Method for producing porous granule
The freeze-vacuum drying of indigestible dextrin solutions produces porous granules with superior solubility and oil adsorption, addressing the limitations of existing methods by enhancing solubility and fluidity while maintaining flavor and structural integrity.
Patent Information
- Application Number
- JP2023062385
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-21
- Publication Date
- 2024-10-07
AI Technical Summary
Existing methods for producing porous granules for oil adsorption face limitations, particularly when using highly soluble materials, resulting in poor solubility and crushability, and require the use of emulsifiers that can impair the flavor of oil-soluble substances.
A method involving freeze-vacuum drying a 100% by weight aqueous solution containing 15-30% by weight of indigestible dextrin to produce non-spherical porous granules with excellent solubility and oil adsorption capabilities, allowing for the adsorption of oil-soluble substances without the need for emulsifiers.
The produced granules exhibit excellent solubility, oil adsorption ability, and fluidity, maintaining the flavor of oil-soluble substances while being resistant to crushing, with a high oil adsorption capacity and ease of manufacturing.
Smart Images

Figure 2024137562000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for producing porous granules and the porous granules obtained by said method, oil-adsorbent granules and a method for producing the same, and foods containing said oil-adsorbent granules. [Background technology]
[0002] Conventionally, as described in, for example, Patent Document 1, a method for producing porous granules for adsorbing oil, which contains at least 80% by weight of at least one selected from the group consisting of monosaccharides, disaccharides, salts, amino acids and amino acid salts, and 5% by weight or less of starch, and has a solubility of at most 100 g in 100 mL of water at 20° C., is mixed with water and dried under reduced pressure, has been known. This publication describes that porous granules cannot be obtained when a raw material with high solubility is used, and describes a method of using a powder with a solubility of at most 100 g in 100 mL of water at 20° C., mixing the powder with water without dissolving the powder in water, and drying under reduced pressure, but the obtained porous granules had an oil adsorption capacity of at most 33% by weight, based on 100% by weight of the entire oil adsorbent granules to which oil has been adsorbed. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Patent No. 5276199 Summary of the Invention [Problem to be solved by the invention]
[0004] The present invention provides a method for producing porous granules that have good solubility and are capable of adsorbing oil-soluble substances, but are not easily crushed, the porous granules obtained by the method, oil-adsorbing granules in which oil-soluble substances are adsorbed onto the granules, a method for producing the oil-adsorbing granules, and foods containing the oil-adsorbing granules. [Means for solving the problem]
[0005] The present inventors have discovered that excellent granules that are porous, have good solubility, and are capable of adsorbing oil-soluble substances can be produced by vacuum freeze-drying a 100% by weight aqueous solution in which 15 to 30% by weight of resistant dextrin is dissolved, which has led to the present invention.
[0006] That is, the present invention relates to the following aspects [1] to [8]. [1] A method for producing non-spherical porous granules, comprising vacuum freeze-drying 100% by weight of an aqueous solution in which 15 to 30% by weight of resistant dextrin is dissolved. [2] The method for producing porous granules described in [1], wherein the loose bulk density of the porous granules is 0.45 g / mL or less. [3] Non-spherical porous granules obtained by freeze-drying 100% by weight of an aqueous solution in which 15 to 30% by weight of resistant dextrin is dissolved. [4] The porous granules described in [3], wherein the loose bulk density of the porous granules is 0.45 g / mL or less. [5] An oil-absorbing granule having an oil-soluble substance adsorbed onto the porous granule described in [3] or [4]. [6] The oil adsorbent granule according to [5], characterized in that it contains up to 74% by weight of oil-soluble substances when the entire oil adsorbent granule is taken as 100% by weight. [7] A method for producing oil-adsorbing granules, comprising a step of adsorbing an oil-soluble substance onto the porous granules described in [3] or [4]. [8] A method for producing oil adsorbent granules according to [7], characterized in that the oil adsorbent granules contain up to 74% by weight of oil-soluble substances when the entire oil adsorbent granule is taken as 100% by weight. [9] A food containing the oil adsorbent granules described in [5] or [6]. Effect of the Invention
[0007] The method for producing the porous granules of the present invention is simple and does not involve any complicated steps. Furthermore, the granules obtained by the method have excellent solubility and oil adsorption capacity due to their porous structure, and have excellent flowability after adsorption of oil-soluble substances, and further have sufficient strength despite their porous structure. The oil adsorbent granules of the present invention do not require an emulsifier when adsorbing oil-soluble substances, so they retain the flavor of the oil-soluble substances themselves without compromising them, have high fluidity, are not easily crushed even when subjected to impact during distribution, and are less likely to leak oil, and have excellent solubility that allows them to dissolve quickly when added to water or hot water.In addition, in the manufacturing method, there is no restriction on the method or order of adding the oil-soluble substances and the granules, and they can be mixed by a general method to achieve a high oil adsorption amount. Furthermore, foods containing the oil-adsorbing granules have high fluidity, and have the excellent effect of allowing the foods to be produced easily. [Brief description of the drawings]
[0008] [Figure 1] The figures show porous granules produced by blending 25% resistant dextrin, and oil-adsorbing granules that have been adsorbed with 30% oil adsorption capacity. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] In the present invention, by vacuum freeze-drying a 100% aqueous solution in which 15 to 30% by weight of resistant dextrin is dissolved, it is possible to produce excellent granules that are porous, have good solubility, and are capable of adsorbing oil-soluble substances, and by having the granules adsorb oil-soluble substances, it is possible to produce oil-adsorbing granules.
