Method for testing battery cell stack related to position of battery cell layer

The method uses optical cameras and X-ray irradiation to ensure precise alignment of battery cell layers, addressing lamination accuracy issues and minimizing material waste in battery production.

JP2024137848AActive Publication Date: 2024-10-07パワーコエスエー
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2024043395
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-21
Filing Date
2024-03-19
Publication Date
2024-10-07
Estimated Expiration
2044-03-19

AI Technical Summary

Technical Problem

Existing laminating machines for battery cell layers face challenges in achieving precise lamination accuracy, leading to potential short circuits and increased material consumption due to oversizing to avoid these issues, which affects the electrochemical performance and weight of the battery.

Method used

A method involving optical camera systems for geometry calculation and X-ray irradiation to determine the positioning and spacing of battery cell layers, combined with multiple inspection steps to ensure accurate alignment and prevent short circuits, while minimizing material waste.

Benefits of technology

This method allows for rapid and precise inspection of battery cell layer stacks, ensuring reliable production of batteries without short circuits and reducing material consumption, thus optimizing performance and weight.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024137848000001_ABST
    Figure 2024137848000001_ABST
Patent Text Reader

Abstract

To provide a testing method for a battery cell layer laminate.SOLUTION: A testing method for a battery cell layer laminate includes: obtaining a geometrical shape of at least one large area part of a large area part of at least an anode 2a and / or a cathode 2b; laminating battery cell layers on a laminate 1; irradiating the laminate with X-ray for location testing of the anode and / or the cathode to obtain a maximum inter-edge distance present between edges of an electrode of a type considered with respect to at least one pair of opposing side surfaces of the laminate by using detected X-ray; testing whether or not the distance is smaller than a first permissible error value; defining as an overhang amount a half of a value for which the distance is smaller than a first permissible error value when a result is positive; obtaining the distance from a sum of shortest dimensions related to all calculation directions of the electrode of the type considered on the one hand, and on the other hand, testing whether or not it is smaller than value obtained from difference between a second permissible error value and a half of the overhung amount; and evaluating that the laminate is permissible when the result is positive.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for inspecting a stack of multiple battery cell layers in the form of an anode, a cathode, and a separator, sometimes referred to as an electrode separator composite (ESV), which may be provided as a component part of a battery.

[0002] In the automated manufacture of batteries, the battery cell layers are laminated into a stack using a lamination machine (see US 2022 / 0216501 A1), where the lamination accuracy of the battery cell layers, in particular of the electrodes, is a quality criterion for the throughput of the lamination machine. All edges of polygonal, in particular rectangular, battery cell layers must have a defined spacing distance from one another and within a defined tolerance range, on the one hand to ensure the best possible electrochemical performance of the battery and on the other hand to avoid short circuits between adjacent electrodes due to insufficient lamination accuracy. Such short circuits can lead to failure of the battery in question.

[0003] Taking into account the lamination accuracy of the currently used lamination machines, in order to reliably avoid short circuits between adjacent electrodes due to insufficient lamination accuracy, it may be envisaged that the separator of the stack is dimensioned larger than the anode, and the anode is also dimensioned larger than the cathode, so that an overhang of, for example, 1 millimeter occurs over the entire circumference between the separator and the anode on the one hand, and between the anode and the cathode on the other hand. Such an overhang also makes it possible to avoid a deterioration of the chemical performance of the stack due to inaccurate positioning of the electrodes. However, oversizing of the anode and the separator due to such tolerances increases the material consumption in the production of the stack, thus increasing the cost, space required and weight of the stack and thus the weight of the battery. It may therefore be worthwhile to minimize the oversizing of the battery cell layers in the stack due to such tolerances. To this end, in order to avoid short circuits between adjacent electrodes due to insufficient lamination accuracy, the lamination accuracy of the lamination machine used for the lamination should be increased and / or the quality assurance should be improved within the framework of the production of the stack, so that the production of short-circuited stacks can be sufficiently reliably avoided or reliably selected within the framework of production.

[0004] WO 2016 / 114257 discloses a method for inspecting ESVs using X-rays.

[0005] The problem on which the invention is based is to provide a method for determining the stacking accuracy of battery cell layers of a battery cell stack, which can be carried out as simply and / or quickly as possible with sufficient accuracy.

[0006] This problem is solved in a method according to claim 1. Preferred embodiments of the method according to the invention are the subject of further claims and will become apparent from the following description of the invention.

[0007] According to the invention, a method is provided for testing at least one stack of a plurality of battery cell layers in the form of an anode as a first type of electrode, a cathode as a second type of electrode, and a separator (separating and electrically insulating the anode and the cathode), where the battery cell layers have polygonal, preferably rectangular, large area portions. The large area portions of the battery cell layers can have at least partially different sizes. The battery cell layers are stacked with a stacking direction aligned perpendicular to the large area portions. The electrodes of the battery cells can differ at least with respect to the active material contained, whereby the electrode designated as the anode is anodically active and the electrode designated as the cathode is cathodically active (respectively with respect to the discharge of the battery cell).

