Holding pad and method for manufacturing the same

The holding pad with convex portions on a photocurable resin layer addresses the challenge of maintaining appropriate holding force and easy detachment, ensuring stable adhesion and reducing polishing complications.

JP2024141511APending Publication Date: 2024-10-10FUJIBO HLDG
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2023053206
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-29
Publication Date
2024-10-10

AI Technical Summary

Technical Problem

Existing holding pads for polishing processes face challenges in maintaining appropriate holding force while ensuring easy attachment and detachment of objects, often leading to complications in the peeling process and potential damage during polishing.

Method used

A holding pad with a holding layer featuring a plurality of convex portions arranged in a dot shape on the surface, integrated with a frame member, utilizing a photocurable resin to adjust suction force and facilitate easy separation, manufactured through a method involving a masking process and solvent washing.

Benefits of technology

The holding pad provides stable adhesion and easy release of polished objects, minimizing damage and process complexity, thereby enhancing the efficiency and reliability of polishing operations.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024141511000001_ABST
    Figure 2024141511000001_ABST
Patent Text Reader

Abstract

To provide a holding pad which facilitates attachment / detachment of a polished object, while maintaining holding force with respect to the polished object.SOLUTION: A holding pad includes a holding layer for holding a polished object, wherein the holding layer integrally has a holding surface, and a plurality of projections are arranged in a dot shape on the holding surface.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a holding pad for holding an object to be polished and a manufacturing method thereof, and more particularly to a holding pad capable of suitably holding an object to be polished when polishing a semiconductor wafer or the like, and a manufacturing method thereof. [Background technology]

[0002] Chemical mechanical polishing (CMP) is commonly used as a polishing method for flattening the surfaces of optical materials, semiconductor wafers, semiconductor devices, substrates for hard disks, silicon wafers, and sapphire glass. The CMP method will be described with reference to Fig. 1. Fig. 1 is a cross-sectional view of a polishing apparatus for carrying out the CMP method, in which an object to be polished W is sandwiched between a polishing pad 3 provided on a polishing platen 4 and a holding pad 10 provided on a holding platen 2, and is rotated while being pressed, thereby polishing the object to be polished W. The holding pad 10 is provided with a frame-shaped member 12, enabling efficient polishing. During polishing, a slurry is supplied between the polishing pad 3 and the workpiece W. The slurry is supplied to the polishing surface through grooves or holes and then discharged. The slurry is a mixture (dispersion liquid) of water, various chemical components, and hard fine abrasive grains, and as the chemical components and abrasive grains are flowed, they move relative to the workpiece W, thereby increasing the polishing effect (see Patent Document 1).

[0003] The holding pad is required to have the holding power (adhesive power) to hold the object to be polished so that it does not slip or fall off during the polishing process. However, if the holding power of the object to be polished is increased, it may take a long time to remove the object after polishing, and there is also a risk of damaging the object during the removal process. Therefore, a holding pad with an appropriate adhesive power is required. For example, in Patent Documents 2 and 3, the adsorptive power is adjusted by disposing a protective layer, in which holes or grooves are partially formed, on the surface of the skin layer of a porous polyurethane sheet. However, in the methods of Patent Documents 2 and 3, if the protective layer peels off, the adsorption force varies, which may cause the polished object to fall off. In addition, the manufacturing process becomes complicated because a porous polyurethane sheet or the like is first formed and then a protective layer is placed on the surface of the sheet. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Patent Publication No. 2020-28930 [Patent Document 2] Patent Publication No. 2012-71366 [Patent Document 3] Patent Publication No. 2012-71399 Summary of the Invention [Problem to be solved by the invention]

[0005] The present invention provides a holding pad that maintains the holding force for the workpiece to be polished while facilitating attachment and detachment of the workpiece, and a method for manufacturing the same. [Means for solving the problem]

