Polymeric deposition aid for laundry
Patent Information
- Application Number
- JP2022514717
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2019-09-25
- Filing Date
- 2020-09-23
- Publication Date
- 2024-12-05
- Estimated Expiration
- 2040-09-23
AI Technical Summary
Existing laundry products face challenges in delivering fabric care benefit agents effectively due to the repulsive forces between anionic surfactants and fabrics, leading to mechanical and chemical damage, such as wrinkles, fading, and reduced delivery efficiency.
Development of a laundry deposition aid polymer with specific structural units and molecular weight, enhancing the deposition efficiency of fabric care benefit agents by improving their affinity to fabrics.
The deposition aid polymer significantly enhances the delivery efficiency of fabric care benefit agents, reducing mechanical and chemical damage to fabrics.
Smart Images

Figure 2021061773000001 
Figure 2021061773000002 
Figure 2021061773000003
Abstract
Description
Technical Field
[0001] The present invention relates to an adhesion aid polymer for washing. Specifically, the present invention provides structural units of formula (I) in an amount of more than 50% to 99% by weight based on the weight of the adhesion aid polymer,
Chemical Formula
Chemical Formula
Chemical Formula
[0002] Washing fabrics is useful for removing stains, odors, and dirt. Nevertheless, the washing process tends to cause mechanical and chemical damage to fibers, resulting in wrinkles, fading, pilling, fuzzing, dye migration, stiffness, fabric damage, fiber degradation, and other problems that consumers find undesirable. Therefore, laundry products (e.g., detergents, fabric softeners) are often formulated to contain fabric care beneficial agents to mitigate some of the undesirable washing problems.
[0003] Many fabric care agents have been found to offer only limited benefits due to their inefficient delivery to fabrics during the washing process. The affinity between fabric care agents and fabrics is typically compromised by the lack of a natural attraction between the agent and the fabric. This stems from the fact that most fabric care agents are either anionic or nonionic to avoid undesirable interactions with anionic surfactants, which are typically contained in laundry product formulations and can result in poor washing performance. Given that most fibers used in fabrics (e.g., cotton, wool, silk, and nylon) carry a slightly anionic charge in the washing solution, a repulsive force exists between the fabric care agent and the fabric, resulting in a significant decrease in delivery efficiency.
[0004] One approach to enhance the delivery of fabric care beneficial agents is described by Wang et al. in U.S. Patent No. 7,056,879. Wang et al. disclose a laundry product composition comprising: a) at least one water-insoluble silicone derivative fabric care beneficial agent in about 0.1% to about 10% by weight of the composition, having a particle size of about 1 nm to 100 microns; b) at least one cationic cellulose delivery enhancer in about 0.01% to about 5% by weight of the composition; c) a surfactant in about 1% to about 80% by weight of the composition; d) a builder in about 3.96% to about 80% by weight of the composition; and e) a compatible enzyme in about 0.001% to about 5% by weight of the composition, selected from lipase enzymes, protease enzymes, or mixtures thereof, wherein the ratio of delivery enhancer to fabric care beneficial agent is about 1:50 to about 1:1.
[0005] Nevertheless, there remains a continuing need for adhesion enhancers to improve the delivery efficiency of fabric care beneficial agents incorporated into laundry products.
[0006] The present invention relates to (a) a structural unit of formula (I) in an amount of more than 50 to 99% by weight, based on the weight of the adhesion aid polymer, [ka] In the formula, each R 1 However, hydrogen, -C 1-4 Alkyl groups, and -CH2OR 3 Independently selected from the group consisting of elements, each R 3 However, -C 1-12 A structural unit of formula (I) independently selected from the group consisting of alkyl groups and phenyl groups, and a structural unit of formula (II) in an amount of 1 to less than 50% by weight, based on the weight of the adhesion aid polymer, [ka] In the formula, each R 2 However, it is independently selected from the group consisting of parts (III), (IV), and (V), [ka] In the formula, A - However, these are counter anions that balance the cation charge on N, and each R 4 However, hydrogen, -C 1-12 A group consisting of alkyl groups and phenyl groups is independently selected, and each R 5 However, hydrogen and -C 1-8 The present invention provides a laundry adhesive polymer comprising a structural unit of formula (II), independently selected from the group consisting of alkyl groups, wherein the adhesive polymer has a weight-average molecular weight of less than 100,000 daltons, provided that the adhesive polymer has an average of at least two structural units of formula (II) per molecule. [Modes for carrying out the invention]
[0007] Surprisingly, the adhesion-enhancing polymers described herein, having a weight-average molecular weight of less than 100,000 daltons, have been found to be highly effective in significantly improving the adhesion efficiency of fabric care beneficial agents (e.g., hydrophobic poly(dimethylsiloxane) fabric conditioners).
[0008] Unless otherwise specified, ratios, percentages, parts, etc., are expressed by weight. Weight percentages (or weight %) in a composition are percentages of dry weight, i.e., excluding any water that may be present in the composition.
[0009] Where used herein, unless otherwise specified, "weight-average molecular weight" and "M" refer to the same thing. wThe term "weight-average molecular weight" is used interchangeably to refer to weight-average molecular weight when measured in the conventional manner using gel permeation chromatography (GPC) and conventional standards such as polystyrene standards. GPC techniques are discussed in detail in *Modern Size Exclusion Liquid Chromatography: Practice of Gel Permeation and Gel Filtration Chromatography*, Second Edition, Striegel, et al., John Wiley & Sons, 2009. Weight-average molecular weight is reported herein in units of Daltons.
