Water-soluble conductive copolymer, method for producing the same and aqueous solution thereof

A novel copolymer with a polythiophene structure addresses the agglomeration issues of conventional water-soluble conductive polymers by ensuring high conductivity and film homogeneity, enhancing its suitability for touch panels, capacitive sensors, and heaters.

JP2024144840APending Publication Date: 2024-10-15TOSOH CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023056983
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

Conventional water-soluble conductive polymers, such as PEDOT:PSS and self-doped polythiophenes, exhibit high conductivity but suffer from agglomeration during film formation, leading to insufficient film homogeneity and performance issues.

Method used

A novel copolymer with a polythiophene structure, characterized by specific repeating units (M1 and M2) in a ratio of (1/999) to (999/1), is synthesized through oxidative polymerization in water or an organic solvent, ensuring high conductivity and excellent film homogeneity.

Benefits of technology

The copolymer maintains high conductivity and achieves superior film homogeneity, making it suitable for applications in touch panels, capacitive sensors, and heaters with improved industrial applicability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024144840000017
    Figure 2024144840000017
  • Figure 2024144840000018
    Figure 2024144840000018
  • Figure 2024144840000001
    Figure 2024144840000001
Patent Text Reader

Abstract

To provide a novel water-soluble copolymer having high conductivity, an aqueous solution thereof and use thereof.SOLUTION: There is used a copolymer (P) containing M1 (thiophene unit) and M2 (comonomer unit), wherein M1 and M2 may be self-doped and the molar ratio, M1 / M2, is 1 to 9999. [In M1, R represents an organic group having a total carbon number of 1 to 18 having at least one substituent selected from the group consisting of a sulfonic acid group and a phosphonic acid group. M+ represents a hydrogen ion, an alkali metal ion, a conjugate acid of an amine compound or a quaternary ammonium cation. In M2, q represents an integer of 1 to 4. M represents a methyl group.]SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a novel water-soluble conductive copolymer having a polythiophene structure, a method for producing the same, and an aqueous solution thereof. [Background technology]

[0002] The application of water-soluble conductive polymers to transparent conductive film-forming materials used in touch panels, capacitance sensors, heaters, and the like is being considered.

[0003] As water-soluble conductive polymers, for example, polythiophenes substituted with branched alkylenesulfonic acid have been reported so far (see, for example, Patent Document 1). [Prior art documents] [Patent documents]

[0004] [Patent Document 1] International Publication No. 2014 / 007299 Summary of the Invention [Problem to be solved by the invention]

[0005] The transparent conductive film-forming material disclosed in Patent Document 1 described in the Background Art is a homogeneous aqueous solution that is highly conductive and has excellent coatability and film-forming properties compared to PEDOT:PSS and the like, which are known as dispersions. However, there remains a problem in that the homogeneity of the film is insufficient.

[0006] The present invention has been made in view of the above-mentioned background art, and an object of the present invention is to provide a novel thiophene copolymer and an aqueous solution thereof, which exhibit high electrical conductivity and excellent film uniformity when a coating film is formed. [Means for solving the problem]

[0007] As a result of intensive research aimed at solving the above problems, the present inventors have found that the invention described below can solve the above problems, and have completed the present invention.

[0008] [1] A copolymer (P) comprising at least one repeating unit (M1) represented by the following general formula (M1) and at least one repeating unit (M2) represented by the following general formula (M2), wherein the repeating unit (M1) and the repeating unit (M2) may each be independently self-doped, and the ratio of the repeating unit (M1) / the repeating unit (M2) (mol / mol) is from (1 / 999) to (999 / 1).

[0009] [ka]

[0010] In general formula (M1), R represents an organic group having a total of 1 to 18 carbon atoms and having at least one substituent selected from the group consisting of a sulfonic acid group and a phosphonic acid group. + represents a hydrogen ion, an alkali metal ion, a conjugate acid of an amine compound, or a quaternary ammonium cation. In the general formula (M2), q represents an integer of 1 to 4. Me represents a methyl group.] [2] The copolymer (P) according to the above item [1], wherein the ratio of repeating units (M1) / repeating units (M2) (mol / mol) is from (1 / 9) to (999 / 1).

[0011] [3] The copolymer (P) according to the above [1] or [2], wherein the repeating unit (M1) is a repeating unit (M3) represented by the following general formula (M3):

[0012] [ka]

[0013] [In general formula (M3), R 1represents a hydrogen atom, a methyl group, an ethyl group, a linear or branched alkyl group having 3 to 6 carbon atoms, or a fluorine atom; m independently represents an integer of 1 to 10; and n independently represents 0 or 1. M + represents M in general formula (M1). + is equivalent to.] [4] A method for producing the copolymer (P) according to any one of the above [1] to [3], characterized in that a thiophene compound represented by the following general formula (1) and a thiophene compound represented by the following general formula (2) are copolymerized in water or an organic solvent by an oxidation reaction.

[0014] [ka]

[0015] [R and M in the above general formula (1)] + respectively represent R and M in general formula (M1). + and q in the above general formula (2) is the same as q in the general formula (M2). Me represents a methyl group. [5] The method for producing the copolymer (P) according to the above item [4], wherein the thiophene compound represented by the general formula (1) is a thiophene compound represented by the following general formula (3):

[0016] [ka]

[0017] [R in general formula (3)] 1 , m, n and M + are R in general formula (M3), 1 , m, n, and M in general formula (M1) + is equivalent to.] [6] An aqueous solution containing the copolymer (P) according to any one of [1] to [3] above. Effect of the Invention

[0018] The copolymer (P) having a polythiophene structure according to the present invention has excellent film uniformity compared to conventional water-soluble conductive polymers while maintaining high electrical conductivity, and is therefore suitable for use as a transparent conductive film forming material for use in touch panels, capacitive sensors and heaters, and is extremely useful industrially. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] The present invention will be described in detail below.

