Electrolyte materials for solid oxide electrolyzer cells

IN606770BActive Publication Date: 2026-10-23BLOOM ENERGY CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
IN202247065216
Authority / Receiving Office
IN · IN
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-05-14
Filing Date
2022-11-14
Publication Date
2026-10-23
Estimated Expiration
2041-05-12

AI Technical Summary

Technical Problem

Solid oxide electrolyzer cells (SOEC) face significant challenges with cathode delamination at high current densities, which increases with oxide ion transport flux, leading to cell voltage degradation.

Method used

The use of electrolyte compositions comprising scandia and ceria stabilized zirconia, with specific mol% ratios, and optionally ytterbia, to enhance electronic conductivity and mitigate oxygen precipitation at the electrolyte/air electrode interface, thereby reducing delamination.

Benefits of technology

These electrolyte compositions allow SOEC to operate at higher current densities with reduced cell resistance and overpotential, maintaining stable voltage over extended periods.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

A solid oxide electrolyzer electrolyte composition includes a scandia and ceria stabilized zirconia, containing 5 to 12 mol% scandia, 1 to 7 mol% ceria, and 80 to 94 mol% zirconia, or a yttria and ceria stabilized zirconia containing 3 to 10 mol% yttria, 1 to 6 mol% ceria, and 84 to 96 mol% zirconia.
Need to check novelty before this filing date? Find Prior Art

Description

FIELD

[0001] The present invention is directed to electrolyte materials for use in solid oxide electrolyzercells (SOEC) that mitigate cathode delamination.BACKGROUND

[0002] Solid oxide fuel cells (SOFC) can be operated as electrolyzer cells in order to producehydrogen and oxygen from water. Such cells are referred to as solid oxide electrolyzer cells(SOEC). In SOFC mode, oxygen ions are transported from the cathode side (air) to the anodeside (fuel) and the driving force is the chemical gradient of partial pressure of oxygen acrossthe electrolyte. In SOEC mode, a positive potential is applied to the air side of the cell andthe oxygen ions are transported from the fuel side to the air side. Since the cathode andanode are reversed between SOFC and SOEC (i.e. SOFC cathode is SOEC anode, and SOFCanode is SOEC cathode), the SOFC cathode (SOEC anode) is referred to as the air electrode,and the SOFC anode (SOEC cathode) is referred to as the fuel electrode. A SOEC includesa ceramic (e.g., solid oxide) electrolyte, an air electrode, and a fuel electrode. During SOECmode, water in the fuel stream is reduced (H2O + 2e->O-2 + H2) to form H2 gas and O-2 ions,O-2 ions are transported through the solid electrolyte, and then oxidized on the air side (2O-2 -> O2)to produce molecular oxygen. Since the open circuit voltage for a SOFC operating withair and wet fuel (hydrogen, reformed natural gas) is on the order of .9 to 1V (depending on watercontent), the positive voltage applied to the air side electrode in SOEC mode raises the cell voltageup to typical operating voltages of 1.1 to 1.3V. In constant current mode, the cell voltages willincrease with time if there is degradation of the cell which can arise from both ohmic sources andelectrode polarization.

[0003] One of the major hurdles encountered with state-of-the-art SOEC is the delamination of theair electrode at high current densities. The degree of delamination increases with the current densityand the flux of oxide ion transport.SUMMARY

[0004] In one embodiment, a solid oxide electrolyzer cell electrolyte composition includes a scandiaand ceria stabilized zirconia, comprising 5 to 12 mol% scandia, 1 to 7 mol% ceria, and 80 to 94mol% zirconia. In one embodiment, the electrolyte composition comprises 5 to 10 mol% scandia,1 to 5 mol% ceria, and 84 to 94 mol% zirconia. In another embodiment, the electrolyte compositioncomprises 5 to 10 mol% scandia, 2 to 5 mol% ceria, and 84 to 94 mol% zirconia. In oneembodiment, the electrolyte composition further comprises 0.5 to 3 mol % ytterbia.

[0005] In another embodiment, a solid oxide electrolyzer cell electrolyte composition includes ayttria and ceria stabilized zirconia, comprising 3 to 10 mol% yttria, 1 to 6 mol% ceria, and 84 to 95mol% zirconia.

[0006] A solid oxide electrolyzer cell includes the above electrolyte composition(s), an airelectrode, and a fuel electrode.FIGURES

[0007] FIG. 1A is a perspective view of a solid oxide electrolyzer cell (SOEC) stack, and FIG. 1Bis a side cross-sectional view of a portion of the stack of FIG. 1A.

