Accelerated deterioration test method for coating film
By embedding a test piece in corrosive dust and controlling moisture absorption and drying cycles, the method addresses the inadequacy of conventional tests in simulating paint film deterioration in corrosive environments, achieving rapid and accurate evaluation of paint film performance.
Patent Information
- Application Number
- JP2023050414
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-27
- Publication Date
- 2024-10-09
- Estimated Expiration
- 2043-03-27
AI Technical Summary
Conventional paint film deterioration acceleration tests fail to adequately reproduce the deterioration of paint films in corrosive dust environments, which are characterized by faster corrosion rates due to corrosive components and moisture.
A method involving embedding a test piece with a coating film in corrosive dust, spraying water to impregnate it, and controlling temperature and humidity to accelerate moisture absorption and drying cycles, simulating the corrosive dust environment.
The method effectively reproduces the deterioration of paint films in corrosive dust environments, providing a high correlation with real-world conditions and reducing the time required for evaluating paint film performance.
Smart Images

Figure 2024139463000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for accelerated deterioration testing of coating films. [Background technology]
[0002] In steelworks, raw materials such as ore, coal, and coke are unloaded and transported using conveyor belts to produce crude steel. During this process, raw materials may spill off the belt (conveyor belt) and accumulate as dust on the conveyor belt and / or the frame of the rack. Such dust (also called "corrosive dust") contains corrosive components such as sulfur components and is therefore highly corrosive to metal plates such as steel plates that form the building structure.
[0003] The dust accumulated on the structure absorbs moisture when water is supplied from rainfall or the like. In this case, due to the corrosive components of the dust and the increased time that the dust remains wet, corrosion of the structure progresses up to 10 times faster than in a typical outdoor environment.
[0004] In order to prevent corrosion of the framework, it is effective to use stainless steel for the members constituting the framework, but this is not practical in terms of cost, so for example, members made of low carbon steel with the surface covered with a paint film are used. Since the deterioration of a coating film takes a long time to progress, the performance of the coating film is evaluated by a coating film deterioration acceleration test, which artificially accelerates the deterioration of the coating film (see Patent Document 1). [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2008-185502 A Summary of the Invention [Problem to be solved by the invention]
[0006] Conventional coating deterioration accelerated tests are designed to simulate deterioration of coatings under general outdoor exposure environments, and therefore cannot adequately reproduce deterioration of coatings in corrosive dust environments. Therefore, an object of the present invention is to provide a method for accelerated deterioration testing of a coating film, which can adequately reproduce deterioration of the coating film in a corrosive dust environment. [Means for solving the problem]
[0007] As a result of extensive investigations, the present inventors have found that the above object can be achieved by employing the following configuration, and have completed the present invention. That is, the present invention provides the following [1] to [7]. [1] A method for accelerating deterioration of a coating film, comprising: an embedding step of embedding a test piece having a coating film disposed on the surface of a metal plate in corrosive dust containing a corrosive component to bring the coating film into contact with the corrosive dust; a spraying step of spraying water onto the corrosive dust to cause the corrosive dust to absorb moisture; a wetting step of increasing the temperatures of the test piece and the corrosive dust to promote absorption of the moisture in the corrosive dust by the coating film; and a drying step of drying the test piece and the corrosive dust. [2] The accelerated deterioration test method for a coating film according to the above [1], wherein the corrosive component is a sulfur component. [3] The accelerated deterioration test method for a coating film according to [1] or [2] above, wherein the water sprayed in the spraying step is pure water. [4] The method for accelerated deterioration testing of a coating film according to any one of [1] to [3] above, wherein in the spraying step, the water content of the corrosive dust is saturated. [5] The accelerated deterioration test method for a coating film according to any one of the above [1] to [4], wherein the metal plate is a steel plate. [6] The coating film deterioration acceleration test method according to any one of [1] to [5] above, wherein the spraying step, the wetting step and the drying step are carried out under the following conditions, respectively: The above spraying process: Temperature 25-60℃, time 8-16 hours The above moistening process: temperature 40-60℃, relative humidity 90-100%, time 8-16 hours The drying process: Temperature 50-70℃, relative humidity 45-55%, time 20-28 hours [7] The coating film deterioration acceleration test method according to any one of [1] to [6] above, wherein the spraying step, the wetting step and the drying step are carried out under the following conditions, respectively: The above spraying process: Temperature 35℃, time 12h The above humidification process: temperature 50℃, relative humidity 95%, time 12 hours The above drying process: Temperature 60℃, relative humidity 50%, time 24 hours Effect of the Invention
[0008] According to the present invention, deterioration of a coating film in a corrosive dust environment can be sufficiently reproduced. [Brief description of the drawings]
[0009] [Figure 1] FIG. 2 is a cross-sectional view showing a schematic diagram of a testing machine used in a coating deterioration acceleration test. [Diagram 2] 1 is a graph showing the relationship between the diffusion coefficient of a coating film and temperature. [Diagram 3] 1 is a graph showing the results of a water absorption and drying behavior test. [Figure 4] 1 is a graph showing the relative life spans of test pieces for standard use and specifications 1 to 3. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] FIG. 1 is a cross-sectional view that illustrates a test machine 7 used in a coating deterioration acceleration test. First, the test box 1 and the dust tray 2 arranged inside the test machine 7 will be described. The test box 1 is a container with an open top and a drain hole 6, which is a through hole, formed in the bottom. The material of the test box 1 is, for example, a resin such as polypropylene. The test box 1 shown in Fig. 1 has a rectangular parallelepiped shape, but the shape of the test box 1 is not limited to this.
