Liquid jet head
The liquid ejecting head addresses stress concentration at reinforcing film ends by employing a strategically designed reinforcing film with varying thickness and slope conditions, enhancing stability and reducing crack risks.
Patent Information
- Application Number
- JP2023054581
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-30
- Publication Date
- 2024-10-11
AI Technical Summary
Existing liquid ejecting heads face stress concentration at the ends of reinforcing films, leading to potential cracks despite the presence of reinforcing films, as they vibrate around the boundary between film-provided and non-provided areas.
A liquid ejecting head design with a reinforcing film that overlaps the boundary between the partition wall and pressure chamber, having varying thicknesses along the stacking direction to disperse stress, satisfying specific thickness and slope conditions to reduce stress concentration.
The design effectively reduces the likelihood of stress concentration and cracks by uniformly distributing stress, ensuring stable diaphragm vibration and prolonged head performance.
Smart Images

Figure 2024142442000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a liquid jet head. [Background technology]
[0002] As described in Patent Document 1, it is known that in a liquid ejection head, a reinforcing film is provided on the vibration plate to suppress the occurrence of cracks in the vibration plate. The vibration plate has a boundary between a portion located on a partition wall separating adjacent pressure chambers and a portion located on the pressure chamber. The vibration plate vibrates with the boundary portion as a fulcrum by being connected to the partition wall. That is, the occurrence of the cracks is caused by stress concentration occurring at the boundary portion of the vibration plate. Therefore, the reinforcing film is formed along the boundary portion. The reinforcing film is formed on the surface of the vibration plate opposite to the surface on which the pressure chamber exists. The reinforcing film is formed so as to cover the boundary portion from this opposite surface. Therefore, the reinforcing film prevents stress concentration at the boundary portion of the vibration plate by suppressing deformation of the vibration plate with the boundary portion as a fulcrum. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2019-5924 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, even when the reinforcing film is provided, the diaphragm vibrates with a fulcrum other than the boundary. Specifically, the diaphragm vibrates with the boundary between the part with the reinforcing film and the part without the reinforcing film, that is, the end of the reinforcing film, as the fulcrum. Therefore, there is a risk that stress concentration will occur at the end of the reinforcing film. Therefore, there is still a risk of cracks occurring. [Means for solving the problem]
[0005] The present disclosure can be realized in the following forms or application examples.
[0006] According to a first aspect of the present disclosure, there is provided a liquid jet head. This liquid jet head is a liquid jet head in which a piezoelectric element that deforms when a voltage is applied thereto and includes a first electrode, a piezoelectric layer, and a second electrode, a vibration plate that vibrates when the piezoelectric element is driven, a reinforcing film, and a pressure chamber substrate that constitutes a partition wall that defines a pressure chamber communicating with a nozzle together with the vibration plate, are laminated in a stacking direction. The vibration plate is vibrated in the stacking direction by the piezoelectric element, thereby applying pressure to the liquid in the pressure chamber. The reinforcing membrane is formed along a first direction that is a direction perpendicular to the stacking direction, and overlaps the boundary between the partition wall and the pressure chamber when viewed in the stacking direction. In a cross section parallel to the stacking direction and a direction from the boundary toward the center of the pressure chamber, a first thickness of the reinforcing membrane in the stacking direction at a first position as the position of the boundary is defined as Y1, a second thickness of the reinforcing membrane in the stacking direction at a second position closer to the center of the pressure chamber than the first position is defined as Y2, and the absolute value of the slope of a tangent to an inclined surface of the reinforcing membrane that is not in contact with the vibration plate is defined as a1, and a second thickness of the reinforcing membrane in the stacking direction at a second position is defined as a2. Y1>Y2 …(1) and 0 <a1<a2 …(2) The above formulas (1) and (2) are satisfied. [Brief description of the drawings]
[0007] [Figure 1] FIG. 2 is a block diagram showing a schematic configuration of a liquid ejection device 500. [Diagram 2] FIG. 2 is an exploded perspective view showing the configuration of a liquid jet head 510. [Diagram 3] 2 is an explanatory diagram showing the configuration of a liquid jet head 510 in a plan view. FIG. [Figure 4] FIG. 4 is a cross-sectional view taken along the line IV-IV in FIG. [Diagram 5]2 is an enlarged cross-sectional view showing the vicinity of a piezoelectric element 300. FIG. [Figure 6] 6 is a cross-sectional view taken along line VI-VI of FIG. [Figure 7] 4 is an enlarged plan view showing the vicinity of a groove 71 in FIG. 3. FIG. [Figure 8] 7 is an enlarged cross-sectional view showing the vicinity of a reinforcing film 51 in FIG. 6. FIG. [Figure 9] 3 is a cross-sectional view showing the cross-sectional shape of a reinforcing film 51. FIG. [Figure 10] 1 is an explanatory diagram showing a curve that defines a thickness Y of an end portion 51s of a reinforcing membrane 51. FIG. [Figure 11] 4 is an explanatory diagram showing a cross section of a diaphragm 50 before displacement. FIG. [Figure 12] 13 is an explanatory diagram showing a cross section of the reinforcing film Ob and the diaphragm 50 before displacement. FIG. [Figure 13] 5 is an explanatory diagram showing a cross section of a reinforcing film 51 and a diaphragm 50 before displacement. FIG. [Figure 14] 11 is an explanatory diagram showing a cross section of the diaphragm 50 after displacement. FIG. [Figure 15] 13 is an explanatory diagram showing a cross section of the reinforcing film Ob and the diaphragm 50 after displacement. FIG. [Figure 16] 11 is an explanatory diagram showing a cross section of the reinforcing film 51 and the diaphragm 50 after displacement. FIG. [Figure 17] 11 is a perspective view of the diaphragm 50 after displacement. FIG. [Figure 18] 13 is a perspective view of the reinforcing film Ob and the diaphragm 50 after displacement. FIG. [Figure 19] 13 is a perspective view of the reinforcing film 51 and the diaphragm 50 after displacement. FIG. [Figure 20] 11 is a cross-sectional view showing the cross-sectional shape of a reinforcing film 51b. FIG. [Figure 21] 13 is a cross-sectional view showing a cross section of a pressure chamber 12c according to a third embodiment. FIG. [Figure 22] 13 is an explanatory diagram showing the diaphragm 50 after displacement in the third embodiment. FIG. [Diagram 23] FIG. 13 is an explanatory diagram showing a reinforcing membrane 51d of a fourth embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] A. First embodiment: A1. Overall configuration of the liquid ejection device: FIG. 1 is a block diagram showing a schematic configuration of a liquid ejection device 500 including a liquid jet head 510 according to a first embodiment of the present disclosure. In this embodiment, the liquid ejection device 500 is configured as an inkjet printer, and forms an image by ejecting ink onto printing paper P. FIG. 1 shows three mutually orthogonal axes, namely, an X-axis, a Y-axis, and a Z-axis. The X-axis, the Y-axis, and the Z-axis shown in other drawings all correspond to the X-axis, the Y-axis, and the Z-axis in FIG. 1. When specifying a direction, a positive direction is indicated by "+" and a negative direction is indicated by "-", and positive and negative signs are used in combination to indicate the direction.
[0009] The liquid ejection device 500 includes a liquid ejection head 510 , an ink tank 550 , a transport mechanism 560 , a moving mechanism 570 , and a control unit 540 .
[0010] The liquid ejection head 510 has a large number of nozzles 21, and ejects ink in the -Y direction to form an image on the printing paper P. The configuration of the liquid ejection head 510 will be described in detail later. Examples of the ejected ink include a total of four colors of ink: black, cyan, magenta, and yellow. The liquid ejection head 510 is mounted on a carriage 572 (to be described later) of the moving mechanism 570, and moves back and forth in the main scanning direction together with the movement of the carriage 572. In this embodiment, the main scanning direction is the +Z direction and the -Z direction. The +Z direction and the -Z direction are also referred to as the "Z-axis direction."
[0011] The ink tank 550 contains ink to be ejected from the liquid ejection head 510. The ink tank 550 is not mounted on the carriage 572. The ink tank 550 and the liquid ejection head 510 are connected by a resin tube 552, and ink is supplied from the ink tank 550 to the liquid ejection head 510 via the tube 552.
[0012] The transport mechanism 560 transports the print paper P in the sub-scanning direction. The sub-scanning direction is a direction perpendicular to the Z-axis direction, which is the main scanning direction, and in this embodiment, is the +X and -X directions. The +X and -X directions are also referred to as the "X-axis directions." The transport mechanism 560 includes a transport rod 564 to which three transport rollers 562 are attached, and a transport motor 566 that drives and rotates the transport rod 564. The transport motor 566 drives and rotates the transport rod 564, causing the multiple transport rollers 562 to rotate, and the print paper P is transported in the +X direction, which is the sub-scanning direction.
[0013] The movement mechanism 570 includes a conveyor belt 574, a movement motor 576, and a pulley 577 in addition to the above-mentioned carriage 572. The carriage 572 mounts the liquid ejection head 510 in a state in which it is capable of ejecting ink. The carriage 572 is attached to the conveyor belt 574. The conveyor belt 574 is stretched between the movement motor 576 and the pulley 577. The movement motor 576 rotates the conveyor belt 574, which moves back and forth in the main scanning direction. As a result, the carriage 572 attached to the conveyor belt 574 also moves back and forth in the main scanning direction.
[0014] The control unit 540 controls the entire liquid ejection device 500. For example, the control unit 540 controls the reciprocating movement of the carriage 572 in the main scanning direction and the transport movement of the print paper P in the sub-scanning direction. In this embodiment, the control unit 540 also functions as a drive control section for a piezoelectric actuator, which will be described later. That is, the control unit 540 controls the ejection of ink onto the print paper P by outputting a drive signal to the liquid ejection head 510 to drive the piezoelectric actuator. The control unit 540 is composed of a processing circuit, such as a CPU (Central Processing Unit) or an FPGA (Field Programmable Gate Array), and a storage circuit, such as a semiconductor memory, for example.
