All-solid battery and manufacturing method of all-solid battery

By designing the positive electrode active material layer and insulating member with inclined portions, the all-solid-state battery addresses current concentration issues, preventing lithium precipitation and improving energy efficiency.

JP2024145930APending Publication Date: 2024-10-15HONDA MOTOR CO LTD

Patent Information

Application Number
JP2023058542
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

Current concentration at the boundary between the positive electrode active material layer and the insulating member in all-solid-state batteries leads to local precipitation of lithium on the negative electrode side, which is problematic.

Method used

The positive electrode active material layer is designed with a first inclined portion that spreads away from the positive electrode current collector, and the insulating member has a second inclined portion that widens toward the collector, preventing current concentration and lithium precipitation.

Benefits of technology

This design effectively suppresses local lithium precipitation on the negative electrode, enhancing energy efficiency by reducing current concentration at the boundary.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024145930000001_ABST
    Figure 2024145930000001_ABST
Patent Text Reader

Abstract

To suppress a concentration of a current in a boundary of a positive electrode active material layer and an insulation member in a positive electrode of an all-solid battery, and suppress a local deposition of lithium on a negative electrode containing a metallic lithium or a lithium alloy.SOLUTION: An all-solid battery 1 comprises: a positive electrode 10 for the all-solid battery, in which a positive electrode active material layer 12 is formed in a positive electrode collector 11; a negative electrode 30 for the all-solid battery, in which a negative electrode active material layer 32 is formed in a negative electrode collector 31; and a solid electrolyte layer 20 that is arranged to between the positive electrode 10 for the all-solid battery and the negative electrode 30 for the all-solid battery. The positive electrode 10 for the all-solid battery comprises: the positive electrode collector 11; the positive electrode active material layer 12 formed in the positive electrode collector 11; and an insulation member 13 that is provided to an outer periphery of the positive electrode active material layer 12. The positive electrode active material layer 12 includes a first inclination part 12a that is inclined so as to be expanded in a direction separating from the positive electrode collector 11, and the negative electrode active material layer 32 contains a metallic lithium or a lithium alloy.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an all-solid-state battery and a method for manufacturing an all-solid-state battery. [Background technology]

[0002] An all-solid-state battery is manufactured, for example, by applying an electrode mixture onto a positive electrode current collector to form a positive electrode active material layer, and then cutting out a sheet having an insulating member formed on the outer periphery of the positive electrode active material layer and a solid electrolyte disposed on the upper surface of the positive electrode active material layer from the sheet into an arbitrary shape, stacking the positive electrodes and negative electrodes alternately, and press molding the resultant.

[0003] In the positive electrode of the all-solid-state battery thus obtained, the positive electrode active material layer has an inclined portion that inclines so as to widen toward the positive electrode current collector (see, for example, Patent Document 1). [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2020-173954 A Summary of the Invention [Problem to be solved by the invention]

[0005] When the positive electrode active material layer has an inclined portion that is inclined so as to widen toward the positive electrode current collector, current concentrates at the boundary between the positive electrode active material layer and the insulating member, causing localized precipitation of lithium on the negative electrode side containing metallic lithium or a lithium alloy, which is a problem.

[0006] In order to solve the above problems, the present application aims to suppress current concentration at the boundary between a positive electrode active material layer and an insulating member in a positive electrode of an all-solid-state battery, and to suppress localized lithium precipitation on the negative electrode side containing metallic lithium or a lithium alloy, thereby contributing to energy efficiency. [Means for solving the problem]

[0007] In order to achieve the above object, the present invention provides the following means. [1] A positive electrode for an all-solid-state battery, in which a positive electrode active material layer is formed on a positive electrode current collector; a negative electrode for an all-solid-state battery in which a negative electrode active material layer is formed on a negative electrode current collector; a solid electrolyte layer disposed between the all-solid-state battery positive electrode and the all-solid-state battery negative electrode, The positive electrode for an all-solid-state battery includes a positive electrode current collector, a positive electrode active material layer formed on the positive electrode current collector, and an insulating member provided on an outer periphery of the positive electrode active material layer, the positive electrode active material layer has a first inclined portion that is inclined so as to widen in a direction away from the positive electrode current collector, The negative electrode active material layer comprises metallic lithium or a lithium alloy.

