Detection method, detection support device, detection support program, and detection support method

The method addresses laser-induced damage in SERS by using multi-scale nanostructures on a substrate for sensitive detection of trace substances, enhancing Raman scattering without substantial harm.

JP2024142015AActive Publication Date: 2024-10-10EVCARE CORP +1
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023053953
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-29
Publication Date
2024-10-10
Estimated Expiration
2043-03-29

AI Technical Summary

Technical Problem

Existing detection methods using surface-enhanced Raman scattering (SERS) cause damage to target substances due to the focusing of excitation lasers.

Method used

A detection method involving the use of a substrate with a multi-scale nanostructure, where a sample containing the substance is placed and irradiated with a laser beam, allowing for high-sensitivity detection while minimizing damage.

Benefits of technology

The method enables sensitive detection of trace amounts of substances with minimal damage, utilizing nanostructures formed by electrolytic reduction or metal colloid solutions to enhance Raman scattering intensity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

To provide a detection method for detecting a minute amount of detection target substance with high sensitivity in a state where the target substance is less damaged.SOLUTION: A detection method for detecting a substance is provided, including a radiation step of radiating a laser beam, and a measurement step of measuring Raman scattered light generated by the radiation of the laser beam. In the measurement step, a sample including the substance is placed on a substrate having a multi-scale nano structure, and the laser beam is radiated to perform the measurement.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a detection method, a detection support device, a detection support program, and a detection support method. [Background technology]

[0002] There are various methods for detecting substances, and methods capable of detecting minute amounts of substances are required in various fields.

[0003] Surface-Enhanced Raman Scattering (SERS) is a phenomenon in which the intensity of Raman scattering is greatly amplified when molecules are adsorbed on the surface of a precious metal with a nanoscale structure, compared to that on a bulk substrate. As a highly sensitive analytical method, SERS is used in a wide range of fields, including trace substance analysis, pathological diagnosis, environmental measurement, and food safety management.

[0004] Patent Document 1 discloses a method for detecting a substance by using surface-enhanced Raman scattering. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] Patent Publication No. 2020-204495 Summary of the Invention [Problem to be solved by the invention]

[0006] However, it is known that a problem exists in that the focused excitation laser can damage the material.

[0007] Therefore, the present disclosure has been made in consideration of the above problems, and its purpose is to provide a detection method that can detect trace amounts of a target substance with high sensitivity while causing minimal damage to the target substance. [Means for solving the problem]

[0008] According to the present disclosure, there is provided a detection method for detecting a substance, comprising an irradiation step of irradiating laser light and a measurement step of measuring Raman scattered light generated by the irradiation of the laser light, in which in the measurement step, a sample containing the substance is placed on a substrate having a multi-scale nanostructure, and the laser light is irradiated to perform measurement.

[0009] Other problems and solutions disclosed in this application will be made clear in the section on preferred embodiments of the invention and the drawings. Effect of the Invention

[0010] According to the present disclosure, it is possible to detect trace amounts of a target substance with high sensitivity while minimizing damage to the target substance. [Brief description of the drawings]

[0011] [Figure 1] This is an SEM image of AgNSsF5mMA. [Diagram 2] This is an SEM image of AgNSsF10mMA. [Diagram 3] This is an SEM image of AgNSsF15mMA. [Figure 4] FIG. 1 shows the Raman scattering spectrum of Cor / AgNSsF5mMA. [Diagram 5] FIG. 1 shows the Raman scattering spectrum of Cor / AgNSsF10mMA. [Figure 6] FIG. 1 shows the Raman scattering spectrum of Cor / AgNSsF15mMA. [Figure 7] FIG. 2 is a diagram showing the assignment of Raman scattering peaks. [Figure 8] FIG. 1 shows the Raman scattering spectrum of Cor / AgNPsF. [Figure 9] FIG. 1 shows a Raman scattering spectrum of Cor / Si. [Figure 10] FIG. 1 shows a Raman scattering spectrum of trisodium citrate. [Figure 11] FIG. 1 shows the Raman scattering spectra of AgNPs / Cor / Si, Cor+AgNPs / Si, and Cor / Si. [Figure 12] This is a microscope image taken during Raman scattering measurement of AgNPs / Cor / Si. [Figure 13] FIG. 1 shows the Raman scattering spectrum (OD0) of CorS1-6 / Si. [Figure 14] FIG. 1 shows the Raman scattering spectra (OD3) of AgNPs / CorS1-6 / Si and AgNPs / Si. [Figure 15] FIG. 13 shows Raman scattering measurements from the back surface of a well. [Figure 16] FIG. 1 shows the Raman scattering spectra (OD1) of AgNPs / CorS5 / Well, CorS5 / AuNPs / Well, CorS5 / AgNPs+AuNPs / Well, and CorS5 / Well. [Figure 17] FIG. 1 shows the Raman scattering spectrum (OD1) of AgNPs / CorS1-6 / Well. [Figure 18] FIG. 1 shows the baseline-corrected Raman scattering spectrum of AgNPs / CorS1-6 / Well. [Figure 19] FIG. 1 is a diagram illustrating an example of a configuration of a detection system according to the present disclosure. [Figure 20] FIG. 2 is a diagram showing a hardware configuration of an information processing device 16 according to the present disclosure. [Figure 21] FIG. 2 is a diagram showing a software configuration of an information processing device 16 in the present disclosure. [Figure 22] FIG. 1 is a diagram showing an example of a typical processing flow of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] The contents of the embodiment of the present invention will be listed and described below. One embodiment of the present invention has the following configuration. [Item 1] A method for detecting a substance, comprising: an irradiation step of irradiating with laser light; a measuring step of measuring Raman scattered light generated by irradiation with the laser light; Equipped with A detection method in which, in the measuring step, a sample containing the substance is placed on a substrate having a multi-scale nanostructure, and the laser light is irradiated to perform measurement. [Item 2] The nanostructure is formed by a compound containing a metal. Item 1. The detection method according to item 1. [Item 3] The nanostructures include nanostructures at least on the scale of 10-100 nm; 3. The detection method according to item 1 or 2. [Item 4] 4. The detection method according to item 3, wherein the nanostructure is formed by electrolytic reduction of metal ions or heating a metal colloid solution under reflux. [Item 5] When the nanostructure is formed by electrolytic reduction of metal ions, the electrolytic reduction is 5 mA / cm 2 to 15mA / cm 2 This is done by applying a current of The detection method according to claim 4.

