METHOD FOR MANUFACTURING HALF-SECTION PCaPC FLOOR SLAB
By synchronizing manufacturing conditions and using guide pins and spacing materials, the method addresses joint unevenness in half-section PCaPC deck slabs, improving accuracy and durability.
Patent Information
- Application Number
- JP2023046612
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-23
- Publication Date
- 2024-10-04
AI Technical Summary
Existing methods for constructing half-section PCaPC deck slabs result in unevenness and gaps at joints due to differences in manufacturing conditions, such as timing, curing, and placement, leading to performance and durability issues.
The method involves manufacturing half-section PCaPC deck slabs using the same pretensioning material and facility, ensuring synchronized tensioning, curing, and symmetrical temporary storage, with guide pins and spacing materials to maintain alignment and prevent corrosion, thereby improving joint accuracy.
This approach reduces warpage and shortening differences between slabs, enhances joint accuracy, and increases the durability and load-bearing performance of the integrated deck slabs.
Smart Images

Figure 2024135759000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a half-section PCaPC deck slab. [Background technology]
[0002] Conventionally, in order to avoid traffic congestion when replacing bridge decks, the deck is divided into two in the direction perpendicular to the bridge axis, and each half section is replaced. In addition, when doing so, it is also common to replace a general RC deck with a half-section PCaPC (precast prestressed) deck using a pretensioning method, and when replacing each half section with a PCaPC deck, the lateral fastening of these half-section PCaPC decks is performed on-site by applying prestress using the post-tensioning method to connect and integrate them.
[0003] For example, Patent Document 1 discloses a staged construction method for precast decks, in which, when constructing a road by laying multiple concrete precast decks 11 on bridge girders in the bridge axis direction, the concrete precast deck 11 is divided into two in a direction perpendicular to the bridge axis to form a driving lane deck 11A and an overtaking lane deck 11B, and the decks 11A and 11B adjacent to each other in the direction perpendicular to the bridge axis are connected with a cotter joint 13, and each driving lane deck 11A or each overtaking lane deck 11B is replaced by releasing the cotter joint 13 (see claim 1 in the scope of claims of Patent Document 1, paragraphs
[0043] to
[0072] of the specification, Figure 9 of the drawings, etc.).
[0004] The staged construction method of precast deck slabs in Patent Document 1 is said to enable easy replacement of each concrete precast deck slab for a driving lane or each concrete precast deck slab for an overtaking lane.
[0005] Patent Document 2 discloses a method for constructing a concrete slab for an elevated road, in which a joint protrusion 50 is integrally provided at the joint end of a precast concrete slab 23, a joint recess 51 is integrally formed at the joint end of the other precast concrete slab 43, a guide pin 55 made of a material having a lower modulus of lateral elasticity than concrete is protruded from the joint end face of one of the precast concrete slabs 43, and the guide pin 55 is inserted into a guide hole 54 opened in the joint end face of the other precast concrete slab 23, thereby guiding the joint protrusion 50 into the joint recess 51 and guiding and setting both precast concrete slabs 23, 43 to desired positions, thereby constructing a concrete slab 20 (see claim 1 in the claims of Patent Document 2, paragraphs
[0039] to
[0056] of the specification, and Figures 7 to 9 of the drawings, etc.).
[0006] The method of constructing a concrete deck for an elevated road in Patent Document 2 is said to enable strict positional control so that no steps are created between the two precast concrete slabs.
[0007] Furthermore, Patent Document 3 discloses a joint structure 1 comprising a first precast deck 10 and a second precast deck 20 that are divided in the width direction D2 of the road and joined to each other along the width direction D2, the joint structure comprising a cushioning material 30 arranged along either the recess 13 or the protrusion 23, a tensioning means 50 that tensions the first precast deck 10 and the second precast deck 20, and a filling material 40 filled between the first end face 12 and the second end face 22 (see claim 1 in the claims of Patent Document 3, paragraphs
[0019] to
[0046] of the specification, Figures 2 to 4 of the drawings, etc.).
[0008] The joint structure of Patent Document 3 is said to enable efficient joining of precast deck slabs, as well as to increase the rigidity of the joints and improve the quality of the deck.
