A tin-plated steel sheet for aerosol can bottom covers having high-pressure strength and method of producing same.
Patent Information
- Application Number
- IN202221032964
- Authority / Receiving Office
- IN · IN
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-06-09
- Publication Date
- 2026-10-29
- Estimated Expiration
- 2042-06-09
AI Technical Summary
Existing methods for producing high-strength tin-plated steel sheets for aerosol can bottom covers require costly and time-consuming aging treatments, leading to defects like stretcher strains and increased production costs, while also restricting the thickness of the material due to limitations in double cold reduction mills.
A method involving a specific chemical composition (C: 0.03 - 0.06%, Mn: 0.2 - 0.4%, Si: 0.005 - 0.03%, P: 0.005 - 0.02%, Al: 0.02 - 0.06%, S: 0.005 - 0.01%, N: 0.0001 - 0.005%) and a manufacturing process including converter smelting, continuous casting, hot rolling, acid pickling, cold rolling, continuous annealing, secondary rolling, and electro-tinning to produce a tin-plated steel sheet with a thickness of 0.30 - 0.39mm, yielding 550 - 610 MPa strength and avoiding yield point elongation.
The solution achieves high-pressure resistance, excellent formability, and cost-effective production of tin-plated steel sheets that meet 2021-FEA standards for aerosol containers without yield point elongation or stretcher strains, utilizing a double cold reduction route that reduces the thickness requirement and minimizes additional processing steps.
Abstract
Description
FIELD OF THE INVENTIONThe present invention relates to a tin-plated steel sheet for an aerosol CANends / bottom cover and a method for producing the same, and particularly to asteel sheet for an aerosol can bottom having a high-pressure strength and a methodfor producing the same.BACKGROUND OF THE INVENTIONThe aerosol CANs are filled with propellant for ejecting the contents. Thecontents inside the CAN are in a high-pressure state with pressure ranging from12 to 18 bars. Therefore, tin-plated material of thickness in the range of 0.30mmto 0.39mm with yield strength in the range of 550-610 Mpa is most suitable formaking the bottom covers of aerosol cans to resist high-pressure inside the canswithout failure. However, there are certain difficulties associated with theproduction of high-strength tin plates of thickness more than 0.30mm.Conventionally to produce high strength Tin plated material of YS more than 500Mpa, double reduction method is used where annealed material is subjected to asecondary reduction of more than 33% to strengthen the material by strainhardening mechanism. But in this case the thickness of the required material ismore than 0.30mm and the annealed material will require to have a thickness ofmore than 0.50 mm to achieve the required 33% reduction during secondaryrolling. Designed for producing thinner gauge materials, the Double coldreduction mills have the capability of feeding material with a maximum inputthickness of 0.50mm restricting the use of annealed material of less than 0.50mm.US9315877B2 reveals a method of for the production of steel sheets for bottomcovers of aerosol cans where the thickness of the sheet is between 0.27 to 0.34mmwhich includes, as chemical composition, C: 0.025 to 0.065 mass %, Mn: 0.10 to0.28 mass %, P: 0.005 to 0.03 mass %, Al: 0.01 to 0.04 mass %, N: 0.0075 to0.013 mass %, Si: limited to 0.05 mass % or less, S: limited to 0.009 mass % orless, and the balance consisting of Fe and unavoidable impurities, wherein yieldpoint YP in rolling direction after aging treatment is in range of 460 to 540 Mpa.This process involves a further process of aging treatment leading to a high cost ofproduction. Also due to aging treatment, the material has a yield point elongationwhich may lead to defects like Stretcher strains.US9506131B2 disclosed a steel sheet containing C: 0.02% or more and 0.10% orless, Si: 0.01% or more and 0.5% or less, P: 0.001% or more and 0.100% or less,S: 0.001% or more and 0.020% or less, N: 0.007% or more and 0.025% or less,Al: 0.01% or more and {−4.2×N (%)+0.11}% or less, Mnf: 0.10% or more andless than 0.30% where Mnf is defined by equation Mnf=Mn−1.71×S, and thebalance being Fe and inevitable impurities, in which the steel sheet has a thicknessof 0.35 (mm) or less, the product of the lower yield point (N / mm2) of the steelsheet (mm) is 160 (N / mm). The method uses higher nitrogen (>0.0070%)percentage in order to carry out natural strain aging of the material for 10 daysafter giving a pre-strain of 10%. Natural aging of 10 days