Burned residue disposal field and burned residue disposal method
By using precast blocks made from incineration residue, cement, and water to divide and stabilize disposal areas, the method enhances disposal efficiency, reduces leachate treatment costs, and accelerates the site's usability, addressing the inefficiencies of traditional disposal methods.
Patent Information
- Application Number
- JP2023046551
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-23
- Publication Date
- 2024-10-04
AI Technical Summary
Existing incineration residue disposal methods face challenges in efficiently utilizing disposal areas due to the need for intermediate and same-day soil coverings, and the presence of walls within the disposal site reduces the amount of waste that can be disposed of, leading to long maintenance times and high costs.
The method involves manufacturing precast blocks using the superfluid construction method with incineration residue, cement, and water, which are used to divide the disposal area into sections, forming stable solidified layers with low permeability to prevent scattering and leaching, and incorporating a water-impermeable protective mat.
This approach allows for more efficient disposal of incineration residue without the need for intermediate coverings, reduces leachate treatment costs, and enables the site to be abolished in a significantly shorter time frame, while preventing subsidence and maintaining structural integrity.
Smart Images

Figure 2024135721000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to the disposal of waste incineration residues, and more specifically, to a disposal site divided into blocks using the waste incineration residues to be disposed of, and a method for disposing of the waste incineration residues at this disposal site. [Background technology]
[0002] In recent years, the amount of waste generated in Japan has been on the decline thanks to various efforts led by the national and local governments. However, a huge amount of waste, exceeding 400 million tons, is still generated annually, and securing disposal sites remains a major problem. Breaking down the waste, approximately 42 million tons of general waste and approximately 390 million tons of industrial waste are generated, with industrial waste accounting for nearly 90% of the total.
[0003] Industrial waste and general waste are broadly divided into those that are recycled and those that are disposed of, and those that are disposed of are further divided into those that are incinerated and those that are not. For example, in the case of general waste, waste that is disposed of is divided into those that are sent directly to incineration facilities and those that are sent to intermediate treatment facilities, and the processing residues generated at intermediate treatment facilities that are incinerated are sent to incineration facilities again. Processing residues generated at intermediate treatment facilities that are not incinerated and incineration residues generated at incineration facilities are sent to final disposal sites.
[0004] Incineration residues make up the majority of both general waste and industrial waste sent to final disposal sites, and the current final disposal sites are essentially "ash dumps." Meanwhile, in 2021, the Ministry of the Environment reported that the remaining lifespan of final disposal sites in Japan is 21.4 years. Therefore, how to efficiently dispose of waste, especially incineration residues, in landfills is an urgent issue.
[0005] Incineration residues are divided into bottom ash and fly ash. Bottom ash is what collects at the bottom of the furnace at an incineration facility, while fly ash is what collects in the dust collector or adheres to the boiler. Fly ash is discharged at only about one-third the volume of bottom ash, but it contains more dioxins and heavy metals such as lead, zinc, and cadmium than bottom ash. For this reason, a liquid chelating agent is added to the fly ash before it is landfilled at the final disposal site. The heavy metal ions in the fly ash are less likely to dissolve into the environment due to chemical bonding with the liquid chelating agent.
[0006] Residues from incineration of general waste are often disposed of in general waste disposal sites, while waste from industrial waste is often disposed of in managed final disposal sites. General waste disposal sites are also classified as "managed" final disposal sites, and these sites must be maintained and managed so that leachate from the site and surrounding groundwater meet the standards set by ministerial ordinances. Furthermore, in order to abolish a managed final disposal site, it is necessary that the quality of the water collected within the site is recognized as meeting the specified effluent standards for more than two years. Therefore, in managed final disposal sites, incineration residues are not buried directly on the natural ground, but rather, as shown in Figure 10, a waterproof sheet is laid on the natural ground, and a protective layer (sand or soil) is also installed before the incineration residues are buried. Also, as shown in Figure 10, a landfill method called semi-aerobic landfilling method is sometimes adopted to remove moisture in the landfill site through drainage pipes and remove gas generated in the landfill site through gas vent pipes.
[0007] However, even if measures like those shown in Figure 10 are implemented, they do not necessarily meet the ministerial ordinance standards, and the current situation is that a certain amount of leachate from the disposal site is stored and treated before being discharged. In other words, even maintaining many managed final disposal sites is difficult, and it is said that it will take 20 to 30 years before they are decommissioned, so they will have to be operated as final disposal sites for an extremely long period of time. Therefore, not only will the costs of maintenance, such as the discharge treatment of leachate, be high, but it will also take a considerable amount of time before the airspace above the site can be used as a former site.
