CMP device

The CMP apparatus addresses wafer damage and slurry sticking by using a pressurized moisturizing fluid system to maintain moisture and cool the wafer surface during polishing, enhancing polishing efficiency and reducing adhesion.

JP2024132732APending Publication Date: 2024-10-01TOKYO SEIMITSU CO LTD

Patent Information

Application Number
JP2023043630
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-17
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

Polishing wafers made of difficult-to-process materials using existing CMP apparatuses results in excessive temperature rise, damage, and slurry adhesion due to evaporation and drying, leading to sticking issues.

Method used

A CMP apparatus with a storage pocket, annular retainer ring, membrane film, and fluid supply system that uses pressurized moisturizing fluid to suppress slurry adhesion by maintaining moisture and cooling the wafer surface during polishing.

Benefits of technology

The apparatus effectively reduces slurry adhesion and temperature rise by moisturizing the wafer surface, ensuring consistent polishing performance and preventing damage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024132732000001_ABST
    Figure 2024132732000001_ABST
Patent Text Reader

Abstract

To provide a chemical mechanical polishing (CMP) device which can suppress the adhesion of slurry to a workpiece.SOLUTION: A chemical mechanical polishing (CMP) device 1 includes: a substantially annular retainer ring 40 in which a storage pocket 40a that can store a workpiece W is formed on the center, and which is provided so as to surround the lower end of a carrier 30; a membrane film 50 whose peripheral edge is grasped by the retainer ring 40 and which forms a pressure propagation chamber C between the carrier 30 and itself; a backing film 60 which is bonded to the membrane film 50 in the storage pocket 40a and can hold the workpiece W; and a fluid supply source 32 which supplies pressurized fluid including moisturizing water to the pressure propagation chamber C. When the workpiece W is polished, the pressurized fluid is supplied into the storage pocket 40a through a communication hole 70 formed in the membrane film 50 and the backing film 60 so as to connect the pressure propagation chamber C with the storage pocket 40a.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a CMP apparatus for polishing a wafer. [Background technology]

[0002] 2. Description of the Related Art In the field of semiconductor manufacturing, CMP apparatuses are known that polish and flatten semiconductor wafers such as silicon wafers (hereinafter referred to as "workpieces").

[0003] The polishing apparatus described in Patent Document 1 is an air-float type CMP apparatus that applies chemical mechanical polishing, or so-called CMP (Chemical Mechanical Polishing) technology. In this CMP apparatus, air is introduced into an air chamber formed between the carrier of the polishing head and the rubber sheet during polishing to form a pressure fluid layer, and the surface of the wafer (surface to be polished) is pressed against the polishing cloth through this pressure fluid layer. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2001-212754 A Summary of the Invention [Problem to be solved by the invention]

[0005] However, when a wafer made of a difficult-to-process material is polished using the CMP device described in Patent Document 1, the polishing is performed over a long period of time at high pressure and high rotation speed, causing the wafer temperature to rise excessively, which causes the slurry adhering to the wafer to evaporate and adhere to the wafer. Furthermore, when air blown out from the holes in the rubber sheet dries the slurry that has entered between the wafer and the rubber sheet, the slurry is more likely to adhere to the wafer.

[0006] Therefore, a technical problem arises that must be solved in order to prevent the slurry from adhering to the workpiece, and an object of the present invention is to solve this problem. [Means for solving the problem]

[0007] In order to achieve the above-mentioned object, the CMP apparatus of the present invention is a CMP apparatus which polishes a workpiece by pressing it against a polishing pad, and which comprises: a substantially annular retaining ring having a central storage pocket capable of storing the workpiece and arranged to surround the lower end of a carrier; a membrane film whose periphery is gripped by the retaining ring to form a pressure transmission chamber between the retaining ring and the carrier; a backing film which is joined to the membrane film within the storage pocket and capable of holding the wafer; and a fluid supply source which supplies a pressurized fluid containing moisturizing water to the pressure transmission chamber; and when the workpiece is polished, the pressurized fluid is supplied into the storage pocket through communication holes formed in the retaining ring and the backing film so as to connect the pressure transmission chamber and the storage pocket. Effect of the Invention