[0011] The dust collector 2 is a container with an open top, similar to the test box 1. However, the dust collector 2 has no through-hole formed in the bottom surface. The material, shape, etc. of the dust collector 2 may be the same as those of the test box 1. The dust collector 2 shown in FIG.
[0012] 1, first, a dust collector 2 is placed on the inner bottom surface of a tester 7, and a test box 1 is placed on top of the dust collector 2. Next, a net 5 is placed on the bottom surface of the test box 1. The material of the net 5 is, for example, a resin such as polypropylene. A part of the dust 4 is spread on the net 5 as bedding material. Next, the test piece 3 is placed on the bedding material (dust 4). After that, the remaining dust 4 is placed inside the test box 1 to cover the test piece 3. In this way, the dust 4 is contained inside the test box 1 with the test piece 3 buried inside.
[0013] The dust 4 is corrosive dust containing corrosive components such as sulfur components, and originates from raw materials such as ore, coal, and coke that are transported by belt conveyers in a steelworks to produce crude steel, for example. Specifically, among these raw materials, those that fall off the belt during transportation and accumulate on the frame of the belt conveyor or the like can be used as the corrosive dust. For example, dust derived from coke (coke dust) contains sulfur components as corrosive components.
[0014] The test piece 3 is assumed to be a part of a member constituting the frame of a belt conveyor or the like, and has a metal plate and a coating film disposed on its surface (one side or both sides). Examples of the metal plate include conventionally known steel plates used for the frame, and specific examples thereof include low carbon steel plates such as SS material (rolled steel for general structure), SM material (rolled steel for welded structure), etc. SPCC material (cold rolled steel plate), which has almost the same composition as these low carbon steel plates, may also be used. As the paint to be applied to the coating film, for example, a conventionally known paint such as a modified epoxy resin paint, a polyurethane resin paint, a silicone resin paint, an organic zinc-rich paint, or an inorganic zinc-rich paint may be appropriately used, and a commercially available product may also be used. The coating film may be a multi-layer coating film formed by sequentially applying two or more types of coating material. The thickness of the coating film (film thickness) is, for example, 100 to 400 μm, but is not limited to this.
[0015] Incidentally, since the test box 1 has a drain hole 6, which is a through hole, formed in the bottom surface thereof, the dust 4 contained inside the test box 1 can fall through the drain hole 6. However, since a net 5 is placed on the bottom surface of the test box 1, the dust 4 is prevented from falling by the net 5. For this reason, it is preferable to appropriately select a size and shape for the mesh of the net 5 that makes it difficult for the dust 4 to pass through.
[0016] A spraying device 8 is provided on the upper surface side inside the testing machine 7. The spraying device 8 sprays water 9 downward. As the water 9, pure water is used instead of salt water. The test machine 7 may be any machine capable of driving the spraying equipment 8 and appropriately changing the internal conditions such as temperature and humidity, and may be, for example, a test machine conforming to JIS K 5600-7-9 (such as a CCT test machine).
[0017] In such a configuration, to conduct a coating deterioration acceleration test, first, as described above, the test piece 3 is embedded in the dust 4 contained in the test box 1, and the coating of the test piece 3 is brought into contact with the dust 4 (embedding process).
[0018] In this state, the spraying equipment 8 of the test machine 7 is driven to spray water 9 onto the dust 4 contained in the test box 1, thereby moistening the dust 4 (spraying step). In the spraying step, it is preferable to moisten the dust 4 until the moisture content of the dust 4 becomes saturated. In the spraying step, not only the dust 4 but also the coating film of the test piece 3 may be moistened. Excess water 9 that is not absorbed by the dust 4 passes through drainage holes 6 formed in the bottom surface of the test box 1 and falls into the dust receiver 2.
