Robot arm

By press-heat-molding a composite resin on the FRP cylindrical body of a robot arm, the robot arm achieves high torsional strength and stable fixing strength, addressing the strength deficiencies of conventional FRP robot arms for collaborative human operation.

JP2024133260AActive Publication Date: 2024-10-01SANGO GOSEI
View PDF 20 Cites 0 Cited by

Patent Information

Application Number
JP2024113065
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2024-07-16
Publication Date
2024-10-01
Estimated Expiration
2041-01-28

AI Technical Summary

Technical Problem

Conventional robot arms made of thermosetting FRP lack sufficient strength, particularly at the joint portions where functional parts are attached, and existing joining methods fail to provide stable fixing strength.

Method used

The robot arm is formed by press-heat-molding a composite resin of thermosetting resin and fibers on the outer and inner surfaces of a thermosetting FRP cylindrical body, with a mounting member assembled inside the cylindrical body and secured using bolts, and a composite resin layer is formed on the outer surface to enhance torsional strength and fixing strength.

Benefits of technology

The robot arm achieves high torsional strength and stable fixing strength at the mounting portions, ensuring safety and lightweight operation, suitable for collaborative work with humans.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024133260000001_ABST
    Figure 2024133260000001_ABST
Patent Text Reader

Abstract

To provide a robot arm in which while a required high torsional strength is secured, weight is sufficiently light by attaching a functional portion to a main body portion of the robot arm, the main body portion being formed as a thermoplastic setting FRP made, cylindrical body, and safety is high as a robot arm operating among human beings, with a human being, or assisting a human being, and particularly to provide a robot arm having a high fixing strength in the mounting portion of a mounting member.SOLUTION: In a robot arm 5, a closed space 10 is provided in a fitting portion of an inner side surface 6b of an end portion of a thermoplastic setting FRP made, cylindrical body 6 and a mounting member 9, and a composite resin layer 8b formed by combining a thermoplastic resin and fiber is molded in this closed space 10 under pressure and heat; a mounting member 9 assembled by its being fitted in an inside diameter of the end portion of thermoplastic setting FRP made, cylindrical body 6 and the thermoplastic setting FRP made, cylindrical body 6 are fastened to each other with a bolt 11; and the composite resin layer 8a formed by combining a thermoplastic resin and fiber is molded on an outer side surface 6a of the end portion of the thermoplastic setting FRP made, cylindrical body 6 under pressure and heat.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a robot arm formed by pressurizing and heating a resin composite of thermosetting resin and fiber onto at least one of the outer and inner surfaces of a thermosetting FRP cylindrical body. [Background technology]

[0002] In general, industrial robots used for laser processing, etc., require tip precision of about 1 / 100 mm, which requires high rigidity. In recent years, however, with the progress of the declining birthrate and aging population, there is an increasing need for industrial robots that work together with humans or assist humans. Such industrial robots do not require high rigidity like conventional industrial robots, but rather are strongly desired to be lightweight from the viewpoints of energy saving and global environmental conservation. As one of the means, it has been considered to replace the main body of the robot arm with a thermosetting FRP cylindrical body. In this case, various reinforcing fibers are used, such as carbon fiber, glass fiber, and aramid fiber, but among these, CFRP (carbon fiber reinforced plastics), which uses carbon fiber as the reinforcing fiber, which is excellent in terms of specific strength and specific elastic modulus, is considered to be particularly promising.

[0003] This robot arm, whose main body is a cylindrical body made of thermosetting FRP, needs to be able to perform various functions by attaching functional parts to the main body. To attach the functional parts to the main body made of this cylindrical body made of thermosetting FRP, a joining method that is balanced with the torsional strength of the cylindrical body made of thermosetting FRP is required.