[0006] As a result of investigations, the inventors have found a holding pad that has a plurality of protrusions arranged in a dot pattern on the holding surface of the holding layer, which makes it possible to adjust the adsorption force appropriately without requiring a separate member such as a protective layer, and which facilitates the release of the polished object. [1] A holding pad having a holding layer for holding an object to be polished, The retaining layer integrally comprises a retaining surface; A holding pad, the holding surface of which has a plurality of protrusions arranged in a dot pattern. [2] The holding pad described in [1], wherein the total area of ​​the contact portions of the convex portions that come into contact with the workpiece is 3% or more and 40% or less of the area of ​​the hypothetical holding surface when the holding surface is assumed to be flat. [3] The holding pad described in [1], wherein the number of lines formed by the convex portions on the holding surface is 40 lines or more and 150 lines or less. [4] The holding pad described in [1], wherein the average height of the convex portions is 0.3 mm or more and 1.5 mm or less. [5] The holding pad described in [1], wherein the shape of the convex portion is a truncated cone. [6] The holding pad described in [1], wherein the holding layer is made of a photocurable resin. [7] The holding pad described in [6], wherein the photocurable resin is an acrylic ultraviolet curable resin. [8] A holder comprising a frame-shaped member on the outer periphery of the holding surface of the holding pad described in [1], the frame-shaped member being made of glass epoxy or SUS. [9] A method for manufacturing a holding pad, comprising: a holding layer for holding an object to be polished, the holding layer having an integral holding surface; and a plurality of protrusions arranged in a dot pattern on the holding surface, the method comprising the steps of: Preparing a mold; placing a photocurable resin in the mold; A step of placing a masking sheet on the photocurable resin so that a convex portion can be formed; a step of curing the unmasked photocurable resin by irradiating light from above the masking sheet; and washing away the uncured photocurable resin with a solvent to obtain a retaining layer made of cured photocurable resin.

[10] A method for manufacturing a holding pad, comprising: a holding layer for holding an object to be polished, the holding layer having an integral holding surface and a substrate on the opposite side of the holding surface as a separate member; and a plurality of protrusions are arranged in a dot pattern on the holding surface, Preparing a mold; placing a substrate in the mold; disposing a photocurable resin on the substrate; a step of irradiating the photocurable resin with light from a substrate side to bond the substrate and the photocurable resin; A step of arranging a masking sheet on the opposite side of the substrate from the photocurable resin so that a convex portion can be formed; a step of curing the unmasked photocurable resin by irradiating light from above the masking sheet; and washing away the uncured photocurable resin with a solvent to obtain a substrate-attached support layer made of cured photocurable resin adhered to the substrate. Effect of the Invention

[0007] The holding pad has a holding layer for holding the object to be polished, the holding layer having an integral holding surface on which a plurality of protrusions are arranged in a dot pattern, and does not require a separate member such as a protective layer; the adhesive force can be appropriately adjusted, making it easy to peel the pad from the object to be polished. [Brief description of the drawings]

[0008] [Figure 1] FIG. 1 is a schematic diagram of polishing. [Diagram 2] FIG. 2 is an enlarged view of the support surface of the support layer 11. As shown in FIG. [Diagram 3] Fig. 3(a) is the support surface of the support layer 11. Fig. 3(b) is a diagram in which the contact portions of the protrusions of the support surface are shaded. Fig. 3(c) shows a hypothetical support surface. [Figure 4] FIG. 4 is a diagram for explaining the line degree. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Hereinafter, a mode for carrying out the invention will be described, however, the present invention is not limited to the mode for carrying out the invention.

[0010] <<Retention pad>> 1, the holding pad 10 is provided on the lower surface of the holding platen 2 and holds the workpiece W to be polished by adsorption onto a holding surface 110. The holding pad 10 and a frame-shaped member 12 provided on the outer periphery of the holding surface 110 of the holding layer 11 constitute a holder 1. The outer circumferential portion means the inner circumferential portion of the holding surface that is away from the center of rotation when the holding surface rotates and the portion closer to the center of rotation is defined as the inner circumferential portion. The holding pad 10 includes a base material, a double-sided tape (not shown) and the like in addition to the holding layer 11, but may be composed of the holding layer 11 alone.