[0020] One aspect of the present invention relates to the following copolymer (P):

[0021] As a transparent conductive film forming material, the application of PEDOT:PSS, a conductive polythiophene obtained by polymerizing 3,4-ethylenedioxythiophene (EDOT) in the presence of a water-soluble polymer dopant such as polystyrene sulfonate (PSS), has been considered. However, although PEDOT:PSS exhibits high conductivity, it is prone to aggregation because it is a dispersion solution with particle sizes of tens to hundreds of nm. Therefore, there was a problem that aggregation occurs during thin film formation, resulting in insufficient performance in terms of conductivity, film formability, etc.

[0022] On the other hand, conventionally known self-doped polythiophenes (e.g., PEDT-S, or polythiophenes substituted with branched alkylene sulfonic acid), which are different from the externally doped PEDOT:PSS described above, are highly conductive and form a homogeneous solution with a particle size of 0.8 nm or less. Although they have superior coating properties and film-forming properties compared to PEDOT:PSS, there is still the problem that the film uniformity is insufficient.

[0023] The copolymer (P) according to the present invention has been made in view of the above-mentioned background art, and an object of the present invention is to provide a novel thiophene copolymer and an aqueous solution thereof, which exhibit high electrical conductivity and excellent film uniformity when a coating film is formed.

[0024] The copolymer (P) of the present application comprises at least one repeating unit (M1) represented by the following general formula (M1) and at least one repeating unit (M2) represented by the following general formula (M2), and the repeating unit (M1) and the repeating unit (M2) may each be independently self-doped, and the ratio of the repeating unit (M1) / repeating unit (M2) (mol / mol) is (1 / 999) to (999 / 1).

[0025] [ka]

[0026] In general formula (M1), R represents an organic group having a total of 1 to 18 carbon atoms and having at least one substituent selected from the group consisting of a sulfonic acid group and a phosphonic acid group. + represents a hydrogen ion, an alkali metal ion, a conjugate acid of an amine compound, or a quaternary ammonium cation. In the general formula (M2), q represents an integer of 1 to 4. Me represents a methyl group.] In the above general formula (M1), R represents an organic group having a total of 1 to 18 carbon atoms and having at least one substituent selected from the group consisting of a sulfonic acid group and a phosphonic acid group.

[0027] The organic group having a total of 1 to 18 carbon atoms in a state that does not have at least one substituent selected from the group consisting of a sulfonic acid group and a phosphonic acid group is not particularly limited, and examples thereof include a methyl group, an ethyl group, a propyl group, an isopropyl group, a butyl group, an isobutyl group, a tert-butyl group, a hexyl group, an isohexyl group, a heptyl group, an octyl group, a 2-ethylhexyl group, a nonyl group, a decyl group, a methoxymethyl group, an ethoxymethyl group, a propoxymethyl group, an isopropoxymethyl group, a butoxymethyl group, an isobutoxymethyl group, a tert-butoxymethyl group, a hexyloxymethyl group, an isohexyloxymethyl group, a heptyloxymethyl group, and an octyloxymethyl group.

[0028] In the above general formula (M1), the organic group having a total of 1 to 18 carbon atoms and having at least one substituent selected from the group consisting of a sulfonic acid group and a phosphonic acid group is not particularly limited, and examples thereof include a methyl sulfonate group, a methyl phosphonate group, a 2-ethyl sulfonate group, a 2-ethyl phosphonate group, a 3-propyl sulfonate group, a 3-propyl phosphonate group, a 2-propyl sulfonate group, a 2-propyl phosphonate group, a 4-butyl sulfonate group, a 4-butyl phosphonate group, a 3-butyl sulfonate group, a 3-butyl phosphonate group, a 6-hexyl sulfonate group, a 6-hexyl phosphonate group, a 5-hexyl sulfonate group, a 5-hexyl phosphonate ... Examples of such an acid include a hexyl group, a methoxymethyl sulfonate group, a methoxymethyl phosphonate group, a 2-ethoxymethyl sulfonate group, a 2-ethoxymethyl phosphonate group, a 3-propoxymethyl sulfonate group, a 3-propoxymethyl phosphonate group, a 2-propoxymethyl sulfonate group, a 2-propoxymethyl phosphonate group, a 4-butoxymethyl sulfonate group, a 4-butoxymethyl phosphonate group, a 3-butoxymethyl sulfonate group, a 3-butoxymethyl phosphonate group, a 6-hexyloxymethyl sulfonate group, a 6-hexyloxymethyl phosphonate group, a 5-hexyloxymethyl sulfonate group, and a 5-hexyloxymethyl phosphonate group.

[0029] In general formula (M1), M + represents a hydrogen ion, an alkali metal ion, a conjugate acid of an amine compound, or a quaternary ammonium cation.

[0030] The alkali metal ion may, for example, be a lithium ion, a sodium ion, a potassium ion, or a cesium ion.

[0031] The conjugate acid of the amine compound refers to a cationic species formed by addition of a hydron (H+) to the amine compound.

[0032] The amine compound may be any amine compound that reacts with a sulfonic acid group or a phosphonic acid group to form a conjugate acid, and may be an N(R 2)3 [As a conjugate acid, [NH(R 2 )3] + or pyridine compounds or imidazole compounds having an sp2 hybrid orbital.

