Piezoelectric device

The piezoelectric device achieves high output by using laminated piezoelectric films with intermediate gaps to control rigidity and length, addressing resonance frequency and signal strength limitations in conventional devices.

JP2024139333APending Publication Date: 2024-10-09NISSHINBO MICRO DEVICES INC
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023050223
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-27
Publication Date
2024-10-09

AI Technical Summary

Technical Problem

Conventional piezoelectric devices face challenges in adjusting resonance frequency and output signal strength due to limitations in changing the rigidity and length of the vibration region, leading to reduced displacement and output when used as microphones or ultrasonic transmitters/receivers.

Method used

The piezoelectric device incorporates a configuration with a first and second laminated region of piezoelectric films sandwiched by electrodes, and an intermediate region with gaps or voids, allowing for a thicker and longer vibration region with controlled rigidity, enhancing displacement and output.

Benefits of technology

This configuration enables higher output signals by maintaining good film quality and resonance frequency while suppressing rigidity increases, resulting in high-output piezoelectric devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024139333000001_ABST
    Figure 2024139333000001_ABST
Patent Text Reader

Abstract

To provide a piezoelectric device of a high output.SOLUTION: A piezoelectric device 100 comprises: a support substrate 1; and a vibration region 7 that is supported by being bonded to the support substrate 1. The vibration region 7 is constructed by a first piezoelectric film 3a and a second piezoelectric film 3b, and first to fourth electrodes 4a to 4d arranged while nipping them. The piezoelectric device contains: a first lamination region A1 constructed by the first piezoelectric film 3a, the first electrode 4a, and the second electrode 4b; a second lamination region A2 constructed by the second piezoelectric film 3b, the third electrode 4c, and the fourth electrode 4d; and an intermediate region A3 that connects the first lamination region A1 and the second lamination region A2. The intermediate region A3 is constructed by a region having a gap 10.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a piezoelectric device, and more particularly to a high-output piezoelectric device. [Background technology]

[0002] Piezoelectric devices, which have a thin film (piezoelectric film) of piezoelectric material, can detect voltage changes caused by displacement of the piezoelectric film that constitutes the vibration region, or can displace the piezoelectric film by applying a voltage to it, and can be used as piezoelectric sensors, piezoelectric actuators, etc.

[0003] For example, a conventional piezoelectric device employs a cantilever structure in which one end of a vibration region is bonded to a support substrate and supported by the support substrate. This type of piezoelectric device is disclosed in, for example, Patent Document 1. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Patent No. 5936154 Summary of the Invention [Problem to be solved by the invention]

[0005] FIG. 6 shows a schematic cross-sectional view for explaining a conventional piezoelectric device. As shown in FIG. 6, in a conventional piezoelectric device 400, a first piezoelectric film 3a and a second piezoelectric film 3b are laminated on a support substrate 1 via an insulating film 2, a first electrode 4a and a second electrode 4b are arranged on either side of the first piezoelectric film 3a, and a second electrode 4b and a third electrode 4c are arranged on either side of the second piezoelectric film 3b. A cavity 5 is formed in the support substrate 1, and the first piezoelectric film 3a, the second piezoelectric film 3b, and the first to third electrodes 4a to 4c on the cavity 5 are partitioned by slits 6 (FIG. 7), thereby forming a vibration region 7 whose one end is joined to and supported by the support substrate 1. 8a and 8b are lead electrodes, and the lead electrode 8a is connected to the first electrode 4a and the third electrode 4c, and the lead electrode 8b is connected to the second electrode 4b.

[0006] Fig. 7 is a schematic plan view illustrating an example of the arrangement of the slits 6 in the piezoelectric device 400 in Fig. 6. When the slits 6 are arranged as shown in Fig. 7, a piezoelectric device 400 having two vibration regions 7 with a cantilever structure is formed. Note that the cross-sectional view taken along line CC in Fig. 7 corresponds to Fig. 6, and Fig. 7 does not show the third electrode 4c, the extraction electrodes 8a and 8b, etc., shown in Fig. 6, but shows only the arrangement of the slits 6 penetrating the first piezoelectric film 3a and the second piezoelectric film 3b, etc., covering the cavity 5.