[0008] There are also other problems with the use of the site. As already mentioned, the majority of materials landfilled at managed final disposal sites are incineration residues. Incineration residues are inorganic and it is difficult to imagine that they would generate gases such as carbon dioxide, but in reality, some incineration residues contain unburned remains, which can cause gas generation. Gas is usually generated over a long period of time, and if gas is generated after the site is reused, for example, the site will sink by the amount of gas generated, which will have an impact on facilities and structures built on the site.
[0009] Furthermore, conventional managed final disposal sites have problems in terms of space utilization. The incineration residues transported to managed final disposal sites are spread evenly in a 50 cm layer, for example, and compacted by heavy machinery such as bulldozers. As mentioned above, the fly ash is treated with the addition of a liquid chelating agent, so it is initially somewhat moist, but when it dries, it becomes more likely to scatter. Therefore, it is necessary to take measures to prevent scattering, and intermediate soil is placed on the incineration residues after compaction, as shown in Figures 10 and 11. The intermediate soil is placed on top of 5 to 6 layers of stacked incineration residues, so there are periods when the incineration residues are exposed. Therefore, in recent years, immediate soil cover (daily cover), which covers the landfill site after each day's landfill work, has become mainstream.
[0010] Installing intermediate or immediate cover means that the incineration residue cannot be landfilled. As mentioned above, the remaining life of the final disposal site is 21.4 years as of 2021, and it is extremely important to make effective use of the remaining disposal area. Therefore, there was a strong demand for disposal technology that would allow the omission of intermediate or immediate cover.
[0011] Therefore, Patent Document 1 discloses an invention for disposing of incineration residues by applying the "superfluid method." This superfluid method is a technology developed by the applicant of the present application. For example, Patent Document 2 discloses an invention in which cement, coal ash, and water (at about the optimum water content) are mixed to produce a mixture, which is then transported to a construction site, where it is vibrated to make it fluid, and cast at a specified location. With this technology, the mixture is simply kept in a moist powder state, so that the mixture hardly adheres to the transporting means and kneading means that handle it. As a result, the transporting means and kneading means are easy to clean, and materials can be used without waste. [Prior art documents] [Patent documents]
[0012] [Patent Document 1] JP 2015-73981 A [Patent Document 2] Japanese Patent Application Publication No. 10-311142 Summary of the Invention [Problem to be solved by the invention]
[0013] The invention disclosed in Patent Document 1 disposes of incineration residue in landfill while forming a stable solidification plate, so there is no need for intermediate or immediate soil cover to prevent the incineration residue from scattering. As a result, more incineration residue can be disposed of in landfill by the amount equivalent to intermediate or immediate soil cover. Although this invention requires the mixing of cement, it has been confirmed by trial calculations that the disposal volume is improved by about 5% overall even after subtracting the amount of cement used.
[0014] In many cases, at final disposal sites with vast areas, the disposal area is divided horizontally beforehand and then landfilled. To divide the disposal area, walls such as earth dams and gravity retaining walls are constructed. In other words, so-called "foreign objects" that are different from the waste to be disposed of (especially incineration residues) occupy part of the disposal area, and therefore it is not possible to dispose of the waste in proportion to the amount of foreign objects. The invention disclosed in Patent Document 1 succeeds in improving the disposal area vertically, but it can be said that there is room for improvement in the disposal area horizontally.
[0015] The object of the present invention is to solve the problems associated with the conventional technology, i.e., to provide an incineration residue disposal site and an incineration residue disposal method that can prevent the reduction in the amount of waste disposed of due to walls that divide the disposal area. [Means for solving the problem]
[0016] The present invention is based on the unprecedented idea of applying the superfluid construction method developed by the applicant to manufacture precast blocks, and then using these precast blocks to divide the disposal area.
[0017] The incineration residue disposal site of the present invention is a disposal site for incineration residue, and is equipped with a partition wall in which multiple precast blocks are stacked. The disposal area is divided into two or more disposal sections by the partition walls. The precast blocks are manufactured by vibrating a block material made by mixing incineration residue, cement, and water that has been brought in, and then hardening it. In the disposal section, a "non-fluid plastic mixture" made by adding cement and water to incineration residue is spread evenly in layers, and the surface of the layered plastic mixture is subjected to surface vibration before hardening.
[0018] The incineration residue disposal site of the present invention may be one that uses precast blocks to which a water-impermeable protective mat is attached. The protective mat is attached in close contact with the surface of the precast block that comes into contact with the plastic mixture.