[0004] Patent Document 1 discloses a mechanical equipment part in which a metal joint is press-fitted into the end of an FRP cylinder, the mechanical equipment part having an FRP cylinder and a metal joint press-fitted into the end of the FRP cylinder, with the objective of providing a structure that prevents damage from occurring at the end of the FRP cylinder due to the press-fit joining operation of the metal joint while ensuring the required high torsional strength, and that also prevents the progression of deterioration of that part. The mechanical equipment part is characterized in that a slit is made in the axial direction from the end face of the FRP cylinder. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2006-103032 A Summary of the Invention [Problem to be solved by the invention]

[0006] However, the mechanical equipment part disclosed in Patent Document 1 had a problem in that it was not possible to obtain sufficient strength, particularly in the joints where other members were attached to the FRP cylinder that constituted the robot arm. Conventionally, the FRP cylinder that constituted the robot arm was generally made by cutting an FRP cylinder about 3 m thick to a specified length, and fixing attachment members for other members to the inside of both ends. In this case, the mounting member was press-fitted into the mounting member fitting portion formed on the inside of the end of the FRP cylinder, and then the bolt was inserted through the mounting member fitting portion from the outside of the end of the FRP cylinder and fastened with the bolt. However, this did not provide sufficient fixing strength. In that case, even if a measure is taken such as applying an adhesive to the fitting portion of the mounting member before press-fitting the mounting member, the adhesive may run off, resulting in unstable fixing strength.

[0007] In view of the problems in the prior art described above, the object of the present invention is to provide a robot arm which has a main body made of a cylindrical thermosetting FRP body to which a functional part is attached, thereby making it sufficiently lightweight and highly safe for use among humans, together with humans, or assisting humans, while ensuring the necessary high torsional strength, and in particular to provide a robot arm with strong fixing strength at the mounting parts of its attachment members. [Means for solving the problem]

[0008] That is, the robot arm according to the present invention is characterized in that it is formed by pressurizing and heating a resin composite of thermosetting resin and fiber onto at least one of the outer and inner surfaces of a cylindrical body made of thermosetting FRP.

[0009] The robot arm according to the present invention is also characterized in that it is formed by pressurizing and heating a resin composite of thermosetting resin and fiber onto at least one of the outer and inner surfaces of the end of a cylindrical body made of thermosetting FRP.

[0010] Furthermore, the robot arm of the present invention is a robot arm having an attachment member attached to the inner diameter of the end of a thermosetting FRP cylindrical body, and is characterized in that an attachment part that fits inside the end of the thermosetting FRP cylindrical body is formed by pressurizing and heating a resin composite of thermosetting resin and fiber onto the inner surface of the end of the thermosetting FRP cylindrical body.

[0011] In addition, the robot arm of the present invention is a robot arm that is assembled by fitting an attachment member to the inner diameter of the end of a cylindrical body made of thermosetting FRP, and is characterized in that it is formed by pressurizing and heating a resin that is a composite of thermosetting resin and fiber onto the outer surface of the end of the cylindrical body made of thermosetting FRP.

[0012] In addition, the robot arm of the present invention is a robot arm assembled by fitting an attachment member to the inner diameter of the end of a cylindrical body made of thermosetting FRP, and is characterized in that a closed space is provided at the fitting portion between the inner surface of the end of the cylindrical body made of thermosetting FRP and the attachment member, and a resin composite of thermosetting resin and fiber is pressurized and heated to form in this space.

[0013] Furthermore, the robot arm of the present invention is characterized in that an attachment member is fitted and assembled to the inner diameter of the end of a thermosetting FRP cylindrical body, and the thermosetting FRP cylindrical body is fastened to the attachment member with screws, and a resin composite of thermosetting resin and fiber is pressurized and heated to be molded onto the outer surface of the end of the thermosetting FRP cylindrical body.

[0014] The manufacturing method of a robot arm of the present invention is characterized by comprising an inner diameter lamination process for forming a composite resin layer on the outer surface of a mounting member, a preforming and solidifying process, a pressing process for pressing and fitting the mounting member, which has been subjected to the preforming and solidifying process and has a fiber molded raw material placed on its outer surface, into the inside of the end of a thermosetting FRP cylindrical body, a bolt tightening process for fastening the mounting member pressed and fitted to the inside of the end of the thermosetting FRP cylindrical body by the pressing process to the thermosetting FRP cylindrical body with bolts, and an outer diameter lamination process for forming a composite resin layer on the outer surface of the thermosetting FRP cylindrical body.