[0033] Substituent R 2 each independently represents a hydrogen atom, an alkyl group having 1 to 18 carbon atoms, or an alkyl group having a substituent and a total of 1 to 18 carbon atoms.

[0034] The alkyl group having 1 to 18 carbon atoms is not particularly limited, and examples thereof include a methyl group, an ethyl group, an n-propyl group, an isopropyl group, an n-butyl group, an isobutyl group, a sec-butyl group, a tert-butyl group, an n-pentyl group, an isopentyl group, a neopentyl group, a tert-pentyl group, a cyclopentyl group, an n-hexyl group, a 2-ethylbutyl group, a cyclohexyl group, an octyl group, a 2-ethylhexyl group, a nonyl group, a decyl group, a dodecyl group, a tetradecyl group, a hexadecyl group, and an octadecyl group.

[0035] Examples of the substituted alkyl group having a total of 1 to 18 carbon atoms include a halogen atom, an alkyl group having 1 to 18 carbon atoms, an amino group, or an alkyl group having 1 to 18 carbon atoms and a hydroxyl group. Specific examples include a trifluoromethyl group, a 2-hydroxyethyl group, and the like.

[0036] Among these, the substituent R 2 are preferably independently a hydrogen atom, a methyl group, an ethyl group, a propyl group, an isopropyl group, a butyl group, a hexyl group, an octyl group, a 2-ethylhexyl group, or a 2-hydroxyethyl group.

[0037] N(R) forms the conjugate acid of an amine compound 2Examples of the amine compound represented by formula (3) include ammonia, methylamine, dimethylamine, trimethylamine, ethylamine, diethylamine, triethylamine, normal-propylamine, isopropylamine, normal-butylamine, tertiary butylamine, dibutylamine, tributylamine, hexylamine, dihexylamine, trihexylamine, octylamine, dioctylamine, trioctylamine, ethanolamine compounds (e.g., aminoethanol, dimethylaminoethanol, methylaminoethanol, diethanolamine, N-methyldiethanolamine, triethanolamine), 3-amino-1,2-propanediol, 3-methylamino-1,2-propanediol, 3-dimethylamino-1,2-propanediol, N-isopropyl-N,N-dimethylamine, and N-ethyl-N,N-dimethylamine.

[0038] N(R 2 Examples of compounds other than the amine compounds represented by formula 3 include imidazole compounds (eg, imidazole, N-methylimidazole, 1,2-dimethylimidazole), pyridine, picoline, lutidine, and the like.

[0039] The above-mentioned quaternary ammonium cation refers to a cationic species formed by introducing four substituents into the nitrogen atom.

[0040] The quaternary ammonium cation may be any quaternary ammonium cation that forms an ion pair with the anion of a sulfonic acid group or a phosphonic acid group, and may be, for example, a quaternary ammonium cation having an sp3 hybrid orbital [N(R 3 )4] + Examples of the cation include an ammonium cation represented by the following formula:

[0041] Substituent R 3 each independently represents an alkyl group having 1 to 18 carbon atoms, or an alkyl group having a substituent and a total of 1 to 18 carbon atoms.

[0042] The alkyl group having 1 to 18 carbon atoms is not particularly limited, and examples thereof include a methyl group, an ethyl group, an n-propyl group, an isopropyl group, an n-butyl group, an isobutyl group, a sec-butyl group, a tert-butyl group, an n-pentyl group, an isopentyl group, a neopentyl group, a tert-pentyl group, a cyclopentyl group, an n-hexyl group, a 2-ethylbutyl group, a cyclohexyl group, an octyl group, a 2-ethylhexyl group, a nonyl group, a decyl group, a dodecyl group, a tetradecyl group, a hexadecyl group, and an octadecyl group.

[0043] Examples of the substituted alkyl group having a total of 1 to 18 carbon atoms include a halogen atom, an alkyl group having 1 to 18 carbon atoms, an amino group, or an alkyl group having 1 to 18 carbon atoms and a hydroxyl group. Specific examples include a trifluoromethyl group, a 2-hydroxyethyl group, and the like.

[0044] Among these, the substituent R 3 are preferably, independently, a methyl group, an ethyl group, a propyl group, an isopropyl group, a butyl group, a hexyl group, an octyl group, a 2-ethylhexyl group, a decyl group, a dodecyl group, or a 2-hydroxyethyl group.

[0045] [N(R 3 )4] + Examples of the quaternary ammonium cation represented by the formula (I) include tetramethylammonium, tetraethylammonium, tetrapropylammonium, tetrabutylammonium, tetraoctylammonium, trimethylpropylammonium, trimethylbutylammonium, trimethyloctylammonium, trimethyldecylammonium, trimethyldodecylammonium, trimethyltetradecylammonium, and trimethyloctadecylammonium.

[0046] The sulfonic acid group or phosphonic acid group in R of general formula (M1) forms an ion pair with the above-mentioned M+.

[0047] That is, in the general formula (M1), the sulfonic acid group or phosphonic acid group may be in an acid form or in a neutralized salt form having an alkali metal ion, a conjugate acid of an amine compound, or a quaternary ammonium cation as a counter cation.

[0048] In the above general formula (M2), q represents an integer of 1 to 4.

[0049] The copolymer (P) of the present invention is characterized in that the ratio of repeating units (M1) / repeating units (M2) (mol / mol) is from (1 / 999) to (999 / 1).