[0015] A2. Detailed configuration of the liquid jet head: Fig. 2 is an exploded perspective view showing the configuration of the liquid jet head 510. Fig. 3 is an explanatory diagram showing the configuration of the liquid jet head 510 in a plan view. Fig. 3 shows the configuration around the pressure chamber substrate 10 in the liquid jet head 510. In Fig. 3, the protective substrate 30 and the case member 40 are omitted to facilitate understanding of the technology. Fig. 4 is a cross-sectional view showing the position IV-IV in Fig. 3.
[0016] As shown in FIG. 2, the liquid jet head 510 has a pressure chamber substrate 10, a communication plate 15, a nozzle plate 20, a compliance substrate 45, a protective substrate 30, a case member 40, and a wiring substrate 120, and further has a piezoelectric element 300 shown in FIG. 3 and a vibration plate 50 shown in FIG. 4. The pressure chamber substrate 10, the communication plate 15, the nozzle plate 20, the compliance substrate 45, the vibration plate 50, the piezoelectric element 300, the protective substrate 30, and the case member 40 are laminated members, and form the liquid jet head 510 by being laminated. In the present disclosure, the direction in which the laminated members forming the liquid jet head 510 are laminated is also referred to as the lamination direction Am10. The +Y direction and the -Y direction are also referred to as the "Y-axis direction". The lamination direction Am10 is also a direction along the +Y-axis direction.
[0017] The pressure chamber substrate 10 is formed using, for example, a silicon substrate. As shown in FIG. 3, the pressure chamber substrate 10 has a plurality of pressure chambers 12 arranged along a predetermined direction in the pressure chamber substrate 10. The direction in which the plurality of pressure chambers 12 are arranged is also referred to as the arrangement direction Am21. The +X direction and the -X direction are also referred to as the "X-axis direction". The arrangement direction Am21 is also a direction along the X-axis direction. The pressure chambers 12 are formed in a rectangular shape whose length in the Z-axis direction is longer than its length in the X-axis direction in a plan view.
[0018] In this embodiment, the pressure chambers 12 are arranged in two rows, each with the arrangement direction Am21 in the X-axis direction. In the example of FIG. 3, two pressure chamber rows are formed in the pressure chamber substrate 10: a first pressure chamber row La with the arrangement direction Am21 in the X-axis direction, and a second pressure chamber row Lb with the arrangement direction Am21 in the X-axis direction. The second pressure chamber row Lb is disposed adjacent to the first pressure chamber row La in a direction intersecting the arrangement direction Am21 of the first pressure chamber row La. The direction intersecting the arrangement direction Am21 is also referred to as an intersecting direction Am30. In the example of FIG. 3, the intersecting direction Am30 is the Z-axis direction, and the second pressure chamber row Lb is adjacent to the first pressure chamber row La in the -Z direction.
[0019] The pressure chambers 12 belonging to the first pressure chamber row La and the pressure chambers 12 belonging to the second pressure chamber row Lb are arranged so that their positions in the arrangement direction Am21 coincide with each other and are adjacent to each other in the intersecting direction Am30. In each pressure chamber row, the pressure chambers 12 adjacent to each other in the X-axis direction are partitioned by partition walls 11 shown in FIG. 6, as will be described later.
[0020] 2, a communication plate 15, a nozzle plate 20, and a compliance substrate 45 are laminated in this order on the -Y direction side of the pressure chamber substrate 10. The communication plate 15 is, for example, a flat member using a silicon substrate. As shown in FIG. 4, the communication plate 15 is provided with a nozzle communication passage 16, a first manifold portion 17, a second manifold portion 18, and a supply communication passage 19.
[0021] As shown in Fig. 4, the nozzle communication passage 16 is a flow path that communicates between the pressure chambers 12 and the nozzles 21. The first manifold portion 17 and the second manifold portion 18 function as part of a manifold 100 that serves as a common liquid chamber to which the multiple pressure chambers 12 communicate. The first manifold portion 17 is provided so as to penetrate the communication plate 15 in the Y-axis direction. In addition, as shown in Fig. 4, the second manifold portion 18 is provided on the surface of the communication plate 15 on the -Y direction side, without penetrating the communication plate 15 in the Y-axis direction.
[0022] The supply communication passages 19 are flow paths that communicate with one end of the pressure chambers 12 in the Z-axis direction. There are multiple supply communication passages 19, which are arranged along the X-axis direction, i.e., the arrangement direction Am21, and are individually provided for each pressure chamber 12. The supply communication passages 19 communicate between the second manifold portion 18 and each pressure chamber 12, and supply ink within the manifold 100 to each pressure chamber 12.
[0023] The nozzle plate 20 is provided on the opposite side of the communication plate 15 to the pressure chamber substrate 10, that is, on the +Y direction side of the communication plate 15. The nozzle plate 20 is made of, for example, a silicon substrate.
[0024] A plurality of nozzles 21 are formed in the nozzle plate 20. Each nozzle 21 is connected to each pressure chamber 12 via a nozzle communication passage 16. As shown in Fig. 2, the plurality of nozzles 21 are arranged along the arrangement direction Am21 of the pressure chambers 12, i.e., the X-axis direction. The nozzle plate 20 is provided with two nozzle rows in which the plurality of nozzles 21 are arranged. The two nozzle rows correspond to the first pressure chamber row La and the second pressure chamber row Lb, respectively.
[0025] As shown in FIG. 4, the compliance substrate 45 is provided together with the nozzle plate 20 on the opposite side of the communication plate 15 from the pressure chamber substrate 10, that is, on the surface of the communication plate 15 in the +Y direction. The compliance substrate 45 is provided around the nozzle plate 20 and covers the openings of the first manifold portion 17 and the second manifold portion 18 provided in the communication plate 15. In this embodiment, the compliance substrate 45 includes a sealing film 46 made of a flexible thin film and a fixed substrate 47 made of a hard material such as metal. As shown in FIG. 4, the region of the fixed substrate 47 facing the manifold 100 is an opening 48 that is completely removed in the thickness direction. Therefore, one surface of the manifold 100 is a compliance portion 49 sealed only by the sealing film 46.
[0026] As shown in Fig. 4, a vibration plate 50 and a piezoelectric element 300 are laminated on the side of the pressure chamber substrate 10 opposite the nozzle plate 20, i.e., on the surface of the pressure chamber substrate 10 on the -Y direction side. The piezoelectric element 300 flexes and deforms the vibration plate 50, causing a pressure change in the ink in the pressure chamber 12. In Fig. 4, the configuration of the piezoelectric element 300 is shown in a simplified manner to facilitate understanding of the technology. The piezoelectric element 300 will be described in detail later. The vibration plate 50 is provided on the -Y direction side of the piezoelectric element 300, and the pressure chamber substrate 10 is provided on the +Y direction side of the vibration plate 50.
[0027] 4, a protective substrate 30 having approximately the same size as the pressure chamber substrate 10 is further bonded to the surface of the pressure chamber substrate 10 on the +Y direction side by an adhesive or the like. The protective substrate 30 has holding portions 31 which are spaces for protecting the piezoelectric elements 300. The holding portions 31 are provided for each row of the piezoelectric elements 300 arranged along the arrangement direction Am21, and in this embodiment, are formed in two rows in the Z axis direction. In addition, the protective substrate 30 has through holes 32 between the two rows of holding portions 31, which extend along the X axis direction and penetrate along the Y axis direction.
[0028] 4, a case member 40 is fixed onto the protective substrate 30. The case member 40 forms a manifold 100, which communicates with the multiple pressure chambers 12, together with the communication plate 15. The case member 40 has approximately the same outer shape as the communication plate 15 in a plan view, and is joined across the protective substrate 30 and the communication plate 15.
[0029] The case member 40 has a storage section 41, a supply port 44, a third manifold section 42, and a connection port 43. The storage section 41 is a space having a depth capable of storing the pressure chamber substrate 10 and the protective substrate 30. The third manifold section 42 is a space formed on both outer sides of the storage section 41 in the Z-axis direction in the case member 40. The third manifold section 42 is connected to the first manifold section 17 and the second manifold section 18 provided on the communication plate 15, thereby forming a manifold 100. The manifold 100 has an elongated shape that is continuous along the X-axis direction. The supply port 44 communicates with the manifold 100 and supplies ink to each manifold 100. The connection port 43 is a through hole that communicates with the through hole 32 of the protective substrate 30, and the wiring substrate 120 is inserted through the through hole.
[0030] In the liquid jet head 510 of this embodiment, ink supplied from an ink tank 550 shown in Fig. 1 is taken in through a supply port 44 shown in Fig. 4. After the internal flow paths from the manifold 100 to the nozzles 21 are filled with ink, a voltage based on a drive signal is applied to each of the piezoelectric elements 300 corresponding to the multiple pressure chambers 12. As a result, the vibration plate 50 is deflected and deformed together with the piezoelectric elements 300 described below, increasing the pressure in each pressure chamber 12, and ink droplets are ejected from each nozzle 21.
[0031] The configuration of the -Y direction side of the pressure chamber substrate 10 will be described with reference to Fig. 3 to Fig. 6. Fig. 5 is an enlarged cross-sectional view showing the vicinity of the piezoelectric element 300. Fig. 6 is a cross-sectional view taken along line VI-VI in Fig. 3. The liquid jet head 510 has, on the -Y direction side of the pressure chamber substrate 10, a vibration plate 50, a piezoelectric element 300, and further a reinforcing film 51, an individual lead electrode 91, and a common lead electrode 92.
