Sterilization agent visualization material

A laminated disinfectant visualization material with a colored and water-repellent layer changes color upon ethanol water application, addressing the need for simple and effective sterilization verification in wet environments.

JP2024144323APending Publication Date: 2024-10-11CANON KK
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2024050581
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-28
Filing Date
2024-03-26
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

Existing methods for visualizing cleaning and sterilization actions require the application of a specific liquid, lacking simplicity and effectiveness in environments where exposure to water is frequent, such as in restaurants, where ethanol water is commonly used as a disinfectant.

Method used

A disinfectant visualization material with a laminated structure comprising a base material, a colored part, and a water-repellent part, where the colored part changes color upon application of ethanol water, ensuring visibility of the sterilizing effect even in wet conditions.

Benefits of technology

The material effectively changes color upon ethanol water application, allowing confirmation of sterilization despite frequent water exposure, maintaining a sterilizing effect and simplifying verification of disinfectant use.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024144323000001_ABST
    Figure 2024144323000001_ABST
Patent Text Reader

Abstract

To provide a sterilization agent visualization material that, even if it is frequently exposed to water, develops color upon application of ethanol water having a sterilization effect, and thereby allows checking of the sterilization effect.SOLUTION: A sterilization agent visualization material has a structure in which a base material, a color development part, and a water repellent part are stacked in this order, and upon application of a sterilization agent, a color development state of the color development part changes.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a disinfectant visualization material. [Background technology]

[0002] The act of cleaning or disinfection is considered important, and a technology for visualizing the act has been disclosed. Patent Document 1 discloses a method for confirming that a specific invisible solution has been removed by cleaning or disinfecting a target area by irradiating the area with ultraviolet light after cleaning or disinfecting the target area with the solution.

[0003] Patent Document 2 discloses that a composition containing a pH indicator dye, an alkaline substance, and a disinfectant is used for disinfection. The disinfection by this composition can be visually confirmed.

[0004] However, the methods for visualizing cleaning and sterilization actions as described in Patent Documents 1 and 2 require the application of a specific liquid, and therefore lack convenience. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] U.S. Patent No. 8,519,360 [Patent Document 2] US Patent Application Publication No. 2014 / 0057987 Summary of the Invention [Problem to be solved by the invention]

[0006] The present inventors have considered that the use of a material (disinfectant visualization material) whose color state changes when a disinfectant such as a disinfectant is applied would be effective in solving the problem of lack of simplicity that the above-mentioned conventional technology faces. Furthermore, the present inventors have found problems in actually using the disinfectant visualization material.

[0007] Ethanol water is generally used as a disinfectant. Therefore, it is necessary to use a material whose color state changes when a neutral disinfectant such as ethanol water is applied. However, in situations where disinfectants and disinfectants are expected to be used, such as restaurants, the material is often exposed to water. Since water is insufficient in terms of disinfection effect, we thought that a disinfectant visualization material that can confirm that ethanol water has been applied is necessary. In other words, we came up with the idea of ​​providing a disinfectant visualization material that changes color when ethanol water, which has a disinfecting effect, is applied and the disinfection effect can be confirmed even in situations where the material is often exposed to water. [Means for solving the problem]

[0008] The disinfectant visualization material according to the present invention has a structure in which a base material, a color portion, and a water-repellent portion are laminated in this order, and the color portion changes in color when a disinfectant is applied. Effect of the Invention

[0009] The disinfectant-visualizing material according to the present invention has a water-repellent portion, and therefore changes color when ethanol water, which has a disinfecting effect, is applied to the material, even in situations where the material is frequently exposed to water, thereby making it possible to confirm the disinfecting effect. [Brief description of the drawings]

[0010] [Figure 1] FIG. 1 is a schematic diagram of a disinfectant-visualizing material according to a first embodiment of the present invention. [Diagram 2] FIG. 2 is a schematic diagram of a disinfectant-visualizing material according to a second embodiment of the present invention. [Diagram 3] FIG. 13 is a schematic diagram of a disinfectant-visualizing material according to a third embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Hereinafter, embodiments of the present invention will be described, but the present invention is not limited to these.

[0012] In this embodiment, the surface to be sterilized may be any surface, such as a desk, table, chair, floor, wall, etc., and may be either horizontal or vertical. The surface to be sterilized may be a wood, plastic, or metal surface, and the surface may be provided with a film or coated with particles.

[0013] In this embodiment, the disinfectant and the coloring part are arranged separately, and when used, the disinfectant reacts with a coloring agent (described later) contained in the coloring part. The coloring agent is arranged on the surface to be disinfected, and the coloring state (appearance) changes when the disinfectant comes into contact with the surface. This change in appearance can be recognized visually.