[0010] As used herein and in the appended claims, the term “structural unit” refers to a remnant of a given raw material, and therefore the structural unit of ethylene oxide is shown below. [ka] In the formula, the dotted line represents the bond point to the polymer backbone, R 1 It is hydrogen.
[0011] Preferably, the laundry adhesive polymer of the present invention comprises (a) structural units of formula (I) in an amount of more than 50 to 99% by weight (preferably 60 to 98% by weight, more preferably 75 to 97% by weight, even more preferably 82 to 96% by weight, most preferably 90 to 95% by weight) based on the weight of the adhesive polymer, [ka] In the formula, each R 1 However, hydrogen, -C 1-4 Alkyl groups, and -CH2OR 3 Group (preferably hydrogen, -C) 1-4 Alkyl groups, and mixtures thereof, more preferably hydrogen, -C 1-2 A alkyl group and mixtures thereof, more preferably hydrogen, a methyl group and mixtures thereof, most preferably hydrogen) is independently selected from the group, and each R 3However, -C 1-12 A structural unit of formula (I) independently selected from the group consisting of alkyl groups and phenyl groups, and a structural unit of formula (II) in an amount of 1 to less than 50% by weight (preferably 2 to 40% by weight, more preferably 3 to 25% by weight, even more preferably 4 to 18% by weight, most preferably 5 to 10% by weight) based on the weight of the adhesion aid polymer, [ka] In the formula, each R 2 However, it is independently selected from the group consisting of parts (III), (IV), and (V), [ka] In the formula, A - However, N is a counter anion that balances the cation charge, and each R 4 However, hydrogen, -C 1-12 Alkyl groups, and phenyl groups (preferably hydrogen and -C) 1-12 Alkyl alkyl groups, more preferably hydrogen and -C 1-4 Alkyl alkyl groups, more preferably hydrogen and -C 1-2 A alkyl group (most preferably hydrogen and methyl group) is independently selected from the group, and each R 5 However, hydrogen and -C 1-8 Alkyl alkyl groups (preferably hydrogen and -C) 1-4 The adhesion aid polymer comprises a structural unit of formula (II), independently selected from the group consisting of alkyl groups, more preferably hydrogen and methyl groups, most preferably hydrogen, and the adhesion aid polymer has a weight-average molecular weight of less than 100,000 daltons, provided that the adhesion aid polymer has an average of at least two (preferably 2.5 to 300, more preferably 3 to 50, even more preferably 3 to 20, most preferably 3.5 to 15) structural units of formula (II) per molecule.
[0012] Preferably, the laundry adhesive polymer of the present invention has a weight-average molecular weight of less than 100,000 daltons, M WThe present invention has the following characteristics. More preferably, the laundry adhesive polymer of the present invention has a weight-average molecular weight of 2,000 to 90,000 Daltons. Even more preferably, the laundry adhesive polymer of the present invention has a weight-average molecular weight of 2,500 to 75,000 Daltons. Even more preferably, the laundry adhesive polymer of the present invention has a weight-average molecular weight of 3,000 to 50,000 Daltons. Most preferably, the laundry adhesive polymer of the present invention has a weight-average molecular weight of 12,000 to 30,000 Daltons.
[0013] Preferably, the laundry adhesion additive polymer of the present invention comprises, based on the weight of the adhesion additive polymer, more than 50 to 99% by weight (preferably 60 to 98% by weight, more preferably 75 to 97% by weight, even more preferably 82 to 96% by weight, most preferably 90 to 95% by weight) of structural units of formula (I), where each R 1 is hydrogen, -C 1-4 Alkyl groups, and -CH2OR 3 Independently selected from the group consisting of elements, each R 3 is -C 1-12 A group is independently selected from the group consisting of alkyl groups and phenyl groups. More preferably, the laundry adhesion polymer of the present invention comprises more than 50 to 99% by weight (preferably 60 to 98% by weight, more preferably 75 to 97% by weight, even more preferably 82 to 96% by weight, most preferably 90 to 95% by weight) of structural units of formula (I), based on the weight of the adhesion polymer, where each R 1 is hydrogen, -C 1-4 A alkyl group and mixtures thereof are independently selected. More preferably, the laundry adhesion polymer of the present invention comprises more than 50 to 99% by weight (preferably 60 to 98% by weight, more preferably 75 to 97% by weight, even more preferably 82 to 96% by weight, most preferably 90 to 95% by weight) of structural units of formula (I), based on the weight of the adhesion polymer, where each R 1 is hydrogen, -C 1-2A alkyl group and mixtures thereof are independently selected. More preferably, the laundry adhesion polymer of the present invention comprises more than 50 to 99% by weight (preferably 60 to 98% by weight, more preferably 75 to 97% by weight, even more preferably 82 to 96% by weight, most preferably 90 to 95% by weight) of structural units of formula (I), based on the weight of the adhesion polymer, where each R 1 R is independently selected from the group consisting of hydrogen, methyl groups, and mixtures thereof. Most preferably, the laundry adhesion polymer of the present invention comprises more than 50 to 99% by weight (preferably 60 to 98% by weight, more preferably 75 to 97% by weight, even more preferably 82 to 96% by weight, most preferably 90 to 95% by weight) of structural units of formula (I), based on the weight of the adhesion polymer, where each R 1 It is independently selected from the group consisting of hydrogen atoms.