[0050] When the ratio of repeating unit (M1) / repeating unit (M2) (mol / mol) is greater than (1 / 999), the copolymer (P) tends to have improved water solubility, which is preferable in that the effects of the invention specific to the present application are easily achieved. On the other hand, when the ratio of repeating unit (M1) / repeating unit (M2) (mol / mol) is less than (999 / 1), the coatability tends to be improved, which is preferable in that the effects of the invention specific to the present application are easily achieved.

[0051] From the viewpoint of water solubility and coatability of the copolymer (P), the ratio of repeating units (M1) / repeating units (M2) (mol / mol) is preferably from (1 / 99) to (999 / 1), and more preferably from (2 / 1) to (99 / 1).

[0052] In the copolymer (P) of the present application, q represents an integer of 1 to 4. From the viewpoint of the water solubility and coatability of the copolymer (P), q is preferably 2, 3, or 4, and more preferably 3.

[0053] Regarding the repeating unit (M1), in terms of obtaining a highly homogeneous film, it is preferable that the repeating unit (M3) represented by the following general formula (M3) or the repeating unit (M4) represented by the following general formula (M4) is used, and it is more preferable that the repeating unit (M3) is used.

[0054] [ka]

[0055] [In general formula (M3), R 1 represents a hydrogen atom, a methyl group, an ethyl group, a linear or branched alkyl group having 3 to 6 carbon atoms, or a fluorine atom, m independently represents an integer of 1 to 10, and n independently represents 0 or 1. In formulae (M3) and (M4), M + represents M in general formula (M1). + is equivalent to.] The linear or branched alkyl group having 3 to 6 carbon atoms is not particularly limited, but examples thereof include a propyl group, an isopropyl group, a butyl group, an isobutyl group, a pentyl group, a hexyl group, and a cyclohexyl group.

[0056] The above R 1 From the viewpoint of the water solubility and coatability of the copolymer (P), is preferably a hydrogen atom, a methyl group, an ethyl group, or a fluorine atom, and more preferably a hydrogen atom or a methyl group.

[0057] The above-mentioned m is preferably 2, 3, 4, 5 or 6, and more preferably 2 or 3, from the viewpoint of the water solubility and coatability of the copolymer (P).

[0058] The above n is preferably 1 from the viewpoint of the water solubility and coatability of the copolymer (P).

[0059] In the general formulae (M3) and (M4), M + represents M in general formula (M1). + is synonymous with.

[0060] The sulfonic acid group in the general formula (M3) or the phosphonic acid group in the general formula (M4) is as described above in M + It forms an ion pair with

[0061] That is, the sulfonic acid group in general formula (M3) and the phosphonic acid group in general formula (M4) may be in an acid form or in a neutralized salt form having an alkali metal ion, a conjugate acid of an amine compound, or a quaternary ammonium cation as a counter cation.

[0062] The weight average molecular weight of the copolymer (P) of the present invention is not particularly limited, but is preferably in the range of 1,000 to 1,000,000 in terms of polystyrene sulfonic acid in order to obtain a highly homogeneous membrane, and is preferably in the range of 1,000 to 200,000 for use as a water-soluble conductive polymer. From the viewpoint of removing unreacted monomers, low molecular weight impurities, and inorganic salts from the polymer, it is more preferably in the range of 1.5,000 to 100,000.

[0063] The weight average molecular weight is measured by size exclusion liquid chromatography. More specifically, the copolymer (P) of the present invention is a self-doped conductive copolymer in which a sulfonic acid group or a phosphonic acid group in a side chain of the thiophene compound represented by the above general formula (M1) acts as a p-type dopant, and can be represented, for example, by the following general formula (5).

[0064] [ka]

[0065] [In the general formula (5), R and M in the general formula (A) and the general formula (B) + represents R and M in general formula (M1). + In the general formulas (C) and (D), q is the same as q in the general formula (M2). m and n each represent the abundance ratio of the repeating units and are real numbers satisfying (1 / 999)≦m / n≦(999 / 1). In the above general formula (5), the above general formula (C) is derived from the above general formula (2M), the above general formula (D) represents the state in which the above general formula (C) is oxidized by the action of a p-type dopant due to the sulfonic acid group or phosphonic acid group in the side chain of the above general formula (1M), the above general formula (A) is derived from the above general formula (1M), and the above general formula (B) represents the state in which the above general formula (A) is oxidized by the action of a p-type dopant due to the sulfonic acid group or phosphonic acid group in the side chain of the above general formula (1M).

[0066] That is, the above general formula (5) represents a copolymer (P) containing a repeating unit represented by the above general formula (A) or general formula (B) (so-called thiophene monomer unit) and a repeating unit represented by the general formula (C) or general formula (D) (so-called comonomer unit), and is not necessarily limited to a copolymer containing these units consecutively, and may be a copolymer containing discontinuous repeating units in a π-conjugated main chain, such as a random copolymer, so long as it has the desired electrical conductivity.

[0067] The copolymer (P) of the present application can be produced by copolymerizing a thiophene compound represented by the following general formula (1) and a thiophene compound represented by the following general formula (2) in water or an organic solvent by an oxidation reaction.

[0068] [ka]

[0069] [R and M in the above general formula (1)] + R and M in general formula (M1) + and q in the above general formula (2) is the same as q in the general formula (M2). Me represents a methyl group. Hereinafter, a thiophene compound represented by the following general formula (1) will be referred to as a "thiophene monomer", and a thiophene compound represented by the following general formula (2) will be referred to as a "comonomer".

