Coating method

The coating method for automobile parts uses a thermoplastic polyurethane resin with reduced shaping air and controlled thickness to address environmental and efficiency challenges, achieving improved coating efficiency and chipping resistance in a 3-coat, 1-preheat, 1-bake process.

JP2024136215APending Publication Date: 2024-10-04DAIHATSU MOTOR CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023047252
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-23
Publication Date
2024-10-04

AI Technical Summary

Technical Problem

Existing coating methods for automobile parts face challenges in reducing preheating steps for environmental friendliness and cost, while maintaining coating efficiency and chipping resistance, particularly when using electrostatic atomization coating devices.

Method used

A coating method that applies an intermediate coating with a thermoplastic polyurethane resin, reduces shaping air usage, and controls the dry thickness of the intermediate coating to less than 13 μm, followed by a base coating without preheating and a clear coating, all within a 3-coat, 1-preheat, 1-bake process.

Benefits of technology

This method improves environmental friendliness by reducing preheating, enhances coating efficiency by minimizing shaping air use, and maintains excellent chipping resistance through the use of thermoplastic polyurethane resin, preventing mixed layers and ensuring high-quality coating results.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024136215000001_ABST
    Figure 2024136215000001_ABST
Patent Text Reader

Abstract

To provide a coating method which can obtain a coated matter that reduces the number of times of preheating and can improve environment property, reduces a use amount of shaping air and can improve coating efficiency, reduces a coating amount of an intermediate coating material and can suppress a mixed layer, and is excellent in chipping resistance (impact absorption property).SOLUTION: A coating method includes an intermediate coating step, a base coating step, a preheating step, a clear coating step and a baking step. In the intermediate coating step, the intermediate coating material contains a thermoplastic polyurethane resin. The intermediate coating material is coated by an air reduction coating method. Dry thickness of an intermediate coating film 3 is 13 μm or less.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a coating method, and more particularly to a coating method for components that constitute an automobile body. [Background technology]

[0002] The automobile parts are made of, for example, metal and / or resin. The automobile parts are painted, for example, with various paints. For example, as shown in FIG. 2A, first, the automobile parts as the objects to be painted are electrocoated to form an electrocoated film. Next, the automobile parts are painted with an intermediate coat, and the intermediate coat is formed on the electrocoated film. Next, the automobile parts are subjected to a first preheat (first time). Next, the automobile parts are painted with a base coat, and the base coat is formed on the intermediate coat. Next, the automobile parts are subjected to a second preheat (second time). Next, the automobile parts are painted with a clear coat, and the clear coat is formed on the base coat. Thereafter, the automobile parts are baked. In this way, the automobile parts are painted (3 coat 2 preheat 1 bake method).

[0003] On the other hand, in the field of painting, from the viewpoint of improving environmental friendliness and reducing costs, omission of the preheating step is required. In such a case, for example, the number of preheatings is reduced to one. For example, as shown in FIG. 2B, first, an automobile component is electrocoated to form an electrocoating film. Next, the automobile component is coated with an intermediate coat, and an intermediate coat film is formed on the electrocoating film. Next, the automobile component is base coated without being preheated, and a base coat film is formed on the intermediate coat film. Next, the automobile component is preheated. Next, the automobile component is clear coated, and a clear coat film is formed on the base coat film. After that, the automobile component is baked. In this way, the automobile component is coated (3 coat 1 preheat 1 bake method).

[0004] Furthermore, in the field of painting, there is a demand for improved paint application efficiency in order to reduce costs.

[0005] More specifically, for example, a bell coater has been used in the past for applying an undercoat paint. In a bell coater, the paint atomized by a rotary atomization method is propelled in a straight line by shaping air to coat the object to be coated.

[0006] However, in the above method, the shaping air that bounces off the workpiece scatters paint particles, which can result in low coating efficiency. Therefore, there is a demand for improving coating efficiency.