[0008] FIG. 2 is a plot of voltage at different current for different electrolyzer cells. The figureshows cell voltage of two electrolyte compositions (A and B) operated for extended periods of timeat various currents.DETAILED DESCRIPTION

[0009] FIG. 1A is a perspective view of a solid oxide electrolyzer cell (SOEC) stack 20, and FIG.1B is a side cross-sectional view of a portion of the stack 20 of FIG. 1A. Referring to FIGS. 1Aand 1B, the stack 20 includes multiple electrolyzer cells 1 that are separated by interconnects 9,which may also be referred to as gas flow separator plates or bipolar plates. Each electrolyzer cell1 includes an air electrode 3, a solid oxide electrolyte 5, and a fuel electrode 7. The stack 20 alsoincludes internal fuel riser channels 22.

[0010] Each interconnect 9 electrically connects adjacent electrolyzer cells 1 in the stack 20. Inparticular, an interconnect 9 may electrically connect the fuel electrode 7 of one electrolyzer cell 1to the air electrode 3 of an adjacent electrolyzer cell 1. FIG. 1B shows that the lower electrolyzercell 1 is located between two interconnects 9.

[0011] Each interconnect 9 includes ribs 10 that at least partially define fuel channels 8 and airchannels 8 on opposite sides of the interconnect The interconnect 9 may operate as a gas-fuelseparator that separates a fuel, such as a water vapor, flowing to the fuel electrode 7 of one cell 1 inthe stack 20 from oxidant, such as air, flowing to the air electrode 3 of an adjacent cell 1 in the stack20. At either end of the stack 20, there may be an air end plate or fuel end plate (not shown) forproviding air or fuel, respectively, to the end electrode. The end plates are electrically connected toa power source (e.g., voltage or current source) which provides electrical power to the stack 20 forthe electrolysis reaction in which water provided to the fuel electrode 7 is separated into hydrogenon the fuel side and oxygen which are transported from the fuel electrode 7 to the air electrode3 through the electrolyte 5.

[0012] The air electrode 3 may comprise a mixture of an electrically conductive material andan electrically insulating ceramic material. The electrically conductive material maycomprise a perovskite electrically conductive material, such as lanthanum strontiummanganate, or a metal, such as platinum. The electrically insulating ceramic material maycomprise an ionically conductive stabilized or partially stabilized zirconia (ZrO2) material,such as a rare earth stabilized (e.g., doped) zirconia, such as scandia (Sc2O3) stabilizedzirconia (SSZ), yttria (Y2O3) stabilized zirconia (YSZ), and / or ytterbia (Yb2O3) stabilizedzirconia (YbSZ). The fuel electrode 7 may comprise a cermet material, such as a nickel anda stabilized zirconia and / or doped ceria cermet.

[0013] Without wishing to be bound by a particular theory, the delamination of the air electrode 3may be caused by the precipitation of oxygen at the electrolyte / air electrode interface which canlead to high pressures resulting in air electrode delamination.

[0014] Embodiments of the invention provide electrolyte 5 materials that help mitigate the airelectrode delamination and allow SOEC to operate at higher current densities. It has been foundthat increasing the amount of ceria in a Scandia-Ceria doped Zirconia fluorite material helps mitigateair electrode delamination. For example, SOEC's were tested with two different electrolytematerials with one having approximately twice the amount of ceria as the other. The electrolyteswere A) 88mol% ZrO2-10mol% Sc2O3-2mol%CeO2, which can written as Zr0.8Sc0.182Ce0.018O2-x,and B) 88mol% ZrO2-10mol% Sc2O3-1mol%CeO2-1mol%Yb2O3, which can be written asZr0.793Sc0.180Ce0.009Yb0.018O2-x. The SOEC stack consisted of cells numbered 1-5 with electrolyte Aand cells numbered 6-10 with electrolyte B, and was operated for extended periods of time at thedifferent currents, 1A, 2A, 4A, 10A, 15A, and 20A. At low currents (1-4A), cells with bothelectrolyte compositions behaved well and similarly, as shown in the FIG. 2.

[0015] However, at higher currents (10A and above), the cells with electrolyte composition B(lower ceria content) exhibited a higher voltage increase during operation, indicating higherresistance and cell over potential. The two type of cells have the same air and fuel electrodes andthe only difference is the electrolyte composition. Without wishing to be bound by a particulartheory, the inventor believes that the higher ceria content in the electrolyte increases the electronicconductivity in the electrolyte, which mitigates the precipitation of oxygen at the electrolyte / cathodeinterface.