[0011] (retention layer) The retaining layer 11 has an integral retaining surface 110 on which a plurality of protrusions 110A are arranged in a dot pattern, as shown in Fig. 3. As shown in Fig. 3(a), a plurality of protrusions 110A are arranged approximately evenly on the retaining surface 110. The term "integral" as used here means that the retaining surface of the retaining layer is entirely made of the same material, and that the protrusions 110A are formed in a state in which they cannot be separated from the remaining portions of the retaining surface other than the protrusions 110A.

[0012] The total area of ​​the contact portions 111A of the convex portion 110A that come into contact with the workpiece W is preferably 3% or more and 40% or less of the area of ​​the hypothetical holding surface when the holding surface is assumed to be flat, and more preferably 10% or more and 30% or less. The contact portion 111A of the protrusion 110A that contacts the workpiece W is 111A in Fig. 3, and the total contact portion is the total area of ​​the shaded portion in Fig. 3(b). The hypothetical holding surface when the holding surface 110 is assumed to be flat means the holding surface when the protrusion 110A does not exist and it is assumed to be flat, that is, the state in Fig. 3(c), and the shaded portion in Fig. 3(c) corresponds to the area of ​​the hypothetical holding surface. Hereinafter, in this specification, the total area of ​​the contact portion 111A of the protrusion 110A that contacts the workpiece W relative to the area of ​​the hypothetical holding surface may be simply referred to as the "area ratio". The workpiece W is held by the surface tension of water on the holding surface 110 of the holding layer 11. When the area ratio is small, the number of protruding portions 110A is small and the area other than the protruding portions 110A is large, so that the surface tension in these portions is large and the adsorptive force is strong.

[0013] In the holding surface 110, the number of lines formed by the convex portion 110A is preferably 40 lines or more and 150 lines or less, and more preferably 50 lines or more and 100 lines or less. The number of lines is the fineness of the dots, and is the number of dots per inch (25.4 mm). For example, if black is the convex portion in FIG. 4, 5 dots are contained per inch, so the number of lines is 5 lines, and the area ratio is 50%. The polished object W is held by the holding surface 110 of the holding layer 11 due to the surface tension of water, so that when it is peeled off, air gets between the holding surface 110 and the polished object W, and the polished object W is peeled off. As the number of lines increases, the number of dots increases, and air gets in easily, making peeling easier, but if the number of lines is too large, the dots become too fine, making it difficult to create the convex portion 110A.

[0014] The average height of the protrusions 110A is preferably 0.3 mm or more and 1.5 mm or less, and more preferably 0.5 mm or more and 1.3 mm or less. The protrusions preferably account for 18% to 88% of the total height of the retention layer, and more preferably 33% to 66%. When the average height of the protrusions 110A is within the above range, the adhesion and releasability of the polished object are good. Here, the height of the protrusions 110A is α in FIG. 2. The shape of the convex portion 110A is a truncated cone in this example, but it may also be an approximately truncated cone, a truncated elliptical cone, a truncated polygonal pyramid, a cylinder, an elliptical cylinder, or a polygonal cylinder. A truncated cone is preferred because it is easy to manufacture and is less likely to damage the object to be polished. The adhesiveness and releasability of the holding surface 110 to the workpiece W can be easily adjusted by adjusting the area ratio, the number of lines formed by the convex portions 110A, the height and shape of the convex portions 110A, and the like.

[0015] The retaining layer 11 is made of a curable resin. The curable resin may be a photocurable resin that is cured by applying light, or a thermosetting resin that is cured by applying heat. The curable resin is cured in a portion to which light or heat is applied, and is not cured in a portion to which light or heat is not applied. In this specification, a resin that is not cured by not applying light or heat is called an uncured curable resin, and a resin that is cured by applying light or heat is called a cured curable resin. The retaining layer 11 is preferably made of a photocurable resin. The photocurable resin is not particularly limited as long as it is a resin that is polymerized and cured by light of a specific wavelength, and examples of the photocurable resin include polyester resin, unsaturated polyester resin, vinyl ether resin, vinyl ester resin, acrylic resin, and epoxy resin. More preferably, examples of the photocurable resin include acrylic resin and epoxy resin. The resin may be used alone or in combination of two or more types. During polishing, a slurry is supplied between the polishing pad 3 and the polished object W. The slurry is a mixture (dispersion) of water, various chemical components, and hard, fine abrasive grains, and may chemically deteriorate the retention layer 11. Therefore, the retention layer 11 is preferably made of an acrylic ultraviolet-curing resin, which has a higher crosslink density and better chemical resistance than thermosetting resins or room-temperature curing resins.

