AI Technical Summary
The challenge is to achieve high breakdown voltage in semiconductor devices with a narrow outer peripheral region to maintain a high area ratio for current density without increasing the device size.
The semiconductor device incorporates a semiconductor substrate with an element region and an outer peripheral region, featuring p-type guard rings and n-type guard rings, along with high concentration spacing regions to facilitate depletion layer expansion, maintaining high voltage despite a narrow width.
This configuration allows for high breakdown voltage performance while reducing the outer peripheral region's width, enhancing current density and suppressing high electric fields, thus optimizing device efficiency.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[Technical field]
[0001] The technology disclosed in this specification relates to a semiconductor device.
[0002] In the semiconductor device disclosed in Patent Document 1, an element region and an outer periphery region are provided on a semiconductor substrate. A MOSFET (metal-oxide-semiconductor field effect transistor) is provided in the element region. The outer periphery region is disposed around the element region. The outer periphery region is provided with a plurality of p-type guard rings that extend in an annular shape so as to surround the element region in multiple layers. When the semiconductor device is turned off, a depletion layer spreads from the element region to the outer periphery region. At this time, the depletion layer spreads to the outer periphery region via each guard ring. By spreading the depletion layer in the outer periphery region in this manner, a voltage can be held in the outer periphery region. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2019-046908 A Summary of the Invention [Problem to be solved by the invention]
[0004] If the width of the peripheral region is wide, the area ratio of the element region to the entire semiconductor substrate becomes small, making it impossible to pass a current through the semiconductor substrate at a high density. This specification proposes a technology for achieving a high breakdown voltage by using a peripheral region with a narrow width. [Means for solving the problem]
[0005] The semiconductor device disclosed in this specification includes a semiconductor substrate having an element region and an outer peripheral region disposed around the element region, and an upper electrode in contact with an upper surface of the semiconductor substrate within the element region. The element region includes a p-type main region in contact with the upper electrode, and an n-type element drift region disposed below the main region. The outer peripheral region includes a plurality of p-type guard rings extending in an annular shape so as to surround the element region in multiple layers when the semiconductor substrate is viewed from above, a plurality of n-type interval regions disposed between the guard rings, and an n-type outer peripheral drift region that is continuous with the element drift region and disposed below the guard rings and the interval regions. At least one of the interval regions is a high-concentration interval region having a higher n-type impurity concentration than the element drift region.
[0006] When the semiconductor device is turned off, a depletion layer spreads from the element region to the peripheral region. At this time, the depletion layer spreads to the peripheral region (i.e., each interval region and the peripheral drift region) through each guard ring. At least one of the interval regions is a high-concentration interval region having a higher n-type impurity concentration than the element drift region. Since fixed charges (i.e., donors) are present in a high concentration in the high-concentration interval region, when the high-concentration interval region is depleted, a high electric field is generated in the high-concentration interval region. Therefore, a high voltage can be held between the pair of guard rings sandwiching the high-concentration interval region. Therefore, according to the structure of this semiconductor device, a high breakdown voltage can be achieved by the narrow width of the peripheral region. [Brief description of the drawings]
[0007] [Figure 1] 2 is a cross-sectional view of the semiconductor device according to the embodiment (a cross-sectional view taken along line II in FIG. 2). [Diagram 2] 1 is a plan view of a semiconductor device according to an embodiment; [Diagram 3] FIG. 4 is a diagram showing an electric field distribution in the outer circumferential region. [Figure 4] 4 is a graph showing an electric field distribution along line IV-IV in FIG. [Diagram 5] FIG. 13 is a diagram showing a non-depleted region when the guard ring is wide. [Figure 6] FIG. 13 is a diagram showing a non-depleted region when the width of the guard ring is narrow. [Figure 7] 3A to 3C are explanatory diagrams of a manufacturing method of a semiconductor device according to an embodiment. [Figure 8] 3A to 3C are explanatory diagrams of a manufacturing method of a semiconductor device according to an embodiment. [Figure 9] 3A to 3C are explanatory diagrams of a manufacturing method of a semiconductor device according to an embodiment. [Figure 10] 1 is a cross-sectional view of a semiconductor device according to a first modified example; [Figure 11] 1 is a cross-sectional view of a semiconductor device according to a second modified example; [Figure 12] 11 is a cross-sectional view of a semiconductor device according to a third modified example. [Figure 13] 4 is a cross-sectional view of a semiconductor device according to a fourth modification; [Figure 14] 13 is a cross-sectional view of a semiconductor device according to a fifth modified example. [Figure 15] 13 is a cross-sectional view of a semiconductor device according to a sixth modified example. [Figure 16] 13 is a cross-sectional view of a semiconductor device according to a seventh modification. [Figure 17] 13 is a cross-sectional view of a semiconductor device according to an eighth modification. [Figure 18] 13 is a cross-sectional view of a semiconductor device according to a ninth modification. [Figure 19] 16 is a cross-sectional view of a semiconductor device according to a tenth modification. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] In an example semiconductor device disclosed in the present specification, a plurality of gate trenches may be provided on the upper surface of the semiconductor substrate in the element region, penetrating the main region and reaching the element drift region. The element region may further include a plurality of p-type electric field relaxation regions disposed below the gate trenches, and a plurality of n-type current path regions disposed between the electric field relaxation regions. The element drift region may be disposed below the electric field relaxation regions and the current path regions. The positions of the guard rings in the thickness direction of the semiconductor substrate may overlap the positions of the electric field relaxation regions in the thickness direction.