[0070] In the thiophene monomer used for copolymerization, the sulfonic acid group or phosphonic acid group may be in an acid form or in a neutralized salt form having an alkali metal ion, a conjugate acid of an amine, or a quaternary ammonium cation as a counter cation.

[0071] In the method for producing the copolymer (P) of the present invention, the mixing ratio of the thiophene compounds represented by the general formulas (1) and (2) is not particularly limited. However, in terms of obtaining a highly homogeneous film, the ratio of the thiophene monomer / the comonomer (mol / mol) is preferably from (1 / 999) to (999 / 1), and more preferably from (1 / 9) to (999 / 1).

[0072] Specific examples of the thiophene compound represented by the above general formula (1) include sodium 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-methyl-1-propanesulfonate, sodium 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-ethyl-1-propanesulfonate, sodium 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-propyl-1-propanesulfonate, sodium 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-propyl-1-propanesulfonate, -[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-butyl-1-propanesulfonic acid sodium salt, 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-pentyl-1-propanesulfonic acid sodium salt, 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-hexyl-1-propanesulfonic acid sodium salt, 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-hexyl-1-propanesulfonic acid sodium salt, -2-yl)methoxy]-1-isopropyl-1-propanesulfonic acid sodium salt, 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-isobutyl-1-propanesulfonic acid sodium salt, 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-isopentyl-1-propanesulfonic acid sodium salt, 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-fluoro-1-propanesulfonic acid sodium salt Sodium sulfonate, potassium 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-methyl-1-propanesulfonate, 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-methyl-1-propanesulfonic acid, ammonium 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-methyl-1-propanesulfonate, or ammonium 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-methyl-1-propanesulfonic acid triethylammonium, etc.

[0073] The thiophene compound represented by the above general formula (1) can be easily synthesized from thieno[3,4-b]-1,4-dioxin-2-methanol and a sultone compound according to a known method (for example, the method described in WO 2014 / 007299).

[0074] The thiophene compound represented by the above general formula (2) can be synthesized according to a known method (for example, the method described in JP 2017-171746 A).

[0075] From the viewpoints of water solubility and coatability of the copolymer (P), the thiophene compound represented by the above general formula (1) is preferably a thiophene compound represented by the following general formula (3) or a thiophene compound represented by the following general formula (4), and more preferably a thiophene compound represented by the following general formula (3).

[0076] [ka]

[0077] [R in general formula (3)] 1 , m, and n are R in general formula (M3). 1 , m, and n are synonymous with each other. + is M in general formula (M1). + is equivalent to.] Regarding the sulfonic acid group in the general formula (3) or the phosphonic acid group in the general formula (4), + It forms an ion pair with

[0078] That is, the sulfonic acid group in general formula (3) and the phosphonic acid group in general formula (4) may be in an acid form or in a neutralized salt form having an alkali metal ion, a conjugate acid of an amine compound, or a quaternary ammonium cation as a counter cation.

[0079] The solvent used in the copolymerization is water or an organic solvent. Examples of water include pure water, and may be distilled water or ion-exchanged water. Examples of organic solvents include organic solvents such as dimethyl sulfoxide, dimethylacetamide, or chloroform. These organic solvents may be used alone or in combination with water. Of these solvents, water or dimethyl sulfoxide is preferred, and water is more preferred. The solvent may be degassed or substituted with an inert gas such as nitrogen.

[0080] The amount of the solvent used in the copolymerization is not particularly limited, but is preferably in the range of 0.1 to 100 times by mass, and more preferably in the range of 1 to 20 times by mass, based on the total charged mass of the thiophene compound represented by the general formula (1) and the thiophene compound represented by the general formula (2).

[0081] The copolymerization reaction is an oxidation reaction that proceeds by oxidative polymerization through an oxidative dehydrogenation reaction, and is not particularly limited, but may be, for example, an oxidation reaction using an oxidizing agent such as persulfates, iron salts (III), hydrogen peroxide, permanganates, dichromates, cerium sulfate (IV), or oxygen, which may be used alone or in combination of two or more. Another example is oxidation by electrolysis, which may be used alone or in combination of two or more.

[0082] Specific examples of persulfates include persulfuric acid, ammonium persulfate, sodium persulfate, and potassium persulfate.

[0083] Specific examples of iron salts (III) include FeCl3, Fe2(SO4)3, iron perchlorate, and iron (III) para-toluenesulfonate. Either anhydride or hydrate may be used.

[0084] Specific examples of permanganate include sodium permanganate, potassium permanganate, and magnesium permanganate.

[0085] Specific examples of dichromates include ammonium dichromate and potassium dichromate.

[0086] Of these oxidizing agents, FeCl3, Fe2(SO4)3, or persulfates are particularly preferred.

[0087] The amount of the oxidizing agent used in the copolymerization is not particularly limited, but is preferably 0.5 to 50 times by mole, more preferably 1 to 20 times by mole, and even more preferably 1 to 10 times by mole, based on the total number of moles of the thiophene monomer and the comonomer charged.

[0088] In the copolymerization, an iron salt or a copper salt may be present as a catalyst for promoting the oxidative dehydrogenation reaction by an oxidizing agent. Although not particularly limited, examples of the catalyst include FeCl2, FeCl3, FeSO4, Fe2(SO4)3, CuCl, CuCl2, and CuSO4. Among these salts, trivalent iron salts may also function as an oxidizing agent. The salts of these catalysts may be anhydrous or hydrated.

