Indirect heating vapor deposition device and method of controlling indirect heating vapor deposition device
The indirect heating vapor deposition apparatus addresses the issue of droplet scattering by using controlled electron beam preheating and inner wall surface modification to improve wettability, ensuring better film quality and properties.
Patent Information
- Application Number
- JP2023050243
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-27
- Publication Date
- 2024-10-09
AI Technical Summary
Conventional indirect heating vapor deposition apparatuses suffer from the issue of minute particles adhering to the substrate surface due to droplets of evaporated material scattering from the container wall during film formation, which deteriorates film quality and properties.
The apparatus includes a preheating step with controlled electron beam currents to melt the vapor deposition material, followed by an inner wall surface modification step to cover the container's inner wall with the melted material, improving wettability and preventing droplet scattering.
This approach effectively suppresses droplet scattering and adhesion to the substrate, enhancing film quality by maintaining the inner wall surface with the vapor deposition material, thereby reducing minute particle generation.
Smart Images

Figure 2024139349000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an indirect heating evaporation apparatus that heats a container filled with an evaporation material by electron beam bombardment to heat and evaporate the evaporation material, and a method for controlling the indirect heating evaporation apparatus. [Background technology]
[0002] Conventionally, deposition devices have been known in which a substrate is placed in a vacuum chamber and a deposition source is provided facing the substrate. Examples of indirect heating deposition devices include electron beam bombardment deposition sources that emit an electron beam (thermal electrons) into a container filled with deposition material (see, for example, Patent Document 1).
[0003] The indirect heating evaporation device described in Patent Document 1 describes a technology including a container (liner) filled with an evaporation material, an evaporation electron beam source, a preheating electron beam source, and an evaporation material supply mechanism. The evaporation electron beam source irradiates the container with thermoelectrons in an evaporation heating region. The preheating electron beam source irradiates the container with thermoelectrons in a preheating region. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Patent Publication No. 2022-68958 Summary of the Invention [Problem to be solved by the invention]
[0005] However, in conventional indirect heating deposition devices, when observing the substrate surface after film formation, many fine particles may be found, which is one of the factors that deteriorate the film quality and film characteristics. The reason why these fine particles adhere to the substrate surface is that evaporated particles of the deposition material adhere to the wall surface of the container as droplets during film formation, and the attached droplets are pulled away from the wall surface of the container by external energy and scattered into the vacuum. Alternatively, the droplets bump and scatter into the vacuum. As a result, it is thought that the scattered deposition material adheres to the substrate surface.
[0006] In consideration of the above problems, an object of the present invention is to provide an indirect heating evaporation apparatus and a control method for an indirect heating evaporation apparatus that can prevent droplets from scattering from a container and adhering to a substrate during evaporation. [Means for solving the problem]
[0007] One aspect of the indirect heating deposition apparatus of the present invention includes a container filled with deposition material, an electron beam generating source that irradiates the container filled with the deposition material with an electron beam that evaporates the deposition material, and a control unit that controls the electron beam generating source. The control unit controls the electron beam generating source to perform a preheating process of preheating the deposition material before a deposition process of depositing the deposition material on a substrate. During the preheating process, the electron beam current of the electron beam generating source is set to a first preheating current. Thereafter, the electron beam current of the electron beam generating source is set to a second preheating current that is higher than the first preheating current, and an inner wall surface modification process is performed to cover the inner wall surface of the container with the molten deposition material.
[0008] In addition, the control method for an indirect heating evaporation apparatus of the present invention includes a preheating step of controlling an electron beam generating source to preheat an evaporation material, and a deposition step of controlling the electron beam generating source to deposit the evaporation material onto a substrate after the preheating step. Then, during the preheating step, the electron beam current of the electron beam generating source is set to a first preheating current to preheat the deposition material, and then the electron beam current of the electron beam generating source is set to a second preheating current that is higher than the first preheating current to perform an inner wall surface modification step of covering the inner wall surface of the container with the molten deposition material. Effect of the Invention
[0009] As described above, according to one aspect of the present invention, it is possible to prevent droplets from scattering from a container during deposition and adhering to a substrate. [Brief description of the drawings]
[0010] [Figure 1] 1 is a schematic configuration diagram of an indirect heating evaporation device according to a first embodiment of the present invention. [Diagram 2] FIG. 2 is a diagram showing a time chart of a control method for the indirect heating evaporation apparatus according to the first embodiment of the present invention. [Diagram 3] FIG. 4 is a schematic diagram of an indirect heating evaporation apparatus according to a second embodiment of the present invention. [Figure 4] FIG. 11 is a diagram showing an example of a scanning coil current waveform in the indirect heating evaporation device according to the second embodiment of the present invention. [Diagram 5] FIG. 11 is a diagram showing a time chart of a control method for an indirect heating evaporation apparatus according to a second embodiment of the present invention. [Figure 6] FIG. 2 is a diagram showing the relationship between the electron beam current and the remaining amount of evaporation material in the indirect heating evaporation device according to the first embodiment and in the indirect heating evaporation device according to the second embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Hereinafter, examples of embodiments of the present invention will be described with reference to the accompanying drawings. In addition, components having substantially the same functions or configurations in each figure are given the same reference numerals and duplicated explanations are omitted.