[0008] In the present invention, by supplying a pressurized fluid containing moisturizing water into the storage pocket through the communicating hole, drying of the workpiece and an increase in the workpiece temperature are suppressed, thereby suppressing adhesion of the slurry to the workpiece. [Brief description of the drawings]

[0009] [Figure 1] 1 is a perspective view showing a wafer polishing apparatus to which a wafer suction device according to an embodiment of the present invention is applied; [Diagram 2] FIG. 2 is a vertical cross-sectional view showing a schematic view of a polishing head. [Diagram 3] FIG. 2 is a vertical cross-sectional view showing a schematic view of a main part of a polishing head. [Figure 4] FIG. 2 is a schematic diagram showing the structure of a fluid supply source that generates pressurized fluid containing moisturizing water. [Diagram 5] 13 is an image showing pressure distribution in Experimental Example 1. [Figure 6]13 is an image showing pressure distribution in Experimental Example 2. [Figure 7] 1 is a table showing the amount of adhered slurry, the platen surface temperature, and the polishing rate in Experimental Example 3. [Figure 8] Graph showing the polishing profile of Experimental Example 3. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] An embodiment of the present invention will be described with reference to the drawings. In the following, when the number, numerical value, amount, range, etc. of components are mentioned, the number is not limited to the specific number, and may be more or less than the specific number, unless otherwise specified or when it is clearly limited to a specific number in principle.

[0011] In addition, when referring to the shape or positional relationship of components, etc., this includes things that are substantially similar or approximate to those shapes, etc., unless otherwise specified or considered to be clearly different in principle.

[0012] In addition, the drawings may exaggerate characteristic parts to make the features easier to understand, and the dimensional ratios of the components may not be the same as the actual ones. In addition, in cross-sectional views, hatching of some components may be omitted to make the cross-sectional structure of the components easier to understand.

[0013] 1 is a perspective view showing a schematic diagram of a CMP apparatus 1 according to one embodiment of the present invention. The CMP apparatus 1 polishes the bottom surface of a workpiece W flat. The workpiece W is, for example, a wafer made of a material containing silicon carbide (SiC) or a wafer made of gallium nitride (GaN), but is not limited to these. The CMP apparatus 1 includes a platen 2 and a polishing head 10.

[0014] The platen 2 is formed in a disk shape and is connected to a rotating shaft 3 arranged below the platen 2. The rotating shaft 3 is rotated by the drive of a motor 4, causing the platen 2 to rotate in the direction of arrow D1 in Fig. 1. A polishing pad 5 is attached to the upper surface of the platen 2, and a CMP slurry S, which is a mixture of an abrasive and a chemical agent, is supplied from a nozzle 6 onto the polishing pad 5.

[0015] The polishing head 10 is formed in a disk shape with a smaller diameter than the platen 2, and is connected to a rotating shaft 10a disposed above the polishing head 10. The rotating shaft 10a is rotated by a motor (not shown), causing the polishing head 10 to rotate in the direction of arrow D2 in FIG. 1. The polishing head 10 can be raised and lowered in the vertical direction V by a lifting device (not shown). When polishing the workpiece W, the polishing head 10 descends to press the workpiece W against the polishing pad 5. The workpiece W to be polished by the polishing head 10 is delivered by a wafer transport mechanism (not shown).

[0016] The operation of the CMP apparatus 1 is controlled by a controller 7. The controller 7 controls each of the components constituting the CMP apparatus 1. The controller 7 is, for example, a computer, and is composed of a CPU, a memory, and the like. The functions of the controller 7 may be realized by control using software, or may be realized by something that operates using hardware.

[0017] Next, the polishing head 10 will be described with reference to FIGS.