[0008] The battery cell layer may preferably be designed plate-like. As "plate-like" here is understood a body or body section having two (outer) large surface areas extending in the longitudinal and transverse directions of the body (for example in the case of a meandering course of a strip-shaped separator, the section lying between adjacent electrodes here represents a plate-shaped separator), in which the (maximum) height of the body, corresponding to the (maximum) spacing distance of the large surface areas, is smaller (in particular by a factor of at most 1 / 10 or 1 / 100 or 1 / 100) than the (maximum) length and the (maximum) width.

[0009] In a first calculation step of the method, the geometry (i.e. the geometric data, in particular with regard to shape and dimensions) of at least one of the major surface areas of at least (all) anodes and / or (all) cathodes, possibly additionally of the separator, is determined, preferably in the individualized state of the battery cell layers.

[0010] The calculation of the geometry of at least the anode and / or cathode can preferably be performed on the basis of images of an optical camera system, i.e. by an image generating system based on visible light, including one or more cameras. This allows for a simple and cost-effective implementation of the first calculation step. Here, the image capture of the camera of the camera system can preferably be recorded in a top view, i.e. with a "line of sight" to large areas of the battery cell layer, particularly preferably with a vertical alignment of the optical axis of the camera of the camera system with respect to these large areas. This can likewise be advantageously applied for the implementation of the first calculation step, since it allows the capture of the largest possible area of ​​the battery cell.

[0011] In the stacking step, the battery cell layers are stacked in the stack. Here, it may be preferably envisaged that the battery cell layers are stacked in the stack in a defined order and / or the order in which this is done is determined and stored. These first calculation step and stacking step can preferably be carried out at least partly simultaneously, for example by determining the geometry of the upper large area portion from the battery cell layer placed on the formed stack or further from the battery cell layer to be placed next. However, it may be envisaged that the stacking step is only carried out in connection with the first calculation step.

[0012] Subsequently, a number of method steps are carried out for a position check at least of the anode and / or the cathode, insofar as these have been geometrically determined in the first calculation step, whereby, if a position check is carried out for the anode and the cathode, these method steps are carried out separately (but preferably at least temporarily simultaneously) for the anode on the one hand and the cathode on the other hand, respectively.

[0013] In the second calculation step, the stack is first irradiated with X-rays, which are irradiated by an X-ray irradiator and detected by an X-ray detector, where the X-rays (i.e. at least one beam, in particular the central beam) are aligned vertically with respect to a large area of ​​the battery cell layer. Here, a relative movement between the stack and the X-rays is preferably caused by moving the stack while the X-ray irradiator and the X-ray detector are stationary. This relative movement may preferably be linear. The detected X-rays are then used to determine for at least one pair of opposing side surfaces of the stack the maximum edge separation distance that exists between the edges of this pair. Here, the separation distance is determined according to the invention essentially along the most direct or shortest possible path.

[0014] In a first inspection step, it is then checked whether this maximum edge spacing is smaller than a first tolerance value. If not, i.e. if the maximum edge spacing is not smaller than the first tolerance value and is therefore equal to or greater than the first tolerance value, the stack is evaluated as unacceptable. On the other hand, if it is positive, i.e. if the maximum edge spacing is smaller than the first tolerance value, a second inspection step is further performed.

[0015] In this second test step, it is checked whether the determined maximum edge spacing is smaller than a value resulting from the sum of the shortest (geometric) dimensions of all the individual electrodes (anodes or cathodes) in the calculation direction (direction of connection between the pairs of opposite side surfaces of the stack) on the one hand and the difference between a second tolerance value and half the overhang on the other hand. As overhang, half the value by which the maximum edge spacing is smaller than the first tolerance value is defined here. If this second test step leads to a negative test result, i.e. if the maximum edge spacing is not small and is therefore equal to or greater than the value resulting from the sum of the shortest dimensions of all the individual electrodes on the one hand and the difference between the second tolerance value and half the overhang on the other hand, the stack is evaluated as unacceptable. On the other hand, if the second test step produces a positive test result, i.e. the maximum edge separation distance is smaller than the value resulting from the sum of the shortest extensions of all the respective electrodes on the one hand and the difference between the second tolerance value and the half overhang on the other hand, the stack is evaluated as acceptable. It may be envisaged that a stack evaluated as acceptable may be used without restriction for the manufacture of batteries.

[0016] The method according to the invention aims at preferably combining the geometrical data from the first calculation step with the calculation results from the second calculation step, whereby the specific evaluation by the multiple inspection steps makes it possible to check the position of all the anodes and / or cathodes. This is possible despite the relatively easily maintained type of (vertical) irradiation of the stack with X-rays during the second calculation step. This type of irradiation may lead in particular to the inability to accurately determine the edges of all these respective electrodes by the evaluation of the X-rays measured by the X-ray detector. Rather, even though only the spacing distance between the mutually most widely spaced edges of the respective electrodes forming the selected side pair of the stack is determined, the combination with all the geometrical data of the respective electrodes (anodes and / or cathodes) and the specific evaluation according to the multiple inspection steps ensures with a relatively high degree of accuracy that all the electrodes considered have a sufficient positional accuracy. This allows a relatively quick inspection of the stack, since the possible vertical irradiation allows the X-rays to move through the stack in a quick and easy manner.

