Manufacturing method of fastening structure
Patent Information
- Application Number
- JP2023045967
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-22
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2043-03-22
AI Technical Summary
【0010】 以上説明したように、本発明の締結構造体の製造方法によれば、セルフピアスリベットで締結される対象のうちセルフピアスリベットの先端側と接する部材がダイキャスト製品となる場合に、セルフピアスリベットの打ち込みに起因したダイキャスト製品の割れを抑制しつつ製造効率の向上を図ることが可能になるという優れた効果を有する。
Smart Images

Figure 2024135338000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a fastening structure. [Background technology]
[0002] Patent Document 1 below discloses a technique for joining (fastening) a pair of overlapping plate materials to be joined using a self-piercing rivet. To briefly explain this prior art, a self-piercing rivet joins a pair of plate materials to be joined by drilling holes in the pair of plate materials with a hollow leg. In this prior art, the joint joined by the self-piercing rivet is heated to increase the ductility of the joint and suppress the occurrence of fractures (cracks) in the joint. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2010-188383 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, there are cases where the member in contact with the tip side of the self-piercing rivet among the objects to be joined (fastened) with the self-piercing rivet is a die-cast product. In such cases, the above-mentioned prior art may be applicable, but there is room for improvement in terms of improving manufacturing efficiency.
[0005] In consideration of the above, an object of the present invention is to provide a method for manufacturing a fastening structure that can improve manufacturing efficiency while suppressing cracks in the die-cast product caused by the driving of the self-piercing rivet, when the member in contact with the tip side of the self-piercing rivet among the objects fastened with the self-piercing rivet is a die-cast product. [Means for solving the problem]
[0006] The method for manufacturing a fastening structure of the present invention described in claim 1 includes a molding step of molding a first member by die casting, and a driving step of driving a self-piercing rivet into a joint where a second member is overlapped on the first member from the side of the second member after the molding step, while heat from the molding process remains in the first member.
[0007] According to the above configuration, the first member is molded by die casting in the molding step. In the driving step after the molding step, while the heat from the molding remains in the first member, a self-piercing rivet is driven from the second member side into the overlapping portion where the first member and the second member are overlapped. As a result, the first member is more ductile than at room temperature when the self-piercing rivet is driven, so that the first member is less likely to crack in the driving step. In other words, the heat applied to the first member during molding of the first member can be effectively utilized to suppress cracking of the first member. Furthermore, in this method for manufacturing a fastening structure, the driving step is performed without waiting for the first member to cool after the molding step, so that the time until the first member cools can be effectively utilized and the manufacturing time of the fastening structure can be shortened.
[0008] The method for manufacturing a fastening structure of the present invention described in claim 2, in the configuration described in claim 1, heats the portion of the first member that overlaps with the second member from a support member that supports the first member from the side opposite the driving side of the self-pierce rivet in the driving process.
[0009] According to the above configuration, in the driving step, the portion of the first member that overlaps with the second member is heated by the support member that supports the first member from the side opposite to the driving side of the self-piercing rivet. This makes it possible to further increase the ductility of the first member in the driving step, making the first member even less likely to crack in the driving step. In addition, because the heat generated during the forming of the first member remains in the first member, the amount of heat required to ensure good ductility of the first member can be reduced. Effect of the Invention
[0010] As described above, the manufacturing method of the fastening structure of the present invention has the excellent effect of making it possible to improve manufacturing efficiency while suppressing cracks in the die-cast product that are caused by the driving of the self-piercing rivet, when the member that is in contact with the tip side of the self-piercing rivet among the objects to be fastened with the self-piercing rivet is a die-cast product. [Brief description of the drawings]
[0011] [Figure 1] A cross-sectional view showing a portion of a fastening structure manufactured by a fastening structure manufacturing method according to one embodiment. [Diagram 2] 4 is a cross-sectional view showing a state before a self-pierce rivet is driven into a portion where a first member and a second member are overlapped. FIG. [Diagram 3] A cross-sectional view showing an example of a molding die used in a molding process in a manufacturing method for a fastening structure according to one embodiment, together with a first member. [Figure 4] 1 is a cross-sectional view showing an example of a fastening device used in a driving step in a manufacturing method for a fastened structure according to one embodiment, together with a first member, a second member, and a self-piercing rivet. FIG. [Diagram 5] A cross-sectional view showing a driving step in a manufacturing method of a fastening structure according to one embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] A method for manufacturing a fastening structure according to one embodiment of the present invention will be described with reference to FIGS.
[0013] 1 shows in cross section a portion of a fastened structure 10 manufactured by the manufacturing method for a fastened structure according to the present embodiment. The fastened structure 10 has a first member 12, a second member 14, and a self-piercing rivet 16.