increases the time ofproduction significantly.The prior arts mentioned above need a further aging process to increase thestrength of the material. This adds to the cost and time of production. Further dueto aging treatment the material has yield point elongation which can lead to issueslike stretcher strain. Also to facilitate aging the chemistry of raw material requiresthe presence of Nitrogen in excess of 70ppm. This is detrimental to steel qualityand can lead to issues like pin holes.OBJECTS OF THE INVENTIONThe basic object of the present invention is directed toward the generation of tinplated steel sheets for the bottom covers of aerosol cans.A still further object of the present invention is directed to provide tin-plated steelsheets with good formability.A still further object of the present invention is to provide the tin-plated steel sheetmaterial with pressure resistance to withstand the high-pressure condition insidethe aerosol cans.A still further object of the present invention is to produce aerosol cans from saidtin-plated steel sheets without yield point elongation, and which will not beaffected by further natural aging.A still further object of the present invention is directed to the production of tinplated steel sheet material with required properties through double reduction toeliminate the additional process involved after tin-plating as mentioned in theprior arts.SUMMARY OF THE INVENTIONThe present invention provides a tin-plated steel sheet adapted for aerosol canbottom covers having high-pressure strength comprises the base steel sheetcomposition in terms of weight %: C: 0.03 - 0.06 %; Mn: 0.2 - 0.4%; Si: 0.005 –0.03%; P: 0.005 - 0.02%; Al: 0.02 - 0.06%; S: 0.005 - 0.01 %; N: 0.0001 - 0.005%; the balance being Fe and other unavoidable impurities.In one aspect of the present invention, the tin-plated steel sheet is having thicknessin the range of 0.30 - 0.39mm, yield strength in the range of 550 - 610 MPa,tensile strength in the range of 560 - 620 MPa, total elongation in the range of 2.5- 5% and hardness HR30Tm in the range of 73 - 76.In another aspect of the present invention, the tin-plated steel sheet in the form ofaerosol can bottom is capable to withstand pressure as per the 2021-FEAstandards for aerosol containers.In another aspect of the present invention, thetin-plated steel sheet is free of yieldpoint elongation and stretcher strains during forming of can bottom covers.Further, the present invention provides a method of manufacturing tin-plated steelsheet adapted for aerosol can bottom covers having high-pressure strengthcomprises following steps.Step 1: Converter Smelting: Obtaining molten steel from basic oxygen furnace(BOF) and RH degasser comprises following chemical composition in terms ofweight %: C: 0.03 - 0.06 %; Mn: 0.2 - 0.4%; Si: 0.005 – 0.03%; P: 0.005 - 0.02%;Al: 0.02 - 0.06%; S: 0.005 - 0.01 %; N: 0.0001 - 0.005 %; the balance being Feand other unavoidable impurities.Step 2: Slab Continuous Casting: Refining and continuous casting the molten steelto obtain a solid slab.Step 3: Hot Rolling: The solid slab is reheated to a temperature of 1150 - 1250 °C.The reheated slab is subjected to roughing rolling in roughing mill with roughingmill delivery temperature in the range of 980 - 1080°C. The rough rolled steel issubjected to finish rolling with finish mill exit temperature ranging from Ac3 °C -Ac3+100 °C. The finished rolled steel is cooled at an average run-out table coolingrate in the range of 10 to 30 °C / second to obtain a hot-rolled coil.Step 4: Acid Pickling: Pickling the hot-rolled coil in a continuous line withconcentrations of acid HCl to remove the surface scale to form a hot-rolledpickled coil.Step 5: Cold Rolling Reduction: Cold rolling the hot-rolled pickled coil or the hotrolled coil to form a cold-rolled coil. The cold reduction of thehot-rolled pickledcoil in the range of 75 - 80%.Step 6: Continuous Annealing: Continuously annealing the cold-rolled coil toobtain an annealed steel. The annealing soaking temperature is 700-720 °C. Theannealing soaking time is 40 - 200s. The cold-rolled steel is over-aged at thetemperature from 420- 430 °C. The skin pass elongation of the annealed steel toan annealed steel coil.Step 7: Secondary Rolling Reduction: The annealed steel coil is subjected tosecondary rolling reduction, wherein the rolling reduction is 20-24% to obtainsecondary rolled steel coil.Step 8: Tinning: Electro tinning on the secondary rolled steel coil to obtain the tinplated steel sheet having a hardness grade of TH580. The reflow temperature iscontrolled to 230 