[0019] The incineration residue disposal site of the present invention is a method for disposing of incineration residue in the incineration residue disposal site of the present invention, which includes a partitioning step, a kneaded material generating step, a plastic layer forming step, and a solidified layer forming step. In the partitioning step, a partition wall is constructed by stacking a plurality of precast blocks, and the disposal area is divided into two or more disposal sections by the partition wall. In the kneaded material generating step, cement and water are added to the incineration residue brought to the incineration residue disposal site and kneaded to generate a non-fluid plastic kneaded material, and in the plastic layer forming step, the plastic kneaded material is spread evenly in layers in the disposal section to form a plastic layer. In the solidified layer forming step, a surface vibration is applied to the surface of the plastic layer to cause cement and water to permeate around the particles of the incineration residue to form a fluid plastic fluid layer, and when the plastic fluid layer hardens after a predetermined period of time, a solidified layer of the incineration residue is formed. The precast blocks are manufactured by vibrating and then hardening a block material made from a mixture of incineration residue, cement, and water brought to an incineration residue disposal site.
[0020] The incineration residue disposal site of the present invention can also be a method further comprising a precast block manufacturing process. In this precast block manufacturing process, a block material (a material obtained by kneading incineration residue, cement, and water brought to the incineration residue disposal site) is poured into a formwork, and a surface vibration is applied to the surface of the block material, and a hardened precast block is obtained after a predetermined time has passed. In this case, in the partition division process, the precast blocks obtained in the precast block manufacturing process are piled up to construct partition walls.
[0021] The incineration residue disposal site of the present invention can also be a method of forming multiple solidified layers stacked one on top of the other in the disposal area by repeatedly performing the plastic layer forming step and the solidified layer forming step.
[0022] The incineration residue disposal site of the present invention can also be a method further comprising a reinforcing step. In this reinforcing step, a plurality of strip-shaped (or rod-shaped) reinforcing materials are laid on the surface of the solidified layer. One end of the reinforcing material is connected to the surface of the precast block that comes into contact with the solidified layer. In this case, in the plastic layer formation step in the upper stage, a plastic mixture is spread evenly on the reinforcing material in the lower stage.
[0023] The incineration residue disposal site of the present invention can also be constructed in such a way that when a solidified layer is formed up to almost the top of the partition wall (including the top), an upper partition wall is constructed on the upper surface of the solidified layer. In this case, in the partition division process, the upper partition wall can be constructed in a planar arrangement different from that of the lower partition wall. Effect of the Invention
[0024] The incineration residue disposal site and incineration residue disposal method of the present invention have the following effects. (1) Since the incineration residue is disposed of in landfill while forming a stable solidification layer, there is no need for intermediate or immediate soil covering to prevent the incineration residue from scattering. Moreover, since the partition walls that divide the disposal area are made of precast blocks that use incineration residue, the disposal area is improved both vertically and horizontally. As a result, the incineration residue can be disposed of in landfill more efficiently than with conventional technology. (2) Both the layer formed after the disposal of incineration residue and the solidified layer precast blocks that make up the partition walls are solidified bodies with a permeability coefficient of the order of 10-7 to 10-9 (cm / s), which can eliminate seepage water from the outside, such as rainwater, and can suppress the leaching of harmful substances originating from heavy metals in the incineration residue. As a result, the treatment costs per unit of leachate are reduced, and since the amount of leachate itself is greatly reduced, the overall cost of treating the leachate is reduced. (3) As mentioned above, a solidified body with a hydraulic conductivity of the order of 10-7 to 10-9 (cm / s) is formed, which makes it possible to suppress the leaching of harmful substances in the incineration residue. This makes it possible to decommission the disposal site in an extremely short period of time (approximately 2.5 years) compared to the conventional period (20 to 30 years) and reuse the site. (4) The incineration residue contains little organic matter and a large amount of silicon and alumina, which react with water and cement to produce stable crystals. Therefore, there is no subsidence caused by gas generation such as carbon dioxide, and the site can be used safely and at an early stage. [Brief description of the drawings]
[0025] [Figure 1] FIG. 2A is a cross-sectional view showing a schematic diagram of the incineration residue disposal site of the present invention, and FIG. 2B is a plan view showing a schematic diagram of the incineration residue disposal site of the present invention. [Diagram 2] An explanatory diagram showing the process of landfill disposal of incineration residue using the "Super Fluid Method." [Diagram 3] FIG. 2 is a cross-sectional view showing a precast block with protective mats attached to both sides. [Figure 4] A front view showing a schematic of a partition wall formed by stacking six layers of precast blocks. [Diagram 5] A step diagram showing the procedure for forming a solidified layer while building partition walls in stages. [Figure 6] A cross-sectional view showing a schematic diagram of partition walls arranged in a "staggered" configuration, in which the partition walls are not continuous vertically. [Figure 7] (a) is a cross-sectional view showing a schematic of the reinforcing material laid between the solidified layers, (b) is a plan view showing a schematic of the reinforcing material laid between the solidified layers, and (c) is a partial cross-sectional view explaining the connection between the reinforcing material and the connector. [Figure 8] 1 is a flow chart showing the flow of main steps of the incineration residue disposal method of the present invention. [Figure 9] A step diagram showing the process of forming a solidified layer while constructing partition walls for each disposal compartment. [Figure 10] A partial cross-sectional view showing the structure of a conventional managed final disposal site. [Figure 11] FIG. 2 is a partial cross-sectional view illustrating intermediate cover soil in a conventional managed final disposal site. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0026] An example of an embodiment of the incineration residue disposal site and the incineration residue disposal method of the present invention will be described with reference to the drawings.