[0089] The pH condition of the copolymerization in the previous stage is, for example, a pH at which the thiophene compounds represented by the above general formulas (1) and (2) can be oxidatively polymerized, and is not particularly limited, but is preferably less than pH 7.0 because a faster reaction rate can be obtained. If necessary, a method for lowering the pH may be taken, and is not particularly limited, but examples thereof include a method of adding an acid such as sulfuric acid, para-toluenesulfonic acid, methanesulfonic acid, hydrochloric acid, nitric acid, or acetic acid.

[0090] The pressure for the copolymerization may be any of normal pressure, reduced pressure, and increased pressure.

[0091] The reaction atmosphere for the copolymerization may be air or an inert gas such as nitrogen or argon, and is more preferably an inert gas.

[0092] The reaction temperature of the copolymerization is, for example, a temperature at which the thiophene compounds represented by the above general formulas (1) and (2) can be oxidatively polymerized, and is not particularly limited, but is preferably in the range of -10 to 150°C, more preferably in the range of 0 to 100°C.

[0093] The reaction time of the copolymerization is, for example, a time during which the oxidative polymerization of the thiophene compound represented by the general formula (1) and the thiophene compound represented by the general formula (2) proceeds sufficiently, and is not particularly limited, but is preferably in the range of 0.5 to 200 hours, and more preferably in the range of 0.5 to 80 hours.

[0094] The reaction method of the copolymerization is not particularly limited, but for example, the thiophene compound represented by the above general formula (1) and the thiophene compound represented by the above general formula (2) may be dissolved in water in advance, and the oxidizing agent may be added dropwise to the solution all at once or slowly, or conversely, the thiophene compound represented by the above general formula (1) and the aqueous solution of the thiophene compound represented by the above general formula (2) may be added dropwise to a solid or aqueous solution of the oxidizing agent all at once or slowly. When two or more kinds of oxidizing agents are used, the oxidizing agents may be added sequentially.

[0095] The method for purifying the copolymer (P) of the present invention obtained by the above-mentioned copolymerization is not particularly limited, and examples thereof include solvent washing, reprecipitation, centrifugal sedimentation, ultrafiltration, dialysis, ion exchange resin treatment, etc. Each of these methods may be performed alone or in combination.

[0096] A typical method for isolating and purifying the copolymer (P) of the present invention is, for example, as follows.

[0097] First, the solution after the copolymerization reaction is added to a poor solvent such as acetone to precipitate the copolymer (P), and the copolymer (P) obtained by filtration under reduced pressure is washed with the poor solvent until the filtrate becomes colorless and transparent. If the copolymer (P) contains an Fe salt, it is preferable to add it once to an aqueous sodium hydroxide solution, dissolve it in water, and convert it into a Na salt type copolymer (P) in which the counter cation is a Na ion.

[0098] Next, the copolymer (P) is precipitated by adding the mixture to a poor solvent such as alcohol, and the alkali is removed. The solid obtained by filtration under reduced pressure is washed with a poor solvent such as alcohol, and then washed with a poor solvent such as acetone to obtain the Na salt type copolymer (P).

[0099] When the obtained Na salt type copolymer (P) is subsequently converted into H type copolymer (P) in which the counter cation is a hydrogen ion, it is treated with a cation exchange resin. Examples of the treatment method include a method in which an aqueous solution of the obtained Na salt type copolymer (P) is passed through a column packed with a cation exchange resin, and a body feed method in which a cation exchange resin is added to an aqueous solution. Furthermore, an anion exchange treatment may be performed to remove a trace amount of anions.

[0100] The solution thus obtained is roughly concentrated, and then added to a poor solvent such as acetone to cause precipitation. The solid obtained by filtration under reduced pressure is thoroughly washed with a poor solvent and dried under reduced pressure to obtain the H-type copolymer (P).

[0101] In each step of the post-polymerization treatment, centrifugation and homogenization may be performed as necessary. This can improve filtration efficiency. Furthermore, when a persulfate salt is used as the polymerization oxidizing agent, ultrafiltration, dialysis, and cation-anion exchange resin mixing treatment are performed to remove inorganic salts.

[0102] By preparing an aqueous conductive polymer solution containing the copolymer (P) of the present invention, molding and processing for various applications becomes possible.

[0103] The conductive polymer aqueous solution containing the copolymer (P) can be produced by mixing and dissolving the copolymer (P) in water at room temperature or under heating (preferably 100°C or less), although there is no particular limitation thereon. In this case, a general mixing and dissolving operation using a stirrer tip or stirring blade can be used, and as another method, ultrasonic irradiation or homogenization treatment (for example, the use of a mechanical homogenizer, ultrasonic homogenizer, or high-pressure homogenizer, etc.) may be performed. When homogenization treatment is performed, it is preferable to perform it while cooling or heating in order to prevent thermal deterioration of the polymer.

[0104] The concentration of the copolymer (P) in the aqueous conductive polymer solution is not particularly limited, but is usually 50% by mass or less, preferably 20% by mass or less, and more preferably 10% by mass or less from the viewpoint of viscosity, based on 100% by mass of the entire aqueous conductive polymer solution.

[0105] The aqueous conductive polymer solution may contain generally known additives such as a binder and a surfactant.