[0032] As shown in FIG. 5, the vibration plate 50 applies pressure to the liquid in the pressure chamber 12 by being vibrated in the stacking direction Am10 by driving the piezoelectric element 300.
[0033] As shown in FIG. 6, the area of the vibration plate 50 where the first electrode 60, the piezoelectric layer 70, the second electrode 80, and the pressure chamber 12 overlap in the stacking direction Am10 is called the active portion 50r1. The area of the vibration plate 50 where the active portion 50r1 is a different part and where the pressure chamber 12 overlaps in the stacking direction Am10 is called the inactive portion 50r2. Furthermore, in the vibration plate 50 described later, the surface on which the piezoelectric element 300 is provided in the stacking direction Am10 is called the first surface 50a1, and the surface on which the pressure chamber substrate 10 is provided is called the second surface 50a2 (see the upper left part of FIG. 6). The direction from the boundary B1 toward the center 12o of the pressure chamber 12 is called the second direction Am40. The second direction Am40 is also parallel to the X-axis direction.
[0034] As shown in Fig. 5, the vibration plate 50 is composed of an elastic film 55 made of silicon oxide provided on the pressure chamber substrate 10 side, and an insulating film 56 made of zirconium oxide. The surface on the -Y direction side of the flow path of the pressure chamber 12, etc. is composed of the elastic film 55. The pressure chamber 12 is formed by anisotropically etching the pressure chamber substrate 10 from the -Y direction side toward the +Y direction. The elastic film 55 functions as a stop layer for the anisotropic etching. To facilitate understanding of the technology, the elastic film 55 and the insulating film 56 are omitted from the drawings other than Fig. 5.
[0035] The piezoelectric element 300 applies pressure to the pressure chamber 12 via the vibration plate 50. As shown in Fig. 5 and Fig. 6, the piezoelectric element 300 has a first electrode 60, a piezoelectric layer 70, and a second electrode 80. The first electrode 60, the piezoelectric layer 70, and the second electrode 80 are laminated in order from the +Y direction side to the -Y direction side, as shown in Fig. 5 and Fig. 6. The piezoelectric layer 70 is provided between the first electrode 60 and the second electrode 80 in the lamination direction Am10 in which the first electrode 60, the second electrode 80, and the piezoelectric layer 70 are laminated, i.e., in the Y-axis direction.
[0036] 6, the reinforcing film 51 is formed along a direction perpendicular to the stacking direction Am10 of the vibration plate 50, and is formed so as to overlap the boundary B1 between the partition wall 11 and the pressure chamber 12 when viewed in the stacking direction Am10. The first direction Am20 is a direction including the Z-axis direction and the X-axis direction. The reinforcing film 51 will be described in detail later.
[0037] The first electrode 60 and the second electrode 80 are both electrically connected to the wiring board 120 shown in FIG. 4. The first electrode 60 and the second electrode 80 apply a voltage corresponding to a drive signal to the piezoelectric layer 70. A drive voltage that varies depending on the amount of ink ejected is supplied to the first electrode 60, and a constant reference voltage signal is supplied to the second electrode 80 regardless of the amount of ink ejected. The amount of ink ejected is the amount of volume change required for the pressure chamber 12. When a potential difference occurs between the first electrode 60 and the second electrode 80 by driving the piezoelectric element 300, the piezoelectric layer 70 is deformed. The deformation of the piezoelectric layer 70 causes the vibration plate 50 to deform or vibrate, changing the volume of the pressure chamber 12. The change in volume of the pressure chamber 12 applies pressure to the ink contained in the pressure chamber 12, and ink is ejected from the nozzle 21 through the nozzle communication passage 16.
[0038] As shown in FIG. 3, the first electrodes 60 are individual electrodes provided for the multiple pressure chambers 12. The first electrodes 60 are made of, for example, platinum (Pt). As shown in FIG. 6, the width of the first electrodes 60 in the X-axis direction is narrower than the width of the pressure chambers 12. That is, both ends of the first electrodes 60 in the X-axis direction are located inside the pressure chambers 12 relative to both ends of the pressure chambers 12 in the X-axis direction. As shown in FIG. 5, the end 60a in the +Z direction and the end 60b in the Z direction of the first electrodes 60 are each disposed outside the pressure chambers 12. For example, in the first pressure chamber row La, the end 60a of the first electrodes 60 is disposed at a position on the +Z direction side of the end 12a of the pressure chambers 12 in the +Z direction. The end 60b of the first electrodes 60 is disposed at a position on the -Z direction side of the end 12b of the pressure chambers 12 in the -Z direction.
[0039] As shown in FIG. 5, the width of the piezoelectric layer 70 in the Z-axis direction is longer than the width of the pressure chamber 12 in the Z-axis direction, which is the longitudinal direction of the pressure chamber 12. As shown in FIG. 6, the piezoelectric layer 70 is provided extending along the arrangement direction Am21 of the pressure chambers 12, i.e., the X-axis direction. Therefore, on both sides of the pressure chamber 12 in the Z-axis direction, the piezoelectric layer 70 extends to the outside of the pressure chamber 12. The piezoelectric layer 70 may be a crystal film with a perovskite structure, so-called perovskite crystal, formed on the first electrode 60 and made of a ferroelectric ceramic material exhibiting an electromechanical conversion effect. In this embodiment, lead zirconate titanate (PZT) is used as the piezoelectric layer 70.
[0040] 5, the end 70a in the +Z direction of the piezoelectric layer 70 is located on the +Z direction side, that is, outside the end 60a of the first electrode 60, in the first pressure chamber row La. That is, the end 60a of the first electrode 60 is covered by the piezoelectric layer 70. On the other hand, the end 70b in the -Z direction of the piezoelectric layer 70 is located on the +Z direction side, that is, inside the end 60b of the first electrode 60, and the end 60b of the first electrode 60 is not covered by the piezoelectric layer 70.
[0041] 6, grooves 71 are formed in the piezoelectric layer 70 between corners 80c of adjacent second electrodes 80 as regions where the piezoelectric layer 70 does not exist. The grooves 71 are provided at positions corresponding to the partition walls 11. The grooves 71 are formed by completely removing the piezoelectric layer 70 in the Y-axis direction.
[0042] FIG. 7 is an enlarged plan view showing the vicinity of the groove portion 71 in FIG. 3. In FIG. 7, the groove portion 71 belonging to the second pressure chamber row Lb in FIG. 3 is shown. The groove portion 71 has a substantially rectangular external shape in a plan view. The width of the groove portion 71 in the X-axis direction is formed wider than the width of the partition wall 11 in the X-axis direction. The width of the groove portion 71 in the Z-axis direction is formed narrower than the width of the pressure chamber 12 in the Z-axis direction. By providing the groove portion 71 in the piezoelectric layer 70, the rigidity of the portion of the vibration plate 50 facing the end of the pressure chamber 12 in the X-axis direction, that is, the arm portion of the vibration plate 50, is suppressed. The arm portion of the vibration plate 50 corresponds to the inactive portion 50r2. Therefore, the groove portion 71 can displace the piezoelectric element 300 more satisfactorily.
[0043] 5 and 6, the second electrode 80 is provided on the opposite side of the piezoelectric layer 70 from the first electrode 60, i.e., on the +Y direction side of the piezoelectric layer 70. As shown in Fig. 3, the second electrode 80 is a common electrode provided in common to the multiple pressure chambers 12 and common to the multiple active sections 50r1. In this embodiment, iridium (Ir) is used as the material for the second electrode 80.
[0044] 3, the second electrode 80 has a predetermined width in the Z-axis direction and is provided extending along the arrangement direction Am21 of the pressure chambers 12, i.e., the X-axis direction. As shown in FIG. 6, the second electrode 80 is also provided on the side surface of the groove portion 71 of the piezoelectric layer 70 and on the vibration plate 50 which is the bottom surface of the groove portion 71.
[0045] 5, the end 80a of the second electrode 80 in the +Z direction is disposed outside, i.e., on the +Z direction side, of the end 60a of the first electrode 60 covered with the piezoelectric layer 70. The end 80a of the second electrode 80 is located outside the end 12a of the pressure chamber 12 and outside the end 60a of the first electrode 60. In this embodiment, the end 80a of the second electrode 80 approximately coincides with the end 70a of the piezoelectric layer 70 in the Z axis direction.
[0046] As shown in FIG. 5, the end 80b in the -Z direction of the second electrode 80 is disposed on the -Z direction side, which is outer than the end 12b in the -Z direction of the pressure chamber 12, and disposed on the +Z direction side, which is inner than the end 70b of the piezoelectric layer 70. The end 70b of the piezoelectric layer 70 is located on the inside, which is on the +Z direction side, of the end 60b of the first electrode 60. Therefore, the end 80b of the second electrode 80 is located on the piezoelectric layer 70 on the +Z direction side of the end 60b of the first electrode 60. On the -Z direction side of the end 80b of the second electrode 80, there is a portion where the surface of the piezoelectric layer 70 is exposed. In this way, the end 80b of the second electrode 80 is disposed on the +Z direction side of the end 70b of the piezoelectric layer 70 and the end 60b of the first electrode 60.
[0047] A wiring portion 85 is provided on the side of the end portion 80b of the second electrode 80, which is in the same layer as the second electrode 80 but is electrically discontinuous with the second electrode 80 (see the upper left part of FIG. 5). The wiring portion 85 is formed from near the end portion 70b of the piezoelectric layer 70 to the end portion 60b of the first electrode 60, with a gap between the wiring portion 85 and the end portion 80b of the second electrode 80. A wiring portion 85 is provided for each active portion 50r1. That is, a plurality of wiring portions 85 are arranged at predetermined intervals along the X-axis direction.