[0009] However, the staged construction method of precast decks in Patent Document 1, the method of constructing a concrete deck for an elevated road in Patent Document 2, and the joint structure in Patent Document 3 do not solve the problem of steps and gaps occurring at the joints due to differences in manufacturing, because the construction times of the half-section precast decks divided into two parts perpendicular to the bridge axis and factory-produced using the pretensioning method are different.
[0010] Possible factors that cause differences in levels and gaps include shrinkage and deflection due to creep and drying shrinkage of concrete, curing conditions, temporary placement (support position, etc.) conditions, differences in concrete age, etc. In other words, in the precast deck stage construction method of Patent Document 1, the method of constructing a concrete deck for an elevated road of Patent Document 2, and the joint structure of Patent Document 3, there is no idea of making the above-mentioned various conditions that arise from differences in the manufacturing process of the half-section PCa deck divided into two in the direction perpendicular to the bridge axis, which are produced at different times in factories using this pretensioning method, as much as possible, the same, and so differences in levels and gaps occur in the joints, causing problems with load-bearing capacity and durability. [Prior art documents] [Patent documents]
[0011] [Patent Document 1] JP 2014-177767 A [Patent Document 2] JP 2015-151768 A [Patent Document 3] Patent Publication No. 2021-67052 Summary of the Invention [Problem to be solved by the invention]
[0012] Therefore, the present invention has been devised in consideration of the above-mentioned problems, and its purpose is to provide a manufacturing method for half-section PCaPC deck slabs that can suppress individual differences in the amount of warping and shortening between integrated half-section PCa deck slabs by adjusting various conditions during manufacturing of pretensioned half-section PCaPC deck slabs, thereby achieving improved accuracy of the joints. [Means for solving the problem]
[0013] The manufacturing method for a half-section PCaPC deck slab of claim 1 is a manufacturing method for a half-section PCa PC deck slab in which the deck of a bridge is divided into two in a direction perpendicular to the bridge axis, into a first PCaPC deck slab and a second PCaPC deck slab, and the first PCaPC deck slab and the second PCaPC deck slab are constructed at different times and integrated on site, characterized in that the first PCaPC deck slab and the second PCaPC deck slab are manufactured by pouring concrete simultaneously under the same pretensioning conditions using the same tendons in the same pretensioning facility.
[0014] The manufacturing method for a half-section PCaPC deck slab of claim 2 is characterized in that, in the manufacturing method for a half-section PCaPC deck slab of claim 1, the first PCaPC deck slab and the second PCaPC deck slab are cured in the same curing facility under matching curing conditions.
[0015] The manufacturing method for a half-section PCaPC deck slab of claim 3 is characterized in that, in the manufacturing method for a half-section PCaPC deck slab of claim 1 or 2, the first PCaPC deck slab and the second PCaPC deck slab are supported and temporarily placed / stored at positions that are symmetrical when joined at the joint surface.
[0016] The manufacturing method for a half-section PCaPC deck slab of claim 4 is characterized in that, in the manufacturing method for a half-section PCaPC deck slab of claim 3, when the first PCaPC deck slab is constructed during the construction of the first phase of construction, the temporary placement position of the second PCaPC deck slab is supported and temporarily stored at a position that is symmetrical to the main girder position of the first PCaPC deck slab when joined at the joint surface, in accordance with the main girder position of the first PCaPC deck slab on site.
[0017] The manufacturing method for half-section PCaPC deck slab of claim 5 is characterized in that, in the manufacturing method for half-section PCaPC deck slab of claim 1, the joint between the first PCaPC deck slab and the second PCaPC deck slab is partitioned with a convex material and a concave material that fit into each other, a spacing retaining material that fits into the convex material and the concave material is sandwiched between the two to maintain the spacing, and concrete is poured simultaneously under the same pretensioning conditions using the same tensioning material in the same pretensioning facility.
[0018] The manufacturing method for a half-section PCaPC deck slab of claim 6 is characterized in that, in the manufacturing method for a half-section PCaPC deck slab of claim 5, a guide pin protruding from either the convex material or the concave material is installed, and a pin receiver that fits with the guide pin is installed on the other material.