[0014] Preferably, the laundry adhesive polymer of the present invention contains 1 to less than 50% by weight (preferably 2 to 40% by weight, more preferably 3 to 25% by weight, even more preferably 4 to 18% by weight, most preferably 5 to 10% by weight) of structural units of formula (II), where each R 2 It is independently selected from the group consisting of parts of equation (III), equation (IV), and equation (V), A - is a counter anion that balances the cation charge on N (preferably A - Cl - F - , Br - , and I - , more preferably, Cl - and Br - Most preferably, Cl - (Selected from the group consisting of), each R 4 is hydrogen, -C 1-12 Alkyl groups, and phenyl groups (preferably hydrogen and -C) 1-12 Alkyl alkyl groups, more preferably hydrogen and -C 1-4 Alkyl alkyl groups, more preferably hydrogen and -C 1-2A alkyl group (most preferably hydrogen and methyl group) is independently selected from the group, and each R 5 is hydrogen and -C 1-8 Alkyl alkyl groups (preferably hydrogen and -C) 1-4 A structural unit of formula (II) is independently selected from the group consisting of alkyl groups, more preferably hydrogen and methyl groups, most preferably hydrogen, provided that the adhesion-enhancing polymer has an average of at least two (preferably 2.5 to 300, more preferably 3 to 50, even more preferably 3 to 20, most preferably 3.5 to 15) structural units of formula (II) per molecule. More preferably, the laundry adhesion-enhancing polymer of the present invention contains 1 to less than 50% by weight (preferably 2 to 40% by weight, more preferably 3 to 25% by weight, even more preferably 4 to 18% by weight, most preferably 5 to 10% by weight) of structural units of formula (II) based on the weight of the adhesion-enhancing polymer, where each R 2 These are independently selected from the group consisting of parts of equation (III) and equation (IV), and each R 4 is hydrogen, -C 1-12 Alkyl alkyl group (preferably -C) 1-8 Alkyl alkyl group, more preferably -C 1-4 The adhesion promoter polymer is independently selected from the group consisting of alkyl groups (most preferably methyl groups) and phenyl groups, provided that the polymer has an average of at least two (preferably 2.5 to 300, more preferably 3 to 50, even more preferably 3 to 20, most preferably 3.5 to 15) structural units of formula (II) per molecule. Preferably, R 2 If is the part of equation (III), then R 4 At least one of the groups (preferably at least two, more preferably all three) is -C 1-12 Alkyl alkyl group (preferably -C) 1-4 Alkyl alkyl group, more preferably -C 1-2 Alkyl group, most preferably methyl group. Preferably R 2 If is the part of equation (IV), then R 4 At least one (preferably both) of the groups is -C 1-12 Alkyl alkyl group (preferably -C) 1-4an alkyl group, more preferably, -C 1-2 an alkyl group, most preferably, a methyl group). Most preferably, the laundry adhesion aid polymer of the present invention contains 1 to less than 50% by weight (preferably 2 to 4% by weight, more preferably 3 to 25% by weight, even more preferably 4 to 18% by weight, most preferably 5 to 10% by weight) of the structural unit of formula (II) based on the weight of the adhesion aid polymer, wherein each R 2 is a moiety of formula (IV), and at least one (preferably both) of the R 4 groups is -C 1-12 an alkyl group (preferably -C 1-4 an alkyl group, more preferably, -C 1-2 an alkyl group, most preferably, a methyl group), provided that the adhesion aid polymer has an average of at least two (preferably 2.5 to 300, more preferably 3 to 50, even more preferably 3 to 20, most preferably 3.5 to 15) structural units of formula (II) per molecule.
[0015] Preferably, the laundry adhesive polymer of the present invention contains an active moiety capable of forming covalent bonds with cellulose (e.g., azetidinium groups, epoxide groups, halomethyl groups (e.g., chloromethyl moieties, fluoromethyl moieties)) in an amount of 1% by weight or less, based on the weight of the adhesive polymer. More preferably, the laundry adhesive polymer of the present invention contains an active moiety capable of forming covalent bonds with cellulose (e.g., azetidinium groups, epoxide groups, halomethyl groups (e.g., chloromethyl moieties, fluoromethyl moieties)) in an amount of 0.5% by weight or less, based on the weight of the adhesive polymer. Even more preferably, the laundry adhesive polymer of the present invention contains an active moiety capable of forming covalent bonds with cellulose (e.g., azetidinium groups, epoxide groups, halomethyl groups (e.g., chloromethyl moieties, fluoromethyl moieties)) in an amount of 0.2% by weight or less, based on the weight of the adhesive polymer. More preferably, the laundry adhesive polymer of the present invention contains an active moiety capable of forming covalent bonds with cellulose (e.g., azetidinium groups, epoxide groups, halomethyl groups (e.g., chloromethyl moieties, fluoromethyl moieties)) in an amount of 0.1% by weight or less, based on the weight of the adhesive polymer. Even more preferably, the laundry adhesive polymer of the present invention contains an active moiety capable of forming covalent bonds with cellulose (e.g., azetidinium groups, epoxide groups, halomethyl groups (e.g., chloromethyl moieties, fluoromethyl moieties)) in an amount of 0.01% by weight or less, based on the weight of the adhesive polymer. Most preferably, the laundry adhesive polymer of the present invention contains an active moiety capable of forming covalent bonds with cellulose (e.g., azetidinium groups, epoxide groups, halomethyl groups (e.g., chloromethyl moieties, fluoromethyl moieties)) in an amount below the detectable limit.