[0017] According to a preferred embodiment of the method according to the invention, it may be assumed that in the first calculation step the course of the edges or edge sections forming all corners of each electrode, i.e. anode or cathode, is determined. This would result in the complete geometry of a large area of ​​each of these electrodes. This makes it possible to achieve sufficiently accurate test results for the entire stack, even if the first calculation step is carried out only for some battery cell layers, for example exclusively for the cathodes and / or anodes. In principle, however, it may be sufficient to determine the course of the edges or edge sections forming only some corners of each electrode in the first calculation step.

[0018] In order to achieve the most reliable possible inspection results for the stack, it may be envisaged that the second calculation step and the subsequent inspection step are preferably carried out for at least two or exactly two pairs of opposite sides of the stack. Thus, in connection with the preferred design of the battery cell layers with a rectangular large area, a calculation and inspection is carried out for each combination of edges that defines, on the one hand, the maximum distance for the length of each electrode, and, on the other hand, the maximum distance for the width of each electrode. This allows a particularly precise inspection of the mutual position of the battery cell layers to be carried out, which can nevertheless be realized with only two simple linear relative movements between the stack and the X-ray. The second calculation step and the carrying out of the first and second inspection steps can be carried out in succession for at least two or exactly two pairs, so that the stack is, for example, first moved relative to the X-ray along the longitudinal direction of the stack and then, after a rotation of, for example, 90° around the stacking direction, moved relative to the X-ray along the width direction. However, simultaneous capture of two pairs of edges can be carried out as well.

[0019] According to a preferred embodiment of the method according to the invention, it may be envisaged that only one type of electrode, in particular only the cathode, is inspected according to the second calculation step and the first and second inspection steps. This may be due to the fact that for this type of electrode based on a specifically structured structure, the position of all edges cannot be determined exactly or unambiguously on the basis of an image that can be determined by evaluation of the X-rays detected by the X-ray detector, which may be due to the relatively significant absorption properties for X-rays.

[0020] In contrast, for the relative position of other types of electrodes, in particular anodes, a simpler and / or more accurate type of evaluation may be envisaged. For this purpose, in a further calculation and inspection step of the method according to the invention, which may possibly be carried out as part of the second calculation step or simultaneously with the second calculation step, the stack is irradiated with X-rays irradiated by an X-ray irradiator and detected by an X-ray detector, where the X-rays are aligned vertically with respect to a large area portion of the battery cell layer, where the X-rays detected with respect to at least one side of the stack are used to determine the maximum edge spacing distance existing between the edges of all electrodes of this type assigned to this side of the stack, and on the basis of which it is checked whether this edge spacing distance is smaller than the third tolerance value. Here, if a negative result occurs, i.e. if the maximum edge spacing distance is not smaller but rather equal to or greater than the third tolerance value, the stack is evaluated as unacceptable or rejected. A stack evaluated as rejected can in particular be considered as definitively unsuitable for further use in the manufacture of batteries. In the case of a positive result, on the other hand, the stack is evaluated as acceptable. Preferably, in order to achieve the most accurate inspection results possible, further calculation and inspection steps are performed on all sides of the stack, but at least on the sides of the stack that define at least two of the edges of the stack extending in the stack direction.

[0021] The procedure according to the second calculation step and the first and second inspection steps is based on a simplification of the calculation results. This simplification is based on the fact that for the evaluation, it is always assumed that the smallest of all respective electrodes in terms of the dimension between the edges of a pair represents one of the edges that determines the maximum edge-to-edge distance of this pair. The smallest electrode is here determined within the framework of the first calculation step. This may result in an evaluation of the stack as unacceptable, which is not given in reality, since the smallest of the electrodes does not necessarily represent one of the edges that defines the maximum edge-to-edge distance. The simplification is therefore selected in such a way that a certain degree of inaccuracy is only present with respect to the evaluation of the stack as unacceptable.

[0022] It may therefore be expedient to newly inspect the stack assessed as unacceptable, in particular in the second calculation step and in the first and second inspection steps, possibly also in further calculation and inspection steps. For this purpose, it may be expedient to provide that, if the stack is assessed as unacceptable, in a third inspection step the stack is additionally inspected with respect to the maintenance of at least one tolerance range, where in the negative case the stack is assessed as rejected and in the positive case the stack is assessed as acceptable.

[0023] In a third inspection step, the stack may be preferably irradiated with X-rays irradiated by an X-ray irradiator and detected by an X-ray detector, where the orientation of the stack relative to the X-rays is selected such that at least one edge of the stack extending along the stacking direction is completely captured in at least two different positions in the space covered by the X-rays, on the basis of which the relative positions of the corners of the battery cell layers forming said edge of the stack (or the edge sections defining these corners) are determined. This procedure may be similar or correspond to a procedure in conventional computed tomography.