[0027] 1.Overview FIG. 1 is a diagram showing a schematic diagram of an incineration residue disposal site 100 of the present invention, where (a) is a vertical cross-sectional view, and (b) is a plan view seen from above. As shown in this figure, the incineration residue disposal site 100 is provided with a partition wall 120 formed by stacking a number of precast blocks 110, and the entire disposal area of the incineration residue disposal site 100 is divided into two or more disposal sections 130 by arranging the partition walls 120. For convenience, the horizontal direction from upstream to downstream in the incineration residue disposal site 100 (left-right direction in the figure) is referred to as the "main axis direction," and the horizontal direction perpendicular to the main axis direction (up-down direction in the figure) is referred to as the "secondary axis direction." For example, in this figure, one row of partition walls 120 is arranged in the main axis direction, and three rows of partition walls 120 are arranged in the secondary axis direction, thereby dividing the disposal area of the incineration residue disposal site 100 into six sections, i.e., six disposal sections 130 are formed. Furthermore, structures such as earth dams DM will be constructed on the downstream side of the incineration residue disposal site 100 (the right side in the figure), and earth dams DM or cut slopes will also be constructed around the disposal area.
[0028] The disposal section 130 is an area for landfill disposal of the incineration residue that has been brought in. In the present invention, the incineration residue is disposed of by using the "super fluid method" as described below. The precast blocks 110 that constitute the partition wall 120 are also manufactured by the "super fluid method" using the incineration residue as a material. Conventionally, when dividing a final disposal site into sections, walls such as earth dams DM and gravity retaining walls were placed in the disposal area. Therefore, the amount of waste that could be disposed of was reduced by the volume of the earth dams DM, etc. In contrast, in the present invention, the disposal area is divided into sections by the precast blocks 110 that use the incineration residue as a material, in other words, the division is performed while the incineration residue is being disposed of, so that more incineration residue can be disposed of than in the conventional technology.
[0029] Here, the procedure for disposing of incineration residue using the "super fluid method" will be described with reference to Figure 2. First, the incineration residue including fly ash is carried into the incineration residue disposal site 100 by a transport vehicle such as a closed dump truck Dt, and is unloaded at a predetermined location (A in Figure 2).
[0030] (Mixture production process) When the incineration residue is brought in, water and cement are added to the residue and it is mixed (stirred and mixed) using a stabilizer or backhoe Bh to produce a non-fluid "plastic mixture" (B in Figure 2). Of course, instead of using machinery to mix, a plastic mixture can also be produced using a separately prepared mixing plant. This "plastic mixture" is in a state similar to wet soil, a so-called zero slump state, and its fluidity is extremely low compared to the "plastic fluid layer" explained later.
[0031] When mixing incineration residue, water, and cement, it is advisable to add an appropriate amount of water to reduce the water-cement ratio. This is to obtain a small coefficient of permeability when the plastic mixture is solidified by surface vibration in a later process. Here, we will explain what we mean by "the appropriate amount of water." As described later, -7 ~10 -9In order to obtain a permeability coefficient of the order of 10000 cm / s, the particle arrangement of the incineration residue must be uniform and dense, and water must be added to liquefy the plastic mixture. However, if too much water is added, the plastic state cannot be maintained, making the plastic mixture difficult to handle, and there is also the problem of bleeding, which means that the desired permeability coefficient cannot be obtained because the appropriate strength is not expressed. In addition, a small amount of water cannot be expected to liquefy sufficiently, and there is a risk of thermal cracking. Therefore, an appropriate amount of water is required, and an example of a method for determining this appropriate amount is a method based on the optimal water content. Generally, the dry unit volume weight (dry density) is used as a value that represents the degree of compaction, and the greater this value, the greater the strength, the better the degree of compaction, and the smaller the permeability coefficient. Even under the same compaction conditions, the dry unit volume weight obtained varies depending on the amount of water contained, and the water content that gives the largest dry unit volume weight is the "optimum water content." In addition, since a large amount of plastic kneaded material may be compacted at one time, it is desirable to determine the amount of water that is slightly greater than the optimum water content of the plastic kneaded material as the "appropriate amount of water." For example, when the "optimum water content" is used as the standard, the "appropriate amount of water" may be "optimum water content + 1 to 5%."
