Manufacturing method of foam-molded product, and molding die
The method addresses the inefficiencies in conventional foam molded product manufacturing by employing direct heating and cooling techniques through the mold's back surfaces and strategic design, resulting in a substantial reduction of the manufacturing cycle.
Patent Information
- Application Number
- JP2023044513
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-20
- Publication Date
- 2024-10-03
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Conventional methods for manufacturing foam molded products involve multiple steps and lengthy manufacturing cycles due to inefficient heating and cooling processes.
A method involving direct heating and cooling of the mold using infrared rays and mist/high-pressure air through exposed back surfaces, combined with a mold design featuring through holes and exposure openings, allows for efficient heating and cooling of the mold.
This approach significantly shortens the manufacturing cycle by enabling rapid heating and cooling of the mold, reducing the overall production time.
Smart Images

Figure 2024134288000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for producing a foam-molded product and a molding die. [Background technology]
[0002] It has been proposed to produce foam-molded products of a predetermined shape, for example, as follows (for example, Patent Document 1). First, a foaming agent and a crosslinking agent are added to and kneaded with a polyolefin resin, and the resulting crosslinkable foamable composition is filled into a closed mold A, heated under pressure, shaped, and an intermediate molded product is removed. Next, the intermediate molded product is placed into a closed mold B separate from the closed mold A, heated under pressure to decompose the foaming agent and crosslinking agent, and then cooled to obtain a foam smaller than the intermediate molded product. The resulting foam is then placed into mold C, heated under pressure, and thermocompression molded to obtain a foam-molded product of the desired shape. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2009-255366 A Summary of the Invention [Problem to be solved by the invention]
[0004] The above-mentioned method has many steps since it involves a primary step to obtain an intermediate molded product, a secondary step to obtain a foamed body, and a tertiary step to obtain a foamed molded product. In addition, it may take time to heat and cool the mold, which results in a long production cycle.
[0005] The present invention has been proposed in view of the above-mentioned problems associated with the conventional technology, and aims to provide a method for producing a foam-molded product and a molding die that can shorten the production cycle. [Means for solving the problem]
[0006] The first aspect of the method for producing an expansion molded product according to the present invention is an injection step of injecting an unfoamed solid raw material containing a foaming agent into a molding surface of a mold that forms a cavity; a heating step of heating the mold from the outside with infrared rays after the injection step; A cooling step of cooling the mold after the heating step, The heating step is characterized in that the rear surface of the mold opposite to the molding surface is directly heated with the infrared rays.
[0007] A second aspect of the method for producing an expansion-molded product according to the present invention is the same as the first aspect, In the cooling step, the forming mold may be cooled by spraying mist and high-pressure air onto a rear surface of the mold.
[0008] A first aspect of the mold according to the present invention is A mold for forming a foam-molded product using an unfoamed solid raw material containing a foaming agent, a mold portion having a molding surface forming a cavity; A support portion that supports the mold portion, The mold section is provided with a plurality of through holes leading from the molding surface to a mold back surface on the opposite side to the molding surface, The support portion has an exposure opening for exposing the rear surface of the mold to the outside.