[0024] According to a preferred embodiment of the method according to the invention, it may be provided that during or after the stacking of the battery cell layers in the context of the stacking step, the battery cell layers are inspected for the presence of buckles, since such buckles may falsify the results of the stack inspection. By buckles is meant here an angled course of a large area of ​​the battery cell layer, in particular an angled course of at least 45° or at least 90°. Here, the angle of this course may also be approximately 0° / 360°, so that two sections of this battery cell layer run approximately parallel. Such a buckle inspection may also be carried out simultaneously with the first calculation step, in particular it may be integrated into the first calculation step by using the same device, in particular an optical camera system.

[0025] Buckle inspection may suitably be performed by determining and evaluating the geometry of the battery cell layers and / or by determining and evaluating the geometry of the stack.

[0026] Within the scope of the buckle inspection, the determination of the geometry of the battery cell layers and / or the determination of the geometry of the stack can likewise preferably be carried out using an optical camera system. Here, the images of the camera system can preferably be recorded in a top view with respect to a large area of ​​the battery cell layers. Such an arrangement of the camera system with respect to the battery cell layers can be envisaged in particular when the geometry of the individual battery cell layers is determined after or during, respectively, placement on the stack to be formed. Alternatively, it can be envisaged that, in order to determine the geometry of the battery cell layers in the formed stack, the images of the camera system are recorded in a side view with respect to the stack.

[0027] Determining the geometry of the stack may in particular involve determining the height of the stack along the stacking direction, i.e. the extension of the stack, at multiple points, which may also be done mechanically in a relatively simple and cost-effective manner.

[0028] The battery cells used within the scope of the method according to the invention can preferably be designed such that the large area of ​​the anode is larger than the large area of ​​the cathode and / or the large area of ​​the separator is larger than the large area of ​​the cathode and preferably also larger than the large area of ​​the anode. The design of the different sizes of the large areas of the different battery cell layers should achieve a total overhang of each of the relatively large battery cell layers (separator and anode) compared to the next smaller battery cell layer, respectively. This makes it possible in particular to carry out the second calculation step and possibly further calculation and inspection steps in a favorable manner. This can be due to different absorption rates of the different battery cell layers for X-rays. These different absorption rates can be due to differences in the materials from which the different battery cell layers are designed. Here, the cathode can have the highest absorption rate and the separator the lowest.

[0029] In the following, the invention is explained in more detail on the basis of designs and examples shown in the drawings, which are each shown in a schematic diagram. [Brief description of the drawings]

[0030] [Figure 1] FIG. 2 is a cross-sectional view of a section of a stack of battery cell layers in the form of an anode, cathode, and separator. [Diagram 2] FIG. 1 shows stacking areas for the cathode, anode and separator of the stack. [Diagram 3] FIG. 2 shows an individualized battery cell layer of a stack according to a first variant and a camera system for use in the first calculation step of the method according to the invention. [Figure 4] FIG. 2 shows an individualized battery cell layer of a stack according to a second variant and a camera system for use in the first calculation step of the method according to the invention. [Diagram 5] FIG. 2 shows a stack and a camera system according to a first variant for use in the buckle inspection of the method according to the invention. [Figure 6] FIG. 2 shows a stack and a camera system according to a second variant for use in the buckle inspection of the method according to the invention. [Figure 7] FIG. 2 is a side view of a laminate and a mechanical measurement system for use in buckle inspection of the method according to the invention. [Figure 8] FIG. 8 is a top view of the stack and the measurement system according to FIG. [Figure 9] FIG. 2 shows a stack and an X-ray system for use in the second calculation step of the method according to the invention. [Figure 10] FIG. 2 illustrates one position of the stack relative to an X-ray detector of an X-ray system. [Figure 11] FIG. 2 illustrates one position of the stack relative to an X-ray detector of an X-ray system. [Figure 12] FIG. 2 illustrates one position of the stack relative to an X-ray detector of an X-ray system. [Figure 13] FIG. 2 illustrates one position of the stack relative to an X-ray detector of an X-ray system. [Figure 14] FIG. 2 illustrates one position of the stack relative to an X-ray detector of an X-ray system. [Figure 15] FIG. 2 is a diagram showing dimensions of the stack relative to the cathode. [Figure 16] FIG. 2 shows a stack and an X-ray system for use in the third inspection step of the method according to the invention. [Figure 17] FIG. 17 shows an image of a section of a laminate made with the X-ray system according to FIG. 16.

[0031] Within the framework of battery cell production, a stack 1 can be produced which comprises battery cell layers in the form of plate-like electrodes 2 and electrically insulating plate-like separators 3 in alternating sequence along a stacking direction 4. These electrodes 2 are again arranged in the stack 1 in a design and arrangement corresponding to their use as anodes 2a and cathodes 2b, alternatingly. The electrodes 2 and the separators 3 have rectangular large areas, where the anodes 2a, cathodes 2b and large areas of the separators 3 are of different sizes in order to avoid short circuits between adjacent anodes 2a and cathodes 2b and excessive losses in terms of the electrical performance of the battery to be produced, despite imprecision in the stacking which is at least still within the corresponding tolerance range. According to FIG. 1, it may be assumed that the cathode 2b has the smallest large area and the separator 3 has the largest large area, which results in an overhang of the anode 2a with respect to the cathode 2b on the one hand and an overhang of the separator 3 with respect to the anode 2a (and thus also to the cathode 2b) on the other hand on the edge side over the entire extent (i.e. both with respect to the width and the length of the battery cell layer).