[0010] The resistant dextrin used in the present invention is not particularly limited, and any commonly available commercially available product can be used. By using the resistant dextrin, the absorption of carbohydrates can be suppressed, and low-calorie granules can be prepared.
[0011] The ratio of the resistant dextrin to water used in the present invention may be 15 to 30% by weight, preferably 25% by weight or less, and more preferably less than 25% by weight, when the entire aqueous solution in which the resistant dextrin is dissolved is taken as 100% by weight.
[0012] In the present invention, the drying method is not particularly limited as long as it is conventional vacuum freeze-drying, and the drying method makes the resulting granules porous, has excellent solubility, and has excellent adsorption ability for oil-soluble substances, and further, can have sufficient strength despite its porous structure.
[0013] The porous granules of the present invention are non-spherical, and the particle size of the porous granules is not particularly limited, but is preferably at least 100 μm, more preferably at least 200 μm, even more preferably 300 μm to 2 cm, and particularly preferably 500 μm to 1 cm, and can be obtained by sieving. Furthermore, the method for producing the porous granules preferably includes a crushing step and a sieving step, and after freeze-vacuum drying, the dried product may be crushed and sieved, or may be frozen, crushed, and then dried. For sieving, a sieve according to JIS standard Z8801-1:2006 having an optimal mesh size for obtaining the above particle size can be used.
[0014] In the present invention, the granules are not particularly limited as long as they have a porous structure but are strong, can well adsorb oil-soluble substances, and are unlikely to leak even after adsorbing oil, but the loose bulk density of the granules is preferably 0.10 g / mL or more, and is preferably 0.50 g / mL or less, more preferably 0.45 g / mL or less, even more preferably 0.42 g / mL or less, particularly preferably 0.40 g / mL or less or less than 0.40 g / mL, and may be less than 0.30 g / mL. The granules were filled into a 100 ml stainless steel cup placed on a horizontal surface, and the granules were leveled off with a leveling plate after filling, and the measured weight was divided by 100 to obtain the value obtained as the loose bulk density (g / mL).
[0015] In the present invention, the porous granules are not particularly limited as long as they have strength, are not easily crushed, and are strong enough to prevent oil leakage after adsorption of an oil-soluble substance, but preferably the compressive stress of a test piece prepared to be 18 mm x 18 mm x 17 mm is 1.0 kgf or more, more preferably 1.2 kgf or more, and even more preferably 1.5 kgf or more. In the present invention, a push-pull scale FB-5 (manufactured by Imada Co., Ltd.) was used to apply pressure to the measurement object with a cylindrical plunger having a diameter of 12 mm, and the compressive stress (kgf) was measured to determine the strength.