[0019] The manufacturing method for a half-section PCaPC deck slab of claim 7 is characterized in that, in the manufacturing method for a half-section PCaPC deck slab of claim 6, the guide pin and the pin receiver are formed from a non-corrosive material. Effect of the Invention
[0020] According to the inventions of claims 1 to 7, by adjusting the various conditions during manufacturing of pretensioned half-section PCaPC deck slabs, it is possible to suppress individual differences in the amount of warping and shortening between the half-section PCaPC deck slabs that are integrated on site, thereby achieving improved precision of the joints.
[0021] In particular, according to the invention of claim 2, since curing is performed under coordinated curing conditions, individual differences in the amount of warping or shortening between half-section PCaPC deck slabs caused by differences in curing conditions can be suppressed, thereby achieving improved precision of the joints.
[0022] In particular, according to the invention of claim 3, the first PCaPC deck slab and the second PCaPC deck slab are supported and temporarily stored at positions that are symmetrical when joined at the joint surface, so that the creep phenomena caused by the temporary placement and storage conditions of the first PCaPC deck slab and the second PCaPC deck slab can be made equivalent, individual differences such as creep phenomena caused by differences in temporary placement and storage conditions can be suppressed, and the precision of the joint can be improved.
[0023] In particular, according to the invention of claim 4, the temporary placement position of the second PCaPC deck slab is supported and temporarily stored at a position that is symmetrical when joined at the joint surface with the main girder position of the first PCaPC deck slab, thereby suppressing poor jointing caused by deflection due to creep phenomenon during the temporary placement of the second PCaPC deck slab from the time of construction of the second phase line to the time of construction of the second phase line.
[0024] In particular, according to the invention of claim 5, the joint between the first PCaPC deck slab and the second PCaPC deck slab is partitioned by a convex material and a concave material that fit into each other, and a spacing retaining material that fits into the convex material and the concave material is sandwiched between the two to maintain the spacing.Therefore, even with the pretensioning method, it is possible to suppress individual differences such as the amount of warping and shortening between the half-section PCaPC deck slabs as a pseudo-match cast, and improve the precision of the joint.
[0025] In particular, according to the inventions of claims 6 and 7, since a guide pin and a pin receiver are provided, it is possible to further improve the accuracy of the joint.
[0026] In particular, according to the invention of claim 7, the guide pins that protrude into the gap between the convex and concave materials that form the water path can be made non-corroded, and therefore the entire PC deck integrated with the half-section PCaPC deck can be made highly durable. [Brief description of the drawings]
[0027] [Figure 1] FIG. 1 is a schematic cross-sectional view for explaining a method for manufacturing a half-section PCaPC deck slab according to an embodiment of the present invention. [Diagram 2]FIG. 2 is a perspective view showing the manufacturing state of the joint between the first PCaPC deck and the second PCaPC deck. [Diagram 3] FIG. 3 is a partially enlarged view of FIG. 2, further enlarging the joint between the first PCaPC deck and the second PCaPC deck. [Figure 4] Figure 4 shows the first half of the construction flow for a conventional half-section PCaPC deck. [Diagram 5] Figure 5 shows the latter half of the construction flow for a conventional half-section PCaPC deck slab. [Figure 6] FIG. 6 is a perspective view showing a segment of a box girder bridge. [Figure 7] FIG. 7 is an explanatory diagram of a manufacturing method using the match cast method. [Figure 8] FIG. 8 is a diagram showing that the match-cast manufacturing method cannot be applied to pretensioned PC deck slabs. [Figure 9] Figure 9 is a diagram explaining the support positions of the first PCaPC deck slab and the second PCaPC deck slab in their temporary placement and storage state, where (a) is a diagram showing the temporary placement state before construction, (b) is a diagram showing the temporary placement state during the construction of the first phase line, and (c) is a diagram showing the state during the construction of the second phase line. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0028] Hereinafter, one embodiment for carrying out the manufacturing method for a half-section PCaPC deck slab according to the present invention will be described in detail with reference to the drawings.
[0029] <Previous issues> First, the problems of the conventional half-section PCaPC deck will be explained using Figures 4 and 5. Figure 4 is a diagram showing the first half of the construction flow of the conventional half-section PCaPC deck, and Figure 5 is a diagram showing the second half of the construction flow of the conventional half-section PCaPC deck.