[0032] The plate-like separators 3 may at least partially be sections of a serpentine-guided separator strip (not shown). The overhanging edge regions of adjacent separators 3 may be glued together.

[0033] 2 shows possible configuration specifications for sufficiently accurate stacking of the battery cell layers for one of all four edges of the stack 1 extending along the stacking direction 4, where these configuration specifications should be met for all of these edges. Thus, for all of the anode 2a, cathode 2b, and separator 3, there is one respective stacking area A within which the edges of these different types of battery cell layers should reside. A ,A K ,A S In addition, for each of the various types of battery cell layers, the optimum position S A ,S K ,SS are shown, and in this case, the optimal positions S A ,S K ,S S are the lamination areas A A ,A K ,A S These lamination areas A extend to the center of the interior. A ,A K ,A S For example, the width of each optimal position S A ,S K ,S S The difference between the stacking area A and the stacking area B for the different types of battery cell layers of all the battery cells of the stack 1 can be 1.0 mm or ±0.5 mm on either side of the stacking area A. A ,A K ,A S In addition to the above, various lamination regions A are also included as setting specifications for sufficiently accurate lamination. A ,A K ,A S The minimum spacing distance d between AK ,d AS The anode 2a stacking region A may be provided. A and cathode 2b for stacking area A K The minimum spacing distance d between AK , and the lamination region A for the anode 2a A and separator 3 for lamination area A S The minimum spacing distance d between AS can be, for example, 0.8 mm each. This results in the minimum spacing distance d AK ,d AS , and the anode 2a stacked tube region A A Through the linking portion including the width of the cathode 2b stacking region A K and separator 3 for lamination area A S There is also a minimum spacing distance between

[0034] The method according to the invention allows, by a combination of several calculation and testing steps, a simple and rapid as possible test of the stack 1 with regard to a sufficiently accurate position of at least the electrodes 2 of the stack 1 .

[0035] In a first calculation step of the method, the geometry of each one of the large area portions of all battery cell layers is determined. This is done using an optical camera system in top view (see Figs. 3 and 4), with the help of which at least one image of each of the individualized battery cell layers is recorded and evaluated. Here, a first light source (not shown) can preferably be arranged on the same side of the individualized battery cell layer as the at least one camera 5 of the camera system, and a second light source (not shown) can be arranged on the opposite side of the individualized battery cell layer.

[0036] If the capture area 5a of the at least one camera 5 used is sufficiently large, the individualized battery cell layer can be completely captured without any relative movement with respect to this camera 5. However, in order to achieve a relatively high resolution, it may also be envisaged to move the individualized battery cell layer and the at least one camera 5 relative to one another, in which case only a section of the battery cell layer is captured by the at least one camera 5 in each case. A relatively high resolution without relative movement can be achieved when using several cameras 5, which may furthermore each have a capture area 5a smaller than the large surface area of ​​the battery cell layer. Figure 4 shows an example in this respect, in which a camera 5 is respectively assigned to each of the four corners of the individualized battery cell layer.

[0037] Preferably, simultaneously with or after determining the geometry of the individualized battery cell layers in the first calculation step, the battery cell layers are stacked in the stack 1 in a defined number, and optionally in a later ordered order, in a stacking step of the method.

[0038] During or after the stacking of the battery cell layers, these battery cell layers are also inspected for the presence of buckles. This can likewise be done using a camera system. This can preferably be the same camera system as that used in the first calculation step. However, it can also be a different camera system. Different camera systems can be used advantageously, for example, in the context of a series of inspections of multiple stacks, which simultaneously undergo different calculation and inspection steps that are carried out sequentially on the individual stacks.

[0039] Figures 5 to 8 show various means for carrying out the buckle inspection. For the buckle inspection according to figures 5 and 6 respectively one camera system is used.

[0040] In the camera system according to Fig. 5, the camera 5 is positioned in a top view of the large area of ​​the battery cell layer for recording an image. This allows the camera to determine the geometry of the large area of ​​the battery cell layer of the (formed) stack 1, comparable to the procedure according to the first calculation step, and to check for the presence of buckles (not shown). This can preferably be performed with the geometric data for each battery cell layer previously determined in the first calculation step. However, this is not necessarily necessary, since buckles of the battery cell layer usually lead to geometric deviations of such magnitude that a buckle check may be sufficient based on a comparison of the geometry determined then with a reference geometry defined for all battery cell layer types. Since the geometry of all battery cell layers of the stack 1 cannot be completely captured when recording images in a top view, it is envisaged that the buckling inspection is carried out sequentially on the individual battery cell layers during stacking using a camera system according to FIG. 5, i.e. for each battery cell layer that is placed on the stack 1 formed during stacking, respectively, at least one image is captured using camera 5 before a further battery cell layer is placed on the stack 1.