[0014] First Embodiment The disinfectant visualization material 100 according to the present embodiment has a structure in which a base material 101, a coloring portion 102, and a water-repellent portion 103 are laminated in this order. The coloring portion 102 changes in color when a disinfectant is applied. By providing such a disinfectant visualization material on a target to which a disinfectant is applied, the coloring portion 102 changes in color when ethanol water is applied, so that it is possible to confirm that the disinfectant has been applied. In addition, when water is applied to this disinfectant visualization material, the water-repellent effect of the water-repellent portion 103 makes it difficult for water to reach the coloring portion 102. Therefore, even in a situation where exposure to water occurs frequently, the disinfectant visualization material changes color when ethanol water having a disinfecting effect is applied, and the disinfecting effect can be confirmed. That is, the disinfectant visualization material according to the present embodiment has a different coloring state when water is applied and when ethanol water is applied, and it is possible to distinguish between the two.

[0015] The disinfectant is provided with a colored portion when the disinfectant is provided to the disinfectant visualization material, and the time during which the disinfectant reacts with the colored portion is short. This allows the material to be easily stored for a long time. Here, providing the disinfectant means that the disinfectant reaches the colored portion, and examples of the providing include spraying the disinfectant and wiping with a duster containing the disinfectant.

[0016] The disinfectant visualization material in this embodiment only needs to have a structure in which a substrate, a color portion, and a water-repellent portion are laminated in this order, and may have other portions between the substrate, the color portion, and the water-repellent portion.

[0017] The disinfectant-visualizing material in this embodiment is in the form of a film, but may be in the form of a sphere as described in the second embodiment.

[0018] (Water-repellent part) The water-repellent portion in this embodiment is not particularly limited as long as it contains a material having water repellency (which may also be called a water repellent agent), but it is preferable to use a material that is easily permeable to ethanol water. In addition, the water-repellent portion according to this embodiment may have a contact angle with water of 80 degrees or more.

[0019] The water-repellent portion in this embodiment may contain at least one resin selected from the group consisting of acrylic resin, acrylamide resin, and polyalkylene. These resins also include derivatives of these resins within the scope of the effects of the present invention. As derivatives of these resins, for example, with respect to a part of the side chains of these resins, the ester group or amide group contained in the side chain may be an aliphatic hydrocarbon or an aromatic hydrocarbon. Furthermore, the hydrocarbon group contained in these resins may be a saturated or unsaturated hydrocarbon, and may be a straight-chain or branched hydrocarbon. Furthermore, a part of these resins may be substituted. Furthermore, the hydrocarbon group contained in these resins may contain an aliphatic hydrocarbon or an aromatic hydrocarbon. Here, the carbon number of the aliphatic hydrocarbon may be 7 or more and 40 or less, preferably 10 or more and 30 or less, and more preferably 11 or more and 26 or less. For example, the water-repellent portion may contain a resin obtained by polymerizing lauryl methacrylate or stearyl methacrylate. The molecular weight of the above acrylic resin or acrylamide resin is preferably 5000 or more and 200000 or less.

[0020] Here, it is preferable that the water-repellent portion contains a material that has high adhesion to the color-changing portion. In particular, when the color-changing portion contains a phthalein dye that is soluble in ethanol, if there is a defect in the water-repellent portion, the phthalein dye may be wiped off by wiping with ethanol water. Therefore, the water-repellent portion is required to have high adhesion to the color-changing portion. As a material that realizes high adhesion, it is preferable that the water-repellent portion contains a compound containing oxygen (carbonyl group). This is because when the water-repellent portion contains a compound containing oxygen (carbonyl group), the adhesion between the water-repellent portion and the color-changing portion is increased when the color-changing portion contains a phthalein dye. This is thought to be because there is a high affinity between the hydroxyl group contained in the phthalein dye and the carbonyl group of the compound contained in the water-repellent portion.

[0021] Furthermore, the water-repellent portion according to this embodiment may have at least one compound represented by the following formula (1) and formula (2).

[0022] [ka] CH3-(CH2)n-CH3Formula (2)

[0023] In the above formula (1), R is a linear or branched hydrocarbon group having a carbon number of 7 or more and 40 or less. R in the above formula (1) is preferably a hydrocarbon group having a carbon number of 10 or more and 30 or less, and more preferably a hydrocarbon group having a carbon number of 11 or more and 26 or less. In addition, the molecular weight of the compound represented by the above formula (1) can be 5,000 or more and 200,000 or less.

[0024] In the above formula (2), n may be an integer of 15 or more and 40 or less, or n may be an integer of 22 or more and 34 or less.

[0025] In this embodiment, the thickness of the water-repellent portion in the stacking direction can be 10 nm or more and 800 nm or less, preferably 10 nm or more and 600 nm or less, and more preferably 10 nm or more and 400 nm or less.