[0009] According to this configuration, the electric field relaxation region can prevent a high electric field from being applied to the gate trench.
[0010] In the semiconductor device according to the example disclosed in this specification, at least one of the current path regions may be a high-concentration current path region having a higher n-type impurity concentration than the element drift region.
[0011] According to this configuration, it is possible to reduce the electrical resistance of the high concentration current path, which is a part of the current path.
[0012] In the semiconductor device disclosed in the present specification, the peripheral region may further include an n-type upper region disposed above the guard rings and the spacing regions, and the upper region may have an n-type impurity concentration lower than that of the high-concentration spacing region.
[0013] In the semiconductor device disclosed in the present specification, the upper surface of the semiconductor substrate in the peripheral region may be provided with a mesa portion located lower than the upper surface of the semiconductor substrate in the element region, and a plurality of the guard rings may be disposed in an area including a bottom surface of the mesa portion.
[0014] In this way, an upper region or a mesa portion may be provided on the upper portion of the guard ring. Either configuration can achieve a high breakdown voltage in the outer circumferential region.
[0015] In one example of a semiconductor device disclosed in this specification, the plurality of spacing regions may include a first spacing region and a second spacing region disposed on an outer periphery side of the first spacing region. The second spacing region may be the high-concentration spacing region. An n-type impurity concentration of the first spacing region may be lower than an n-type impurity concentration of the high-concentration spacing region.
[0016] A higher electric field is more likely to occur in the inner region of the outer circumferential region than in the outer circumferential region. According to the above configuration, the first spacing region (i.e., a region with a low n-type impurity concentration) is provided in the inner region of the outer circumferential region, thereby suppressing the generation of a high electric field. Furthermore, the second spacing region (i.e., a high concentration spacing region) is provided in the outer region of the outer circumferential region, thereby making it possible to hold a high voltage on both sides of the second spacing region. Thus, according to this configuration, the first spacing region can suppress a high electric field on the inner side, and the second spacing region can ensure a withstand voltage, thereby making it possible to reduce the width of the outer circumferential region.
[0017] In the semiconductor device disclosed in this specification as an example, the width of the multiple guard rings may be narrower as the guard rings are disposed closer to the outer periphery.
[0018] According to this configuration, the generation of a high electric field can be suppressed in the inner peripheral region of the outer peripheral region by the wide guard ring.
[0019] The method for manufacturing a semiconductor device as an example disclosed in this specification may include a step of ion-implanting n-type impurities into the high concentration interval region and the high concentration current path region simultaneously.
[0020] According to this configuration, the semiconductor device can be manufactured efficiently.
