Semiconductor device and oxide film thickness measurement method for semiconductor device
The semiconductor device configuration allows for efficient oxide film thickness measurement by correlating resistance values with film thickness, addressing inefficiencies in conventional methods and enhancing manufacturing speed.
Patent Information
- Application Number
- JP2023053681
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-29
- Publication Date
- 2024-10-10
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Conventional methods for measuring oxide film thickness in semiconductor devices are inefficient and time-consuming, particularly for mass-produced devices, making it difficult to ensure appropriate insulation and prevent time-dependent dielectric breakdown.
A semiconductor device configuration and method that involves forming a wiring across the boundary between trench and non-trench regions, allowing the thickness of the oxide film to be measured by correlating resistance values with film thickness, without the need for cross-sectional analysis.
Enables easy and efficient measurement of oxide film thickness, reducing manufacturing time and maintaining insulation quality without reducing the active area or number of devices.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a semiconductor device and an oxide film thickness measuring method for a semiconductor device. [Background technology]
[0002] As a conventional semiconductor device, a semiconductor device having an STI structure has been disclosed (for example, Patent Document 1). In a semiconductor device having an STI structure, an oxide film is formed so as to fill one or more trenches formed on the surface of a substrate, and the surface of the oxide film is planarized. As a result, multiple semiconductor elements formed on the surface of the substrate are insulated by the trenches.
[0003] Here, if the thickness of the oxide film is small, the shoulder of the trench may be exposed, or the oxide film formed on the shoulder may become thin. This may result in the generation of parasitic transistors between the semiconductor elements, and the characteristics of the transistor may change from the desired characteristics. In addition, the withstand voltage of the oxide film may decrease, making it easier for time-dependent dielectric breakdown (TDDB) to occur. Therefore, in order to properly insulate the semiconductor elements, it is important to ensure the thickness of the oxide film filling the trench. The shoulder of the trench is a region near the boundary between the trench region where the trench is formed and the non-trench region where the semiconductor element is formed without the trench.
[0004] In order to prevent TDDB and the like, conventional semiconductor device manufacturing processes employ methods for checking whether an oxide film has an appropriate thickness, such as cutting the semiconductor device and checking the cross section of the oxide film, or checking the current-voltage characteristics (IV characteristics) of a transistor. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2023-017246 A Summary of the Invention [Problem to be solved by the invention]
[0006] However, with the conventional techniques, it is difficult to measure the thickness of the oxide film on all mass-produced semiconductor devices, and there is room for improvement in shortening the manufacturing time of semiconductor devices.
[0007] In view of the above circumstances, an object of the present invention is to provide a semiconductor device that allows the thickness of an oxide film to be easily measured, and a method for measuring the thickness of an oxide film of a semiconductor device. [Means for solving the problem]
[0008] In order to solve the above problems, the semiconductor device of the present invention comprises a substrate in which a semiconductor element and one or more trenches are formed, an oxide film disposed within the trenches, and wiring disposed across the boundary between a trench region of the substrate in which the trenches are formed and a non-trench region in which the trenches are not formed and the semiconductor element is formed, from the non-trench region to the oxide film in the trench region, the wiring covering a portion of a wall surface forming the trench.
[0009] In order to solve the above-mentioned problems, the present invention provides a method for measuring an oxide film thickness of a semiconductor device comprising: a substrate in which a semiconductor element and one or more trenches are formed; an oxide film disposed in the trench; and wiring disposed across a boundary between a trench region of the substrate in which the trench is formed and a non-trench region in which the semiconductor element is formed without the trench, and spanning the oxide film in the trench region from the non-trench region to the oxide film in the trench region, the wiring covering a portion of a wall surface forming the trench, the method including the steps of: measuring a first resistance value of the wiring when the oxide film has a first thickness; measuring a second resistance value of the wiring when the oxide film has a second thickness smaller than the first thickness; and measuring the second thickness based on the first resistance value and the second resistance value.