[0016] Based on these results, the following compositions of doped zirconia are provided for SOECelectrolyte 5 materials.

[0017] 10mol% scandia doped zirconia with 1 to 5mol% CeO2 doping as shown below:89mol%ZrO2-10mol%Sc2O3-1mol%CeO2;88mo%ZrO2-10mol%Sc2O3-2mol%CeO2;87mo%ZrO2-10mol%Sc2O3-3mol%CeO2;86mo%ZrO2-10mol%Sc2O3-4mol%CeO2;85mo%ZrO2-10mol%Sc2O3-5mol%CeO2.

[0018] 9mol% scandia doped zirconia with 1-5mol% CeO2 doping, as shown below:90mol%ZrO2-9mol%Sc2O3-1mol%CeO2 to 86mol%ZrO2-9mol%Sc2O3-5mol%CeO2;8mol%Scandia doped zirconia with 1-5mol% CeO2 doping;7mol%Scandia doped zirconia with 1-5mol% CeO2 doping;6mol%Scandia doped zirconia with 1-5mol% CeO2 doping;5mol%Scandia doped zirconia with 1-5mol% CeO2 doping.

[0019] Ytterbia may also be added to the scandia and ceria stabilized zirconia at 0. 5 to 3 mol%,such as 0.75 to 1.5 mol%, as shown below:10mol%Scandia-1mol%Yb2O3 doped zirconia with 1-5mol% CeO2 doping;88molZr2O2-10mol%Sc2O3-1mol%Yb2O3-1mol%CeO2;87molZr2O2-10mol% Sc2O3-1mol%Yb2O3-2mol%CeO2;86molZr2O2-10mol% Sc2O3-1mol%Yb2O3-3mol%CeO2;85molZr2O2-10mol% Sc2O3-1mol%Yb2O3-4mol%CeO2;84molZr2O2-10mol% Sc2O3-1mol%Yb2O3-5mol%CeO2.

[0020] As above: 5-9mol%Scandia doped zirconia-1mol%Yb2O3-(1-5mol%CeO2).

[0021] Thus, compositions with at least 2 mol% ceria, such as 2 to 7 mol%, including 2 to 5 mol%ceria, are preferred based on FIG. 2.

[0022] In another embodiment, the electrolyte compositions may comprise yttria and ceriastabilized zirconia. The compositions may comprise 3 to 10 mol% yttria, 1 to 6 mol% ceria, and 84to 96 mol% zirconia.

[0023] In one embodiment, the electrolyte composition comprises 3 mol% yttria, 1 to 5 mol% ceria,(such as 1, 2, 3, 4 or 5 mol% ceria), and 92 to 96 mol% zirconia. In another embodiment, theelectrolyte composition comprises 8 mol% yttria, 2 to 6 mol% ceria, (such as 2, 3, 4, 5 or 6 mol%ceria,) and 86 to 90 mol% zirconia. In another embodiment, the electrolyte composition comprises10 mol% yttria, 1 to 4 mol% ceria, (such as 1, 2, 3 or 4 mol% ceria), and 86 to 89 mol% zirconia.

[0024] The yttria and ceria stabilized zirconia may be formed by mixing yttria stabilized zirconiapowder and ceria powder followed by sintering the powder blends into the electrolyte composition.Alternatively, the yttria and ceria stabilized zirconia may be formed by mixing yttria powder,zirconia powder and ceria powder followed by sintering the synthesized powders into the electrolytecomposition.

[0025] 8YSZ (8 mol% yttria stabilized zirconia) and CeO2 powder blends may be formed asfollows: mix (100-x) mol% 8YSZ powder with x mol% CeO2 powder, where x ranges from 2 to 6,as shown in the Table 1 below.Table 18YSZ + 2CeO28YSZ + 3CeO28YSZ + 4CeO28YSZ + 5CeO28YSZ + 6CeO2

[0026] 8YSZ and CeO2 synthesized powders may be formed as follows: mix 8mol% (Y2O3) with xmol% (CeO2) and (92-x) mol% (ZrO2) powders, where x ranges from 2 to 5, as shown in the Table2 below.Table 28YSZ + 2 CeO2: synthesize 8mol%(Y2O3) + 2mol%(CeO2) + 90mol%(ZrO2)8YSZ + 3 CeO2: synthesize 8mol%(Y2O3) + 3mol%(CeO2) + 89mol%(ZrO2)8YSZ + 4 CeO2: synthesize 8mol%(Y2O3) + 4mol%(CeO2) + 88mol%(ZrO2)8YSZ + 5 CeO2: synthesize 8mol%(Y2O3) + 5mol%(CeO2) + 87mol%(ZrO2)

[0027] 3YSZ and CeO2 powder blends may be formed as follows: mix (100-x) mol% 3YSZ powderwith x mol% CeO2 powder, where x ranges from 1 to 5.

