Structure for sheet
Patent Information
- Application Number
- JP2023091408
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-06-06
- Filing Date
- 2023-06-02
- Publication Date
- 2024-10-23
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing sheets for roof repair, particularly those used on deteriorated artificial slate roofs, suffer from poor handling properties due to excessive stretching, which can lead to damage and alignment issues, and they do not adequately prevent leaks.
A structural sheet comprising a functional layer, an adhesive layer, and a reinforcing body, which provides enhanced tensile strength and resistance to stretching, ensuring easy handling and effective attachment to various structures.
The structural sheet maintains integrity under tension, preventing damage and facilitating easy alignment, while providing effective leak prevention and durability on roofs and other structures.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[Technical Field]
[0001] The present specification discloses a sheet that is attached to a structure when in use. [Background technology]
[0002] When artificial slate roofs are exposed to wind and rain for a long period of time, they deteriorate. Leaks from deteriorated roofs become a concern. To prevent leaks, paint is applied to the artificial slate. However, in cases where the artificial slate roof is severely deteriorated, applying paint may not prevent leaks.
[0003] International Patent Publication No. 2021 / 010456 discloses a sheet having a polymer cement layer and a resin layer. When this sheet is attached to a roof, it can suppress roof leaks. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] International Patent Publication 2021 / 010456 Summary of the Invention [Problem to be solved by the invention]
[0005] The sheet is applied to the roof by a worker under tension. This tension can cause the sheet to stretch. Excessive stretching can make it difficult for the worker to align the sheet. Stretching can also damage the sheet. The worker must handle the sheet carefully to avoid damage. The sheet disclosed in International Patent Publication No. 2021 / 010456 is difficult to handle. A sheet with excellent handleability is desired.
[0006] In the repair of roofs other than artificial slate roofs, there is also a demand for sheets with excellent handleability. In the repair or reinforcement of structures other than roofs, there is also a demand for sheets with excellent handleability.
[0007] The present applicant intends to provide a structural sheet that is easy to handle. [Means for solving the problem]
[0008] The structural sheet disclosed in the present specification has a functional layer, an adhesive layer, and a reinforcing body. [Effects of the Invention]
[0009] This structural sheet has a reinforcing member, so it is less likely to stretch or be damaged even when tension is applied, and is easy to handle. [Brief explanation of the drawings]
[0010] [Figure 1] FIG. 1 is a perspective view showing a portion of a structural sheet according to one embodiment. [Figure 2] FIG. 2 is a cross-sectional view taken along line II-II in FIG. [Figure 3] FIG. 3 is an enlarged view showing the portion indicated by reference numeral III in FIG. [Figure 4] FIG. 4 is a front view of the structural sheet of FIG. 1 shown together with a roof. [Figure 5] FIG. 5 is an enlarged view showing the portion marked with the symbol V in FIG. [Figure 6] FIG. 6 is an enlarged view showing the portion designated by reference numeral VI in FIG. [Figure 7] FIG. 7 is an enlarged plan view showing a part of a reinforcing body included in the structural sheet of FIG. [Figure 8] FIG. 8 is a cross-sectional view showing a part of a structural sheet according to another embodiment. DETAILED DESCRIPTION OF THE INVENTION
[0011] Hereinafter, preferred embodiments will be described in detail with reference to the drawings as appropriate.
[0012] [First embodiment] [Layer structure] 1-3 show a sheet 2 for structures. In FIG. 1, arrow X represents the width direction of the sheet 2, arrow Y represents the length direction of the sheet 2, and arrow Z represents the thickness direction of the sheet 2. The planar shape of this sheet 2 is generally rectangular. As is clear from FIG. 3, this sheet 2 has a functional layer 4, an intermediate layer 6, an adhesive layer 8, and a reinforcing body 10. The reinforcing body 10 is embedded in the intermediate layer 6. The materials of each layer will be described in detail later. This sheet 2 is attached to a structure. The sheet 2 may have release paper or a release film. The release paper and release film are laminated with the adhesive layer 8.
[0013] [Roof repair] A typical use of this structural sheet 2 is in repairing a roof 12. Figures 4-6 show a repaired roof 12. These figures show two sheets 2 (a first sheet 2a and a second sheet 2b) along with the roof 12. The specifications of the second sheet 2b are the same as those of the first sheet 2a. Examples of roofs 12 include artificial slate roofs, tile roofs, steel roofs (including folded-plate roofs), copper roofs, galvanized iron roofs, and concrete roofs.
[0014] In FIG. 4, the position of the lower edge 14a of the first sheet 2a is roughly aligned with the position of the lower end 16 of the roof 12. The first sheet 2a is attached as a whole to the roof 12. As shown in FIG. 5, the roof 12 has a step 18. The first sheet 2a is curved in the vicinity of the step 18. This curvature allows the first sheet 2a to follow the step 18.
[0015] As shown in Figure 6, the second sheet 2b overlaps the vicinity of the upper edge 20a of the first sheet 2a near its lower edge 14b. This overlap forms a seam 22. The portion of the second sheet 2b other than the seam 22 is attached to the roof 12. The upper edge 20a of the first sheet 2a forms a step 24 between the first sheet 2a and the roof 12. The second sheet 2b is curved near this step 24. This curvature allows the second sheet 2b to follow the step 24.