[0009] A second aspect of the mold according to the present invention is the mold according to the first aspect of the present invention, The mold section closes a first mold and a second mold to form the cavity, The plurality of through holes may be provided in the mold portions of both the first mold and the second mold. Effect of the Invention
[0010] According to the method for producing an expansion-molded product of the present invention, the molding mold can be efficiently heated and cooled, thereby shortening the production cycle. According to the molding die of the present invention, heating and cooling can be performed efficiently, thereby shortening the production cycle. [Brief description of the drawings]
[0011] [Figure 1] FIG. 2 is a schematic perspective view of a molding die in an open state. [Diagram 2] FIG. 2 is a schematic perspective view of a molding die in a closed state. [Diagram 3] FIG. 2 is a schematic perspective view of a first die of a molding die as viewed from below. [Figure 4] FIG. 2 is an explanatory diagram showing a step of supplying a solid raw material to a molding die in the process of producing a foam-molded product. [Diagram 5] FIG. 2 is an explanatory diagram showing a step of closing a molding die in the process for producing an expansion-molded product. [Figure 6] FIG. 2 is an explanatory diagram showing a step of heating a molding die in the process for producing an expansion-molded product. [Figure 7] FIG. 2 is an explanatory diagram showing a step in the manufacturing process of a foam-molded product in which the foam-molded product foams and expands. [Figure 8] 8 is an enlarged cross-sectional view showing a part of the mold of FIG. 7. [Figure 9] FIG. 2 is an explanatory diagram showing a step of cooling a molding die in the process for producing an expansion-molded product. [Figure 10] FIG. 2 is an explanatory diagram showing a step of opening a molding die in the process for producing an expansion-molded product. [Figure 11] FIG. 2 is an explanatory diagram showing a step of demolding the foam-molded article in the manufacturing process of the foam-molded article. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Next, the manufacturing method and molding die for a foam-molded product according to the present invention will be described below with reference to the accompanying drawings, using preferred examples. The embodiments and drawings described below are intended to illustrate a part of the embodiment of the present invention, and are not intended to be used for the purpose of limiting the present invention to these configurations, and may be modified as appropriate within the scope of the present invention. EXAMPLES
[0013] The manufacturing apparatus for manufacturing the foam-molded article 50 includes a mold 10 (see Figs. 1 and 2) for molding the foam-molded article 50, a heating means 12 (see Figs. 6 and 7) for heating the mold 10, and a cooling means 14 (see Fig. 9) for cooling the mold 10. The manufacturing apparatus may also include demolding assistance means 16 (Figs. 10 and 11) for assisting in demolding the obtained foam-molded article 50 from the mold 10. The foam-molded article 50 is, for example, a molded article of a polyolefin-based foam such as polyethylene or polypropylene.
[0014] The mold 10 shown in Figs. 1 and 2 is used to mold an expansion-molded product 50 using an unfoamed solid raw material 40 (see Fig. 6) containing a foaming agent. The mold 10 includes a first mold 20 and a second mold 30 that can be opened and closed relative to the first mold 20. In the mold 10, a cavity 10a is formed between the first mold 20 and the second mold 30 when the molds are closed (see Figs. 5 to 9). In the embodiment, the first mold 20 is a female mold having a concave first molding surface 22a, and the second mold 30 is a male mold having a convex second molding surface 32a (see Fig. 4). In the mold 10, when the molds are closed, the second mold 30 is disposed above the first mold 20 (see Figs. 2 and 5).
[0015] As shown in FIG. 1 and FIG. 3, the first mold 20 includes a first mold section (mold section) 22 having a first molding surface (molding surface) 22a forming the cavity 10a, and a first support section (support section) 24 supporting the first mold section 22. The first mold section 22 is provided with a plurality of first through holes (through holes) 23 (see FIG. 8) leading from the first molding surface 22a to a first mold back surface (mold back surface) 22b on the opposite side to the first molding surface 22a. The first mold section 22 is plate-shaped. The first mold back surface 22b of the first mold section 22 is uneven in accordance with the unevenness of the first molding surface 22a (see FIG. 4). The first support section 24 has a first exposure opening (exposure opening) 24a that exposes the first mold back surface 22b to the outside. The first support section 24 of the embodiment is arranged in the form of a wall surrounding the first mold back surface 22b on the lower surface of the outer edge of the rectangular plate-shaped first mold section 22. In this way, the first support part 24 supports the outer periphery of the first mold part 22 on the first mold back surface 22b side. The lower end of the first support part 24 is located below the first mold back surface 22b, which has a convex shape that protrudes downward. The first exposed opening 24a is formed surrounded by the first support part 24. The first exposed opening 24a is arranged at a position overlapping the first mold back surface 22b below the first mold back surface 22b, and the lower side of the first mold back surface 22b is opened by the first exposed opening 24a. In this way, in the first mold 20, the lower side of the first mold back surface 22b is not blocked by a chamber or the like.