[0016] Preferably, the laundry adhesive polymer of the present invention contains 1% by weight or less of a carboxylic acid portion, based on the weight of the adhesive polymer. More preferably, the laundry adhesive polymer of the present invention contains 0.5% by weight or less of a carboxylic acid portion, based on the weight of the adhesive polymer. Even more preferably, the laundry adhesive polymer of the present invention contains 0.2% by weight or less of a carboxylic acid portion, based on the weight of the adhesive polymer. Even more preferably, the laundry adhesive polymer of the present invention contains 0.1% by weight or less of a carboxylic acid portion, based on the weight of the adhesive polymer. Even more preferably, the laundry adhesive polymer of the present invention contains 0.01% by weight or less of a carboxylic acid portion, based on the weight of the adhesive polymer. Most preferably, the laundry adhesive polymer of the present invention contains a carboxylic acid portion below the detectable limit.
[0017] Preferably, the laundry adhesive polymer of the present invention contains 1% by weight or less of a carbonyl portion, based on the weight of the adhesive polymer. More preferably, the laundry adhesive polymer of the present invention contains 0.5% by weight or less of a carbonyl portion, based on the weight of the adhesive polymer. Even more preferably, the laundry adhesive polymer of the present invention contains 0.2% by weight or less of a carbonyl portion, based on the weight of the adhesive polymer. Even more preferably, the laundry adhesive polymer of the present invention contains 0.1% by weight or less of a carbonyl portion, based on the weight of the adhesive polymer. Even more preferably, the laundry adhesive polymer of the present invention contains 0.01% by weight or less of a carbonyl portion, based on the weight of the adhesive polymer. Most preferably, the laundry adhesive polymer of the present invention contains a carbonyl portion below the detectable limit.
[0018] Preferably, the laundry adhesive polymer of the present invention comprises (a) 82 to 96% by weight of structural units of formula (I) based on the weight of the adhesive polymer, where each R 1 However, hydrogen and -C 1-4 A structural unit of formula (I) independently selected from the group consisting of alkyl groups, and a structural unit of formula (II) in an amount of 4 to 18% by weight based on the weight of the adhesion-enhancing polymer, wherein each R2 is independently selected from the group consisting of the moiety of formula (III) and the moiety of formula (IV), each R 4 is independently selected from the group consisting of hydrogen and -C 1-8 alkyl group, and the structural unit of formula (II), and the adhesion aid polymer contains an azetidinium moiety, a carboxylic acid moiety, a carbonyl moiety, and a halomethyl moiety (e.g., chloromethyl moiety, fluoromethyl moiety) below the detectable limit. The adhesion aid polymer has a weight average molecular weight of 5,000 to 30,000 daltons, provided that the adhesion aid polymer has an average of at least 2 (preferably 2.5 to 300, more preferably 3 to 50, even more preferably 3 to 20, most preferably 3.5 to 15) structural units of formula (II) per molecule. More preferably, the laundry adhesion aid polymer of the present invention comprises (a) 82 to 96% by weight of the structural unit of formula (I) based on the weight of the adhesion aid polymer, wherein each R 1 is independently selected from hydrogen and a methyl group, the structural unit of formula (I), and (b) 4 to 18% by weight of the structural unit of formula (II) based on the weight of the adhesion aid polymer, wherein each R 2 is independently selected from the group consisting of the moiety of formula (III) and the moiety of formula (IV), each R 4 is a methyl group, the structural unit of formula (II), and the adhesion aid polymer contains an azetidinium moiety, a carboxylic acid moiety, a carbonyl moiety, and a halomethyl moiety (e.g., chloromethyl moiety, fluoromethyl moiety) below the detectable limit. The adhesion aid polymer has a weight average molecular weight of 5,000 to 30,000 daltons, provided that the adhesion aid polymer has an average of at least 2 (preferably 2.5 to 300, more preferably 3 to 50, even more preferably 3 to 20, most preferably 3.5 to 15) structural units of formula (II) per molecule. Most preferably, the laundry adhesion aid polymer of the present invention comprises (a) 82 to 96% by weight of the structural unit of formula (I) based on the weight of the adhesion aid polymer, wherein each R 1 is hydrogen, the structural unit of formula (I), and (b) 4 to 18% by weight of the structural unit of formula (II) based on the weight of the adhesion aid polymer, wherein each R2 However, this is the part of equation (IV), and each R 4 The adhesion aid polymer contains a methyl group, which is a structural unit of formula (II), and the adhesion aid polymer contains azetidinium moieties, carboxylic acid moieties, carbonyl moieties, and halomethyl moieties (e.g., chloromethyl moieties, fluoromethyl moieties) below the detectable limit, and the adhesion aid polymer has a weight-average molecular weight of 5,000 to 30,000 daltons, provided that the adhesion aid polymer has an average of at least two (preferably 2.5 to 300, more preferably 3 to 50, even more preferably 3 to 20, and most preferably 3.5 to 15) structural units of formula (II) per molecule.