[0106] A conductive coating can be produced using the conductive polymer aqueous solution. For example, a conductive coating can be easily obtained by applying the conductive polymer aqueous solution to a substrate and drying it. Examples of the substrate include glass, plastic, polyester, polyacrylate, polycarbonate, a resist substrate, and aluminum. Examples of the application method include a casting method, a dipping method, a bar code method, a roll coating method, a gravure coating method, a flexographic printing method, a spray coating method, and an inkjet printing method. There is no particular limitation on the film thickness, but it is preferable that the film thickness is 10 -2 ~10 2 The surface resistance of the resulting coating film is not particularly limited, but is preferably in the range of 1 to 10 9 Those in the Ω / □ range are preferred.

[0107] In the present invention, the term "water solubility sufficient for molding and processing for various applications" refers to a particle size distribution (D) measured by a particle size distribution analyzer in a 10% by mass or less aqueous polymer solution prepared at room temperature or under heating. 50 ) is 5 nm or less and has a water solubility sufficient to pass through a 0.02 μm filter.

[0108] In the present invention, good electrical conductivity means that the electrical conductivity (electrical conductivity) in a film state is 50 S / cm or more. [Brief description of the drawings]

[0109] [Figure 1] 1 shows an optical microscope photograph of the conductive polymer film produced in Example 1. [Diagram 2] 1 shows an optical microscope photograph of the conductive polymer film produced in Comparative Example 1. EXAMPLES

[0110] Examples of the copolymer (P) of the present invention are shown below, but the present invention is not limited to these examples. Analytical instruments and measurement methods used in the examples are listed below. [Surface resistivity measurement] Equipment: Mitsubishi Chemical Loresta GP MCP-T600 [Film thickness measurement] Equipment: BRUKER DEKTAK XT [Particle size measurement] Equipment: Nikkiso Microtrac Nanotrac UPA-UT151 [NMR measurement] Equipment: JEOL JNM-ECZ400SVXR-300S [Viscosity measurement] Tuning fork vibration viscometer: A&D SV-1A [Conductivity measurement] 0.5 mL of the conductive polymer aqueous solution described below was applied to a 30 mm square non-alkali glass plate, dried overnight at room temperature, and then heated on a hot plate at 150° C. for 60 minutes to obtain a conductive polymer film. The film thickness and surface resistance were calculated based on the following formula.

[0111] Conductivity [S / cm]=10 4 / (Surface resistivity [Ω / □]×film thickness [μm]) If the surface resistance value was stable and the conductive polymer film formed was smooth, the coating property was judged to be good. Synthesis Example 1 (Synthesis of 2-(2-(2-((2,3-dihydrothieno[3,4-b][1,4]dioxin-2-yl)methoxy)ethoxy)ethoxy)ethanol methyl ether (hereinafter abbreviated as TEG3OMe) [see formula (6) below]) In a 200mL three-neck flask, 5.0g (30.5mmol) of 2-(2-(2-methoxyethoxy)ethoxy)ethan-1-ol, 8.71g (45.6mmol) of 4-methylbenzenesulfonyl chloride, and 100mL of tetrahydrofuran were added, and then 3.61g (45.7mmol) of pyridine was added dropwise at room temperature under a nitrogen stream, and 3.66g of a 10% by mass aqueous solution of NaOH was further added, and the reaction solution was refluxed overnight. After cooling, the reaction solution was concentrated, 100mL of water was added, and then extracted with 300mL of toluene. The obtained organic layer was washed with 100mL of a 1M aqueous hydrochloric acid solution, and then dehydrated using sodium sulfate. The organic layer thus obtained was concentrated to obtain a crude product. This crude product was purified by silica gel column chromatography (eluent: toluene / ethanol=20:1 (v / v)) to obtain 7.86 g of intermediate A as a brown oil (yield 81%).

[0112] Next, in a nitrogen atmosphere, 1.69g (21.1mmol) of 60% sodium hydride and 20mL of tetrahydrofuran were charged into a 300mL separable flask, and then 4.00g (23.2mmol) of (2,3-dihydrothieno[3,4-b][1,4]dioxin-2-yl)methanol [abbreviated as HMEDOT] dissolved in 80mL of tetrahydrofuran was added over 40 minutes while stirring at room temperature. Then, the mixture was kept at room temperature for 60 minutes. 6.72g (21.1mmol) of intermediate A was dissolved in 100mL of dimethylformamide and dried using 8g of molecular sieves 4A to prepare a solution, which was added dropwise to the above reaction solution over 30 minutes. After that, the reaction solution was aged at room temperature overnight, and then 3mL of water was added dropwise and mixed to quench the reaction. After the solvent was distilled off, 100 mL of water and 100 mL of heptane were added and the mixture was separated. The aqueous layer was washed with 100 mL of heptane, and the resulting organic layers were combined and dried over sodium sulfate. The solvent was distilled off to obtain a crude product. This crude product was purified using a silica gel column (eluent: toluene / ethyl acetate = 10:1 to 1:1 (v / v)) to obtain 3.05 g (9.58 mmol) of 3TEGOMe (corresponding to the above comonomer) as a pale yellow oily substance in a yield of 45%. 1 H-NMR confirmed that the compound was TEG3OMe.