[0018] The polishing head 10 includes a head body 20 , a carrier 30 , a retainer ring 40 , a membrane film 50 , and a backing film 60 .

[0019] The head body 20 is connected to a rotating shaft 10a, and rotates together with the rotating shaft 10a when the rotating shaft 10a is rotated by the drive of a motor (not shown). The head body 20 is connected to a carrier 30 disposed below the head body 20 via a connecting portion 21, and the head body 20 and the carrier 30 rotate in unison.

[0020] The carrier 30 is provided with fluid supply lines 31 arranged at equal intervals around the periphery of the carrier 30. The lower ends of the fluid supply lines 31 open into a pressure transmission chamber C formed between the lower surface 30a of the carrier 30 and the membrane film 50.

[0021] The fluid supply line 31 is connected to a fluid supply source (RS) 32 and a vacuum source (not shown). The fluid supply source 32 and the vacuum source are switchably connected to the fluid supply line 31 via a valve (not shown) or the like. The fluid supply source 32 can supply a pressurized fluid containing at least moisturizing water to the pressure transmission chamber C via the fluid supply line 31. The pressure of the pressurized fluid supplied to the fluid supply line 31 is adjusted by a regulator (not shown). The pressurized fluid supplied into the pressure transmission chamber C forms a pressure transmission layer above the membrane film 50 by a rim formed on the outer periphery of the carrier 30, and presses the entire surface of the membrane film 50 downward. In addition, the vacuum source can supply a negative pressure into the pressure transmission chamber C via the fluid supply line 31.

[0022] A carrier pressing means 33 is provided between the head body 20 and the carrier 30. The carrier pressing means 33 is an air bag or the like that is inflated by air supplied from an air supply source (not shown). The pressure of the air supplied from the air supply source is adjusted by a regulator (not shown). The carrier pressing means 33 presses the workpiece W against the polishing pad 5 via the carrier 30 according to the pressure of the supplied air.

[0023] The retainer ring 40 is disposed so as to surround the vicinity of the lower end of the carrier 30 .

[0024] The retainer ring 40 is made of a resin such as glass epoxy, polyether ether ketone (PEEK), polyphenylene sulfide (PPS), etc. The retainer ring 40 is formed in an annular shape and has a storage pocket 40a for storing the workpiece W in approximately the center.

[0025] The retainer holder 41 is formed in a ring shape, and a lower surface 41a is joined to an upper surface 40b of the retainer ring 40 via a membrane film 50 to hold the retainer ring 40. The retainer holder 41 is attached to a retainer pressing member 43 via a snap ring 42. A retainer pressing means 44 is provided between the head body 20 and the retainer pressing member 43. Reference numeral 45 denotes a cover that covers the upper part of the snap ring 42.

[0026] The retainer pressing means 44 is an air bag or the like that is inflated by air supplied from an air supply source (not shown). The pressure of the air supplied from the air supply source is adjusted by a regulator (not shown). The retainer pressing means 44 presses the retainer ring 40 against the polishing pad 5 according to the pressure of the supplied air.

[0027] The membrane film 50 has its periphery sandwiched between the retainer ring 40 and the retainer holder 41 to separate the pressure transmission chamber C and the storage pocket 40a. When compressed air is introduced into the pressure transmission chamber C, the membrane film 50 elastically deforms downward within the storage pocket 40a.

[0028] The membrane film 50 is preferably made of a material having both appropriate strength and flexibility, such as a resin such as polyether ether ketone (PEEK), polyphenylene sulfide (PPS), or polyethylene terephthalate (PET). From the viewpoints of physical properties and availability, PEEK is particularly preferable for the membrane film 50, but PPS and PET are also preferable because they have a Young's modulus close to that of PEEK and are relatively easily available.

[0029] The backing film 60 is, for example, a suede film. The backing film 60 is attached to the membrane film 50 with its center positioned on the rotation axis 10a of the polishing head 10. When compressed air is introduced into the pressure transmission chamber C, the backing film 60 elastically deforms in accordance with the elastic deformation of the membrane film 50.