[0030] As shown in Figure 4, the construction flow for a conventional half-section PCaPC deck is as follows: 1. In the process of restricting passing lanes and installing temporary protective fences, the passing lane is restricted and a temporary protective fence G1 is installed to separate the construction area from the shared lane. Next, in the process of removing the RC deck in the passing lane, the existing RC deck B1 in the passing lane is cut into small pieces and removed. Then, in the process of installing the PC deck in the passing lane, a new PCaPC deck (second PCaPC deck 20) is installed in the passing lane section where the RC deck was removed.
[0031] After that, in 4. Passing lane wall parapet construction process, wall parapet K1 is constructed on the ground cover of the newly constructed PCaPC deck (second PCaPC deck 20). After that, in 5. Temporary guardrail relocation and lane switching process, temporary guardrail G1 is relocated, the division with the construction area and the lane for traffic control are changed, and the first half of the flow is completed.
[0032] As shown in Figure 5, next, in process 6. Removal of RC deck slab in driving lane, the existing RC deck slab of the driving lane is cut into small pieces and removed. Then, in process 7. Installation of PC deck slab in driving lane, a new PCaPC deck slab is installed in the driving lane where the RC deck slab was removed.
[0033] After that, in process 8. PC plate joining (tensioning PC steel), the PC steel is tensioned and prestress is applied using the post-tensioning method to integrate the newly constructed half-section PCaPC deck slabs. Then, in process 9. Running lane wall balustrade construction, wall balustrades are constructed on the ground covering section of the newly constructed PCaPC deck slab installed in the passing lane. This completes the construction of the conventional half-section PCaPC deck slab, in other words, the replacement work of the existing RC deck slab with a new PC deck slab by construction of half sections at a time is completed, and the lane restrictions are lifted.
[0034] Thus, in the conventional construction flow for half-section PCaPC decks, the timing of installation of the new half-section PCaPC decks differed greatly between the driving lane and the passing lane. Generally, precast components (PCa decks) are manufactured by working backwards from the on-site construction schedule, which inevitably means that the manufacturing timing of the PCaPC decks for the driving lane and the passing lane differs, and as mentioned in the background technology, differences in manufacturing lead to individual differences in the amount of warping and shortening between the integrated half-section PCa decks, which resulted in problems such as steps and gaps at the joints.
[0035] <Matchcast> Next, the manufacturing method of the match cast method will be briefly explained using Figures 6 to 8. Figure 6 is a perspective view showing a segment BS of a box girder bridge, and Figure 7 is an explanatory diagram of the manufacturing method of the match cast method. Also, Figure 8 is a diagram showing that the manufacturing method of the match cast method cannot be applied to a pretensioned PC deck slab.
[0036] As a technology for improving the accuracy of joints, a technique using the match-cast method is known for manufacturing box girder bridge segments BS as shown in Figure 6. The match-cast method of manufacturing is a manufacturing method in which, as shown in Figure 7, in the manufacturing of a new NEW segment, which is a precast member, the joint surface of an existing OLD segment, which is an existing precast member, is used as a formwork to manufacture concrete in a stockyard near the site, and the newly manufactured NEW segment is then moved and the joint surface of the other end is used as the joint surface of the OLD segment, and this process is repeated in sequence.
[0037] However, as shown in Figure 8, in a pretensioned PC deck, there are tendons such as PC steel 2, and if they are manufactured using the match-cast method, the half-section PCaPC decks 101, 102 become integrated and cannot be constructed at different times.
[0038] [Manufacturing method for half-section PCaPC deck slabs in actual form] Therefore, in the manufacturing method of the half-section PCaPC deck according to the practical embodiment of the present invention, concrete is poured simultaneously under the same pretensioning conditions using the same tendons in the same pretensioning facility. Specifically, as shown in Fig. 1, a pair of upper and lower PC steel members 2,...,2 are tensioned between parallel abbots 1,1 of the same pretensioning facility so as to have the same tension, and a space divided into two by steel plates is created between them, and concrete is poured simultaneously into the steel plates to manufacture the half-section PCaPC deck. Fig. 1 is a schematic cross-sectional view for explaining the manufacturing method of the half-section PCaPC deck according to the practical embodiment of the present invention.