[0019] Several embodiments of the present invention will be described in detail in the following examples.
[0020] The abbreviations listed in the table below will be used in the examples. [Table 1] Analysis method: Molecular weight analysis of epichlorohydrin copolymers: [Table 2]
[0021] Molecular weight analysis of amine-functionalized copolymers: All samples were prepared at 5 mg / mL in a GPC mobile phase. The exact concentration of each sample was recorded. The samples were shaken in a horizontal shaker at ambient temperature for at least 2 hours to facilitate the dissolution process. The prepared samples were then filtered into autosampler vials using a 45 μm nylon syringe filter and injected. No resistance was observed during the filtration process for any of the exemplified amine-functionalized polymers.
[0022] The GPC instrument setup used consisted of a Waters Alliance 2690 separation module (degassa, pump, autosampler, column oven) and a Wyatt Optilab UT-rEX refractive index detector (RI). A Waters e-SAT / IN module was used to convert the analog signal from the RI detector into a digital signal for data acquisition. An Empower 3 was used for data acquisition and processing.
[0023] GPC conditions: [Table 3]
[0024] NMR analysis of ECH copolymer: All samples were prepared at 5 mg / mL in a GPC mobile phase. The exact concentration of each sample was recorded. The samples were shaken in a horizontal shaker at ambient temperature for at least 2 hours to facilitate the dissolution process. The prepared samples were then filtered into autosampler vials using a 45 μm nylon syringe filter and injected. No resistance was observed during the filtration process for any of the exemplified amine-functionalized polymers.
[0025] Molecular weight analysis of amine-functionalized copolymers: Sample preparation: 500 mg of the sample was dissolved in 2.2 mL of acetone-d6 containing 5 mM mitigating agent to form a homogeneous solution, which was then transferred to a 10 mm NMR tube. Quantitative analysis 13 ¹³C NMR spectroscopy was performed using a Bruker 600 MHz spectrometer equipped with a 10 mm cryogenic probe, with the following parameters. Pulsed magnetic field gradient NMR allowed for molecular weight quantification using a 0.1 wt% solution in CDCl3 containing 2 mM relaxant by diffusion measurement. Diffusion measurement was performed using a 400 MHz instrument equipped with a 5 mm BBO probe. Repetition time: 7 seconds, scans: 128, 90° pulse: 12 μs, T: 25°C, spectral width: 240 ppm, spectral center: 90 ppm. XPS analysis of cotton fabrics: [Table 4]
[0026] Example P1: EO-ECH polymer ECH (4.63 mL) and toluene (150 mL) were charged into a syringe under an inert atmosphere, capped with a sealed GC vial, and then added to a 300 mL stainless steel pressure reactor equipped with a stirrer utilizing a gas-entrained impeller blade. The temperature was controlled at the mantle via resistance heating and cooling water supplied through an internal cooling loop using a research control valve. The reactor was dried at 100°C and completely purged with nitrogen. The reactor was pressurized with approximately 15 psig of nitrogen, followed by the addition of EO (8.85 mL) using a Camille reactor control system. The reaction mixture was heated to 40°C. A catalyst mixture in toluene (6 mL) was prepared in a glove box from TiBA (25% in toluene, 2.48 g) and triethylamine (79 mg), taken into a syringe, capped, and removed from the box. The catalyst mixture was added to a shot tank and charged into the reactor.
[0027] An immediate exothermic reaction of approximately 4°C was observed, and approximately 9 mL of EO was added to maintain the pressure for about 1 hour. Next, the mixture was quenched by adding ethanol (6 mL) via a shot tank. After cooling to RT and purging with nitrogen, the mixture was removed from the reactor and concentrated in a rotary evaporator. The mixture was transferred to a jar and further dried at 50°C using a glove box vacuum pump. The product polymer (12.2 g) was isolated. The ECH content of the polymer was quantitatively determined. 13 ¹³C NMR revealed that the polymer content was 16% by weight. GPC revealed that the polymer content was 16% by weight. w and M n These values were 11.9 and 2.9 kDa, respectively.
[0028] Example P2: EO-ECH polymer ECH (1.54 mL) and toluene (150 mL) were charged into a syringe under an inert atmosphere, capped with a sealed GC vial, and then added to a 300 mL stainless steel pressure reactor equipped with a stirrer utilizing a gas-entrained impeller blade. The temperature was controlled at the mantle via resistance heating and cooling water supplied through an internal cooling loop using a research control valve. The reactor was dried at 100°C and completely purged with nitrogen. The reactor was pressurized with approximately 15 psig of nitrogen, followed by the addition of EO (8.85 mL) using a Camille reactor control system. The reaction mixture was heated to 40°C. A catalyst mixture in toluene (8 mL) was prepared in a glove box from TiBA (25% in toluene, 1.86 g) and tetraoctylammonium bromide (427 mg), taken into a syringe, capped, and removed from the box. The catalyst mixture was added to a shot tank and charged into the reactor.