[0016] The porous granules of the present invention can be used, for example, as oil adsorption granules, which are a base material for adsorbing oil. The oil-soluble substance to be adsorbed by the porous granules is not particularly limited as long as it does not dissolve the porous granules. For example, fats and oils may be liquid or solid at room temperature, or fat-soluble vitamins, oil-based flavors, and oil-based colorants. Examples of oils that are liquid at room temperature include sesame oil, salad oil, white bean oil, corn oil, soybean oil, rapeseed oil (canola oil), rice oil, rice bran oil, wheat germ oil, camellia oil, safflower oil, coconut oil (palm kernel oil), cottonseed oil, sunflower oil, perilla oil, linseed oil, olive oil, peanut oil, almond oil, avocado oil, hazelnut oil, walnut oil, grapeseed oil, mustard oil, lettuce oil, fish oil, whale oil, shark oil, and liver oil, while examples of fats that are solid at room temperature include cacao butter, peanut butter, palm oil, lard (pork fat), hemp (beef fat), chicken oil, rabbit fat, mutton fat, horse fat, schmaltz, and shortening. In addition, examples include butter or margarine, the moisture content of which is preferably adjusted to at most 4% by weight. In addition, the oil-soluble substance to be adsorbed by the granules may be any oil-soluble substance in the mixture as long as it does not dissolve the granules. The porous granules of the present invention have a high oil adsorption capacity, and can adsorb oils and fats that are liquid at room temperature, which have been difficult to retain up to now.
[0017] In the present invention, the porous granules and the oil-soluble substance are mixed to obtain oil-adsorbing granules with good flowability. There are no particular precautions to be taken during mixing. The method and order of adding the porous granules and the oil-soluble substance are not particularly limited. The oil-soluble substance may be added to the porous granules, or the porous granules may be added to the oil-soluble substance. However, it is more common to add the oil-soluble substance to the porous granules, and this makes it easier to obtain oil-adsorbing granules with good flowability. The mixing ratio of the porous granules and the oil-soluble substance is not particularly limited as long as the amount of the porous granules is sufficient to adsorb the oil-soluble substance. The oil-adsorbing granules as a whole can adsorb up to 74% by weight of the oil-soluble substance, preferably 73% by weight or less, more preferably 70% by weight or less, and the lower limit is not particularly limited, but is preferably 35% by weight or more, more preferably 40% by weight or more, and even more preferably 45% by weight or more. If the oil-soluble substance is solid, it is heated to a degree that the oil-soluble substance becomes liquid before or during mixing with the porous granules. Oil sorbent granules are granules in which the porous granules absorb, contain or retain oil.
[0018] The porous granules of the present invention can be used in various foods, and can be used to produce foods containing oil-adsorbing granules. For example, oil-adsorbing granules that have been previously adsorbed with an oil-soluble substance can be mixed with a food that does not dissolve the granules to produce a food containing oil-adsorbing granules with good fluidity. The food to be mixed is not particularly limited as long as the granules are not dissolved, but the water content is preferably at most 10% by weight, more preferably at most 7% by weight, and even more preferably at most 4% by weight. For example, solid (powder, granule, small piece, block, etc.) foods, seasonings, spices, sugar or sweeteners can be mixed with the oil-adsorbing granules to produce foods containing oil-adsorbing granules, and examples of such foods include seasonings containing oil-adsorbing granules, sugars containing oil-adsorbing granules, confectioneries containing oil-adsorbing granules, beverages containing oil-adsorbing granules, and health foods containing oil-adsorbing granules. Specifically, by mixing oil-absorbent granules that have absorbed fats and oils, which are usually included with instant ramen, with powdered soup to produce a dried ramen soup containing oil-absorbent granules, it is possible to produce a dried ramen soup that does not form lumps and has excellent fluidity, and hands do not get dirty when eating, making it easy to eat. Also, by producing furikake or fried rice seasoning with oil-absorbent granules that have absorbed sesame oil or the like and powdered seasoning, it is possible to easily enjoy the flavor of sesame oil, while by mixing oil-absorbent granules that have absorbed flavorings with sugar for coffee or tea to produce flavored sugar, it is possible to enjoy flavored coffee or flavored tea, and oil-absorbent granules containing fat-soluble vitamins can also be used as health foods. Furthermore, an oil-soluble substance-containing material that does not dissolve the granules can be mixed with the porous granules of the present invention to produce an oil-adsorbing granule-containing food with good flowability. The oil-soluble substance-containing material to be mixed is not particularly limited as long as it does not dissolve the granules, but the water content in the material is preferably at most 10% by weight, more preferably at most 7% by weight, and