[0026] The method for providing the water-repellent portion, i.e., the method for applying the water-repellent agent, is not particularly limited as long as it can form a uniform film. For example, a method for forming an aqueous emulsion of 5% by mass or more and 60% by mass or less in water can be used. The particle size of this aqueous emulsion is not particularly limited, but the average particle size is preferably 10 μm or less, and more preferably 1 μm or less. If the average particle size exceeds 10 μm, the stability of the emulsion tends to decrease. The average particle size is measured by a laser diffraction / scattering type particle size distribution measuring device, and the particle size (median particle size) at which the percentage integrated value (volume basis) is 50% is taken as the average particle size (μm).

[0027] In the configuration (third embodiment) in which a water repellent agent is applied (a water repellent part is provided) on a protective part provided on a coloring part described later, the water repellent part contains a urethane resin, so that the adhesion between the water repellent part and the protective part is increased. This is thought to be because, when the material contained in the protective part has an amino group, the amino group contained in the urethane resin forms a stable bond. The average molecular weight of the urethane resin can be 300 or more and 3000 or less.

[0028] As the urethane resin, a conventionally known material can be used. The urethane resin is obtained by reacting a polyol compound with a polyisocyanate compound, and has an isocyanate group. The urethane resin is preferably made into an aqueous emulsion and mixed with the aqueous emulsion of the water repellent. The mixing ratio at this time can be 1:10 to 10:1, and preferably 3:7 to 7:3.

[0029] (Colored part) The colored portion in this embodiment may be any portion whose color state changes when a disinfectant is applied. That is, the colored portion includes a material (which may also be called a coloring agent) whose color state changes when a disinfectant is applied. The colored portion may have a binder to improve adhesion to the substrate. A resin may be used as the binder, and for example, a urethane resin or polyvinyl alcohol may be used.

[0030] In the present embodiment, the thickness of the colored portion in the stacking direction can be 1 μm to 80 μm, 5 μm to 60 μm, or 15 μm to 50 μm. By making the thickness of the colored portion 80 μm or less, the adhesion to the substrate is improved, and by making the thickness of the colored portion 1 μm or more, the colored state of the colored portion is improved.

[0031] The colored portion in this embodiment may be laminated on at least a part of the substrate, and may be provided on the entire surface of the substrate. Examples of the colored portion provided on at least a part of the substrate include a polka dot pattern and a checkerboard pattern. In addition, the starting position and the ending position of wiping when wiping with a disinfectant may be indicated by the pattern of the colored portion. In addition, when the colored portion is provided on a rectangular substrate, the pattern may be such that the area of ​​the colored portion near the center is smaller than that of the four corners.

[0032] In this embodiment, the change in color state refers to a change that allows a visually confirmed difference in color before and after application of the disinfectant, such as a change from an invisible state to a visible state, a change from a visible state to an invisible state, or a visually recognizable color change.

[0033] Here, visually recognizable color changes include changes in color shades and color changes. A change in color shade is, for example, a change from dark red to light red or vice versa, and a color change is, for example, a change from red to blue. Visually recognizable color changes also include, for example, a change from colorless to colored or vice versa.

[0034] The colored portion may contain a combination of a plurality of materials that exhibit different color changes.

[0035] The phenomenon of changing the color state is chromism. Examples of chromism include photochromism, thermochromism, electrochromism, acidichromism, solvatochromism, and vapochromism. In the present embodiment, a substance that causes these phenomena is called a chromic substance, and can be specifically called a photochromic substance, a thermochromic substance, an electrochromic substance, an acidichromic substance, a solvatochromic substance, or a vapochromic substance.

[0036] Acidichromic substances change color with changes in pH, and the color range varies depending on the properties of each substance. For example, metanil yellow, metacresol purple, thymol blue, tropaeoline O, 2,4-dinitrophenol, methyl yellow, bromophenol blue, Congo red, methyl orange, bromochlorophenol blue, alizarin red S, bromocresol green, methyl orange-xylene cyanol FF, 2,5-dinitrophenol, methyl orange-indigo carmine, methyl red, methyl orange-xylene cyanol FF-phenolphthalein, lacmoid, chlorophenol red, o-nitrophenol, p-nitrophenol, bromocresol green-methyl red, bromocresol purple, bromophenol red, methyl red-methylene blue, bromothymol blue, neutral red, phenol red, neutral red-bromothymol blue, cresol red, α-naphtholphthalein, bromothymol blue-phenol red, curcumin, phenolphthalein, cresol red-thymol blue, o-cresolphthalein, α-naphtholbenzein, thymolphthalein, thymol blue-phenolphthalein, Alizarin Yellow GG, Alizarin Yellow R, Tropaeolin O, nitramine, 1,3,5-trinitrobenzene, indigo carmine, methyl violet, litmus, and methyl purple. From the viewpoint of low toxicity, metanil yellow, meta-cresol purple, thymol blue, bromophenol blue, bromochlorophenol blue, alizarin red S, bromocresol green, methyl red, lacmoid, chlorophenol red, o-nitrophenol, bromocresol purple, bromophenol red, bromothymol blue, neutral red, phenol red, cresol red, α-naphtholphthalein, phenolphthalein, o-cresolphthalein, thymolphthalein, alizarin yellow GG, alizarin yellow R, tropaeolin O, methyl violet, litmus, and methyl purple are preferable.More preferred are metacresol purple, thymol blue, tropeolin O, bromophenol blue, bromochlorophenol blue, alizarin red S, bromocresol green, methyl red, lacmoid, chlorophenol red, o-nitrophenol, bromocresol purple, bromophenol red, bromothymol blue, neutral red, phenol red, cresol red, α-naphtholphthalein, phenolphthalein, o-cresolphthalein, thymolphthalein, alizarin yellow GG, alizarin yellow R, litmus, and methyl purple, as they change color at a pH between 3 and 11. The substance that changes color in the alkaline pH range is at least one selected from the group consisting of p-nitrophenol, bromothymol blue, neutral red, phenol red, cresol red, phenolphthalein, cresolphthalein, thymolphthalein, alizarin yellow, troperion, and indigo carmine. It is desirable that the color change occurs when the disinfectant is alkaline and when the disinfectant is acidic.