[0041] In contrast, in the camera system according to FIG. 6, the camera 5 is arranged to record images in a side view with respect to the stack 1. This allows the course of all battery cell layers to be determined simultaneously in the corresponding side view and the presence of buckles (not shown) can be checked. For a buckle check as complete as possible, images of at least two opposite sides of the stack 1 should be created and evaluated here, for which the camera system can comprise at least two cameras 5 (not shown). Alternatively, however, a relative rotation between the stack 1 and the camera system can also be provided in such a way that several sides of the stack are captured by the images of the individual cameras 5 one after the other. With the camera system according to FIG. 6, all battery cell layers can be checked simultaneously for the presence of buckles, so that the corresponding buckle check can preferably be carried out on an already fully formed stack 1.

[0042] The buckle inspection according to Figures 7 and 8 is based on determining the respective height of the stack 1 at a number of measurement points. This can be done mechanically, for example, by means of a measuring probe 6. Here, preferably at least one measurement point is assigned to each edge of the stack 1 running along the stacking direction 4 or is arranged close to said edges, since in particular the corners of the battery cell layers forming these edges are exposed to the risk of buckling during stacking.

[0043] Following the lamination step with buckle inspection, a second calculation step is performed, in which the stack 1 is irradiated with X-rays 9 irradiated by an X-ray irradiator 7 and detected by an X-ray detector 8 (see FIG. 9 ). Here, it is assumed that the X-rays 9 are aligned vertically with respect to a large area of ​​the battery cell layers, the vertical alignment being associated with a central beam 9a of the X-rays 9 propagating from the X-ray irradiator 7 in a tapered or conical manner.

[0044] By evaluation of the X-rays detected by means of the X-ray detector 8, the positions of at least the edges of the anode 2a and the cathode 2b, if possible, are determined.

[0045] Since the anode 2a is on the one hand larger than the cathode 2b and on the other hand only moderately absorbs X-rays, it is possible to determine the position of all edges of the anode 2a from the X-rays captured by the X-ray detector 8, since for these edges there is sufficient contrast in the corresponding image. The very slight absorption of X-rays by the separator 3, which has a large surface area even larger than that of the anode 2a, does not significantly impair this evaluation.

[0046] For the position check of the anodes 2a, the determined positions of the edges of the anodes 2a by the further calculation and check steps of the method are calculated to determine the maximum distance d between the edges of all the anodes 2a forming the individual sides of the stack 1. max (See FIG. 9) is obtained, and the maximum interval distance d max is checked whether it is smaller than a respective (third) tolerance value, which may be different for various aspects of the stack 1. If this precondition is respectively fulfilled, the stack 1 is evaluated as acceptable. If not, the stack 1 is evaluated as unacceptable or rejected.

[0047] For the cathodes 2b, a position check as provided for the anodes 2a is not necessarily possible, since the position of the edges covered by the other cathodes 2b cannot be known or cannot be uniquely known due to the relatively strong absorption of X-rays by the cathodes 2b. This applies in particular to an edge of one of the cathodes 2b which is overlapped by all the other cathodes 2b with respect to the arrangement with respect to the X-ray irradiator 7. The method therefore envisages, in a second calculation step, determining from the detected X-rays for the two pairs of opposite sides of the stack 1, the maximum edge separation distance (K_W_R_TD) which exists between all the edges of the cathodes 2b of each pair, respectively. This is specifically shown in FIG. 15. If the anodes 2a are designed in such a way that the position check described for this cannot be carried out, the method described for the cathodes 2b can also be advantageously applied for the anodes 2a.

[0048] In FIG. 15, for the sake of simplicity, only three cathodes 2b of the stack 1 are shown, the first cathode 2b' of which has the largest dimension (length or width) in terms of the extension of the stack 1 between a specific pair of sides. Here, this first cathode 2b' may be larger in terms of this dimension than the second cathode 2b'', which may correspond to the defined nominal dimension associated therewith. In contrast, the third cathode 2b''' is the smallest (of all cathodes 2b of the stack) in terms of the considered dimension. Due to the at least partial covering of the edges of the second cathode 2b'' and the third cathode 2b''' by the first cathode 2b' for X-rays, an unambiguous calculation of these covered edges may be hindered. For this reason, the second calculation step and the subsequent first and second inspection steps are based on a simplification of the calculation results. However, this simplification is chosen so that imprecision only exists for assessment of stack 1 as unacceptable, whereby a stack assessed as acceptable always meets all configurations at least with respect to the positional accuracy of electrode 2.

[0049] For this purpose, in a first inspection step, it is assumed that it is checked whether the maximum edge-to-edge distance (K_W_R_TD) existing between the edges of the specific pair of cathodes 2b on the side surface of the laminate 1 is smaller than a first tolerance value (K_W_R_TDmax). In this case, the laminate 1 is evaluated as unacceptable in the negative case (K_W_R_TD ≧ K_W_R_TDmax), and in the positive case (K_W_R_TD < K_W_R_TDmax), a second inspection step is carried out.