[0016] When the retaining layer 11 is made of a photocurable resin, it is easy to manufacture a retaining layer 11 having an integral retaining surface 110 on which multiple convex portions 110A are arranged in a dot pattern, and it is easy to adjust the area ratio, the number of lines formed by the convex portions 110A, and the height and shape of the convex portions 110A. As a result, the adhesion and releasability of the retaining surface 110 to the workpiece W can be easily adjusted.

[0017] The density of the support layer 11 is 0.5 kg / m 3 More than 3.0kg / m 3 Less than 1.0 kg / m is preferable. 3 More than 2.0kg / m 3 The density within the above range is preferable because it provides excellent attachment / detachment properties for the object to be polished.

[0018] In this specification, the Shore A hardness refers to a value measured in accordance with Japanese Industrial Standards (JIS K7311). The Shore A hardness of the retaining layer 11 of the present invention is preferably not less than 60 and not more than 90, and more preferably not less than 70 and not more than 80. When the Shore A hardness is within the above range, the polished state of the object to be polished is good.

[0019] In this specification, the compressibility is an index of softness, and the compressive elastic modulus is an index of the ease of return to normal after compressive deformation. The compressibility and compressive elasticity can be determined using a Shopper type thickness gauge (pressure surface: circular with a diameter of 1 cm) in accordance with the Japanese Industrial Standards (JIS L1021). Specifically, the method is as follows. The thickness t0 is measured after applying the initial load for 30 seconds from the no-load state, and then the thickness t1 is measured after applying the final load for 5 minutes from the thickness t0 state. Next, all loads are removed from the thickness t1 state, and the specimen is left for 5 minutes (to be in a no-load state), after which the initial load is again applied for 30 seconds and the thickness t0' is measured. The compression ratio can be calculated using the formula: Compression ratio (%) = 100 × (t0-t1) / t0 (initial load is 100 g / cm 2 , final load is 1120g / cm 2 (It is.) The compressive elastic modulus can be calculated using the formula: Compressive elastic modulus (%) = 100 × (t0'-t1) / (t0-t1) (initial load is 100 g / cm 2 , final load is 1120g / cm 2 (It is.)

[0020] The compressibility of the support layer 11 is preferably 0.1% or more and 10% or less, and more preferably 0.5% or more and 5% or less. The compressive elastic modulus of the retaining layer 11 is preferably 60% or more and 90% or less, and more preferably 70% or more and 80% or less. When the compressive modulus and the compressive elastic modulus are within the above ranges, the polished state of the object to be polished is good.

[0021] The thickness (height) of the support layer 11 can be adjusted within the range of 0.5 to 1.7 mm, and is more preferably 0.7 to 1.5 mm. When the thickness of the support layer 11 is within the above range, the workability during replacement of the support pad is good.

[0022] The retaining layer 11 has a frame-shaped member 12 on the outer periphery of the retaining surface 110, and the retaining pad 10 and the frame-shaped member 12 form the retainer 1. The frame-shaped member 12 surrounds the workpiece W to prevent the workpiece W from shifting sideways or falling off during polishing. A recess may be formed on the surface of the portion of the retaining surface 110 that includes the frame-shaped member 12 (13 in FIG. 2). The frame-shaped member 12 is attached to the retaining surface 110 with an adhesive layer. If the retaining surface 110 of the retaining layer 11 becomes too smooth, the adhesion between the frame-shaped member 12 and the retaining surface 110 decreases. However, when a recess is formed in the portion of the retaining surface 110 of the retaining layer 11 of the present invention that includes the frame-shaped member 12, peeling between the frame-shaped member 12 and the retaining layer 11 can be suppressed, and the intrusion of slurry between them can be suppressed. The frame member 12 is made of glass epoxy or SUS. Glass epoxy is a composite material of glass fiber and epoxy resin obtained by impregnating or applying epoxy resin to glass woven fabric. SUS is stainless steel (stainless used steel). Considering the frictional heat and wear generated by contact with the polishing pad 3 during polishing, it is preferable that the frame member 12 has excellent heat resistance.