[0021] The semiconductor device 10 of the embodiment shown in FIGS. 1 and 2 has a semiconductor substrate 12. The semiconductor substrate 12 is made of SiC. However, the semiconductor substrate 12 may be made of other semiconductor materials (e.g., Si, GaN, etc.). An upper electrode 20 is provided on the upper surface 12a of the semiconductor substrate 12. The upper electrode 20 is in contact with the center of the upper surface 12a of the semiconductor substrate 12. A MOSFET is provided inside the semiconductor substrate 12 in the area covered by the upper electrode 20. Hereinafter, the area of the semiconductor substrate 12 covered by the upper electrode 20 is referred to as an element region 14. In addition, the area around the element region 14 (i.e., the area between the element region 14 and the outer peripheral end face of the semiconductor substrate 12) is referred to as an outer peripheral region 16. The upper surface 12a of the semiconductor substrate 12 in the outer peripheral region 16 is covered with an interlayer insulating film 22 (a silicon oxide film in this embodiment). The upper surface of the interlayer insulating film 22 is covered with a protective insulating film 24 (a polyimide film in this embodiment). A lower electrode 26 is provided on the lower surface 12b of the semiconductor substrate 12. The lower electrode 26 is in contact with the lower surface 12b of the semiconductor substrate 12 in an area spanning the element region 14 and the peripheral region 16.
[0022] In the following description, a direction perpendicular to the thickness direction of the semiconductor substrate 12 is referred to as the x direction, and a direction perpendicular to both the thickness direction of the semiconductor substrate 12 and the x direction is referred to as the y direction.
[0023] A plurality of gate trenches 30 are provided on the upper surface 12a of the semiconductor substrate 12 in the element region 14. Each gate trench 30 extends linearly in the y direction on the upper surface 12a. The plurality of gate trenches 30 are arranged at intervals in the x direction. A gate insulating film 32 and a gate electrode 34 are arranged in each gate trench 30. The gate insulating film 32 covers the inner surface of the gate trench 30. The gate electrode 34 is insulated from the semiconductor substrate 12 by the gate insulating film 32. The upper surface of the gate electrode 34 is covered by the interlayer insulating film 22. The gate electrode 34 is insulated from the upper electrode 20 by the interlayer insulating film 22.
[0024] Within the semiconductor substrate 12, a plurality of source regions 40, a plurality of contact regions 42, a body region 44, a plurality of electric field relief regions 46, a deep region 48, and a plurality of guard rings 50 are provided.
[0025] The multiple source regions 40 are n-type regions. The multiple source regions 40 are provided in the element region 14. Each source region 40 contacts the gate insulating film 32 at the upper end of the side surface of the corresponding gate trench 30. Each source region 40 is in ohmic contact with the upper electrode 20.
[0026] The contact regions 42 are p-type regions. The contact regions 42 are arranged in the element region 14. Each contact region 42 is in ohmic contact with the upper electrode 20 adjacent to the source region 40.
[0027] The body region 44 is a p-type region having a lower p-type impurity concentration than the contact region 42. The body region 44 contacts the source region 40 and the contact region 42 from below. The body region 44 contacts the gate insulating film 32 below the source region 40.
[0028] The multiple electric field relaxation regions 46 are p-type regions. The multiple electric field relaxation regions 46 are arranged in the element region 14. Each electric field relaxation region 46 extends downward from the body region 44. Each electric field relaxation region 46 extends from the body region 44 to a position lower than the lower end of the gate trench 30. Each electric field relaxation region 46 is arranged in a position not in contact with the gate trench 30. Although not shown, each electric field relaxation region 46 extends linearly in the y direction, similar to the gate trench 30.
[0029] The deep region 48 is a p-type region. The deep region 48 is disposed along the boundary between the element region 14 and the peripheral region 16. The deep region 48 extends downward from the body region 44. The deep region 48 extends from the body region 44 to a position lower than the lower end of the gate trench 30. In other words, the deep region 48 extends from the body region 44 to approximately the same depth as the lower end of each electric field relief region 46.
[0030] The guard rings 50 are p-type regions. The guard rings 50 are disposed in the outer peripheral region 16. As shown in FIG. 2, when the semiconductor substrate 12 is viewed from above, the guard rings 50 extend in an annular shape so as to surround the element region 14 in multiple layers. As shown in FIG. 1, each guard ring 50 is separated from the body region 44 and the deep region 48. A gap is provided between each guard ring 50, and each guard ring 50 is separated from each other. In the thickness direction of the semiconductor substrate 12, the position of each guard ring 50 overlaps with the position of each electric field relaxation region 46 and the position of the deep region 48. More specifically, each guard ring 50 is disposed in approximately the same depth range as each electric field relaxation region 46 and the deep region 48. As shown in FIGS. 1 and 2, each guard ring 50 has a narrower width as the guard ring 50 located on the outer side. That is, the width of each guard ring 50 gradually narrows from the inner peripheral side to the outer peripheral side.