[0019] Furthermore, the temperature inside the testing machine 7 (i.e., the test piece 3 and the dust 4) is raised above room temperature (e.g., 25°C) to cause the moisture in the dust 4 to be absorbed into the coating film of the test piece 3 and promote this absorption (wetting process). The spraying step and the wetting step may be the same step. Thereafter, the test piece 3 (particularly the coating film) and the dust 4 are dried (drying step).
[0020] Here, the reasons for carrying out the spraying step, the wetting step and the drying step will be explained.
[0021] First, we define an environment with precipitation >0 mm / h or relative humidity (RH) >80% as a "wet" environment, while an environment that does not meet the wetness criteria as a "dry" environment. The coating on the test specimen absorbs water in a wet environment and dries in a dry environment.
[0022] The present inventors placed the coating film in a constant temperature and humidity chamber while in contact with water, and measured the change in coating mass over time at each temperature in a wet environment and a dry environment to determine the water content of the coating film. Furthermore, the diffusion coefficient D (unit: m 2 / s). (M t / M ∞ ) = (4 / L) × (Dt / π) 2 t: Elapsed time (unit: s) M t : Moisture content of coating film at elapsed time t M ∞ : Saturation moisture content of coating film L: Coating thickness (unit: m) D: Diffusion coefficient (unit: m / s 2 )
[0023] FIG. 2 is a graph showing the relationship between the diffusion coefficient of a coating film and temperature. As shown in Figure 2, the diffusion coefficient increases with increasing temperature, both when the coating film absorbs water and when it dries. When comparing at the same temperature, the diffusion coefficient tends to be larger when the coating film is drying than when the coating film absorbs water. When a coating absorbs water, the water molecules penetrate into the coating while expanding the polymer network of the coating, which is made of polymers, so the diffusion coefficient is considered to be relatively small. On the other hand, when a coating dries, the water molecules are expelled from the expanded polymer network, so the diffusion coefficient is considered to be relatively large. Considering such differences in diffusion coefficients, it is clear that the water absorption behavior is significantly affected by the duration of the wet environment (continuous wetting time).
[0024] In the real environment, the continuous wet period is often 24 to 48 hours. Therefore, from the viewpoint of reproducing the real environment, a test (water absorption and drying behavior test) was conducted in which a test piece buried in dust was exposed to a wet environment that met the following conditions, and then exposed to a dry environment that met the following conditions. Wet environment: Temperature 25℃, relative humidity 95%, time 48h Dry environment: Temperature 30℃, relative humidity 60%, time 120h
[0025] Figure 3 is a graph showing the results of the water absorption and drying behavior test. The horizontal axis shows the elapsed time (unit: h), and the vertical axis shows the moisture saturation rate of the coating film and dust. The moisture saturation rate is the ratio of the moisture content at each elapsed time to the saturated moisture content. In the water absorption and drying behavior test, water was first supplied to the dust in which the test specimen was embedded at the start of the wet environment. The dust layer was set to a thickness of 35 mm, simulating the dust that accumulates on the structure of a belt conveyor transporting coke. In a wet environment, not only the coating film but also the dust absorbs water. For this reason, as shown in Figure 3, even after the environment is changed to a dry environment, the coating film continues to absorb the moisture from the dust until a certain time has elapsed, and the coating film continues to absorb water (the moisture saturation rate of the coating film increases).
[0026] Based on the relationship between the diffusion coefficient of the coating film and temperature (FIG. 2) and the results of the water absorption and drying behavior test (FIG. 3), the inventors came up with the idea of carrying out the above-mentioned spraying step, wetting step and drying step. By carrying out these steps, the water absorption and drying behavior of the coating film and dust in an actual environment can be reproduced, making it possible to sufficiently reproduce the deterioration of the coating film in a corrosive dust environment in a short period of time while having a high correlation with the actual environment.
[0027] The conditions of temperature, humidity, time, etc. for the spraying step, wetting step, and drying step are appropriately set based on the properties of the coating film, but it is preferable to carry out each step under the following conditions, which allows the deterioration of the coating film in a corrosive dust environment to be more fully reproduced (see [Examples] below).
[0028] The temperature in the spraying step is preferably 25 to 60° C., more preferably 30 to 40° C., and even more preferably 35° C. The time for the spraying step is preferably 8 to 16 hours, more preferably 10 to 14 hours, and even more preferably 12 hours. The temperature in the moistening step is preferably 40 to 60° C., more preferably 45 to 55° C., and even more preferably 50° C. The relative humidity in the moistening step is preferably 90 to 100%, more preferably 93 to 98%, and even more preferably 95%. The duration of the moistening step is preferably 8 to 16 hours, more preferably 10 to 14 hours, and even more preferably 12 hours. The temperature in the drying step is preferably 50 to 70° C., more preferably 55 to 65° C., and even more preferably 60° C. The relative humidity in the drying step is preferably 45 to 55%, more preferably 48 to 53%, and even more preferably 50%. The time for the drying step is preferably 20 to 28 hours, more preferably 22 to 26 hours, and even more preferably 24 hours. EXAMPLES
[0029] The present invention will be specifically described below with reference to examples, although the present invention is not limited to the examples described below.