[0113] It was found that TEG3OMe dissolves in an amount of 0.5 parts by mass or more in 100 parts by mass of water at 30° C. or less. 1 H-NMR (400MHz, CDCl3)δ3.37 (s, 3H), 3.53-3.56 (m, 2H), 3.63-3.69 (m,11H), 3.75-3.79 (m, 1H), 4.06 (dd,J=11.7,7.5Hz, 1H), 4.25 (dd,J=11.9,2.3Hz, 1H), 4.30-4.35 (m, 1H), 6.31-6.33 (m, 2H)

[0114] [ka]

[0115] Example 1 Synthesis of H-type copolymer (P) [see formula (7) below] 6.48g (18.8mmol) of sodium 3-[(2,3-dihydrothieno[3,4,-b]-[1,4]dioxin-2-yl)methoxy]-1-methyl-1-propanesulfonate synthesized by the method described in International Publication No. 2014 / 007299, 2.00g (6.28mmol) of TEG3OMe described above, and 451g of water were added to a 1000mL round-bottom flask equipped with a mechanical stirrer, and then stirred under a nitrogen atmosphere to dissolve everything. To this solution, a solution of 2.56g (15.8mmol) of iron(III) chloride dissolved in 50.9g of water was added. The mixture was then cooled to 10°C. After cooling was completed, a solution of 14.5g (60.8mmol) of sodium persulfate dissolved in 46.6g of water was added dropwise over 1 hour. After the dropwise addition, the temperature was raised to 20° C. over 30 minutes, and after maintaining the temperature for 3 hours, the mixture was diluted with pure water to obtain a polymerization liquid with a concentration of 1% by mass.

[0116] Next, the polymer aqueous solution was poured into 2000 mL of Amberlite IRA96SB (manufactured by Organo) at a space velocity of 1 h -1 The anions were removed by passing the solution through the column under the condition of 1 h space velocity. Furthermore, 1000 mL of Amberlite 120B (manufactured by Organo), which had been converted to the acid form with dilute hydrochloric acid, was used. -1 The aqueous solution of H-type polymer was concentrated by distilling off water under reduced pressure to obtain an aqueous solution of H-type copolymer (P) with a concentration of 1.5% by mass.

[0117] The aqueous solution of H-type copolymer (P) was diluted to a concentration of 1.2% by mass, cast onto an alkali-free glass plate (50 mm x 50 mm), and annealed at 150°C for 60 minutes to produce a membrane. The surface resistance, thickness and conductivity of the obtained membrane were 10.9 Ω / □, 6.19 μm and 141 S / cm, respectively. The particle diameter D of the H-type copolymer (P) was also measured. 50 The particle diameter was 1.0 nm, and the viscosity of a 1.0 mass% aqueous solution was 11 mPa·s (20°C).

[0118] [ka]

[0119] The H-type copolymer (P) aqueous solution was applied onto a glass substrate, and the surface of the dried film was observed under an optical microscope, confirming that a good quality coating film with excellent smoothness and uniformity had been formed (see FIG. 1).

[0120] Comparative Example 1 In Example 1, 8.64 g (25.1 mmol) of sodium 3-[(2,3-dihydrothieno[3,4,-b]-[1,4]dioxin-2-yl)methoxy]-1-methyl-1-propanesulfonate was used, and synthesis of an aqueous solution of a polymer was attempted in accordance with Example 1, except that TEG3OMe was not used. As a result, a conductive polymer (H-type polymer B), which is a single polymer, and an aqueous solution of H-type polymer B with a concentration of 1.2 mass% were obtained.

[0121] The H-type polymer B aqueous solution was applied onto a glass substrate. After drying, the surface of the film was observed under an optical microscope, and it was confirmed that the surface was rough, fine voids were present, and the coating film had low homogeneity (see FIG. 1).

Claims

1. A copolymer (P) comprising at least one repeating unit (M1) represented by the following general formula (M1) and at least one repeating unit (M2) represented by the following general formula (M2), wherein the repeating unit (M1) and the repeating unit (M2) may each be independently self-doped, and the ratio of the repeating unit (M1) / repeating unit (M2) (mol / mol) is 1 to 9999. 【Chemistry 1】 In the general formula (M1), R represents an organic group having a total of 1 to 18 carbon atoms and having at least one substituent selected from the group consisting of a sulfonic acid group and a phosphonic acid group. + represents a hydrogen ion, an alkali metal ion, a conjugate acid of an amine compound, or a quaternary ammonium cation. In the general formula (M2), q represents an integer of 1 to 4. Me represents a methyl group.

2. 2. The copolymer (P) according to claim 1, wherein the ratio of repeating units (M1) / repeating units (M2) (mol / mol) is from 1 to 999.

3. The copolymer (P) according to claim 1, wherein the repeating unit (M1) is a repeating unit (M3) represented by the following general formula (M3): 【Chemistry 2】 [In the general formula (M3), R 1 represents a hydrogen atom, a methyl group, an ethyl group, a linear or branched alkyl group having 3 to 6 carbon atoms, or a fluorine atom; m independently represents an integer of 1 to 10; and n independently represents 0 or 1. + represents M in general formula (M1). + is equivalent to.]

4. A method for producing the copolymer (P) according to claim 1, characterized in that a thiophene compound represented by the following general formula (1) and a thiophene compound represented by the following general formula (2) are copolymerized by an oxidation reaction in water or an organic solvent. 【Chemistry 3】 [R and M in the above general formula (1)] + respectively represent R and M in general formula (M1). + and q in the above general formula (2) is the same as q in the general formula (M2). Me represents a methyl group.

5. The method for producing the copolymer (P) according to claim 4, wherein the thiophene compound represented by the general formula (1) is a thiophene compound represented by the following general formula (3): 【Chemistry 4】 [R in general formula (3)] 1 , m, n, and M + are R in general formula (M3), 1 , m, n, and M in general formula (M1) + is equivalent to.]

6. An aqueous solution comprising the copolymer (P) according to claim 1.

Citation Information

Patent Citations

  • Polythiophenes, water-soluble conductive polymer using same, and method for producing same

    WO2014007299A1