Semiconductor device and oxide film thickness measurement method for semiconductor device
The semiconductor device's electrode configuration facilitates efficient oxide film thickness measurement through capacitance analysis, addressing inefficiencies in conventional methods and enhancing production speed and quality.
Patent Information
- Application Number
- JP2023053700
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-29
- Publication Date
- 2024-10-10
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Conventional methods for measuring oxide film thickness in semiconductor devices are inefficient and time-consuming, particularly in mass production, making it difficult to ensure appropriate insulation and prevent time-dependent dielectric breakdown (TDDB).
A semiconductor device configuration with a first electrode having a main body covering the trench region and an extending portion towards the oxide film, allowing capacitance measurement to determine oxide film thickness without cutting the device or checking I-V characteristics.
Enables easy and accurate measurement of oxide film thickness, reducing manufacturing time and maintaining device integrity by preventing parasitic transistors and ensuring proper insulation without reducing the active area.
Smart Images

Figure 2024141852000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a semiconductor device and an oxide film thickness measuring method for a semiconductor device. [Background technology]
[0002] As a conventional semiconductor device, a semiconductor device having an STI structure has been disclosed (for example, Patent Document 1). In a semiconductor device having an STI structure, an oxide film is formed so as to fill one or more trenches formed on the surface of a substrate, and the surface of the oxide film is planarized. As a result, multiple semiconductor elements formed on the surface of the substrate are insulated by the trenches.
[0003] Here, if the thickness of the oxide film is small, the shoulder of the trench may be exposed, or the oxide film formed on the shoulder may become thin. This may result in a parasitic transistor between the semiconductor elements, and the characteristics of the transistor may change from the desired characteristics. In addition, the withstand voltage of the oxide film may decrease, making it easier for time-dependent dielectric breakdown (TDDB) to occur. Therefore, in order to properly insulate the semiconductor elements, it is important to ensure the thickness of the oxide film in which the trench is buried. The shoulder of the trench is a region near the boundary between the trench region where the trench is formed and the non-trench region where the semiconductor element is formed without the trench.
[0004] In order to prevent TDDB and the like, conventional semiconductor device manufacturing processes employ methods for checking whether an oxide film has an appropriate thickness, such as cutting the semiconductor device and checking the cross section of the oxide film, or checking the current-voltage characteristics (IV characteristics) of a transistor. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2023-017246 A Summary of the Invention [Problem to be solved by the invention]
[0006] However, with the conventional techniques, it is difficult to measure the thickness of the oxide film on all mass-produced semiconductor devices, and there is room for improvement in shortening the manufacturing time of semiconductor devices.
[0007] In view of the above circumstances, an object of the present invention is to provide a semiconductor device that allows the thickness of an oxide film to be easily measured, and a method for measuring the thickness of an oxide film of a semiconductor device. [Means for solving the problem]
[0008] In order to solve the above problems, the semiconductor device of the present invention is a semiconductor device formed on a scribe line of a substrate in which a semiconductor element and one or more trenches are formed, and includes an oxide film disposed in the trench, and a first electrode having a main body portion covering a trench region in which the trenches of the substrate are formed and an extension portion extending from the main body portion toward the oxide film.