[0030] First, the dust and the test specimen were prepared. As the dust, coke dust containing a sulfur component was used. The metal plate of the test specimen was a steel plate (cold-rolled steel plate) of SPCC material that had been subjected to a blasting treatment. The paint shown in Table 1 below was applied to this steel plate to form a coating film, and test specimens of the standard specification and specifications 1 to 3 were obtained. The test pieces were processed to have artificial defects before being subjected to the tests described below.
[0031] [Table 1]
[0032] A coating deterioration accelerated test was carried out using the test machine explained based on FIG. 1 (a test machine conforming to JIS K 5600-7-9). That is, while the test piece was buried in the dust, pure water was sprayed from the spraying equipment (spraying process). Next, the temperature inside the testing machine was raised to promote the absorption of the moisture in the dust by the coating film (wetting process). After that, the test piece and dust were dried (drying process). The spraying step, the wetting step and the drying step were carried out under the following conditions. ·Spraying process: Temperature 35℃, time 12h Wetting process: Temperature 50℃, relative humidity 95%, time 12h Drying process: Temperature 60℃, relative humidity 50%, time 24 hours In order to shorten the time for the spraying process, the dust thickness was set to 10 mm. In the spraying process, the amount of pure water sprayed was 3±1 mL / h / 80 cm. 2 Then, pure water was sprayed onto the dust until the moisture content of the dust reached saturation.
[0033] In addition to the above-mentioned accelerated deterioration test of the coating film, a field exposure test was also conducted in which the test specimens were buried in dust (thickness: 35 mm) and exposed to actual outdoor conditions. After the test, the blister area of the artificial defect in the test piece was measured, and the ratio of the blister area to the blister area of the standard specification was calculated as the relative life. FIG. 4 is a graph showing the relative life span of the test pieces for standard use and specifications 1 to 3. As shown in Figure 4, the relationship between the relative life spans of the standard specification and specifications 1 to 3 was almost consistent between the example and the field exposure test. That is, the coating deterioration accelerated test of the example was able to sufficiently reproduce the deterioration of the coating in a corrosive dust environment in a short period of time while having a high correlation with the actual environment. [Explanation of symbols]
[0034] 1: Test box 2: Dust collector 3: Test piece 4: Dust (corrosive dust) 5: Net 6: Water drainage hole 7: Testing machine 8: Spray equipment 9:Water
Claims
1. an embedding step of embedding a test piece having a coating film disposed on a surface of a metal plate in corrosive dust containing a corrosive component to bring the coating film into contact with the corrosive dust; a spraying step of spraying water onto the corrosive dust to moisten the corrosive dust; a wetting step of increasing the temperature of the test piece and the corrosive dust to promote absorption of moisture from the corrosive dust by the coating; a drying step of drying the test piece and the corrosive dust; The accelerated deterioration test method for a coating film comprises:
2. The method for accelerated deterioration testing of a coating film according to claim 1 , wherein the corrosive component is a sulfur component.
3. The method for accelerated deterioration testing of a coating film according to claim 1 or 2, wherein the water sprayed in the spraying step is pure water.
4. 3. The accelerated deterioration test method for a coating film according to claim 1, wherein in the spraying step, a moisture content of the corrosive dust is saturated.
5. The method for accelerated deterioration testing of a coating film according to claim 1 or 2, wherein the metal plate is a steel plate.
6. The method for accelerated deterioration testing of a coating film according to claim 1 or 2, wherein the spraying step, the wetting step and the drying step are carried out under the following conditions, respectively. The spraying step: temperature 25 to 60°C, time 8 to 16 hours The moistening step: temperature 40-60°C, relative humidity 90-100%, time 8-16 hours The drying step: temperature 50 to 70° C., relative humidity 45 to 55%, time 20 to 28 hours
7. The method for accelerated deterioration testing of a coating film according to claim 1 or 2, wherein the spraying step, the wetting step and the drying step are carried out under the following conditions, respectively. The spraying step: temperature 35° C., time 12 hours The moistening step: temperature 50° C., relative humidity 95%, time 12 hours Drying step: temperature 60° C., relative humidity 50%, time 24 hours
Citation Information
Patent Citations
Indoor soil corrosion simulator
CN201653876U
Experimental indoor accelerated test device of simulation soil corrosion
CN206772789U
Underground-environment testing apparatus
JP1990291945A
Coating composition
JP2006348109A
Corrosion resistance evaluation method of coated steel product, and compound corrosion resistance evaluation method of coated steel product
JP2008261813A