[0048] 3 and 5, an individual lead electrode 91 is connected to the first electrode 60, which is an individual electrode, and a common lead electrode 92, which is a driving common electrode, is electrically connected to the second electrode 80, which is a common electrode. The individual lead electrode 91 and the common lead electrode 92 function as drive wiring for applying a voltage to the piezoelectric layer 70 to drive the piezoelectric layer 70.
[0049] 3 and 4, the individual lead electrodes 91 and the common lead electrode 92 are extended so as to be exposed in through holes 32 formed in the protective substrate 30, and are electrically connected to the wiring substrate 120 in the through holes 32. The wiring substrate 120 has a plurality of wirings formed thereon for connection to the control unit 540 and a power supply circuit (not shown). In this embodiment, the wiring substrate 120 is formed of, for example, a flexible substrate (FPC: Flexible Printed Circuit).
[0050] An integrated circuit 121 having a switching element is mounted on the wiring board 120. A signal for driving the piezoelectric element 300, which is propagated on the wiring board 120, is input to the integrated circuit 121. Based on the input signal, the integrated circuit 121 controls the timing at which the signal for driving the piezoelectric element 300 is supplied to the first electrode 60. This controls the timing at which the piezoelectric element 300 is driven and the amount of drive of the piezoelectric element 300.
[0051] Gold (Au) is used as the material for the individual lead electrodes 91 and the common lead electrode 92. The individual lead electrodes 91 are provided for each active section 50r1, that is, for each first electrode 60. As shown in Fig. 5, for example, in the first pressure chamber row La, the individual lead electrode 91 is connected to the vicinity of the end portion 60b of the first electrode 60 via a wiring portion 85, and is drawn out onto the diaphragm 50 in the -Z direction.
[0052] As shown in FIG. 3, for example, in the first pressure chamber row La, the common lead electrode 92 is bent at both ends in the X-axis direction and is drawn out in the -Z direction from above the second electrode 80 to above the diaphragm 50. The common lead electrode 92 has an extension portion 92a and an extension portion 92b. As shown in FIG. 5, for example, in the first pressure chamber row La, the extension portion 92a is provided to extend along the X-axis direction in a region corresponding to the end portion 12a of the pressure chamber 12, and the extension portion 92b is provided to extend along the X-axis direction in a region corresponding to the end portion 12b of the pressure chamber 12. The extension portion 92a and the extension portion 92b are provided continuously in the X-axis direction with respect to the multiple active portions 50r1. The extension portion 92a and the extension portion 92b are provided to extend from the inside of the pressure chamber 12 to the outside of the pressure chamber 12 in the Z-axis direction.
[0053] Therefore, as shown in Figure 4, the liquid ejection head 510 is formed by stacking, in a stacking direction Am10, a piezoelectric element 300 including a first electrode 60, a piezoelectric layer 70, and a second electrode 80, a vibration plate 50 that vibrates when driven by the piezoelectric element 300, a reinforcing film 51, and a pressure chamber substrate 10 that forms a partition 11 that, together with the vibration plate 50, defines a pressure chamber 12 communicating with the nozzle 21.
[0054] A2: Detailed explanation of the reinforcing membrane 51 The reinforcing film 51 reduces stress concentration by dispersing stress generated in the vibration plate 50. As shown in FIG. 6, the reinforcing film 51 is formed along a direction perpendicular to the stacking direction Am10, and is formed so as to overlap the boundary B1 between the partition wall 11 and the pressure chamber 12 when viewed in the stacking direction Am10. Overlapping the boundary B1 between the partition wall 11 and the pressure chamber 12 includes the case where the wall surface 11s of the partition wall 11 facing the pressure chamber 12 overlaps with the pressure chamber 12 from the position in the X-axis direction. Furthermore, the reinforcing film 51 is not formed on the active portion 50r1, but is formed on a part of the non-active portion 50r2. The reinforcing film 51 is formed on the first surface 50a1 side of the vibration plate 50. The reinforcing film 51 is formed so as to contact the second electrode 80 on the vibration plate 50. The reinforcing film 51 is formed in the X-axis direction from the position of the partition wall 11 to the position of the pressure chamber 12, straddling the boundary B1 between them.
[0055] As shown in FIG. 7, the reinforcing film 51 is formed in the range of the groove 71 so as to straddle adjacent pressure chambers 12 in a rectangular shape elongated in the Z-axis direction. In FIG. 7, the hatched portion indicates the inactive portion 50r2 of the groove 71. That is, the reinforcing film 51 is formed at least in the center of the active portion 50r1 in the Z-axis direction. Furthermore, the reinforcing film 51 is formed in the same manner in each of the multiple grooves 71. In addition, the length S1 of the reinforcing film 51 in the Z-axis direction is not continuous with the common lead electrode 92, or is formed within the range of the piezoelectric element 300. The reinforcing film 51 may be disposed so as to correspond to the entire active portion 50r1 in the Z-axis direction.
[0056] FIG. 8 is a cross-sectional view showing an enlarged view of the vicinity of the reinforcing film 51 in FIG. 6. FIG. 9 is a cross-sectional view showing the cross-sectional shape of the reinforcing film 51. In FIG. 8 and FIG. 9, a cross section parallel to the stacking direction Am10 and a second direction Am40 from the boundary B1 toward the center 12o of the pressure chamber 12 among the directions perpendicular to the stacking direction Am10 is shown. On the vibration plate 50, the end of the active portion 50r1 in the X-axis direction is called the position Xm. On the vibration plate 50, the end of the reinforcing film 51 in the X-axis direction is called the tip 51sc. Here, the tip 51sc overlaps with the non-active portion 50r2. In FIG. 9, the intersection of the first surface 50a1 of the vibration plate 50 and the boundary B1 is set as the origin 0. Furthermore, in FIG. 9, the second electrode 80 in the non-active portion 50r2 is omitted from the illustration because it can be substantially regarded as a part of the vibration plate 50. In the reinforcing film 51, a portion above the pressure chamber 12 in the +X direction from the origin 0 is called an end portion 51s.
[0057] FIG. 10 is an explanatory diagram showing a curve that defines the thickness Y of the end 51s of the reinforcing membrane 51. In FIG. 10, the locus T1 of the thickness Y calculated by the formula (3) is shown. The XY coordinates in FIG. 10 correspond to the XY coordinates in FIG. 9. That is, the locus T1 in FIG. 9 is shown based on the formula (3). The thickness Y of the end 51s is defined along the locus T1 as shown in FIG. 9. In the formula (3), when the first distance L between the boundary B1 as the origin 0 and the end 51s of the reinforcing membrane 51 closest to the center 12o of the pressure chamber 12 in the direction from the boundary B1 to the center 12o of the pressure chamber 12, and the thickness H of the reinforcing membrane 51 at the origin 0, the thickness Y of the reinforcing membrane 51 at an arbitrary distance X can be calculated as follows. In FIG. 9, the end 51s of the reinforcing membrane 51 closest to the boundary B1 and the center 12o of the pressure chamber 12 is the tip 51sc.
number
[0058] Equation (3) can be obtained by assuming that end 51s is a cantilever beam with boundary B1 in the -Y direction as the fixed end and tip 51sc as the free end. The thickness Y of end 51s defined by equation (3) makes the bending moment from tip 51sc to boundary B1 of reinforcing film 51 uniform when width S1 in the Z-axis direction in FIG. 7 is constant. In other words, thickness Y is calculated so that the section modulus from tip 51sc to boundary B1 is large. Such a cantilever beam is also called a cantilever beam of uniform strength.
[0059] Therefore, the thickness Y of the reinforcing film 51 in the stacking direction Am10 decreases in a second direction Am40 from the boundary B1 toward the center 12o of the pressure chamber 12.
[0060] The end 51s of the reinforcing film 51 is formed based on the locus T1 so as to further satisfy the conditions of the following formulas (1) and (2). On the vibration plate 50, the first thickness of the reinforcing film 51 in the stacking direction Am10 at the first position X1 as the position of the boundary B1 is defined as Y1, and the second thickness of the reinforcing film 51 in the stacking direction Am10 at the second position X2 closer to the center 12o of the pressure chamber 12 than the first position X1 is defined as Y2. The center 12o of the pressure chamber 12 is the center of the width of the pressure chamber 12 at the longest straight line portion of both side surfaces located at the boundary B1. Therefore, in the pressure chamber 12, the opposing side surfaces located at the boundary B1 may have non-parallel portions. The second position X2 is a position at the second thickness Y2 that reaches the locus T1. In addition, the absolute value of the inclination of the tangent a that is tangent to the inclined surface 51sa, which is the surface of the reinforcing film 51 that is not in contact with the vibration plate 50, is defined. That is, when the absolute value of the slope of the first tangent at the first position X1 is a1 and the absolute value of the slope of the second tangent at the second position X2 is a2, the end 51s of the reinforcing membrane 51 satisfies the conditions of equations (1) and (2). Y1>Y2 …(1) 0 <a1<a2 …(2)
[0061] With regard to the inclined surface 51sa, the surface of the reinforcing film 51 that does not contact the diaphragm 50 is, more specifically, the surface that does not contact a portion that is substantially regarded as the diaphragm 50. As described above, the second electrode 80 in the non-active portion 50r2 is substantially regarded as the diaphragm 50. Therefore, in the first embodiment, the surface of the reinforcing film 51 that does not contact the diaphragm 50 is the surface of the reinforcing film 51 that does not contact the diaphragm 50.
[0062] The reinforcing film 51 is made of a material having a lower Young's modulus than the diaphragm 50. For example, when the zirconium oxide of the diaphragm 50 has a Young's modulus of 200 GPa, the reinforcing film 51 is made of an organic material having a Young's modulus of 2.7 GPa. In this configuration, in this embodiment, the thickness H of the reinforcing film 51 is set to be 2.5 times the thickness Y of the diaphragm 50.