[0010] In order to solve the above-mentioned problems, the present invention provides an oxide film thickness measurement method for a semiconductor device comprising: a substrate in which a semiconductor element and one or more trenches are formed; an oxide film disposed in the trench; and wiring disposed across a boundary between a trench region of the substrate in which the trench is formed and a non-trench region in which the semiconductor element is formed without the trench, from the non-trench region to the trench region, wherein the wiring covers a portion of a wall surface forming the trench, the trench and the oxide film are formed extending in a first direction in a planar view of the substrate, and the wiring extends in a second direction intersecting the first direction in a planar view of the substrate, and has a portion crossing the trench and the oxide film, the method including the steps of: measuring a first resistance value of the wiring when the oxide film has a first thickness; measuring a second resistance value of the wiring when the oxide film has a second thickness smaller than the first thickness; and measuring the second thickness based on the first resistance value and the second resistance value. Effect of the Invention
[0011] According to the present invention, it is possible to provide a semiconductor device that allows easy measurement of the thickness of an oxide film, and a method for measuring the thickness of an oxide film of a semiconductor device. [Brief description of the drawings]
[0012] [Figure 1] FIG. 1 is a plan view of a wafer including a semiconductor device according to a first embodiment of the present disclosure. [Figure 2A] FIG. 2A is a diagram showing a configuration of a semiconductor device according to a first embodiment of the present disclosure. [Figure 2B] FIG. 2B is a diagram showing a configuration of the semiconductor device according to the first embodiment of the present disclosure. [Figure 3A] FIG. 3A is a diagram for explaining the correlation between the thickness of the oxide film 2 and the resistance value of the wiring 3. As shown in FIG. [Figure 3B] FIG. 3B is a diagram for explaining the correlation between the thickness of the oxide film 2 and the resistance value of the wiring 3. As shown in FIG. [Figure 3C] FIG. 3C is a diagram for explaining the correlation between the thickness of the oxide film 2 and the resistance value of the wiring 3. As shown in FIG. [Figure 4] FIG. 4 is a diagram for explaining the method for measuring the oxide film thickness of a semiconductor device according to the first embodiment of the present disclosure. [Diagram 5] FIG. 5 is a diagram for explaining a modified example of the semiconductor device according to the first embodiment of the present disclosure. [Figure 6A] FIG. 6A is a diagram showing a configuration of a semiconductor device according to a second embodiment of the present disclosure. [Figure 6B] FIG. 6B is a diagram showing a configuration of a semiconductor device according to a second embodiment of the present disclosure. [Figure 7A] FIG. 7A is a diagram for explaining a method for measuring an oxide film thickness of a semiconductor device according to a second embodiment of the present disclosure. [Figure 7B] FIG. 7B is a diagram for explaining the method for measuring the oxide film thickness of a semiconductor device according to the second embodiment of the present disclosure. [Figure 8] FIG. 8 is a diagram for explaining a first modified example of the semiconductor device according to the second embodiment of the present disclosure. [Figure 9] FIG. 9 is a diagram for explaining a second modified example of the semiconductor device according to the second embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] Hereinafter, an embodiment will be described with reference to the drawings. Note that the same or similar reference numerals are used to designate the same functions or configurations, and the description thereof will be omitted as appropriate.
[0014] [First embodiment] (Configuration of Semiconductor Device) FIG. 1 is a plan view of a wafer including a semiconductor device according to a first embodiment of the present disclosure.
[0015] The wafer W is a semiconductor substrate on which the semiconductor element 10 is formed. Specifically, the wafer is a Si substrate containing Si (silicon). Note that the wafer W is not limited to a Si substrate, and may be a substrate containing SiC (silicon carbide) or a substrate containing GaAs (gallium arsenide).