[0037] Two or more kinds of coloring agents may be used. For example, it is preferable to use coloring agents that maintain their color for different periods of time, since this can serve as an indicator to show the time since the disinfectant came into contact with the surface.

[0038] The coloring agent may be provided to show text information, image information (figure), or both image information and text information. Although the text information and image information are not particularly limited, it is considered that if the text information and image information are displayed in a way that makes the user of the sterilization area happy, the user will be more likely to apply the sterilization agent voluntarily. The coloring agent changes color and recovers as the sterilization agent evaporates. Here, recovery means that the coloring agent returns to the state before the sterilization agent was applied. In other words, the coloring agent in this embodiment can be one that changes its coloring state for a certain period of time when the sterilization agent is applied, and then returns to the state before the sterilization agent was applied. For example, the coloring agent in a state that is invisible to the naked eye can be changed to a state that is visible to the naked eye by applying the sterilization agent, and can be made to return to the state that is invisible to the naked eye after a certain period of time has passed. In this way, the coloring agent is reversible, so that it can be used in situations where sterilization needs to be repeated.

[0039] The coloring portion is dissolved in water or a solvent that dissolves the coloring agent to form a liquid, and is applied to the substrate by various methods. Various methods can be used for the application method, such as a bar coat method, an inkjet method, a flexographic method, a screen method, an offset method, and a spin coating method. For example, the inkjet method is a method in which the marking composition in this embodiment is discharged from an inkjet recording head to record an image on a recording medium. Methods for discharging the marking composition include a method of applying mechanical energy to the marking composition and a method of applying thermal energy to the composition. Other than using the marking composition in this embodiment, the steps of the inkjet recording method can be performed by known methods.

[0040] The colored portion in this embodiment may contain a phthalein dye. Examples of the phthalein dye in this embodiment include o-cresolphthalein, thymolphthalein, and phenolphthalein.

[0041] <Base material> The substrate in this embodiment may be any substrate on which a color-developing portion is provided.

[0042] When the substrate is a resin sheet, it is preferable because it is lightweight and flexible. Examples of the resin sheet include polyester resins such as polyethylene terephthalate, polybutylene terephthalate, and polyethylene terephthalate / isophthalate copolymer; polyolefin resins such as polyethylene, polypropylene, and polymethylpentene; polyvinyl fluoride, polyvinylidene fluoride, polytetrafluoroethylene, and ethylene-tetrafluoroethylene copolymer-based polyfluorinated ethylene resins; aliphatic polyamide resins such as nylon 6 and nylon 6,6; vinyl polymer resins such as polyvinyl chloride, vinyl chloride / vinyl acetate copolymer, ethylene / vinyl acetate copolymer, ethylene / vinyl alcohol copolymer, polyvinyl alcohol, and vinylon; cellulose resins such as cellulose triacetate and cellophane; acrylic resins such as polymethyl methacrylate, polyethyl methacrylate, polyethyl acrylate, and polybutyl acrylate; other synthetic resins such as polystyrene, polycarbonate, polyarylate, and polyimide; and the like. The resin sheet may be used alone or in combination or laminated form of two or more types. It is preferable to provide a receiving layer for holding the colored portion on the substrate. This is because when the color developer is ink, the receiving layer is easily retained.

[0043] In the present embodiment, it is preferable that the receiving layer of the substrate does not react with the coloring agent. For example, in the case of a coloring agent that changes color in an alkaline state, it is preferable that the receiving layer is neutral or acidic. If the receiving layer reacts with the coloring agent, it will change color before reacting with the disinfectant, which is undesirable.