[0032] (Plastic layer formation process) Once the non-fluid plastic mixture is produced, it is spread evenly in a layer within the partition wall 120 using heavy machinery such as a backhoe Bh to form a layer of the plastic mixture (hereinafter referred to as the "plastic layer") (C in FIG. 2).
[0033] (solidified layer formation process) Once the plastic layer is formed, a vibration plate Vb attached to a backhoe Bh or similar device is used to apply surface vibration to the surface of the layered body (D in Figure 2). When vibration is applied to the non-fluid plastic layer for approximately 30 to 60 seconds, cement and water penetrate around (between) the particles of the incineration residue, causing the plastic layer to become fluid, resulting in the formation of a fluid-like (superfluid) "plastic fluid layer." When vibration is applied to materials that contain a relatively large number of spherical particles, such as incineration residue, the bearing effect of the spherical particles contained within the particles makes it easy for the particles to separate, and as a result, water and cement are evenly distributed around the particles. The plastic layer then loses effective stress, and only pore water pressure remains, causing the liquefaction phenomenon. When the plastic layer liquefies, it becomes a pudding-like plastic fluid layer (superfluid layer).The particle arrangement becomes uniform and dense due to the liquefaction, and since the incineration residue contains small amounts of organic matter and large amounts of silicon and alumina, a stable crystalline body (solidified body) is produced by the hydration reaction of water and cement.
[0034] After the plastic fluid layer is formed, after a certain period of time (approximately one day) the plastic fluid layer hardens and forms the "solidified layer SL". The solidified layer SL formed by the superfluid method has few cracks and is high strength, and its permeability coefficient is 10 -7 ~10 -9 Therefore, there is no need to place intermediate cover soil on the solidified layer SL as a measure to prevent scattering, and a large amount of incineration residue can be disposed of by the volume of the intermediate cover soil.
[0035] 2. Incineration residue disposal site The incineration residue disposal site 100 of the present invention will be described. The incineration residue disposal method of the present invention is a method for disposing of incineration residue at the incineration residue disposal site 100. Therefore, the incineration residue disposal site 100 will be described first, and then the incineration residue disposal method of the present invention will be described.
[0036] As described above, the incineration residue disposal site 100 has a disposal area divided into two or more disposal compartments 130 by the placement of the partition walls 120. The partition walls 120 are formed by stacking a number of precast blocks 110. Below, each of the main elements that make up the incineration residue disposal site 100 will be explained in detail.
[0037] (Precast Blocks) The precast block 110 is manufactured by the "super fluid method" using incineration residue, and is manufactured in the same procedure as the disposal of incineration residue by the super fluid method described above. That is, an appropriate amount of water and cement is added to the incineration residue brought to the incineration residue disposal site 100, and then the residue is kneaded to generate a non-fluid "plastic mixture." Note that, in order to distinguish it from the "plastic mixture" generated for disposal in the disposal area 130, the "plastic mixture" obtained for manufacturing the precast block 110 will be simply referred to as the "block material."
[0038] Once the non-fluid "block material" has been produced, it is poured into a formwork. Then, a "plastic fluid" in a fluid state (superfluid state) is formed by applying surface vibrations to the surface of the block material or by applying vibrations to the formwork. After a prescribed period of time (approximately three days) has passed since this plastic fluid was formed, the plastic fluid hardens to form a precast block 110. The precast block 110 formed by the superfluid method has few cracks and is strong, just like the "solidified layer" described above, and its permeability coefficient is 10 -7 ~10 -9 It is on the order of (cm / s).
[0039] A protective mat 140 may be attached to the precast block 110 as shown in FIG. 3. In particular, the protective mat 140 may be attached to the surface of the precast block 110 that comes into contact with the plastic layer spread evenly within the partition wall 120 (i.e., both side surfaces). For convenience, FIG. 3 shows a solidified layer SL in which the plastic layer hardens after vibration is applied. The protective mat 140 may be attached after being in close contact with the surface of the precast block 110. The protective mat 140 is a sheet (or plate) made of nonwoven fabric provided with a resin layer that is water-stopping and weather-resistant. For example, the protective mat 140 may be "Appeal (registered trademark) L1500" or "Appeal (registered trademark) LN650" manufactured by Unitika Ltd. Alternatively, an asphalt sheet can be used as the protective mat 140, or asphalt can be laid directly on the surface of the precast block 110 to create the protective mat 140, or a corrosion-resistant coating using the SuraSura method of the Corrosion-Resistant Lining Method Association can be used as the protective mat 140.