[0016] As shown in Figs. 1 to 3, the first mold 20 has an air supply section 26. The air supply section 26 is provided in the first support section 24. The air supply section 26 is a cylindrical member that protrudes outward from the first support section 24, communicates with the inside and outside of the first support section 24, and can be connected to the demolding auxiliary means 16 (see Figs. 10 and 11). Therefore, the demolding auxiliary means 16 can send air into the space surrounded by the first mold section 22 and the first support section 24 in the first mold 20 via the air supply section 26.
[0017] As shown in FIG. 1 and FIG. 2, the second mold 30 includes a second mold section (mold section) 32 having a second molding surface (molding surface) 32a forming the cavity 10a, and a second support section (support section) 34 supporting the second mold section 32. The second mold section 32 is provided with a plurality of second through holes 33 (see FIG. 8) leading from the second molding surface 32a to a second mold back surface (mold back surface) 32b on the opposite side of the second molding surface 32a. The second mold section 32 is plate-shaped. The second mold back surface 32b of the second mold section 32 is uneven in accordance with the unevenness of the second molding surface 32a (see FIG. 4). The second support section 34 has a second exposure opening (exposure opening) 34a that exposes the second mold back surface 32b to the outside. The second support section 34 of the embodiment is arranged in the form of a wall surrounding the second mold back surface 32b on the upper surface of the outer edge of the rectangular plate-shaped second mold section 32. In this manner, the second support portion 34 supports the outer periphery of the second mold portion 32 on the second mold back surface 32b side. The second exposed opening 34a is formed surrounded by the second support portion 34. The second exposed opening 34a is disposed at a position overlapping the second mold back surface 32b on the upper side of the second mold back surface 32b, and the upper side of the second mold back surface 32b is opened by the second exposed opening 34a. In this manner, in the second mold 30, the upper side of the second mold back surface 32b is not blocked by a chamber or the like.
[0018] As shown in Figs. 1 to 3, the molding die 10 includes an attachment portion 28 used when the molding die 10 is set in a floating state. The attachment portion 28 is provided on the first die 20. The attachment portion 28 in the embodiment is an L-shaped plate member. One plate portion of the L-shaped plate member is fixed to the side surface of the first support portion 24 by welding or the like, whereby the attachment portion 28 is fixed to the first support portion 24. The attachment portion 28 is provided on both side surfaces of the first support portion 24 that sandwich the first exposed opening 24a. The other plate portion of the L-shaped plate member protrudes outward from the side surface of the first support portion 24. The attachment portion 28 is supported by an installation portion 42 (see Figs. 6 to 7 and 9) of the manufacturing apparatus, whereby the molding die 10 is set in a state in which the first exposed opening 24a and the second exposed opening 34a of the molding die 10 are opened.
[0019] The first mold part 22 and the second mold part 32 are preferably made of metal, and are particularly preferably made of nickel. The first mold part 22 and the second mold part 32 may be made of aluminum, which has excellent thermal conductivity, but nickel is preferable because it has good thermal conductivity and appropriate strength.
[0020] The plate thickness of the first mold part 22 and the second mold part 32 is not particularly limited, but is preferably about 3.0 mm to 5.0 mm. When the plate thickness of the first mold part 22 and the second mold part 32 is in the above range, when the first mold back surface 22b and the second mold back surface 32b are heated from the outside, heat is easily transferred to the first molding surface 22a and the second molding surface 32a. In addition, when the first mold back surface 22b and the second mold back surface 32b are cooled from the outside, heat in the cavity 10a is easily released to the outside.
[0021] The first mold part 22 and the second mold part 32 may be machined products, but are preferably electroformed products. When the first mold part 22 and the second mold part 32 are electroformed products, the plate-like first mold part 22 and the second mold part 32 can be formed thin.