[0044] The substrate in this embodiment may be transparent or opaque, or may be colored. If the coloring agent is colored before it reacts with the disinfectant, it is preferable that the substrate be colored in a color close to that color.

[0045] In this embodiment, the substrate may be made of release paper, metal plate, wood, or the like. An adhesive may be provided to bond the substrate to another member. The adhesive may be provided on the entire surface of the substrate, or on a portion of the substrate. The adhesive is easily peeled off when it is provided on a portion of the substrate. The adhesive may be easily peeled off when it contains a UV-curable resin.

[0046] The substrate in this embodiment may also include inkjet paper having a retention layer for inkjet ink. Inkjet paper has a receiving layer provided on a material mainly composed of cellulose, and the coloring material and the like are retained in the receiving layer, while other components of the ink, such as water and a moisturizing agent, are absorbed by the cellulose at the bottom of the receiving layer. In this embodiment, too, the coloring agent contained in the coloring portion is provided on or within the receiving layer, so that when the disinfectant is applied, the moisture and the like in the disinfectant is absorbed by the cellulose of the paper. As a result, the disinfectant is quickly absorbed, and the fragility caused by the swelling of the coloring portion is suppressed, resulting in excellent durability.

[0047] The method of applying the coloring agent mentioned in the coloring section to the substrate is not particularly limited as long as a uniform film can be formed. When applying in water, it is preferable to make the coloring agent into a water-based emulsion of 5% by mass to 60% by mass in water. The particle size in the water-based emulsion is not particularly limited, but the average particle size is preferably 10 μm or less, and more preferably 1 μm or less. If the average particle size exceeds 10 μm, the stability of the emulsion tends to decrease. The average particle size is measured by a laser diffraction / scattering type particle size distribution measuring device, and the particle size (median particle size) at a percentage integrated value (volume basis) of 50% is taken as the average particle size (μm).

[0048] Second Embodiment The disinfectant visualization material according to the second embodiment of the present invention is spherical as shown in FIG. 2. In this embodiment, the spherical shape is not limited to a spherical shape having the same major axis and minor axis. The disinfectant visualization material 200 according to this embodiment has a structure in which a colored portion 202 and a water-repellent portion 203 are laminated in this order on a spherical substrate 201. In this structure, as in the first embodiment of the present invention, the presence of the water-repellent portion 203 makes it difficult for water to reach the colored portion 202. Therefore, even in a situation where exposure to water occurs frequently, the material changes color when ethanol water having a disinfecting effect is applied, and the disinfecting effect can be confirmed.

[0049] The sterilization visualization agent material according to this embodiment is spherical, which makes it possible to increase the surface area to which the sterilization agent is applied.

[0050] Third embodiment The disinfectant visualizing material 300 according to the third embodiment of the present invention has a protective part 304 between a color part 302 and a water-repellent part 303. 301 is a substrate. The protective part 304 may be provided at a position other than between the color part 302 and the water-repellent part 303. The presence of the protective part 304 makes it possible to protect the color part 302 when the disinfectant visualizing material is wiped off when the disinfectant is applied. As a result, the disinfectant visualizing material can be used for a long period of time.

[0051] (Protection Department) In this embodiment, the protective part may have a silsesquioxane structure. Here, the thickness of the protective part may be 10 nm or more and 300 nm or less in the stacking direction. Furthermore, the protective part may have a silsesquioxane structure containing at least one functional group selected from the group consisting of a vinyl group, an epoxy group, an amino group, a styryl group, a methacryl group, an acrylic group, an isocyanurate group, a ureido group, a mercapto group, and an isocyanate group. In addition, the protective part may have polyethyleneimine.

[0052] The protective part 304 may be sufficiently durable to allow the disinfectant to penetrate to the extent that the colored part changes color and to withstand repeated wiping with the disinfectant. When using a combination of a neutral disinfectant and a colored part having a color range on the alkaline side, it is preferable that the protective part contains an alkaline material.

[0053] For example, the protective part may be an organic-inorganic hybrid material such as an acrylic resin, a vinyl chloride resin, a polyamide resin, a polyester resin, a urethane resin, or a polyethyleneimine resin, or a polyphosphazene or a silsesquioxane. Among them, silsesquioxane is preferable. Silsesquioxane (hereinafter sometimes abbreviated as SQ) is a siloxane-based compound whose main chain skeleton is composed of Si-O bonds, and is represented by the composition formula [R1(SiO1.5)n]. The R1 is preferably at least one substituent selected from the group consisting of a vinyl group, an epoxy group, an amino group, a styryl group, a methacryl group, an acrylic group, an isocyanurate group, a ureido group, a mercapto group, and an isocyanate group. When silsesquioxane plays a role of binding particles composed of a large number of solid substances, it is possible to achieve a superior film strength while maintaining a high porosity. Silsesquioxane is not particularly limited in the form of polymer, and examples thereof include known linear polysiloxane, cage polysiloxane, ladder polysiloxane, etc. The silsesquioxane structure is a structure in which each silicon atom is bonded to three oxygen atoms, and each oxygen atom is bonded to two silicon atoms (the number of oxygen atoms relative to the number of silicon atoms is 1.5). From the viewpoint of cost, linear polysiloxane, cage polysiloxane, and ladder polysiloxane may be mixed.