[0012] 1. First embodiment 1-1. Configuration of indirect heating evaporation equipment First, the configuration of an indirect heating evaporation apparatus according to a first embodiment (hereinafter referred to as "this example") will be described with reference to FIG. FIG. 1 is a schematic diagram of the indirect heating evaporation apparatus of this embodiment.
[0013] The indirect heating deposition apparatus 1 shown in FIG. 1 is an apparatus that heats and evaporates a deposition material filled in a container, thereby depositing the material on an object to be deposited. 1, the indirect heating deposition apparatus 1 includes a plurality of liners 2 which are specific examples of containers, a holder 3 which is a specific example of a container holding part, a support member 5, an adhesion-preventing cover 7, a vacuum chamber 10, an electron beam generating source 15 which is a specific example of an electron source, an electron gun control part 30 and a film formation control system 40 which are specific examples of a control part, a first film thickness sensor 8, and a second film thickness sensor 26. The indirect heating deposition apparatus 1 also includes a first shutter 6, a second shutter 27, and a substrate holding part 120 which holds a substrate 121 which is an object to be film-formed.
[0014] The liner 2 and holder 3, support member 5, adhesion-preventing cover 7, electron beam source 15, first film thickness sensor 8, second film thickness sensor 26, first shutter 6, second shutter 27, and substrate holder 120 are installed in a vacuum chamber 10.
[0015] The liner 2 is formed in a cylindrical shape with a bottom, and has a circular bottom 2a and a peripheral wall 2b that is continuous with the periphery of the bottom 2a. The liner 2 is made of a high melting point material such as molybdenum or tungsten. The liner 2 is filled with a deposition material 4. As the deposition material 4, a material that is meltable and has a small ionization tendency, such as gold (Au) or copper (Cu), is suitable.
[0016] Further, a groove is formed in the bottom 2a of the liner 2. A protrusion provided on a support member 5 described later fits into the groove formed in the bottom 2a. Note that a protrusion may be provided on the bottom 2a, and a groove into which the protrusion fits may be formed on the support member 5. The liner 2 is held by the holder 3 via the support member 5.
[0017] Although the liner 2 is formed in a cylindrical shape in the above example, the present invention is not limited to this. For example, the liner 2 may be formed in a square tube shape.
[0018] The support member 5 is formed in a cylindrical shape. The support member 5 has a bottom surface portion 5a, a side surface portion 5b continuous with the periphery of the bottom surface portion 5a, and a flange portion 5d. The bottom surface portion 5a is formed in a circular shape. An opening portion 5c is formed in the bottom surface portion 5a. The liner 2 is placed on the bottom surface portion 5a. The bottom portion 2a of the liner 2 is exposed from the opening portion 5c formed in the bottom surface portion 5a. As described above, the bottom surface portion 5a has a protrusion that fits into the groove portion provided in the bottom portion 2a. This makes it easy to position the liner 2 relative to the support member 5.
[0019] The flange portion 5d is formed on the upper end of the side surface portion 5b, which is the end opposite to the bottom surface portion 5a. The flange portion 5d protrudes radially outward from the upper end of the side surface portion 5b. The flange portion 5d abuts against the edge of a holding hole 3a of the holder 3, which will be described later.
[0020] In addition, the diameter of the side surface portion 5b of the support member 5 is set to be larger than the diameter of the peripheral wall portion 2b of the liner 2. Therefore, a gap is formed between the peripheral wall portion 2b of the liner 2 and the side surface portion 5b of the support member 5. This makes it difficult for heat from the liner 2 to be transferred to the holder 3, and prevents the temperature of the peripheral wall portion 2b of the liner 2 from decreasing.
[0021] The holder 3 is formed in a circular plate shape. The holder 3 has holding holes 3a through which the support member 5 passes. The holding holes 3a are formed in a circular shape, and the flange portion 5d of the support member 5 abuts against the edge of the holding holes 3a. The material of the holder 3 may be any material that has a large thermal resistance. Therefore, the heat of the liner 2 is not easily transferred to the holder 3.
[0022] Moreover, the number of holding holes 3a provided in the holder 3 is multiple, corresponding to the number of liners 2. However, the holder (container holding portion) according to the present invention may have one holding hole and hold one liner (container).
[0023] A rotary drive shaft 14, which is a specific example of a drive mechanism, is connected to the center of the holder 3. The rotation drive shaft 14 rotates the holder 3 to move the multiple liners 2 held by the holder 3 in the horizontal direction. The rotation drive shaft 14 is cooled so as not to impair its rotation function. The rotation drive shaft 14 is rotated by a rotation drive unit (not shown). The rotation drive unit is connected to a rotation control unit 43 of the film formation control system 40. The rotation drive unit is driven under the control of the rotation control unit 43 of the film formation control system 40, which will be described later.
[0024] The deposition-prevention cover 7 is formed in a substantially box-like shape and covers the holder 3 and the liner 2. The deposition-prevention cover 7 has an upper plate 7a and a side plate 7b continuous with the upper plate 7a. The upper plate 7a of the deposition-prevention cover 7 is formed with an evaporation opening 7c.