[0009] In order to solve the above-mentioned problems, the present invention provides a method for measuring an oxide film thickness of a semiconductor device comprising: a substrate in which a semiconductor element and one or more trenches are formed; an oxide film disposed in the trench; and a first electrode having a main body portion covering a trench region of the substrate in which the trench is formed and an extension portion extending from the main body portion toward the oxide film, the method being formed in a scribe line of the substrate, the method including the steps of: measuring a first capacitance of the first electrode when the oxide film has a first thickness; measuring a second capacitance of the first electrode when the oxide film has a second thickness that is thinner than the first thickness; and measuring the second thickness based on the first capacitance and the second capacitance. Effect of the Invention
[0010] According to the present invention, it is possible to provide a semiconductor device that allows easy measurement of the thickness of an oxide film, and a method for measuring the thickness of an oxide film of a semiconductor device. [Brief description of the drawings]
[0011] [Figure 1] FIG. 1 is a plan view of a wafer including a semiconductor device according to an embodiment of the present disclosure. [Figure 2A] FIG. 2A is a diagram showing a configuration of a semiconductor device according to an embodiment of the present disclosure. [Figure 2B] FIG. 2B is a diagram showing a configuration of a semiconductor device according to an embodiment of the present disclosure. [Figure 2C] FIG. 2C is a diagram for explaining the surface area of the main body portion. [Figure 3A] FIG. 3A is a diagram for explaining the correlation between the thickness of the oxide film 2 and the capacitance of the first electrode 30. As shown in FIG. [Figure 3B] FIG. 3B is a diagram for explaining the correlation between the thickness of the oxide film 2 and the capacitance of the first electrode 30. As shown in FIG. [Figure 3C] FIG. 3C is a diagram for explaining the correlation between the thickness of the oxide film 2 and the capacitance of the first electrode 30. As shown in FIG. [Figure 4] FIG. 4 is a diagram for explaining a method for measuring an oxide film thickness of a semiconductor device according to an embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Hereinafter, an embodiment will be described with reference to the drawings. Note that the same or similar reference numerals are used to designate the same functions or configurations, and the description thereof will be omitted as appropriate.
[0013] [Embodiment] (Configuration of Semiconductor Device) FIG. 1 is a plan view of a wafer including a semiconductor device according to an embodiment of the present disclosure.
[0014] The wafer W is a semiconductor substrate on which the semiconductor element 10 is formed. Specifically, the wafer is a Si substrate containing Si (silicon). Note that the wafer W is not limited to a Si substrate, and may be a substrate containing SiC (silicon carbide) or a substrate containing GaAs (gallium arsenide).
[0015] The wafer W is provided with a scribe line region SL and an active region AC of a predetermined width. A semiconductor device 100 is formed as a test element group (TEG) in the scribe line region SL. The active region AC may be interpreted as a non-trench region of the wafer W where a trench, which will be described later, is not formed. Region X shown in FIG. 1 is a region of the multiple scribe line regions SL where the semiconductor device 100 is formed. The configuration of the semiconductor device 100 will be described with reference to FIGS. 2A, 2B, and 2C.
[0016] 2A and 2B are diagrams showing the configuration of a semiconductor device according to an embodiment of the present disclosure. Fig. 2A shows an enlarged view of region X in Fig. 1. Fig. 2B shows a cross section of the semiconductor device 100 shown in Fig. 2A taken along line AA.
[0017] 2A and 2B, the left side shows a semiconductor device 100 provided in a trench region TC of a substrate 20. The right side shows a second electrode 30A provided in an active region AC of the substrate 20.
[0018] The semiconductor device 100 includes a substrate 20 which is a part of a wafer W (FIG. 1), an oxide film 2 disposed in a trench 1, and a first electrode 30.
[0019] One or more trenches 1 are formed in a trench region TC of the substrate 20. The trenches 1 are arranged at intervals in a direction D1. The material of the oxide film 2 can be appropriately selected depending on the application, purpose, etc., and one example is a silicon oxide film.
[0020] The first electrode 30 is an electrode corresponding to a gate electrode, a drain electrode, a source electrode, etc. formed in the trench region TC. The material of the first electrode 30 can be appropriately selected depending on the application, purpose, etc., and one example is Poly Si (porous silicon).
[0021] The first electrode 30 has a main body 31 covering the trench region TC and a plurality of extensions 32 extending from the main body 31 toward the oxide film 2 in the trench 1. The first electrode 30 may be interpreted as an electrode having a plurality of protrusions formed on the surface of a plate-shaped electrode.
[0022] The main body 31 is provided in the trench region TC of the substrate 20 while covering the openings of each of the multiple trenches 1. The main body 31 is a rectangular electrode when the substrate 20 is viewed in plan.