[0015] It is preferable that the inner diameter lamination step and the preforming and solidifying step are carried out by placing a fiber forming raw material in a recess formed in the outer surface of the mounting member.

[0016] The outer lamination step is preferably performed by winding a pressure tape around the outside of the fiber forming raw material wound around the outer surface of the thermosetting FRP cylindrical body, and then applying pressure to perform the forming step.

[0017] For the thermosetting FRP cylindrical body, it is particularly preferable that the reinforcing fibers contain at least carbon fibers excellent in specific strength and specific elastic modulus, from the viewpoint of realizing high strength and torsional torque transmission characteristics. Effect of the Invention

[0018] The robot arm of the present invention can be made to have the requisite high torsional strength while being sufficiently lightweight and highly safe as a mechanical device that operates between humans, together with humans, or assisting humans, and in particular can be made to have strong fixing strength at the mounting portion of the mounting member. [Brief description of the drawings]

[0019] [Figure 1] 1(a) is a schematic diagram of a shaped raw cloth material used in the shaping method of the present invention, and (b) is a schematic diagram of a woven fabric base material constituting the shaped raw cloth material shown in FIG. [Diagram 2] FIG. 1 is a perspective view of a robot arm according to an embodiment of the present invention. [Diagram 3] FIG. 3 is a partial longitudinal sectional view of the robot arm of FIG. 2. [Figure 4] FIG. 3 is a partial cross-sectional view of the robot arm of FIG. 2. [Diagram 5] FIG. 4 is a perspective view showing the same part as the partial cross-sectional view of FIG. [Figure 6] 11A to 11C are other explanatory diagrams of the embodiment of the manufacturing method for a robot arm of the present invention. [Figure 7] 11A to 11C are other explanatory diagrams of the embodiment of the manufacturing method for a robot arm of the present invention. [Figure 8] 11A to 11C are other explanatory diagrams of the embodiment of the manufacturing method for a robot arm of the present invention. [Figure 9] 11A to 11C are other explanatory diagrams of the embodiment of the manufacturing method for a robot arm of the present invention. [Figure 10] 11A to 11C are other explanatory diagrams of the embodiment of the manufacturing method for a robot arm of the present invention. [Figure 11] 11A to 11C are other explanatory diagrams of the embodiment of the manufacturing method for a robot arm of the present invention. [Figure 12] 11A to 11C are other explanatory diagrams of the embodiment of the manufacturing method for a robot arm of the present invention. [Figure 13]1A to 1C are explanatory diagrams of an embodiment of a manufacturing method for a robot arm of the present invention. [Figure 14] 14 is a partial vertical sectional view of a robot arm according to another embodiment of the present invention. [Figure 15] FIG. 15 is a graph showing the results of measuring the safety factor when a load of 60 kgm of bending strength is applied to the robot arm 5 according to the embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0020] The fiber material used in manufacturing the robot arm according to the embodiment of the present invention will be described below. The robot arm according to the embodiment of the present invention is manufactured using a raw material 1 for molding shown in Fig. 1(a). As shown in Fig. 1(a), the raw material 1 for molding is formed by adhering a resin material 4 mainly composed of a thermosetting resin to at least one surface of a woven fabric substrate 3 including a plurality of reinforcing fiber bundles 2.

[0021] The woven fabric substrate 3 is a bidirectional fabric obtained by weaving a plurality of reinforcing fiber bundles 2, which are aligned in one direction so as to be parallel to each other, in two directions that intersect at right angles, as shown in Fig. 1(b). The bidirectional fabric has the advantages that it is easily deformed into a three-dimensional shape due to changes in the relative positions of the reinforcing fiber bundles 2, and that it is easy to obtain a laminated molding material having mechanical pseudo-isotropy with a small number of sheets. The reinforcing fiber bundles 2 may be carbon fiber bundles, graphite fiber bundles, glass fiber bundles, aramid fiber bundles, or the like, and are preferably carbon fiber bundles. By using the carbon fiber bundles, the mechanical properties of the final product, that is, the fiber-reinforced resin molded product, can be improved.