[0025] The evaporation opening 7c is formed at a position facing the substrate 121 held by the substrate holding part 120. Evaporation particles generated when the deposition material 4 is heated pass through the evaporation opening 7c of the deposition-preventing cover 7.
[0026] In addition, a first shutter 6 is disposed between the evaporation opening 7c and the substrate 121. The first shutter 6 is supported by a first opening / closing drive unit 18 so as to be able to open and close the evaporation opening 7c. The first opening / closing drive unit 18 is rotationally driven based on a control signal from the rotation control unit 43. The first shutter 6 is opened and closed as a result of the first opening / closing drive unit 18 being rotationally driven. When the first shutter 6 is closed, the evaporation particles that have passed through the evaporation opening 7c are blocked by the first shutter 6. When the first shutter 6 is opened, the evaporation particles that have passed through the evaporation opening 7c reach the substrate 121.
[0027] The substrate holding part 120 is disposed above the adhesion-preventing cover 7. The substrate holding part 120 is formed in a circular plate shape, and holds the substrate 121 on its lower surface. A rotary drive shaft is connected to the center of the upper surface of the substrate holding part 120. The rotary drive shaft rotates the substrate holding part 120, and moves the substrate 121 held by the substrate holding part 120 in the horizontal direction. The rotary drive shaft is cooled so as not to impair its rotation function.
[0028] When a deposition film is to be attached to the substrate 121, the substrate holding unit 120 is rotated by the rotary drive shaft to move the substrate 121 above the evaporation opening 7c. As a result, the substrate 121 faces the liner 2 arranged at a position facing the evaporation opening 7c. When the deposition material 4 filled in the liner 2 is heated and evaporated, the evaporated particles are deposited on the substrate 121. Note that, although the substrate holding unit 120 holds one substrate 121 in FIG. 1, the substrate holding unit 120 according to the present invention may hold a plurality of substrates.
[0029] A first film thickness sensor 8 for measuring the film thickness formed by the evaporated particles is disposed near a position facing the evaporation opening 7c in the substrate holding part 120. The first film thickness sensor 8 outputs the measured film thickness information to a film formation control system 40 described later. The film formation control system 40 measures the deposition rate and the accumulated film thickness (accumulated film thickness) based on the film thickness information obtained from the first film thickness sensor 8. Then, the film formation control system 40 outputs signals to the electron gun control part 30 and the rotation control part 43 so that the measured deposition rate becomes a preset deposition rate.
[0030] The second film thickness sensor 26 is disposed at a position diagonally above the liner 2 and away from the evaporation opening 7c. Specifically, the second film thickness sensor 26 is disposed at a position outside the deposition cover 7 that does not affect the inflow of vapor from the evaporation opening 7c to the substrate holder 120. The second film thickness sensor 26 measures the film thickness of the evaporated particles of the deposition material 4 that evaporates from the liner 2 and leaks out of the deposition cover 7. The second film thickness sensor 26 outputs the measured film thickness information to a film formation control system 40, which will be described later. The film formation control system 40 measures the deposition rate based on the film thickness information obtained from the second film thickness sensor 26. The film formation control system 40 outputs a signal to the electron gun control unit 30 and the rotation control unit 43 so that the measured deposition rate becomes a preset deposition rate.
[0031] A second shutter 27 that blocks evaporated particles proceeding toward the second film thickness sensor 26 is disposed near the second film thickness sensor 26. The second shutter 27 is supported so as to be openable and closable by a second opening and closing drive unit 28. The second opening and closing drive unit 28 is rotationally driven based on a control signal from the rotation control unit 43. The second shutter 27 is opened and closed as a result of the second opening and closing drive unit 28 being rotationally driven.
[0032] When the second shutter 27 is closed, it blocks evaporated particles proceeding from the liner 2 toward the second film thickness sensor 26. When the second shutter 27 is opened, evaporated particles generated from the liner 2 reach the second film thickness sensor 26. The second shutter 27 is disposed at a position away from the substrate holding part 120 and at a position where the opening and closing operation of the second shutter 27 does not affect the inflow of vapor from the evaporation opening 7c to the substrate holding part 120.
[0033] Moreover, in order to prevent the first shutter 6 from blocking the evaporated particles traveling from the liner 2 through the second shutter 27 toward the second film thickness sensor 26, it is necessary to set the position at which the first shutter 6 is provided high. In this case, it is preferable that the surface of the first shutter 6 that blocks the evaporated particles is large enough to block the evaporated particles traveling toward the first film thickness sensor 8 and the substrate 121.
[0034] Next, the electron beam source 15 will be described. The electron beam source 15 is disposed below the holder 3 at an arbitrary position on the rotation orbit of the liner 2. Thus, when the liner 2 held by the holder 3 via the support member 5 is disposed at the deposition position, the bottom 2a of the liner 2 is located above the electron beam source 15. The electron beam source 15 has a filament and a Wehnelt that forms an electric field distribution. An opening that exposes the filament is formed in the Wehnelt. The filament is formed of a wire made of tungsten material. A cathode power supply 16 and an acceleration power supply 17 that constitute the electron gun power supply are connected to this filament.