[0016] The wafer W is provided with a scribe line region SL and an active region AC of a predetermined width. A semiconductor device 100 is formed as a test element group (TEG) in the scribe line region SL. The active region AC may be interpreted as a non-trench region of the wafer W where a trench, which will be described later, is not formed. Region X shown in FIG. 1 is a region of the multiple scribe line regions SL where the semiconductor device 100 according to the first embodiment is formed. The configuration of the semiconductor device 100 according to the first embodiment will be described with reference to FIGS. 2A and 2B.
[0017] Figures 2A and 2B are diagrams showing the configuration of a semiconductor device according to a first embodiment of the present disclosure. Figure 2A shows an enlarged view of region X in Figure 1. Figure 2B shows a cross section of the semiconductor device 100 shown in Figure 2A taken along line AA.
[0018] The semiconductor device 100 includes a substrate 20 in which a semiconductor element and one or more trenches 1 are formed, an oxide film 2 disposed in the trench 1, and a wiring 3.
[0019] The substrate 20 is a part of the wafer W shown in Fig. 1. A plurality of trenches 1 are arranged at intervals in a direction D1. The material of the oxide film 2 can be appropriately selected depending on the application, purpose, etc., and a silicon oxide film is one example.
[0020] The wiring 3 is a conductive member extending in a direction D2 intersecting the direction D1 and disposed on the substrate 20. The wiring 3 is an electrode corresponding to a gate electrode, a drain electrode, a source electrode, etc., and the material of the wiring 3 can be appropriately selected depending on the application, purpose, etc., and one example is Poly Si (porous silicon).
[0021] 2A, the wiring 3 is disposed on the substrate 20 such that its center portion overlaps with a boundary 30 on the substrate 20. Specifically, the wiring 3 is disposed across the boundary 30 from the active region AC (non-trench region) to the oxide film 2 of the trench region TC. The boundary 30 is the portion where the trench region TC, in which the trench 1 of the substrate 20 is formed, and the active region AC come into contact.
[0022] 2B, the wiring 3 has a step 4 on its surface, and covers part of the wall surface 1A that forms the trench 1. Part of the wiring 3 is disposed in the active region AC, and the remaining part of the wiring 3 is disposed inside the trench 1. This part covers part of the wall surface 1A that forms the trench 1, and also covers part of the upper surface of the oxide film 2. Since the wiring 3 has the step 4 in this way, the cross-sectional area of the wiring 3 is larger than if there was no step.
[0023] (Method of manufacturing a semiconductor device) Next, a manufacturing method of the semiconductor device 100 according to the first embodiment will be briefly described.
[0024] First, a silicon oxide film is formed so as to cover the active region AC of the substrate 20. Next, a silicon nitride film is formed so as to cover the silicon oxide film by using a known CVD (Chemical Vapor Deposition) method. Next, the silicon oxide film and the silicon nitride film are patterned by using known photolithography and etching techniques.
[0025] Next, the substrate 20 is etched using the silicon oxide film and silicon nitride film as a mask, thereby forming a trench 1 in the substrate 20. Next, an oxide film 2 made of an insulator such as SiO2 is formed to cover the substrate 20 using a known CVD method. The oxide film 2 is formed to a thickness that covers the upper surfaces of the silicon oxide film and silicon nitride film. The oxide film 2 is filled into the trench 1 formed in the previous process.
[0026] Next, the oxide film 2 is planarized by a known CMP (Chemical Mechanical Polishing) method. Specifically, in planarization by the CMP method, the oxide film 2 is polished while a polishing liquid (slurry) is flowed. Next, the silicon oxide film and the silicon nitride film are removed by etching.
[0027] Next, an insulating film is formed on the substrate 20 using a known thermal oxidation method. Then, a polysilicon film is formed on the insulating film using a known CVD method. Next, the insulating film and the polysilicon film are patterned by known photolithography and etching techniques to form the wiring 3.
[0028] Next, a description will be given of the correlation between the thickness of the oxide film 2 and the resistance value of the wiring 3. FIG. 3A, FIG. 3B, and FIG. 3C are diagrams for explaining the correlation between the thickness of the oxide film 2 and the resistance value of the wiring 3.