[0040] (Partition wall) As shown in Figure 4, the partition wall 120 is a wall-like body formed by stacking multiple tiers (six tiers in the figure) of precast blocks 110. When stacking the precast blocks 110, it is advisable to stack them in a so-called "staggered arrangement" so that the boundaries between adjacent precast blocks 110 above and below do not continue as shown in this figure. Of course, when there are special circumstances, such as when the number of tiers to be stacked is small, the precast blocks 110 can also be stacked in a "staggered arrangement" so that the boundaries between the precast blocks 110 continue above and below.
[0041] (Disposal area) The disposal section 130 is an area obtained by dividing the disposal area of the incineration residue disposal site 100 into two planes by placing the partition walls 120, and is an area for landfill disposal of incineration residue brought to the incineration residue disposal site 100. As explained so far, disposing of incineration residue using the "super fluid method" means forming a solidified layer SL containing the incineration residue, so for convenience, "landfilling incineration residue" will be expressed as "forming a solidified layer SL".
[0042] Various procedures can be used to install the partition walls 120, that is, to form the disposal section 130 and form the solidified layer SL. For example, the partition walls 120 can be constructed to the final planned height from the beginning, and then the solidified layer SL can be formed in stages. Alternatively, as shown in FIG. 5, the solidified layer SL can be formed while constructing the partition walls 120 in stages. In other words, the solidified layer SL is formed in the disposal section 130 in which the disposal area of the incineration residue disposal site 100 is divided vertically as well. The procedure for forming the solidified layer SL in the disposal section 130 divided vertically will be described below with reference to FIG. 5.
[0043] First, as shown in FIG. 5(a), a partition wall 120 (first tier partition wall 120) is constructed to a predetermined height (however, lower than the final planned height), and then, as shown in FIG. 5(b), a solidified layer SL is formed up to the vicinity (or the top) of the first tier partition wall 120. Next, as shown in FIG. 5(c), a partition wall 120 (second tier partition wall 120) is constructed so as to be added to the upper part of the first tier partition wall 120. Then, as shown in FIG. 5(d), a solidified layer SL is formed up to the vicinity of the top of the second tier partition wall 120. In this manner, the construction of the partition walls 120 and the formation of the solidified layer SL are repeated to build up the solidified layer SL up to the final planned height.
[0044] In FIG. 5, the second partition wall 120 is constructed so as to be added to the top of the first partition wall 120, that is, so as to have the same planar arrangement, but the upper partition wall 120 can also be constructed so as to have a different planar arrangement from the lower partition wall 120. For example, in FIG. 6, the partition walls 120 adjacent to each other vertically are not continuous, in a "staggered arrangement." In this figure, the partition walls 120 of the first to fourth layers are constructed, solidified layers SL are formed from the first to third layers, and the partition walls 120 of the second layer are arranged between the partition walls 120 of the first layer, and similarly, the partition walls 120 of the third layer are arranged between the partition walls 120 of the second layer, and the partition walls 120 of the fourth layer are arranged between the partition walls 120 of the third layer.
[0045] As described above, the partition wall 120 can be constructed to the final planned height from the beginning, while the solidified layer SL is formed in stages with a layer thickness of a predetermined dimension (for example, about 20 cm). Therefore, as shown in Fig. 7, a reinforcing material 150 can be laid between the solidified layers SL adjacent to each other above and below. Fig. 7 is a schematic diagram showing the reinforcing material 150 laid between the solidified layers SL, where (a) is a vertical cross-sectional view, (b) is a plan view seen from above, and (c) is a partial cross-sectional view explaining the connection between the reinforcing material 150 and a connector 160.
[0046] The reinforcing material 150 is a member capable of providing shear reinforcement to the solidified layers SL stacked one above the other, and may be, for example, a band-shaped (or rod-shaped) member made of steel. In particular, a "strip" used in the Terre Armée (registered trademark) method may be used as the reinforcing material 150. One end (the left end in the figure) of the reinforcing material 150 is connected to the precast block 110 so as to function integrally with the partition wall 120. Specifically, one end of the reinforcing material 150 is connected to a connector 160 fixed to the precast block 110. When connecting the connector 160 and the reinforcing material 150, various conventional methods such as connection using bolts or pins, or joining using adhesives or tape may be used.
[0047] Since the reinforcing material 150 provides shear reinforcement to the solidified layer SL, it is natural that it is provided on the side of the precast block 110 where the solidified layer SL is formed, and it is natural that the connector 160 is also provided on the solidified layer SL side. Note that in the example of Fig. 7, two rows (Fig. 7(a)) x two columns (Fig. 7(b)) of reinforcing material 150 are connected to one precast block 110, but this is not limiting and the reinforcing material 150 can be connected in any number of rows x columns.