[0016] [Primer layer] The structural sheet 2 is usually attached to the roof 12 via a primer layer. In this specification, the phrase "the sheet is attached to the roof" also refers to the case where the sheet 2 is attached to the roof 12 via a primer layer or the like. The primer layer is not shown in Figures 5 and 6.
[0017] Preferably, the material of the primer layer is a curable resin composition. Examples of the curable resin include a thermosetting resin and a photocurable resin. A preferred curable resin is an epoxy compound. Examples of the epoxy compound include bisphenol A epoxy resin, bisphenol F epoxy resin, bisphenol S epoxy resin, orthocresol novolac epoxy resin, alicyclic epoxy resin, aliphatic epoxy resin, diglycidyl ethers of phenols, and diglycidyl ethers of alcohols.
[0018] Examples of curing agents for epoxy compounds include polyfunctional phenols, amines, polyamines, mercaptans, imidazoles, acid anhydrides, and phosphorus-containing compounds. Examples of polyfunctional phenols include monocyclic bifunctional phenols such as hydroquinone, resorcinol, and catechol; polycyclic bifunctional phenols such as bisphenol A, bisphenol F, naphthalenediols, and biphenols, as well as their halides and alkyl group-substituted derivatives. Further examples of polyfunctional phenols include novolaks and resols, which are polycondensates of phenols and aldehydes. Examples of amines include aliphatic or aromatic primary amines, secondary amines, tertiary amines, quaternary ammonium salts, and aliphatic cyclic amines; guanidines; and urea derivatives.
[0019] A combination of a bisphenol A epoxy or bisphenol F epoxy base resin and a polyamine or mercaptan curing agent is particularly preferred. The primer layer containing an epoxy resin may also contain additives such as a coupling agent, a viscosity modifier, and a curing accelerator.
[0020] The primer layer can be formed by applying a solution or emulsion containing an epoxy compound to the roof 12. A preferred example of the emulsion is a two-component reactive curing water-based epoxy resin emulsion (product name "Aronble Coat P-300") manufactured by Toagosei Co., Ltd.
[0021] The thickness of the primer layer in a wet state is preferably 50 μm or more and 300 μm or less. A primer layer having a thickness of 50 μm or more has excellent thickness uniformity. From this viewpoint, the thickness is more preferably 70 μm or more, and particularly preferably 80 μm or more. A primer layer having a thickness of 300 μm or less can suppress misalignment of the structural sheet 2 with the roof 12. From this viewpoint, the thickness is more preferably 270 μm or less, and particularly preferably 250 μm or less.
[0022] [Sheet tensile strength and elongation] The tensile strength of this structural sheet 2 is preferably 5.0 MPa or more. A sheet 2 with a tensile strength of 5.0 MPa or more is less likely to break even when tension is applied. This sheet 2 has excellent handleability. From this viewpoint, the tensile strength is more preferably 5.6 MPa or more, and particularly preferably 6.0 MPa or more. From the viewpoint of conformability, the tensile strength is preferably 10.0 MPa or less, more preferably 9.5 MPa or less, and particularly preferably 9.0 MPa or less.
[0023] The elongation at break of this structural sheet 2 is preferably 15.0% or less. A sheet 2 with an elongation of 15.0% or less is less likely to deform even when tension is applied. This sheet 2 has excellent handleability. From this viewpoint, the elongation is more preferably 13.0% or less, and particularly preferably 11.0% or less. From the viewpoint of conformability, the elongation is preferably 5.0% or more, more preferably 7.0% or more, and particularly preferably 8.5% or more.
[0024] In this specification, the tensile strength and elongation of the sheet 2 are measured in accordance with the general nonwoven fabric testing method specified in "JIS L1913:2010." Test pieces for measurement are cut out from the structural sheet 2 or its original roll. Five test pieces whose length direction coincides with the length direction of the structural sheet 2 or its original roll, and five test pieces whose length direction coincides with the width direction of the structural sheet 2 or its original roll, are used for measurement. The tensile strength and elongation are calculated by averaging the 10 measured values. Test pieces are cut out from a zone that includes all layers included in the sheet 2 (in this embodiment, the functional layer 4, intermediate layer 6, adhesive layer 8, and reinforcing body 10).
[0025] If it is difficult to cut out test pieces whose length direction coincides with the width direction of the structural sheet 2 or its original web, ten test pieces whose length direction coincides with the length direction of the structural sheet 2 or its original web are used for measurement. The ten measured values are averaged to calculate the tensile strength and elongation.
[0026] [Water vapor permeability] The water vapor permeability of the structural sheet 2 is 10 g / m 210 days or more is preferable. After this sheet 2 is attached to a structure, moisture contained in the structure or moisture present between the structure and the sheet 2 can be discharged through the sheet 2. This sheet 2 can inhibit corrosion of metals in the structure. This sheet 2 is also suitable for structures that contain moisture (for example, structures with insufficiently dried concrete). This sheet 2 is also suitable for installation in rainy weather. From these points of view, the water vapor transmission rate is set to 20 g / m 2 25g / m 2 1 day or more is particularly preferable. The water vapor transmission rate is 50 g / m 2 ·day or less is preferable.