[0063] The reinforcing film 51 is formed by stacking an organic material on the vibration plate 50. The silicon oxide layer is formed by stacking layers La1 to La4, for example, as shown in FIG. 9. Furthermore, the higher the layer of silicon oxide, the shorter the length in the X-axis direction. That is, the positions of both ends of each layer La1 to La4 are different in the X-axis direction. Therefore, at the end 51s of the reinforcing film 51, recesses 51r1 to 51r3 are formed between each layer La1 to La4. The recesses 51r1 to 51r3 are also collectively referred to as recesses 51r. Each of the recesses 51r is formed deeper toward the boundary B1 side as it moves away from the layer in the +Y direction. That is, the width of each layer in the reinforcing film 51 in the X-axis direction is formed smaller for the higher layer. Therefore, the thickness Y of the end 51s of the reinforcing film 51 is smaller as it approaches the piezoelectric element 300.
[0064] Moreover, in each of the layers La1 to La4, the corners located at the end 51s of the reinforcing film 51 are chamfered. FIG. 9 illustrates a corner 51r4 of the layer La1. That is, the corner located at the end 51s of the reinforcing film 51 is a convex portion protruding from the reinforcing film 51 from the origin 0, which is the boundary B1, to the tip 51sc of the reinforcing film 51. The corners of the end 51s of the reinforcing film 51 are formed by removing the corners of each layer, for example, by anisotropic etching. Therefore, the end 51s of the reinforcing film 51 is formed closer to the locus T1 than when it is not chamfered.
[0065] In actual production, the reinforcing film 51 is formed by laminating materials as described above. Therefore, a recess 51r is generated at the end 51s of the reinforcing film 51. That is, the reinforcing film 51 having recesses and projections can be easily formed by setting the conditions of formulas (1) and (2) to correspond to actual production capacity, compared to the case where the reinforcing film 51 is formed according to the locus T1.
[0066] A3: Dispersion of stress by the reinforcing film 51 The stress generated in the diaphragm 50 by the reinforcing film 51 of the present disclosure will be described. In order to relatively evaluate the stress generated in the diaphragm 50, three types of analysis objects, namely, a first comparative example, a second comparative example, and an embodiment of the present disclosure, are used. Structural analysis by the finite element method is used to calculate the stress generated in the diaphragm 50. In the structural analysis by the finite element method, in addition to the shape of the analysis object, it is necessary to set the physical property value of the material, the support condition, the load condition, the mesh size, and the like. As described above, the Young's modulus as the physical property value of the material is 200 Gpa for the diaphragm 50 and 2.7 GPa for the reinforcing film 51. The support condition is that the partition 11 is fixed. The load condition is that a concentrated load F in the +Y direction is applied to the position Xm. However, the concentrated load F is not the same value in the three types of analysis objects described below. The concentrated load F is set so that the displacement amount U at the position Xm is a constant value. The displacement amount U will be described later. The mesh size is experimentally set according to the size and stress distribution of the analysis object. Three types of diaphragms 50 as analysis targets will be described below.
[0067] Fig. 11 is an explanatory diagram showing a cross section of the vibration plate 50 before displacement as a first comparative example. In the first comparative example of Fig. 11, only the vibration plate 50, the partition wall 11, and the pressure chamber 12 are shown, with the reinforcing film 51 in Fig. 8 removed. In the first comparative example of Fig. 11, in order to facilitate understanding of the technology, notation of XY coordinates, locus T1, and the like is omitted. Illustrations are similarly omitted in the drawings described later.
[0068] 11, the vibration plate 50 is in a state before receiving the concentrated load F due to pressure in the +Y direction. Specifically, this pressure is a state in which pressure is generated in the +Y direction by the ink flowing in the pressure chambers 12 due to pressure fluctuations in the multiple pressure chambers 12 when the liquid ejecting head 510 ejects ink. The position and direction of the concentrated load F are similar in the drawings described below.
[0069] FIG. 12 is an explanatory diagram showing a cross section of the reinforcing film Ob and the diaphragm 50 before displacement as a second comparative example. In the second comparative example of FIG. 12, a diaphragm 50 including a reinforcing film Ob is shown as a comparison object with the reinforcing film 51 of the present disclosure. The reinforcing film Ob has an end portion Obs as an end portion 51s of the reinforcing film 51. As shown in the second comparative example of FIG. 12, the end portion Obs is formed in a single layer with a rectangular cross-sectional shape. The thickness Y of the end portion Obs is a constant thickness Hob from the origin 0, which is the boundary B1, to the tip Obsc of the reinforcing film 51. In other words, the thickness Y of the end portion Obs is not formed along the locus T1 according to the formula (3).
[0070] Fig. 13 is an explanatory diagram showing a cross section of the reinforcing film 51 and the diaphragm 50 before displacement as an embodiment of the present disclosure. In the embodiment of the present disclosure in Fig. 13, the reinforcing film 51 is shown without the XY coordinates and some notations in Fig. 8.
[0071] FIG. 14 is an explanatory diagram showing a cross section of the diaphragm 50 after displacement as a first comparative example. In the first comparative example of FIG. 14, the position Xm in FIG. 11 is displaced in the +Y direction by the displacement amount U. In the first comparative example of FIG. 14, the displacement amount U of each part is shown typically by coloring in which the displacement amount U is divided into four stages based on the actual analysis result. That is, in the first comparative example of FIG. 14, the darker the color, the larger the displacement amount is shown. However, since the scale of the displacement amount is different in the similar drawings of FIG. 14 to FIG. 16, the displacement amount may differ even if the color is the same. As shown in FIG. 14, the diaphragm 50 is curved so as to reach the maximum displacement amount U at the position Xm, with the boundary B1 as the fulcrum.
[0072] Fig. 15 is an explanatory diagram showing a cross section of the reinforcing film Ob and the diaphragm 50 after displacement as a second comparative example. Fig. 16 is an explanatory diagram showing a cross section of the reinforcing film 51 and the diaphragm 50 after displacement as an embodiment of the present disclosure. In the second comparative example of Fig. 15 and the embodiment of the present disclosure of Fig. 16, as in the first comparative example of Fig. 14, the position Xm is displaced in the Y direction by a displacement amount U. The stress of the diaphragm 50 in the states of Figs. 14 to 16 will be described below.
[0073] FIG. 17 is a perspective view of the vibration plate 50 after displacement as a first comparative example. In the first comparative example of FIG. 17, a perspective view of the boundary B1 between the vibration plate 50 and the partition wall 11 is shown, in order to show the stress at the boundary B1. In the first comparative example of FIG. 17, the stress of each part is shown typically by coloring in which the maximum stress level is divided into four stages based on the actual analysis results. The stress of each part is similar to that of the second comparative example of FIG. 18 and the embodiment of the present disclosure of FIG. 19, which will be described later. Therefore, the distribution of stress can be compared relatively from the spread of the color of each part. In the first comparative example of FIG. 17, a state in which the darker the color, the larger the amount of displacement is shown. The boundary B11 and the boundary B12 show the ends in the Z-axis direction on the boundary B1 in FIG. 17. The boundary B11 is an end in the +Z direction from the boundary B12.
[0074] FIG. 18 is a perspective view of the reinforcing film Ob and the diaphragm 50 after displacement as a second comparative example. FIG. 19 is a perspective view of the reinforcing film 51 and the diaphragm 50 after displacement as an embodiment of the present disclosure. As shown in FIGS. 17 to 19, the distribution of the largest stress among the four stages of stress occurs in the vicinity of the partition wall 11 between the boundary B11 and the boundary B12 in the diaphragm 50. That is, in the diaphragm 50, the boundary B1 is a fixed end and a concentrated load F is received, so stress concentration occurs in the boundary B1 that is not displaced. However, in the second comparative example of FIG. 18, the diaphragm 50 with the reinforcing film Ob has a wider distribution of the largest stress than the diaphragm 50 in the first comparative example of FIG. 17. Furthermore, in the embodiment of the present disclosure of FIG. 19, the diaphragm 50 with the reinforcing film 51 has an even wider distribution of the largest stress than the diaphragm 50 with the reinforcing film Ob. The reinforcing film Ob has a constant thickness Y from the boundary B1 to the tip Obsc, so that the section modulus is also constant. On the other hand, the reinforcing membrane 51 has a section modulus that makes the bending moment uniform from the boundary B1 to the tip 51sc. Therefore, the reinforcing membrane 51 can further disperse stress concentration near the boundary B1 compared to the reinforcing membrane Ob having a constant thickness Y.
[0075] More specifically, the shape of the second surface 50a2 bent by the concentrated load F is linear in the reinforcing membrane 51 in the first comparative example in Fig. 14, and stress is concentrated at the base of the beam. On the other hand, in the reinforcing membrane 51 in the embodiment of the present disclosure in Fig. 16, the shape of the second surface 50a2 bent by the concentrated load F is closer to a circular arc, and stress is more evenly distributed.
[0076] By adopting such an embodiment, the reinforcing film 51 of the present disclosure is formed on the vibration plate 50 so as to overlap with the first position X1, which is the boundary B1 between the partition wall 11 and the pressure chamber 12, when viewed in the stacking direction Am10. Furthermore, the thickness Y of the reinforcing film 51 is formed to be thinner at the second position X2, which is closer to the center 12o of the pressure chamber 12 from the boundary B1. Furthermore, the thickness Y of the reinforcing film 51 is formed to be sharply thinner at the second position X2 than at the first position X1. As a result, the possibility of stress concentration at one point in the direction from the boundary B1 toward the center 12o of the pressure chamber 12 can be reduced. In other words, the possibility of cracks occurring in the vibration plate 50 can be reduced.