[0022] The diameters of the through holes 23, 33 in the first mold section 22 and the second mold section 32 are not particularly limited, but are preferably set to about 0.1 mm to 0.3 mm. By setting the diameter within this range, it is possible to prevent traces of the through holes 23, 33 from remaining on the foam-molded product 50. The first through holes 23 in the first mold section 22 and the second through holes 33 in the second mold section 32 may have the same diameter or different diameters. The intervals between adjacent through holes 23, 33 in the first mold section 22 and the second mold section 32 are not particularly limited. The intervals between adjacent first through holes 23 in the first mold section 22 and the intervals between adjacent second through holes 33 in the second mold section 32 may be the same or different. Methods of forming the through holes 23, 33 include, for example, when the first mold part 22 and the second mold part 32 are electrocast products, forming them using a lost core when casting the first mold part 22 and the second mold part 32, or forming the first mold part 22 and the second mold part 32 using a porous electrocast mold.
[0023] The first support portion 24 and the second support portion 34 may be made of the same material as the first mold portion 22 and the second mold portion 32, but the first support portion 24 and the second support portion 34 in the embodiment are made of a different material than the first mold portion 22 and the second mold portion 32. For example, the first support portion 24 and the second support portion 34 may be made of a material having a lower thermal conductivity than the first mold portion 22 and the second mold portion 32, a material that is less easily heated by infrared rays than the first mold portion 22 and the second mold portion 32, or a material having a higher strength than the first mold portion 22 and the second mold portion 32, or the like.
[0024] Next, a description will be given of a manufacturing method of the foam-molded article 50 using the above-mentioned molding die 10. The manufacturing method of the embodiment includes an injection step of injecting unfoamed solid raw material 40 containing a foaming agent into molding surfaces 22a, 32a of the molding die 10 that form the cavity 10a, a heating step of heating the molding die 10 from the outside with infrared rays after the injection step, a cooling step of cooling the molding die 10 after the heating step, and a demolding step of demolding the foam-molded article 50 from the molding die 10 after the cooling step.
[0025] As shown in FIG. 4, in the injection step, the first mold 20 and the second mold 30 are opened, and the granular or pellet-like solid raw material 40 is supplied to the first molding surface 22a of the first mold portion 22 in the first mold 20. Here, the supply amount of the solid raw material 40 is set to be smaller than the volume of the cavity 10a. In the manufacturing method of the present disclosure, a method called starvation foaming is adopted in which the foamed material is filled into the cavity 10a by foaming and expanding the solid raw material 40, rather than densely filling the cavity 10a with foamed beads as in foamed bead molding. The injection step of the present disclosure does not require supplying the solid raw material 40 to the cavity 10a under pressure, or closing the mold 10 while compressing the solid raw material 40 supplied to the cavity 10a. In this way, since it is only necessary to put the solid raw material 40 into the first molding surface 22a, the efficiency of the injection step can be improved and the equipment related to the supply of the solid raw material 40 can be simplified. Then, as shown in Fig. 5, after the solid raw material 40 is supplied, the molding die 10 is closed. The solid raw material 40 contains a resin composition. The resin composition is not particularly limited, but examples thereof include polyolefin resins such as polyethylene (PE) and polypropylene (PP), and polyester elastomers (TPEE). The solid raw material 40 is not limited to a granular or pellet-like shape, and may be in a sheet-like shape or the like.