[0027] [Feature Layer] As is clear from FIG. 3 , in this embodiment, the functional layer 4 is located at the top. In other words, when the sheet 2 is attached to a structure, the functional layer 4 is located farthest from the structure. The functional layer 4 contributes to the functions desired for the sheet 2. Examples of such functions include light resistance, weather resistance, heat resistance, abrasion resistance, chemical resistance, water impermeability, moisture impermeability, and moisture permeability. The functional layer 4 can contribute to one or more functions.
[0028] A preferred material for the functional layer 4 is a polymer composition. This functional layer 4 is generally flexible. The sheet 2 having this functional layer 4 can conform to the unevenness of the underlying surface. The polymer composition includes a base polymer. Synthetic resin, synthetic rubber, and natural rubber can be included as the base polymer in the composition. A functional layer 4 whose base polymer is a synthetic resin is also called a "resin layer."
[0029] If light resistance is desired for the functional layer 4, a base polymer that is resistant to degradation by ultraviolet light is preferred. Specifically, a polymer having a stronger bond energy than ultraviolet light (410 KJ / mol) is preferred. Examples of polymers that can contribute to the light resistance of the functional layer 4 and the flexibility of the sheet 2 include acrylic resin, acrylic urethane resin, acrylic silicone resin, fluororesin, flexible epoxy resin, and polybutadiene.
[0030] From the viewpoint of light resistance, a resin particularly suitable for the base polymer of the functional layer 4 is an acrylic silicone resin. The acrylic silicone resin contains a siloxane bond. The acrylic silicone resin also has excellent heat resistance and cold resistance. Specific examples of compositions containing an acrylic silicone resin include Dainichiseika Chemicals Co., Ltd.'s product name "Cool Life SP Black (CB1) P5-0", Fujikura Kasei Co., Ltd.'s product name "Bell Earth Elastic Black", Toagosei Co., Ltd.'s product name "Aronble Coat T-1000", and Nippon Shokubai Co., Ltd.'s product names "Acryset EMN325E" and "U-Double EF008".
[0031] When the functional layer 4 is desired to be water impermeable and moisture permeable, the water vapor transmission rate of the functional layer 4 is 10 g / m 2 ·day or more 50g / m 2 ·day or less is preferable. The water vapor transmission rate is measured in accordance with the provisions of "JIS Z0208".
[0032] The polymer composition of the functional layer 4 may contain additives such as pigments, fillers, reinforcing materials, and antifouling agents as needed. A functional layer 4 containing a pigment has excellent cosmetic properties. The polymer composition may contain organic pigments and inorganic pigments. Examples of fillers include metal oxide particles such as silica, alumina, and titania. Examples of reinforcing materials include cellulose nanofibers. The content of each additive is adjusted depending on the function.
[0033] In Figure 3, arrow T1 indicates the thickness of the functional layer 4. From the viewpoint of functionality, thickness T1 is preferably 10 µm or more, more preferably 30 µm or more, and particularly preferably 50 µm or more. From the viewpoints of the conformability, productivity, and light weight of the sheet 2, thickness T1 is preferably 500 µm or less, more preferably 300 µm or less, and particularly preferably 150 µm or less. The structural sheet 2 may have two or more functional layers 4. It is preferable that the distribution of thickness T1 is within the range of ±50 µm.
[0034] [Middle layer] The intermediate layer 6 contributes to the rigidity of the sheet 2. A preferred material for the intermediate layer 6 is a composite material of a polymer and a filler. Examples of polymers for the composite material include acrylic resin, acrylic silicone resin, fluororesin, silicone resin, epoxy resin, ethylene-vinyl acetate copolymer, and styrene-butadiene copolymer. Examples of fillers for the composite material include cement, silica, alumina, titanium oxide, calcium carbonate, and carbon black. A preferred composite material is polymer cement. This polymer cement contains a polymer and cement. A typical polymer is acrylic resin. Examples of cement include Portland cement, alumina cement, and mixtures thereof. Portland cement is preferred. An intermediate layer 6 made of polymer cement is also called a "polymer cement hardened layer."
[0035] When the intermediate layer 6 contains a polymer and cement, the mass ratio of the polymer to the solid content of the intermediate layer 6 is preferably 10% or more and 40% or less. An intermediate layer 6 with this ratio of 10% or more has excellent adhesion to other layers (functional layer 4 or adhesive layer 8). From this perspective, this ratio is more preferably 15% or more, and particularly preferably 20% or more. An intermediate layer 6 with this ratio of 40% or less can contain a sufficient amount of cement. From this perspective, this ratio is more preferably 35% or less, and particularly preferably 30% or less.
[0036] When the intermediate layer 6 contains a polymer and cement, the mass ratio of cement to the solid content of the intermediate layer 6 is preferably 20% or more and 70% or less. A sheet 2 having an intermediate layer 6 with this ratio of 20% or more can achieve high tensile strength and low elongation. This sheet 2 has excellent handleability. From this viewpoint, this ratio is more preferably 30% or more, and particularly preferably 35% or more. An intermediate layer 6 with this ratio of 70% or less can contain a sufficient amount of polymer. From this viewpoint, this ratio is more preferably 60% or less, and particularly preferably 55% or less.