[0022] The resin material 4 attached to the surface of the textile substrate 3 is mainly composed of a thermosetting resin capable of bonding the layers of the textile substrate 3. Examples of thermosetting resins include epoxy, urethane, and polyester. By making the resin material 4 mainly composed of a thermosetting resin, the handling property is improved when bonding the layers of the textile substrate 3 after laminating the forming raw cloth material 1 and transforming it into a three-dimensional shape, and the productivity is improved. The main component is the component that has the largest proportion among the components constituting the resin material 4.

[0023] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. FIG. 2 shows a robot arm 5 according to one embodiment of the present invention. The robot arm 5 is formed by injection molding an FRP cylinder 6, which is one embodiment of a thermosetting FRP cylindrical body, with a resin composite of thermosetting resin and fiber, and functional parts 7a, 7b made of a composite resin composite of thermosetting resin and fiber are molded on the outer diameter side of both ends of the FRP cylinder 6. The functional parts 7a, 7b function as, for example, joints with operating parts, gripping parts, joints, etc. (not shown).

[0024] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. FIG. 2 shows a robot arm 5 according to one embodiment of the present invention. The robot arm 5 is formed by pressurizing and heating an FRP cylinder 6, which is one embodiment of a thermosetting FRP cylindrical body, with a resin composite of thermosetting resin and fiber, and functional parts 7a and 7b made of a composite resin composite of thermosetting resin and fiber are molded on the outer diameter sides of both ends of the FRP cylinder 6. The functional parts 7a and 7b function as, for example, joints with operating parts, gripping parts, joints, etc. (not shown).

[0025] The robot arm 5 according to this embodiment is formed by pressurizing and heating composite resin layers 8a, 8b, which are a composite of thermosetting resin and fiber, on at least one of the outer surface 6a and the inner surface 6b of a cylindrical body 6 made of thermosetting FRP, as shown in Figures 3, 5, and 4.

[0026] Specifically, the robot arm 5 according to this embodiment is formed by pressurizing and heating resin layers 8a, 8b, which are a composite of thermosetting resin and fiber, on at least one of the outer surface 6a and the inner surface 6b of the end A of a cylindrical body 6 made of thermosetting FRP.

[0027] Furthermore, the robot arm 5 in this embodiment is a robot arm 5 in which an attachment member 9 is attached to the inner diameter of the end A of the thermosetting FRP cylindrical body 6, and a composite resin layer 8b composed of a thermosetting resin and fiber is pressurized and heated and molded on the inner surface 6b of the end of the thermosetting FRP cylindrical body 6 to form a closed space 10, which is an attachment part that fits inside the end of the thermosetting FRP cylindrical body 6.

[0028] In addition, the robot arm 5 according to this embodiment is a robot arm 5 in which an attachment member 9 is fitted to the inner diameter of the end of a cylindrical body 6 made of thermosetting FRP, and a composite resin layer 8a made of a thermosetting resin and fiber is pressurized and heated and molded onto the outer surface 6a of the end of the cylindrical body 6 made of thermosetting FRP.

[0029] In addition, the robot arm 5 according to this embodiment is a robot arm 5 in which an attachment member 9 is fitted to the inner diameter of the end of a cylindrical body 6 made of thermosetting FRP, and a closed space 10 serving as an attachment portion is provided at the fitting portion between the inner surface 6b of the end of the cylindrical body 6 made of thermosetting FRP and the attachment member 9, and a composite resin layer 8b made of a composite of thermosetting resin and fiber is pressurized and heated and molded into this closed space 10.

[0030] In addition, the robot arm 5 in this embodiment is formed by fastening the thermosetting FRP cylindrical body 6 and the mounting member 9 fitted and assembled to the inner diameter of the end of the thermosetting FRP cylindrical body 6 with bolts 11, and by pressurizing and heating a composite resin layer 8a made of a composite of thermosetting resin and fiber onto the outer surface 6a of the end of the thermosetting FRP cylindrical body 6.