[0030] The membrane film 50 and the backing film 60 are formed with communication holes 70 that communicate the pressure transmission chamber C and the storage pocket 40a. The hole diameter of the communication holes 70 is set to, for example, about 3 to 5 mm. As a result, the pressurized fluid F in the pressure transmission chamber C is supplied into the storage pocket 40a through the communication holes 70 as shown by the arrows in FIG. 3. As a result, the pressurized fluid F transmits the pressing force of the carrier pressing means 33 to the workpiece W, and can suppress the slurry S from getting between the upper surface Wa of the workpiece W and the backing film 60. In addition, the negative pressure in the pressure transmission chamber C is supplied into the storage pocket 40a through the communication holes 70, and the workpiece W is adsorbed and held by the backing film 60.

[0031] In addition, it is preferable that the pressurized fluid F is filled between the upper surface Wa of the workpiece W and the membrane film 50 when the workpiece W is polished. This makes it possible to further suppress the slurry S from getting between the upper surface Wa of the workpiece W and the backing film 60.

[0032] The pressurized fluid F may be any fluid that contains a quantity of moisturizing water sufficient to moisturize the upper surface Wa of the workpiece W and is pressurized to a degree sufficient to pressurize the workpiece W. For example, it may be a fluid consisting only of pressure-adjusted de-ionized water (DIW), or mist air consisting of pressure-adjusted clean dry air (CDA) to which water droplets of DIW have been added.

[0033] When using a pressurized fluid F consisting only of DIW, a liquid film of DIW covers the upper surface Wa of the workpiece W, moisturizing the upper surface Wa and preventing the adhesion of the slurry to the upper surface Wa. When using mist air consisting of a mixture of water and gas, the upper surface Wa of the workpiece W is humidified, preventing the adhesion of the slurry to the upper surface Wa, and a uniform pressure distribution with excellent pressure responsiveness can be achieved.

[0034] The fluid supply source 32 may have any configuration as long as it can supply the pressurized fluid F containing a quantity of moisturizing water that can moisturize the upper surface Wa of the workpiece W. For example, as shown in FIG. 4(a), the fluid supply source 32 that supplies the mist air may be configured to branch into a CDA line 34 connected to a CDA supply source (not shown) through which the CDA flows, and a DIW line 35 connected to a DIW supply source (not shown) through which the DIW flows, and generate the pressurized fluid F by dropping an appropriate amount of DIW into the CDA to add water, or as shown in FIG. 4(b), the CDA line 34 may be connected to a buffer 36 that stores DIW, and the CDA may be passed through the DIW to be humidified, and then the CDA may be cooled below the dew point by a cooler 37 to generate water droplets to generate the pressurized fluid F.

[0035] In this manner, the CMP apparatus 1 according to this embodiment is a CMP apparatus 1 which polishes the workpiece W by pressing it against the polishing pad 5, and includes a substantially annular retainer ring 40 which has a central storage pocket 40a capable of storing the workpiece W and is arranged to surround the lower end of the carrier 30, a membrane film 50 whose periphery is gripped by the retainer ring 40 to form a pressure transmission chamber C between the retainer ring 40 and the carrier 30, a backing film 60 which is joined to the membrane film 50 within the storage pocket 40a and is capable of holding the workpiece W, and a fluid supply source 32 which supplies a pressurized fluid F containing moisturizing water to the pressure transmission chamber C, and when the workpiece W is polished, the pressurized fluid is supplied into the storage pocket 40a through a communication hole 70 formed in the membrane film 50 and the backing film 60 so as to connect the pressure transmission chamber C to the storage pocket 40a.