[0037] The intermediate layer 6 containing polymer and cement has excellent water vapor permeability. Even if a structure is covered with the sheet 2 having this intermediate layer 6, the metal in the structure is unlikely to corrode. The water vapor permeability of the intermediate layer 6 is 20 g / m 2 ·day or more 60g / m 2 ·day or less is preferable. The water vapor transmission rate is measured in accordance with the provisions of "JIS Z0208".
[0038] The intermediate layer 6 can be formed from a mixture obtained from a composition containing a polymer and a composition containing cement. When the substrate is an acrylic resin, a preferred composition containing a polymer is an acrylic emulsion. This acrylic emulsion is obtained by emulsion polymerization of a monomer. The emulsion polymerization can be carried out using an emulsifier. The polymerization can be carried out in water containing a surfactant. Typical monomers are acrylic acid esters or methacrylic acid esters. The content of the monomer component in the acrylic emulsion is 20% by mass to 100% by mass.
[0039] Specific examples of compositions containing a polymer suitable for the intermediate layer 6 include "Spring Coat Brush Mixture" (product name) from Kikusui Chemical Industry Co., Ltd. and "Aronbull Coat A450 Base" (product name) from Toagosei Co., Ltd. Specific examples of compositions containing cement suitable for the intermediate layer 6 include "Spring Coat Brush Powder" (product name) from Kikusui Chemical Industry Co., Ltd. and "Aronbull Coat A450 Setter" (product name) from Toagosei Co., Ltd.
[0040] In Figure 3, arrow T2 indicates the thickness of the intermediate layer 6. In this embodiment, as described above, the reinforcing body 10 is embedded in the intermediate layer 6. Therefore, the thickness T2 is measured including the reinforcing body 10. From the viewpoint of the handleability of the sheet 2, the thickness T2 is preferably 100 µm or more, more preferably 300 µm or more, and particularly preferably 500 µm or more. From the viewpoints of the conformability, productivity, and lightness of the sheet 2, the thickness T2 is preferably 1500 µm or less, more preferably 1000 µm or less, and particularly preferably 700 µm or less. It is preferable that the distribution of the thickness T2 is within a range of ±100 µm.
[0041] The material of the intermediate layer 6 may be a resin composition or a rubber composition. The sheet for structure 2 may have two or more intermediate layers 6. The sheet for structure 2 may have two intermediate layers 6 made of different materials. The sheet for structure 2 may have a layer structure that does not include an intermediate layer 6.
[0042] From the viewpoint of adhesion of the intermediate layer 6 to the functional layer 4 , it is preferable that the base polymer of the intermediate layer 6 is the same type as the base polymer of the functional layer 4 .
[0043] [Adhesive layer] The adhesive layer 8 abuts against the substrate. The adhesive strength of the adhesive layer 8 allows the sheet 2 to be attached to the structure. A preferred material for the adhesive layer 8 is a polymer-based adhesive composition. Examples of polymers suitable for this adhesive composition include acrylic resin, silicone, polyurethane, polyester, natural rubber, and synthetic rubber. A particularly preferred polymer for the substrate is acrylic resin. Specific examples of adhesive compositions include Toyochem's product names "Olivine BPS6574," "Olivine BPS6554," and "Olivine BPS5565K."
[0044] The pressure-sensitive adhesive composition may contain a curing agent. When the substrate is an acrylic resin, a preferred curing agent is an isocyanate curing agent. The ratio of the isocyanate curing agent to 100 parts by mass of the acrylic resin is preferably 1.0 part by mass or more, more preferably 2.0 parts by mass or more, and particularly preferably 2.5 parts by mass or more. This ratio is preferably 10 parts by mass or less, more preferably 8 parts by mass or less, and particularly preferably 7 parts by mass or less.
[0045] The PSA composition may contain a tackifier. Examples of tackifiers include rosin-based tackifiers, terpene-based tackifiers, petroleum resin-based tackifiers, and phenolic resin-based tackifiers. The ratio of the tackifier to 100 parts by mass of the base polymer is preferably 0.5 parts by mass or more, more preferably 1.0 parts by mass or more, and particularly preferably 1.5 parts by mass or more. This ratio is preferably 15 parts by mass or less, more preferably 10 parts by mass or less, and particularly preferably 7 parts by mass or less. Specific examples of tackifiers include Arakawa Chemical's products under the trade names "Ester Gum H," "Ester Gum AA-V," and "Ester Gum 105."
[0046] In FIG. 3, the arrow T3 indicates the thickness of the adhesive layer 8. From the viewpoint of adhesiveness, the thickness T3 is preferably 20 μm or more, more preferably 40 μm or more, and particularly preferably 50 μm or more. From the viewpoints of productivity, lightness, and ease of handling of the sheet 2, the thickness T3 is preferably 300 μm or less, more preferably 200 μm or less, and particularly preferably 150 μm or less. The amount of the adhesive layer 8 is 20 g / m 2 More than 250g / m 2 The following is preferred: The structural sheet 2 may have two or more adhesive layers 8.