[0008] In the all-solid-state battery of the present invention, the positive electrode active material layer has a first inclined portion that is inclined so as to widen in a direction away from the positive electrode current collector. This makes it possible to suppress current concentration at the boundary between the positive electrode active material layer and the insulating member, and to suppress localized precipitation of lithium on the side of the all-solid-state battery negative electrode containing metallic lithium or a lithium alloy.

[0009] [2] The all-solid-state battery according to [1], wherein the insulating member has a second inclined portion that is inclined so as to widen toward the positive electrode current collector.

[0010] Since the insulating member has the second inclined portion that is inclined so as to widen toward the positive electrode current collector, current concentration at the boundary between the positive electrode active material layer and the insulating member can be suppressed.

[0011] [3] A method for producing the all-solid-state battery according to [1] or [2], forming, at intervals on a positive electrode current collector, a plurality of insulating members each having an inclined portion inclined so as to widen toward the positive electrode current collector; forming a positive electrode active material layer between adjacent insulating members on the positive electrode current collector to obtain a positive electrode for an all-solid-state battery; laminating the all-solid-state battery positive electrode and the all-solid-state battery negative electrode with a solid electrolyte layer interposed therebetween; The present invention relates to a method for producing an all-solid-state battery.

[0012] According to the method for producing an all-solid-state battery of the present invention, the all-solid-state battery of the present invention can be obtained.

[0013] [4] The method for producing the all-solid-state battery according to [3], further comprising a pressurizing step of pressing the positive electrode current collector, the positive electrode active material layer, and the insulating member after forming the positive electrode active material layer.

[0014] By including a pressurizing step of pressing the positive electrode current collector, the positive electrode active material layer, and the insulating member after forming the positive electrode active material layer, it is possible to easily form a positive electrode active material layer having a first inclined portion that is inclined so as to widen in the direction away from the positive electrode current collector.

[0015] [5] The method for producing an all-solid-state battery according to [4], further comprising a cutting step of cutting the insulating member and the positive electrode current collector after the pressurizing step.

[0016] If a cutting step of cutting the insulating member and the positive electrode current collector is performed after the pressing step, an all-solid-state battery of a predetermined size can be obtained. Effect of the Invention

[0017] According to the present invention, in the positive electrode of an all-solid-state battery, current concentration at the boundary between the positive electrode active material layer and the insulating member can be suppressed, and localized precipitation of lithium can be suppressed on the negative electrode side containing metallic lithium or a lithium alloy. [Brief description of the drawings]

[0018] [Figure 1] FIG. 1 is a cross-sectional view showing an example of an all-solid-state battery according to an embodiment of the present invention. [Diagram 2] FIG. 1 is a diagram showing a result of simulating the current density of an all-solid-state battery according to an embodiment of the present invention. [Diagram 3] FIG. 1 is a cross-sectional view showing an example of a conventional all-solid-state battery. [Figure 4] FIG. 1 is a diagram showing the results of simulating the current density of a conventional all-solid-state battery. [Diagram 5] 1A to 1C are cross-sectional views showing a method for manufacturing an all-solid-state battery according to an embodiment of the present invention. [Figure 6] FIG. 2 is a plan view showing a method for manufacturing an all-solid-state battery according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] Hereinafter, an embodiment of the present invention will be described in detail.

[0020] [All-solid battery] 1 is a cross-sectional view showing an example of an all-solid-state battery according to an embodiment of the present invention. In the drawings used in the following description, characteristic parts may be enlarged for convenience in order to make the characteristics easier to understand, and the dimensional ratios of each component are not limited to those shown in the drawings.