[0007] Therefore, a method for applying paint while reducing the amount of shaping air used has been proposed. For example, the following electrostatic atomization type coating device has been proposed. That is, the electrostatic atomization type coating device includes a rotary head, a drive unit, a voltage application unit, and a voltage control unit. The rotary head is formed so that the inner diameter expands from the base toward the open end. In addition, a plurality of grooves are formed radially on the inner peripheral surface of the open end. The drive unit rotates the rotary head. The voltage application unit applies a voltage to the rotating rotary head to form an electrostatic field between the open end of the rotary head and the object to be painted in the earthed state. The voltage control unit adjusts the strength of the electrostatic field by controlling the voltage output from the voltage application unit. In this way, the thread-like paint discharged from the open end is electrostatically atomized while controlling the particle size of the electrostatically atomized paint (see, for example, Patent Document 1).

[0008] Such an electrostatic atomization coating device allows coating of a substrate without using shaping air. Hereinafter, the method of coating a substrate without using shaping air will be referred to as the airless method. [Prior art documents] [Patent documents]

[0009] [Patent Document 1] JP 2017-042749 A Summary of the Invention [Problem to be solved by the invention]

[0010] However, when the electrostatic atomization coating device is used, the paint is not sprayed with shaping air, so the coating does not dry sufficiently. Therefore, as shown in Figure 2C, when the electrostatic atomization coating device is used (airless method) to apply the intermediate coating, if the number of preheating times is reduced (3 coat 1 preheat 1 bake method), there is a problem that the intermediate coating and base coating will become mixed layers.

[0011] In order to prevent the intermediate coating film and the base coating film from intermixing, it has been considered to reduce the amount of intermediate coating paint applied, for example, as shown in Fig. 2D. However, in such a case, the thickness of the intermediate coating film becomes thin, which is problematic in that the chipping resistance (shock absorption) of the coated object decreases.

[0012] Therefore, in the field of painting, there is a demand for a painting method that can improve environmental friendliness by reducing the number of times preheating is performed, improve painting efficiency by reducing the amount of shaping air used, reduce the amount of intermediate paint applied to suppress inter-layer mixing, and obtain a coated object with excellent chipping resistance (shock absorption properties).

[0013] The present invention is a coating method that can improve environmental friendliness by reducing the number of times preheating is performed, improve coating efficiency by reducing the amount of shaping air used, reduce the amount of intermediate paint applied to suppress inter-layer mixing, and obtain a coated object with excellent chipping resistance (shock absorption properties). [Means for solving the problem]

[0014] The present invention [1] includes a coating method comprising an intermediate coating step of coating an intermediate coating on an electrodeposition-coated substrate to form an intermediate coating film, a base coating step of coating a base coating on the substrate without preheating the substrate to form a base coating film on the intermediate coating film, a preheating step of preheating the substrate to which the intermediate coating and base coating have been applied, a clear coating step of coating a clear coating on the preheated substrate to form a clear coating film on the base coating film, and a baking step of baking the substrate to which the intermediate coating, base coating and clear coating have been applied, wherein in the intermediate coating step, the intermediate coating comprises a thermoplastic polyurethane resin, the intermediate coating is applied by an air-reducing coating method, and the dry thickness of the intermediate coating film is 13 μm or less.

[0015] In the above coating method, the base coating is formed without preheating the substrate (intermediate coating), and then the substrate (intermediate coating and base coating) that has been coated with the intermediate coating and base coating is preheated. Therefore, in the above coating method, the number of preheating steps can be reduced, improving environmental friendliness.

[0016] In the above coating method, the intermediate coating is applied by a reduced air coating method, which reduces the amount of shaping air used and improves coating efficiency.

[0017] Furthermore, in the above coating method, the dry thickness of the intermediate coating film is equal to or less than a predetermined value, so that the amount of intermediate coating paint applied can be reduced and mixing of the intermediate coating film and the base coating film can be suppressed.