[0031] An n-type drain region 60 is provided inside the semiconductor substrate 12. The drain region 60 is distributed across the element region 14 and the peripheral region 16. The drain region 60 is in ohmic contact with the lower electrode 26 in an area spanning the element region 14 and the peripheral region 16.
[0032] An n-type region 54 is provided inside the semiconductor substrate 12. The n-type region 54 has a lower n-type impurity concentration than the drain region 60 and the source region 40. In the element region 14, the n-type region 54 is disposed between the drain region 60 and the body region 44. That is, the n-type region 54 is distributed from a position in contact with the drain region 60 to a region between the electric field relaxation regions 46. In the following, the portion of the n-type region 54 disposed between the electric field relaxation regions 46 is referred to as a current path region 55. In the following, the portion of the n-type region 54 in the element region 14 disposed below the electric field relaxation regions 46 and the current path regions 55 is referred to as an element drift region 56. In FIG. 1, a region of the n-type region 54 having a higher n-type impurity concentration than the element drift region 56 (hereinafter referred to as a high-concentration n-type region) is indicated by dot hatching. As shown in FIG. 1, each current path region 55 is a high-concentration n-type region. That is, in this embodiment, all the current path regions 55 are high concentration n-type regions. Each current path region 55 contacts the body region 44 from below. Each current path region 55 contacts the gate insulating film 32 on the lower side of the body region 44. Each current path region 55 contacts the side surface of the corresponding electric field relief region 46. The element drift region 56 contacts each current path region 55 and each electric field relief region 46 from below.
[0033] The n-type region 54 is distributed across the element region 14 and the peripheral region 16. In the peripheral region 16, the n-type region 54 is distributed from a position in contact with the drain region 60 to the upper surface 12a of the semiconductor substrate 12. The n-type region 54 is distributed in the intervals between the guard rings 50, and separates the guard rings 50 from each other. The n-type region 54 also separates the guard rings 50 from the deep region 48 and the body region 44. In the following, the portion of the n-type region 54 in the peripheral region 16 that is disposed between the guard rings 50 is referred to as an interval region 58. In the following, the portion of the n-type region 54 in the peripheral region 16 that is disposed above the guard rings 50 and the interval regions 58 is referred to as an upper region 57. In the following, the portion of the n-type region 54 in the peripheral region 16 that is disposed below the guard rings 50 and the interval regions 58 is referred to as an outer drift region 59. Each interval region 58 is a high-concentration n-type region. That is, in this embodiment, all of the spacing regions 58 are high-concentration n-type regions. The upper region 57 and the periphery drift region 59 have approximately the same n-type impurity concentration as the element drift region 56. The upper region 57 contacts each of the guard rings 50 and each of the spacing regions 58 from above. The periphery drift region 59 contacts each of the guard rings 50 and each of the spacing regions 58 from below. The periphery drift region 59 and the element drift region 56 are continuously distributed in the lateral direction.
[0034] Next, the operation of the semiconductor device 10 will be described. When the semiconductor device 10 is in use, a higher potential than that of the upper electrode 20 is applied to the lower electrode 26. When a potential equal to or higher than the gate threshold is applied to the gate electrode 34, a channel is formed in the body region 44 at a position adjacent to the gate insulating film 32. Then, electrons flow from the source region 40 to the drain region 60 through the channel, the current path region 55, and the element drift region 56. That is, the MOSFET is turned on. Since the n-type impurity concentration of the current path region 55 is high, the electrical resistance of the current path region 55 is low. Therefore, electrons can pass through the current path region 55 with low loss. Therefore, the on-resistance of the MOSFET is low.
[0035] When the potential of the gate electrode 34 is reduced to a value less than the gate threshold, the channel disappears and the flow of electrons stops. This turns off the MOSFET. When the MOSFET is turned off, a depletion layer spreads from the body region 44 and the electric field relaxation region 46 to the current path region 55 and the device drift region 56. The depletion layer spreading to the current path region 55 and the device drift region 56 holds the voltage applied between the body region 44 and the drain region 60. In addition, the provision of the electric field relaxation region 46 makes it easy for the depletion layer to spread around the lower end of the gate trench 30. This prevents a high electric field from being applied to the gate insulating film 32 located at the lower end of the gate trench 30.