[0007] 6 and 7, the resonant frequency of the vibrating region 7 can be adjusted by the rigidity and length L of the vibrating region 7. Specifically, the resonant frequency increases when the rigidity of the vibrating region 7 is increased, and the resonant frequency increases when the length L of the vibrating region 7 is decreased. Note that the length L of the vibrating region 7 is the length from the joint end with the support substrate 1 to the open end, as shown in FIG.

[0008] In order to form a piezoelectric film with good film quality, the thickness of the piezoelectric film formed by sputtering or CVD (Chemical Vapor Deposition) is usually set to 0.5 to 1.0 μm, and it is difficult to significantly change the thickness of the piezoelectric film. Since the rigidity of the vibration region 7 is determined once the type and thickness of the piezoelectric material constituting the piezoelectric film are determined, it is difficult to significantly change the rigidity of the vibration region 7 in order to adjust the resonance frequency of the vibration region 7. Therefore, the resonance frequency of the vibration region 7 is generally adjusted by changing the length of the vibration region 7.

[0009] For example, when the piezoelectric device 400 shown in Figures 6 and 7 is used as a microphone, the resonant frequency of the vibration region 7 is adjusted to about 20 kHz to increase the sensitivity of the microphone. In this case, the length of the vibration region 7 is about 500 µm. When the length of the vibration region 7 is shortened in this way to adjust the resonant frequency, the displacement of the piezoelectric film constituting the vibration region 7 becomes small, resulting in a problem of a decrease in the output signal.

[0010] Furthermore, when the piezoelectric device 400 is used as an ultrasonic transmitter / receiver for obstacle detection or ultrasonic diagnosis, the length of the vibration region 7 is adjusted to be even shorter, resulting in a further decrease in the output signal. Such a decrease in the output signal is not limited to the cantilever-structured piezoelectric device 400 shown in Figures 6 and 7, but is also a problem that occurs in piezoelectric devices with a bridge structure in which two opposing sides of the vibration region are bonded to a support substrate and supported thereon, and in piezoelectric devices with a membrane structure in which no slits are formed and the periphery of the vibration region is bonded to a support substrate and supported thereon.

[0011] SUMMARY OF THE PRESENT EMBODIMENTS An object of the present invention is to provide a high-output piezoelectric device. [Means for solving the problem]

[0012] The piezoelectric device of the present invention comprises a support substrate, a piezoelectric film constituting a vibration region supported by being bonded to the support substrate, and electrodes arranged on either side of the piezoelectric film, the piezoelectric film including at least a first piezoelectric film and a second piezoelectric film, the vibration region including a first stacked region constituted by the first piezoelectric film and a first electrode and a second electrode arranged on either side of the first piezoelectric film, a second stacked region constituted by the second piezoelectric film and a third electrode and a fourth electrode arranged on either side of the second piezoelectric film, and an intermediate region arranged between the first stacked region and the second stacked region, connecting the first stacked region and the second stacked region, the intermediate region being constituted by a region having a gap. Effect of the Invention

[0013] According to the piezoelectric device of the present invention, the vibration region can be made thick by configuring it to include a first stacking region, an intermediate region, and a second stacking region, and the increase in rigidity of the vibration region is suppressed by configuring the intermediate region to have a gap, so that the displacement of the first piezoelectric film that constitutes the first stacking region and the second piezoelectric film that constitutes the second stacking region is large, making it possible to provide a high-output piezoelectric device. [Brief description of the drawings]

[0014] [Figure 1] 1 is a schematic cross-sectional view of a piezoelectric device (embodiment 1) according to one embodiment of the present invention. [Diagram 2] 4 is a plan view illustrating an example of an arrangement of slits and connecting posts in the piezoelectric device of Embodiment 1. FIG. [Diagram 3] 4 is a schematic cross-sectional view of a piezoelectric device according to another embodiment of the present invention (embodiment 2). FIG. [Figure 4] 11 is a plan view illustrating an example of an arrangement of slits and connecting walls in a piezoelectric device according to Embodiment 2. FIG. [Diagram 5] FIG. 4 is a schematic cross-sectional view of a piezoelectric device according to still another embodiment (embodiment 3) of the present invention. [Figure 6] FIG. 1 is a schematic cross-sectional view of a conventional piezoelectric device. [Figure 7] FIG. 11 is a schematic plan view illustrating an example of an arrangement of slits in a conventional piezoelectric device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] The piezoelectric device of the present invention will be described with reference to the drawings, but the present invention is not limited to these embodiments, and the members, materials, etc. described below can be modified in various ways within the scope of the present invention. Furthermore, the same reference numerals in the drawings indicate equivalent or identical items, and the size and positional relationship between each component are for convenience only and do not strictly reflect the actual situation.