[0047] Reinforcement The reinforcement 10 can contribute to the high tensile strength of the sheet 2. The reinforcement 10 can also contribute to the low elongation of the sheet 2. A sheet 2 including the reinforcement 10 has excellent handleability. As described above, the reinforcement 10 is embedded in the intermediate layer 6. The reinforcement 10 may be embedded in the functional layer 4. The reinforcement 10 may be embedded in the adhesive layer 8. The reinforcement 10 may be located between the functional layer 4 and the intermediate layer 6. The reinforcement 10 may be located between the intermediate layer 6 and the adhesive layer 8. In this specification, the reinforcement 10 refers to an object that can impart a higher tensile strength to the sheet 2 than a hypothetical sheet that has the same layer structure as the sheet 2 except that it does not have the reinforcement 10. The layered reinforcement 10 is also referred to as a "reinforcement layer."
[0048] [Tensile strength and elongation of reinforcement] The tensile strength of this reinforcing body 10 is preferably 5.0 MPa or more. When the tensile strength of the reinforcing body 10 is 5.0 MPa or more, the sheet 2 is less likely to break even when tension is applied. This sheet 2 has excellent handleability. From this viewpoint, the tensile strength is more preferably 5.5 MPa or more, and particularly preferably 6.0 MPa or more. From the viewpoint of the conformability of the sheet 2, the tensile strength of the reinforcing body 10 is preferably 15.0 MPa or less, more preferably 10.0 MPa or less, and particularly preferably 7.0 MPa or less.
[0049] The elongation at break of this reinforcing body 10 is preferably 15.0% or less. A sheet 2 having an elongation of the reinforcing body 10 of 15.0% or less is less likely to deform even when tension is applied. This sheet 2 has excellent handleability. From this viewpoint, the elongation of the reinforcing body 10 is more preferably 13.0% or less, and particularly preferably 11.0% or less. From the viewpoint of the conformability of the sheet 2, the elongation of the reinforcing body 10 is preferably 5.0% or more, more preferably 7.0% or more, and particularly preferably 8.5% or more.
[0050] The tensile strength and elongation are measured in accordance with the general nonwoven fabric testing method specified in "JIS L1913:2010." Test pieces for measurement are cut out from the reinforcement 10 or its original fabric. Five test pieces whose length direction coincides with the length direction of the reinforcement 10 or its original fabric, and five test pieces whose length direction coincides with the width direction of the reinforcement 10 or its original fabric are used for measurement. The tensile strength and elongation are calculated by averaging the 10 measured values.
[0051] In a plan view, the ratio of the outline area of the reinforcing body 10 to the area of the structural sheet 2 is preferably 60% or more. A reinforcing body 10 with this ratio of 60% or more can contribute to the ease of handling of the sheet 2. From this perspective, this ratio is more preferably 70% or more, and particularly preferably 75% or more. This ratio may be 100%. From the perspective of conformability at the seam 22, this ratio is preferably 95% or less.
[0052] [fabric] FIG. 7 shows the reinforcing body 10. In this reinforcing body 10, a plurality of warp threads 26a and a plurality of weft threads 26b are woven. In other words, the reinforcing body 10 is a woven fabric (cloth). In this embodiment, this woven fabric has a plain weave. A woven fabric is a type of fabric. The reinforcing body 10, which is a fabric, can be impregnated with the composition of the intermediate layer 6. This impregnation can contribute to the high tensile strength of the sheet 2. This impregnation can also contribute to the low elongation of the sheet 2. The reinforcing body 10 may be a fabric other than a woven fabric. Examples of fabrics other than a woven fabric include knitted fabrics and cross-point fused meshes.
[0053] Examples of materials for the reinforcement 10 include synthetic resin compositions and metals. Preferred base resins for synthetic resin compositions include polyethylene terephthalate, polyethylene naphthalate, aramid, vinylon, polypropylene, polystyrene, and polyvinylidene fluoride. Preferred metals include aluminum alloys, carbon steel, and alloy steels. By employing warp threads 26a and weft threads 26b with high tensile strength, the sheet 2 can achieve a sufficiently high tensile strength. By employing warp threads 26a and weft threads 26b with low elongation, the sheet 2 can achieve a sufficiently low elongation.
[0054] As is clear from Figure 7, this reinforcing body 10 has many holes 28. In this embodiment, the planar shape of each hole 28 is generally square. The intermediate layer 6 penetrates the holes 28. This penetration can contribute to the high tensile strength of the sheet 2. This penetration can also contribute to the low elongation of the sheet 2.
[0055] In FIG. 7, arrow P1 indicates the pitch of the thread 26. The pitch P1 is preferably 1.0 mm or more and 50 mm or less. In a reinforcement 10 having a pitch P1 of 1.0 mm or more, a large amount of polymer cement or the like passes through the holes 28. This reinforcement 10 can contribute to the high tensile strength and low elongation of the sheet 2. From this viewpoint, the pitch P1 is more preferably 1.2 mm or more, and particularly preferably 1.5 mm or more. In a reinforcement 10 having a pitch P1 of 50 mm or less, this reinforcement 10 can contribute to the high tensile strength and low elongation of the sheet 2. From this viewpoint, the pitch P1 is more preferably 40 mm or less, and particularly preferably 35 mm or less.
[0056] 7, the arrow D1 indicates the thickness of the thread 26. A thread 26 with a large thickness D1 can achieve high tensile strength and low elongation of the sheet 2. From this viewpoint, the thickness D1 is preferably 0.05 mm or more, more preferably 0.10 mm or more, and particularly preferably 0.15 mm or more. The thickness is preferably 1.0 mm or less.