[0048] The procedure for forming the solidified layer SL while laying the reinforcing material 150 will be described below. First, the partition wall 120 is constructed to a specified height (or final planned height). At this time, the reinforcing material 150 is not yet connected to the connector 160. Next, the solidified layer SL is repeatedly formed. Then, when the solidified layer SL is piled up to the fixing position of the connector 160, the reinforcing material 150 is laid on the upper surface of the solidified layer SL, and one end of the reinforcing material 150 is further connected to the connector 160. In this way, the formation of the solidified layer SL and the laying of the reinforcing material 150 are repeatedly performed to form the shear-reinforced solidified layer SL.
[0049] 3. Incineration Residue Disposal Method Next, the incineration residue disposal method of the present invention will be described. The incineration residue disposal method of the present invention is a method for disposing of incineration residue at the incineration residue disposal site 100 of the present invention described so far. Therefore, we will avoid overlapping explanations with the contents explained about the incineration residue disposal site 100, and only explain the contents unique to the incineration residue disposal method of the present invention. In other words, the contents not described here are the same as those explained in "1. Overall Overview" and "2. Incineration Residue Disposal Site".
[0050] FIG. 8 is a flow diagram showing the main steps of the incineration residue disposal method of the present invention. As shown in this figure, when disposing of incineration residue at the incineration residue disposal site 100, first, the incineration residue to be disposed is carried into the incineration residue disposal site 100 (Step 201 in FIG. 8). Then, the carried-in incineration residue is used as a material to manufacture a precast block 110 by the "super fluid method". Specifically, an appropriate amount of water and cement are added to the carried-in incineration residue and kneaded to generate a "block material" (Step 202 in FIG. 8), and the block material is put into a formwork and subjected to surface vibration to form a "plastic fluid" (Step 203 in FIG. 8). Then, after a predetermined period of time has passed after the plastic fluid is formed, the precast block 110 in which the plastic fluid has hardened is formed (Step 204 in FIG. 8).
[0051] Once the precast blocks 110 are manufactured, the partition wall 120 is constructed by stacking the precast blocks 110 (Step 205 in FIG. 8). As described above, the partition wall 120 can be constructed to the final planned height from the beginning, or the partition wall 120 can be constructed in stages by a predetermined height. Therefore, it is possible to manufacture the entire number of precast blocks 110 planned at the beginning, or to manufacture only the number of precast blocks 110 required for the partition wall 120 to be constructed in stages.
[0052] Once the partition wall 120 is constructed, that is, the disposal section 130 is formed, the incineration residue is disposed of in earnest. Specifically, an appropriate amount of water and cement are added to the incineration residue brought in and kneaded to generate a "plastic mixture" (Step 206 in FIG. 8), and the plastic mixture is transported to the disposal section 130 and spread evenly in layers to form a "plastic layer" (Step 207 in FIG. 8). Then, a "plastic fluid layer" in a fluid state (superfluid state) is formed by applying surface vibration to the surface of the layered body using a vibration plate Vb or the like, and then, after a predetermined period of time (approximately one day), a "solidified layer SL" in which the plastic fluid layer hardens is formed (Step 208 in FIG. 8).
[0053] By repeatedly forming the solidified layer SL, the solidified layer SL is piled up to the fixing position of the connector 160. At this time, the reinforcing material 150 is laid on the upper surface of the solidified layer SL, and one end of the reinforcing material 150 is further connected to the connector 160 (Step 209 in FIG. 8). When constructing the partition wall 120 in stages by a predetermined height, the solidified layer SL is formed near the top of the first stage of the partition wall 120, and then the second stage of the partition wall 120 is constructed (Step 205 in FIG. 8), and a series of steps (Steps 206 to 209 in FIG. 8) are repeated. Then, when the solidified layer SL is piled up to the final planned height, the final cover soil is laid on the top (Step 210 in FIG. 8).
[0054] Incidentally, although it has been explained that the partition walls 120 can be constructed stepwise by dividing them in the height direction, the partition walls 120 can also be constructed stepwise by dividing them in the plane. FIG. 9 is a step diagram showing a situation in which a solidified layer SL is formed while constructing the partition walls 120 for each disposal section 130. In the example of this figure, first, as shown in FIG. 9(a), a partition wall 120 for dividing the first disposal section 130 (indicated by a number in a circle in the figure) is constructed. At this time, the partition wall 120 can be constructed to the final planned height from the beginning, or the partition wall 120 can be constructed stepwise by a predetermined height. Next, as shown in FIG. 9(b), a solidified layer SL is formed up to the vicinity of the top of the partition wall 120 constructed in the first disposal section 130.