[0016] In the piezoelectric device of the present invention, the vibration region includes a first stacking region, an intermediate region, and a second stacking region, and the intermediate region is configured as a region having a gap. The vibration region of the piezoelectric device configured in this manner can be configured to be thick. Furthermore, the rigidity of this vibration region is smaller than that of a vibration region of the same thickness configured with a single piezoelectric film, and does not change significantly compared to the rigidity of a structure in which the first piezoelectric film of the first stacking region and the second piezoelectric film of the second stacking region are stacked without sandwiching the intermediate region. As a result, the displacement of the first piezoelectric film and the second piezoelectric film is large, making it possible to configure a high-output piezoelectric device.

[0017] (Embodiment 1) Fig. 1 is a schematic cross-sectional view for explaining a first embodiment of a piezoelectric device of the present invention. As shown in Fig. 1, a first electrode 4a, a first piezoelectric film 3a, and a second electrode 4b are laminated on a support substrate 1 made of, for example, a silicon substrate, with an insulating film 2 made of, for example, a thermal oxide film interposed therebetween, and the first electrode 4a and the second electrode 4b are disposed with the first piezoelectric film 3a sandwiched therebetween. The first electrode 4a and the second electrode 4b are made of, for example, molybdenum, and the first piezoelectric film 3a is made of, for example, aluminum nitride, zinc oxide, PZT (lead zirconate titanate), or the like.

[0018] A connecting portion 9 made of, for example, polysilicon is laminated on the second electrode 4b. A part of the connecting portion 9 forms, for example, a connecting pillar portion 9a having a cylindrical structure. A plurality of connecting pillar portions 9a are arranged on the second electrode 4b in the region that forms the vibration region 7. The plurality of connecting pillar portions 9a are arranged at intervals from one another, thereby forming a configuration having gaps 10 between the connecting pillar portions 9a.

[0019] The fourth electrode 4d, the second piezoelectric film 3b, and the third electrode 4c are laminated on the connecting portion 9 and the connecting column portion 9a, and the third electrode 4c and the fourth electrode 4d are arranged with the second piezoelectric film 3b sandwiched therebetween. The third electrode 4c and the fourth electrode 4d are made of, for example, molybdenum, and the second piezoelectric film 3b is made of, for example, aluminum nitride, zinc oxide, PZT, etc. From the viewpoint of stress control, it is preferable that the first piezoelectric film 3a and the second piezoelectric film 3b are made of the same piezoelectric material.

[0020] A cavity 5 is formed in the support substrate 1, and the first piezoelectric film 3a, the second piezoelectric film 3b and the first to fourth electrodes 4a to 4d on the cavity 5 are partitioned by slits 6 to form a vibration region 7 having one end joined to and supported by the support substrate 1. 8a and 8b are extraction electrodes, with the extraction electrode 8a connected to the first electrode 4a and the third electrode 4c, and the extraction electrode 8b connected to the second electrode 4b and the fourth electrode 4d.

[0021] Fig. 2 is a schematic plan view illustrating an example of the arrangement of the slits 6 and the connecting pillars 9a of the piezoelectric device 100 of Fig. 1. By arranging the slits 6 as shown in Fig. 2, it is possible to configure the piezoelectric device 100 having two vibration regions 7 with a cantilever structure. Note that the cross-sectional view taken along line AA in Fig. 2 corresponds to Fig. 1, and Fig. 2 does not show the third electrode 4c, the extraction electrodes 8a and 8b, etc. shown in Fig. 1, but only shows the arrangement of the slits 6 and the connecting pillars 9a that penetrate the first piezoelectric film 3a and the second piezoelectric film 3b that cover the cavity 5.