[0036] Furthermore, when the MOSFET is turned off, a depletion layer spreads from the body region 44 and the deep region 48 to the n-type region 54 in the peripheral region 16 (i.e., the upper region 57, the spacing region 58, and the peripheral drift region 59). The potential of each guard ring 50 is floating. The depletion layer extending from the body region 44 and the deep region 48 extends to the outer periphery inside the n-type region 54 via the multiple guard rings 50. The multiple guard rings 50 promote the spread of the depletion layer to the outer periphery. The depletion layer extending to the n-type region 54 in the peripheral region 16 holds the voltage applied between the body region 44 and the outer periphery end face of the semiconductor substrate 12.
[0037] FIG. 3 shows the distribution of equipotential lines in the outer peripheral region 16 when the MOSFET is off. As shown in FIG. 3, the equipotential lines extend laterally in the lower part of the deep region 48. The equipotential lines bend upward at the lower part of each interval region 58, enter each interval region 58, and extend to the upper surface 12a. Since the equipotential lines enter each interval region 58 in this manner, the electric field of each guard ring 50 is higher for the guard ring 50 on the inner periphery side and lower for the guard ring 50 on the outer periphery side. That is, the electric field of each guard ring 50 decreases with increasing distance from the deep region 48. In this embodiment, the n-type impurity concentration of each interval region 58 is higher than the n-type impurity concentration of the element drift region 56. Therefore, a high electric field is easily generated in each interval region 58, and many equipotential lines are easily introduced into each interval region 58. Therefore, a potential difference is easily generated between each guard ring 50. Therefore, a large potential difference can be maintained between each guard ring 50, and a large potential difference can be maintained in the outer peripheral region 16. Therefore, even if the width of the peripheral region 16 is narrowed, a high breakdown voltage can be achieved in the peripheral region 16. In this manner, by making the n-type impurity concentration of the spacing region 58 higher than the n-type impurity concentration of the element drift region 56, the breakdown voltage performance of the peripheral region 16 can be improved and the width of the peripheral region 16 can be reduced.
[0038] FIG. 4 shows the electric field distribution in the outer drift region 59 at the position of the line IV-IV in FIG. 3 (i.e., the position below each guard ring 50). The horizontal axis of FIG. 4 shows the position of each guard ring 50 located above the line IV-IV. As described above, the electric field of each guard ring 50 is higher for the guard ring 50 located closer to the inner circumference and lower for the guard ring 50 located closer to the outer circumference. Therefore, as shown in FIG. 4, in the outer drift region 59 below each guard ring 50, the electric field decreases from the inner circumference side to the outer circumference side. In addition, the electric field concentrates at the position where the equipotential lines are bent. Therefore, a peak of the electric field is locally formed near the end A on the outer circumference side of the lower surface of each guard ring 50. The value of each peak decreases from the inner circumference side to the outer circumference side. In this way, a high electric field is easily generated near the end A of the guard ring 50 on the inner circumference side. A higher electric field is generated near the end A of the guard ring 50 on the inner circumference side than the lower part of the deep region 48. In contrast, in the semiconductor device of this embodiment, the width of each guard ring 50 becomes wider toward the inner circumference, thereby suppressing the high electric field near the inner guard ring 50. The suppression of the high electric field near the inner guard ring 50 will be described below with reference to FIGS.
[0039] FIG. 5 shows a case where the guard ring 50 is wide, and FIG. 6 shows a case where the guard ring 50 is narrow. In FIGS. 5 and 6, the shaded region 50x is a non-depleted region remaining in the guard ring 50 when the MOSFET is off. In other words, in FIGS. 5 and 6, the guard ring 50 and the n-type region 54 are depleted outside the region 50x. When the guard ring 50 is wide as shown in FIG. 5, the volume of the guard ring 50 is large, so the width of the depletion layer extending from the pn junction into the guard ring 50 is small. Therefore, the interval W1 between the non-depleted regions 50x between adjacent guard rings 50 is narrow. On the other hand, when the guard ring 50 is narrow as shown in FIG. 6, the volume of the guard ring 50 is small, so the width of the depletion layer extending from the pn junction into the guard ring 50 is large. Therefore, the interval W1 between the non-depleted regions 50x between adjacent guard rings 50 is wide. When the interval W1 is narrow as shown in FIG. 5, it is difficult for the equipotential lines to enter the interval region 58, compared to when the interval W1 is wide as shown in FIG. 6. Therefore, when the interval W1 is narrow as shown in FIG. 5, the electric field generated near the end A is smaller than when the interval W1 is wide as shown in FIG. 6. When the width of each guard ring 50 is wider toward the inner circumference as shown in FIG. 3, high electric field concentration near the end A of the guard ring 50 on the inner circumference side is suppressed. This makes it possible to reduce the difference ΔE between the peak value of the electric field near the end A of the guard ring 50 on the inner circumference side and the electric field at the bottom of the deep region 48, as shown in FIG. 4. In addition, the guard ring 50 on the outer circumference side is prone to electric field concentration near the end A, but even if electric field concentration occurs in the guard ring 50 on the outer circumference side as shown in FIG. 4, the electric field is not so high and no problem occurs. In addition, by reducing the width of the guard ring 50 on the outer circumference side, the width of the outer circumference region 16 can be reduced. In this way, according to this configuration, it is possible to reduce the width of the entire outer circumference region 16 while suppressing the generation of a high electric field in the guard ring 50 on the inner circumference side.