[0014] The first member 12 and the second member 14 are both made of metal. More specifically, the first member 12 is made of an aluminum alloy, for example, and the second member 14 is made of steel, for example. The first member 12 is a die-cast product formed by die-casting. The first member 12 and the second member 14 are, for example, members for a vehicle.
[0015] The self-piercing rivet 16 is made of special steel such as chrome molybdenum steel, and has a head 16A and a leg 16B extending cylindrically from the head 16A. As shown in Fig. 2, before the self-piercing rivet 16 is driven into the overlapping portion 40 of the first member 12 and the second member 14, the inner diameter of the tip side of the leg 16B gradually increases toward the tip. The tip side of the leg 16B is formed in this manner so that the tip side of the leg 16B can be easily deformed in the direction of increasing the diameter when the self-piercing rivet 16 is driven into the members.
[0016] Next, an example of an apparatus used in a method for manufacturing the fastening structure 10 (see FIG. 1) will be described with reference to FIGS.
[0017] 3 shows an example of a molding die 20 of a die device used in a molding step in the manufacturing method of a fastening structure. The molding die 20 includes a first molding die 22 and a second molding die 24. When the first molding die 22 and the second molding die 24 are in a closed state, a molding cavity 26 is formed between the first molding die 22 and the second molding die 24. Molten metal (aluminum alloy in this embodiment) is pressed into the cavity 26.
[0018] Fig. 4 shows an example of a fastening device 30 used in the driving step in the manufacturing method of a fastening structure. In this embodiment, the fastening device 30 shown in Fig. 4 is installed in a location relatively close to the molding die 20 shown in Fig. 3.
[0019] 4, the fastening device 30 includes a die 32 as a support member that supports the first member 12 from the side opposite to the side where the self-piercing rivet 16 is driven. The die 32 is made of steel, for example, and has a general support surface 32A that supports the first member 12 from below. The die 32 also has a recess 32B that comes into contact with a deformed portion of the first member 12 when the first member 12 is deformed by driving the self-piercing rivet 16. The recess 32B is recessed with respect to the general support surface 32A, and is formed in a circular shape in a plan view.
[0020] The die 32 also includes a built-in heater 34, which is provided at a position corresponding to the recess 32B. The heater 34 is shown diagrammatically in the drawing. The heater 34 is connected to a power source (not shown), and is capable of increasing its temperature by energizing it. The heater 34 is configured to be energized by a user's operation or by automatic control.
[0021] The fastening device 30 also includes a cylinder 36 and a punch 38. The cylinder 36 is formed in a cylindrical shape, and the self-piercing rivet 16 can be inserted into it. The cylinder 36 is disposed so that its axis corresponds to the center of the recess 32B of the die 32, and presses the first member 12 and the second member 14 supported by the die 32 against the general support surface 32A of the die 32. The punch 38 is a columnar member, and is movable in its axial direction within the cylinder 36 by a driving device (not shown), and is configured to press the self-piercing rivet 16 inserted into the cylinder 36 from above. In the drawing, the direction in which the punch 38 presses the self-piercing rivet 16 is indicated by an arrow P.
[0022] Next, a method for manufacturing a fastening structure will be described with reference to Figures 3 to 5. This method for manufacturing a fastening structure includes a molding step and a driving step.
[0023] 3, in the molding step, the first member 12 is molded by die casting. More specifically, in this molding step, the first molding die 22 and the second molding die 24 are closed, and molten metal (aluminum alloy in this embodiment) is forced into the cavity 26. The molten metal forced into the cavity 26 is solidified to mold the first member 12, and then the first molding die 22 and the second molding die 24 are opened, and the first member 12 is removed from the molding die 20.
[0024] In the driving step following the molding step, while heat generated during molding remains in first member 12 shown in Fig. 4, self-piercing rivet 16 is driven from the second member 14 side into overlapping portion 40 where second member 14 is overlapped on first member 12, as shown in Fig. 5. An example of this driving step will be described in more detail.
[0025] 4, the first member 12 is supported on the general support surface 32A of the die 32, and the second member 14 is superimposed on the first member 12. In this embodiment, as an example, an end portion of the first member 12 is supported by the die 32. Next, the first member 12 and the second member 14 are sandwiched between the lower end surface of the cylinder 36 and the general support surface 32A of the die 32.
[0026] Next, electricity is passed through the heater 34 to generate heat, thereby heating the die 32. Note that electricity may be passed through the heater 34 before the first member 12 and the second member 14 are sandwiched between the lower end surface of the cylinder 36 and the general support surface 32A of the die 32. Next, the self-pierce rivet 16 inside the cylinder 36 is pressed from above with the punch 38.