[0050] In the second inspection step, it is checked whether the maximum edge-to-edge distance (K_W_R_TD) is smaller than a value obtained on the one hand from the sum of the shortest dimensions (length or width) (K_W_R_min) of all the cathodes of the laminate in the calculation direction and on the other hand from the difference between a second tolerance value (T_G) and half of the overhang (v_R). As the overhang (v_R), here, half of the value by which the maximum edge-to-edge distance (K_W_R_TD) is smaller than the first tolerance value (K_W_R_TDmax) is defined. The second tolerance value (T_G) can here correspond to the maximum positional deviation defined (considered in the extension direction between the side surfaces of the pair) as acceptable for the edges of the cathode 2b. If this second inspection step results in a negative inspection result (K_W_R_TD ≧ (T_G - v_R) + K_W_R_min), the laminate is evaluated as unacceptable. In contrast, if the second inspection step results in a positive inspection result (K_W_R_TD < (T_G - v_R) + K_W_R_min), the laminate is evaluated as acceptable.

[0051] In order to determine the position of the edge within the framework of the second calculation step and further calculation and inspection steps, it is not necessary to capture this edge over its entire length with X-rays. Instead, two different sections of the edge can be determined in succession (see FIGS. 10 to 14) and the associated partial results can be combined with one another for the calculation of the individual edge course. For this purpose, the stack 1 can be moved in a targeted manner, for example according to FIGS. 10 to 14, through the linear capture areas of two linear detectors 10, which in combination represent the X-ray detector 8. In FIGS. 10 to 14, the edge sections still being captured in the respective capture step are shown with right-leaning shading, while the edge sections already previously captured are shown with left-leaning shading. By moving the battery cell stack 1 through the capture areas of the linear detectors 10, a flat capture area is obtained. This also makes it possible to simultaneously capture the edges assigned to two pairs of opposite sides of the stack 1. The linear detectors 10 are arranged in the form of mutually perpendicular crosses in the embodiment according to FIGS. 10 to 14. Other arrangements are possible as well, for example L-shaped. The movement of the stack 1 is aligned vertically with respect to the capture area of ​​one of these linear detectors 10, respectively.

[0052] Based on the simplification of the calculation result of the second calculation step, it is envisaged that the stack 1 assessed as unacceptable in the second calculation step and the associated first and second inspection steps is additionally inspected in a third inspection step, in which a more complex inspection of the type of computed tomography is carried out in this connection. For this purpose, the stack 1 according to FIG. 16, fixed on the workpiece support 11, is positioned in the field of the X-rays 9 in such a way that at least one edge of the stack 1 extending along the stacking direction 4 is captured. By rotating the stack 1 about the rotation axis 12, the shadow of the X-rays 9 through this edge is determined at several positions of the stack, on the basis of which the relative positions of the corners of the battery cell layers forming this edge of the stack 1 are determined. In this regard, FIG. 17 shows an example of an image generated on the basis of the X-rays 9 captured from a section of the stack 1 including the edge under consideration.

[0053] Preferably, this third inspection step is performed on at least two edges of the stack 1, where if there are only two edges inspected, they should be diagonally opposite each other in the stack 1.

[0054] Based on the edge positions determined in the third inspection step, it is then further checked whether these are within a defined tolerance range, in which case the laminate 1 is evaluated as rejected in the negative case and as acceptable in the positive case. The third inspection step is therefore used to verify whether the laminate 1 determined in the second calculation step and the first and second inspection steps belonging thereto as unacceptable and thus potentially unsuitable for use in the manufacture of batteries is also unsuitable and thus rejected or whether it has merely been graded as unacceptable on the basis of a simplification based on the first and second inspection steps. Such a grading is then taken into account by the third inspection step, thereby preventing the laminate 1 suitable for the manufacture of batteries from being treated as rejected. [Explanation of symbols]

[0055] 1. Laminate 2 electrodes 2a Anode 2b Cathode 2b' First cathode 2b'' Second cathode 2b'' Third cathode 3. Separator 4 Lamination direction 5. Camera 5a Camera capture area 6 Measuring probe 7 X-ray irradiator 8. X-ray detector 9 X-ray 9a Central beam of X-rays 10 Linear detector 11 Workpiece support 12 Rotation axis AA Anode stacking area A K Cathode stacking area A S Separator lamination area S A Optimal location of the anode edge S K Optimal location of cathode edge S S Optimal position of separator edge d AK The minimum spacing between the anode and cathode edges of a battery cell d AS The minimum spacing between the anode edge and the separator edge of a battery cell d max The maximum separation distance between the similarly existing edges of all anodes K_W_R_TD Maximum edge spacing of cathode for stack side pairs K_W_R_TDmax First tolerance value K_W_R_min The shortest dimension of the cathode relative to the stack side pair T_G Second tolerance value v_R Overhang amount