[0040] Next, a method for manufacturing the semiconductor device 10 will be described. The semiconductor device 10 is manufactured from a semiconductor substrate constituted by a drain region 60. First, as shown in FIG. 7, an n-type layer 90 is epitaxially grown on the drain region 60. The n-type layer 90 has the same n-type impurity concentration as the element drift region 56. Next, as shown in FIG. 8, p-type impurities are selectively ion-implanted into the n-type layer 90 through a mask 92 to form the field relaxation region 46, the deep region 48, and the guard ring 50. Next, as shown in FIG. 9, n-type impurities are ion-implanted into the entire semiconductor substrate to the same depth as the field relaxation region 46, the deep region 48, and the guard ring 50. Here, the n-type impurities are implanted at a concentration lower than that of the field relaxation region 46, the deep region 48, and the guard ring 50. As a result, a high-concentration n-type region having a higher n-type impurity concentration than that of the element drift region 56 is formed in the current path region 55 and the interval region 58. Next, the source region 40, the contact region 42, and the body region 44 are formed by ion implantation. Thereafter, the semiconductor device 10 is completed by forming necessary electrodes, insulating films, etc.
[0041] According to this manufacturing method, p-type impurity ions can be simultaneously implanted into the electric field relaxation region 46 and the guard ring 50, and n-type impurity ions can be simultaneously implanted into the current path region 55 and the spacing region 58. Furthermore, according to this manufacturing method, there is no need to provide a mask when implanting ions into the current path region 55 and the spacing region 58. Therefore, according to this manufacturing method, the semiconductor device 10 can be efficiently manufactured.
[0042] In the above-described embodiment, the spacing region 58 in which the high-concentration n-type region is formed is an example of a high-concentration spacing region. Also, in the above-described embodiment, the current path region 55 in which the high-concentration n-type region is formed is an example of a high-concentration current path region. Also, in the above-described embodiment, the contact region 42 and the body region 44 are an example of a main region.
[0043] In the above embodiment, a high-concentration n-type region (i.e., a region hatched in FIG. 1) having a higher n-type impurity concentration than element drift region 56 is formed in spacing region 58 in peripheral region 16. However, a high-concentration n-type region may be formed in spacing region 58 as well as in a region outside spacing region 58. For example, as shown in FIG. 10, a high-concentration n-type region may be formed across spacing region 58 and upper region 57. Also, as shown in FIG. 11, a high-concentration n-type region may be formed across spacing region 58, upper region 57, and peripheral drift region 59.
[0044] In the above embodiment, the high-concentration n-type regions are formed in all the interval regions 58. However, the high-concentration n-type regions may be formed only in some of the interval regions 58. For example, as shown in FIG. 12, the high-concentration n-type regions may be formed in the interval regions 58 on the outer periphery side (i.e., closer to the outer periphery surface of the semiconductor substrate 12), and the high-concentration n-type regions may not be formed in the interval regions 58 on the inner periphery side (i.e., closer to the element region 14). That is, the interval region 58 on the outer periphery side may be a high-concentration interval region, and the interval region 58 on the inner periphery side may have a lower n-type impurity concentration than the high-concentration interval region. As described above, when the high-concentration n-type regions are formed in the interval regions 58, the interval regions 58 can hold a high potential difference, but a high electric field is likely to be generated in the interval regions 58. As shown in FIG. 12, the electric field can be alleviated by lowering the n-type impurity concentration of the interval region 58 on the inner periphery side where a high electric field is likely to be generated. In addition, by increasing the concentration of n-type impurities in the space region 58 on the outer periphery side where a high electric field is less likely to occur, it is possible to narrow the line width of the space region 58 on the outer periphery side. This allows the width of the outer periphery region 16 to be reduced.