[0036] With this configuration, the pressurized fluid F containing moisturizing water in the pressure transmission chamber C is supplied into the storage pocket 40a through the communicating hole 70, thereby moisturizing the upper surface Wa of the workpiece W and cooling the workpiece W, thereby suppressing adhesion of the slurry S to the workpiece W. EXAMPLES

[0037] Next, an experiment using the CMP apparatus 1 according to the above-mentioned embodiment will be described. In the following, the pressing method using the CMP apparatus 1 to press and polish the workpiece W with a pressurized fluid containing moisturizing water is referred to as the "water float method", which is distinguished from the "air float method", which is a conventional pressing method in which the workpiece W is polished with air introduced into an air chamber formed under the carrier.

[0038] (Experimental Example 1) For the water float method (Example 1) using only DIW as the pressurized fluid, the pressure propagation of the pressurized fluid and the responsiveness from the start of polishing were measured.

[0039] 5 is a measurement image showing the pressure distribution immediately after the start of pressurization and a predetermined time after the start of pressurization for Example 1 in which the DIW flow rate was set to 0.1150 ml / min and the conventional air float method (Comparative Example 1). In this experimental example, the pressing forces of the carrier pressing means 33 and the retainer pressing means 44 were set to 9 psi. In the measurement image shown in FIG. 5, bright areas indicate that relatively high pressures are acting, and the large diameter ring portion shown in the image in FIG. 5 corresponds to the retainer ring 40, and the small diameter circle portion corresponds to the storage pocket 40a.

[0040] 5(a) and (b) show that in Comparative Example 1, pressure is sufficiently transmitted to the workpiece W one second after the start of air supply. In contrast, in Example 1, pressure transmission does not occur until DIW is distributed between the backing film 60 and the workpiece W, so that the workpiece W is not sufficiently pressed immediately after the start of DIW supply, but 15 seconds after the start of DIW supply, DIW fills the space between the workpiece W and the backing film 60 and pressure is transmitted to the workpiece W. In other words, according to this experimental example, although there is a lag in responsiveness compared to Comparative Example 1, pressure transmission is ensured.

[0041] (Experimental Example 2) Next, in the water float method (Examples 2 to 5) using only DIW as the pressurized fluid, the pressure propagation was measured when the pressure by the carrier pressing means 33 and the retainer pressing means 44 was changed.

[0042] 6 shows measurement images of pressure distribution when the pressing forces of the carrier pressing means 33 and the retainer pressing means 44 are changed to 1 psi, 3 psi, 5 psi, 7 psi, and 9 psi for Examples 2 to 5 and a conventional air float system (Comparative Example 2) described below. In the measurement image shown in FIG. 6, bright areas indicate areas where relatively high pressure is acting, and the large diameter ring portion shown in the image in FIG. 6 corresponds to the retainer ring 40, and the small diameter circular portion corresponds to the storage pocket 40a. Also, "WP / RP" in FIG. 6 indicates the pressing forces of the carrier pressing means 33 and the retainer pressing means 44. Example 2: DIW flow rate 1.15 l / min Example 3: DIW flow rate 0.57 l / min Example 4: DIW flow rate 0.285 l / min Example 5: DIW flow rate 0.15 l / min

[0043] 6, it can be seen that in Examples 2 to 4, good pressure distributions can be obtained at each pressing force, similar to Comparative Example 2. On the other hand, it can be seen that in Example 5, a pressure distribution showing sufficient pressure cannot be obtained, compared to Comparative Example 2. Therefore, it can be seen that in this experimental example, it is preferable to ensure a DIW flow rate of 0.285 ml / min or more.

[0044] (Experimental Example 3) Next, in the water float method (Examples 6 to 7) using DIW and CDA as the pressurized fluid, the amount (thickness) of the slurry adhered to the workpiece W when polishing the P-TEOS film and the amount of the workpiece W polished per unit time (polishing rate) were measured.