[0027] As a result, as shown in Fig. 5, the self-piercing rivet 16 is lowered, the leg 16B of the self-piercing rivet 16 pierces the second member 14, and the first member 12 pressed by the self-piercing rivet 16 and the second member 14 is deformed toward the recess 32B of the die 32. A part of the first member 12 deforms along the recess 32B, and the tip side of the leg 16B of the self-piercing rivet 16 bites into the first member 12 while expanding in diameter. At this time, the heat generated by the heater 34 heats the deformed portion of the first member 12 that overlaps with the second member 14 from the recess 32B of the die 32. Thereafter, the cylinder 36 and the punch 38 are raised, and the fastening structure 10 shown in Fig. 1 is removed from the fastening device 30.
[0028] 5 is performed while heat from the formation of the first member 12 remains in the first member 12, so that the self-piercing rivet 16 is driven into the first member 12 in a state in which the first member 12 is more ductile than at room temperature. This makes the first member 12 less likely to crack in the driving step. In other words, the heat imparted to the first member 12 during the formation of the first member 12 can be effectively utilized to prevent cracking of the first member 12.
[0029] In the present embodiment, in the driving step, the heater 34 generates heat to heat the portion of the first member 12 that overlaps with the second member 14 through the recess 32B of the die 32, so that the ductility of the first member 12 in the driving step can be further increased, making the first member 12 even less likely to crack in the driving step. In addition, because the heat generated during molding remains in the first member 12, the amount of heat required to ensure good ductility of the first member 12 can be reduced.
[0030] Moreover, in this embodiment, the manufacturing time of the fastening structure 10 (see FIG. 1) can be shortened. To further explain this point, for example, when the first member 12 is a large part, it takes time for the first member 12 molded by die casting to cool down, but in this embodiment, the first member 12 and the second member 14 are fastened (joined) together without waiting for the molding heat of the first member 12 to cool down, so that the time until the molding heat of the first member 12 cools down can be effectively utilized. Note that the first member 12 may be a patch instead of a large part.
[0031] In addition, in this embodiment, the molding process and the driving process are performed in close proximity to each other, which reduces the labor required for transportation. This improves productivity. This effect is particularly significant when the first member 12 is a large component.
[0032] As described above, according to the manufacturing method for the fastening structure of the present embodiment, when the member that is in contact with the tip side of the self-piercing rivet 16 among the objects to be fastened with the self-piercing rivet 16 is a die-cast product, it is possible to improve manufacturing efficiency while suppressing cracks in the die-cast product that are caused by the driving of the self-piercing rivet 16.
[0033] 1 to 5, the method for manufacturing a fastening structure may further include a heating step of separately heating the portion of the first member 12 that overlaps with the second member 14 from the side opposite to the second member 14 after the molding step and before driving the self-piercing rivet 16 into the overlapping portion 40. In such a modification, the susceptible portion of the first member 12 is heated separately, further increasing the ductility of the susceptible portion of the first member 12.
[0034] In addition, in the above embodiment, the first member 12 is heated from the recess 32B of the die 32 during the driving process. However, as a modification of the above embodiment, for example, the heater (34) built into the die (32) may also be arranged near the general support surface (32A) of the die (32) so that the first member (12) is heated from the general support surface (32A) and the recess (32B) of the die (32).
[0035] As a modification of the above embodiment, a configuration may be adopted in which the first member 12 is not heated from the die 32 serving as a supporting member in the driving step.
[0036] The above-described embodiment and the multiple modified examples can be implemented in appropriate combinations.
[0037] While one example of the present invention has been described above, the present invention is not limited to the above, and it goes without saying that the present invention can be implemented in various modified forms without departing from the spirit and scope of the present invention. [Explanation of symbols]
[0038] 10 Fastening structure 12 First member 14 Second member 16 Self-pierce rivet 32 Die (support member) 40 Overlapped section
Claims
1. a molding step of molding the first member by die casting; a driving step of driving a self-piercing rivet into a superposed portion where a second member is superposed on the first member from the second member side while heat generated during the molding remains in the first member after the molding step; A method for manufacturing a fastening structure comprising the steps of:
2. 2. The method for manufacturing a fastening structure according to claim 1, wherein in the driving step, a portion of the first member that overlaps with the second member is heated from a support member that supports the first member from an opposite side to a driving side of the self-pierce rivet.
Citation Information
Patent Citations
Warm self-piercing riveting method and device for high-strength light metal plates
CN108421948A
Easy-to-rivet secondary aluminum die casting for new energy automobile and preparation method of easy-to-rivet secondary aluminum die casting
CN117363906A
Die casting system
JP2010064121A
Rivet joining method
JP2010188383A