[0045] In the above-described embodiment, the electric field relaxation region 46 is connected to the body region 44. However, the electric field relaxation region 46 may be separated from the body region 44, and the potential of the electric field relaxation region 46 may be floating. In the above-described embodiment, the electric field relaxation region 46 is formed at the intermediate position between the adjacent gate trenches 30. However, as shown in FIG. 13, the electric field relaxation region 46 may be disposed at the lower part of the gate trench 30. Note that, as shown in FIG. 13, the electric field relaxation region 46 may be in contact with the lower end of the gate trench 30, or the electric field relaxation region 46 may be separated from the lower end of the gate trench 30. Even when the electric field relaxation region 46 is disposed at the lower part of the gate trench 30, the electric field relaxation region 46 may be connected to the body region 44, or the electric field relaxation region 46 may be separated from the body region 44.
[0046] In the above-described embodiment, the upper surface 12a of the semiconductor substrate 12 is disposed at the same height in the element region 14 and in the peripheral region 16. However, as shown in FIG. 14, a mesa portion 70 may be provided on the upper surface 12a in the peripheral region 16 so that the upper surface 12a in the peripheral region 16 is located lower than the upper surface 12a in the element region 14. In this case, each guard ring 50 may be disposed in a range including the bottom surface of the mesa portion 70 (i.e., the upper surface 12a in the peripheral region 16). That is, the n-type upper region 57 may not be present above each guard ring 50. Even in this configuration, the withstand voltage in the peripheral region 16 can be improved by each guard ring 50.
[0047] In the above-described embodiment, the electric field relaxation region 46 is provided in the element region 14. However, the electric field relaxation region 46 does not have to be provided in the element region 14. In this case, the guard ring 50 may be formed to a depth that overlaps with the body region 44, as shown in FIG.
[0048] In the above-described embodiment, a MOSFET is formed in the element region 14. However, other switching elements such as an IGBT (insulated gate bipolar transistor) may be formed in the element region 14. Also, as shown in FIG. 16, a diode may be formed in the element region 14. In FIG. 16, a p-type contact region 142 and a p-type anode region 144 are formed in the element region 14. The anode region 144 has a lower p-type impurity concentration than the contact region 142. The contact region 142 is in ohmic contact with the upper electrode 20, and the anode region 144 is in contact with the contact region 142 from below. The element drift region 56 is in contact with the anode region 144 from below. The guard ring 50 is formed at a depth that overlaps with the anode region 144.
[0049] 13, 14 and 15, similarly to Fig. 12, a high concentration n-type region may not be formed in the spacing region 58 on the inner periphery side. For example, as shown in Figs. 17, 18 and 19, a high concentration n-type region may be formed in the spacing region 58 on the outer periphery side, and a high concentration n-type region may not be formed in the spacing region 58 on the inner periphery side.
[0050] The configurations of the techniques disclosed in this specification are listed below. (Configuration 1) A semiconductor device comprising: a semiconductor substrate having an element region and a peripheral region disposed around the element region; an upper electrode in contact with an upper surface of the semiconductor substrate within the element region; having The element region is a p-type main region in contact with the upper electrode; an n-type device drift region disposed below the main region; having The outer circumferential region is a plurality of p-type guard rings extending in an annular shape so as to surround the element region in multiple layers when the semiconductor substrate is viewed from above; a plurality of n-type spacing regions disposed between the guard rings; an n-type peripheral drift region contiguous with the element drift region and disposed below a plurality of the guard rings and a plurality of the spacing regions; having At least one of the plurality of spacing regions is a high-concentration spacing region having a higher n-type impurity concentration than the element drift region. Semiconductor device. (Configuration 2) A plurality of gate trenches are provided on the top surface of the semiconductor substrate in the element region, the gate trenches passing through the main region and reaching the element drift region; The element region is A plurality of p-type electric field relaxation regions disposed below the gate trench; a plurality of n-type current path regions disposed between the electric field relief regions; and the element drift region is disposed below a plurality of the electric field relaxation regions and a plurality of the current path regions, a position of each of the guard rings in a thickness direction of the semiconductor substrate overlaps a position of each of the electric field relaxation regions in the thickness direction; 2. The semiconductor device according to configuration 1. (Configuration 3) 3. The semiconductor device according to configuration 2, wherein at least one of the current path regions is a high-concentration current path region having a higher n-type impurity concentration than the element drift region. (Configuration 4) the periphery region further includes an n-type upper region disposed above a plurality of the guard rings and a plurality of the spacing regions; the upper region has a lower n-type impurity concentration than the high concentration spacing region; 4. The semiconductor device according to configuration 2 or 3. (Configuration 5) a mesa portion is provided on the upper surface of the semiconductor substrate in the peripheral region and located lower than the upper surface of the semiconductor substrate in the element region; A plurality of the guard rings are disposed in an area including a bottom surface of the mesa portion. 