[0018] In addition, in the above coating method, the intermediate coating contains a thermoplastic polyurethane resin. Thermoplastic polyurethane resin has excellent impact absorption properties. Therefore, according to the above coating method, even if the intermediate coating film is relatively thin, it is possible to obtain a coated object with excellent chipping resistance (impact absorption properties). Effect of the Invention

[0019] According to the coating method of the present invention, the number of preheating cycles can be reduced to improve environmental friendliness, the amount of shaping air used can be reduced to improve coating efficiency, and the amount of intermediate paint applied can be reduced to suppress inter-layer mixing, resulting in a coated object with excellent chipping resistance (shock absorption). [Brief description of the drawings]

[0020] [Figure 1] Figures 1A to 1F are schematic process diagrams showing one embodiment of the coating method of the present invention. Figure 1A shows an electrodeposition-coated substrate. Figure 1B shows an intermediate coating process in which an intermediate coating film is formed on an electrodeposition-coated substrate. Figure 1C shows a base coating process in which a base coating film is formed on the intermediate coating film. Figure 1D shows a preheating process in which the substrate is preheated. Figure 1E shows a clear coating process in which a clear coating film is formed on the base coating film. Figure 1F shows a baking process in which the substrate is baked. [Diagram 2] Figures 2A to 2D are schematic diagrams of a coated object obtained by a conventional coating method. Figure 2A is a schematic diagram of a coated object obtained by a conventional 3-coat, 2-preheat, 1-bake method. Figure 2B is a schematic diagram of a coated object obtained by a conventional 3-coat, 1-preheat, 1-bake method. Figure 2C is a schematic diagram of a coated object obtained by a conventional airless method. Figure 2D is a schematic diagram of a coated object when the amount of intermediate coating paint used is reduced in the conventional airless method. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0021] 1A to 1F are schematic process diagrams showing one embodiment of the coating method of the present invention. In this coating method, the object to be coated 1 is, for example, a member constituting an automobile body (hereinafter, automobile member). Examples of automobile members include the main body of the automobile and various panels (e.g., door panels). Examples of materials for automobile members include metals (e.g., steel plates) and resins (e.g., conductive resins). The object to be coated 1 passes through a coating line and is coated with various paints in multiple coating booths in the coating line.

[0022] More specifically, in this coating method, first, an electrodeposition-coated substrate 1 is prepared as shown in Fig. 1A. The electrodeposition-coated substrate 1 is obtained, for example, by passing the substrate 1 through an electrodeposition coating booth in a coating line to form an electrodeposition coating film 2.

[0023] Next, in this coating method, as shown in Fig. 1B, an intermediate coating paint is applied (intermediate coating) to the electrodeposition-coated substrate 1. As a result, an intermediate coating film 3 is formed on the electrodeposition coating film 2 of the substrate 1 (intermediate coating step).

[0024] Examples of the intermediate coating paint include water-based intermediate coating paints and solvent-based intermediate coating paints. As the intermediate coating paint, water-based intermediate coating paints are preferably used.

[0025] A water-based intermediate coating paint contains, for example, water, an intermediate coating resin component that is dissolved and / or dispersed in water, and a pigment.

[0026] In the water-based intermediate coating paint, the intermediate coating resin component is a resin component having a hydrophilic group. Examples of the hydrophilic group include a carboxyl group, a hydroxyl group, a methylol group, an amino group, a sulfonic acid group, and a polyoxyethylene group. A preferred example of the hydrophilic group is a hydroxyl group.

[0027] The intermediate coating resin component contains a thermoplastic polyurethane resin as an essential component. That is, the intermediate coating paint contains a thermoplastic polyurethane resin as an essential component. The thermoplastic polyurethane resin is not particularly limited and is produced by a known method. For example, the thermoplastic polyurethane resin is produced as a urethane prepolymer and / or a urethane polymer in accordance with the description of JP-A-4-219177.

[0028] The thermoplastic polyurethane resin is dissolved and / or dispersed in water by a known method. For example, a water dispersion of the thermoplastic polyurethane resin is produced in accordance with the description in JP-A-4-219177.

[0029] The number average molecular weight of the thermoplastic polyurethane resin is, for example, 5000 or more, or preferably 10000 or more. The number average molecular weight of the thermoplastic polyurethane resin is, for example, 50000 or less, or preferably 35000 or less.

[0030] Thermoplastic polyurethane resin has excellent impact absorption properties, so if the intermediate coating contains a thermoplastic polyurethane resin, it is possible to obtain a coated article 1 having excellent chipping resistance (impact absorption properties).