[0045] 7 is a table showing the amount of slurry adhered to the upper surface Wa of the workpiece W after 30 minutes of polishing, the surface temperature of the platen 2, and the polishing rate for Examples 6 to 7 and the conventional air float method (Comparative Example 3) described below. The polishing conditions for this experimental example were set as follows: the pressing force of the carrier pressing means 33 and the retainer pressing means 44 was 5 psi, the rotation speed of the platen 2 was 90 rpm, the rotation speed of the polishing head 10 was 87 rpm, the flow rate of CDA was 30 L / min, and the polishing time was 30 minutes. Silica slurry was used as the slurry S. Example 6: DIW flow rate 0.015ml / min Example 7: DIW flow rate 0.030ml / min

[0046] 7, it can be seen that the amount of adhered slurry after 30 minutes of polishing is 200 μm in Comparative Example 3, whereas the amount of adhered slurry is sufficiently reduced to 0.06 μm in Example 6 and 0.05 μm in Example 7. Also, according to FIG. 7, in Examples 6 to 7 and Comparative Example 3, the surface temperature of the platen 2 during 30 minutes of polishing is similar and there is no significant difference in the polishing rate, so it is considered that the lubricating effect of the slurry S is maintained even if the slurry S is diluted by the amount of DIW injected.

[0047] FIG. 8 is a graph showing polishing profiles for Examples 6 to 7 and Comparative Example 3, with the polishing rate plotted on the vertical axis and the radial distance from the center of the workpiece W plotted on the horizontal axis.

[0048] 7 and 8, in Experimental Examples 6 to 7 and Comparative Example 3, there was no significant difference in the polishing rate over the entire surface of the workpiece W, so it is believed that the DIW did not have any adverse effects such as diluting the slurry S and deteriorating the polishing rate, and that the presence of DIW suppressed the adhesion of the slurry to the upper surface Wa of the workpiece W.

[0049] Furthermore, the present invention can be modified in various ways other than those described above without departing from the spirit of the present invention, and it goes without saying that the present invention extends to such modifications. [Explanation of symbols]

[0050] 1:CMP equipment 2: Platen 3: (Platen) rotation axis 4: Motor 5: Polishing pad 6: Nozzle 7: Controller 10: Polishing head 10a: Rotating shaft (of polishing head) 20: Head body 21:Connection part 30: Career 30a: (Carrier) bottom surface 31: Fluid supply line 32 :Fluid supply source 33: Carrier pressing means 40: Retainer ring 40a: Storage pocket 40b: Top surface (of retainer ring) 41: Retainer holder 41a: (retainer holder) bottom surface 42: Snap ring 43: Retainer pressing member 44: Retainer pressing means 45: Cover 50:Membrane film 60: Backing film 70:Communication hole C: Pressure propagation chamber S: Slurry V: Vertical direction W: Work Wa: Top surface (of workpiece)

Claims

1. A CMP apparatus that presses a workpiece against a polishing pad to polish it, a substantially annular retainer ring having a central storage pocket capable of storing the workpiece and surrounding a lower end of the carrier; a membrane film whose periphery is held by the retainer ring to form a pressure transmission chamber between the membrane film and the carrier; A backing film that is joined to the membrane film in the storage pocket and is capable of holding the workpiece; a fluid supply source that supplies a pressurized fluid including moisturizing water to the pressure transmission chamber; Equipped with A CMP apparatus characterized in that, when the workpiece is polished, the pressurized fluid is supplied into the storage pocket through communication holes formed in the membrane film and the backing film so as to connect the pressure transmission chamber and the storage pocket.

2. 2. The CMP apparatus according to claim 1, wherein the pressurized fluid is filled between the workpiece and the backing film when the workpiece is polished.

3. 2. The CMP apparatus according to claim 1, wherein the pressurized fluid is mist air made by mixing DIW and compressed air.

4. 2. The CMP apparatus according to claim 1, wherein the pressurized fluid is DIW.

Citation Information

Patent Citations

  • Polishing head structure for polishing device

    JP2001212754A

Cited By

  • CMP device

    JP2026164210A