[0022] 1 and 2, in the vibration region 7 of the piezoelectric device 100 of this embodiment, a first stacked region A1 consisting of the first electrode 4a, the first piezoelectric film 3a, and the second electrode 4b, and a second stacked region A2 consisting of the fourth electrode 4d, the second piezoelectric film 3b, and the third electrode 4c are disposed between them, with a middle region A3 consisting of a connecting column portion 9a connecting them and a gap 10. One end of the connecting column portion 9a is joined to the second electrode 4b, and the other end is joined to the fourth electrode 4d, thereby connecting the first stacked region A1 and the second stacked region A2.

[0023] The connecting pillars 9a are arranged so that the vibration region 7 has the desired vibration characteristics. As an example, as shown in Figs. 1 and 2, the connecting pillars 9a are arranged in a row from the joint with the support substrate 1 supporting the vibration region 7 to the end of the vibration region 7 in a direction parallel to at least the short side of the rectangular vibration region 7, so that the first laminated region A1 and the second laminated region A2 can be configured to vibrate together. When the connecting pillars 9a are arranged in this manner, the gaps 10 are also arranged in a direction parallel to the short side of the vibration region 7, and the rigidity of the vibration region 7 including the intermediate region A3 is not larger than the rigidity of the laminated film in a structure in which the first piezoelectric film 3a and the second piezoelectric film 3b are laminated without sandwiching the intermediate region A3. In order to achieve the desired vibration characteristics, it is preferable to appropriately change the arrangement of the connecting pillars 9a, as well as the shape, the number of the connecting pillars 9a, and the material constituting the connecting pillars 9a.

[0024] Next, a configuration that can achieve high output in the piezoelectric device 100 of this embodiment shown in FIGS. 1 and 2 will be described in detail while comparing it with a conventional piezoelectric device 400 shown in FIGS.

[0025] The thicker the vibration region 7, the greater the displacement of the surface of the vibration region 7, making it possible to achieve higher output. In the piezoelectric device 100, the intermediate region A3 is disposed so that the thickness of the vibration region 7 is greater than the thickness of the vibration region 7 of the piezoelectric device 400, and the first piezoelectric film 3a and the second piezoelectric film 3b are disposed on the surface of the vibration region 7. Therefore, the displacement of the first piezoelectric film 3a and the second piezoelectric film 3b is large, making it possible to achieve high output.

[0026] The longer the length of the vibration region 7 (the length corresponding to L in FIG. 7), the greater the displacement of the vibration region 7, making it possible to achieve higher output. Since the vibration region 7 of the piezoelectric device 100 is configured to be thicker as described above, the resonance frequency of the vibration region 7 of the piezoelectric device 100 is higher than the resonance frequency of the vibration region 7 of the piezoelectric device 400, which has the same length. In other words, when configuring a vibration region 7 that resonates at the same frequency, the length of the vibration region 7 of the piezoelectric device 100 is configured to be longer than the length of the vibration region of the piezoelectric device 400. This makes it possible to achieve higher output.

[0027] If the rigidity of the vibration region 7 becomes too high, it hinders the displacement of the vibration region 7, which hinders the achievement of higher output. In the piezoelectric device 100, the multiple connecting pillars 9a are arranged at a distance from each other, and the intermediate region A3 is configured to have a gap 10, thereby suppressing an increase in the rigidity of the vibration region 7. It is also possible to configure the rigidity of the vibration region 7 of the piezoelectric device 100 to be approximately equal to the rigidity of the vibration region of the piezoelectric device 400. Therefore, there is no hindrance to achieving higher output.

[0028] Furthermore, the piezoelectric film constituting the vibration region 7 can be formed with good film quality, thereby enabling high output. In the piezoelectric device 100, the thicknesses of the first piezoelectric film 3a and the second piezoelectric film 3b can be set within a range in which a piezoelectric film with good film quality can be formed (0.5 to 1.0 μm when formed by sputtering or the like). In other words, the film quality of the piezoelectric film constituting the vibration region 7 of the piezoelectric device 100 can be configured to be substantially the same as the film quality of the piezoelectric film constituting the vibration region of the piezoelectric device 400. Therefore, high output is not hindered.