[0077] Furthermore, by providing the reinforcing film 51 on the non-active portion 50r2, it is possible to reinforce the non-active portion 50r2 in which stress is generated due to the vibration of the active portion 50r1, without significantly impeding the vibration of the active portion 50r1.
[0078] Moreover, the reinforcing film 51 is formed on the first surface 50a1, which is outside the pressure chamber 12, which is a part of the flow path. The second surface 50a2, on which the pressure chamber substrate 10 is provided, is the surface that defines the space of the pressure chamber 12, and is therefore located inside the flow path. Therefore, the reinforcing film 51 can be easily formed on the first surface 50a1, which has fewer surrounding obstacles, compared to when the reinforcing film 51 is formed on the second surface 50a2.
[0079] B. Second embodiment: FIG. 20 is a cross-sectional view showing the cross-sectional shape of the reinforcing film 51b. The reinforcing film 51b in the second embodiment corresponds to the reinforcing film 51 in the first embodiment. The reinforcing film 51b has a smaller thickness Y closer to the piezoelectric element 300, and has a recess 51r on the inclined surface 51bsa due to a step of the thickness Y. The reinforcing film 51b has recesses 51r at one or more locations. Furthermore, the reinforcing film 51b has a tangent a and a thickness Y defined for each recess 51r between the boundary B and the tip 51bsc of the reinforcing film 51b. In the following description, in order to facilitate understanding of the technology, a case where the recess 51r is provided at one location will be described as shown in FIG. 20. Other points of the liquid jet head 510 other than the reinforcing film 51b are the same as those of the first embodiment.
[0080] In the cross section of FIG. 20, the recess 51br is located closer to the center 12o of the pressure chamber 12 than the second position X2. The reinforcing film 51b is defined by the relationship between formulas (1) and (2) of the first embodiment in the section from the boundary B1 to the recess 51br. The reinforcing film 51b further defines a third thickness of the reinforcing film 51b in the stacking direction Am10 at the third position X3, which is the position of the recess 51br, as Y3, and a fourth thickness of the reinforcing film 51b in the stacking direction Am10 at the fourth position X4, which is closer to the center 12o of the pressure chamber 12 than the recess 51br, as Y4. As with the tangent a described above, when the absolute value of the slope of the third tangent at the third position X3 is a3 and the absolute value of the slope of the fourth tangent at the fourth position X4 is a4, the reinforcing film 51b satisfies the following formulas (4), (5), and (6). Y1>Y2>Y3>Y4 …(4) a3 <a2 …(5) 0 <a3<a4 …(6)
[0081] When the number of recesses 51br in the reinforcing membrane 51b is two or more, the tangent a and the thickness Y are newly defined for each recess 51br at positions corresponding to the third position X3 and the fourth position X4. That is, even when recesses 51br are provided at multiple positions like the reinforcing membrane 51 of the first embodiment, the reinforcing membrane 51b is formed so that the newly defined tangent a and thickness Y satisfy the same relationship as the tangent a1 to tangent a4 and the thickness Y1 to thickness Y4.
[0082] In this manner, the thickness Y of the reinforcing film 51b can be divided into two layers with the position of the recess 51br as the boundary. Therefore, the reinforcing film 51b may be easier to form by forming the inclined surface in two layers than by forming the inclined surface in one layer.
[0083] Furthermore, the recesses 51br of the reinforcing film 51b facilitate deformation when the reinforcing film 51b is displaced in the +Y direction together with the displacement of the diaphragm 50. Therefore, the recesses 51br can relieve the compressive stress applied to the reinforcing film 51b. This effect is similar to that in the case of a plurality of recesses 51r as in the first embodiment.
[0084] C. Third embodiment: Fig. 21 is a cross-sectional view showing a cross section of a pressure chamber 12c of the third embodiment. Fig. 21 shows a cross section corresponding to Fig. 6 of the first embodiment. The pressure chamber 12c of the third embodiment has a space that extends to the adjacent piezoelectric element 300c in the X-axis direction so as to straddle the groove portion 71. Therefore, the boundary B2 between the partition 11c and the pressure chamber 12c is located at the same position as the piezoelectric element 300c in the X-axis direction. In other words, the piezoelectric element 300c is formed so as to overlap the boundary B2 between the partition 11c and the pressure chamber 12c when viewed along the stacking direction Am10.
[0085] In the piezoelectric element 300c, the thickness in the Y-axis direction on the side of the center 12co of the pressure chamber 12c from the boundary B2 to the groove portion 71 is defined based on formula (3) in the same manner as the thickness Y of the reinforcing film 51 shown in Fig. 10. Therefore, the piezoelectric element 300c is formed such that the thickness Y of the piezoelectric element 300c decreases from the boundary B1 toward the center 12co of the pressure chamber 12. That is, in the third embodiment, the reinforcing film 51 is not provided, and instead the cross-sectional shape of the piezoelectric element 300c is made to be the cross-sectional shape based on Fig. 10, thereby dispersing the stress generated in the vibration plate 50.
[0086] Fig. 22 is an explanatory diagram showing the vibration plate 50 after displacement in the third embodiment. Fig. 22 shows a state of the vibration plate 50 displaced by a displacement amount U due to pressure being applied to the vibration plate 50 in the +Y direction. As shown in Fig. 22, the displacement of the vibration plate 50 occurs at the position of the groove portion 71 since the vibration plate 50 is located between the adjacent piezoelectric elements 300c. Therefore, stress concentration occurs at the boundary B2 of the vibration plate 50.
[0087] The piezoelectric element 300c is formed so as to become thinner from the boundary B2 toward the center 12co of the pressure chamber 12, and has a section modulus to make the bending moment uniform. Therefore, the piezoelectric element 300c can reduce the possibility of stress concentrating at one point in the direction from the boundary B2 toward the center 12co of the pressure chamber 12c. In other words, the possibility of cracks occurring in the vibration plate 50 can be reduced.
[0088] D. Fourth embodiment: FIG. 23 is an explanatory diagram showing a reinforcing film 51d of the fourth embodiment. In the above embodiment, the reinforcing film 51 is formed on the first surface 50a1. However, the reinforcing film 51 may be formed on the second surface 50a2. For example, as in the reinforcing film 51d of FIG. 23, the reinforcing film 51d may be formed across the partition wall 11 and the diaphragm 50. As described above, overlapping the boundary B1 between the partition wall 11 and the pressure chamber 12 includes overlapping from the position of the wall surface 11s of the partition wall 11 facing the pressure chamber 12 in the X-axis direction to the pressure chamber 12. That is, the reinforcing film 51d reinforces the boundary B1 so as to cover it from the second surface 50a2.
[0089] With this configuration, the reinforcing film 51b can directly reinforce the boundary B1, where stress concentration occurs, between the partition wall 11 and the pressure chamber 12. Therefore, the reinforcing film 51b can reinforce the boundary B1 more accurately than when the boundary B1 is reinforced from the first surface 50a1 where no partition wall 11 exists.
[0090] E1. Variation 1: In the first embodiment, the reinforcing film 51 has a recess 51r at the end 51s. However, the reinforcing film 51 may be formed along the locus T1, so that the end 51s does not have to have the recess 51r. The recess 51r is generated by stacking the material of the reinforcing film 51. Therefore, for example, the size of the recess 51r can be reduced by increasing the number of stacked layers. That is, in practice, it is possible to form the end 51s having a section modulus equivalent to the shape of the end 51s formed along the locus T1.
[0091] E2. Variation 2: In the first embodiment, the thickness Y of the end 51s of the reinforcing membrane 51 is defined so as to satisfy the conditions of formulas (1) and (2). However, when the absolute value of the thickness Y3 of the end 51s and the gradient of the tangent a is a3 at the third position X3, which is an intermediate position between the first position X1 and the second position X2, the thickness Y of the end 51s may be defined so as to satisfy the conditions of formulas (7), (8), and (9). Y1>Y3>Y2 …(7) 0>a1>a3>a2 …(8) |Y1-Y3|<|Y1-Y3| …(9)
[0092] In this manner, the reinforcing film 51 is formed closer to the locus T1 than in the case defined by formulas (1) and (2). That is, the reinforcing film 51 may be able to reduce the concentration of stress generated in the diaphragm 50 compared to the first embodiment.
[0093] E3. Variation 3: In the first embodiment, the reinforcing membrane 51 is defined by formulas (1) and (2). However, the reinforcing membrane 51 may be defined by formula (10) that takes into account actual manufacturing errors. The reinforcing membrane 51 satisfies formula (10) when a first distance L is defined between the boundary B1 and an end 51s of the reinforcing membrane 51 that is closest to the center 12o of the pressure chamber 12 in a direction from the boundary B1 toward the center 12o of the pressure chamber 12. The second distance X2 is also the distance from the first position X1 to the second position X2.
number
[0094] In this embodiment, the reinforcing membrane 51 has a more uniform stress distribution than when it is defined by formulas (1) and (2).
[0095] Although formula (10) has a tolerance of ±20% for manufacturing error, the range may be ±30%, or +20% to -10%, depending on the actual manufacturing capacity.
[0096] Furthermore, the reinforcing membrane 51 does not have to be defined by formulas (1) and (2). That is, the reinforcing membrane 51 may be defined only by formula (10).
[0097] E4. Variation 4: In the above embodiment, the reinforcing film 51 is formed by laminating materials. However, the reinforcing film 51 may be formed of a material that solidifies from a fluid, such as an adhesive or UV ink. For example, by changing the wettability of the surface of the diaphragm 50 at the position where the tip 51sc of the reinforcing film 51 is to be provided, the amount of material into which the material of the reinforcing film 51 flows before solidification changes. In other words, the curved shape of the inclined surface 51sa of the reinforcing film 51 can be adjusted by changing the wettability of the surface of the diaphragm 50 and the surface tension of the material of the reinforcing film 51 before solidification.