[0057] The structural sheet 2 may include a reinforcing body 10 other than fabric. Examples of the reinforcing body 10 other than fabric include nonwoven fabric, long fiber, resin film, and metal foil. The reinforcing body 10 may also be a large number of short fibers dispersed in the composition.
[0058] [Other Layers] The sheet for structure 2 may have another layer located on the functional layer 4. A typical other layer is a clear paint layer. The other layer may be a layer that reinforces or adds a function such as design or heat insulation. The sheet for structure 2 may have a layer located between the functional layer 4 and the intermediate layer 6. The sheet for structure 2 may have a layer located between the intermediate layer 6 and the adhesive layer 8.
[0059] Total Thickness In Figure 3, the arrow Tt indicates the total thickness of the sheet 2. The total thickness Tt is preferably 200 µm or more, more preferably 400 µm or more, and particularly preferably 500 µm or more. The total thickness Tt is preferably 5.0 mm or less, more preferably 3.0 mm or less, and particularly preferably 1.0 mm or less. The distribution of the total thickness Tt is preferably within a range of ±100 µm.
[0060] [Manufacturing method] An example of a manufacturing method for this structural sheet 2 will be described below. In this manufacturing method, the polymer composition of the functional layer 4 is mixed with a solvent to obtain a first coating material. This first coating material is applied onto a base film to obtain a first coating film. This first coating film is heated, and the solvent volatilizes from the first coating material. This heating hardens the base polymer, and the functional layer 4 is obtained.
[0061] Next, the composite material of the intermediate layer 6 is mixed with a solvent to obtain a second coating. This second coating is applied onto the functional layer 4 to obtain a second coating. The reinforcing body 10 is pressed against this second coating. This second coating is heated, and the solvent evaporates from the second coating. This heating hardens the polymer, and an intermediate layer 6 containing the reinforcing body 10 is obtained.
[0062] Next, the adhesive composition of the adhesive layer 8 is mixed with a solvent to obtain a third coating material. This third coating material is applied onto a release film to obtain a third coating film. This third coating film is heated to volatilize the solvent from the third coating material, thereby obtaining the adhesive layer 8.
[0063] This adhesive layer 8 is overlaid on the intermediate layer 6. Furthermore, the base film is peeled off from the functional layer 4, and the release film is peeled off from the adhesive layer 8, thereby obtaining the sheet for structure 2. The release film may remain on the sheet for structure 2.
[0064] [effect] This structural sheet 2 has excellent conformability, and therefore, as mentioned above, can be applied to roofs 12 that have steps. By patching together multiple sheets 2, the surface of the roof 12 can be covered with the sheet 2 over a wide area. Because the sheet 2 has an adhesive layer 8, there is no need to apply an adhesive to the roof 12. Because this adhesive layer 8 has excellent adhesiveness, the surface of the roof 12 can be covered with the sheet 2 over a wide area even if the surface of the roof 12 is made of a combination of materials. For example, even if the surface of the roof 12 includes both metal and artificial slate, the surface of the roof 12 can be covered with the sheet 2 over a wide area.
[0065] The entire surface of the roof 12 may be covered with the sheet 2. In this specification, the surface of the roof 12 means the surface that can be seen when the roof 12 is viewed vertically from above. A repair method in which the entire surface of the roof 12 is covered with a single type of sheet 2 is not found in conventional construction methods.
[0066] This sheet 2 is lighter than steel plates, copper plates, galvanized iron plates, etc. Therefore, even if a wide area of the surface of the roof 12 is covered with the sheet 2, the adverse effect on the earthquake resistance of the building is small. From the viewpoint of earthquake resistance, the density of the sheet 2 is 4.0 g / cm 3 Less than 3.0 g / cm is preferred 3 Less than 2.5 g / cm is more preferable. 3 The following is particularly preferable: This density is much smaller than the density of aluminum-zinc alloy plated steel sheets (trade name "Galvalume steel sheets") which are commonly used for repairing the roof 12.
[0067] [Other uses] This sheet 2 can contribute to the repair or reinforcement of structures other than the roof 12. Examples of structures other than the roof 12 include residential walls, pillars, eaves, fences, gates, doors, parapets, copings, etc. This sheet 2 may also be used in commercial buildings, factories, warehouses, bridges, sewage facilities, railway facilities, tunnels, etc.
[0068] [Repair and reinforcement] After a structure (such as a roof 12) is repaired or reinforced with this sheet 2, the sheet 2 or the structure may be damaged or deteriorated over time. A newly prepared structural sheet 2 can be attached to the damaged or deteriorated area, allowing for re-repair or re-reinforcement. By overlaying a new sheet 2 on the old sheet 2, the value of the structure can be preserved and maintained for an extremely long period of time. This overlaying can be achieved by the adhesive strength of the adhesive layer 8 of the new sheet 2. This re-repair and re-reinforcement does not require the old sheet 2 to be discarded. This re-repair and re-reinforcement can reduce the generation of waste. This sheet 2 is in line with the purpose of a circular economy. Even if low-density sheets 2 are stacked, the adverse effect on the earthquake resistance of the structure is small.