[0039] However, although the PC steel material 2 has been described as an example, the tension member may be made of a continuous fiber reinforcing material that combines continuous fibers such as carbon fibers, such as carbon fiber cables (CFRP strands), or aramid fibers with synthetic resins such as epoxy resins.
[0040] Specifically, a box-shaped steel plate 11, which is a rectangular parallelepiped with an open top and which constitutes the outer shell of the first PCaPC deck 10, one of the two divided half-section PCaPC decks, is installed, and a box-shaped steel plate 21, which is a rectangular parallelepiped with an open top and which constitutes the outer shell of the other, second PCaPC deck 20, is installed. Then, the side of the box-shaped steel plate 11, which forms the joint between the first PCaPC deck 10 and the second PCaPC deck 20, is made into a convex material 12, and the side of the box-shaped steel plate 21 is made into a concave material 22 to separate them, and the same concrete 13, 23 is poured at the same time.
[0041] By manufacturing in this manner, each of the half-section PCaPC deck slabs 10, 20, which are divided into two in the direction perpendicular to the bridge axis, is made into a composite deck consisting of box-shaped steel plates 11, 21 and concrete 13, 23 poured into these box-shaped steel plates 11, 21. As a result, even with pretensioned prestressed members that could not be produced using the match-cast method due to the tendons getting in the way, it is possible to suppress individual differences in the amount of warping and shortening between the half-section PCaPC deck slabs as a quasi-match-cast, and achieve improved precision in the joints.
[0042] Next, the joint between the first PCaPC slab 10 and the second PCaPC slab 20 will be described in more detail with reference to Figures 2 and 3. Figure 2 is a perspective view showing the manufacturing state of the joint between the first PCaPC slab 10 and the second PCaPC slab 20, and Figure 3 is a partially enlarged view further enlarging the joint between the first PCaPC slab 10 and the second PCaPC slab 20.
[0043] As shown in Figures 2 and 3, the convex member 12 has a convex strip 12a extending horizontally in the vertical center, and the concave member 22 has a concave strip 22a extending horizontally in the vertical center, so that they fit together. After the convex member 12 and the concave member 22 are connected and fitted together on-site, they form a shear key that resists shear forces acting in the vertical direction. For this reason, as described above, if a step or gap occurs in the fitting state of the convex member 12 and the concave member 22 that constitute the joint, this will ultimately have a significant impact on the load-bearing performance and durability of the PCaPC deck slab in which the first PCaPC deck slab 10 and the second PCaPC deck slab 20 are joined.
[0044] In the manufacturing method for a half-section PCaPC deck slab according to this practical embodiment, as shown in Figures 2 and 3, concrete is poured in a state in which multiple spacing retaining materials 3 of the same shape that fit into the convex members 12 and concave members 22 are sandwiched between them to maintain the gap, as shown in Figures 2 and 3. These spacing retaining materials 3 have the function of maintaining the gap between the convex members 12 and concave members 22 at the same distance until the poured concrete 13, 23 develops the strength to fix the tension of the PC steel members 2, which acts as the prestress of the pretension, with its adhesive force.
[0045] In addition, each spacing retaining material 3 has a circular hole 3a drilled in the center, and by inserting rod material such as round steel through the circular holes 3a of multiple spacing retaining materials 3, the spacing retaining materials 3 are kept parallel to each other, thereby maintaining the same distance between the convex material 12 and the concave material 22.
[0046] Furthermore, as shown in Figures 2 and 3, in the manufacturing method for the half-section PCaPC deck slab relating to this practical form, a guide pin 14 protruding from the convex strip 12a of the convex material 12 is installed, and a pin receiver 24 that fits with this guide pin 14 is installed inside the concave strip 22a of the concave material 22, and concrete 13, 23 are poured, respectively.
[0047] By providing guide pins 14 and pin receivers 24, when the PC plates are tensioned and integrated using the post-tensioning method in the aforementioned PC plate joining (PC steel tensioning) process, the guide pins 14 and pin receivers 24 guide the first PCaPC deck slab 10 and the second PCaPC deck slab 20 in the vertical and axial directions, and the first PCaPC deck slab 10 and the second PCaPC deck slab 20 are joined in an accurate position, thereby improving the precision of the joint.