[0031] A manufacturing process for the robot arm 5 according to the above embodiment will be described below. First, an inner diameter lamination process is performed to form a composite resin layer 8b on the outer surface of the mounting member 9. As shown in Fig. 6, a fiber forming raw cloth material 1 is placed in a recess 10 formed on the outer surface of the mounting member 9. At this time, the environmental temperature is 20°C, and the workpiece temperature is about 30°C.

[0032] Next, the preforming and solidifying process is performed as shown in Figure 7. In the preforming process, the environmental temperature is set to 50°C, and the workpiece temperature is set to about 50°C. In the solidifying process, the environmental temperature is set to -15°C, and the workpiece temperature is set to about -15°C. Next, a press-fitting process is performed as shown in Fig. 8. The press-fitting process is performed by placing the fiber forming raw material 1 in a recess 10 formed on the outer surface of the inside of the end of the thermosetting FRP cylindrical body 6, and press-fitting the mounting member 9 that has been subjected to the preliminary forming and solidification process. The environmental temperature during the press-fitting process is set to 20°C, and the workpiece temperature is set to about -15°C.

[0033] Next, a bolt tightening process is performed as shown in Fig. 9. In this bolt tightening process, the mounting member 9 that has been press-fitted and joined to the inside of the end of the thermosetting FRP cylindrical body 6 in the press-fitting process is fastened to the thermosetting FRP cylindrical body 6 by the bolt 11. The environmental temperature in this bolt tightening process is set to 20°C, and the workpiece temperature is set to about 20°C.

[0034] Next, an outer diameter lamination process is performed to form a composite resin layer 8a on the outer surface of the thermosetting FRP cylindrical body 6. In this outer diameter lamination process, first, the fiber forming raw material 1 is wound around the outer surface of the thermosetting FRP cylindrical body 6 as shown in Fig. 10. At this time, the environmental temperature is 20°C, and the workpiece temperature is about 30°C. 11, a pressure tape 12 is wound around the fiber forming raw material 1 wound around the outer surface of the thermosetting FRP cylindrical body 6, and an outer diameter pressure tape winding process is performed to apply pressure. At this time, the environmental temperature is 20°C, and the workpiece temperature is about 30°C.

[0035] In this state, the forming process is carried out as shown in Fig. 12. The environmental temperature in this forming process is 80°C, and the workpiece temperature is kept at about 80°C for 2 hours. Finally, the pressure tape is removed as shown in FIG. 13, completing the manufacture of the robot arm 5 according to the embodiment of the present invention.

[0036] 14 shows a partial vertical cross-sectional view of a robot arm according to another embodiment of the present invention. The robot arm 5 of this embodiment is otherwise similar to the robot arm 5 of the above-mentioned embodiment, but differs in that it is provided with an integrated connecting part 8a which is a composite resin layer formed by injection molding using a resin composited with fibers, connecting the outer surface of the end of the thermosetting FRP cylindrical body 6 provided with the recess 9a and through hole 6a of the mounting member 9 and the through hole 6c of the thermosetting FRP cylindrical body 6 and the closed space 10 of the fitting part of the mounting member 9.

[0037] FIG. 15 shows the results of measuring the safety factor when a bending strength load of 60 kgm is applied to the robot arm 5 according to the embodiment of the present invention. As shown in the figure, the thermosetting FRP cylindrical body 6 alone has a safety factor of 11.1, whereas when the mounting member 9 is simply press-fitted into the inside of the end of the thermosetting FRP cylindrical body 6, the safety factor is 0.5, and when the fiber molding raw material 1 is placed and molded on the inside of the end of the thermosetting FRP cylindrical body 6 but outside the mounting member 9, and on the outside of the end of the thermosetting FRP cylindrical body 6, the safety factor is 5.5. In contrast, the robot arm 5 according to the embodiment of the present invention, which is fastened with bolts 11 and has fiber molding raw material 1 placed on the inside and outside, reached a safety factor of 9.0. [Explanation of symbols]

[0038] 5...Robot arm, 6...Thermosetting FRP cylindrical body, 7a, 7b...Functional parts, 8...Composite resin layer.