[0035] Cathode power supply 16 supplies a predetermined current to the cathode. Then, the cathode is heated by Joule heating to a temperature at which thermions can be emitted. Acceleration power supply 17 is grounded, and a negative high voltage with respect to the earth potential, for example, a voltage of 300V to 6kV, is applied. Holder 3 is at earth potential, and liner 2 held by holder 3 is at earth potential.
[0036] Then, after applying a negative high voltage to the electron beam generating source 15 by the acceleration power supply 17, the cathode is heated to a temperature at which thermions can be emitted, for example, to about 2300° C., whereby thermions are emitted from the cathode. The emitted thermions are accelerated by the electric field of the electron beam generating source 15, generating an electron beam 25. This electron beam 25 is irradiated onto the bottom 2 a of the liner 2.
[0037] When the bottom 2a of the liner 2 is electron impact heated by the electron beam 25, the temperature of the liner 2 rises. Then, the deposition material 4 is heated by conductive heat and radiation from the liner 2. When the electron impact heating of the bottom 2a of the liner 2 is continued for a certain period of time, the deposition material 4 sublimes or evaporates. The evaporated particles of the deposition material 4 pass through the evaporation opening 7c of the deposition cover 7 and proceed toward the substrate 121. As a result, the evaporated particles of the deposition material 4 are deposited on the substrate 121, and a deposition film of a desired thickness is attached to the substrate 121.
[0038] Next, the film formation control system 40 will be described. The film formation control system 40 includes a film thickness control unit 41, a deposition device control unit 42, and a rotation control unit 43. The film thickness control unit 41 is connected to the first film thickness sensor 8 and the second film thickness sensor 26, and acquires film thickness information from the first film thickness sensor 8 and the second film thickness sensor 26. The film thickness control unit 41 measures the deposition speed (deposition rate) and the accumulated film thickness based on the film thickness information acquired from the first film thickness sensor 8 and the second film thickness sensor 26. The film thickness control unit 41 performs feedback control so that the deposition speed approaches a set value, and outputs a signal to the electron gun control unit 30. As a result, the electron gun control unit 30 adjusts the electron current, thereby changing the deposition speed on the substrate 121.
[0039] Moreover, the film thickness control unit 41 is connected to the deposition apparatus control unit 42. Then, the film thickness control unit 41 outputs the measured cumulative film thickness information to the deposition apparatus control unit 42. The deposition apparatus control unit 42 is connected to the rotation control unit 43 and the electron gun control unit 30. The deposition apparatus control unit 42 outputs a control signal to the rotation control unit 43 and outputs setting conditions for the film formation process to the electron gun control unit 30. Furthermore, when the cumulative film thickness information acquired from the film thickness control unit 41 reaches a set film thickness value, the deposition apparatus control unit 42 outputs a control signal to the rotation control unit 43 and outputs an output stop signal to the electron gun control unit 30.
[0040] In addition, the rotation control unit 43 outputs drive signals to the first opening and closing drive unit 18 and the second opening and closing drive unit 28 based on a control signal from the deposition device control unit 42. Then, the first opening and closing drive unit 18 and the second opening and closing drive unit 28 perform the opening and closing operations of the first shutter 6 and the second shutter 27.
[0041] 1-2. Example of indirect heating evaporation equipment operation Next, an example of the operation of the indirect heating evaporation apparatus 1 having the above-mentioned configuration will be described with reference to FIG. Fig. 2 is a time chart showing an example of the operation of the indirect heating evaporation apparatus 1. The horizontal axis in Fig. 2 indicates elapsed time, the vertical axis (first axis) indicates the electron beam current of the electron beam generating source 15, and the vertical axis (second axis) indicates the evaporation rate (evaporation speed). The solid line indicates the electron beam current of the electron beam generating source 15. The dotted line indicates the evaporation rate measured by the first film thickness sensor 8, and the dashed-dotted line indicates the evaporation rate measured by the second film thickness sensor 26.
[0042] 2, the deposition device control unit 42 outputs a control signal to the electron gun control unit 30 to perform a preheating step of preheating the deposition material 4. Then, the electron gun control unit 30 controls the electron beam generating source 15 to irradiate the liner 2 with the electron beam 25. As a result, the electron beam 25 bombards the bottom 2a of the liner 2 with electrons. By irradiating the electron beam 25, the deposition material 4 accommodated in the liner 2 is preheated and melted.
[0043] At this time, the electron gun control unit 30 increases the electron beam current of the electron beam generation source 15 to the first pre-heating current in accordance with a program preset in the deposition device control unit 42. Then, the electron gun control unit 30 controls the output of the electron beam generation source 15 so that the output (electron beam current) of the electron beam generation source 15 becomes constant at the first pre-heating current.
[0044] Furthermore, when the output of the electron beam generating source 15 increases to the first pre-heating current and is maintained at the first pre-heating current, the deposition device control unit 42 outputs a control signal to the rotation control unit 43. Note that the timing for outputting the control signal from the deposition device control unit 42 to the rotation control unit 43 may be after a time set by a program has elapsed.