[0048] Here, the guide pin 14 and the pin receiver 24 are preferably made of a material that does not corrode, such as resin, FRP (Fiber Reinforced Plastics), ceramics, etc. The gap between the convex material 12 and the concave material 22 that form the joint between the first PCaPC deck 10 and the second PCaPC deck 20 is highly likely to become a water path, and the guide pin 14 that protrudes into the gap and the pin receiver 24 that communicates with the gap can be made to not corrode.
[0049] In addition, the numerals 15 and 25 denote sheaths 15 and 25 through which the tensioning material used to integrate the first PCaPC deck 10 and the second PCaPC deck 20 by tensioning them using the post-tensioning method in the aforementioned PC plate joining (PC steel tensioning) process is inserted.
[0050] Thereafter, in the manufacturing method for the half-section PCaPC deck according to the present embodiment, the first PCaPC deck 10 and the second PCaPC deck 20 are cured in the same curing facility under the same curing conditions. Specifically, the first PCaPC deck 10 and the second PCaPC deck 20 are installed side by side in the same curing facility and cured so that the curing conditions, such as the steam curing temperature, are as similar as possible. This is to eliminate individual differences in the rate at which the hydration reaction progresses and differences in the amount of creep due to differences in curing conditions.
[0051] In addition, in the manufacturing method for the half-section PCaPC deck slab according to the present embodiment, the first PCaPC deck slab 10 and the second PCaPC deck slab 20 are temporarily placed and stored while being supported in accordance with the fulcrum positions of the deck slabs in the final integrated and joined state. Specifically, as shown in Fig. 9(a), in the pre-construction stage, the first PCaPC deck slab 10 and the second PCaPC deck slab 20 are temporarily placed and stored while being supported in positions that are symmetrical when joined at the joint surface of the convex material 12 and the concave material 22. "Symmetrical" means that the fulcrum positions during temporary placement are equidistant (D1=D1, D2=D2) from the end of the convex material 12 or the end of the concave material 22, which are the joint surfaces.
[0052] Then, as shown in Figure 9(b), when the first PCaPC deck 10, which is one of the two divided half-section PCaPC decks, is constructed during the first phase of construction, the temporary placement position of the second PCaPC deck 20 is supported and temporarily stored in a position that is symmetrical to the main girder position of the first PCaPC deck 10 when joined at the joint surface, in accordance with the main girder position of the first PCaPC deck 10 on-site. In other words, it is stored so that the support positions at the time of temporary placement are equidistant (D1'=D1', D2'=D2') from the end of the convex material 12 or the end of the concave material 22, which will be the joint surface.
[0053] As shown in Figure 9(c), even if the first PCaPC deck 10 and the second PCaPC deck 20 are deflected due to creep between the time of the first stage line construction and the time of the second stage line construction, the deflection δ1 will be approximately the same because the support conditions are approximately the same when the concrete is poured. In other words, by temporarily storing them in this way, it is possible to suppress individual differences in creep phenomena and the like caused by differences in temporary storage and storage conditions.
[0054] According to the manufacturing method for half-section PCaPC deck slabs of this embodiment described above, by matching the various conditions during manufacturing of the first PCaPC deck slab 10 and the second PCaPC deck slab 20, which are pretensioned half-section PCaPC deck slabs, it is possible to suppress individual differences between the first PCaPC deck slab 10 and the second PCaPC deck slab 20, which are integrated on-site in the PC plate joining (PC steel tensioning) process, such as the amount of warping and shortening, and to eliminate steps and gaps between the convex material 12 and the concave material 22, thereby achieving improved precision at the joint.
[0055] Furthermore, according to the manufacturing method of the half-section PCaPC deck slab of this embodiment, the slabs are manufactured by installing guide pins 14 and pin receivers 24. Therefore, when the slabs are tensioned and integrated using the post-tensioning method in the PC plate joining (PC steel tensioning) process, the guide pins 14 and pin receivers 24 guide the slabs in the vertical and bridge axis directions, allowing the first PCaPC deck slab 10 and the second PCaPC deck slab 20 to be joined in an accurate position, thereby improving the precision of the joint.