[0023] <<Method of manufacturing the holding pad>> The method for manufacturing the holding pad 10 of the present invention is not particularly limited, but the following method is one example. A method for manufacturing a holding pad (10) comprising: a holding layer (11) for holding an object to be polished; the holding layer (11) integrally comprises a holding surface (110); a substrate is provided as a separate member on the opposite side of the holding surface (110); and a plurality of protrusions (110A) are arranged in a dot pattern on the holding surface (110), the method comprising the steps of: The process of preparing the mold (Step 1), Step 2: placing a substrate in the mold; Step 3: placing a photocurable resin on the substrate; a step of irradiating the photocurable resin with light from the substrate side to bond the substrate and the photocurable resin (Step 4); A step of arranging a masking sheet on the opposite side of the substrate from the photocurable resin so that the protrusion 110A can be formed (Step 5); A step of curing the unmasked photocurable resin by irradiating light from above the masking sheet (Step 6); and (Step 7) obtaining a substrate-attached retaining layer 11 made of cured photocurable resin by washing away the uncured photocurable resin with a solvent.

[0024] (Step 1) First, a mold is prepared. The mold is not particularly limited as long as it can form the retaining layer 11, but it is preferable that the mold has a shape that can form the shape of the retaining layer 11. The material of the mold is not particularly limited as long as it can form the retaining layer, and examples of the material include a metal mold, a plastic mold, a resin mold, and the like.

[0025] (Step 2) Next, a substrate is placed in the mold. The substrate is not particularly limited as long as it is a substrate on which a photocurable resin can be placed and does not block light, and flexible films, nonwoven fabrics, woven fabrics, etc. can be used. The placement of the substrate is not essential as a step of the manufacturing method, but it is preferable to use it because it allows the photocurable resin to be stably cured. It can be omitted as necessary.

[0026] (Step 3) A photocurable resin is placed on the substrate. The photocurable resin may be a commercially available resin such as "Cosmolite" manufactured by Toyobo Co., Ltd., "PG Plate" manufactured by Toray Industries, Inc., or "Fuji Torelief" manufactured by Fujifilm Corporation, or a resin having desired properties may be manufactured by oneself. The photocurable resin may be used in either a liquid or solid state at room temperature, but it is preferable to use a resin that is solid at room temperature from the viewpoint of workability.

[0027] (Step 4) Next, the photocurable resin is irradiated with light from the substrate side to bond the substrate and the photocurable resin. "Irradiating light from the substrate side" means that in Step 3, in a state where the curable resin is placed on the substrate inside the mold, light is irradiated from below the substrate (from the bottom of the mold). As described above, by using a substrate that transmits light, the photocurable resin placed on the substrate can be cured. This process allows the photocurable resin on the substrate side to be cured uniformly, so that in the subsequent process, the convex parts 110A located on the opposite side to the substrate are not independent of each other, and are not independently separable, but the entire holding layer and holding surface are formed as an integral body. The substrate is not exposed from the supporting surface 110 of the supporting layer 11 .

[0028] The light irradiating device is not particularly limited as long as it is a device that emits light in a wavelength range including the wavelength of light at which the photocurable resin is cured, and examples thereof include ultraviolet ray irradiating devices, and more specifically, high pressure mercury lamps, UV-LED lamps, and black light blue fluorescent lamps (BLB), with BLB being preferred. The wavelength of the ultraviolet ray irradiation is preferably 315 nm to 400 nm, and the irradiation time is preferably 1 minute to 15 minutes.

[0029] (Step 5) A masking sheet is placed on the side of the photocurable resin opposite to the substrate side, so that a convex portion can be formed. That is, the masking sheet is placed on the side where the photocurable resin is exposed, not on the side where the substrate and the photocurable resin are in contact. The substrate and the photocurable resin are bonded by the above-mentioned photocuring, but the side where the substrate is not bonded is in an uncured state at this point. A masking sheet is placed on the uncured curable resin. The masking sheet is not particularly limited as long as it is a sheet made of a material that blocks light, and cellulose triacetate (TAC) or polyethylene terephthalate (PET) can be used.