to 265 °C.To facilitate the production of high strength Tin plated steel sheet of thicknessrange of 0.30mm to 0.39mm through a double cold reduction route, the materialwas annealed at a temperature of 700-720 Deg Celsius in a continuous annealingline to get fine-grained microstructure. The microstructure thus obtained hadgrains with ASTM grain number 10 which are 20% smaller than the grains ofannealed material generally used for Double reduced material, with microstructureof base steel having 98-99% ferrite phase and 1-2% pearlite phase and grains areoriented in the rolling direction as well as has an excellent anisotropic property ofΔR values ranging from 0.8-1. As a result, the annealed material produced was ofhigher strength as compared to annealed material generally used for doublereduced material. The final properties could be achieved with 22-24% reductionduring secondary rolling instead of 33% due to the high strength of the inputmaterial. Hence the thickness of the annealed material could be controlled within0.50mm which is within the process capability of a double cold reduction mill.A further aspect of the present invention is directed to Aerosol can having canbottom obtained of having high-pressure strength base steel sheet composition interms of weight %:C: 0.03 - 0.06 %;Mn: 0.2 - 0.4%;Si: 0.005 – 0.03%;P: 0.005 - 0.02%;Al: 0.02 - 0.06%;S: 0.005 - 0.01 %;N: 0.0001 - 0.005 %;the balance being Fe and other unavoidable impurities, and wherein the tin-platedsteel sheet is having thickness in the range of 0.30 - 0.39mm, yield strength in therange of 550 - 610 MPa, tensile strength in the range of 560 - 620 MPa, totalelongation in the range of 2.5 - 5% and hardness HR30Tm in the range of 73 - 76.A still further aspect of the present invention is directed to said aerosol canwherein the can bottom covers can withstand pressure as per the 2021-FEAstandards for aerosol containers.The aboveand other aspects and advantages of the present invention are describedhereunder in greater details with reference to following accompanying nonlimiting illustrative drawing and examples.BRIEF DESCRIPTION OF ACCOMPANYING DRAWINGFigure 1: the micrograph showing microstructure of base steel having 98-99%ferrite phase and 1-2% pearlite phase with grain oriented in rolling direction.DETAILED DESCRIPTION OF THE INVENTION WITH REFERENCETO ACCOMPANYING DRAWING AND EXAMPLESThe present invention provides a tin-plated steel sheet for aerosol can bottomcovers having high-pressure strength comprises the base steel sheet withfollowing chemical composition in terms of weight %: C: 0.03 - 0.06 %; Mn: 0.2 -0.4%; Si: 0.005 – 0.03%; P: 0.005 - 0.02%; Al: 0.02 - 0.06%; S: 0.005 - 0.01 %;N: 0.0001 - 0.005 %; the balance being Fe and other unavoidable impurities. Thetin-plated steel has good formability, ageing resistance and surface tin coating, itschemical compositions and method of manufacturing are described here underwith explanation on metallurgical factors deciding the range of constituents in acomposition.The tin-plated steel sheet is having thickness in the range of 0.30 - 0.39mm, yieldstrength in the range of 550 - 610 MPa, tensile strength in the range of 560 - 620MPa, total elongation in the range of 2.5 - 5% and hardness HR30Tm in the rangeof 73 - 76. The tin-plated steel sheet is used to make the can bottom to withstandpressure as per the 2021-FEA standards for aerosol containers. The tin-plated steelsheet is devoid of yield point elongation and no stretcher strains are avoidedduring forming of can bottom covers.Hereinafter, the steel composition is described hereunder with an explanation onmetallurgical factors governing the ranges of the constituents in a compositionaccording to a preferred embodiment wherein all the elements are in weight % aredemonstrated.Carbon (0.030-0.060 wt.%) - While carbon increases the steel strength, itreduces the cold workability and the deep drawability of the cold-rolled steel sheetremarkably and thus the higher limit of the cold-rolled sheet is set at 0.1 wt.%. Forimproving the R-value i.e. drawabilty it is desirable to reduce the C level less than0.06 wt.%. Lowering the carbon content below 0.02 wt.% results in poor ageingproperties since below 0.02 wt.