[0056] Furthermore, according to the manufacturing method for half-section PCaPC deck slabs of this embodiment, curing is performed under coordinated curing conditions, thereby suppressing individual differences between the first PCaPC deck slab 10 and the second PCaPC deck slab 20, such as the amount of warping and shortening, which are caused by differences in curing conditions, and improving the accuracy of the joints.
[0057] In addition, according to the manufacturing method for half-section PCaPC deck slabs of this embodiment, the deck slabs are temporarily placed and stored by supporting them in accordance with the fulcrum positions of the slabs in their final integrated and joined state, thereby suppressing individual differences between the first PCaPC deck slab 10 and the second PCaPC deck slab 20, such as creep phenomena caused by differences in temporary placement or storage conditions, and improving the precision of the joints.
[0058] Furthermore, according to the manufacturing method for the half-section PCaPC deck slab of this embodiment, the guide pin 14 and the pin receiver 24 are formed from a material that does not corrode, thereby making it possible to make the entire PC deck slab in which the first PCaPC deck slab 10 and the second PCaPC deck slab 20 are integrated highly durable.
[0059] Although the manufacturing method of the half-section PCaPC deck slab according to the embodiment of the present invention has been described in detail above, the above-mentioned and illustrated embodiments are merely examples of the present invention. Therefore, the technical scope of the present invention should not be interpreted as being limited by these. [Explanation of symbols]
[0060] 1: Abbott 2: PC steel material (tension material) 3: Spacing material 3a: Circular hole 10: 1st PCaPC floor slab 11: Box steel plate 12: Convex material 12a: Convex stripe 13: Concrete 14: Guide pin 15;Sheath 20: 2nd PCaPC floor slab 21: Box steel plate 22: Concave material 22a: Groove 23: Concrete 24: Pin receiver 25;Sheath 101,102: Half-section PCaPC floor slab B1:RC floor slab G1: Temporary security fence K1: Wall railing
Claims
1. A method for manufacturing a half-section PCa deck in which a bridge deck is divided into a first PCa PC deck and a second PCa PC deck in a direction perpendicular to the bridge axis, and the first PCa PC deck and the second PCa PC deck are constructed at different times and integrated on-site, The first PCaPC floor slab and the second PCaPC floor slab are manufactured by simultaneously pouring concrete under the same pretensioning conditions using the same tension material in the same pretensioning facility. A method for manufacturing a half-section PCaPC deck slab, characterized by the above.
2. The first PCaPC floor slab and the second PCaPC floor slab are cured under the same curing conditions in the same curing facility. A method for manufacturing a half-section PCaPC deck slab as claimed in claim 1.
3. The first PCaPC floor slab and the second PCaPC floor slab are supported and temporarily stored in positions that are symmetrical when joined at the joint surface. A method for manufacturing a half-section PCaPC deck slab according to claim 1 or 2.
4. When constructing the first PCaPC deck during the construction of the first stage line, the temporary placement position of the second PCaPC deck shall be supported and temporarily stored in a position that is symmetrical to the main girder position of the first PCaPC deck when joined at the joint surface, in accordance with the main girder position of the first PCaPC deck on-site. A method for manufacturing a half-section PCaPC deck slab as claimed in claim 3.
5. The joint between the first PCaPC deck and the second PCaPC deck is partitioned with a convex material and a concave material that fit into each other, and a spacing retaining material that fits into the convex material and the concave material is sandwiched between them to maintain the spacing, and the concrete is poured simultaneously under the same pretension conditions using the same tension material in the same pretension facility to manufacture the structure. A method for manufacturing a half-section PCaPC deck slab as claimed in claim 1.
6. A guide pin is provided to protrude from either the convex member or the concave member, and a pin receiver that fits with the guide pin is provided on the other member. A method for manufacturing a half-section PCaPC deck slab as claimed in claim 5.
7. The guide pin and the pin receiver are made of a material that does not corrode. A method for manufacturing a half-section PCaPC deck slab as described in claim 6.
Citation Information
Patent Citations
Change-over method of concrete slab for highway road, and change-over PC slab by the method
JP2015151768A
Manufacturing method and construction method for precast concrete member
JP2016216981A
Stepwise construction method of concrete precast floor slab for bridge
JP2014177767A
Joining structure and joining method
JP2021067052A