[0029] As described above, according to the piezoelectric device 100 of this embodiment, the length, rigidity, and thickness of the vibration region 7 and the film quality of the piezoelectric film can be suitably set to achieve high output.

[0030] (Embodiment 2) Next, a second embodiment of the piezoelectric device of the present invention will be described. Fig. 3 is a schematic cross-sectional view for explaining the second embodiment of the piezoelectric device of the present invention. As shown in Fig. 3, a first electrode 4a, a first piezoelectric film 3a, and a second electrode 4b are laminated on a support substrate 1 made of, for example, a silicon substrate, via an insulating film 2 made of, for example, a thermal oxide film, and the first electrode 4a and the second electrode 4b are disposed with the first piezoelectric film 3a sandwiched therebetween. The first electrode 4a and the second electrode 4b are made of, for example, molybdenum, and the first piezoelectric film 3a is made of, for example, aluminum nitride, zinc oxide, PZT, or the like.

[0031] A connecting portion 9 made of, for example, polysilicon is laminated on the second electrode 4b. A part of the connecting portion 9 constitutes, for example, a connecting wall portion 9b having a wall-like structure. A plurality of connecting wall portions 9b are arranged on the second electrode 4b in the region that constitutes the vibration region 7. The plurality of connecting wall portions 9b are arranged at intervals from each other, so that a gap 10 is formed between the connecting wall portions 9b.

[0032] The fourth electrode 4d, the second piezoelectric film 3b, and the third electrode 4c are laminated on the connecting portion 9 and the connecting wall portion 9b, and the third electrode 4c and the fourth electrode 4d are arranged with the second piezoelectric film 3b sandwiched therebetween. The third electrode 4c and the fourth electrode 4d are made of, for example, molybdenum, and the second piezoelectric film 3b is made of, for example, aluminum nitride, zinc oxide, PZT, etc. From the viewpoint of stress control, it is preferable that the first piezoelectric film 3a and the second piezoelectric film 3b are made of the same piezoelectric material.

[0033] A cavity 5 is formed in the support substrate 1, and the first piezoelectric film 3a, the second piezoelectric film 3b and the first to fourth electrodes 4a to 4d on the cavity 5 are partitioned by slits 6 to form a vibration region 7 supported by one end bonded to the support substrate 1. Like the above-mentioned piezoelectric device 100, the piezoelectric device 200 of this embodiment also has extraction electrodes (not shown), one of which is connected to the first electrode 4a and the third electrode 4c, and the other is connected to the second electrode 4b and the fourth electrode 4d.

[0034] Fig. 4 is a schematic plan view illustrating an example of the arrangement of the slits 6 and the connecting wall portion 9b of the piezoelectric device 200 of Fig. 3. By arranging the slits 6 as shown in Fig. 4, it is possible to configure the piezoelectric device 200 having two vibration regions 7 with a cantilever structure. Note that the cross-sectional view taken along line BB in Fig. 4 corresponds to Fig. 3, and Fig. 4 does not illustrate the third electrode 4c shown in Fig. 3, but only illustrates the arrangement of the slits 6 and the connecting wall portion 9b penetrating the first piezoelectric film 3a and the second piezoelectric film 3b that cover the cavity 5.

[0035] 3 and 4, in the vibration region 7 of the piezoelectric device 200 of this embodiment, a first stacked region A1 consisting of the first electrode 4a, the first piezoelectric film 3a, and the second electrode 4b, and a second stacked region A2 consisting of the fourth electrode 4d, the second piezoelectric film 3b, and the third electrode 4c are also arranged between them, with a connecting wall portion 9b connecting them and an intermediate region A3 consisting of a gap 10. One end of the connecting wall portion 9b is joined to the second electrode 4b, and the other end is joined to the fourth electrode 4d, thereby connecting the first stacked region A1 and the second stacked region A2.