[0028] 3YSZ and CeO2 synthesized powders may be formed as follows: mix 3mol% (Y2O3) with xmol% (CeO2) and (97-x) mol% (ZrO2) powders, where x ranges from 1 to 5.

[0029] 10YSZ and CeO2 powder blends may be formed as follows: mix (100-x) mol% 10YSZpowder with x mol% CeO2 powder, where x ranges from 1 to 4.

[0030] 10YSZ and CeO2 synthesized powders may be formed as follows: mix 10 mol% (Y2O3)with x mol% (CeO2) and (90-x) mol% (ZrO2) powders, where x ranges from 1 to 4.

[0031] The preceding description of the disclosed aspects is provided to enable any person skilledin the art to make or use the present invention. Various modifications to these aspects will be readilyapparent to those skilled in the art, and the generic principles defined herein may be applied to otheraspects without departing from the scope of the invention. Thus, the present invention is notintended to be limited to the aspects s hown herein but is to be accorded the widest scope consistentwith the principles and novel features disclosed herein.

Claims

1. A solid oxide electrolyzer electrolyte composition comprising a scandia and ceria stabilized zirconia, comprising: 5 to 12 mol% scandia; 1 to 7 mol% ceria; and 80 to 94 mol% zirconia.

2. The electrolyte composition of claim 1, comprising: 5 to 10 mol% scandia; 1 to 5 mol% ceria; and 84 to 94 mol% zirconia.

3. The electrolyte composition of claim 1, comprising: 5 to 10 mol% scandia; 2 to 5 mol% ceria; and 84 to 94 mol% zirconia.

4. The electrolyte composition of claims 1, 2 or 3, further comprising 0.5 to 3 mol % ytterbia.

5. A solid oxide electrolyzer electrolyte composition comprising a yttria and ceria stabilized zirconia comprising: 3 to 10 mol% yttria; 1 to 6 mol% ceria; and 84 to 96 mol% zirconia.

6. The electrolyte composition of claim 5, wherein the electrolyte composition comprises: 3 mol% yttria; 1 to 5 mol% ceria; and 92 to 96 mol% zirconia.

7. The electrolyte composition of claim 5, wherein the electrolyte composition comprises: 8 mol% yttria; 2 to 6 mol% ceria; and 86 to 90 mol% zirconia.

8. The electrolyte composition of claim 5, wherein the electrolyte composition comprises: 10 mol% yttria; 1 to 4 mol% ceria; and 86 to 89 mol% zirconia.

9. A solid oxide electrolyzer cell comprising: the electrolyte composition of claim 1; an air electrode; and a fuel electrode.

10. A solid oxide electrolyzer cell comprising: the electrolyte composition of claim 2; an air electrode; and a fuel electrode.

11. A solid oxide electrolyzer cell comprising: the electrolyte composition of claim 3; an air electrode; and a fuel electrode.

12. A solid oxide electrolyzer cell comprising: the electrolyte composition of claim 4; an air electrode; and a fuel electrode.

13. A solid oxide electrolyzer cell comprising: the electrolyte composition of claim 5; an air electrode; and a fuel electrode.

14. A solid oxide electrolyzer cell comprising: the electrolyte composition of claim 6; an air electrode; and a fuel electrode.

15. A solid oxide electrolyzer cell comprising: the electrolyte composition of claim 7; an air electrode; and a fuel electrode.

16. A solid oxide electrolyzer cell comprising: the electrolyte composition of claim 8; an air electrode; and a fuel electrode.

17. A solid oxide electrolyzer stack, comprising: a plurality of solid oxide electrolyzer cells of claim 9; and a plurality of interconnects separating the plurality of solid oxide electrolyzer cells.

18. A solid oxide electrolyzer stack, comprising: a plurality of solid oxide electrolyzer cells of claim 13; and a plurality of interconnects separating the plurality of solid oxide electrolyzer cells.