[0045] Next, the rotation control unit 43 drives the second opening / closing drive unit 28 to open the second shutter 27. Furthermore, the deposition device control unit 42 outputs a control signal to the electron gun control unit 30 to increase the output of the electron beam generation source 15. This causes the deposition material 4 contained in the liner 2 to evaporate, and evaporated particles are generated from the liner 2. Then, the evaporated particles generated from the liner 2 reach the second film thickness sensor 26 opened by the second shutter 27. Then, the evaporated particles generated from the liner 2 are measured by the second film thickness sensor 26. Also, the deposition rate measured by the second film thickness sensor 26 increases.
[0046] Next, the indirect heating deposition apparatus 1 performs an inner wall surface modification process of covering the inner wall surface of the liner 2 with the deposition material 4. In this inner wall surface modification process, film thickness information (deposition rate) measured by the second film thickness sensor 26 is output, i.e., fed back, to a film thickness control unit 41. Then, the film thickness control unit 41 outputs a control signal to the electron gun control unit 30 via the deposition apparatus control unit 42 so that the film thickness information (deposition rate) at the second film thickness sensor 26 becomes a first target rate set in advance. Then, the electron gun control unit 30 controls the electron beam generation source 15 based on the control signal from the film thickness control unit 41.
[0047] Here, the high melting point metal material constituting the liner 2 has a high surface energy per unit area, and when the surface is clean, it has the property of being easily wetted by liquid. However, in reality, the surface energy decreases as the surface oxidizes, and the wettability decreases. Therefore, when the evaporated deposition material 4 adheres to the inner wall of the liner 2 and liquefies, the contact angle with the liner 2 increases, and it is likely to exist in the form of droplets. The droplets that come into contact with the inner wall of the liner 2 are in a state where scattering and bumping easily occur, which is one of the causes of the generation of minute particles in the film formed on the substrate 121.
[0048] In contrast, the surface energy of the molten deposition material 4 generally decreases as its temperature increases, improving its wettability with the liner 2. When the molten deposition material 4 is further heated, the contact angle with the inner wall surface of the liner 2 approaches 0° as the temperature increases. As a result, the molten deposition material 4 creeps up the inner wall of the liner 2 due to capillary action, and the entire inner wall surface of the liner 2 is covered with the molten deposition material 4.
[0049] Thus, in the operation example of the indirect heating deposition apparatus 1 of this embodiment, during the preheating process of the deposition material 4, the deposition material 4 is heated with the second preheating current larger than the first preheating current, thereby performing an inner wall surface modification process of covering the inner wall surface of the liner 2 with the deposition material 4. Then, by covering the entire inner wall surface of the liner 2 with the deposition material 4, the wettability of the surface of the liner 2 can be improved. As a result, the contact angle on the surface of the liner 2 can be reduced, and the generation of droplets of the deposition material 4 on the surface of the liner 2 during the deposition process described below can be suppressed.
[0050] Furthermore, when the deposition material 4 is an element with a low ionization tendency, it is difficult to oxidize, and the surface energy per unit area can be maintained high. As a result, by performing the inner wall surface modification process on the liner 2 described above, the wettability of the surface of the liner 2 can be improved.
[0051] The liner 2 is supported by the support member 5 and is not in contact with the holder 3. A gap is formed between the peripheral wall portion 2b of the liner 2 and the side surface portion 5b of the support member 5. This makes it difficult for heat from the liner 2 to be transferred to the holder 3. As a result, a decrease in the temperature of the liner 2 can be prevented, and adhesion of droplets of the deposition material 4 to the inner wall of the liner 2 can be suppressed.
[0052] The first target rate of the second film thickness sensor 26 in the inner wall surface modification process needs to be set to a deposition rate at which the molten surface temperature of the deposition material 4 rises sufficiently. Therefore, as shown in Fig. 2, the film thickness control unit 41 controls the electron gun control unit 30 via the deposition device control unit 42 to increase the electron beam current (output) of the electron beam generation source 15 so as to achieve the first target rate. As a result, the second pre-heating current, which is the electron beam current (output) of the electron beam generation source 15 in the inner wall surface modification process, is increased more than the first pre-heating current.
[0053] When the evaporation rate measured by the second film thickness sensor 26 reaches the first target rate and a predetermined time set in the program has elapsed, the indirect heating evaporation apparatus 1 performs an evaporation rate stabilization step and an idling step before the evaporation step. In the evaporation rate stabilization step, the film thickness control unit 41 controls the electron gun control unit 30 via the evaporation apparatus control unit 42 so that the evaporation rate becomes the second target rate during the evaporation step.
[0054] That is, the film thickness control unit 41 outputs a signal to the electron gun control unit 30 so that the deposition rate measured by the second film thickness sensor 26 becomes the preset second target rate. The electron gun control unit 30 adjusts the electron current based on the signal from the film thickness control unit 41 to stabilize the deposition rate. In the example shown in Fig. 2, the electron gun control unit 30 reduces the electron beam current to be less than the second pre-heating current.
[0055] Here, the deposition rate measured by the first film thickness sensor 8 and the deposition rate measured by the second film thickness sensor 26 are determined by the relative position from the deposition source, and are generally related to each other by a cosine distribution. Therefore, by using the deposition rate measured by the second film thickness sensor 26, it is possible to approach the second target rate during the deposition process.