[0026] The solid raw material 40 contains a foaming agent. The foaming agent is preferably a thermal decomposition type that decomposes when heated to generate gas, and is not particularly limited. For example, one or more of azodicarbonamide (ADCA), 2,2'-azobisisobutyronitrile, diazoaminobenzene, benzenesulfonylhydrazide, benzene-1,3-sulfonylhydrazide, diphenyloxide-4,4'-disulfonylhydrazide, 4,4'-oxybisbenzenesulfonylhydrazide, paratoluenesulfonylhydrazide, N,N'-dinitrosopentamethylenetetramine, N,N'-dinitroso-N,N'-dimethylphthalamide, terephthalazide, pt-butylbenzazide, sodium bicarbonate, ammonium bicarbonate, etc. are used. In particular, azodicarbonamide and 4,4'-oxybisbenzenesulfonylhydrazide are preferred.
[0027] The solid raw material 40 may be one in which at least a part of the resin composition contained in the solid raw material 40 has been crosslinked by electron beam. The electron beam crosslinking is a crosslinked structure in which the resin composition contained in the solid raw material 40 is intermolecularly bonded by irradiating the solid raw material 40 with an electron beam. Such electron beam crosslinking is performed before the injection step.
[0028] The solid raw material 40 may contain a chemical crosslinking agent. The chemical crosslinking agent crosslinks the resin composition contained in the solid raw material 40 by heating. The chemical crosslinking agent is not particularly limited, and examples of the chemical crosslinking agent include organic peroxides such as dicumyl peroxide, 2,5-dimethyl-2,5-bis-tertiary butylperoxyhexane, and 1,3-bis-tertiary peroxy-isopropyl benzene.
[0029] As shown in FIG. 6 and FIG. 7, in the heating step, the mold 10 is installed in a floating state so as not to block the first exposed opening 24a and the second exposed opening 34a, by supporting the mounting portion 28 by the installation portion 42. In the heating step, infrared rays are irradiated from the heating means 12 installed on the lower side of the first mold 20 to heat the first mold part 22. Here, the lower heating means 12 is arranged at a position overlapping the first exposed opening 24a below the first exposed opening 24a, and irradiates infrared rays to the first mold back surface 22b through the first exposed opening 24a. In this way, in the heating step, the first mold back surface 22b opposite to the first molding surface 22a in the first mold part 22 is directly heated by infrared rays. Similarly, in the heating step, infrared rays are irradiated from the heating means 12 installed on the upper side of the second mold 30 to heat the second mold part 32. Here, the upper heating means 12 is disposed above the second exposed opening 34a at a position overlapping with the second exposed opening 34a, and irradiates the second mold back surface 32b with infrared rays through the second exposed opening 34a. Thus, in the heating step, the second mold back surface 32b opposite the second molding surface 32a in the second mold section 32 is directly heated with infrared rays.
[0030] The heating means 12 is capable of irradiating infrared rays (see the wavy arrows in Figs. 6 and 7), and examples thereof include an infrared heater. Near infrared rays or mid-infrared rays are preferable to far-infrared rays because they have a better heating efficiency for the first mold part 22 and the second mold part 32. Mid-infrared rays are also preferable to near-infrared rays because they provide a better balance between the heating efficiency for the first mold part 22 and the second mold part 32 and the reduction in the load on the first mold part 22 and the second mold part 32. The wavelength of near-infrared rays is in the range of approximately 0.75 μm or more and less than 2.5 μm, the wavelength of mid-infrared rays is in the range of approximately 2.5 μm or more and 4 μm or less, and the wavelength of far-infrared rays is in the range of approximately more than 4 μm and 1000 μm or less.
[0031] In the heating step, the first mold part 22 and the second mold part 32 are heated, so that the solid raw material 40 melts, and the melted resin composition is foamed and expanded by the gas generated by the decomposition of the foaming agent to become a foam. In addition, when the solid raw material 40 contains a chemical crosslinking agent, the resin composition is crosslinked to form a crosslinked structure. Then, excess gas such as air and foaming agent gas in the cavity 10a is discharged to the outside of the cavity 10a through the through holes 23, 33 provided in the first mold part 22 and the second mold part 32 as the resin composition foams and expands (see the straight arrows in Figures 7 and 8). In this way, in the heating step, excess gas is discharged from the cavity 10a through the multiple through holes 23, 33, so that molding defects such as underfilling can be avoided in the obtained foam-molded product 50. In particular, since the through holes 23, 33 are provided in both the first mold part 22 and the second mold part 32, excess gas can be smoothly discharged from the cavity 10a. Then, the foam-molded product 50 is formed in the cavity 10a.