[0054] Silane coupling agents, which are the raw material for silsesquioxane, include vinyltrimethoxysilane, vinyltriethoxysilane, 2-(3,4-epoxycyclohexyl)ethyltrimethoxysilane, 3-glycidoxypropylmethyldimethoxysilane, 3-glycidoxypropyltrimethoxysilane, 3-glycidoxypropylmethyldiethoxysilane, 3-glycidoxypropyltriethoxysilane, N-2-(aminoethyl)-3-aminopropylmethyldimethoxysilane, N-2-(aminoethyl)-3-aminopropyltrimethoxysilane, 3-aminopropyltrimethoxysilane, 3-aminopropyltriethoxysilane, Examples of the silane include p-styryltrimethoxysilane, 3-methacryloxypropylmethyldimethoxysilane, 3-methacryloxypropyltrimethoxysilane, 3-methacryloxypropylmethyldiethoxysilane, 3-methacryloxypropyltriethoxysilane, 3-acryloxypropyltrimethoxysilane, tris-(trimethoxysilylpropyl)isocyanurate, 3-ureidopropyltrialkoxysilane, 3-mercaptopropylmethyldimethoxysilane, 3-mercaptopropyltrimethoxysilane, 3-isocyanatepropyltriethoxysilane, and 3-trimethoxysilylpropylsuccinic anhydride. One or more of these may be used.

[0055] When the colored part contains O-cresolphthalein, a protective part containing 3-aminopropyltrimethoxysilane is provided, and a repellent part is provided on the protective part, so that the coloration is unlikely to occur in water with poor disinfection effect, and is likely to occur in 80% ethanol water with high disinfection effect. In addition, the water-repellent part contains urethane resin, so that the film becomes thinner and stronger. This is thought to be due to the loose interaction between the amino group of 3-aminopropyltrimethoxysilane and the amino group contained in the urethane resin. In other words, it can be said that the nitrogen atom contained in the amino group interacts with the nitrogen atom contained in the protective part, increasing the adhesion.

[0056] The above-mentioned silane coupling agent may be dissolved in a solvent to prepare a coating liquid. The solvent is preferably an organic solvent. The organic solvent is not particularly limited, but may be alcohol, carboxylic acid, aliphatic or alicyclic hydrocarbons, aromatic hydrocarbons, esters, ketones, ethers, or a mixture of two or more of these. The alcohol may be, for example, methanol, ethanol, 2-propanol, butanol, 2-methoxyethanol, 2-ethoxyethanol, 1-methoxy-2-propanol, 1-ethoxy-2-propanol, 1-propoxy-2-propanol, 4-methyl-2-pentanol, 2-ethylbutanol, 3-methoxy-3-methylbutanol, ethylene glycol, diethylene glycol, glycerin, or the like. As the carboxylic acid, specifically, n-butyric acid, α-methylbutyric acid, i-valeric acid, 2-ethylbutyric acid, 2,2-dimethylbutyric acid, 3,3-dimethylbutyric acid, 2,3-dimethylbutyric acid, 3-methylpentanoic acid, 4-methylpentanoic acid, 2-ethylpentanoic acid, 3-ethylpentanoic acid, 2,2-dimethylpentanoic acid, 3,3-dimethylpentanoic acid, 2,3-dimethylpentanoic acid, 2-ethylhexanoic acid, and 3-ethylhexanoic acid are preferably used. As the aliphatic or alicyclic hydrocarbons, specifically, n-hexane, n-octane, cyclohexane, cyclopentane, and cyclooctane are preferable. As the aromatic hydrocarbons, toluene, xylene, and ethylbenzene are preferable. As the esters, ethyl formate, ethyl acetate, n-butyl acetate, ethylene glycol monomethyl ether acetate, ethylene glycol monoethyl ether acetate, ethylene glycol monobutyl ether acetate, and γ-butyrolactone are preferable. Preferred ketones include acetone, methyl ethyl ketone, methyl isobutyl ketone, cyclohexanone, etc. Preferred ethers include dimethoxyethane, tetrahydrofuran, dioxane, diisopropyl ether, etc.

[0057] In preparing the coating solution, it is preferable to use alcohols among the above-mentioned various solvents from the viewpoint of solution stability.

[0058] The coating liquid can be prepared by adding a predetermined amount of a silane coupling agent to an organic solvent.

[0059] When forming a layer using a coating liquid, it is preferable to carry out the coating in an atmosphere of dry air or an inert gas such as dry nitrogen. The relative humidity of the dry atmosphere is preferably 30% or less.