[0056] When the deposition rate reaches the second target rate during the deposition process and a predetermined time set by the deposition device control unit 42 has elapsed, an idling process is performed. Then, the deposition device control unit 42 outputs a control signal to the rotation control unit 43. Then, the rotation control unit 43 drives the second opening and closing drive unit 28 to close the second shutter 27, and drives the first opening and closing drive unit 18 to open the first shutter 6. As a result, the measurement value of the second film thickness sensor 26 becomes 0. On the other hand, the evaporated particles of the deposition material 4 pass through the evaporation opening 7c of the adhesion prevention cover 7 and reach the first film thickness sensor 8 arranged near the first shutter 6. Then, the film thickness control unit 41 measures the deposition rate (deposition speed) and the accumulated film thickness based on the film thickness information obtained from the first film thickness sensor 8.
[0057] The behavior of the deposition rate becomes unstable after the opening and closing operations of the first shutter 6 and the second shutter 27. During the idling process, the electron beam current is not controlled based on the deposition rate, but the film formation control system 40 outputs a control signal to the electron gun control unit 30 so as to maintain the electron beam current set in the deposition rate stabilization process for several seconds.
[0058] Next, when the idling step is completed, the indirect heating evaporation apparatus 1 performs the evaporation step. In the evaporation step, the film thickness control unit 41 measures the evaporation rate and the accumulated film thickness based on the film thickness information obtained from the first film thickness sensor 8. Then, the film thickness control unit 41 outputs a signal to the electron gun control unit 30 so that the measured evaporation rate is constant at a second target rate set in advance. The electron gun control unit 30 adjusts the electron current based on the signal from the film thickness control unit 41 to stabilize the evaporation rate. Note that, since the electron beam current is brought close to the second target rate by the evaporation rate stabilization step and the idling step, the evaporation rate can be made to quickly reach the second target rate.
[0059] The evaporated particles of the sublimated or evaporated deposition material 4 pass through the evaporation opening 7c, reach the substrate 121 held by the substrate holder 120, and adhere (deposit) thereon. This causes the evaporated particles to accumulate on the substrate 121, making it possible to form a desired film on the substrate 121.
[0060] Furthermore, the accumulated film thickness measured by the film thickness control unit 41 is output to the deposition device control unit 42. When the accumulated film thickness reaches a set film thickness value, the deposition device control unit 42 outputs a control signal to the rotation control unit 43. Then, the rotation control unit 43 drives the first opening and closing drive unit 18 to close the first shutter 6. Furthermore, the deposition device control unit 42 controls the electron gun control unit 30 to stop the irradiation of the electron beam 25 by the electron beam generation source 15. This completes the operation of the indirect heating deposition device 1.
[0061] 2. Second embodiment Next, an indirect heating evaporation apparatus according to a second embodiment will be described with reference to FIGS. Fig. 3 is a schematic diagram of an indirect heating evaporation device according to a second embodiment. Fig. 4 is a diagram showing an example of a scanning coil current waveform. And Fig. 5 is a time chart showing an example of the operation of the indirect heating evaporation device according to the second embodiment.
[0062] The indirect heating evaporation apparatus 1B according to the second embodiment differs from the indirect heating evaporation apparatus 1 according to the first embodiment in that a scanning coil is provided in the electron beam generating source 15. Therefore, here, the parts common to the indirect heating evaporation apparatus 1 according to the first embodiment are denoted by the same reference numerals and redundant explanations will be omitted.
[0063] As shown in FIG. 3, the indirect heating evaporation apparatus 1B includes a cathode power supply 16 and an acceleration power supply 17 connected to an electron beam generating source 15, a scanning coil 21, a block 22, an anode 24, and a scanning coil current waveform control unit 32.
[0064] The scanning coil 21 is disposed near the electron beam generating source 15. The scanning coil 21 is housed in a cooled block 22. A scanning coil current waveform control unit 32 is connected to the scanning coil 21. The scanning coil current waveform control unit 32 controls the waveform of the current supplied to the scanning coil 21 (hereinafter referred to as the "scanning coil current waveform"). That is, the scanning coil current waveform control unit 32 controls the scanning coil 21 and adjusts the coil current waveform.
[0065] Furthermore, the scan coil current waveform control unit 32 is connected to the electron gun control unit 30. The electron gun control unit 30 outputs a signal received from the film formation control system 40 according to the status of the deposition operation to the scan coil current waveform control unit 32. Then, the scan coil current waveform control unit 32 changes the coil current waveform based on the signal output from the film formation control system 40 via the electron gun control unit 30.
[0066] In addition, an anode 24 having an opening is fixed to the upper surface of the block 22. The anode 24 is disposed between the bottom 2a of the liner 2 and the electron beam generating source 15, and the opening of the anode 24 faces the electron beam generating source 15 at a predetermined distance. The anode 24 is made of a high melting point material since it is subject to a strong thermal load due to radiant heat and reflected electrons from the liner 2. The scanning coil 21 is disposed on the side of the anode 24 facing the liner 2. The scanning coil 21 generates an AC magnetic field when a current flows through it.
