustrated in [Fig. 17]. Alternatively, as illustrated in FIG. 16, the machining is applied to a surface limited in width and / or length of the face 2 of the substrate, above the optical waveguide 5. The partial or extended machining over the entire surface can be applied whether the electrode 7 is located on the same face 2 as the electrode 6 or on the opposite face 9.
[0080] An electro-optical device is thus obtained in X-cut or Z-cut configuration, in which at least part of the residue of the layer 3 modified by proton exchange is removed in an area located or intended to be placed between the pair of electrodes 6, 7.
[0081] Non-intuitively, this surface machining, which can be limited locally to a small portion of the substrate between the pair of electrodes, makes it possible to obtain a great improvement in the response of the electro-optical device, whether as a function of time, temperature, pressure (for example in a vacuum) or at low and very low modulation frequency.
[0082] In Figures 4 to 6, the technical effects obtained on an integrated electro-optical device obtained by proton exchange annealed according to the method of the present disclosure with a machining step are schematically represented.
[0083] In [Fig. 4], a curve 17 of response as a function of the frequency of an electro-optical phase modulator manufactured by APE and machined according to the present disclosure is schematically represented in dashed lines. It is observed that the ratio of the optical phase shift A <1> induced on the applied voltage V remains constant at low frequency and very low frequency. The ratio ± ACb / V is independent of the modulation frequency f, particularly at low frequency and very low frequency.
[0084] In [Fig.5], a half-wave voltage curve 19 (or Vir signal) of an electro-optical phase modulator manufactured by APE and machined according to the present disclosure is schematically represented in dashed lines. It is observed that the Vir signal remains constant at low frequency and very low frequency. Curve 19 of the Vir signal is independent of the modulation frequency f, in particular at low frequency and very low frequency.
[0085] In [Fig.6], a curve 22 of the optical phase shift A is shown on the right <1> induced in the optical wave propagating in the optical waveguide 5 as a function of time, i.e. as a function of the applied voltage values V following curve 20. On curve 22 of the induced optical phase shift, instantaneous steps are observed when the voltage increases or when the voltage decreases. The desired optical phase shift value is thus obtained instantly at each change in the voltage value applied to the electrodes 6, 7.
[0086] A possible interpretation of these improvements in the electro-optical response of the electro-optical device with machined area according to the present disclosure is as follows. The electrical conductivity of the degraded crystal structure at the location of the proton exchange-modified layer 3 may vary depending on the temperature or in a hot vacuum for example. As illustrated in [Fig.3], the fundamental mode 15 of the wave guided by the optical waveguide 5 extends to the surface of the substrate and partly covers the location where the residue of the proton exchange-modified layer 3 is located. When a voltage is applied between the electrodes 6, 7, the electric field lines 14 pass through the different areas which have different electrical conductivities: the substrate 1, the diffusion area 4 and the area where a residue of the proton exchange-modified layer 3 is located. The physical properties of these areas are different.In particular, their conductivity varies differently depending on the environmental conditions, in particular temperature and pressure. The increase in the conductivity of the residue of the layer 3 modified by proton exchange is different from that of the optical waveguide 5 and the substrate. This difference in variation of conductivity modifies the electro-optical overlap and thus the response depending on the modulation frequency applied to the electrodes. Machining the residue on a determined and shallow area of the substrate 1 between the electrodes 6, 7 makes it possible to at least partially remove the residue of the layer 3. This superficial machining, over a depth P in the proportions indicated in detail above, does not disturb the guidance of the single-mode wave in the optical waveguide 5.
[0087] The electro-optical device thus obtained advantageously finds applications in an electro-optical phase modulator, an optical intensity modulator and / or a Mach-Zehnder interferometer. The electro-optical device thus obtained also finds applications in an active directional coupler with evanescent waves, such as for example a 2x2 active coupler on a lithium niobate substrate comprising electrodes arranged in the evanescent wave coupling zone.
Claims
Claims
1. A method of manufacturing an electro-optical device (50) comprising the following steps: manufacturing an optical waveguide (5) in an electro-optical substrate (1) by proton exchange annealing comprising the steps of: a) exposing an area of a surface (2) of the substrate (1) to a proton source so as to create in the substrate a layer (3) modified by proton exchange, said layer (3) extending over said area from the surface (2) of the substrate to a shallow depth (P3) in the substrate, and b) thermally annealing the substrate so as to diffuse hydrogen ions from said layer (3) into a diffusion zone (4) extending in the substrate around said layer (3) to a deep depth (P4) so as to create an optical waveguide (5) in the diffusion zone (4); depositing a pair of electrodes (6, 7), the optical waveguide (5) extending longitudinally between said pair of electrodes (6, 7);characterized in that the method comprises, after the thermal annealing step, a step of machining a residue of said layer (3) to form a machined zone (10, 11, 12) located at least partly between said pair of electrodes (6, 7).;
2. A method according to claim 1 wherein the machined area (10, 11, 12) extends into the substrate (1) to a depth greater than or equal to the shallow depth (P3).
3. A method according to claim 1 or 2 wherein the machined area (10, 12) extends over at least a portion of a deposition surface of said pair of electrodes.
4. Method according to one of claims 1 to 3 in which the machined zone (10, 11, 12) extends over an entire width of the substrate (1) taken transversely to a longitudinal direction of the optical waveguide (5).
5. A method according to claim 1 or 2 wherein the machined area (10) is limited to an area of the waveguide (5) between said pair of electrodes (6,
6. !)■ Method according to one of claims 1 to 5 wherein the machining step is adapted to form several machined zones (10, 11, 12) arranged in series along a longitudinal direction of the optical waveguide (5), said several machined zones (10, 11, 12) being located at least partly between said pair of electrodes (6, 7).
7. Method according to one of claims 1 to 4 in which the machined zone (10) extends over the entire surface of the substrate.
8. Method according to one of claims 1 to 7 in which the machining step is carried out by wet etching, plasma etching, laser etching, lapping or mechanical polishing.
9. Method according to one of claims 1 to 8 comprising a step of depositing a dielectric layer (24), the dielectric layer (24) being arranged on the machined area (10) on the surface of the substrate (1) and / or between the substrate and at least one electrode of the pair of electrodes (6, 7).
10. Electro-optical device (50) obtained according to the method of one of claims 1 to 9.
11. An electro-optical device according to claim 10, used in an electro-optical phase modulator, an optical intensity modulator, a Mach-Zehnder interferometer and / or an active evanescent wave directional coupler.
Citation Information
Patent Citations
Optical phase modulator
US8463081B1
Lithium niobate thick film-based high-speed electro-optical modulator and preparation method thereof
CN109298551A
Optical phase modulator
US20130148920A1