[0029] An immediate exothermic reaction of approximately 3°C was observed, and approximately 9 mL of EO was added to maintain the pressure for about 1 hour. Next, the mixture was quenched by adding ethanol (6 mL) via a shot tank. After cooling to RT and purging with nitrogen, the mixture was removed from the reactor and concentrated in a rotary evaporator. The mixture was transferred to a jar and further dried at 50°C using a glove box vacuum pump. The product polymer (14.0 g) was isolated. The ECH content of the polymer was quantitatively determined. 13 ¹³C NMR revealed that the polymer content was 6.4% by weight. GPC analysis revealed that the polymer content was 6.4% by weight. w and M n These values were 25.6 and 9.3 kDa, respectively.
[0030] Example P3: EO-ECH polymer ECH (3.09 mL) and toluene (150 mL) were charged into a syringe under an inert atmosphere, capped with a sealed GC vial, and then added to a 300 mL stainless steel pressure reactor equipped with a stirrer utilizing a gas-entrained impeller blade. The temperature was controlled at the mantle via resistance heating and cooling water supplied through an internal cooling loop using a research control valve. The reactor was dried at 100°C and completely purged with nitrogen. The reactor was pressurized with approximately 15 psig of nitrogen, followed by the addition of EO (8.85 mL) using a Camille reactor control system. The reaction mixture was heated to 40°C. A catalyst mixture in toluene (8 mL) was prepared in a glove box from TiBA (25% in toluene, 3.71 g) and tetraoctylammonium bromide (853 mg), taken into a syringe, capped, and removed from the box. The catalyst mixture was added to a shot tank and charged into the reactor.
[0031] An immediate exothermic reaction of approximately 3°C was observed, and approximately 9 mL of EO was added to maintain the pressure for about 1 hour. Next, the mixture was quenched by adding ethanol (6 mL) via a shot tank. After cooling to RT and purging with nitrogen, the mixture was removed from the reactor and concentrated in a rotary evaporator. The mixture was transferred to a jar and further dried at 50°C using a glove box vacuum pump. The product polymer (7.4 g) was isolated. The ECH content of the polymer was quantitatively determined. 13 ¹³C NMR revealed that the polymer content was 10.6% by weight. GPC analysis revealed that the polymer content was 10.6% by weight. w and M n These values were 9.9 and 3.1 kDa, respectively.
[0032] Example P4: EO-ECH polymer ECH (9.26 mL) and toluene (150 mL) were charged into a syringe under an inert atmosphere, capped with a sealed GC vial, and then added to a 300 mL stainless steel pressure reactor equipped with a stirrer utilizing a gas-entrained impeller blade. The temperature was controlled at the mantle via resistance heating and cooling water supplied through an internal cooling loop using a research control valve. The reactor was dried at 100°C and completely purged with nitrogen. The reactor was pressurized with approximately 15 psig of nitrogen, followed by the addition of EO (8.85 mL) using a Camille reactor control system. The reaction mixture was heated to 40°C. A catalyst mixture in toluene (8 mL) was prepared in a glove box from TiBA (25% in toluene, 3.71 g) and tetraoctylammonium bromide (853 mg), taken into a syringe, capped, and removed from the box. The catalyst mixture was added to a shot tank and charged into the reactor.
[0033] An immediate exothermic reaction of approximately 3°C was observed, and approximately 9 mL of EO was added to maintain the pressure for about 1 hour. Next, the mixture was quenched by adding ethanol (6 mL) via a shot tank. After cooling to RT and purging with nitrogen, the mixture was removed from the reactor and concentrated in a rotary evaporator. The mixture was transferred to a jar and further dried at 50°C using a glove box vacuum pump. The product polymer (19.2 g) was isolated. The ECH content of the polymer was quantitatively determined. 13 ¹
[0034] Example P5: EO-PO-ECH polymer ECH (3.09 mL), PO (8.26 mL), and toluene (150 mL) were charged into a syringe under an inert atmosphere, capped with a sealed GC vial, and then added to a 300 mL stainless steel pressure reactor equipped with a stirrer utilizing a gas-entrained impeller blade. The temperature was controlled at the mantle via resistance heating and cooling water supplied through an internal cooling loop using a research control valve. The reactor was dried at 100°C and completely purged with nitrogen. The reactor was pressurized with approximately 15 psig of nitrogen, followed by the addition of EO (8.85 mL) using a Camille reactor control system. The reaction mixture was heated to 40°C. A catalyst mixture in toluene (8 mL) was prepared in a glove box from TiBA (25% in toluene, 3.71 g) and tetraoctylammonium bromide (853 mg), taken into a syringe, capped, and removed from the box. The catalyst mixture was added to a shot tank and charged into the reactor.
[0035] No exothermic reaction was observed, and the reactor pressure was kept constant. The mixture was heated to 60°C and held for 72 hours. The mixture was cooled, evacuated, and purged with nitrogen. The mixture was transferred to a jar and further dried at 60°C using a glove box vacuum pump. The product polymer (12.0 g) was isolated.
[0036] Example P6: Amine reaction EO-ECH polymer A Fisher-Porter tube containing a PTFE-coated magnetic stirring rod was loaded with 8.64 g of copolymer prepared according to Example P1 and 7.81 mL of a 45 wt% trimethylamine solution. The solution was stirred, and 20 mL of distilled water was added to adjust the polymer concentration. The Fisher-Porter tube was sealed, and the mixture was stirred at 125°C for 16 hours. The solution was then cooled to room temperature, and the pressure tube was evacuated. Excess amine was removed by bubbling nitrogen into the solution for 1 hour. The solvent was evaporated under reduced pressure, and the crude polymer was incorporated into the minimum amount of methanol. The solution was added to diethyl ether (10 times the amount of methanol) with vigorous stirring to precipitate the polymer. The polymer was isolated as a brown oil (9.55 g). Quantitative analysis 1313C NMR revealed that the copolymer contained 77% by weight of EO and 23% by weight of N,N,N-trimethyl-2-oxiramethaneaminium chloride.