[0067] When a predetermined current is supplied to the filament, the filament is heated by Joule heating to a temperature at which thermoelectrons can be supplied, for example, around 2300° C. When a negative high voltage with respect to the earth potential is applied by the acceleration power supply 17, thermoelectrons emitted from the filament are accelerated by the electric field between the electron beam generating source 15 and the anode 24, generating an electron beam 25. This electron beam 25 is deflected by an AC magnetic field generated by the scanning coil 21, and is irradiated onto the liner 2 in a predetermined scanning pattern.
[0068] 2-2. Example of indirect heating evaporation equipment operation Next, an example of the operation of the indirect heating evaporation apparatus 1B having the above-mentioned configuration will be described with reference to FIGS.
[0069] 5, in the preheating step, the deposition rate stabilization step, the idling step, and the deposition step, the current value supplied to the scanning coil 21 is 0 A. Therefore, in the preheating step, the deposition rate stabilization step, the idling step, and the deposition step, the electron beam 25 is not scanned and is irradiated onto the entire bottom portion 2a of the liner 2, as in the indirect heating deposition apparatus 1 according to the first embodiment.
[0070] 4 and 5, in the inner wall surface modification process, the film formation control system 40 outputs a signal to the scanning coil current waveform control unit 32 via the electron gun control unit 30. Then, the scanning coil current waveform control unit 32 changes the coil current waveform based on the signal output from the film formation control system 40.
[0071] 4, the scanning coil current waveform at this time is set to a ring shape in accordance with the shape of the bottom 2a of the liner 2. Therefore, the electron beam 25 is not irradiated to the center of the bottom 2a, but is irradiated intensively only to the outer edge of the bottom 2a. This makes it possible to efficiently heat the peripheral wall 2b of the liner 2, and to efficiently heat the inner wall surface of the liner 2 and the deposition material 4 in contact with the inner wall surface.
[0072] By efficiently heating the inner wall surface of the liner 2, as shown in Fig. 2 and Fig. 5, the electron beam current in the inner wall surface modification step can be reduced more than that in the indirect heating evaporation apparatus 1 according to the first embodiment. Furthermore, evaporated particles of the evaporation material 4 generated during the inner wall surface modification step do not contribute to the film formation on the substrate 121 and are lost. In contrast, when heating only the outer edge portion of the liner 2 intensively as in the indirect heating evaporation apparatus 1B according to the second embodiment, the loss of the evaporation material 4 can be suppressed compared to when the center portion of the bottom portion 2a of the liner 2 is heated.
[0073] Other configurations are the same as those of the indirect heating evaporation apparatus 1 according to the first embodiment, and therefore description thereof will be omitted. The indirect heating evaporation apparatus 1B according to the second embodiment can also provide the same effects as those of the indirect heating evaporation apparatus 1 according to the first embodiment described above.
[0074] 3. Relationship between electron beam current and remaining amount of deposition material Next, the relationship between the electron beam current and the remaining amount of the deposition material will be described with reference to FIG. 6. FIG. 6 is a diagram showing the relationship between the electron beam current and the remaining amount of the deposition material. The vertical axis in FIG. 6 indicates the electron beam current, and the horizontal axis indicates the remaining amount of the deposition material. The triangles in FIG. 6 indicate an example in which the deposition material 4 is gold (Au) without a scanning coil (the indirect heating deposition apparatus 1 according to the first embodiment). The circles indicate an example in which the deposition material 4 is gold (Au) with a scanning coil (the indirect heating deposition apparatus 1B according to the second embodiment). The squares indicate an example in which the deposition material 4 is copper (Cu) without a scanning coil (the indirect heating deposition apparatus 1 according to the first embodiment). And the diamonds indicate an example in which the deposition material 4 is copper (Cu) with a scanning coil (the indirect heating deposition apparatus 1B according to the second embodiment).
[0075] Here, the heat capacity of the deposition material 4 depends on the amount stored in the liner 2. Therefore, as shown in FIG. 6, when the remaining amount of the deposition material 4 is small, the electron beam current needs to be lowered, and when the remaining amount of the deposition material 4 is large, the electron beam current needs to be increased. In contrast, in the indirect heating deposition apparatus 1, 1B of this embodiment, as described above, in the inner wall surface modification process, the film thickness control unit 41 controls the electron gun control unit 30 so that the deposition rate is constant based on the film thickness information measured by the second film thickness sensor 26. That is, in the inner wall surface modification process, the deposition rate corresponding to the molten surface temperature of the deposition material 4 is constant by the film thickness control unit 41. As a result, even if the remaining amount of the deposition material 4 changes, the molten surface temperature of the deposition material 4 for obtaining the effect of suppressing the generation of droplets can be maintained, and the inner wall surface of the liner 2 can be reliably covered with the deposition material 4.
[0076] The present invention is not limited to the embodiment described above and shown in the drawings, and various modifications can be made without departing from the spirit of the invention described in the claims.
[0077] In the above-described embodiment, the second film thickness sensor 26 is disposed outside the adhesion-prevention cover 7, but the present invention is not limited to this. For example, the second film thickness sensor 26 may be disposed inside the adhesion-prevention cover 7. Also, the second shutter 27 does not have to be provided.