[0029] 3A shows a cross section of a normally formed oxide film 2 and wiring 3. When the oxide film 2 is normally formed, the upper surface of the oxide film 2 and the upper surface of the active region AC are located at substantially the same height, so that no step occurs between the oxide film 2 and the active region AC. Therefore, the cross section of the wiring 3 formed from the active region AC to the oxide film 2 has a flat plate shape.
[0030] 3B shows an oxide film 2 that is thinner than the oxide film 2 in FIG. 3A. When the thickness of the oxide film 2 is small relative to the depth of the trench 1, the position of the top surface of the oxide film 2 differs from the position of the top surface of the active region AC, causing a step between the oxide film 2 and the active region AC. As a result, a part of the wiring 3 enters the trench 1, and a step portion 4 is formed in the wiring 3 that is formed from the active region AC to the oxide film 2.
[0031] The cross-sectional area of the wiring 3 in which the step portion 4 is formed in this manner becomes larger than the cross-sectional area of the wiring 3 shown in Fig. 3A because a part of the wiring 3 enters the inside of the trench 1. When the lengths of the wiring 3 shown in Fig. 3A and the wiring 3 shown in Fig. 3B are equal, the larger the cross-sectional area of the wiring 3, the smaller the resistance value of the wiring 3.
[0032] 3C shows an even thinner oxide film 2. When the oxide film 2 becomes thinner as shown in FIG. 3C, the cross-sectional area of the wiring 3 becomes larger, and the resistance value of the wiring 3 becomes smaller.
[0033] As described above, since there is a correlation between the thickness of the oxide film 2 and the resistance value of the wiring 3, it is possible to measure the thickness of the oxide film 2 by measuring the resistance value of the wiring 3. With reference to Fig. 4, a method for measuring the thickness of the oxide film of the semiconductor device 100 according to the first embodiment will be described.
[0034] (Oxide film thickness measurement method) Fig. 4 is a diagram for explaining the method for measuring the oxide film thickness of a semiconductor device according to the first embodiment of the present disclosure. Fig. 4 shows a graph in which the horizontal axis represents the thickness of the oxide film 2 and the vertical axis represents the resistance value of the wiring 3. A plurality of data points (points a, b, and c) representing the thickness of the oxide film 2 and the resistance value of the wiring 3 are plotted on the graph.
[0035] Tha corresponding to point a represents the thickness of oxide film 2 shown in FIG. 3A, and Ra corresponding to point a represents the resistance value of wiring 3 shown in FIG. 3A.
[0036] Thb corresponding to point b represents the thickness of oxide film 2 shown in FIG. 3B, and Rb corresponding to point b represents the resistance value of wiring 3 shown in FIG. 3B.
[0037] Thc corresponding to point c represents the thickness of the oxide film 2 shown in FIG. 3C, and Rc corresponding to point c represents the resistance value of the wiring 3 shown in FIG. 3C.
[0038] 4, as the thickness of the oxide film 2 decreases with respect to Tha, the resistance value of the wiring 3 tends to decrease with respect to Ra. Since there is a correlation between the thickness of the oxide film 2 and the resistance value of the wiring 3, it is possible to measure the thickness of the oxide film 2 embedded in the trench 1 by measuring the resistance value of the wiring 3.
[0039] The oxide film thickness measuring method according to the first embodiment includes a step of measuring a first resistance value of the wiring 3 when the oxide film 2 has a first thickness, and a step of measuring a second resistance value of the wiring 3 when the oxide film 2 has a second thickness smaller than the first thickness. Furthermore, the oxide film thickness measuring method according to the first embodiment includes a measuring step of measuring the second thickness based on the measured first resistance value and second resistance value.
[0040] Specifically, the difference between Ra and Rb, the difference between Ra and Rc, etc. are collected in advance, and data correlating the measured value of the thickness of the oxide film 2 when these are detected with the difference is stored in a memory. After that, the resistance value of the wiring 3 of the semiconductor device 100 provided on the wafer W shown in FIG. 1 is measured, and the measured resistance value is compared with the above data, thereby making it possible to measure the thickness of the oxide film 2.
[0041] As a result, for example, when the measured resistance value (e.g., Rb) is within a specific range based on the resistance value (Ra) at point a, it can be determined that the oxide film 2 embedded in the trench of the active region AC in which the semiconductor element 10 shown in Fig. 1 is formed is formed normally. On the other hand, when the measured resistance value is not within the specific range, it can be determined that the oxide film 2 is thin, that is, the oxide film 2 is not formed normally.
[0042] [Modification of the first embodiment] Fig. 5 is a diagram for explaining a modified example of the semiconductor device according to the first embodiment of the present disclosure. The semiconductor device 100 shown in Fig. 5 includes a meandering wiring 3, and the wiring 3 has a plurality of meandering portions 40 when the substrate 20 is viewed in a plan view. The central portion of the wiring 3 is arranged in a meandering shape so as to overlap a boundary 30 on the substrate 20 when the substrate 20 is viewed in a plan view. The boundary 30 between the trench 1 and the active region AC is formed along the meandering portion 40 of the wiring 3 when the substrate 20 is viewed in a plan view.
[0043] By using the wiring 3 formed in a meandering shape, the wiring length of the meandering wiring 3 is longer than that of the straight wiring 3 of the first embodiment, so that the change in the resistance value of the wiring 3 when the thickness of the oxide film 2 in each trench 1 becomes smaller becomes larger, thereby improving the measurement sensitivity of the resistance value.
[0044] (Action and effect) As described above, in the semiconductor device 100 and the oxide film thickness measuring method for the semiconductor device 100 according to the first embodiment, the wiring 3 arranged across the oxide film 2 from the active region AC (non-trench region) to the trench region TC is configured to cover a portion of the wall surface 1A forming the trench 1.
[0045] With this configuration, the smaller the thickness of the oxide film 2, the smaller the resistance value of the wiring 3, so it is possible to measure the thickness of the oxide film 2 embedded in the trench 1 by measuring the resistance value of the wiring 3. Therefore, it is possible to easily measure the thickness of the oxide film in the STI structure without cutting the semiconductor device formed in the active region AC to check the cross section of the oxide film or checking the IV characteristics of the transistor formed in the active region AC. Therefore, it is possible to shorten the manufacturing time of mass-produced semiconductor devices.
[0046] Furthermore, the semiconductor device 100 according to the first embodiment is formed on the scribe line (scribe line region SL) of the substrate 20, and thus the thickness of the oxide film 2 can be measured without narrowing the active region AC. Therefore, it becomes possible to easily measure the thickness of the oxide film in the STI structure without reducing the manufacturing volume of mass-produced semiconductor devices.
[0047] [Second embodiment] 6A and 6B are diagrams showing the configuration of a semiconductor device according to a second embodiment of the present disclosure, Fig. 6A shows the semiconductor device 100 when the substrate 20 is viewed in plan.
[0048] The trench 1 and the oxide film 2 of the semiconductor device 100 are formed to extend in a first direction in the substrate 20 when viewed from above. The wiring 3 of the semiconductor device 100 has a portion 31 that extends in a second direction intersecting the first direction when viewed from above.
[0049] Fig. 6B shows a cross section of the semiconductor device 100 shown in Fig. 6A taken along line BB. As shown in Fig. 6B, the wiring 3 is disposed from the active region AC to the upper surface of the oxide film 2, and further disposed from the upper surface of the oxide film 2 to the active region AC. That is, the wiring 3 is formed so that a part of the wiring 3 straddles two boundaries 30 formed at the opening of the trench 1, and covers the entire upper surface of the oxide film 2 in the trench 1.