[0023] The extension portion 32 is a convex conductive member protruding from the main body portion 31 toward the upper surface of the oxide film 2. The direction D2 in which the extension portion 32 extends is a direction intersecting the direction D1. The extension portion 32 may be interpreted as a part of the main body portion 31. By forming the extension portion 32 in the main body portion 31, a part of the main body portion 31 has a shape protruding toward the upper surface of the oxide film 2 in the trench 1.
[0024] Here, it is desirable that the surface area of the main body 31 is approximately equal to the surface area of the plate-like second electrode 30A provided in the active region AC. Approximately equal may be interpreted as including a difference between the surface area of the main body 31 and the surface area of the second electrode 30A being equal to or less than a specific dimension corresponding to a manufacturing tolerance. The second electrode 30A is a plate-like electrode provided in the active region AC (non-trench region).
[0025] 2C is a diagram for explaining the surface area of the main body part. The main body part 31 has a flat facing surface 31a facing the substrate 20. The main body part 31 is configured such that the area of a portion (second region A2) of the entire surface of the main body part 31 excluding a portion (first region A1) facing the openings of the multiple trenches 1 is equal to the entire surface area of the second electrode 30A (see FIG. 2A).
[0026] When the oxide film 2 is embedded shallowly in the trench 1, i.e., when the thickness of the oxide film 2 is small, the extension portion 32 is formed, and the surface area of the extension portion 32 is added to the surface area of the main body portion 31 (second region A2).
[0027] When the surface area of the main body 31 is approximately equal to the surface area of the plate-like second electrode 30A provided in the active region AC, the sum of the surface areas of the main body 31 and the extensions 32, i.e., the surface area of the entire first electrode 30, is larger than the surface area of the entire second electrode 30A. As the thickness of the oxide film 2 in the trench 1 decreases, the number and extension amount of the extensions 32 increase, and the surface area of the first electrode 30 becomes even larger.
[0028] When the surface area of the first electrode 30 is increased in this way, the capacitance of the first electrode 30 increases, so the thickness of the oxide film 2 in the trench 1 can be measured by measuring the amount of change in the capacitance of the first electrode 30 based on the capacitance of the second electrode 30A. The capacitance may be interpreted as an amount representing the ability of a conductor to store electric charge, and may also be interpreted as electrostatic capacitance. The capacitance may also be interpreted as parasitic capacitance. A specific example of a method for measuring the thickness of the oxide film 2 will be described later.
[0029] (Method of manufacturing a semiconductor device) Next, a method for manufacturing the semiconductor device 100 will be briefly described.
[0030] First, a silicon oxide film is formed so as to cover the active region AC of the substrate 20. Next, a silicon nitride film is formed so as to cover the silicon oxide film by using a known CVD (Chemical Vapor Deposition) method. Next, the silicon oxide film and the silicon nitride film are patterned by using known photolithography and etching techniques.
[0031] Next, the substrate 20 is etched using the silicon oxide film and silicon nitride film as a mask, thereby forming a trench 1 in the substrate 20. Next, an oxide film 2 made of an insulator such as SiO2 is formed to cover the substrate 20 using a known CVD method. The oxide film 2 is formed to a thickness that covers the upper surfaces of the silicon oxide film and silicon nitride film. The oxide film 2 is filled into the trench 1 formed in the previous process.
[0032] Next, the oxide film 2 is planarized by a known CMP (Chemical Mechanical Polishing) method. Specifically, in planarization by the CMP method, the oxide film 2 is polished while a polishing liquid (slurry) is flowed. Next, the silicon oxide film and the silicon nitride film are removed by etching.
[0033] Next, an insulating film is formed on the substrate 20 using a known thermal oxidation method. Then, a polysilicon film is formed on the insulating film using a known CVD method. Next, the insulating film and the polysilicon film are patterned using known photolithography and etching techniques to form the first electrode 30.
[0034] Next, a description will be given of the correlation between the thickness of the oxide film 2 and the capacitance of the first electrode 30. FIGS. 3A, 3B, and 3C are diagrams for explaining the correlation between the thickness of the oxide film 2 and the capacitance of the first electrode 30.
[0035] 3A shows a cross section of a normally formed oxide film 2 and a main body portion 31. When the oxide film 2 is normally formed, the upper surface of the oxide film 2 and the upper surface of the trench region TC (the upper surface of the substrate 20) are located at substantially the same height, and no step occurs between the oxide film 2 and the upper surface of the trench region TC. Therefore, the extension portion 32 shown in FIG. 2B is not formed in the main body portion 31, and the cross section of the main body portion 31 is flat and plate-like.
[0036] Fig. 3B shows an oxide film 2 that is thinner than the oxide film 2 in Fig. 3A. When the thickness of the oxide film 2 is small relative to the depth of the trench 1, the position of the upper surface of the oxide film 2 differs from the position of the upper surface of the trench region TC, and a step occurs between the oxide film 2 and the upper surface of the trench region TC. For this reason, in the step of forming the first electrode 30, the extension portion 32 is formed inside the trench 1.
[0037] The surface area of the first electrode 30 having the extensions 32 formed thereon is larger than the surface area of the main body 31 shown in Fig. 3A. When the surface area is increased in this manner, the capacitance of the first electrode 30 is larger than the capacitance of the second electrode 30A shown in Fig. 2B.
[0038] 3C shows an even thinner oxide film 2. As the oxide film 2 becomes thinner as shown in FIG. 3C, the surface area of the first electrode 30 becomes larger, and the capacitance of the first electrode 30 becomes even larger.
[0039] As described above, since there is a correlation between the thickness of the oxide film 2 and the capacitance of the first electrode 30, it is possible to measure the thickness of the oxide film 2 by measuring the capacitance of the first electrode 30. A method for measuring the thickness of the oxide film of the semiconductor device 100 will be described with reference to FIG.
[0040] (Oxide film thickness measurement method) Fig. 4 is a diagram for explaining a method for measuring the oxide film thickness of a semiconductor device according to an embodiment of the present disclosure. Fig. 4 shows a graph in which the horizontal axis represents the thickness of the oxide film 2 and the vertical axis represents the capacitance of the first electrode 30. A number of data points (points a, b, and c) indicating the thickness of the oxide film 2 and the capacitance of the first electrode 30 are plotted on the graph.
[0041] Tha corresponding to point a represents the thickness of the oxide film 2 shown in FIG. 3C, and Ca corresponding to point a represents the capacitance of the first electrode 30 shown in FIG. 3C.
[0042] Thb corresponding to point b represents the thickness of the oxide film 2 shown in FIG. 3B, and Cb corresponding to point b represents the capacitance of the first electrode 30 shown in FIG. 3B.
[0043] Thc corresponding to point c represents the thickness of oxide film 2 shown in FIG. 3A, and Cc corresponding to point c represents the capacitance of main body portion 31 shown in FIG. 3A.
[0044] 4, as the thickness of the oxide film 2 decreases with respect to Thc, the capacitance of the first electrode 30 tends to increase with respect to Cc. Since there is a correlation between the thickness of the oxide film 2 and the capacitance of the first electrode 30, it is possible to measure the thickness of the oxide film 2 embedded in the trench 1 by measuring the capacitance of the first electrode 30.
[0045] The oxide film thickness measuring method according to the embodiment includes a step of measuring a first capacitance of the first electrode 30 when the oxide film 2 has a first thickness, and a step of measuring a second capacitance of the first electrode 30 when the oxide film 2 has a second thickness smaller than the first thickness. Furthermore, the oxide film thickness measuring method according to the embodiment includes a measuring step of measuring the second thickness based on the measured first capacitance and second capacitance.
[0046] Specifically, the difference between Cc and Cb, the difference between Cc and Ca, etc. are collected in advance, and data correlating the measured value of the thickness of the oxide film 2 when these are detected with the difference is stored in a memory. After that, the capacitance of the first electrode 30 of the semiconductor device 100 provided on the wafer W shown in FIG. 1 is measured, and the measured capacitance is compared with the above data, thereby making it possible to measure the thickness of the oxide film 2.
[0047] As a result, for example, when the measured capacitance (e.g., Cb) is within a specific range based on the capacitance (Cc) at point c, it can be determined that the oxide film embedded in the trench of the active region AC in which the semiconductor element 10 shown in Fig. 1 is formed is formed normally. On the other hand, when the measured capacitance is not within the specific range, it can be determined that the oxide film is thin, that is, that the oxide film is not formed normally.
[0048] As described above, the capacitance of the second electrode 30A (FIG. 2A) provided in the active region AC may be measured, and the thickness of the oxide film may be determined based on the capacitance. Specifically, when the capacitance (e.g., Cb) of the first electrode 30 is within a specific range based on the capacitance of the second electrode 30A, it can be determined that the oxide film embedded in the trench of the active region AC in which the semiconductor element 10 shown in FIG. 1 is formed is formed normally. On the other hand, when the measured capacitance is not within the specific range, it can be determined that the oxide film is thin, that is, that the oxide film is not formed normally.
[0049] (Other embodiments) As described above, when the thickness of the oxide film 2 is small, the shoulder of the trench 1 may be exposed or the oxide film 2 formed on the shoulder may become thin, and it is known that the thinner the oxide film 2, the lower the breakdown voltage of the semiconductor device 100. In particular, when the oxide film 2 on the shoulder of the trench 1 is thin, parasitic capacitance occurs, and the semiconductor device 100 may not have the desired characteristics. Therefore, it is important to measure the thickness of the oxide film 2 with high accuracy.
[0050] In order to accurately measure the thickness of the oxide film 2, the oxide film thickness measuring method according to the embodiment of the present disclosure may include a step of measuring the breakdown voltage of the semiconductor device 100 in addition to the above-mentioned step of measuring the capacitance. Specifically, the oxide film thickness measuring method according to the embodiment may include a step of measuring a first breakdown voltage of the semiconductor device 100 when the oxide film 2 has a first thickness, and a step of measuring a second breakdown voltage of the semiconductor device 100 when the oxide film 2 has a second thickness. Furthermore, the oxide film thickness measuring method according to the embodiment may include a measuring step of measuring the second thickness based on the first breakdown voltage and the second breakdown voltage.
[0051] More specifically, data associating the breakdown voltage of the semiconductor device 100 with the thickness of the oxide film 2 is stored in a memory. Thereafter, the breakdown voltage (the first and second breakdown voltages described above) of the first electrode 30 of the semiconductor device 100 provided on the wafer W shown in FIG. 1 is measured, and the measured breakdown voltage is compared with the above data to measure the thickness of the oxide film 2 (the second thickness described above). In this way, by measuring the breakdown voltage of the semiconductor device 100 in addition to measuring the capacitance described above, the accuracy of measuring the thickness of the oxide film 2 can be improved.
[0052] (Action and effect) As described above, the semiconductor device 100 according to an embodiment of the present disclosure includes a first electrode 30 having a main body portion 31 covering a trench region TC in which a trench 1 of a substrate 20 is formed, and an extension portion 32 extending from the main body portion 31 toward the oxide film 2.
[0053] With this configuration, the capacitance of the first electrode 30 increases as the thickness of the oxide film 2 decreases, so it is possible to measure the thickness of the oxide film 2 embedded in the trench 1 by measuring the capacitance of the first electrode 30. This makes it possible to easily measure the thickness of the oxide film in the STI structure without cutting the semiconductor device formed in the active region AC to check the cross section of the oxide film or checking the IV characteristics of the transistor formed in the active region AC. This makes it possible to shorten the manufacturing time of mass-produced semiconductor devices.
[0054] Furthermore, the semiconductor device 100 according to the embodiment can measure the thickness of the oxide film 2 without narrowing the active area AC by being formed on the scribe line (scribe line region SL) of the substrate 20. Therefore, it becomes possible to easily measure the thickness of the oxide film in the STI structure without reducing the manufacturing quantity of mass-produced semiconductor devices.
[0055] In addition, the following supplementary notes are provided in relation to the above description.
[0056] (Appendix 1) A semiconductor device formed on a scribe line of a substrate in which a semiconductor element and one or more trenches are formed, the semiconductor device comprising: an oxide film disposed in the trench; and a first electrode having a main body portion covering a trench region of the substrate in which the trenches are formed and an extension portion extending from the main body portion toward the oxide film.
[0057] (Appendix 2) 2. The semiconductor device according to claim 1, wherein a surface area of the main body portion is equal to a surface area of a second electrode provided in a non-trench region where the trench is not formed and the semiconductor element is formed.
[0058] (Appendix 3) 3. The semiconductor device according to claim 1, wherein a plurality of the trenches are provided, and the extension portion is disposed in each of the plurality of the trenches.
[0059] (Appendix 4) 1. A method for measuring an oxide film thickness of a semiconductor device formed in a scribe line of a substrate, the method comprising: a substrate in which a semiconductor element and one or more trenches are formed; an oxide film disposed in the trench; and an electrode having a main body portion covering a trench region of the substrate in which the trench is formed and an extension portion extending from the main body portion toward the oxide film, the method including the steps of: measuring a first capacitance of the electrode when the oxide film has a first thickness; measuring a second capacitance of the electrode when the oxide film has a second thickness that is thinner than the first thickness; and measuring the second thickness based on the first capacitance and the second capacitance.
[0060] (Appendix 5) 5. The method for measuring an oxide film thickness of a semiconductor device according to claim 4, wherein the surface area of the main body portion is equal to the surface area of a second electrode provided in a non-trench region where the trench is not formed and the semiconductor element is formed.
[0061] (Appendix 6) 6. The method for measuring an oxide film thickness of a semiconductor device according to claim 4 or 5, comprising: a step of measuring a first breakdown voltage of the semiconductor device when the oxide film has the first thickness; a step of measuring a second breakdown voltage of the semiconductor device when the oxide film has the second thickness; and a measurement step of measuring the second thickness based on the first breakdown voltage and the second breakdown voltage. [Explanation of symbols]
[0062] 1. Trench 2. Oxide film 10 Semiconductor elements 20 Substrate 30 1st electrode 30A 2nd electrode 31 Main body 31a Opposite side 32 Stretching section 100 Semiconductor device
Claims
1. 1. A semiconductor device formed in a scribe line of a substrate in which a semiconductor element and one or more trenches are formed, comprising: an oxide film disposed within the trench; a first electrode having a main body portion covering a trench region in which a trench is formed in the substrate and an extension portion extending from the main body portion toward the oxide film; A semiconductor device comprising:
2. 2 . The semiconductor device according to claim 1 , wherein a surface area of said main body portion is equal to a surface area of a second electrode provided in a non-trench region where said trench is not formed and said semiconductor element is formed.
3. The trenches are provided in plurality, The semiconductor device according to claim 1 , wherein the extension portion is disposed in each of the plurality of trenches.
4. 1. A method for measuring an oxide film thickness of a semiconductor device formed in a scribe line of a substrate, the method comprising: a substrate in which a semiconductor element and one or more trenches are formed; an oxide film disposed in the trench; and a first electrode having a main body portion covering a trench region of the substrate in which the trench is formed and an extension portion extending from the main body portion toward the oxide film, the method comprising the steps of: measuring a first capacitance of the first electrode when the oxide film is at a first thickness; measuring a second capacitance of the first electrode when the oxide film has a second thickness that is less than the first thickness; measuring the second thickness based on the first volume and the second volume; A method for measuring an oxide film thickness of a semiconductor device comprising the steps of:
5. 5. The method of measuring an oxide film thickness of a semiconductor device according to claim 4, wherein a surface area of said main body portion is equal to a surface area of a second electrode provided in a non-trench region where said trench is not formed and said semiconductor element is formed.
6. measuring a first breakdown voltage of the semiconductor device when the oxide film has the first thickness; measuring a second breakdown voltage of the semiconductor device when the oxide film has the second thickness; a measuring step of measuring the second thickness based on the first withstand voltage and the second withstand voltage; 6. The method for measuring an oxide film thickness of a semiconductor device according to claim 4, further comprising:
Citation Information
Patent Citations
Semiconductor device and method for manufacturing the same
JP2023017246A