Claims

1. A method for testing a stack (1) of multiple battery cell layers in the form of an anode (2a) as a first type of electrode (2), a cathode (2b) as a second type of electrode (2), and a separator (3), comprising: The battery cell layers have polygonal large area portions and are stacked along a stacking direction (4) aligned perpendicular to the large area portions, wherein: In a first calculation step, the geometry of at least one of the large area portions of at least said anode (2a) and / or said cathode (2b) is determined, In the lamination step, the battery cell layer is laminated on the laminate (1), Subsequently, for position inspection of the anode (2a) and / or the cathode (2b), In a second calculation step, the stack (1) is irradiated with X-rays (9) irradiated by an X-ray irradiator (7) and detected by an X-ray detector (8), the X-rays (9) being aligned vertically with respect to a large area portion of the battery cell layer, and the detected X-rays are used to determine, for at least one pair of opposing sides of the stack (1), the maximum edge separation distance (K_W_R_TD) existing between the edges of the electrodes of the considered type of said pair; In a first test step, it is checked whether said maximum edge separation distance (K_W_R_TD) is smaller than a first tolerance value (K_W_R_TDmax), where If negative, the laminate (1) is rated as unacceptable; If so, a second test step is performed, in which In the second inspection step, a protrusion amount (v_R) is defined as half of a value where the maximum edge interval distance (K_W_R_TD) is smaller than the first allowable error value (K_W_R_TDmax); It is checked whether the maximum edge separation distance (K_W_R_TD) is smaller than a value determined on the one hand from the sum of the shortest dimensions (K_W_R_min) of the electrode (2) of the type under consideration in all calculated directions and on the other hand from the difference between a second tolerance value (T_G) and a half overhang (v_R), If negative, the laminate (1) is rated as unacceptable; If positive, the laminate (1) is evaluated as acceptable.

2. 2. The method according to claim 1, wherein in the first calculation step the positions of the edges forming all or only some of the corners of the electrodes (2) of the type considered are determined.

3. 3. The method according to claim 1 or 2, wherein the second calculation step and the first and second inspection steps are performed for at least two pairs of opposite sides of the stack (1).

4. Only one type of electrode (2) is inspected according to the second calculation step and the first and second inspection steps, and in a further calculation and inspection step, the stack (1) is irradiated with X-rays (9) which are irradiated by an X-ray irradiator (7) and detected by an X-ray detector (8), the X-rays (9) being aligned vertically with respect to a large area portion of the battery cell layer, and the maximum separation distance (d) existing between the edges of all electrodes (2) of the other type assigned to said side of the stack (1) is calculated using the X-rays detected with respect to at least one side of the stack (1). max ) is calculated, and based on the calculated value, the interval distance (d max ) are each checked to see if they are less than a third tolerance value, where: If not, the laminate (1) is evaluated as unacceptable or rejected; 4. The method according to claim 1, wherein, in the positive case, the laminate (1) is evaluated as acceptable.

5. If the laminate (1) is evaluated as unacceptable, in a third inspection step, the laminate (1) is additionally inspected for the maintenance of at least one tolerance range, If negative, the laminate (1) is evaluated as excluded; 5. The method according to claim 1, wherein, in the positive case, the laminate (1) is evaluated as acceptable.

6. 6. The method according to claim 5, wherein in the third inspection step, the stack (1) is irradiated with X-rays (9) which are irradiated by an X-ray irradiator (7) and detected by an X-ray detector (8), and an orientation of the stack (1) relative to the X-rays (9) is selected such that at least one edge of the stack (1) extending along the stacking direction (4) is completely captured by the X-rays (9) in at least two different positions, on the basis of which the relative positions of corners of at least the anode (2a) and / or the cathode (2b) which form said edge of the stack (1) are determined.

7. The method of claim 1 , wherein after lamination of the battery cell layers in the laminating step, the battery cell layers are inspected for the presence of buckles.

8. The method of claim 7, wherein the buckle inspection is performed by determining and evaluating the geometry of the battery cell layers and / or by determining and evaluating the geometry of the stack (1).

9. 9. The method according to claim 1, wherein determining the geometry of the battery cell layers and / or determining the geometry of the stack (1) is performed using an optical camera system.

10. The method of claim 9 , wherein the camera system images are recorded in a top view of a large area portion of the battery cell layer.

11. The method according to claims 8 and 10, wherein the geometry of the battery cell layers is determined after being placed on the formed stack (1), respectively.

12. 10. The method according to claims 8 and 9, wherein images of the camera system are recorded in a side view with respect to the stack (1) in order to determine the geometry of the battery cell layers in the formed stack (1).

13. The method of claim 8, wherein determining the geometry of the stack (1) comprises determining the height of the stack (1) at a plurality of locations.

14. The method of claim 13 , wherein the determining of the height is performed mechanically.

Citation Information

Patent Citations

  • Liquid injection device and method

    JP2014225373A

  • Battery cell inspection apparatus for automation of total inspection and inspection method thereof

    JP2020188004A

  • Method for detecting position offset of electrode plates in electrode laminates and device therefor

    WO2016114257A1