[0050] 7A and 7B are diagrams for explaining a method for measuring an oxide film thickness of a semiconductor device according to a second embodiment of the present disclosure.
[0051] 7A shows a cross section of the wiring 3 when the oxide film 2 is formed normally, that is, when the upper surface of the oxide film 2 and the upper surface of the active region AC are located at approximately the same height. When the oxide film 2 is formed normally, the upper surface of the oxide film 2 and the upper surface of the active region AC are located at approximately the same height, so no step occurs between the oxide film 2 and the active region AC. Therefore, the cross section of the wiring 3 formed from the active region AC to the oxide film 2 is a flat plate-like shape.
[0052] 7B shows an oxide film 2 that is thinner than the oxide film 2 in FIG. 7A. When the thickness of the oxide film 2 is small relative to the depth of the trench 1, the position of the top surface of the oxide film 2 differs from the position of the top surface of the active region AC, causing a step to occur between the oxide film 2 and the active region AC. As a result, a portion of the wiring 3, i.e., the portion facing the oxide film 2, enters the inside of the trench 1, and the portion of the wiring 3 is formed in a concave shape that is recessed from the opening of the trench 1 toward the bottom of the trench 1.
[0053] Therefore, the length of the wiring 3 shown in FIG. 7B is longer than that of the wiring 3 shown in FIG. 7A, and therefore the resistance value of the wiring 3 shown in FIG. 7B is different from the resistance value of the wiring 3 shown in FIG. 7A.
[0054] As mentioned above, there is a correlation between the thickness of the oxide film 2 and the resistance value of the wiring 3. Therefore, as in the first embodiment, the thickness of the oxide film 2 embedded in the trench 1 can be measured by measuring the resistance value of the wiring 3.
[0055] [First Modification of the Second Embodiment] Fig. 8 is a diagram for explaining a first modified example of the semiconductor device according to the second embodiment of the present disclosure. A plurality of trenches 1 and oxide films 2 shown in Fig. 8 are arranged at intervals in the second direction described above. Note that Fig. 8 shows two trenches 1 and oxide films 2 embedded in these trenches 1.
[0056] By providing a plurality of trenches 1 and oxide films 2 in this manner, the area of the concave wiring 3 formed on the oxide film 2 can be increased as the number of trenches 1 increases. As a result, when the thickness of the oxide film 2 in each trench 1 is reduced, the wiring 3 can be made even longer than when there is only one trench 1. Therefore, the amount of change in the resistance value of the wiring 3 becomes even larger, and the measurement sensitivity of the resistance value is improved, making it even easier to measure the thickness of the oxide film 2.
[0057] The number of trenches 1 and oxide films 2 is not limited to two, and may be three or more. As the number of trenches 1 and oxide films 2 increases, the length of the wiring 3 becomes longer, and the amount of change in the resistance value of the wiring 3 can be increased.
[0058] [Second Modification of the Second Embodiment] Fig. 9 is a diagram for explaining a second modified example of the semiconductor device according to the second embodiment of the present disclosure. The wiring 3 shown in Fig. 9 is formed in a meandering shape so as to intermittently cross the trench 1 and the oxide film 2 in a first direction. The first direction is the direction in which the trench 1 and the oxide film 2 of the semiconductor device 100 extend when the substrate 20 is viewed in plan.
[0059] Specifically, the meandering wiring 3 has a plurality of meandering portions 40 in a plan view of the substrate 20. The trench 1 and the oxide film 2 are provided so as to overlap at least one of the plurality of meandering portions 40.
[0060] In this way, by overlapping the trench 1 with the meandering portion 40, the area of the concave wiring 3 formed on the oxide film 2 in the trench 1 can be further increased compared to the wiring 3 shown in Fig. 8. In other words, the portion 31 where the wiring 3 crosses the trench 1 and the oxide film 2 can be increased.
[0061] This further increases the length of the wiring 3 when the thickness of the oxide film 2 in each trench 1 is reduced. This further increases the amount of change in the resistance value of the wiring 3, improving the measurement sensitivity of the resistance value, and making it easier to measure the thickness of the oxide film 2.
[0062] (Action and effect) As described above, in the semiconductor device 100 of the second embodiment, the wiring 3 is configured to extend in the second direction when viewed in a plan view of the substrate 20 and to have a portion 31 that crosses the trench 1 and the oxide film 2.
[0063] With this configuration, when the thickness of the oxide film 2 is small, a portion of the wiring 3 is formed in a concave shape recessed from the opening of the trench 1 toward the bottom of the trench 1, thereby changing the resistance value of the wiring 3. Therefore, similarly to the first embodiment, the thickness of the oxide film 2 can be easily measured based on the resistance value of the wiring 3.
[0064] In this disclosure, a configuration example of the semiconductor device 100 formed on the scribe line (scribe line region SL) has been described, but the location where the semiconductor device 100 is formed may be a location other than the scribe line, for example, an area near the peripheral portion of the wafer W shown in FIG. 1.
[0065] In addition, the following supplementary notes are provided in relation to the above description.
[0066] (Appendix 1) a substrate in which a semiconductor device and one or more trenches are to be formed; an oxide film disposed within the trench; a wiring arranged across a boundary between a trench region of the substrate in which the trench is formed and a non-trench region in which the semiconductor element is formed without the trench, from the non-trench region to the oxide film of the trench region; Equipped with The wiring covers a portion of a wall surface that forms the trench.
[0067] (Appendix 2) The wiring is formed in a meandering shape having a plurality of meandering portions when the substrate is viewed in a plan view, 2. The semiconductor device according to claim 1, wherein the boundary is formed along the meandering portion when the substrate is viewed in a plan view.
[0068] (Appendix 3) the trench and the oxide film are formed to extend in a first direction in the substrate when the substrate is seen in a plan view, 3. The semiconductor device according to claim 1, wherein the wiring extends in a second direction intersecting the first direction when the substrate is viewed in a plan view, and has a portion that crosses the trench and the oxide film.
[0069] (Appendix 4) 4. The semiconductor device according to claim 3, wherein the trenches and the oxide films are arranged in a plurality of rows at intervals in the second direction.
[0070] (Appendix 5) 4. The semiconductor device according to claim 3, wherein the wiring is formed in a meandering shape so as to intermittently cross the trench and the oxide film in the first direction.
[0071] (Appendix 6) 6. The semiconductor device according to claim 1, wherein the semiconductor device is formed along a scribe line of the substrate.
[0072] (Appendix 7) 1. A method for measuring an oxide film thickness of a semiconductor device comprising: a substrate in which a semiconductor element and one or more trenches are formed; an oxide film disposed in the trench; and wiring disposed across a boundary between a trench region of the substrate in which the trench is formed and a non-trench region in which the trench is not formed and the semiconductor element is formed, the non-trench region, and the oxide film in the trench region, the wiring covering a portion of a wall surface forming the trench, the method comprising: measuring a first resistance value of the wiring when the oxide film has a first thickness; measuring a second resistance value of the wiring when the oxide film has a second thickness smaller than the first thickness; measuring the second thickness based on the first resistance value and the second resistance value; A method for measuring an oxide film thickness of a semiconductor device comprising the steps of:
[0073] (Appendix 8) 1. A method for measuring an oxide film thickness of a semiconductor device comprising: a substrate in which a semiconductor element and one or more trenches are formed; an oxide film disposed in the trench; and wiring disposed across a boundary between a trench region of the substrate in which the trench is formed and a non-trench region in which the semiconductor element is formed without the trench, from the non-trench region to the trench region, wherein the wiring covers a portion of a wall surface forming the trench, the trench and the oxide film are formed to extend in a first direction in a planar view of the substrate, and the wiring extends in a second direction intersecting the first direction in a planar view of the substrate, the method comprising: measuring a first resistance value of the wiring when the oxide film has a first thickness; measuring a second resistance value of the wiring when the oxide film has a second thickness smaller than the first thickness; measuring the second thickness based on the first resistance value and the second resistance value; A method for measuring an oxide film thickness of a semiconductor device comprising the steps of:
[0074] (Appendix 9) The method for measuring an oxide film thickness of a semiconductor device according to claim 7 or 8, wherein the semiconductor device is formed along a scribe line of the substrate. [Explanation of symbols]
[0075] 1. Trench 1A Wall 2. Oxide film 3. Wiring 4 Step 10 Semiconductor elements 20 Substrate 30 boundaries 31 Crossing 40 Meandering section 100 Semiconductor device
Claims
1. a substrate in which a semiconductor device and one or more trenches are to be formed; an oxide film disposed within the trench; a wiring arranged across a boundary between a trench region of the substrate in which the trench is formed and a non-trench region in which the semiconductor element is formed without the trench, from the non-trench region to the oxide film of the trench region; Equipped with The wiring covers a portion of a wall surface that forms the trench.
2. The wiring is formed in a meandering shape having a plurality of meandering portions when the substrate is viewed in a plan view, The semiconductor device according to claim 1 , wherein the boundary is formed along the meandering portion when the substrate is viewed in a plan view.
3. the trench and the oxide film are formed to extend in a first direction in the substrate when the substrate is seen in a plan view, 2 . The semiconductor device according to claim 1 , wherein the wiring extends in a second direction intersecting the first direction in a plan view of the substrate, and has a portion that crosses the trench and the oxide film.
4. The semiconductor device according to claim 3 , wherein the trenches and the oxide films are arranged in a plurality at intervals in the second direction.
5. 4. The semiconductor device according to claim 3, wherein said wiring is formed in a meandering shape so as to intermittently cross said trench and said oxide film in said first direction.
6. The semiconductor device according to claim 1 , wherein the semiconductor device is formed on a scribe line of the substrate.
7. 1. A method for measuring an oxide film thickness of a semiconductor device comprising: a substrate in which a semiconductor element and one or more trenches are formed; an oxide film disposed in the trench; and wiring disposed across a boundary between a trench region of the substrate in which the trench is formed and a non-trench region in which the semiconductor element is formed without the trench, the non-trench region, and the oxide film in the trench region, the wiring covering a portion of a wall surface forming the trench, the method comprising: measuring a first resistance value of the wiring when the oxide film has a first thickness; measuring a second resistance value of the wiring when the oxide film has a second thickness smaller than the first thickness; a measuring step of measuring the second thickness based on the first resistance value and the second resistance value; A method for measuring an oxide film thickness of a semiconductor device comprising the steps of:
8. 1. A method for measuring an oxide film thickness of a semiconductor device comprising: a substrate in which a semiconductor element and one or more trenches are formed; an oxide film disposed in the trench; and wiring disposed across a boundary between a trench region of the substrate in which the trench is formed and a non-trench region in which the semiconductor element is formed without the trench, from the non-trench region to the trench region, wherein the wiring covers a portion of a wall surface forming the trench, the trench and the oxide film are formed to extend in a first direction in a planar view of the substrate, and the wiring extends in a second direction intersecting the first direction in a planar view of the substrate, the method comprising the steps of: measuring a first resistance value of the wiring when the oxide film has a first thickness; measuring a second resistance value of the wiring when the oxide film has a second thickness smaller than the first thickness; a measuring step of measuring the second thickness based on the first resistance value and the second resistance value; A method for measuring an oxide film thickness of a semiconductor device comprising the steps of:
9. 9. The method for measuring an oxide film thickness of a semiconductor device according to claim 7, wherein the semiconductor device is formed on a scribe line of the substrate.
Citation Information
Patent Citations
Semiconductor device and method for manufacturing the same
JP2023017246A