[0060] Furthermore, as a solution coating method for forming a layer, known coating means can be appropriately adopted, such as, for example, dipping, spin coating, spraying, printing, flow coating, and combinations of these. The film thickness can be controlled by changing the pulling speed in the dipping method or the substrate rotation speed in the spin coating method, and by changing the concentration of the coating solution.

[0061] In the present embodiment, the thickness of the protective part is preferably 10 nm to 1 μm, more preferably 10 nm to 500 nm, and further preferably 10 nm to 300 nm. By setting the thickness of the protective part to 1 μm or less, a good balance between the coloring state and durability of the colored part is achieved.

[0062] (Disinfectant) The disinfectant in this embodiment is a liquid composition used for purposes such as sterilization, disinfection, sterilization, and disinfection, and changes the color state of the colored portion. As the disinfectant in this embodiment, ethanol water containing 60% to 90%, preferably 75% to 85%, of ethanol can be used. EXAMPLES

[0063] The present invention will be described in more detail below with reference to examples and comparative examples, but the present invention is not limited to the following examples as long as it does not deviate from the gist of the invention. Note that, with regard to the amounts of components, "parts" and "%" are based on mass unless otherwise specified.

[0064] <Production of disinfectant visualization material> <Example 1> As the coloring agent contained in the coloring part, 5 g of O-cresolphthalein (manufactured by Tokyo Chemical Industry Co., Ltd.) was dissolved in 95 g of ethanol and applied to glossy paper (product name: Glossy Pro PT-201, manufacturer: Canon) using a barcode of No. 20. After application, the paper was placed on a hot plate heated to 50°C for 30 minutes to dry, and then a protective part was formed on the printed matter as follows. 10 g of ethanol (manufactured by Kishida Chemical Co., Ltd.) was added to 10 g of 3-aminopropyltrimethoxysilane (manufactured by Tokyo Chemical Industry Co., Ltd.). This solution was applied using a Baker-type applicator (manufactured by Tester Sangyo Co., Ltd.) so that the thickness when dried was 150 nm. The paper was placed on a hot plate heated to 50°C for 30 minutes to dry.

[0065] After drying the protective part, a solution in which 10 g of a 10% emulsion of formula (1) (R is a linear alkyl group having 13 carbon atoms) was diluted with 90 g of water was used as the water repellent agent contained in the water repellent part. This solution was applied using a Baker-type applicator (manufactured by Tester Sangyo Co., Ltd.) so that the thickness h when dried was 120 nm, and air-dried at room temperature for 5 hours. This is referred to as membrane 1.

[0066] <Examples 2 to 10> The water repellent and the thickness h of the water repellent portion were changed as shown in Table 1, and other than that, disinfectant visualization materials (films 2 to 10) were prepared in the same manner as in Example 1, and these were designated as Examples 2 to 10. Note that n in the general formula (2) has a distribution of 24 to 33. The urethane resin was emulsified and mixed with the water repellent.

[0067] <Example 11> A disinfectant visualizing material of Example 11 was prepared according to Table 1, except that the base material of Example 1 was fine art paper (manufactured by Canon).

[0068] <Comparative Example 1> Comparative Example 1 was the same as Example 1 in which the water-repellent portion was not formed.

[0069] <Evaluation> <Evaluation (1) Discrimination between water and ethanol water> 80% ethanol water was used as the disinfectant, and pure water was used for comparison. 1 ml of the disinfectant and water were dropped onto a Kimwipe, and the disinfectant was applied to the disinfectant visualization material with the Kimwipe. The film prepared in the above example was placed on white paper and filmed with a video. The filmed video was converted to a grayscale of 0 to 255, and the absolute value of the change in value before and after application was measured. Of the evaluation criteria shown below, "A" and "B" were considered acceptable levels, and "C" was considered an unacceptable level. A: The difference between 80% ethanol and water is 30 or more. B: The difference between 80% ethanol and water is 15 to 30. C: The difference between 80% ethanol and water is less than 15%

[0070] <Evaluation (durability)> Durability was measured by applying 80% ethanol water 10 times and measuring the change in value between the 10th application and the 1st application. A: The difference between the first and tenth times is less than 15. B: The difference between the first and tenth times is 15 or more.

[0071] The results are shown in Table 1. In Table 1, "amino" represents 3-aminopropyltrimethoxysilane.

[0072] [Table 1]

[0073] As shown in Table 1, it was found that the disinfectant visualization material according to the embodiment of the present invention can distinguish between the application of water and the application of ethanol water, because the coloration state is different between the two. That is, the disinfectant visualization material according to the embodiment of the present invention can confirm that the disinfectant, ethanol water, has been applied by the change in coloration state, even in a situation where it is exposed to water.

[0074] Embodiments of the present disclosure include the following methods and compositions.