[0030] (Step 6) By irradiating light from above the masking sheet, the unmasked photocurable resin is cured, and this curing determines the shape of the holding surface 110. The same ultraviolet irradiating device as that used in the process of bonding the base material and the photocurable resin can be used, and the wavelength, illuminance, and irradiation time of the ultraviolet irradiation are adjusted according to the type of photocurable resin and the desired shape of the holding surface 110.

[0031] (Step 7) Next, the uncured photocurable resin is washed away using a solvent. The substrate is bonded to obtain a retention layer 11 made of a photocurable resin cured by light. The solvent is not particularly limited as long as it can remove the uncured photocurable resin, but it is preferable to use water. The obtained retaining layer 11 is connected to a retaining platen 2 to which the adhered substrate is attached, as shown in Fig. 1, and is subjected to a polishing step. If necessary, an adhesive layer such as a double-sided tape may be further provided on the surface of the substrate opposite to the surface to which the photocurable resin is adhered, and the retaining layer 11 may be connected to the retaining platen via this adhesive layer. EXAMPLES

[0032] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these examples.

[0033] In each of the examples and comparative examples, unless otherwise specified, "parts" means "parts by mass".

[0034] (Manufacture of retention layer 11) First, a mold was prepared and a PET film substrate was placed on the bottom side of the mold. Cosmolite (Toyobo Co., Ltd.), a photocurable resin, was placed on top of the substrate, and the BLB was irradiated onto the photocurable resin from the substrate side for 3 minutes to bond the substrate and photocurable resin. A masking sheet with multiple holes so that convex parts could be formed was placed on the surface of the photocurable resin opposite the substrate, and the unmasked photocurable resin was cured by irradiating it with the BLB from above the masking sheet for 3 minutes. By washing away the uncured photocurable resin with water, a retention layer 11 was obtained that was composed of cured photocurable resin with a retention layer height of 0.7 mm, a convex portion height of 0.25 mm, and the convex portion accounting for 35.7% of the total height of the retention layer. A double-sided tape was attached to the surface of the base material opposite to the surface to which the photocurable resin was attached, thereby obtaining a holding pad 10. A retaining layer was produced using a masking sheet that would allow projections to be formed with an area ratio of 10% and a line count of 160, but the diameter of the projections was too small to form the projections.

[0035] Using the same material as the retaining layer 11 described above, retaining pads 10 having the area ratio and number of lines as shown in Table 1 were manufactured and subjected to the following evaluation. Note that for the retaining pads of Examples 2 to 6, the retaining layer had a height of 0.7 mm, the convex portion had a height of 0.25 mm, and the convex portion accounted for 35.7% of the total height of the retaining layer, as in Example 1, while for the retaining pad of Comparative Example 1, there were no convex portions, so the retaining layer had a height of 0.7 mm, the convex portion had a height of 0 mm, and the convex portion accounted for 0% of the total height of the retaining layer.

[0036] [Table 1]

[0037] (adsorption) Using the holding pads of Examples 1 to 6 and Comparative Example 1, a wafer was attached to the holding pad, and a polishing test was carried out under the following conditions. If the wafer shifted sideways or fell off during the polishing test, it was evaluated as × (△), and if it remained attached until the end, it was evaluated as ◯.

[0038] (peelability) Using the holding pads of Examples 1 to 6 and Comparative Example 1, polishing tests were carried out under the following conditions, and then the wafer was peeled off from the holding pad. Those which could be peeled off without any problems were rated as ◯, those which took longer to peel off than those which could be peeled off without any problems were rated as △, and those which damaged the wafer during peeling were rated as ×.

[0039] (Polishing effect) If both adsorption and releasability were rated as "○", polishing could be performed without any problems, and the polishing effect was rated as "○". If either was rated as "△", the polishing effect was rated as "△" because it had a greater effect on polishing than the polishing effect rated as "○". If either was rated as "×", the polishing effect could not be used for polishing, and the polishing effect was rated as "×".