[0031] The intermediate coating resin component may contain other resins as long as the excellent effects of the present invention are not impaired. The other resins are resins other than thermoplastic polyurethane resins. Examples of the other resins include thermoplastic resins other than thermoplastic polyurethane resins and thermosetting resins.

[0032] Examples of thermoplastic resins other than thermoplastic polyurethane resin include polycarbonate resin, polyphenylene ether resin, and aromatic vinyl resin. Examples of thermosetting resins include thermosetting polyurethane resin, acrylic resin, polyester resin, alkyd resin, olefin resin, and epoxy resin. These can be used alone or in combination of two or more kinds.

[0033] When the intermediate coating resin component contains a thermosetting resin, the intermediate coating paint can contain a crosslinking agent. Examples of crosslinking agents include melamine resins, urea resins, and polyisocyanates. These can be used alone or in combination of two or more. The content of the crosslinking agent is appropriately set depending on the purpose and application.

[0034] From the viewpoint of impact absorption (chipping resistance), the intermediate coating resin component preferably does not contain a thermosetting resin or a crosslinking agent and is made of a thermoplastic resin, more preferably a thermoplastic polyurethane resin.

[0035] More specifically, a two-component thermosetting intermediate coating paint can be cited as a conventional intermediate coating paint. Such intermediate coating paint contains a thermosetting resin (first liquid) and a crosslinking agent (second liquid) as intermediate coating resin components. The thermosetting resin (first liquid) and the crosslinking agent (second liquid) are mixed when used and applied to the electrodeposition coating film 2 of the substrate 1. This forms the intermediate coating film 3. The intermediate coating film 3 is also heated and cured to form an intermediate coating layer. In such a case, if the thickness of the intermediate coating layer (the dry thickness of the intermediate coating film 3) is made relatively thin, the intermediate coating layer is likely to crack and peel off. As a result, excellent impact absorption (chipping resistance) cannot be obtained. Another conventional intermediate coating paint is a one-component thermosetting intermediate coating paint. However, a one-component thermosetting intermediate coating paint contains a crosslinking agent (such as a blocked isocyanate), or a clear curing agent (described later) seeps into the coating film of the one-component thermosetting intermediate coating paint. Even in such a case, if the film thickness of the intermediate coat layer (the dry film thickness of the intermediate coat film 3) is made relatively thin, the intermediate coat layer is likely to crack and peel off. As a result, excellent impact absorption (chipping resistance) cannot be obtained. Therefore, from the viewpoint of impact absorption (chipping resistance), it is preferable that neither a two-component thermosetting intermediate coat paint nor a one-component thermosetting intermediate coat paint is used as the intermediate coat paint. More specifically, the intermediate coat resin component preferably does not contain a thermosetting resin or a crosslinking agent and is made of a thermoplastic resin, more preferably a thermoplastic polyurethane resin.

[0036] The pigment is not particularly limited, and includes known color pigments and known metallic pigments. Examples of the color pigment include titanium dioxide, zinc oxide, basic lead sulfate, calcium plumbate, zinc phosphate, aluminum phosphate, zinc molybdate, calcium molybdate, Prussian blue, ultramarine blue, cobalt blue, copper phthalocyanine blue, indanthrone blue, yellow lead, synthetic yellow iron oxide, transparent red iron oxide (yellow), bismuth vanadate, titanium yellow, zinc yellow, strontium chromate, cyanamide lead, monoazo yellow, monoazo yellow, disazo, monoazo yellow, isoindolinone yellow, metal complex azo yellow, quinophthalone yellow, isoindoline yellow Examples of metallic pigments include aluminum powder, flake aluminum oxide, pearl mica, and flake mica. These can be used alone or in combination of two or more. The content of the pigment is, for example, 20 to 120 parts by mass relative to 100 parts by mass of the intermediate coating resin component.