[0032] As shown in FIG. 9, in the cooling step, the attachment portion 28 of the mold 10 is supported by the installation portion 42, and the mold 10 is installed in a floating state so as not to block the first exposed opening 24a and the second exposed opening 34a. In the cooling step, the mold 10 is cooled by spraying mist and high-pressure air to the mold back surfaces 22b, 32b. More specifically, in the cooling step, the mist is sprayed from the mist sprayer 14a installed below the first mold 20, and high-pressure air is sprayed from the air sprayer 14b to cool the first mold part 22. Here, the lower cooling means 14 (14a, 14b) is disposed below the first exposed opening 24a at a position overlapping the first exposed opening 24a, and sprays the mist and high-pressure air from the first exposed opening 24a to the first mold back surface 22b. In this way, in the cooling process, the first mold back surface 22b opposite to the first molding surface 22a in the first mold section 22 is directly cooled with mist and high-pressure air. Similarly, in the cooling process, mist is sprayed from the mist sprayer 14a installed on the upper side of the second mold 30, and high-pressure air is sprayed from the air sprayer 14b to cool the second mold section 32. Here, the upper cooling means 14 (14a, 14b) is disposed at a position overlapping with the second exposed opening 34a above the second exposed opening 34a, and sprays mist and high-pressure air from the second exposed opening 34a to the second mold back surface 32b. In this way, in the cooling process, the second mold back surface 32b opposite to the second molding surface 32a in the second mold section 32 is directly cooled with mist and high-pressure air. Note that the mist refers to fine water droplets sprayed in a mist state. Also, the high-pressure air refers to air with a pressure of 1.2 MPa or more. In the cooling process, the cooling efficiency can be improved by spraying high-pressure air together with the mist. However, if only the mist is sprayed, the cooling efficiency cannot be improved due to the Leidenfrost phenomenon.
[0033] As shown in Figs. 10 and 11, in the demolding step, the first mold 20 and the second mold 30 are opened. The first mold 20 is placed in a state in which the first exposed opening 24a is blocked by the blocking portion 44. In addition, the demolding auxiliary means 16 such as a compressor is connected to the air supply section 26. Then, air is blown from the demolding auxiliary means 16 into the space sealed by the first mold section 22, the first support section 24, and the blocking portion 44, and the air is blown out toward the first molding surface 22a through the multiple first through holes 23 in the first mold section 22. As a result, the foam-molded product 50 attached to the first molding surface 22a is peeled off from the first molding surface 22a, making it easier to remove the foam-molded product 50 from the first mold 20.
[0034] Since the first support part 24 of the first mold 20 described above has a first exposure opening 24a that exposes the first mold back surface 22b to the outside, infrared rays can be directly irradiated to the first mold back surface 22b through the first exposure opening 24a. Similarly, since the second support part 34 of the second mold 30 has a second exposure opening 34a that exposes the second mold back surface 32b to the outside, infrared rays can be directly irradiated to the second mold back surface 32b through the second exposure opening 34a. In this way, the first mold part 22 and the second mold part 32 of the forming mold 10 can be efficiently heated, and the heating process can be shortened. For example, since the first mold part 22 and the second mold part 32 can be heated to about 170°C to 180°C very quickly, the heating process can be shortened to about 10 minutes.