4. The semiconductor device according to configuration 2 or 3. (Configuration 6) the plurality of spacing regions include a first spacing region and a second spacing region disposed on an outer circumferential side of the first spacing region, the second spacing region is the high concentration spacing region, The n-type impurity concentration of the first spacing region is lower than the n-type impurity concentration of the high concentration spacing region. The semiconductor device according to any one of configurations 1 to 5. (Configuration 7) 7. The semiconductor device according to configuration 6, wherein the width of the guard rings is narrower toward the outer periphery. (Configuration 8) 4. A method for manufacturing a semiconductor device according to claim 3, further comprising the step of ion-implanting n-type impurities into the high concentration interval region and the high concentration current path region simultaneously.
[0051] Although the embodiments have been described in detail above, these are merely examples and do not limit the scope of the claims. The technology described in the claims includes various modifications and changes to the specific examples exemplified above. The technical elements described in this specification or drawings exhibit technical utility alone or in various combinations, and are not limited to the combinations described in the claims at the time of filing. In addition, the technology exemplified in this specification or drawings achieves multiple objectives simultaneously, and achieving one of the objectives itself has technical utility. [Explanation of symbols]
[0052] 14: element region, 16: peripheral region, 44: body region, 46: electric field relaxation region, 50: guard ring, 55: current path region, 56: element drift region, 58: spacing region, 59: peripheral drift region
Claims
1. A semiconductor device comprising: a semiconductor substrate having an element region and a peripheral region disposed around the element region; an upper electrode in contact with an upper surface of the semiconductor substrate within the element region; having The element region is a p-type main region in contact with the upper electrode; an n-type device drift region disposed below the main region; having The outer circumferential region is a plurality of p-type guard rings extending in an annular shape so as to surround the element region in multiple layers when the semiconductor substrate is viewed from above; a plurality of n-type spacing regions disposed between the guard rings; an n-type peripheral drift region that is continuous with the element drift region and is disposed below a plurality of the guard rings and a plurality of the spacing regions; an n-type upper region disposed over the plurality of guard rings and the plurality of spacing regions; having At least one of the plurality of spacing regions is a high-concentration spacing region having a higher n-type impurity concentration than the element drift region; the upper region has a lower n-type impurity concentration than the high concentration spacing region; Semiconductor device.
2. A plurality of gate trenches are provided on the top surface of the semiconductor substrate in the element region, the gate trenches passing through the main region and reaching the element drift region; The element region is A plurality of p-type electric field relaxation regions disposed below the gate trench; a plurality of n-type current path regions disposed between the electric field relaxation regions; and the element drift region is disposed below a plurality of the electric field relaxation regions and a plurality of the current path regions, a position of each of the guard rings in a thickness direction of the semiconductor substrate overlaps a position of each of the electric field relaxation regions in the thickness direction; The semiconductor device according to claim 1 .
3. 3. The semiconductor device according to claim 2, wherein at least one of the current path regions is a high-concentration current path region having a higher n-type impurity concentration than the element drift region.
4. the plurality of spacing regions include a first spacing region and a second spacing region disposed on an outer circumferential side of the first spacing region, the second spacing region is the high concentration spacing region, an n-type impurity concentration of the first spacing region is lower than an n-type impurity concentration of the high concentration spacing region; 3. The semiconductor device according to claim 1 or 2.
5. The semiconductor device according to claim 4 , wherein the widths of the plurality of guard rings are narrower toward the outer periphery of the guard rings.
6. 4. The method of manufacturing a semiconductor device according to claim 3, further comprising the step of ion-implanting n-type impurities into said high concentration interval region and said high concentration current path region simultaneously.