[0037] The water-based intermediate coating paint can contain a promoter in an appropriate ratio. Examples of the promoter include dissociation catalysts that dissociate the blocking agent. Examples of the dissociation catalysts include tin octoate, dibutyltin di(2-ethylhexanoate), dioctyltin di(2-ethylhexanoate), dioctyltin diacetate, dibutyltin dilaurate, dibutyltin oxide, monobutyltin trioctate, lead 2-ethylhexanoate, and zinc octoate. The water-based intermediate coating paint can also contain an acid catalyst in an appropriate ratio. Examples of the acid catalyst include phosphoric acid catalysts and sulfonic acid catalysts. These can be used alone or in combination of two or more types.

[0038] The water-based intermediate coating paint can contain additives in an appropriate ratio. Examples of additives include optical interference pigments, extender pigments, dispersants, anti-settling agents, organic solvents, reaction accelerators, defoamers, thickeners, rust inhibitors, UV absorbers, and surface conditioners. These can be used alone or in combination of two or more types.

[0039] The intermediate coating paint is prepared by a known method. For example, the above-mentioned components are blended and mixed in water. The solid content of the intermediate coating paint is, for example, 20% by mass or more and 60% by mass or less.

[0040] In the intermediate coating process, for example, an intermediate coating paint containing a thermoplastic polyurethane resin is atomized in an intermediate coating booth of a painting line. Then, the fine particles of the intermediate coating paint containing a thermoplastic polyurethane resin adhere to the electrodeposition coating film 2 of the substrate 1. In other words, the substrate 1 is coated with an intermediate coating paint containing a thermoplastic polyurethane resin (urethane intermediate coating).

[0041] In the intermediate coating process, a method in which the amount of shaping air used is equal to or less than a predetermined value is adopted as the intermediate coating paint application method. A coating method in which the amount of shaping air used is equal to or less than a predetermined value described below is called an air-reduced coating method. Air-reduced coating methods include the airless method (a coating method that does not use shaping air) described below.

[0042] That is, a bell coater has been conventionally used to apply an undercoat paint to a substrate. However, when a bell coater is used, a large amount of shaping air (for example, more than 250 NL / min, preferably 300 NL / min or more) bounces off the substrate 1, scattering fine particles of paint, resulting in insufficient coating efficiency. Therefore, in this method, the amount of shaping air used is reduced compared to when a bell coater is used.

[0043] More specifically, when applying the intermediate coating material to the substrate, the shaping air flow rate is, for example, 250 NL / min or less, preferably 200 NL / min or less, and more preferably 180 NL / min or less.

[0044] When applying an intermediate coating to an object to be coated, if the shaping air flow rate is equal to or less than the above-mentioned predetermined value, coating efficiency can be improved.

[0045] Particularly preferably, in the application of the intermediate coating paint to the substrate, the shaping air flow rate is 0 NL / min. In other words, in the intermediate coating process, the intermediate coating paint is preferably atomized without using shaping air, and then the substrate 1 is coated (airless method).

[0046] When the airless method is employed, examples of the coating device for coating the intermediate coating paint include the electrostatic atomization coating device described in JP 2017-042749 A and the coating device described in JP 2019-055345 A. The coating conditions are set appropriately depending on the type of coating device.

[0047] When applying the undercoat paint to the substrate, if the airless method (shaping air flow rate 0NL / min) is used, painting efficiency can be improved particularly effectively.

[0048] Then, by coating the substrate 1 with the intermediate coating material in the above-mentioned manner, an intermediate coating film 3 is formed on the electrodeposition coating film 2.

[0049] The dry thickness of the intermediate coating film 3 is relatively thin. More specifically, the dry thickness of the intermediate coating film 3 is 13 μm, preferably 10 μm or less, more preferably 8 μm or less, and even more preferably 6 μm or less. The dry thickness of the intermediate coating film 3 is usually 1 μm or more, and preferably 2 μm or more.

[0050] If the dry thickness of the intermediate coating film 3 is relatively thin, it is possible to prevent the intermediate coating film 3 from intermixing with the base coating film 4 described below.

[0051] Next, in this method, as shown in FIG. 2C, a base paint is applied to the substrate 1 (intermediate coating film 3) without preheating the substrate 1, and a base coating film 4 is formed on the intermediate coating film 3 (base coating process).