[0040] (Conditions of the polishing test conducted to evaluate the adsorption, peelability, and polishing effect) Polishing machine used: 15inch single-sided polishing machine Abrasive temperature: 50~120 degrees Polishing platen rotation speed: 60~100rpm Polishing head rotation speed: 30~50rpm Grinding pressure: 350~500g / cm 2 Polishing slurry (metal film): Potassium permanganate + lubricant liquid Polishing slurry flow rate: 5 cc / min Polishing time: 3 to 20 hours Polished object (metal film): SiC WF [Industrial Applicability]

[0041] The present invention provides a holding pad that ensures the holding force for the workpiece to be polished and can easily attach and detach the workpiece to be polished, and therefore contributes to the manufacture and sale of holding pads, and thus has industrial applicability.

[0042] 1 Holder 10 Retaining Pad 11 Retention layer 110 Holding surface 110A Convex 13 Part of the holding surface having a frame-shaped member (joint part between the holding surface and the frame-shaped member) 12 Frame-shaped member 2 Holding plate 3 Polishing Pads 4 Polishing plate W Object to be polished

Claims

1. A holding pad having a holding layer for holding an object to be polished, The retaining layer integrally comprises a retaining surface; A holding pad, the holding surface of which has a plurality of protrusions arranged in a dot pattern.

2. 2. The holding pad according to claim 1, wherein the total area of ​​the contact portions of the convex portions that contact the workpiece is 3% or more and 40% or less of the area of ​​the hypothetical holding surface when the holding surface is assumed to be flat.

3. The holding pad according to claim 1 , wherein the number of lines formed by the protrusions on the holding surface is 40 lines or more and 150 lines or less.

4. The holding pad according to claim 1 , wherein the average height of the convex portions is 0.3 mm or more and 1.5 mm or less.

5. The support pad according to claim 1 , wherein the convex portion has a truncated cone shape.

6. The support pad according to claim 1 , wherein the support layer is made of a photocurable resin.

7. The holding pad according to claim 6 , wherein the photocurable resin is an acrylic ultraviolet curable resin.

8. 2. A holder comprising: a frame member on an outer periphery of the holding surface of the holding pad according to claim 1, said frame member being made of glass epoxy or SUS.

9. 1. A method for manufacturing a holding pad, comprising: a holding layer for holding an object to be polished, the holding layer being integrally provided with a holding surface, the holding surface having a plurality of protrusions arranged in a dot pattern, the method comprising: Preparing a mold; placing a photocurable resin in the mold; A step of placing a masking sheet on the photocurable resin so that a convex portion can be formed; a step of curing the unmasked photocurable resin by irradiating light from above the masking sheet; and washing away the uncured photocurable resin with a solvent to obtain a retaining layer made of cured photocurable resin.

10. A method for manufacturing a holding pad, comprising: a holding layer for holding an object to be polished, the holding layer having an integral holding surface and a substrate on an opposite side of the holding surface as a separate member; and a plurality of protrusions are arranged in a dot pattern on the holding surface, the method comprising: Preparing a mold; placing a substrate in the mold; disposing a photocurable resin on the substrate; a step of irradiating the photocurable resin with light from a substrate side to bond the substrate and the photocurable resin; A step of arranging a masking sheet on the opposite side of the substrate from the photocurable resin so that a convex portion can be formed; a step of curing the unmasked photocurable resin by irradiating light from above the masking sheet; and using a solvent to wash away the uncured photocurable resin, thereby obtaining a substrate-attached support layer that is adhered to the substrate and composed of cured photocurable resin.

Citation Information

Patent Citations

  • Suction plate and evacuator

    JP2001176957A

  • Method of manufacturing attracting and fixing apparatus

    JP2005019700A

  • Suction apparatus, polishing device, semiconductor device and semiconductor device manufacturing method

    JP2006305713A

  • Holding fixture and method of grinding semiconductor wafer

    JP2007250738A

  • Protective structure of semiconductor wafer, and grinding method of semiconductor wafer using the same

    JP2007250789A