[0078] Furthermore, although an example has been described in which the film thickness on the substrate 121 during the deposition process is detected using the value measured by the first film thickness sensor 8, the present invention is not limited to this. The electron gun control unit 30 may be controlled based on film thickness information measured by the second film thickness sensor 26 without providing the first film thickness sensor 8, and the deposition rate during the deposition process and the film thickness accumulated on the substrate 121 may be measured. Note that the measurement accuracy of the film thickness can be improved by using the first film thickness sensor 8 arranged closer to the substrate 121 than the second film thickness sensor 26.
[0079] In this specification, the words "parallel" and "orthogonal" are used, but these do not mean only "parallel" and "orthogonal" in the strict sense, but may also mean a "substantially parallel" or "substantially orthogonal" state that includes "parallel" and "orthogonal" and is within a range in which the respective functions can be exerted. [Explanation of symbols]
[0080] REFERENCE SIGNS LIST 1, 1B...indirect heating evaporation device, 2...liner (container), 2a...bottom, 2b...circumferential wall, 3...holder, 3a...holding hole, 4...evaporation material, 5...support member, 5a...bottom surface, 5b...side surface, 5c...opening, 5d...flange, 6...first shutter, 7...adhesion prevention cover, 7a...upper surface plate, 7b...side surface plate, 7c...evaporation opening, 8...first film thickness sensor, 10...vacuum chamber, 15...electron beam source, 16...cathode power supply, 17...acceleration power supply, 18...first opening / closing drive unit, 21...scanning coil, 22...block, 24...anode, 25...electron beam, 26...second film thickness sensor, 27...second shutter, 28...second opening / closing drive unit, 30...electron gun control unit, 32: Scanning coil current waveform control unit; 40: Film formation control system; 41: Film thickness control unit; 42: Deposition device control unit; 43: Rotation control unit; 120: Substrate holding unit; 121: Substrate
Claims
1. A container filled with a deposition material; an electron beam generating source that irradiates a container filled with the deposition material with an electron beam that evaporates the deposition material; a control unit for controlling the electron beam generation source, The control unit is a preheating step of preheating the deposition material before a deposition step of controlling the electron beam generating source to deposit the deposition material on a substrate; During the preheating step, an electron beam current of the electron beam generating source is set to a first preheating current; Thereafter, the electron beam current of the electron beam generating source is set to a second preheating current that is higher than the first preheating current, and an inner wall surface modification step is performed in which the inner wall surface of the container is covered with the molten deposition material. Indirect heating vapor deposition equipment.
2. a film thickness sensor that measures a film thickness of evaporated particles of the deposition material evaporated from the container, The control unit has a film thickness control unit that controls an electron beam current of the electron beam generation source based on film thickness information measured by the film thickness sensor.
2. The indirect heating deposition apparatus of claim 1.
3. The film thickness control unit controls the electron beam current of the electron beam generation source so that film thickness information from the film thickness sensor becomes a first target rate set in advance during the inner wall surface modification process.
3. The indirect heating deposition apparatus according to claim 2.
4. The film thickness sensor includes: a first film thickness sensor that measures a film thickness of evaporated particles of the deposition material evaporated from the container during the deposition process; a second film thickness sensor that measures a film thickness of evaporated particles of the deposition material evaporated from the container during the inner wall surface modification process.
4. The indirect heating deposition apparatus according to claim 3.
5. The film thickness control unit controls the electron beam current of the electron beam generation source so that film thickness information from the second film thickness sensor or the first film thickness sensor becomes a second target rate set in advance after the inner wall surface modification process.
5. The indirect heating deposition apparatus according to claim 4.
6. a first shutter that blocks the evaporated particles traveling toward the first film thickness sensor and the substrate; a second shutter that blocks the evaporated particles traveling toward the second film thickness sensor; a first opening / closing drive unit that supports the first shutter so as to be openable and closable; a second opening / closing drive unit that supports the second shutter so as to be openable and closable; 5. The indirect heating deposition apparatus according to claim 4.
7. a scanning coil for scanning the electron beam emitted from the electron beam generating source, The control unit controls the scanning coil during the inner wall surface modification step to irradiate the electron beam onto an outer edge portion of the bottom of the container.
2. The indirect heating deposition apparatus of claim 1.
8. The control unit controls an electron beam current of the electron beam generating source in the inner wall surface modification process according to an amount of the deposition material remaining in the container.
2. The indirect heating deposition apparatus of claim 1.
9. A method for controlling an indirect heating evaporation apparatus including: a container filled with an evaporation material; an electron beam generating source for irradiating the container filled with the evaporation material with an electron beam for evaporating the evaporation material; and a control unit for controlling the electron beam generating source, a preheating step of preheating the deposition material by controlling the electron beam generating source; a deposition step of controlling the electron beam generating source after the preheating step to deposit the deposition material on a substrate, During the preheating step, an electron beam current of the electron beam generating source is set to a first preheating current to preheat the deposition material; Thereafter, the electron beam current of the electron beam generating source is set to a second preheating current that is higher than the first preheating current, and an inner wall surface modification step is performed in which the inner wall surface of the container is covered with the molten adhesion material. A method for controlling an indirect heating evaporation apparatus.
Citation Information
Patent Citations
Indirect heating vapor deposition apparatus
JP2022068958A