[0036] The connecting wall 9b is arranged so that the vibration region 7 has the desired vibration characteristics. As an example, as shown in FIG. 4, the connecting wall 9b is arranged so that it extends from the joint with the support substrate 1 supporting the vibration region 7 to the end of the vibration region 7 in a direction parallel to the short side of the rectangular vibration region 7, so that the first laminated region A1 and the second laminated region A2 can be configured to vibrate integrally. By arranging the connecting wall 9b in this manner, the gap 10 is also arranged in a direction parallel to the short side of the vibration region 7, and the rigidity of the vibration region 7 including the intermediate region A3 is not larger than the rigidity of the laminated film in a structure in which the first piezoelectric film 3a and the second piezoelectric film 3b are laminated without sandwiching the intermediate region A3. In order to achieve the desired vibration characteristics, it is preferable to appropriately change the arrangement of the connecting wall 9b, as well as the shape, the number of the connecting wall 9b, the material of the connecting wall 9b, etc.

[0037] In the piezoelectric device 200 having the connecting wall portion 3b in this manner, the vibration region 7 can be configured to be thick and long, similar to the piezoelectric device 100 described in the above embodiment 1. In addition, the thickness of the piezoelectric film can be set within a range that allows the formation of a piezoelectric film with good film quality.

[0038] The rigidity of the vibration region 7 of the piezoelectric device 200 of this embodiment may be higher than that of the vibration region 7 of the piezoelectric device 100 because the joint area between the connecting wall portion 9b and the second electrode 4b and the fourth electrode 4d is larger than the joint area between the connecting column portion 9a and the second electrode 4b and the fourth electrode 4d in the piezoelectric device 100. However, when compared with the piezoelectric device 400, the rigidity is equivalent and does not hinder the achievement of high output.

[0039] Therefore, according to the piezoelectric device 200 of this embodiment, the length, rigidity, and thickness of the vibration region 7 and the film quality of the piezoelectric film can be suitably set to achieve high output.

[0040] (Embodiment 3) Next, a third embodiment of the piezoelectric device of the present invention will be described. Fig. 5 is a schematic cross-sectional view for explaining the third embodiment of the piezoelectric device of the present invention. As shown in Fig. 5, a first electrode 4a, a first piezoelectric film 3a, and a second electrode 4b are laminated on a support substrate 1 made of, for example, a silicon substrate, via an insulating film 2 made of, for example, a thermal oxide film, and the first electrode 4a and the second electrode 4b are disposed with the first piezoelectric film 3a sandwiched between them. The first electrode 4a and the second electrode 4b are made of, for example, molybdenum, and the first piezoelectric film 3a is made of, for example, aluminum nitride, zinc oxide, PZT, or the like.

[0041] A porous film 11 (corresponding to a connecting portion) is laminated on the second electrode 4b. The porous film 11 is composed of a film having a plurality of voids therein, and is composed of, for example, fluorinated silicate glass (FSG), carbon-doped glass (SiOC), porous silica, or the like.

[0042] The fourth electrode 4d, the second piezoelectric film 3b, and the third electrode 4c are laminated on the porous film 11, and the third electrode 4c and the fourth electrode 4d are arranged with the second piezoelectric film 3b sandwiched between them. The third electrode 4c and the fourth electrode 4d are made of, for example, molybdenum, and the second piezoelectric film 3b is made of, for example, aluminum nitride, zinc oxide, PZT, etc. From the viewpoint of stress control, it is preferable that the first piezoelectric film 3a and the second piezoelectric film 3b are made of the same piezoelectric material.

[0043] A cavity 5 is formed in the support substrate 1, and the first piezoelectric film 3a, the porous film 11, the second piezoelectric film 3b, and the first to fourth electrodes 4a to 4d on the cavity 5 are partitioned by slits 6 to form a vibration region 7 having one end joined to and supported by the support substrate 1. 8a and 8b are extraction electrodes, with the extraction electrode 8a connected to the first electrode 4a and the third electrode 4c, and the extraction electrode 8b connected to the second electrode 4b and the fourth electrode 4d.

[0044] By arranging the slits 6 in the same manner as the slits 6 described in the first and second embodiments, it is possible to configure a piezoelectric device 300 having two vibration regions 7 with a cantilever structure.

[0045] As shown in FIG. 5, the vibration region 7 of the piezoelectric device 300 of this embodiment has a first stacked region A1 consisting of the first electrode 4a, the first piezoelectric film 3a, and the second electrode 4b, and a second stacked region A2 consisting of the fourth electrode 4d, the second piezoelectric film 3b, and the third electrode 4c, with an intermediate region A3 consisting of a porous film 11 having a void therein that connects these regions.