[0075] (Configuration 1) A disinfectant visualization material having a structure in which a base material, a colored portion, and a water-repellent portion are laminated in this order, wherein the colored portion changes its color state when a disinfectant is applied to the disinfectant.

[0076] (Configuration 2) 2. The disinfectant-visualizing material according to claim 1, wherein the water-repellent portion has a contact angle with water of 80 degrees or more.

[0077] (Configuration 3) 3. The disinfectant-visualizing material according to claim 1 or 2, wherein the water-repellent portion contains at least one resin selected from the group consisting of acrylic resins, acrylamide resins, and polyalkylenes.

[0078] (Configuration 4) 3. The disinfectant-visualizing material according to claim 1, wherein the water-repellent portion comprises at least one compound represented by the following formula (1) or (2):

[0079] [ka] CH3-(CH2)n-CH3Formula (2)

[0080] In the above formula (1), R is a linear or branched hydrocarbon group having 7 or more and 40 or less carbon atoms, and in the above formula (2), n is an integer of 15 or more and 40 or less.

[0081] (Configuration 5) 5. The disinfectant-visualizing material according to claim 4, wherein the compound represented by formula (1) has a molecular weight of 5,000 or more and 200,000 or less.

[0082] (Configuration 6) 3. The disinfectant-visualizing material according to configuration 1 or 2, wherein the water-repellent part contains a urethane resin.

[0083] (Configuration 7) 7. The disinfectant-visualizing material according to claim 6, wherein the urethane resin has an average molecular weight of 300 or more and 3,000 or less.

[0084] (Configuration 8) The disinfectant-visualizing material according to any one of configurations 1 to 7, wherein the disinfectant-visualizing material is in a film or a spherical shape.

[0085] (Configuration 9) 9. The disinfectant-visualizing material according to any one of configurations 1 to 8, wherein the thickness of the water-repellent portion in the stacking direction is 10 nm or more and 800 nm or less.

[0086] (Configuration 10) 10. The disinfectant-visualizing material according to any one of claims 1 to 9, further comprising a protective section between the color section and the water-repellent section.

[0087] (Configuration 11) 11. The disinfectant-visualizing material according to claim 10, wherein the protective part has a silsesquioxane structure.

[0088] (Configuration 12) 12. The disinfectant visualization material according to any one of claims 1 to 11, wherein the colored portion comprises a phthalein dye.

[0089] (Configuration 13) 13. The disinfectant visualizing material according to any one of claims 1 to 12, wherein the colored portion contains o-cresolphthalein.

[0090] (Configuration 14) 14. The disinfectant-visualizing material according to any one of claims 1 to 13, wherein the base material contains cellulose.

Claims

1. A disinfectant visualization material having a structure in which a base material, a colored portion, and a water-repellent portion are laminated in this order, wherein the colored portion changes its color state when a disinfectant is applied to the disinfectant.

2. The disinfectant-visualizing material according to claim 1 , wherein the water-repellent portion has a contact angle with water of 80 degrees or more.

3. The disinfectant-visualizing material according to claim 1 , wherein the water-repellent portion contains at least one resin selected from the group consisting of acrylic resins, acrylamide resins, and polyalkylenes.

4. The disinfectant-visualizing material according to claim 1 , wherein the water-repellent portion comprises at least one compound represented by the following formula (1) or (2): 【Chemistry 1】 CH 3 -(CH 2 )n-CH 3 Formula (2) In the above formula (1), R is a linear or branched hydrocarbon group having 7 or more and 40 or less carbon atoms, and in the above formula (2), n is an integer of 15 or more and 40 or less.

5. 5. The disinfectant-visualizing material according to claim 4, wherein the molecular weight of the compound represented by formula (1) is 5,000 or more and 200,000 or less.

6. The disinfectant-visualizing material according to claim 1 , wherein the water-repellent portion contains a urethane resin.

7. The disinfectant-visualizing material according to claim 6, wherein the urethane resin has an average molecular weight of 300 or more and 3,000 or less.

8. The disinfectant-visualizing material according to claim 1 , wherein the disinfectant-visualizing material is in the form of a film or a sphere.

9. 2. The disinfectant-visualizing material according to claim 1, wherein the water-repellent portion has a thickness in the stacking direction of 10 nm to 800 nm.

10. The disinfectant-visualizing material according to claim 1 , further comprising a protective section between the colored section and the water-repellent section.

11. The disinfectant-visualizing material according to claim 10 , wherein the protective part has a silsesquioxane structure.

12. The disinfectant visualizing material according to claim 1 , wherein the colored portion comprises a phthalein dye.

13. The disinfectant visualizing material according to claim 1 , wherein the colored portion contains o-cresolphthalein.

14. The disinfectant-visualizing material according to claim 1 , wherein the substrate comprises cellulose.

Citation Information

Patent Citations

  • Disinfectant Spray with Indicator