[0037] Example P7: Amine reaction EO-ECH polymer A Fisher-Porter tube containing a PTFE-coated magnetic stirring rod was loaded with 5.00 g of copolymer prepared according to Example P2 and 3.25 mL of a 45 wt% trimethylamine solution. The solution was stirred, and 15 mL of distilled water was added to adjust the polymer concentration. The Fisher-Porter tube was sealed, and the mixture was stirred at 125°C for 16 hours. The solution was then cooled to room temperature, and the pressure tube was evacuated. Excess amine was removed by bubbling nitrogen into the solution for 1 hour. The solvent was evaporated under reduced pressure, and the crude polymer was incorporated into a minimum amount of methanol. The solution was added to diethyl ether (10 times the amount of methanol) with vigorous stirring to precipitate the polymer. The polymer was isolated as an off-white powder (4.44 g). Polymer M by SEC w and M n These values were 25.9 and 13.5 kDa, respectively. Quantitative 13 13C NMR revealed that the copolymer contained 93% by weight of EO and 7% by weight of N,N,N-trimethyl-2-oxiramethaneaminium chloride.
[0038] Example P8: Amine reaction EO-ECH polymer A Fisher-Porter tube containing a PTFE-coated magnetic stirring rod was loaded with 5.00 g of copolymer prepared according to Example P2 and 2.72 mL of a 45 wt% trimethylamine solution. The solution was stirred, and 15 mL of distilled water was added to adjust the polymer concentration. The Fisher-Porter tube was sealed, and the mixture was stirred at 125°C for 16 hours. The solution was then cooled to room temperature, and the pressure tube was evacuated. Excess amine was removed by bubbling nitrogen into the solution for 1 hour. The solvent was evaporated under reduced pressure, and the crude polymer was incorporated into the minimum amount of methanol. The solution was added to diethyl ether (10 times the amount of methanol) with vigorous stirring to precipitate the polymer. The polymer was isolated as an off-white powder (4.77 g). Polymer M by SEC w and M n These values were 37.4 and 17.9 kDa, respectively. Quantitative 13 13C NMR revealed that the copolymer contained 92% by weight of EO and 8% by weight of N,N-dimethyl-2-oxiranmethaneaminium chloride.
[0039] Example P9: Amine reaction EO-ECH polymer A Fisher-Porter tube containing a PTFE-coated magnetic stirring rod was loaded with 5.32 g of copolymer prepared according to Example P3 and 5.67 mL of a 45 wt% trimethylamine solution. The solution was stirred, and 15 mL of distilled water was added to adjust the polymer concentration. The Fisher-Porter tube was sealed, and the mixture was stirred at 125°C for 16 hours. The solution was then cooled to room temperature, and the pressure tube was evacuated. Excess amine was removed by bubbling nitrogen into the solution for 1 hour. The solvent was evaporated under reduced pressure, and the crude polymer was incorporated into a minimum amount of methanol. The solution was added to diethyl ether (10 times the amount of methanol) with vigorous stirring to precipitate the polymer. The polymer was isolated as a light brown oil (5.12 g). Polymer M by SEC w and M n These values were 14.9 and 7.7 kDa, respectively. Quantitative 1313C NMR revealed that the copolymer contained 83% by weight of EO and 17% by weight of N,N,N-trimethyl-2-oxiramethaneaminium chloride.
[0040] Example P10: Amine reaction EO-ECH polymer A Fisher-Porter tube containing a PTFE-coated magnetic stirring rod was loaded with 5.56 g of copolymer prepared according to Example P4 and 15.5 mL of a 45 wt% trimethylamine solution. The solution was stirred, and 10 mL of distilled water was added to adjust the polymer concentration. The Fisher-Porter tube was sealed, and the mixture was stirred at 125°C for 16 hours. The solution was then cooled to room temperature, and the pressure tube was evacuated. Excess amine was removed by bubbling nitrogen into the solution for 1 hour. The solvent was evaporated under reduced pressure, and the crude polymer was incorporated into a minimum amount of methanol. The solution was added to diethyl ether (10 times the amount of methanol) with vigorous stirring to precipitate the polymer. The polymer was isolated as a light brown oil (6.01 g). Polymer M by SEC w and M n These values were 16.9 and 6.9 kDa, respectively. Quantitative 13 13C NMR revealed that the copolymer contained 62% by weight of EO and 38% by weight of N,N,N-trimethyl-2-oxiramethaneaminium chloride.
[0041] Example P11: Amine reaction EO-ECH polymer A Fisher-Porter tube containing a PTFE-coated magnetic stirring rod was loaded with 5.50 g of terpolymer prepared according to Example P5 and 10.5 mL of a 45 wt% trimethylamine solution. The solution was stirred, and 15 mL of distilled water was added to adjust the polymer concentration. The Fisher-Porter tube was sealed, and the mixture was stirred at 125°C for 16 hours. The solution was then cooled to room temperature, and the pressure tube was evacuated. Excess amine was removed by bubbling nitrogen into the solution for 1 hour. The solvent was evaporated under reduced pressure, and the crude polymer was incorporated into a minimum amount of methanol. The solution was added to diethyl ether (10 times the amount of methanol) with vigorous stirring to precipitate the polymer. The polymer was isolated as a light brown oil (6.13 g). Polymer M by SEC w and M n These values were 2.1 and 1.5 kDa, respectively. Quantitative 13 13C NMR revealed that the copolymer contained 62 wt% EO, 13 wt% PO, and 25 wt% N,N,N-trimethyl-2-oxiramethaneaminium chloride.
[0042] Comparative Example C1 and Examples 1-4: Liquid Laundry Detergents The liquid laundry detergent formulations used in the adhesion tests of the subsequent examples were prepared by adding the adhesion-enhancing polymers shown in Table 2 to the general formulations listed in Table 1, and by following the standard procedure for preparing liquid laundry formulations. [Table 5] [Table 6]
[0043] Silicone adhesion The silicone adhesion of the liquid laundry detergent formulations of Comparative Example C1 and Examples 1-4 was evaluated using a Terg-o-tometer model TOM-52-A (6 x 1L wells) available from SR Lab Instruments, agitated at 90 cycles per minute under the conditions shown in Table 3. [Table 7]
[0044] Next, the fabric samples were dried and analyzed by X-ray photoelectron spectroscopy (XPS) to quantify the silicone adhering to the surface. The XPS results for the weight percentage of Si adhering are shown in Table 4.
[0045] Next, friction measurements of the fabric sample were obtained using the friction metering apparatus described in Kalihari et al., Rev.Sci.Instrum. 2013, 84, 035104. The fabric sample was attached to a glass substrate using double-sided tape and fixed to a unidirectional sliding deck. A 3 / 8-inch rigid nylon sphere was placed in contact with the fabric surface with an applied vertical force, and the lateral force was measured when the fabric-covered glass substrate was pulled unilaterally across the surface of the sphere. This process was performed with three forces using multiple replicas. The coefficient of friction was determined by calculating the gradient between the measured lateral force and the applied vertical force. The results are reported in Table 4. [Table 8]
Claims
1. 1. A laundry deposition aid polymer comprising: (a) greater than 50 to 99 wt. % of structural units of formula (I), based on the weight of the deposition aid polymer, 【Chemistry 1】 In the formula, each R 1 is hydrogen, -C 1-4 Alkyl groups, and -CH 2 OR 3 groups, and each R 3 But, -C 1-12 Structural units of formula (I) independently selected from the group consisting of alkyl groups and phenyl groups; (b) 1 to less than 50 wt. % of structural units of formula (II), based on the weight of the deposition aid polymer, 【Chemistry 2】 In the formula, each R 2 is independently selected from the group consisting of a moiety of formula (III), a moiety of formula (IV), and a moiety of formula (V); 【Transformation 3】 In the formula, A - is the counter anion that balances the cationic charge on N, and each R 4 is hydrogen, -C 1-12 alkyl groups, and phenyl groups; 5 is hydrogen and -C 1-8 and structural units of formula (II) independently selected from the group consisting of alkyl groups, the deposition aid polymer has a weight average molecular weight of less than 100,000 Daltons; The deposition aid polymer, provided that said deposition aid polymer has an average of at least two structural units of formula (II) per molecule.
2. 10. The deposition aid polymer of claim 1, wherein the deposition aid polymer contains less than detectable limits of azetidinium moieties.
3. 3. The deposition aid polymer of claim 2, wherein the deposition aid polymer contains less than the detectable limit of epoxide moieties.
4. 4. The deposition aid polymer of claim 3, wherein the deposition aid polymer contains less than the detectable limit of halomethyl moieties.
5. The deposition aid polymer of claim 4 , wherein the deposition aid polymer contains less than the detectable limit of carboxylic acid moieties.
6. 6. The deposition aid polymer of claim 5, wherein the deposition aid polymer contains less than the detectable limit of carbonyl moieties.
7. The deposition aid polymer of claim 6, wherein the deposition aid polymer has a weight average molecular weight of 5,000 to 30,000 daltons.
8. The adhesion aid polymer (a) 82 to 96 weight percent, based on the weight of the deposition aid polymer, of structural units of formula (I), wherein each R 1 is hydrogen and -C 1-4 Structural units of formula (I) independently selected from alkyl groups; (b) 4 to 18 weight percent, based on the weight of the deposition aid polymer, of structural units of formula (II), where each R 2 and structural units of formula (II) independently selected from the group consisting of moieties of formula (III) and moieties of formula (IV).
9. Each R 1 are independently selected from hydrogen and a methyl group; Each R 4 But -CH 3 The deposition aid polymer of claim 8, wherein the R 1 -R 2 -R 3 -R 4 -R 5 -R 6 -R 7 -R 8 -R 9 -R 10 -R 11 -R 12 -R 13 -R 14 -R 15 -R 16 -R 17 -R 18 -R 19 -R 20 -R 21 -R 22 -R 23 -R 24 -R 25 -
10. Each R 1 is hydrogen, Each R 2 The deposition aid polymer of claim 9, wherein is a moiety of formula (IV).