[0052] That is, in the base coating step, a base paint is applied to the intermediate coating film 3 in a wet state. Examples of the base paint include water-based base paint and solvent-based base paint. As the base paint, a water-based base paint is preferably used.

[0053] The water-based paint is not particularly limited, and may be any known water-based paint. The water-based paint contains, for example, water, a base resin component that is dissolved and / or dispersed in water, and a pigment.

[0054] Examples of the base resin component include thermosetting resins and thermoplastic resins. Examples of the thermosetting resin include the thermosetting resins described above as the intermediate resin component. Examples of the thermoplastic resin include the thermoplastic polyurethane resins described above and other thermoplastic resins (thermoplastic resins other than thermoplastic polyurethane resins). These can be used alone or in combination of two or more kinds. A preferable example of the base resin component is a thermosetting resin.

[0055] When the base resin component contains a thermosetting resin, the base coating preferably contains a crosslinking agent. Examples of the crosslinking agent include melamine resin, urea resin, and polyisocyanate. Examples of the melamine resin include hydrophilic melamine. Examples of the polyisocyanate include known polyisocyanate compounds (unblocked polyisocyanate) and blocked polyisocyanates. Examples of the blocked polyisocyanate include products of blocking polyisocyanate with a blocking agent. Examples of the blocking agent include oxime, phenol, alcohol, lactam, and mercaptan. These can be used alone or in combination of two or more. The content ratio of the crosslinking agent is appropriately set according to the purpose and application.

[0056] When the base resin component contains a thermosetting resin, the base coating material may be a one-component curing type coating material or a two-component curing type coating material. The base coating material is preferably a one-component curing type coating material.

[0057] Examples of the pigment include the above-mentioned color pigments and metallic pigments. These can be used alone or in combination of two or more. The content ratio of the pigment is appropriately set according to the purpose and application.

[0058] The base paint is prepared by a known method. For example, the above-mentioned components are mixed in water and mixed. The solid content of the base paint is, for example, 20% by mass or more and 50% by mass or less.

[0059] In the base coating process, for example, in a base coating booth of a coating line, the base paint is atomized. Then, the fine particles of the base paint adhere to the intermediate coating film 3 of the substrate 1. In other words, the substrate 1 is coated with the base paint.

[0060] The coating device for coating the base paint is not particularly limited, and may be any known coating device. Examples of the coating device include air spray coating devices, airless spray coating devices, bell coating devices, and electrostatic atomization coating devices. These may be used alone or in combination of two or more types.

[0061] As a coating method for coating the base paint, a coating method in which the amount of shaping air used exceeds a predetermined value (air spraying method) is preferably adopted.

[0062] More specifically, in the application of the base paint, the shaping air flow rate is more than 250 NL / min, preferably 300 NL / min or more.

[0063] If an air spraying method is used in applying the base paint, it is particularly effective in preventing the intermediate coating film 3 and the base coating film 4 from intermixing while reducing the number of times preheating is performed.

[0064] Then, by painting the object 1 with the base paint in the above-mentioned manner, a base coating film 4 is formed on the intermediate coating film 3.

[0065] The dry thickness of the base coating film 4 is preferably relatively thin. More specifically, the dry thickness of the base coating film 4 is, for example, 15 μm or less, preferably 10 μm or less, and more preferably 8 μm or less. The dry thickness of the base coating film 4 is usually 3 μm or more, and preferably 6 μm or more. If the dry thickness of the base coating film 4 is relatively thin, mixing of the intermediate coating film 3 and the base coating film 4 can be particularly effectively prevented.

[0066] Next, in this method, as shown in FIG. 1D, the object 1 that has been coated with the intermediate coat and the base coat is preheated (preheating step).

[0067] In the preheating step, for example, in a preheating booth of a coating line, the object 1 on which the intermediate coating film 3 and the base coating film 4 have been formed is preheated with hot air.

[0068] The preheating conditions are not particularly limited, but for example, the hot air blowing temperature is, for example, 45 to 100° C. The hot air blowing speed is, for example, 0.3 to 10.0 m / s. The hot air speed on the surface of the base coating film 4 is, for example, 1 to 3 m / s. The distance from the hot air blowing port to the base coating film 4 is, for example, 20 to 50 cm. The hot air blowing time is, for example, 0.5 to 3.0 minutes.