even more preferably at most 4% by weight. The oil-soluble substance-containing material is not limited in shape as long as it is based on an oil-soluble substance, and is a solid, paste-like or liquid food, such as chocolate, sesame paste, nut paste, roux, mayonnaise with the water content adjusted to the above-mentioned amount, and may also be a food with high viscosity. When the oil-soluble substance-containing material is mixed with the porous granules of the present invention, the oil-soluble substance in the material is adsorbed to the granules, and oil-adsorbing granule-containing confectionery or beverage such as granular chocolate, oil-adsorbing granule-containing seasoning, oil-adsorbing granule-containing topping, and other oil-adsorbing granule-containing foods with good flowability can be produced. If the oil-soluble substance-containing material contains solid oil at room temperature, heat the material to a liquid state before or during mixing with the porous granules.The mixing ratio of the oil-soluble substance-containing material and the porous granules is not particularly limited as long as the oil-soluble substance in the material is adsorbed by the porous granules and a food with flowability is obtained, but when the weight of the porous granules in the material is 1, the oil-soluble substance is preferably less than 3.0, more preferably 2.9 or less, even more preferably 2.8 or less, and preferably 0.4 or more, more preferably 0.5 or more, even more preferably 0.6 or more, and the oil-soluble substance-adsorbed granules with flowability can be obtained. EXAMPLES
[0019] The present invention will be described in detail below with reference to examples, but the present invention is not limited to the following examples. In the present invention, the percentages of each raw material and ingredient are all by weight unless otherwise specified. EXAMPLES
[0020] Resistant dextrin (Fibersol (registered trademark) 2, Matsutani Chemical Industry Co., Ltd.) and water were mixed in the ratio shown in Table 1, and after the resistant dextrin was completely dissolved in the water, the mixture was placed in a tray and subjected to vacuum freeze-drying in a conventional manner. The dried state and strength of the granules were evaluated as follows.
[0021] Regarding the drying condition, the state immediately after drying was evaluated, and those that were cubic in shape were marked with an O, and those that had not foamed into a cubic shape were marked with an X. Regarding strength, the particles were crushed after drying and sieved through an 8 mesh (a sieve with nominal opening of 2.36 mm) sieve and passed through a 42 mesh (a sieve with nominal opening of 355 μm). Of the porous granules obtained, those that did not break when pressed lightly with a finger were marked with an O, and those that were easily broken were marked with an X, and the results are shown in Table 1.
[0022] [Table 1]
[0023] As shown in Table 1, a blend ratio of 10% resistant dextrin and 90% water did not provide sufficient granule strength, and a blend ratio of 40% resistant dextrin and 60% water did not provide a cube-shaped dried product, whereas a freeze-vacuum drying of an aqueous solution containing 15-30% resistant dextrin did not cause any problems with the drying state and provided granules with even greater strength. It is believed that when the blend ratio of resistant dextrin was 40% or more, the solid content in the solution was too high, which led to poor freezing and foaming during drying, preventing the formation of a cube-shaped dried product.
[0024] An aqueous solution containing 15-30% resistant dextrin was freeze-dried in a vacuum, pulverized, and sieved to obtain porous granules. The loose bulk density of each compound was measured, and the results were 0.13 g / mL for the 15% resistant dextrin compound, 0.24 g / mL for the 20% resistant dextrin compound, 0.32 g / mL for the 25% resistant dextrin compound, and 0.41 g / mL for the 30% resistant dextrin compound. EXAMPLES
[0025] In the freeze-drying process, the volume shrinks due to drying. Assuming that the volume after drying is 50% (v / v), 55% (v / v), or 60% (v / v) of the volume before drying (frozen material), the dried portion of the resistant dextrin is used as the "base material," and the calculated oil adsorption amount that can be held by each granule is calculated. The calculated amount of oil is impregnated into each granule to form an oil-adsorbed granule, and the fluidity is evaluated. The porous granules obtained by freeze-drying and pulverizing an aqueous solution containing 15 to 30% resistant dextrin, and sieving in the same manner as above were also subjected to the same test. The oil adsorption amount for granule 1 and the ratio of the granules to the oil adsorption amount when the oil-adsorbed granule is taken as 100% were also calculated and are shown in Table 2. Figure 1 shows photographs of porous granules produced by mixing 25% resistant dextrin (75% water) and oil-absorbing granules with fluidity that had absorbed 30% of the oil.
[0026] To evaluate fluidity, oil with a melting point of 20°C or less was mixed in. Those with poor fluidity due to the oil clinging to the surface were rated as ×, those that had absorbed all the oil but were at the limit of where they could maintain their fluidity were rated as △, and those that were smooth and had good fluidity were rated as ○.