Claims

1. A robot arm characterized by being formed by pressurizing and heating a composite resin of thermosetting resin and fiber onto at least one of the outer and inner surfaces of a cylindrical body made of thermosetting FRP.

2. A robot arm characterized by being formed by pressurizing and heating a composite resin of thermosetting resin and fiber onto at least one of the outer and inner surfaces of the end of a cylindrical body made of thermosetting FRP.

3. A robot arm having an attachment member attached to the inner diameter of the end of a cylindrical body made of thermosetting FRP, characterized in that a resin composite of thermosetting resin and fiber is pressurized and heated to form an attachment portion that fits inside the end of the cylindrical body made of thermosetting FRP on the inner surface of the end of the cylindrical body made of thermosetting FRP.

4. A robot arm in which an attachment member is fitted to the inner diameter of the end of a cylindrical body made of thermosetting FRP, and which is formed by pressurizing and heating a resin composite of thermosetting resin and fiber onto the outer surface of the end of the cylindrical body made of thermosetting FRP.

5. 5. The robot arm according to claim 4, wherein a composite resin of thermosetting resin and fiber is pressurized and heated between the outer surface of the end of the thermosetting FRP cylindrical body and the concave surface of the mounting member.

6. This robot arm is constructed by fitting and assembling an attachment member to the inner diameter of the end of a cylindrical body made of thermosetting FRP, and is characterized in that the outer surface of the end of the cylindrical body made of thermosetting FRP and the concave surface of the attachment member are injection molded with a resin composited with fibers.

7. A robot arm as described in claim 6, which is formed by connecting the outer surface of the end of a cylindrical body made of thermosetting FRP, which has a recess for a mounting member and a through hole, the through hole of the cylinder, and the concave surface of the fitting portion of the mounting member, and then injection molding the resin composited with fibers.

8. This robot arm is assembled by fitting an attachment member to the inner diameter of the end of a cylindrical body made of thermosetting FRP, and is characterized in that a closed space is provided at the fitting portion between the inner surface of the end of the cylindrical body made of thermosetting FRP and the attachment member, and a resin composite of thermosetting resin and fiber is pressurized and heated to form into this space.

9. A robot arm characterized in that an attachment member is fitted and assembled to the inner diameter of the end of a thermosetting FRP cylindrical body, and the thermosetting FRP cylindrical body is fastened to the attachment member with screws, and a resin composite of thermosetting resin and fiber is pressurized and heated to be molded onto the outer surface of the end of the thermosetting FRP cylindrical body.

10. 1. A method for manufacturing a robot arm, comprising: an inner diameter lamination step of forming a composite resin layer on the outer surface of a mounting member; a preforming and solidifying step; a press-in step of pressing in and fitting a mounting member, which has been subjected to the preforming and solidifying step by placing a fiber molding raw material on its outer surface, to the inside of an end of a thermosetting FRP cylindrical body; a bolt tightening step of fastening the mounting member pressed in and fitted to the inside of the end of the thermosetting FRP cylindrical body by bolts; and an outer diameter lamination step of forming a composite resin layer on the outer surface of the thermosetting FRP cylindrical body.

11. 8. The method for manufacturing a robot arm according to claim 7, wherein the inner diameter lamination step and the preforming and solidifying step are performed by placing a fiber-formed raw cloth material in a recess formed in the outer surface of the mounting member.

12. 9. The method for manufacturing a robot arm according to claim 7 or 8, wherein the outer diameter lamination step comprises winding a pressure tape around the outside of a fiber molding raw material wound around the outer surface of a thermosetting FRP cylindrical body, and applying pressure to the fiber molding process.

Citation Information

Patent Citations

  • JP1980013133U

  • Joint construction of FRP pipe and metal coupling

    JP1983090917A

  • Jointing method of metal pipe and fiber reinforced synthetic resin pipe

    JP1983215310A

  • JP1987050316U

  • Tubular body using composite material

    JP1988214427A