[0069] This preheats the intermediate coating film 3 and the base coating film 4. When the intermediate coating paint and / or the base coating paint contain a thermosetting resin, the intermediate coating film 3 and the base coating film 4 after preheating are in an uncured state (not cured by heat).

[0070] Next, in this method, as shown in FIG. 1E, a clear coating is applied to the preheated object 1 to form a clear coating film 5 on the base coating film 4 (clear coating step).

[0071] That is, in the clear coating step, a clear coating is applied to the uncured base coating film 4. Examples of the clear coating include water-based clear coating and solvent-based clear coating. As the clear coating, a solvent-based clear coating is preferably used.

[0072] The solvent-based clear coating material is not particularly limited. For example, the solvent-based clear coating material contains a known organic solvent, a clear resin component dissolved and / or dispersed in the organic solvent, and the above-mentioned additives.

[0073] Examples of the clear resin component include the above-mentioned thermosetting resin and the above-mentioned thermoplastic resin. A preferable example of the clear resin component is a thermosetting resin.

[0074] When the clear resin component contains a thermosetting resin, the clear coating preferably contains the above-mentioned crosslinking agent. Examples of the crosslinking agent include the above-mentioned melamine resin, the above-mentioned urea resin, and the above-mentioned polyisocyanate (unblocked polyisocyanate and / or blocked polyisocyanate). These can be used alone or in combination of two or more kinds. The content ratio of the crosslinking agent is appropriately set according to the purpose and application.

[0075] When the clear resin component contains a thermosetting resin, the clear coating material may be a one-component curing type coating material or a two-component curing type coating material. The clear coating material is preferably a two-component curing type coating material.

[0076] When the clear coating is a two-component curing coating, the clear coating contains, for example, a clear base agent and a clear hardener. The clear base agent is, for example, a component that contains the above-mentioned clear resin component and does not contain the above-mentioned crosslinking agent. The clear hardener is, for example, a component that does not contain the above-mentioned clear resin component and contains the above-mentioned crosslinking agent. The clear base agent and the clear hardener are, for example, prepared separately and mixed at the time of use.

[0077] In the clear coating process, for example, the clear coating is atomized in a clear coating booth on a coating line. Then, the fine particles of the clear coating adhere to the base coating film 4 of the object 1 to be coated. In other words, the object 1 to be coated is coated with the clear coating.

[0078] The coating equipment for coating the clear coating material is not particularly limited, and may be any known coating equipment. Examples of coating equipment include air spray coating equipment, airless spray coating equipment, bell coating equipment, and electrostatic atomization coating equipment. These may be used alone or in combination of two or more types.

[0079] As a coating apparatus for applying a clear coating, a method is preferably adopted in which the amount of shaping air used in applying the clear coating is equal to or less than the above-mentioned specified value, and more preferably a method (airless method) in which no shaping air is used in applying the clear coating is adopted.

[0080] When the airless method is used, the coating equipment for applying the clear coating can be, for example, the same coating equipment as that for applying the intermediate coating described above. The coating conditions are set appropriately depending on the type of coating equipment.

[0081] Then, by painting the object 1 with the clear paint in the above-mentioned manner, a clear coating film 5 is formed on the base coating film 4.

[0082] The clear coating film 5 has a dry thickness of, for example, 10 μm or more, or preferably 20 μm or more. The clear coating film 5 has a dry thickness of, for example, 60 μm or less, or preferably 50 μm or less.

[0083] Thereafter, in this method, as shown in FIG. 1F, the object 1 that has been coated with the undercoat, base coat and clear coat is subjected to a baking treatment (baking step).

[0084] The baking method is not particularly limited, but examples thereof include hot air heating, infrared heating, and high-frequency heating. The baking conditions are not particularly limited, and are appropriately set depending on the purpose and application.