[0027] [Table 2]
[0028] As shown in Table 2, when the volume after drying was assumed to be 60% (v / v), the fluidity after oil adsorption was poor, but when it was assumed to be 55% (v / v) or 50% (v / v), the fluidity was maintained even after oil adsorption, and it was found that, assuming the entire oil-adsorbed granule to be 100%, the fluidity can be maintained even when a maximum of 73% of oil is adsorbed. In other words, when an aqueous solution containing 15-30% resistant dextrin is freeze-dried in vacuum, it shrinks to about 55% or less of the volume before drying, and it is thought that porous granules with about 20-40% voids throughout the granules are formed.
[0029] Furthermore, when resistant dextrin (Fibersol (registered trademark) 2, DE10-12) powder itself was mixed with liquid oil in a ratio of 1 part resistant dextrin to 0.5 or 0.2 parts liquid oil, no fluidity was observed. EXAMPLES
[0030] Resistant dextrin (Fibersol (registered trademark) 2, DE10-12), DE10-12 dextrin (Pinedex (registered trademark) #2), or DE2-5 dextrin (Pinedex (registered trademark) #100) was mixed with water at a ratio of 15, 20, or 30% in the proportions shown in Table 1. After each dextrin was completely dissolved in the water, the mixture was placed in a tray and subjected to vacuum freeze-drying in a conventional manner. The oil absorbency of the resulting cubic porous granules measuring 18 mm x 18 mm x 17 mm was evaluated.
[0031] The oil absorption was evaluated by placing each porous granule in a petri dish containing liquid oil at 0 min, observing the oil absorption by the porous granule for 60 min, and measuring the time it took for the oil to soak into the entire granule. The amount of oil in the petri dish was set to the extent that it was in contact with the bottom of the granule.
[0032] The time it took for oil to soak into the entire porous granules was 10 minutes for granules using resistant dextrin, 15 minutes for 15%, 17 minutes for 20%, and 55 minutes for 30% for granules using dextrin with DE10 to 12, and none of the granules using dextrin with DE2 to 5 had oil soak into the entire granules after 60 minutes. From the above, it was found that by using resistant dextrin, porous granules with excellent oil absorption properties that can quickly adsorb oil can be obtained. EXAMPLES
[0033] Resistant dextrin (Fibersol (registered trademark) 2) was mixed with water at a ratio of 15, 20 or 30% in the proportions shown in Table 1, and after being completely dissolved in water, it was placed in a tray and subjected to vacuum freeze-drying in a conventional manner. The hardness of the resulting cubic porous granules measuring 18 mm x 18 mm x 17 mm was evaluated.
[0034] The hardness was evaluated by applying pressure to the porous granules made from indigestible dextrin using a push-pull scale FB-5 (manufactured by Imada Co., Ltd.) with a cylindrical plunger having a diameter of 12 mm, and measuring the compressive stress (kgf). The results are shown in Table 3.
[0035] [Table 3]
[0036] The strength of the porous granules produced with each amount of resistant dextrin was 1.8 kgf or more. Generally, a strength of 1 kgf or more per 12 mm diameter is not a problem, so it was found that there was no problem with strength regardless of the amount of resistant dextrin used.
Claims
1. A method for producing non-spherical porous granules, comprising the steps of: freeze-drying 100% by weight of an aqueous solution in which 15 to 30% by weight of indigestible dextrin is dissolved in the aqueous solution in a vacuum.
2. The method for producing porous granules according to claim 1, wherein the loose bulk density of the porous granules is 0.45 g / mL or less.
3. The non-spherical porous granules are obtained by freeze-drying 100% by weight of an aqueous solution in which 15 to 30% by weight of indigestible dextrin is dissolved in vacuum.
4. 4. The porous granule according to claim 3, wherein the loose bulk density of the porous granule is 0.45 g / mL or less.
5. 5. An oil-adsorbing granule comprising the porous granule according to claim 3 or 4 having an oil-soluble substance adsorbed thereon.
6. 6. The oil adsorbent granule according to claim 5, which contains an oil-soluble substance in an amount of up to 74% by weight, when the total weight of the oil adsorbent granule is taken as 100% by weight.
7. A method for producing oil-adsorbent granules, comprising a step of adsorbing an oil-soluble substance onto the porous granules according to claim 3 or 4.
8. 8. The method for producing oil adsorbent granules according to claim 7, characterized in that the oil-soluble substance is contained in an amount of up to 74% by weight when the total weight of the oil adsorbent granules is taken as 100% by weight.
9. A food product comprising the oil-adsorbing granules according to claim 5.
Citation Information
Patent Citations
Apparatus for packing biscuits into container