[0046] The porous film 11 is selected from materials that give the vibration region 7 desired vibration characteristics, and the thickness, film quality, porosity, and the like may be adjusted.

[0047] In the piezoelectric device 300 including the porous film 11 in this manner, the vibration region 7 can be configured to be thick and long, similarly to the piezoelectric devices 100 and 200 described in the above-mentioned embodiments 1 and 2. In addition, the thickness of the piezoelectric film can be set within a range in which a piezoelectric film with good film quality can be formed.

[0048] The rigidity of the vibration region 7, if it is the porous film 11 containing voids, is sufficiently lower than that of the piezoelectric device 400, and high output can be achieved.

[0049] Although one embodiment of the piezoelectric device of the present invention has been described above, the present invention is not limited to the above embodiment and can be modified in various ways. For example, the connecting portion constituting the intermediate region can be formed by combining a connecting column portion and a connecting wall portion. The connecting wall portion can also be configured to arrange short connecting wall portions in a row. The first to fourth electrodes do not necessarily need to be formed over the entire surface of the vibration region, and may be arranged to sandwich at least the region where the displacement of the first piezoelectric film and the second piezoelectric film occurs. The arrangement of the slits 6 can also be changed, and a bridge structure or a membrane structure can be used in addition to a cantilever structure.

[0050] (summary) (1) One embodiment of a piezoelectric device of the present invention comprises a support substrate, a piezoelectric film that constitutes a vibration region supported by being bonded to the support substrate, and electrodes arranged on either side of the piezoelectric film, the piezoelectric film including at least a first piezoelectric film and a second piezoelectric film, the vibration region including a first stacked region constituted by the first piezoelectric film and a first electrode and a second electrode that are arranged on either side of the first piezoelectric film, a second stacked region constituted by the second piezoelectric film and a third electrode and a fourth electrode that are arranged on either side of the second piezoelectric film, and an intermediate region that is arranged between the first stacked region and the second stacked region and connects the first stacked region and the second stacked region, the intermediate region being constituted by a region having a gap.

[0051] According to the piezoelectric device of this embodiment, the vibration region can be made thick and an increase in the rigidity of the vibration region can be suppressed, so that the first piezoelectric film constituting the first laminate film and the second piezoelectric film constituting the second laminate film can be displaced more significantly, making it possible to obtain a high output signal.

[0052] (2) The intermediate region includes a plurality of connecting portions, one end of which is joined to the first stacking region and another end of which is joined to the second stacking region, and is configured to have the gap between the connecting portions that are spaced apart from each other.

[0053] (3) The intermediate region includes a porous film laminated between the first laminate region and the second laminate region. [Explanation of symbols]

[0054] 100~400 Piezoelectric devices 1 Support substrate 2. Insulating film 3a First piezoelectric film 3b Second piezoelectric film 4a~4d 1st~4th electrode 5 Cavity 6 Slit 7 Vibration area 8a, 8b Extraction electrode 9 Connecting part 9a Connecting column 9b Connecting wall 10 Gap 11. Porous membrane

Claims

1. A support substrate; a piezoelectric film that constitutes a vibration region that is bonded to and supported by the support substrate; Electrodes arranged on either side of the piezoelectric film; Equipped with The piezoelectric film is at least a first piezoelectric film and a second piezoelectric film; The vibration region is a first stacking region configured with the first piezoelectric film and a first electrode and a second electrode disposed with the first piezoelectric film sandwiched therebetween, a second stacking region configured with the second piezoelectric film and a third electrode and a fourth electrode disposed with the second piezoelectric film sandwiched therebetween, and an intermediate region disposed between the first stacking region and the second stacking region, connecting the first stacking region and the second stacking region; The intermediate region is composed of a region having a void. Piezoelectric devices.

2. the intermediate region includes a plurality of connecting portions each having one end connected to the first stacking region and another end connected to the second stacking region, and the gap is provided between the connecting portions spaced apart from each other; 2. The piezoelectric device according to claim 1.

3. The intermediate region includes a porous film laminated between the first laminated region and the second laminated region.

2. The piezoelectric device according to claim 1.

Citation Information

Patent Citations

  • Oven dish of talc-containing plastic