[0085] The intermediate coating layer is formed by the baking process. More specifically, the intermediate coating film 3 is dried by the baking process. As a result, the intermediate coating layer is formed on the electrodeposition coating film as a dried coating film of the intermediate coating paint. Furthermore, if the intermediate coating paint contains a thermosetting resin, the intermediate coating film 3 is heated and cured by the baking process.

[0086] Furthermore, a base layer is formed on the intermediate coating layer by the baking process. More specifically, when the base coating contains a thermosetting resin, the base coating (base coating film 4) is thermally cured by the baking process. As a result, a base layer is formed on the intermediate coating layer as a thermosetting film of the base coating.

[0087] Also, a clear layer is formed on the base layer by the baking process. More specifically, if the clear paint contains a thermoplastic resin, the clear paint (clear coating film 5) is thermally cured by the baking process. As a result, a clear layer is formed on the base layer as a thermosetting film of the clear paint.

[0088] That is, in the above coating method, the object 1 is coated by a three-coat, one-preheat, one-bake method. As a result, a multilayer coating film including an intermediate coat layer, a base layer, and a clear coat layer is formed on the object 1.

[0089] Furthermore, according to the above-mentioned coating method, the number of preheating cycles can be reduced to improve environmental friendliness, the amount of shaping air used can be reduced to improve coating efficiency, and the amount of intermediate paint applied can be reduced to suppress inter-layer mixing, resulting in a coated object with excellent chipping resistance (shock absorption).

[0090] That is, in the above coating method, the base coating is formed without preheating the substrate 1 (intermediate coating film 3), and then the substrate 1 (intermediate coating film 3 and base coating film 4) that has been coated with the intermediate coating and base coating is preheated. Therefore, in the above coating method, the number of preheating steps can be reduced, improving environmental friendliness.

[0091] In the above coating method, the intermediate coating is applied by a reduced air coating method, which reduces the amount of shaping air used and improves coating efficiency.

[0092] Furthermore, in the above coating method, the dry thickness of the intermediate coating film 3 is equal to or less than a predetermined value. Therefore, in the above coating method, the amount of intermediate coating paint 3 applied can be reduced, and mixing of the intermediate coating film 3 and the base coating film 4 can be suppressed.

[0093] In addition, in the above coating method, the intermediate coating material 3 contains a thermoplastic polyurethane resin. Thermoplastic polyurethane resin has excellent impact absorption properties. Therefore, according to the above coating method, even if the intermediate coating film is relatively thin, it is possible to obtain a coated object 1 having excellent chipping resistance (impact absorption properties).

[0094] In the above coating method, the dry thickness of the base coating film is preferably equal to or less than a predetermined value. In such a case, the coating method reduces the amount of base paint applied, and can further suppress the intermixing of the intermediate coating film 3 and the base coating film 4.

[0095] In addition, in the above coating method, the clear paint is a two-component curing paint. In this case, the clear paint contains a clear base agent and a clear curing agent. Therefore, when the clear paint is applied to the base coating film, the clear curing agent penetrates the base coating film and promotes the curing of the base coating film 4. As a result, according to the above coating method, even if the amount of base paint applied is reduced, a base coating film 4 having excellent mechanical properties and smoothness is formed. [Explanation of symbols]

[0096] 1 Object to be coated 2 Electrodeposition coating 3. Intermediate coating 4 Base Coating 5 Clear coating

Claims

[Claim 1] A middle coating process in which a middle coating paint is applied to the electrodeposition-coated object to form a middle coating film; a base coating step of coating a base paint on the substrate without preheating the substrate and forming a base coating film on the intermediate coating film; A preheating step of preheating the object to be coated that has been coated with the intermediate coat and the base coat; A clear coating process in which a clear coating is applied to the preheated object to form a clear coating film on the base coating film; a baking process for baking the object to be coated that has been coated with the intermediate coating, the base coating, and the clear coating; Equipped with In the intermediate coating process, The intermediate coating paint contains a thermoplastic polyurethane resin, The intermediate coating is applied by an air reduction coating method, A coating method in which the dry thickness of the intermediate coating film is 13 μm or less.

Citation Information

Patent Citations

  • Electrostatic atomization type coating device and coating method

    JP2017042749A