[0098] F. Variations: (1) In the above embodiment, the reinforcing film 51 is formed within the groove portion 71 so as to straddle adjacent pressure chambers 12, as shown in FIG. 7. However, the reinforcing film 51 does not necessarily have to be formed so as to straddle adjacent pressure chambers 12. The reinforcing film 51 only needs to be formed so as to cover the boundary B1 when viewed along the stacking direction Am10. That is, the reinforcing film 51 may be formed by two reinforcing films 51 for each of the two boundaries B1 within the groove portion 71. A plurality of reinforcing films 51 may be formed.
[0099] (2) In the above embodiment, the reinforcing film 51 is formed in a rectangular shape that is elongated in the Z-axis direction, as shown in Fig. 7. However, the reinforcing film 51 is not limited to a rectangular shape. As described above, the reinforcing film 51 may be in a quadrangular or elliptical shape as long as it can overlap the boundary B1 between the partition wall 11 and the pressure chamber 12 when viewed in the stacking direction Am10.
[0100] Further, the reinforcing film 51 is formed in the center of the active portion 50r1 in the Z-axis direction as shown in Fig. 7. However, the reinforcing film 51 is not limited to the center of the active portion 50r1. For example, the reinforcing film 51 may be formed on the nozzle 21 side in the +Z direction from the center of the active portion 50r1 in Fig. 7. Alternatively, the reinforcing film 51 may be formed over the entire range of the groove portion 71.
[0101] Moreover, the reinforcing membrane 51 does not have to be formed in the same way as the grooves 71 adjacent to each other in the X-axis direction, as shown in Fig. 7. For example, in the second pressure chamber row Lb in Fig. 3, the reinforcing membrane 51 may be formed so that the grooves 71 located at the ends of the row are smaller and the grooves 71 located at the center of the row are larger. Alternatively, the position or shape of the reinforcing membrane 51 may be different in each of the multiple grooves 71.
[0102] (3) In the above embodiment, the reinforcing film 51 is formed so as to be in contact with the second electrode 80 on the diaphragm 50. However, as described above, when the second electrode 80 is not present in the groove portion 71, the reinforcing film 51 may be formed so as to be in contact with the diaphragm 50. Alternatively, when the piezoelectric layer 70 is present in the groove portion 71, the reinforcing film 51 may be formed so as to be in contact with the piezoelectric layer 70.
[0103] (4) In the above embodiment, the diaphragm 50 is made of zirconium oxide. The reinforcing film 51 is made of an organic material. However, the reinforcing film 51 may be made of the same material as the diaphragm 50. That is, the reinforcing film 51 may be made of zirconium oxide or the material of the diaphragm 50 described later.
[0104] (5) In the above embodiment, the piezoelectric layer 70 is made of lead zirconate titanate (PZT). The reinforcing film 51 is made of an organic material. However, the reinforcing film 51 may be made of the same material as the piezoelectric layer 70. That is, the reinforcing film 51 may be made of lead zirconate titanate (PZT) or the material of the piezoelectric layer 70 described later.
[0105] (6) In the above embodiment, the recess 51r is a step having a thickness Y on the inclined surface 51sa. That is, the recess 51r is a recess formed in the thickness direction of the reinforcing film 51. However, the recess 51r does not have to be recessed in the thickness direction. For example, the recess 51r may have a shape having an inflection point or a non-differentiable point on the inclined surface 51sa.
[0106] (7) In the above embodiment, the slope of the tangent line a at the measurement point may be, for example, the slope between two points moved by ±L / 10 along the X-axis direction. Alternatively, the slope of the tangent line a may be the average value of the slopes of the tangent line at any number of measurement points within a range of ±L / 10 along the X-axis direction.
[0107] G. Variations: (1) In the above embodiment, the shape of the pressure chamber 12 is not limited to a rectangle, and may be a parallelogram, a polygon, a circle, an oval, etc. The oval shape here refers to a shape that is based on a rectangle and has semicircular ends at both longitudinal ends, and includes a rectangle with rounded corners, an ellipse, etc.
[0108] (2) In the above embodiment, the arrangement direction Am21 refers to the macroscopic arrangement direction Am21 of the multiple pressure chambers 12. For example, when the multiple pressure chambers 12 are arranged along the X-axis direction so that every other pressure chamber 12 is staggered in the intersecting direction Am30, the X-axis direction is included in the arrangement direction Am21.
[0109] (3) In the above embodiment, the grooves 71 are formed by completely removing the piezoelectric layer 70 in the Y-axis direction. However, the grooves 71 may be formed in a state where the piezoelectric layer 70 is removed in the +Y-axis direction and remains. In other words, the grooves 71 may be formed thinner than other parts of the piezoelectric layer 70.
[0110] H. Other forms: The present disclosure is not limited to the above-mentioned embodiment, and can be realized in various forms without departing from the spirit of the present disclosure. For example, the present disclosure can be realized in the following forms. The technical features in the above-mentioned embodiments corresponding to the technical features in each form described below can be appropriately replaced or combined in order to solve some or all of the problems of the present disclosure, or to achieve some or all of the effects of the present disclosure. Furthermore, if the technical feature is not described as essential in this specification, it can be appropriately deleted.
[0111] (1) According to one aspect of the present disclosure, there is provided a liquid jet head, which is a liquid jet head in which a piezoelectric element that deforms when a voltage is applied thereto and includes a first electrode, a piezoelectric layer, and a second electrode, a vibration plate that vibrates when the piezoelectric element is driven, a reinforcing film, and a pressure chamber substrate that constitutes a partition wall that defines a pressure chamber communicating with a nozzle together with the vibration plate, are laminated in a lamination direction, the vibration plate is vibrated in the lamination direction by the piezoelectric element to apply pressure to liquid in the pressure chamber, the reinforcing film is formed along a first direction that is perpendicular to the lamination direction, and when viewed in the lamination direction, the partition wall and the pressure chamber substrate are laminated in a lamination direction. In a cross section that overlaps the boundary between the pressure chamber and the vibration plate and is parallel to the stacking direction and the direction from the boundary toward the center of the pressure chamber, a first thickness of the reinforcing membrane in the stacking direction at a first position as the position of the boundary is defined as Y1, a second thickness of the reinforcing membrane in the stacking direction at a second position closer to the center of the pressure chamber than the first position is defined as Y2, and the absolute value of the slope of a tangent to an inclined surface of the reinforcing membrane that does not contact the vibration plate is defined as a1, and the absolute value of the slope of a second tangent to the reinforcing membrane at the second position is defined as a2. Y1>Y2 …(1) and 0 <a1<a2 …(2) The above formulas (1) and (2) are satisfied. By adopting such an embodiment, the reinforcing film of the present disclosure is formed on the diaphragm so as to cover a first position which is the boundary between the partition wall and the pressure chamber. Furthermore, the thickness of the reinforcing film is formed to be thinner at a second position on the pressure chamber side from the boundary. Furthermore, the thickness of the reinforcing film is formed to be sharply thinner at the second position than at the first position. As a result, the possibility of stress concentrating at one point in the direction from the boundary toward the pressure chamber can be reduced. In other words, the reinforcing film can reduce the possibility of cracks occurring in the diaphragm.
[0112] (2) In the above embodiment, when the liquid ejection head has an active portion in the vibration plate where the first electrode, the piezoelectric layer, the second electrode, and the pressure chamber overlap in the stacking direction, and a non-active portion in the vibration plate that is a portion different from the active portion and where the pressure chamber overlaps in the stacking direction, the reinforcing film may be formed in a part of the non-active portion. By adopting such an embodiment, the reinforcing film can reinforce the non-active portion in which stress is generated by the vibration of the active portion without significantly impeding the vibration of the active portion.
[0113] (3) In the above embodiment, when the surface of the vibration plate on which the piezoelectric element is provided in the stacking direction is defined as a first surface and the surface on which the pressure chamber substrate is provided is defined as a second surface, the reinforcing film may be formed on the first surface. In this embodiment, the second surface on which the pressure chamber substrate is provided is a surface that defines the space of the pressure chamber, and is therefore located inside the flow path. Thus, the reinforcing film is easily formed on the first surface, which has fewer surrounding obstacles, compared to when the reinforcing film is formed on the second surface.
[0114] (4) In the above aspect, when the surface of the vibration plate in the stacking direction on which the piezoelectric element is provided is defined as a first surface and the surface on which the pressure chamber substrate is provided is defined as a second surface, the reinforcing film may be formed on the second surface. With this aspect, the reinforcing film can directly reinforce the boundary between the partition wall and the pressure chamber, where stress concentration occurs. Therefore, the reinforcing film can reinforce the boundary more accurately than when reinforcing from the first surface where no partition wall exists.
[0115] (5) In the above-described embodiment, the reinforcing film may be configured to satisfy the above formula (10) when a first distance between the boundary and an end of the reinforcing film closest to the center of the pressure chamber in a direction from the boundary to the center of the pressure chamber is L, and a second distance from the first position to the second position is X2. By adopting such an embodiment, the stress distribution becomes more uniform compared to the above-described embodiment.
[0116] (6) In the above aspect, in the liquid ejection head, the reinforcing film has a thickness that decreases toward the piezoelectric element, and the inclined surface is provided with a recess due to a step in the thickness, and in the cross section, the recess is disposed at a position closer to the center of the pressure chamber than the second position, and the reinforcing film further has a third thickness of the reinforcing film in the stacking direction at a third position as the position of the recess is defined as Y3, a fourth thickness of the reinforcing film in the stacking direction at a fourth position closer to the center of the pressure chamber than the recess is defined as Y4, and the tangent has an absolute value of a slope of the third tangent at the third position as a3 and an absolute value of a slope of the fourth tangent at the fourth position as a4, Y1>Y2>Y3>Y4 …(4) a3 <a2 …(5) 0 <a3<a4 …(6) The above formulas (4), (5), and (6) may be satisfied. In this embodiment, the thickness of the reinforcing film can be divided into two layers with the position of the recess as the boundary. Therefore, the reinforcing film may be easier to form by forming a sloped surface with two layers compared to forming a sloped surface with one layer.