[0069] [Second embodiment] [Layer structure] FIG. 8 shows a structural sheet 30 according to another embodiment. The sheet 30 includes a functional layer 32, an intermediate layer 34, an adhesive layer 36, and a reinforcing member 38. The materials, thicknesses, and other specifications of the functional layer 32, intermediate layer 34, adhesive layer 36, and reinforcing member 38 are the same as those of the functional layer 4, intermediate layer 6, adhesive layer 8, and reinforcing member 10 of the structural sheet 2 shown in FIGS. 1-3. In the structural sheet 30, the adhesive layer 36, reinforcing member 38, intermediate layer 34, and functional layer 32 are layered in this order from the bottom up. Even in this layer structure, the reinforcing member 38 can contribute to the high tensile strength and low elongation of the sheet 30.
[0070] [Sheet tensile strength and elongation] The tensile strength of this structural sheet 30 is preferably 5.0 MPa or more. A sheet 30 with a tensile strength of 5.0 MPa or more is less likely to break even when tension is applied. This sheet 30 has excellent handleability. From this viewpoint, the tensile strength is more preferably 5.6 MPa or more, and particularly preferably 6.0 MPa or more. From the viewpoint of the conformability of the sheet 30, the tensile strength is preferably 10.0 MPa or less, more preferably 9.5 MPa or less, and particularly preferably 9.0 MPa or less.
[0071] The elongation at break of this structural sheet 30 is preferably 15.0% or less. A sheet 30 with an elongation of 15.0% or less is less likely to deform even when tension is applied. This sheet 30 has excellent handleability. From this viewpoint, the elongation is more preferably 13.0% or less, and particularly preferably 11.0% or less. From the viewpoint of the conformability of the sheet 30, the elongation is preferably 5.0% or more, more preferably 7.0% or more, and particularly preferably 8.5% or more. [Example]
[0072] The effects of the structural sheet according to the examples will be explained below. The scope of the disclosure of this specification should not be construed as being limited based on the description of these examples.
[0073] [Example 1] The acrylic silicone resin and the solvent were mixed to obtain a first coating material. This first coating material was applied to a release sheet to obtain a first coating film. This first coating film was heated to obtain a functional layer. The thickness of this functional layer was 100 μm.
[0074] An acrylic emulsion (the aforementioned product name "Spring Coat Brush Mixture") and a cement composition (the aforementioned product name "Spring Coat Brush Powder") were mixed to obtain a second coating. This second coating was applied onto the functional layer to obtain a second coating film. A woven fabric (product name "Cheesecloth #40" from Sanko Weaving Co., Ltd.) serving as a reinforcing material was pressed against this second coating film. This second coating film was heated to obtain an intermediate layer containing the reinforcing material. The thickness of this intermediate layer was 300 μm. The tensile strength of this reinforcing material, measured using the aforementioned method, was 5.20 MPa, and the elongation at break was 11.0%.
[0075] A third coating material with a gel fraction of 57% was obtained by mixing 100 parts by mass of an adhesive containing an acrylic resin (the aforementioned product name "Orivine BPS6574") with 6 parts by mass of an isocyanate-based curing agent (product name "BHS8515" from Toyochem Co., Ltd.). This third coating material was applied onto a release film to obtain a third coating film. This third coating film was heated to obtain an adhesive layer. The thickness of this adhesive layer was 100 μm.
[0076] This adhesive layer was then laminated on the intermediate layer. The release sheet was then peeled off from the functional layer, and the release film was peeled off from the adhesive layer to obtain the structural sheet of Example 1 having the layer structure shown in Figure 1-3.
[0077] [Example 2] A structural sheet for Example 2 was obtained in the same manner as Example 1, except that a nonwoven fabric (trade name "ELTAS E01012" by Asahi Kasei Corporation) was used as the reinforcing body. The tensile strength of this reinforcing body was 0.54 MPa, and the elongation at break was 31.0%.
[0078] [Example 3] A structural sheet for Example 3 was obtained in the same manner as Example 1, except that a woven fabric (product name "Cheesecloth #20" manufactured by Sanko Seifu Co., Ltd.) was used as the reinforcing material. The tensile strength of this reinforcing material was 6.15 MPa, and the elongation at break was 10.3%.
[0079] [Comparative Example 1] A structural sheet of Comparative Example 1 was obtained in the same manner as in Example 1, except that no reinforcing member was provided.
[0080] [Sheet properties] The tensile strength and elongation at break of the structural sheets were measured using the methods described above. The results are shown in Table 1 below. Note that the sheet of Comparative Example 1 was significantly elongated in the early stages of the tensile test, making it impossible to objectively measure the tensile strength and elongation.
[0081] [Ease of handling] A worker was asked to attach the structural sheet to a roof. The worker was then asked about the ease of handling. The sheet was rated according to the following criteria. A: Very good B: Good C: Bad The results are shown in Table 1 below.
[0082] [Table 1]
[0083] As is clear from Table 1, the structural sheets of each Example are excellent in handleability. The superiority of this structural sheet is clear from these evaluation results.
[0084] [Disclosure items] Each of the following sections discloses a preferred embodiment.
[0085] [Item 1] A structural sheet having a functional layer, an adhesive layer and a reinforcing body.