[0013] <Details of the embodiment> Hereinafter, preferred embodiments of the present disclosure will be described in detail with reference to the accompanying drawings. In this specification and the drawings, components having substantially the same functional configurations are denoted by the same reference numerals, and redundant description will be omitted.

[0014] [Device configuration] As shown in FIG. 19, the Raman scattering spectrometer according to the embodiment of the present disclosure includes a laser light source 10, a beam splitter 11, an objective lens 12, a spectrometer 13, a CCD detector 14, a sample stage 15, and an information processing device 16. With a SERS chip 20 mounted on the sample stage 15 and a solution containing an analyte introduced into the chip 20, an excitation laser light is irradiated from the laser light source 10 and collected by the objective lens 12. The generated Raman scattered light is input to the spectrometer 13 via the objective lens 12 and the beam splitter 11 and dispersed. The CCD detector 14 is disposed so as to be able to measure a wave number range of a predetermined Raman shift. The Raman signal detected by the CCD detector 14 is sent to the information processing device 16, where it is analyzed, displayed, recorded, and the like. The information processing device 16 also controls the laser light source 10, the CCD detector 14, and the sample stage 15.

[0015] When performing Raman scattering measurement, the target may be a solid or a solution. In the present disclosure, the target is supported on a surface in a solution state, and the target that has become solid after the solvent evaporates is measured.

[0016] It is known that SERS can be observed when certain types of molecules are adsorbed on the surface of metals such as gold (Au) and silver (Ag). In order for SERS to occur, a "surface nanostructure" must be formed on the metal surface, which generates a strong surface electric field through the interaction of excitation light and the metal.

[0017] In the present disclosure, for example, a surface nanostructure is formed using a metal. A liquid to be measured is dropped onto the formed surface nanostructure, dried, and mounted on the sample stage 15. An excitation laser beam is irradiated to measure the Raman signal. The metal may be a noble metal such as gold, silver, or platinum, or may be any metal such as copper or aluminum that exhibits strong plasmon resonance.

[0018] In the present disclosure, the surface nanostructure includes structures such as those shown in Figures 1, 2, and 3. The surface nanostructure may have at least one nanoscale structure formed on the surface so as to come into contact with the detection target and be irradiated with laser light.

[0019] The surface nanostructure in the present disclosure may be, for example, a polyhedron (including an approximately polyhedron) or a granular structure as shown in FIG. 1. The surface nanostructure may have one or more faces of the polyhedron that are concave or convex to a certain degree, the faces themselves may be bent, or the places where the faces of the polyhedron meet may be curved rather than straight, but is not limited to such structures. In addition, the surface nanostructure in the present disclosure may have a structure in which multiple nanostructures including polyhedrons and granules of different scales (hereinafter referred to as multiple scales) are assembled, as shown in FIG. 2 and FIG. 3, and the assembled nanostructures may be, for example, flower-shaped as shown in FIG. 2 or branch-and-leaf-shaped as shown in FIG. 3, but is not limited thereto. Note that even if the substance to be detected is easily decomposed by laser light, for example, a multiple-scale nanostructure as shown in FIG. 2 and FIG. 3 is easy to detect the substance, and therefore is considered to have a property that the target substance is not easily decomposed by excitation laser light.

[0020] The surface nanostructure in the present disclosure may include structures with particle sizes on the scale of 1 nm-10 nm, 10 nm-50 nm, 50-100 nm, 100 nm-200 nm, 200 nm-500, 500 nm-1000 nm, 1 μm-2 μm, 3 μm-5 μm, and 6 μm-10 μm, for example, when the nanostructure is considered as a grain, and may be structures in which multiple scale nanostructures are independent from one another, as shown in the example of Figure 1, or may be structures formed by an assembly of multiple scale nanostructures, as shown in the examples of Figures 2 and 3.

[0021] In the following examples, multi-scale nanostructures are formed using several materials and under several conditions, but the materials and formation conditions are merely examples, and any materials and conditions that can form multi-scale nanostructures are acceptable.

[0022] In the following examples, cortisol was used as the target substance for detection. Cortisol is one of the hormones secreted from the adrenal cortex, and its main functions are known to be the promotion of metabolism such as gluconeogenesis in the liver, protein metabolism in muscles, and fat decomposition in adipose tissue, as well as anti-inflammatory and immunosuppressive effects. Cortisol is also called the stress hormone because it stimulates the sympathetic nerves when the human body feels stress and keeps the body in a state of tension. However, it goes without saying that the target substance for detection is not limited to cortisol.

[0023] [Example 1] Cortisol detection by surface-enhanced Raman scattering In this example, a nanostructure was formed using silver as an example of a metal. Specifically, a 10 g / L silver nitrate aqueous solution was prepared and subjected to electrical reduction to form silver nanostructures (AgNSs). The electrical reduction conditions were 5 mA / cm 2 , 90Sec., 10mA / cm 2 , 45Sec., 15mA / cm 2 The electrolytic reduction was carried out at a current density and time of 30 sec.

[0024] Figure 1 shows the current density of 5mA / cm 2 The AgNSs were prepared under the conditions of 10 mA / cm and 90 sec. 2 The AgNSs were prepared under the conditions of 15 mA / cm and 45 sec. 2The AgNSs were prepared under the conditions of 1 μm-2 μm, 3 μm-5 μm, and 6 μm-10 μm. The structure was on the order of several μm in size. In Fig. 1, the nanostructure was granular (at least one of the following: 1 μm-2 μm, 3 μm-5 μm, and 6 μm-10 μm in size; a structure on the order of several μm in size). In Fig. 2, the nanostructure was flower-shaped (at least one of the following: 10 nm-50 nm, 50-100 nm, and 100 nm-200 nm in size (a few tens of nm to 100 nm in size), which were formed by assembling them together). In Fig. 3, the nanostructure was branch-shaped (at least one of the following: 1 nm-10 nm, 10 nm-50 nm, and 50-100 nm in size (a few nm to tens of nm in size), which were formed by assembling them together).

[0025] Cortisol standard solution (Cor, 1.0 x 10 -9 mol / L) as the analyte, [A] 2 μL of Cor is dropped onto AgNSs5mA / ITO and dried (Cor / AgNSs5mA). [B] 2 μL of Cor is dropped onto AgNSs10mA / ITO and dried (Cor / AgNSs10mA). [C] 2 μL of Cor is dropped onto AgNSs15mA / ITO and dried (Cor / AgNSs15mA). Each sample was obtained.

[0026] These samples were placed on the sample stage 15 and subjected to microscopic Raman scattering spectrum analysis (excitation wavelength: 532 nm, microscope magnification: 100 times). Figures 4, 5, and 6 show the measurements of [A], [B], and [C], respectively.

[0027] Figure 7 shows the assignment of Raman scattering peaks. The peaks shown in standard type are cortisol peaks, those in italics are unknown peaks, and those in bold are peaks unrelated to the sample. Peaks that matched literature values ​​were confirmed. This demonstrated that each silver nanostructure can detect cortisol.

[0028] In addition, when measuring Raman scattering, in the case of [A], 10 times the amount of excitation light was used compared to [B] and [C]. From these facts, the order of the degree of enhancement of Raman scattering is [C]>[B]>>[A], so if stronger Raman scattering intensity is desired, it is desirable to use a finer, multi-scale nanostructure. When strong Raman scattering intensity is desired, the conditions for the electric reduction of an aqueous solution containing metal ions, for example a 10 g / L aqueous solution of silver nitrate, are set at 10 mA / cm. 2 It is desirable to have a value of 15mA / cm or more. 2 It may be more than 5mA / cm 2 Even if the excitation laser power is increased, detection is possible. The electric reduction conditions are 5 mA / cm 2 More than 10mA / cm 2 It may be less than 5mA / cm 2 More than 15mA / cm 2 It may be less than 10mA / cm 2 More than 15mA / cm 2 It may be the following.

[0029] On the other hand, the generation of amorphous carbon by the decomposition of cortisol is shown at 1300 cm in Figs. -1 , 1600cm -1 From the bulge in the baseline in the wavenumber region around 1000 mA, it can be said that 15 mA ≒ 10 mA >> 5 mA. Therefore, if you want to suppress the decomposition of a sample containing cortisol, condition [A] is preferable, but it is also possible to detect it under conditions [B] and [C]. If you want to suppress the decomposition of the substance to be detected, 5 mA / cm is the condition for the electric reduction of an aqueous solution containing metal ions, for example, a 10 g / L aqueous solution of silver nitrate. 2 It is desirable that the value is 10mA / cm or more. 2 More than 15mA / cm 2 Even if the excitation laser irradiation time is adjusted, detection is possible. 2 More than 10mA / cm 2 It may be less than 5mA / cm 2More than 15mA / cm 2 It may be less than 10mA / cm 2 More than 15mA / cm 2 It may be the following.

[0030] [Example 2] Exploration of methods for using silver nanoparticles suitable for detecting cortisol using surface-enhanced Raman scattering In this embodiment, a nanostructure was formed using silver colloid as an example of a metal colloid. A silver nanoparticle colloidal solution was synthesized using citrate ions as a protective agent. 36 mg of silver nitrate was dissolved in 200 mL of ultrapure water, which was heated and refluxed. 4 mL of 1 wt% aqueous solution of trisodium citrate was added thereto, and the mixture was heated and refluxed for another hour and allowed to cool to obtain a silver nanoparticle colloidal solution. Although not shown, a multi-scale nanostructure including at least nanostructures with particle sizes of 10 nm-50 nm and 50-100 nm (nanostructures on the scale of several tens of nm) was obtained. The concentrated silver nanoparticle solution (AgNPs) obtained by centrifuging, redispersing, and centrifuging the silver nanoparticle colloidal solution was used without redispersion [Non-Patent Document 2].

[0031] Cortisol standard solution (Cor) was used as the analyte. [D] According to previous reports, Cor was dropped onto a thin film of AgNPs accumulated at the hexane / water interface and then dried (Cor / AgNPsF) [Non-Patent Document 3, Non-Patent Document 4, Non-Patent Document 2]. [E] A solution containing Cor and AgNPs is dropped onto a silicon single crystal substrate (Si) and dried (Cor+AgNPs / Si). [F] Cor is dropped onto Si and dried (Cor / Si), then AgNPs are dropped onto the Cor surface and dried (AgNPs / Cor / Si). Each sample was obtained.

[0032] These samples were placed on the sample stage 15 and subjected to microscopic Raman scattering spectrum analysis (excitation wavelength: 532 nm, microscope magnification: 100 times). Except for trisodium citrate, the spectra measured at about 10 points for each sample were averaged.

[0033] Measurements were performed for Cor / AgNPsF using neutral density filters of 1 / 100 (OD2), 1 / 1000 (OD3), and 1 / 10000 (OD4) times (Figure 8). As a reference system, the Raman scattering spectrum of Cor / Si measured without using neutral density filters is shown in Figure 9, and the Raman scattering spectrum of trisodium citrate crystals used as a reducing agent and protective agent in the synthesis of silver nanoparticles is shown in Figure 10. The Raman scattering spectra of AgNPs / Cor / Si, Cor+AgNPs / Si, and Cor / Si are also shown in Figure 11.

[0034] Cortisol was measured in the solid state in both samples. Previous reports have shown that the characteristic peaks in the Raman scattering spectrum of solid-state cortisol are 1150, 1220-1240, 1330-1350, 1430-1450, 1610, and 1640 cm -1 These include the three characteristic broad peaks in Figure 9 [Non-Patent Document 5]. Furthermore, previously reported surface-enhanced Raman scattering spectra of cortisol solutions show peaks at 1150, 1270, 1340-1380, 1430-1450, and 1500 cm -1 It is said that a characteristic peak appears around this range, and it has been suggested that the wavenumber at which the characteristic peak appears may vary greatly depending on the state [Non-Patent Document 5]. This shows that when attempting to detect cortisol supported in the wells by surface-enhanced Raman scattering, as aimed at in this example, it is difficult to ignore the possibility that the Raman scattering wavenumber will be different when cortisol is supported in a "multiple layer" and when it is supported as a "single layer (isolated molecular system)."

[0035] On the other hand, in this embodiment, nanoparticles containing trisodium citrate as a protective agent were used, and therefore, as shown in FIG. -1 The Raman scattering signal that appears in the sample should not be used to confirm the presence and quantitation of cortisol.

[0036] From the above, in this embodiment, 1330-1350 and 1500 cm -1It is considered appropriate to mainly use the Raman scattering signal of the AgNPs / Cor / Si to confirm the presence and quantification of cortisol. Based on this, the results of Figures 8 and 11 show that, among the samples prepared, the Raman scattering signal of AgNPs / Cor / Si is significantly enhanced, and each peak appears more clearly than the other systems. In addition, the 1330-1350 and 1500 cm -1 Since the Raman scattering signal of the nanoparticles can be clearly observed, we decided to use the method of dropping a nanoparticle solution onto the Cor surface of Cor / Si as the method for using the nanoparticles in this study.

[0037] Moreover, the microscope image during the measurement of AgNPs / Cor / Si is shown in Figure 12. Point L in the center is the excitation laser light for the Raman scattering measurement. Enhanced Raman scattering occurs only at the locations of black spots such as point R, so black spots such as point R are considered to be aggregates of silver nanoparticles. To detect cortisol, it is sufficient to select and excite point R and obtain a Raman scattering spectrum. From Figure 12, it can be seen that a black spot of the same size as point R (cortisol) is 400 μm 2 It is believed that at least 20 such locations exist within the region, and enhanced Raman scattering signals can be obtained. Assuming that the quantitative nature of the measurement can be fully guaranteed, it is expected that a similar evaluation will be possible in an area that is orders of magnitude smaller than the 96-well plate that is often used in ELISA.

[0038] [Example 3] Detection of different concentrations of cortisol standard solutions by surface-enhanced Raman scattering Concentrated silver nanoparticle solution (AgNPs) obtained in the same manner as in Example 2 was used without redispersion. 3, 1, 0.33, 0.11, 0.037, and 0.012 μg / dL of cortisol standard solutions (CorS1, CorS2, CorS3, CorS4, CorS5, and CorS6, respectively) were used as analytes, and 1 μL of each was dropped onto a single crystal silicon substrate (Si), dried, and then supported (Cor1-6 / Si). 1 μL of AgNPs was dropped onto the Cor side surface of Cor1-6 / Si, and dried (AgNPs / CorS1-6 / Si). As a reference system, AgNPs was dropped onto Si and dried (AgNPs / Si). Microscopic Raman scattering measurements were performed under the following conditions: excitation wavelength: 532 nm, microscope magnification: 100 times, acquisition time: 5 seconds, and number of integrations: none (one-shot measurement). The spectra measured at approximately 10 points were averaged.

[0039] The Raman scattering spectrum of CorS1-6 / Si measured without using a neutral density filter (OD0) is shown in Figure 13, and the Raman scattering spectra of AgNPs / CorS1-6 / Si and AgNPs / Si measured with a 1 / 1000 neutral density filter (OD3) are shown in Figure 14.

[0040] In the section shown by A in Figure 13, the results are for CorS4 / Si, CorS5 / Si, CorS2 / Si, CorS6 / Si, CorS3 / Si, and CorS1 / Si from top to bottom. In the case of CorS1-6 / Si, the Raman scattering intensity did not correspond to the change in the concentration of CorS1-6. In addition, the 1450 cm characteristic of the spectrum when solid cortisol is irradiated with strong light was not observed. -1 In Figure 13, for AgNPs / CorS1-6 / Si, the scattering peaks at 1330-1350 and 1500 cm -1 In addition, no clear Raman scattering signal was observed in the spectrum of CorS1-6 / Si, and the spectrum of CorS1-6 / Si was partially included. Although detailed attribution is difficult, many new Raman scattering peaks due to the presence of cortisol were observed. It is possible that denaturation has occurred due to a local temperature rise caused by the Raman scattering measurement.

[0041] In addition, in the section shown by B in Figure 14, the results are, from the top, AgNPs / CorS5 / Si, AgNPs / CorS6 / Si, AgNPs / CorS2 / Si, AgNPs / CorS1 / Si, AgNPs / CorS3 / Si, AgNPs / CorS4 / Si, and AgNPs / Si. As shown in Figure 14, the concentration of CorS1-6 does not correspond to the Raman scattering signal intensity, as in the case of CorS1-6 / Si shown in Figure 13. This can be explained by the fact that when AgNPs are dropped, the base CorS1-6 is dissolved, and CorS1-6 is re-concentrated in the gaps of the AgNPs aggregates and becomes a solid.

[0042] Generally, the areas where the localized surface plasmon resonance electric field is extremely strong are nanogap (groove)-like areas that occur in nanoparticle aggregates, which corresponds well to the phenomenon observed in this section. For this reason, if an extremely low concentration of cortisol is used as the analysis target so as not to cause local concentration of cortisol, or if a method is used to analyze cortisol that is firmly bound to some surface, it is expected that a Raman scattering spectrum closer to that of a single molecule of cortisol can be obtained. In addition, the intensity of the Raman scattering spectrum of AgNPs / Si is significantly lower than that of AgNPs / CorS1-6 / Si, and it is considered that it does not have a significant effect on the spectrum of AgNPs / CorS1-6 / Si.

[0043] [Example 4] Cortisol detection by surface-enhanced Raman scattering in cortisol evaluation wells As in Examples 2 and 3, gold and silver nanoparticle colloidal solutions were synthesized using citrate ions as a protective agent according to previous reports (synthesis conditions that yield gold nanoparticles with a particle size of approximately 15-20 nm) [Non-Patent Documents 4, 6, and 7]. A concentrated gold nanoparticle solution (AuNPs) obtained by centrifugation of the gold nanoparticle solution was used without redispersion [Non-Patent Documents 8 and 2]. A concentrated silver nanoparticle solution (AgNPs) obtained by the same method as in the previous section was used as the silver nanoparticle solution without redispersion [Non-Patent Document 2].

[0044] In the wells for cortisol evaluation by EIA method, 3, 1, 0.33, 0.11, 0.037, and 0.012 μg / dL cortisol standard solutions (CorS1, CorS2, CorS3, CorS4, CorS5, and CorS6, respectively) were loaded as analytes (CorS1-6 / Well). 1 μL of AgNPs, AuNPs, and an equal mixture of AgNPs and AuNPs (AgNPs+AuNPs) were dropped into these wells to prepare Raman scattering samples (AgNPs / CorS1-6 / Well, AuNPs / CorS1-6 / Well, AgNPs+AuNPs / CorS1-6 / Well). The Raman scattering measurements were performed under the following conditions: excitation wavelength: 532 nm, microscope magnification: 50x, acquisition time: 1 second, and number of integrations: none (1-shot measurement), and the spectra measured at approximately 10 points were averaged. Note that, when measuring the Raman scattering, excitation was performed from the back side of the well (for example, the part indicated by C in Figure 15) and scattered light was obtained.

[0045] The Raman scattering spectra of AgNPs / CorS5 / Well, CorS5 / AuNPs / Well, CorS5 / AgNPs+AuNPs / Well, and CorS5 / Well are shown in Figure 9. A neutral density filter of 1 / 10 (OD1) was used.

[0046] In Figure 16, when AgNPs were used, a significantly higher Raman scattering intensity was obtained compared to the other examples. -1 The Raman scattering peaks at 1350 and 1500 cm were clearly observed when AgNPs were used in combination with AuNPs compared to when only AuNPs were used. -1 Although there was a tendency for the Raman scattering peak of gold nanoparticles to become higher, no positive synergistic effect was observed in this system due to the simultaneous use of gold nanoparticles and silver nanoparticles [Non-Patent Documents 9-11].

[0047] The Raman scattering spectrum of AgNPs / CorS1-6 / Well is shown in Figure 17, and the spectrum with the baseline subtracted as a straight line is shown in Figure 18.

[0048] In the CorS2-6 region, the 1330-1350 and 1500 cm peaks are used as markers for cortisol. -1 The Raman scattering peaks of amorphous carbon, which is expected to be generated by thermal decomposition of the sample, were clearly observed at 1350 and 1600 cm. -1 The proportion of broad scattering peaks with the peak wavenumbers of and are high. This can be a major factor in impairing quantitative performance. This is a feature also seen in Examples 2 and 3, and it is thought that this can be addressed by reducing the excitation light density or by taking measures to prevent nanoparticles from approaching each other too closely when they aggregate.

[0049] In fact, the Raman scattering intensity of this series of samples does not correspond to the concentration change up to CorS1-6, and cannot be used for quantification within this range of concentration conditions. On the other hand, when the relatively low concentration standard sample CorS5-6 is used, the Raman scattering intensity corresponds well to the concentration change, and it is desirable to study using a cortisol solution with an even lower concentration range.

[0050] The area required for one measurement (corresponding to one hole in a well) is 20 μm when using a 100x microscope optical system. 2 This indicates the possibility of significantly reducing the absolute amount of antibody required for quantitative analysis using EIA, ELISA, etc.

[0051] The exposure time required to measure one point was as short as 1 second (due to the performance of the equipment used), and it was found that even if multiple points were measured and it took 2 seconds to move the measurement area per point, each point could be measured in 3 seconds.

[0052] When cortisol was measured directly, it was found that quantitative measurement was possible at concentrations below 0.037 μg / dL.

[0053] It was revealed that the excitation laser caused amorphous carbonization of the sample at a high rate. It is expected that this carbonization can be suppressed by reducing the excitation light density and dispersing the local heat.

[0054] [Non-patent document 1] T. Akiyama, T. Yamamoto, T. Oku, M. Yahiro, T. Kurihara, C. Adachi and S. Yamada, Jpn. J. Appl. Phys., 52, 122301 (2013). [Non-patent document 2] N. Koyama, T. Akiyama and T. Oku, Jpn. J. Appl. Phys., 60, 027002 (2021). [Non-patent document 3] M. Suzuki, Y. Niidome, N. Terasaki, K. Inoue, Y. Kuwahara and S. Yamada, Jpn. J. Appl. Phys., 43, L554 (2004). [Non-patent document 4] T. Akiyama, M. Nakada, N. Terasaki and S. Yamada, Chem. Commun., 395 (2006). [Non-patent document 5] TJ Moore and B. Sharma, Anal Chem., 92, 2052 (2020). [Non-patent document 6] T. Arakawa, T. Kawahara, T. Akiyama and S. Yamada, Jpn. J. Appl. Phys., 46, 2490 (2007). [Non-patent document 7] T. Akiyama, T. Kawahara, T. Arakawa and S. Yamada, Jpn. J. Appl. Phys., 47, 3063 (2008). [Non-patent document 8] J. Turkevich, PC Stevenson and J. Hillier, Discuss. Faraday Soc., 11, 55 (1951). [Non-patent document 9] T. Akiyama, eJ. Surf. Sci. Nanotech., 10, 157 (2012). [Non-patent document 10] Y. Liu, Z. Lu, X. Lin, H. Zhu, W. Hasi, M. Zhang, X. Zhao and X. Lou, RSC Adv., 6, 58387 (2016). [Non-patent document 11] N. Koyama, S. Banya, T. Akiyama, K. Sugawa and T. Oku, Appl. Phys. Express, 13, 055001 (2020).

[0055] As shown in FIG. 19, the detection device (Raman scattering spectroscopic measurement device) according to the embodiment of the present disclosure includes a laser light source 10, a beam splitter 11, an objective lens 12, a spectrometer 13, a CCD detector 14, a sample stage 15, and an information processing device 16. With a solution containing an analyte introduced into the sample stage 15, an excitation laser light is irradiated from the laser light source 10 and collected by the objective lens 12. The generated Raman scattered light is input to the spectrometer 13 via the objective lens 12 and the beam splitter 11 and dispersed. The CCD detector 14 is disposed so as to be able to measure a wave number range of a predetermined Raman shift. The Raman signal detected by the CCD detector 14 is sent to the information processing device 16, where it is analyzed, displayed, recorded, and the like. The information processing device 16 also controls the laser light source 10, the CCD detector 14, and the sample stage 15.

[0056] The detection system of this embodiment includes an information processing device 16. The information processing device 16 is communicably connected to a laser light source 10, a beam splitter 11, an objective lens 12, a spectrometer 13, a CCD detector 14, and a sample stage 15 via a wire or a communication network. The communication network is, for example, the Internet, and is constructed by a public telephone line network, a mobile phone line network, a wireless communication path, Ethernet (registered trademark), or the like.

[0057] The information processing device 16 may be, for example, a general-purpose computer such as a workstation or a personal computer, or may be logically realized by cloud computing. In this embodiment, one device is illustrated for convenience of explanation, but the present invention is not limited to this and may be multiple devices.

[0058] FIG. 20 is a diagram showing an example of the hardware configuration of the information processing device 16. Note that the illustrated configuration is an example, and other configurations may be used. The information processing device 16 includes a CPU 101, a memory 102, a storage device 103, a communication interface 104, an input device 105, and an output device 106. The storage device 103 is, for example, a hard disk drive, a solid state drive, or a flash memory that stores various data and programs. The communication interface 104 is an interface for connecting to a communication network NW, and is, for example, an adapter for connecting to Ethernet (registered trademark), a modem for connecting to a public telephone line network, a wireless communication device for wireless communication, a USB (UNIVERSAL SERIAL BUS) connector or an RS232C connector for serial communication, etc. The input device 305 is, for example, a keyboard, a mouse, a touch panel, a button, a microphone, etc. that input data. The output device 306 is, for example, a display, a printer, a speaker, etc. that output data. Each functional unit of the information processing device 16 described later is realized by the CPU 101 reading a program stored in the storage device 103 into the memory 102 and executing it, and each storage unit of the information processing device 16 is realized as part of the storage area provided by the memory 102 and the storage device 103.

[0059] Fig. 21 shows the functional configuration of the information processing device 16. As shown in Fig. 21, the information processing device 16 includes each of the storage units, that is, an image storage unit 131, a Raman signal storage unit 132, and a model storage unit 133, and each of the processing units, that is, a laser control unit 111, an image acquisition unit 112, a Raman signal acquisition unit 113, a model generation unit 114, and a detection position presentation unit 115.

[0060] The image storage unit 131 stores information about the image acquired by the image acquisition unit 112 using the CCD detector 14 .

[0061] The Raman signal storage unit 132 stores the Raman signal acquired by the Raman signal acquisition unit 113 .

[0062] The model storage unit 133 stores the prediction model generated by the model generation unit 114.

[0063] The above is a description of each storage unit included in the detection support system. Below, a description will be given of each processing unit included in the detection support system.

[0064] The laser control unit 111 controls the laser light source 10 to irradiate the detection target with excitation laser light. The laser control unit 111 may irradiate the laser light to an arbitrary position on the sample stage 15, may irradiate a position designated by a user, or may irradiate a position presented by a detection position presenting unit 115 described later, but is not limited to these.

[0065] The image acquisition unit 112 acquires an image of the sample by the CCD detector 14. The acquired image may include a video.

[0066] The Raman signal acquisition unit 113 acquires a Raman signal by the CCD detector 14 .

[0067] The model generation unit 114 generates a model that predicts a position suitable for detecting the detection target object (i.e., a position where multiple nanoscales exist) in the image acquired by the image acquisition unit 112. For example, the model generation unit 114 may use an image in which a black dot portion considered to be a multiple nanoscale, such as point R in Fig. 12, is cut out as training data, and generate a prediction model that predicts a position where multiple nanoscales exist in another image by machine learning. The input data for the prediction model is image information, and the output data is information on black dots considered to be multiple nanoscales among the black dots in the image.

[0068] The detection position presenting unit 115 presents the position to be detected based on the image information to the user via the output device 106 or the like, using the prediction model generated by the model generating unit 114. The detection position presenting unit 115 accepts a selection from a plurality of detection positions in the presented image from the user, and irradiates the position selected by the laser control unit 111 with the excitation laser light.

[0069] The result presentation unit 116 presents the signal acquired by the Raman signal acquisition unit 113 to a user via the output device 106 or the like. The result presentation unit 116 may convert the signal acquired by the Raman signal acquisition unit 113 into the form of a graph or a table and present it to the user.

[0070] A typical process flow of the information processing device 16 of this embodiment will be described with reference to FIG. 22. The laser control unit 111 irradiates the sample with an excitation laser (1001). The image acquisition unit 112 acquires an image (1002). The Raman signal acquisition unit 113 acquires a Raman signal (1003). The model generation unit 114 generates a prediction model for predicting a detection position in the image (1004). The detection position presentation unit 115 presents the detection position to the user using the prediction model (1005). The detection position presentation unit 115 accepts a selection of a detection position from the user, and irradiates the selected position in the image with an excitation laser light by the laser control unit 111 (1006). The result presentation unit 116 presents the signal acquired by the Raman signal acquisition unit to the user (1007).

[0071] Although the preferred embodiment of the present disclosure has been described in detail above with reference to the attached drawings, the technical scope of the present disclosure is not limited to such examples. It is clear that a person having ordinary knowledge in the technical field of the present disclosure can conceive of various modified or amended examples within the scope of the technical ideas described in the claims, and it is understood that these also naturally belong to the technical scope of the present disclosure.

[0072] The device described in this specification may be realized as a single device, or may be realized by a plurality of devices (e.g., cloud servers) partially or entirely connected via a network. For example, the CPU and storage device of the information processing device 16 may be realized by different servers connected to each other via a network.

[0073] The series of processes performed by the device described in this specification may be realized using any of software, hardware, and a combination of software and hardware. A computer program for realizing each function of the information processing device 16 according to this embodiment may be created and installed in a PC or the like. A computer-readable recording medium in which such a computer program is stored may also be provided. The recording medium may be, for example, a magnetic disk, an optical disk, a magneto-optical disk, a flash memory, or the like. The above computer program may also be distributed, for example, via a network, without using a recording medium.

[0074] Additionally, the processes described herein do not necessarily have to be performed in the order described, some process steps may be performed in parallel, additional process steps may be employed, and some process steps may be omitted.

[0075] In addition, the effects described in this specification are merely descriptive or exemplary and are not limiting. In other words, the technology according to the present disclosure may achieve other effects that are apparent to a person skilled in the art from the description of this specification, in addition to or in place of the above effects. [Explanation of symbols]

[0076] 10 Laser light source 11 Beam splitter 12 Objective Lens 13 Spectrometer 14 CCD detector 15 Sample stage 16 Information processing equipment

Claims

1. A method for detecting a substance, comprising: an irradiation step of irradiating with laser light; a measuring step of measuring Raman scattered light generated by irradiation with the laser light; Equipped with A detection method in which, in the measuring step, a sample containing the substance is placed on a substrate having a multi-scale nanostructure, and the laser light is irradiated to perform measurement.

2. The nanostructure is formed by a compound containing a metal. The detection method according to claim 1 .

3. The nanostructures include nanostructures on the scale of at least 10-100 nm. The detection method according to claim 1 or 2.

4. The detection method according to claim 3 , wherein the nanostructure is formed by electrolytic reduction of metal ions or by heating a metal colloid solution under reflux.

5. When the nanostructure is formed by electrolytic reduction of metal ions, the electrolytic reduction is 5 mA / cm 2 to 15mA / cm 2 This is done by applying a current of The detection method according to claim 4.

Citation Information

Patent Citations

  • Method for producing substrate for generating surface enhanced raman scattering spectra, surface enhanced raman scattering spectra measurement method, and substrate for generating surface enhanced raman scattering spectra

    JP2020204495A