[0117] (7) In the above-described embodiment, in the liquid jet head, the reinforcing film may be made of the same material as the diaphragm. In this embodiment, it is not necessary to prepare a material different from that of the diaphragm for the reinforcing film, and therefore the reinforcing film may be manufactured more easily than when a different material is prepared.
[0118] (8) In the liquid jet head according to the above aspect, the reinforcing film may be made of the same material as the piezoelectric layer. In this manner, it is not necessary to prepare a material different from that of the piezoelectric layer for the reinforcing film, and therefore the reinforcing film may be manufactured more easily than when a different material is prepared.
[0119] (9) According to a second aspect of the present disclosure, there is provided a liquid jet head, which is a liquid jet head in which a piezoelectric element that deforms when a voltage is applied thereto and includes a first electrode, a piezoelectric layer, and a second electrode, a vibration plate that vibrates when the piezoelectric element is driven, a reinforcing film, and a pressure chamber substrate that constitutes a partition wall that defines a pressure chamber communicating with a nozzle together with the vibration plate, are laminated in a lamination direction, the vibration plate is vibrated in the lamination direction by the piezoelectric element to apply pressure to liquid in the pressure chamber, the reinforcing film is formed along a first direction that is perpendicular to the lamination direction, and when viewed in the lamination direction, the partition wall is formed along a first direction that is perpendicular to the lamination direction, and the reinforcing film is formed along a first direction that is perpendicular to the lamination direction, and ... and the pressure chamber, in a cross section parallel to the stacking direction and a direction from the boundary toward the center of the pressure chamber, the above formula (10) is satisfied when a first thickness of the reinforcing membrane in the stacking direction at a first position as the position of the boundary is Y1, a second thickness of the reinforcing membrane in the stacking direction at a second position closer to the center of the pressure chamber than the first position is Y2, a first distance in the first direction between the boundary and the end of the reinforcing membrane closest to the center of the pressure chamber is L, and a second distance from the first position to the second position is X2. By adopting such an embodiment, the stress distribution becomes more uniform compared to the first embodiment. [Explanation of symbols]
[0120] P...printing paper, X...distance, X2...second distance, Xm...position, 10...pressure chamber substrate, 11...partition wall, 11c...partition wall, 11s...wall surface, 12, 12c...pressure chamber, 12a, 12b...end, 12o, 12co...center, 15...communication plate, 16...nozzle communication passage, 17...first manifold portion, 18...second manifold portion, 19...supply communication passage, 20...nozzle plate, 21...nozzle, 30...protective substrate, 31...holding portion, 32...through hole, 40...case member, 41...accommodation portion, 42...third manifold portion, 43...connection port, 44...supply port, 45...co Compliance substrate, 46...sealing film, 47...fixed substrate, 48...opening, 49...compliance portion, 50...diaphragm, 50a1...first surface, 50a2...second surface, 50r1...active portion, 50r2...non-active portion, 51...reinforcing film, 51b...reinforcing film, 51r, 51r1, 51r3, 51br...recess, 51bs...end, 51d...reinforcing film, 51r4...corner, 51s...end, 51sa...inclined surface, 51sc...tip, 55...elastic film, 56...insulating film, 60...first electrode, 60a, 60b...end, 70...piezoelectric layer, 70a, 70b...end, 71... Groove portion, 80... second electrode, 80a, 80b, 80c... end portion, 85... wiring portion, 91... individual lead electrode, 92... common lead electrode, 92a, 92b... extension portion, 100... manifold, 120... wiring board, 121... integrated circuit, 300, 300c... piezoelectric element, 310... piezoelectric element, 500... liquid ejection device, 510... liquid ejection head, 540... control unit, 550... ink tank, 552... tube, 560... transport mechanism, 562... transport roller, 564... transport rod, 566... transport motor, 570... movement mechanism, 572... Carriage, 574...conveyor belt, 576...movement motor, 577...pulley, Am10...direction, Am20...first direction, Am21...arrangement direction, Am30...cross direction, Am40...second direction, B1, B11, B12, B2...boundary, F...concentrated load, L...first distance, La...first pressure chamber row, La1, La2, La3, La4...layer, Lb...second pressure chamber row, Ob...reinforcing membrane, Obs...end, Obsc...tip, S1...width, T1...trajectory, U...displacement, X1...first position, X2...second position, X3...third position, X4...fourth position, a...tangent
Claims
1. In the stacking direction, a piezoelectric element that is deformed by application of a voltage and includes a first electrode, a piezoelectric layer, and a second electrode; a vibration plate that vibrates when driven by the piezoelectric element; A reinforcing film; a pressure chamber substrate which constitutes a partition wall that defines, together with the diaphragm, a pressure chamber communicating with a nozzle; A liquid jet head in which the vibration plate is vibrated in the stacking direction by the piezoelectric element to apply pressure to the liquid in the pressure chamber; the reinforcing film is formed along a first direction that is a direction perpendicular to the stacking direction, and overlaps a boundary between the partition wall and the pressure chamber when viewed in the stacking direction; In a cross section parallel to the stacking direction and the direction from the boundary toward the center of the pressure chamber, A first thickness of the reinforcing membrane in the stacking direction at a first position as the position of the boundary is defined as Y1, a second thickness of the reinforcing film in the stacking direction at a second position closer to the center of the pressure chamber than the first position is defined as Y2; an absolute value of a slope of a tangent of an inclined surface of the reinforcing film that is not in contact with the diaphragm, The absolute value of the gradient of the first tangent at the first position is a1; When the absolute value of the slope of the second tangent at the second position is a2, Y1>Y2 ... (1) and 0<a1<a2...(2) A liquid jet head that satisfies the above formulas (1) and (2).
2. The liquid jet head according to claim 1 , a region of the vibration plate where the first electrode, the piezoelectric layer, the second electrode, and the pressure chamber overlap in the stacking direction is defined as an active portion; When a region of the diaphragm that is a portion different from the active portion and overlaps with the pressure chamber when viewed in the stacking direction is defined as a non-active portion, The reinforcing film is not formed on the active portion, but is formed on a part of the non-active portion.
3. The liquid jet head according to claim 2 , In the diaphragm, When a surface in the stacking direction on which the piezoelectric element is provided is defined as a first surface, and a surface on which the pressure chamber substrate is provided is defined as a second surface, The reinforcing film is formed on the first surface of the liquid ejecting head.
4. The liquid jet head according to claim 2 , In the diaphragm, When a surface on which the piezoelectric element is provided in the stacking direction is defined as a first surface, and a surface on which the pressure chamber substrate is provided is defined as a second surface, The reinforcing film is formed on the second surface of the liquid ejecting head.
5. The liquid jet head according to claim 1 , The reinforcing film is When a first distance between the boundary and an end of the reinforcing membrane that is closest to the center of the pressure chamber in a direction from the boundary toward the center of the pressure chamber is defined as L, and a second distance from the first position to the second position is defined as X2, [0010] A liquid jet head that satisfies the above formula (3).
6. The liquid jet head according to claim 1 , The reinforcing film is The thickness is smaller closer to the piezoelectric element, a recess formed on the inclined surface due to a step in the thickness; In the cross section, the recess is disposed at a position closer to a center of the pressure chamber than the second position, The reinforcing membrane further comprises: A third thickness of the reinforcing film in the stacking direction at a third position as the position of the recess is defined as Y3; a fourth thickness of the reinforcing film in the stacking direction at a fourth position closer to the center of the pressure chamber than the recess is defined as Y4; The tangent line, The absolute value of the gradient of the third tangent at the third position is a3; When the absolute value of the gradient of the fourth tangent at the fourth position is a4, Y1>Y2>Y3>Y4...(4) a3 < a2 ... (5) 0<a3<a4...(6) A liquid jet head that satisfies the above expressions (4), (5), and (6).
7. 7. The liquid jet head according to claim 1, The liquid ejection head, wherein the reinforcing film is made of a same material as the vibration plate.
8. 7. The liquid jet head according to claim 1, The reinforcing film is made of a same material as the piezoelectric layer.
9. In the stacking direction, a piezoelectric element that is deformed by application of a voltage and includes a first electrode, a piezoelectric layer, and a second electrode; a vibration plate that vibrates when driven by the piezoelectric element; A reinforcing film; a pressure chamber substrate which constitutes a partition wall that defines, together with the diaphragm, a pressure chamber communicating with a nozzle; A liquid jet head in which the vibration plate is vibrated in the stacking direction by the piezoelectric element to apply pressure to the liquid in the pressure chamber; the reinforcing film is formed along a first direction that is a direction perpendicular to the stacking direction, and overlaps a boundary between the partition wall and the pressure chamber when viewed in the stacking direction; In a cross section parallel to the stacking direction and the direction from the boundary toward the center of the pressure chamber, A first thickness of the reinforcing membrane in the stacking direction at a first position as the position of the boundary is defined as Y1, A second thickness of the reinforcing film in the stacking direction at a second position closer to the center of the pressure chamber than the first position is defined as Y2, and When a first distance in the first direction between the boundary and an end of the reinforcing membrane that is closest to the center of the pressure chamber is L, and a second distance from the first position to the second position is X2, [0010] A liquid jet head that satisfies the above formula (3).
Citation Information
Patent Citations
Liquid injection head, liquid injection device, and piezoelectric actuator
JP2019005924A