[0086] [Item 2] Item 2. The structural sheet according to item 1, wherein the reinforcing material is fabric.
[0087] [Item 3] Item 3. The structural sheet according to item 2, wherein the material of the fabric is a synthetic resin composition, and the base resin of this synthetic resin composition is polyethylene terephthalate, polyethylene naphthalate, aramid, vinylon, polypropylene, polystyrene, or polyvinylidene fluoride.
[0088] [Item 4] 4. The structural sheet according to item 2 or 3, wherein the fabric has a tensile strength of 5.0 MPa or more as measured by a tensile test.
[0089] [Item 5] 5. The structural sheet according to any one of items 2 to 4, wherein the fabric has an elongation of 15.0% or less as measured by a tensile test.
[0090] [Item 6] Further provided is an intermediate layer located between the functional layer and the adhesive layer, 6. The structural sheet according to any one of items 1 to 5, wherein the material of the intermediate layer is a composite material containing a polymer and cement.
[0091] [Item 7] Item 7. The structure sheet according to item 6, wherein the adhesive layer, the reinforcing body, the intermediate layer, and the functional layer are laminated in this order.
[0092] [Item 8] 7. The structural sheet according to item 6, wherein the reinforcing member is embedded in the intermediate layer.
[0093] [Item 9] 9. The structural sheet according to any one of items 1 to 8, having a tensile strength measured by a tensile test of 5.0 MPa or more.
[0094] [Item 10] 10. The structural sheet according to any one of items 1 to 9, wherein the elongation measured by a tensile test is 15.0% or less.
[0095] [Item 11] A method for repairing or reinforcing a structure using a sheet, comprising: (1) preparing a sheet having a functional layer, an adhesive layer, and a reinforcing body; and (2) A step of attaching the sheet to the surface of the structure by the adhesive force of the adhesive layer. A method for repairing or reinforcing a structure, comprising:
[0096] [Item 12] A method for re-repairing or re-reinforcing a structure that has been repaired or reinforced with an old sheet, (1) preparing a new sheet having a functional layer, an adhesive layer, and a reinforcing body; and (2) A step of attaching the new sheet to the surface of the damaged or deteriorated old sheet by the adhesive strength of the adhesive layer. A method for repairing or re-reinforcing a structure, comprising: [Industrial Applicability]
[0097] The structural sheet described above can be used by being attached to various objects. [Explanation of symbols]
[0098] 2. Structural sheets 2a...First sheet 2b...Second sheet 4. Functional layer 6. Middle class 8...adhesive layer 10. Reinforcement body 12. Roof 18. Step 22. Seam 24. Step 26...Thread 26a···Warp 26b....Weft 28... 30. Structural sheet 32 Functional Layer 34. Middle class 36...adhesive layer 38... Reinforcement body
Claims
1. The adhesive layer includes a functional layer, an adhesive layer, and a reinforcing body. A sheet for structure, the water vapor transmission rate of which is set to a value of 10 g / m 2 ·day or more and 50 g / m 2 ·day or less.
2. 2. The structural sheet according to claim 1, wherein the reinforcing material is a fabric.
3. 3. The structural sheet according to claim 2, wherein the material of the fabric is a synthetic resin composition, and the base resin of the synthetic resin composition is polyethylene terephthalate, polyethylene naphthalate, aramid, vinylon, polypropylene, polystyrene or polyvinylidene fluoride.
4. 4. The structural sheet according to claim 2 or 3, wherein the fabric has a tensile strength of 5.0 MPa or more as measured by a tensile test.
5. 4. The structural sheet according to claim 2 or 3, wherein the fabric has an elongation of 15.0% or less as measured by a tensile test.
6. Further comprising an intermediate layer located between the functional layer and the adhesive layer, 3. The structural sheet according to claim 1, wherein the intermediate layer is made of a composite material containing a polymer and cement.
7. The structure sheet according to claim 6 , wherein the adhesive layer, the reinforcing body, the intermediate layer and the functional layer are laminated in this order.
8. 7. The structural sheet according to claim 6, wherein the reinforcing member is embedded in the intermediate layer.
9. 3. The structural sheet according to claim 1, which has a tensile strength of 5.0 MPa or more as measured by a tensile test.
10. 3. The structural sheet according to claim 1, which has an elongation measured by a tensile test of 15.0% or less.
11. A method for repairing or reinforcing a structure using a sheet, comprising: (1) preparing a sheet having a functional layer, an adhesive layer, and a reinforcing body, and having a water vapor transmission rate set to a value of 10 g / m 2 ·day or more and 50 g / m 2 ·day or less; and (2) A step of attaching the sheet to the surface of the structure by the adhesive force of the adhesive layer. A method for repairing or reinforcing a structure, comprising:
12. A method for re-repairing or re-reinforcing a structure that has been repaired or reinforced with an old sheet, comprising the steps of: (1) preparing a new sheet having a functional layer, an adhesive layer, and a reinforcing body, and having a water vapor transmission rate set to a value of 10 g / m 2 ·day or more and 50 g / m 2 ·day or less; and (2) A step of attaching the new sheet to the surface of the damaged or deteriorated old sheet by the adhesive strength of the adhesive layer. A method for repairing or reinforcing a structure, comprising: