Start-up ring of glass melting furnace
The multi-annular start-up ring with connecting portions addresses the issue of ring breakage in glass melting furnaces, ensuring stable power supply and reducing the frequency of replacements by allowing current to bypass broken sections.
Patent Information
- Application Number
- JP2023049425
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-27
- Publication Date
- 2024-10-09
AI Technical Summary
The existing startup rings in glass melting furnaces using high-frequency induction heating often break during startup due to exothermic and oxidation reactions, leading to rapid changes in load impedance, activation of power interlocks, and the need for frequent replacement.
A start-up ring for glass melting furnaces is designed with multiple annular portions of varying diameters and a connecting portion, made of the same or different materials and thicknesses, to ensure continuous current flow and prevent rapid impedance fluctuations.
The design prevents power interlocks by allowing current to bypass broken annular parts, maintaining stable power supply during startup and reducing the need for frequent ring replacements.
Smart Images

Figure 2024138756000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a start-up ring for a glass melting furnace, and more particularly to a start-up ring for melting glass raw materials when the glass melting furnace is started up. [Background technology]
[0002] A cold crucible induction melter (CCIM) is a type of glass melting furnace that supplies radioactive waste and glass raw materials into a metal container, melts them at high temperatures by high-frequency induction heating using a high-frequency coil, and solidifies them into glass (see, for example, Patent Document 1). In such a CCIM, the surface temperature of the furnace wall is reduced by water-cooling the furnace wall, and the furnace wall is covered with a low-temperature layer of glass (skull layer), which reduces the corrosion rate of the furnace wall. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2006-145543 A Summary of the Invention [Problem to be solved by the invention]
[0004] In the glass melting furnace using high-frequency induction heating as described above, it is necessary to heat the glass raw material put into the furnace at the time of starting (start-up), and a jig called a start-up ring capable of generating heat by a high-frequency coil is arranged in the furnace. Such a start-up ring is, for example, a titanium ring as described in Patent Document 1, and is configured to burn out due to exothermic reaction and oxidation reaction, and eventually disappear in the furnace.
[0005] However, if the start-up ring breaks during start-up, the current stops flowing through the start-up ring, causing the load impedance of the power supply to change suddenly, activating the interlock and cutting off the power supply. When the power supply is cut off, it is necessary to restart the power supply, and if the glass raw material is not melted sufficiently, a new start-up ring must be placed in the furnace.
[0006] The present invention has been devised in view of the above problems, and an object of the present invention is to provide a start-up ring for a glass melting furnace which can avoid power supply interlock at the time of start-up. [Means for solving the problem]
[0007] According to the present invention, there is provided a start-up ring for a glass melting furnace that melts radioactive waste and glass raw materials by high-frequency induction heating using a high-frequency coil, characterized in that the start-up ring has a plurality of annular portions having different diameters and a connecting portion that connects the plurality of annular portions radially.
[0008] The connecting portion may be made of the same material as the annular portion and may be thicker than the annular portion.
[0009] The connecting portion may be made of a material having a higher heat resistance than the annular portion.
[0010] The plurality of annular portions may be formed of the same material with different thicknesses so that they break in order from the annular portion disposed radially outward.
[0011] The plurality of annular portions may be made of different materials so as to break in order starting from the annular portion disposed radially outward.
[0012] The multiple annular portions may be disposed in the same plane or in different planes. Effect of the Invention
[0013] The start-up ring of the glass melting furnace according to the present invention described above comprises a plurality of annular portions and connecting portions connecting these portions, so that even if the outer annular portion is broken due to burn damage caused by high-frequency induction heating, electricity can flow through the inner annular portion and the connecting portions, thereby suppressing sudden fluctuations in the load impedance of the power supply and avoiding power supply interlock at startup. [Brief description of the drawings]
[0014] [Figure 1] FIG. 1 is a cross-sectional view showing a glass melting furnace using a start-up ring according to one embodiment. [Diagram 2] FIG. 11 is a plan view showing the fracture history of a conventional start-up ring. [Diagram 3] 2 is a plan view showing an example of a fracture history of the start-up ring shown in FIG. 1. [Figure 4] 2 is a plan view showing an example of a different fracture history of the start-up ring shown in FIG. 1. [Diagram 5] 11A to 11D are diagrams showing modified examples of the startup ring, where (a) shows a first modified example, (b) shows a second modified example, (c) shows a third modified example, and (d) shows a fourth modified example. [Figure 6] 11A to 11D are diagrams showing modified examples of the startup ring, where (a) shows a fifth modified example, (b) shows a sixth modified example, (c) shows a seventh modified example, and (d) shows an eighth modified example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] Hereinafter, an embodiment of the present invention will be described with reference to Fig. 1 to Fig. 6(d). Here, Fig. 1 is a cross-sectional view showing a glass melting furnace using a start-up ring according to one embodiment. Fig. 2 is a plan view showing the fracture history of a conventional start-up ring. Fig. 3 is a plan view showing an example of the fracture history of the start-up ring shown in Fig. 1.
[0016] The glass melting furnace 1 shown in Fig. 1 is a so-called cold crucible induction furnace (CCIM). The glass melting furnace 1 includes, for example, a furnace wall 2 forming a metal container, a supply nozzle 3 for supplying radioactive waste and glass raw material into the furnace, an oxygen injector 4 for supplying oxygen into the furnace, an exhaust nozzle 5 for exhausting gas in the furnace, a high-frequency coil 6 arranged along the outer periphery of the furnace wall 2, a bubbler 7 for bubbling the molten glass layer, and a flow-down nozzle 8 for discharging the molten glass out of the furnace.
[0017] The glass melting furnace 1 is one of the glass melting furnaces that melts radioactive waste and glass raw materials fed into the furnace at high temperature and solidifies them into glass by high-frequency induction heating using a high-frequency coil 6. A water-cooling jacket is embedded in the furnace wall 2 of the glass melting furnace 1, so that it can be water-cooled. Therefore, the surface temperature of the furnace wall 2 can be lowered, and the furnace wall 2 can be covered with a low-temperature layer of glass (skull layer), so that the corrosion rate of the furnace wall 2 can be reduced.
[0018] The glass melting furnace 1 is not limited to the configuration shown in the figure, but may be any glass melting furnace that melts the radioactive waste and glass raw materials supplied into the furnace at high temperatures and solidifies them into glass by high-frequency induction heating using a high-frequency coil 6.
[0019] At the start-up of the glass melting furnace 1, glass frit (e.g., glass beads) is charged into the furnace to form a glass frit layer 9, and a startup ring 10 is placed on the top of the glass frit layer 9. The startup ring 10 may be placed inside the glass frit layer 9.
[0020] For example, as shown in Fig. 2, a conventional start-up ring 11 is a single ring part made of titanium. The start-up ring 11 is disposed in the glass frit layer 9 so as to be interlinked with the alternating magnetic flux generated by energizing the high-frequency coil 6.
[0021] The start-up ring 11 generates heat by Joule heat as a result of current flowing due to the interlinked alternating magnetic flux, as shown by the dotted arrows in the upper part of Fig. 2. The start-up ring 11 heats and melts the glass frit layer 9, making it conductive and capable of generating heat by itself. The start-up ring 11 is designed to burn out due to its own exothermic reaction and oxidation reaction, and eventually disappear.
[0022] During use of the start-up ring 11, a fractured portion x may occur in a part of the annular portion as shown in the lower part of Fig. 2. When the start-up ring 11 is fractured, the current stops flowing through the start-up ring 11, the load impedance of the power supply changes suddenly, the interlock is activated, and the power supply is cut off. When the power supply is cut off, the power supply needs to be restarted, and if the melting of the glass frit layer 9 is insufficient, a new start-up ring 11 needs to be relocated in the furnace.
[0023] The start-up ring 10 according to this embodiment includes, for example, a plurality of annular portions 12 having different diameters, and a connecting portion 13 that connects the plurality of annular portions 12 in the radial direction, as shown in FIG.
[0024] The annular portion 12 includes, for example, a first annular portion 12a, a second annular portion 12b, and a third annular portion 12c, which are arranged on the same plane in order of diameter as shown in the figure. The first annular portion 12a to the third annular portion 12c are made of the same material (for example, titanium alloy, etc.).
[0025] The connecting portions 13 are arranged, for example, in a cross shape, and the intersections with the first annular portion 12a to the third annular portion 12c are connected by welding so that electricity can flow therethrough. The connecting portions 13 are made of the same material as the first annular portion 12a to the third annular portion 12c, and are thicker than the first annular portion 12a to the third annular portion 12c. Therefore, the connecting portions 13 have a higher heat resistance than the annular portion 12, and can break the annular portion 12 before the connecting portions 13 break it.
[0026] When the start-up ring 10 is disposed above the glass raw material layer 9 and the high-frequency coil 6 is energized, a current flows through the first annular portion 12a, which is the outermost annular portion 12, as shown by the dotted arrow in the upper part of FIG.
[0027] Thereafter, if a breakage portion x occurs in the first annular portion 12a, as shown by the dotted arrow in the middle of Fig. 3, a current circuit is formed in the start-up ring 10 that bypasses the breakage portion x and passes through the outermost path formed by the first annular portion 12a, the second annular portion 12b, and the connecting portion 13. This makes it possible to reduce the change in the passing area of the magnetic flux interlinking with the start-up ring 10, and to prevent the power supply interlock from being activated.
[0028] Furthermore, even if a fracture x occurs in the second annular portion 12b, a current circuit is formed by the first annular portion 12a, the third annular portion 12c, and the connecting portion 13, as shown by the dotted arrow in the lower part of Figure 3, and activation of the power supply interlock can be avoided.
[0029] It should be noted that the location of the broken portion x shown in the figure is merely an example, and a different current circuit is formed so as to pass through the outermost path depending on the location of the broken portion x.
[0030] Here, Fig. 4 is a plan view showing an example of a different fracture history of the start-up ring shown in Fig. 1. When a fracture portion x occurs in the first annular portion 12a from the initial state shown in the upper left, a current circuit is formed by the first annular portion 12a, the second annular portion 12b, and the connecting portion 13, as shown in the lower left.
[0031] Then, as shown in the upper right corner, when a second breakage x occurs in the first annular portion 12a, a current circuit (first annular portion 12a, second annular portion 12b, connecting portion 13) is formed that passes through the outermost path that avoids the two breakage portions x.
[0032] Next, as shown in the middle right section, when a third breakage x occurs in the first annular portion 12a, a current circuit (first annular portion 12a, second annular portion 12b, connecting portion 13) is formed that passes through the outermost path that avoids the three breakage portions x.
[0033] Furthermore, as shown in the lower right section, when a fourth breakage portion x occurs in the first annular portion 12a, a current circuit (first annular portion 12a, second annular portion 12b, connecting portion 13) is formed that passes through the outermost path that avoids the four breakage portions x.
[0034] Next, modified examples of the startup ring 10 will be described with reference to Fig. 5(a) to Fig. 6(d). Fig. 5 shows modified examples of the startup ring, with (a) showing a first modified example, (b) showing a second modified example, (c) showing a third modified example, and (d) showing a fourth modified example. Fig. 6 shows modified examples of the startup ring, with (a) showing a fifth modified example, (b) showing a sixth modified example, (c) showing a seventh modified example, and (d) showing an eighth modified example.
[0035] In the first modified example shown in Fig. 5(a), the number of connecting parts 13 is reduced and the mesh (divided area) of the start-up ring 10 according to the first embodiment shown in Fig. 3 is enlarged. Specifically, the connecting parts 13 are formed in an I-shape.
[0036] In the second modified example shown in Fig. 5(b), the number of connecting parts 13 is increased to reduce the size of the mesh (divided area) of the start-up ring 10 according to the first embodiment shown in Fig. 3. Specifically, eight connecting parts 13 are arranged radially. As in the first and second modified examples, the number of connecting parts 13 can be set to any number as necessary.
[0037] In the third modified example shown in Fig. 5(c), the number of annular portions 12 is increased to reduce the mesh (divided area) of the start-up ring 10 according to the first embodiment shown in Fig. 3. Specifically, a fourth annular portion 12d is disposed inside the third annular portion 12c. The number of annular portions 12 is not limited to 3 or 4, and can be set to any number as required.
[0038] In the fourth modified example shown in Fig. 5(d), the intersections of the connecting parts 13 of the start-up ring 10 according to the first embodiment shown in Fig. 3 are omitted. In the fourth modified example, when the third annular part 12c is broken, no current flows through the start-up ring 10. However, at the stage where a current circuit is formed in the third annular part 12c, it is presumed that the glass frit layer 9 has transitioned to a molten glass layer to an extent that it has electrical conductivity, and therefore the operation of the power supply interlock can be suppressed.
[0039] In the fifth modified example shown in Fig. 6(a), the connecting portion 13 is made of a material having a higher heat resistance than the annular portion 12. For ease of explanation, the heat resistance is indicated by a grayscale shade in the figure. With this configuration, the annular portion 12 can be broken before the connecting portion 13.
[0040] In the sixth modified example shown in Fig. 6(b), the annular portions 12 are formed of the same material with different thicknesses so that they break in order starting from the first annular portion 12a arranged radially outward. Specifically, the first annular portion 12a to the third annular portion 12c are made of the same material, the second annular portion 12b is formed thicker than the first annular portion 12a, and the third annular portion 12c is formed thicker than the second annular portion 12b. Also, the connecting portion 13 is formed thicker than the second annular portion 12b.
[0041] 6(c), the annular portion 12 is made of different materials so that it breaks in order from the first annular portion 12a arranged radially outward. Specifically, the second annular portion 12b is made of a material with a higher heat resistance than the first annular portion 12a, and the third annular portion 12c is made of a material with a higher heat resistance than the second annular portion 12b. For ease of explanation, the figure shows the high and low heat resistance temperatures as shades of gray.
[0042] In the eighth modified example shown in Fig. 6(d), the start-up ring 10 is configured to have a three-dimensional shape. Specifically, the first annular portion 12a to the third annular portion 12c are arranged on different planes and are connected to each other by a connecting portion 13. Note that, although the outer shape of the start-up ring 10 is formed into a truncated cone shape in the eighth modified example, it may be formed into a cone shape.
[0043] The present invention is not limited to the above-described embodiment, and various modifications are possible without departing from the spirit of the present invention. [Explanation of symbols]
[0044] 1 Glass melting furnace 2 Furnace wall 3 Supply nozzle 4 Oxygen injector 5 Exhaust nozzle 6 High frequency coil 7. Bubbler 8. Flow Nozzle 9 Glass raw material layer 10 Startup Ring 11 Conventional Startup Ring 12 Annular section 12a First annular portion 12b Second annular portion 12c Third annular part 12d Fourth annular part 13 Connecting part
Claims
1. A start-up ring for a glass melting furnace that melts radioactive waste and glass raw materials by high-frequency induction heating using a high-frequency coil, A plurality of annular portions having different diameters; A connecting portion that connects the plurality of annular portions in a radial direction; A startup ring comprising:
2. 2. The start-up ring of a glass melting furnace according to claim 1, wherein the connecting portion is made of the same material as the annular portion and is thicker than the annular portion.
3. 2. The start-up ring of a glass melting furnace according to claim 1, wherein the connecting portion is made of a material having a higher heat resistance than the annular portion.
4. 2. The start-up ring of a glass melting furnace according to claim 1, wherein the plurality of annular portions are formed of the same material but with different thicknesses so as to break in order from the annular portion disposed radially outward.
5. 2. The start-up ring of a glass melting furnace according to claim 1, wherein the plurality of annular portions are made of different materials so as to break in order from the annular portion disposed radially outward.
6. The start-up ring of a glass melting furnace according to claim 1 , wherein the plurality of annular portions are arranged in the same plane or in different planes.
Citation Information
Patent Citations
Vitrification system and method of waste resin containing transition metal
JP2006145543A