[0055] When the solidified layer SL is formed in the first disposal section 130 as planned, the partition walls 120 for partitioning the second disposal section 130 are constructed as shown in Fig. 9(c), and the solidified layer SL is formed in the second disposal section 130 as shown in Fig. 9(d). In this manner, the solidified layer SL is formed while the partition walls 120 are constructed sequentially, that is, while the disposal sections 130 are formed sequentially. Note that, in Fig. 9, the disposal sections 130 are formed from upstream to downstream, but this is not limited to this, and the disposal sections 130 can be formed in any order, such as from downstream to upstream, and the solidified layer SL can be formed. [Industrial Applicability]
[0056] The incineration residue disposal site and incineration residue disposal method of the present invention can be particularly effectively implemented at general waste final disposal sites and controlled industrial waste final disposal sites. Given that the present invention provides an ideal solution to the current urgent issue of "shortage of remaining capacity at final disposal sites," it is an invention that can be expected to not only be used industrially but also to make a great contribution to society. [Explanation of symbols]
[0057] 100 Incineration residue disposal site of the present invention 110 Precast blocks (for incineration residue disposal site) 120 (Incineration Residue Disposal Site) Partition Wall 130 (Incineration Residue Disposal Site) Disposal Area 140 (Protective mat for incineration residue disposal site) 150 Reinforcement material (for incineration residue disposal sites) 160 (Incineration Residue Disposal Site) Connectors Bh Backhoe DM earth dam Dt Dump Truck SL solidified layer Vb vibration plate
Claims
1. A disposal site for incineration residue, A partition wall made of a plurality of precast blocks stacked together, the disposal area is divided into two or more disposal compartments by said partition walls; The precast block is manufactured by vibrating a block material made by mixing the incineration residue, cement, and water that has been brought in and then hardening the block material. In the disposal area, a non-fluid plastic mixture obtained by adding cement and water to the incineration residue is spread evenly in a layer, and the surface of the layered plastic mixture is subjected to surface vibration before hardening. An incineration residue disposal site characterized by:
2. A water-impermeable protective mat is attached in close contact with the surface of the precast block that comes into contact with the plastic mixture.
2. The incineration residue disposal site according to claim 1 .
3. A method for disposing of incineration residue at an incineration residue disposal site, comprising: a partitioning step of stacking a plurality of precast blocks to construct partition walls and dividing the disposal area into two or more disposal partitions by the partition walls; A kneaded material generating process for generating a non-fluid plastic kneaded material by adding cement and water to the incineration residue carried into the incineration residue disposal site and kneading the mixture; a plastic layer forming step of forming a plastic layer by spreading the plastic kneaded material in a layer in the disposal section; and a solidified layer forming process for applying a surface vibration to the surface of the plastic layer to cause cement and water to permeate around the particles of the incineration residue to form a fluid plastic fluid layer, and forming a solidified layer in which the plastic fluid layer is hardened. The precast block was manufactured by vibrating a block material made by mixing the incineration residue, cement, and water brought to the incineration residue disposal site and then hardening it.
1. A method for disposing of incineration residue comprising the steps of:
4. The method further includes a precast block manufacturing process in which the block material is poured into a formwork, a surface vibration is applied to the surface of the block material, and the precast block is obtained after a predetermined time has elapsed and the precast block is hardened. In the partitioning process, the precast blocks obtained in the precast block manufacturing process are stacked to construct the partition walls.
4. The incineration residue disposal method according to claim 3.
5. The plastic layer forming step and the solidified layer forming step are repeatedly performed to form a plurality of layers of the solidified layers stacked vertically in the disposal section.
4. The incineration residue disposal method according to claim 3.
6. The method further includes a reinforcing step of laying a plurality of strip-shaped or rod-shaped reinforcing materials on the surface of the solidified layer, One end of the reinforcing member is connected to a surface of the precast block that contacts the solidified layer; In the plastic layer forming step in the upper stage, the plastic kneaded material is spread evenly on the reinforcing material in the lower stage; 6. The incineration residue disposal method according to claim 5.
7. In the partitioning step, the partition walls are constructed to a predetermined height, and when the solidified layer is formed up to the top or approximately the top of the partition walls, an upper partition wall is constructed on the upper surface of the solidified layer; In addition, in the partitioning step, the partition walls of the upper stage are constructed in a planar arrangement different from that of the partition walls of the lower stage.
6. The incineration residue disposal method according to claim 5.
Citation Information
Patent Citations
Placing method for kneaded matter containing large amount of coal cinder
JP1998311142A
Disposal method of burned residue
JP2015073981A