[0035] According to the above-mentioned mold 10, the first mold back surface 22b can be directly cooled through the first exposed opening 24a, and the second mold back surface 32b can be directly cooled through the second exposed opening 34a. In this way, the first mold part 22 and the second mold part 32 of the mold 10 can be efficiently cooled, and the cooling process can be shortened. In the cooling process, if the first mold back surface 22b and the second mold back surface 32b are cooled by blowing mist and high-pressure air, the occurrence of the Leidenfrost phenomenon is suppressed, and the mist attached to the first mold back surface 22b and the second mold back surface 32b efficiently removes heat when it evaporates, so that the cooling efficiency is good. For example, the first mold part 22 and the second mold part 32, which are 170°C to 180°C, can be cooled to about 50°C very quickly, and the cooling process can be shortened to about 1 minute.
[0036] According to the above-mentioned manufacturing method, each step of heating for foaming and crosslinking, molding of the foamed and expanded resin composition, and cooling can be performed in the same mold 10. Moreover, heating and cooling in the mold 10 can be performed efficiently. Thus, according to the above-mentioned molding die 10 and manufacturing method, the manufacturing cycle of the foam-molded product 50 can be significantly shortened. Furthermore, according to the molding die 10, when the solid raw material 40 is injected into the cavity 10a, it is not necessary to provide a pressure difference between the inside and outside of the cavity 10a, and it is not necessary to fill the outside of the mold back surface 22b, 32b of the mold parts 22, 32 with a heating medium such as steam in the heating step, and it is not necessary to fill the outside of the mold back surface 22b, 32b of the mold parts 22, 32 with a cooling medium such as water in the cooling step. Therefore, it is not necessary to provide a partitioned closed space such as a chamber outside the mold back surface 22b, 32b of the mold parts 22, 32, and the manufacturing device can be simplified.
[0037] This disclosure includes the following: A method for producing a foam-molded product, comprising placing an unfoamed solid raw material that has been crosslinked by electron beam and contains a foaming agent into a cavity of a mold having a plurality of through holes, and heating the solid raw material to foam it.
[0038] This disclosure includes the following: A method for producing a foam-molded product, comprising placing an unfoamed solid raw material containing a foaming agent and a chemical crosslinking agent in a cavity of a mold having a plurality of through holes, and heating the solid raw material to foam it.
[0039] This disclosure includes the following: A method for producing a foam-molded product, comprising placing an unfoamed polyolefin-based solid raw material containing a foaming agent in a cavity of a mold having a plurality of through holes, and heating the polyolefin-based solid raw material to foam it. [Explanation of symbols]
[0040] 10 Forming mold, 10a Cavity, 20 First mold, 22 First mold part (mold part), 22a First forming surface (forming surface), 22b First mold back surface (mold back surface), 23 First through hole (through hole), 24 First support part (support part), 24a First exposed opening (exposed opening), 30 Second mold, 32 Second mold part (mold part), 32a Second forming surface (forming surface), 32b Second mold back surface (mold back surface), 33 Second through hole (through hole), 34 Second support part (support part), 34a Second exposed opening (exposed opening)
Claims
1. an injection step of injecting an unfoamed solid raw material containing a foaming agent into a molding surface of a mold that forms a cavity; a heating step of heating the mold from the outside with infrared rays after the injection step; A cooling step of cooling the mold after the heating step, In the heating step, the rear surface of the mold opposite to the molding surface is directly heated by the infrared rays. A method for producing a foam-molded product, comprising the steps of:
2. The method for producing a foam-molded product according to claim 1 , wherein the cooling step cools the molding die by spraying mist and high-pressure air onto a rear surface of the die.
3. A mold for forming a foam-molded product using an unfoamed solid raw material containing a foaming agent, a mold portion having a molding surface forming a cavity; A support portion that supports the mold portion, The mold section is provided with a plurality of through holes leading from the molding surface to a mold back surface on the opposite side to the molding surface, The support portion has an exposure opening for exposing the rear surface of the mold to the outside. A molding die characterized by:
4. The mold section closes a first mold and a second mold to form the cavity, The mold according to claim 3 , wherein the plurality of through holes are provided in both the mold portions of the first mold and the second mold.
Citation Information