% steel is the complete α-ferrite region in the ironcementite phase diagram resulting in no cementite formation. Consequently, morefree carbon will be available in the steel matrix which deteriorates the ageingproperty. Cementite formed in grain boundaries its precipitate size should begreater than 1µm which helps in reducing solute carbon and suppress the YPE forbetter ageing resistance. To avoid YPE and to have yield strength within thedesired limit, the level of Carbon is between 0.02-0.06 wt. percent.Mn (0.2-0.4) wt. % - The Mn ranges from 0.3 to 0.5 % is most desirable giventhat S remains in the favorable range of 0.008wt% or less. Keeping the Mn level0.1wt% with higher Sulphur content may result in surface irregularities such asred shortness, edge crack sliver, etc. The lower limit of Mn is kept at 0.3% toensure the surface properties deteriorate and embrittlement may occur due to hotbrittleness as the amount of Mn is insufficient to fix S. More than 0.5 %Mn makesthe steel hard and the deep draw ability lower.Al (0.02-0.06) wt. % – Al wt% ranges from 0.02-0.06 and is intended for fixingfree N which results in aging if left unfixed. In addition, less than 0.02 % Al willdelay the AlN precipitation causing the insufficient growth of ferrite grains anddeteriorating the {111} texture. An optimized volume fraction of AlN in steelmatrix in combination with NbC precipitate results in excellent drawability andreduced ∆r value as described in the present invention. The same is achieved byoptimizing hot rolling and cold rolling parameters to avoid Ostwald ripeningphenomenon which results in coarse precipitate size along with low r-bar values.Nitrogen (0.005wt% or less) -The upper limit for N is 0.005%; it is advisable tokeep it to a minimum level. Higher N content requires a higher Al addition to fixextra N and increase the volume of AlN precipitates which strengthens thematerial, ultimately deteriorating the drawing property.P (0.005-0.02) wt. %: -. P is an element that improves the strength at a low cost,and the amount of addition thereof varies depending on a target strength level.When the added amount exceeds more than 0.02 wt.% the yield strength levelincreases significantly. In addition, a higher amount of P promotes the formationof surface defects and significantly reduces the corrosion resistance of the basemetal. So, the maximum limit of P is kept at 0.02 %.Si (0.005-0.03) wt.%: Itis an element utilized for increasing the strength of steel.As the silicon content increases the ductility noticeably deteriorates. Since silicondeteriorates tin coating properties by forming SiO2 type of oxides (scale) on thesurface. It is advantageous to add as low amount of silicon to the steel as ispossible, the added amount of silicon is preferably 0.03 wt.% or less.Following abbreviations, terminologies and expressions are used to describe themanner of implementation of the present invention:SRT -Slab Reheating TemperatureFT-Finishing TemperatureCT- Coiling TemperatureAc1 & Ac3 – Critical temperatures in iron-carbide diagramEl – Elongation (%)UTS - Ultimate Tensile Strength (MPa)YS - Yield Strength (MPa)SPM - Skin Pass Elongation (%)Hereinafter, the manufacturing method of the non-oriented electrical steel sheet ofthis invention is demonstrated in detail.A method of manufacturing tin-plated steel sheet for aerosol can bottom covershaving high-pressure strength comprises following steps.Step 1: Converter Smelting: Obtaining molten steel from basic oxygen furnace(BOF) and RH degasser comprises following chemical composition in terms ofweight %: C: 0.03 - 0.06 %; Mn: 0.2 - 0.4%; Si: 0.005 – 0.03%; P: 0.005 - 0.02%;Al: 0.02 - 0.06%; S: 0.005 - 0.01 %; N: 0.0001 - 0.005 %; the balance being Feand other unavoidable impurities.Step 2: Slab Continuous Casting: Refining and continuous casting the molten steelto obtain a solid slab.Step 3: Hot Rolling: The solid slab is reheated to a temperature of 1150 - 1250 °C.The reheated slab is subjected to roughing rolling in roughing mill with roughingmill delivery temperature in the range of 980 - 1080°C. The rough rolled steel issubjected to finish rolling with finish mill exit temperature ranging from Ac3 °C -Ac3+100 °C. The finished rolled steel is cooled at an average run-out table coolingrate in the range of 10 to 30 °C / second to obtain a hot-rolled coil.Step 4: Acid Pickling: Pickling the hot-rolled coil in a continuous line withconcentrations of acid HCl to remove the surface scale to form a hot-rolledpickled coil.Step 5: Cold Rolling Reduction: Cold rolling the hot-rolled pickled coil or the hotrolled coil to form a cold-rolled coil. The cold reduction of the hot-rolled pickledcoil in the range of 75 - 80%.Step 6: Continuous Annealing: Continuously annealing the cold-rolled coil toobtain an annealed steel. The annealing soaking temperature is 700-720 °C. Theannealing soaking time is 40 - 200s. The cold-rolled steel is over-aged at thetemperature from 420- 430 °C. The skin pass elongation of the annealed steel toan annealed steel coil. By annealing the material in lower temperatures of 700-720°C, the annealed steel coil has finer grains of ASTM grain number 10 as comparedto the annealed material is generally used for double reduce material.Step 7: Secondary Rolling Reduction: The annealed steel coil is subjected tosecondary rolling reduction, wherein the rolling reduction is 20-24% to obtainsecondary rolled steel coil.Step 8: Tinning: Electro tinning on the secondary rolled steel coil to obtain the tinplated steel sheet having a hardness grade of TH580. The reflow temperature iscontrolled to 230 to 265 °C.The microstructure of base steel has 98-99% ferrite phase and 1-2% pearlite phaseas shown in Figure 1. The grains are oriented in the rolling direction as well ashas an excellent anisotropic property of ΔR values ranging from 0.8-1 due tolower secondary reduction percentage of 22-24% considering high strength doublereduced material. These microstructural properties ensure minimum earingformation in formed bottom covers which in turn leads to significant decrease inloss due to trimming of ears.Hereinafter, the present invention will be described specifically by way ofexamples.ExamplesComplete description of steel according to the present advancement andcomparative steel grades are illustrated in following table 1 to table 4 and theweight percent range of constituents and the selective process parametersaccording to the invention are validated through following examples 1 & 2:Table 1: Elemental Compositions in weight % of the inventive steel sheets alongwith comparative examples.Table 2: Hot rolling and cold rolling of inventive with comparative steel sheetshaving chemical compositions as per Table 1.Table 3: Tin Coating Parameters of inventive with comparative steel sheetshaving chemical compositions as per Table 1.Table 4: Mechanical properties of comparative steels having chemicalcomposition as per table 1 and being processed as per Table 2 and Table 3Table 1Table 2* SRT- Slab reheating temperature, FT- hot finish rolling temperature, ROT- Runout table at hot coil mill, CR%- Cold rolling reduction %, SS- soaking section,OAS-Over-Ageing Section, SPM- Skin pass elongationTable 3*I - Present inventive example, C- Comparative Examples, G- Good, NG- NotGoodThe mechanical property YS, TS, El, and Yield point elongation was done as perIS-1993-2018The pressure test is done as per 2021-FEA standards for aerosol containers.It can be appreciated from Table 1 to Table 4 that steel sheets remarked as “I” aresatisfying all the scopes of present invention. These steels exhibit improved Yieldstrength of 550-610 MPa, Tensile strength of 560-620 MPa, total elongation in therange of 2.5% to 5%, hardness level (HR30T) in the range of 73 to 76 andexcellent pressure resistance. Whereas, Steel remarked as ‘C’ doesn’t comply withat least one of the scope of the present invention and does not conform withminimum one or more of the end product attributes as mentioned in the scope ofthe present invention. For example, steel no. 4 has a low carbon concentration lessthan 0.02. This lead to low yield strength. Similarly, sample 1 and 2 are havingYS less than 550 MPa and hardness is less than 73 HR30T which is out of scopeof present invention and sample 1 failed in pressure test at customer end afterCAN formation.It is thus possible to produce tin plated steel of Yield strength of 550-610 MPa,Tensile strength of 560-620 MPa, total elongation of 2.5% or more, hardness level(HR30T) in the range of 73 to 76, Excellent pressure resistance invention usingsteel grade with composition by weight %: C: 0.06-0.06 %; Mn: 0.2- 0.4%; Si: 0–0.03%; P: 0-0.02%; Al: 0.02-0.06%; S: 0.01 % or less; N: 0.005 % or less; and thebalance being Fe and other unavoidable impurities, and annealing it in atemperature range of 700 to 720 °C in continuous annealing line followed bysubjecting it to a secondary reduction of 22-24%.
Claims
1. A tin-plated steel sheet adapted for aerosol can bottom covers having highpressure strength comprising of base steel sheet composition in terms of weight %: C: 0.03 - 0.06 %; Mn: 0.2 - 0.4%; Si: 0.005 - 0.03%; P: 0.005 - 0.02%; Al: 0.02 - 0.06%; S: 0.005 - 0.01 %; N: 0.0001 - 0.005 %; the balance being Fe and other unavoidable impurities, and wherein the tin-plated steel sheet is having thickness in the range of 0.30 - 0.39mm, yield strength in the range of 550 - 610 MPa, tensile strength in the range of 560 - 620 MPa, total elongation in the range of 2.5 - 5% and hardness HR30Tm in the range of 73 - 76.
2. The tin-plated steel sheet as claimed in claim 1,in the form of aerosol can bottom which can withstand pressure as per the 2021-FEA standards for aerosol containers.
3. The tin-plated steel sheet as claimed in claim 1,which is free of yield point elongation and stretcher strains during forming of can bottom covers.
4. A method of manufacturing tin-plated steel sheet adapted for aerosol can bottom covers having high-pressure strength comprises following steps: converter smelting: obtaining molten steel from basic oxygen furnace (BOF) and RH degasser comprises following chemical composition in terms of weight %: C: 0.03 - 0.06 %; Mn: 0.2 - 0.4%; Si: 0.005 - 0.03%; P: 0.005 - 0.02%; Al: 0.02 - 0.06%; S: 0.005 - 0.01 % ; N: 0.0001 - 0.005 %; the balance being Fe and other unavoidable impurities; slab continuous casting: refining and continuous casting the molten steel to obtain solid slab; hot rolling: the solid slab is reheated to a temperature of 1150 - 1250 °C, the reheated slab is subjected to roughing rolling in roughing mill with roughing mill delivery temperature in the range of 980 - 1080°C, the rough rolled steel is subjected to finish rolling with finish mill exit temperature ranging from Ac3 °C - Ac3+100 °C, the finish rolled steel is cooled at an average run-out table cooling rate in the range of 10 to 30 °C / second to obtain a hot-rolled coil; acid pickling: pickling the hot-rolled coil in a continuous line with concentrations of acid HCl to remove the surface scale to form a hot-rolled pickled coil; cold rolling reduction: cold rolling the hot-rolled pickled coil or the hot-rolled coil to form a cold-rolled coil, wherein the cold reduction of hot-rolled pickled coil in the range of 75 - 80%; continuous annealing: continuously annealing the cold-rolled coil to obtain an annealed steel, wherein during the continuous annealing, the annealing soaking temperature is 700-720 °C, the annealing soaking time is 40 - 200s, cold-rolled steel is over-aged at the temperature from 420- 430 °C, skin pass elongation of the annealed steel to an annealed steel coil; secondary rolling reduction: the annealed steel coil is subjected to secondary rolling reduction, wherein the rolling reduction is 20-24% to obtain secondary rolled steel coil; and tinning: electro tinning on the secondary rolled steel coil to obtain the tin-plated steel sheet having a hardness grade of TH580, wherein the reflow temperature is controlled to 230 to 265 °C.
5. The method of manufacturing tin-plated steel sheet adapted for aerosol can bottom covers having high-pressure strength as claimed in claim 4, wherein the step of double cold reduction rolling is carried out under controlled conditions of higher front, back tension and use of emulsion wherein oil concentration ranges from 3-4%. such as to provide tin-plated steel sheet having thickness in the range of 0.30 - 0.39mm, yield strength in the range of 550 - 610 MPa, tensile strength in the range of 560 - 620 MPa, total elongation in the range of 2.5 - 5% and hardness HR30Tm in the range of 73 - 76, with microstructure of base steel having 98-99% ferrite phase and 1-2% pearlite phase and grains are oriented in the rolling direction as well as has an excellent anisotropic property of ΔR values ranging from 0.8-1.
6. The method of manufacturing tin-plated steel sheet adapted for aerosol can bottom covers having high-pressure strength as claimed in claim 4, wherein the tin-plated steel sheet is used to make the can bottom to withstand pressure as per the 2021-FEA standards for aerosol containers.
7. The method of manufacturing tin-plated steel sheet adapted for aerosol can bottom covers having high-pressure strength as claimed in claim 4, wherein the tin-plated steel sheet is free of yield point elongation and stretcher strains during forming of can bottom covers.
8. Aerosol can having can bottom obtained of having high-pressure strength base steel sheet composition in terms of weight %: C: 0.03 - 0.06 %; Mn: 0.2 - 0.4%; Si: 0.005 - 0.03%; P: 0.005 - 0.02%; Al: 0.02 - 0.06%; S: 0.005 - 0.01 %; N: 0.0001 - 0.005 %; the balance being Fe and other unavoidable impurities, and wherein the tin-plated steel sheet is having thickness in the range of 0.30 - 0.39mm, yield strength in the range of 550 - 610 MPa, tensile strength in the range of 560 - 620 MPa, total elongation in the range of 2.5 - 5% and hardness HR30Tm in the range of 73 - 76.
9. The aerosol can as claimed in claim 8 wherein the can bottom can withstand pressure as per the 2021-FEA standards for aerosol containers.