[0021] The all-solid-state battery 1 includes an all-solid-state battery positive electrode (hereinafter sometimes abbreviated as "positive electrode") 10, a solid electrolyte layer 20, and an all-solid-state battery negative electrode (hereinafter sometimes abbreviated as "negative electrode") 30. In the all-solid-state battery 1, the positive electrode 10 and the negative electrode 30 are stacked with the solid electrolyte layer 20 interposed therebetween.

[0022] The positive electrode 10 includes a positive electrode current collector 11 , a positive electrode active material layer 12 formed on one main surface 11 a of the positive electrode current collector 11 , and an insulating member 13 provided on the outer periphery of the positive electrode active material layer 12 . The positive electrode active material layer 12 has a first inclined portion 12a that is inclined so as to widen in a direction away from one main surface 11a of the positive electrode current collector 11 (toward the thickness direction of the positive electrode active material layer 12). The angle of the first inclined portion 12a with respect to the one main surface 11a of the positive electrode current collector 11 is not particularly limited and is adjusted according to the capacity of the positive electrode active material layer 12, the thickness of the solid electrolyte layer 20, and the like. In this embodiment, the current density of the all-solid-state battery 1 is derived by simulation, and the angle of the first inclined portion 12a with respect to the one main surface 11a of the positive electrode current collector 11 is adjusted based on the results of the simulation.

[0023] The insulating member 13 has a second inclined portion 13a that is inclined so as to widen toward one main surface 11a of the positive electrode current collector 11 (toward the thickness direction of the positive electrode current collector 11). The angle of the second inclined portion 13a with respect to one main surface 11a of the positive electrode current collector 11 is not particularly limited and is adjusted depending on the capacity of the positive electrode active material layer 12, the thickness of the solid electrolyte layer 20, etc.

[0024] The negative electrode 30 includes a negative electrode current collector 31 and a negative electrode active material layer 32 formed on one main surface 31 a of the negative electrode current collector 31 .

[0025] (positive electrode) The positive electrode current collector 11 is preferably made of at least one material having high electrical conductivity. Examples of highly conductive materials include metals or alloys containing at least one of the metallic elements silver (Ag), palladium (Pd), gold (Au), platinum (Pt), aluminum (Al), copper (Cu), chromium (Cr), and nickel (Ni), and nonmetallic materials such as carbon (C). Considering the manufacturing cost as well as the high conductivity, aluminum, nickel, or stainless steel is preferable. Furthermore, aluminum does not easily react with the positive electrode active material, the negative electrode active material, and the solid electrolyte. Therefore, when aluminum is used for the positive electrode current collector 11, the internal resistance of the all-solid-state battery 1 can be reduced.

[0026] Examples of the shape of the positive electrode current collector 11 include a foil shape, a plate shape, a mesh shape, a nonwoven fabric shape, a foam shape, etc. In order to improve the adhesion with the positive electrode active material layer 12, carbon or the like may be disposed on the surface of the positive electrode current collector 11, or the surface may be roughened.

[0027] The positive electrode active material layer 12 contains a positive electrode active material that gives and receives lithium ions and electrons. The positive electrode active material is not particularly limited as long as it is a material that can reversibly release and absorb lithium ions and transport electrons, and any known positive electrode active material that can be applied to the positive electrode of an all-solid-state lithium ion battery can be used. For example, lithium cobalt oxide (LiCoO2), lithium nickel oxide (LiNiO2), lithium manganese oxide (LiMn2O4), solid solution oxide (Li2MnO3-LiMO2 (M=Co, Ni, etc.)), lithium manganese nickel cobalt oxide (LiNi x Mn y Co z O2, x+y+z=1), composite oxides such as olivine-type lithium phosphate (LiFePO4), conductive polymers such as polyaniline and polypyrrole, sulfides such as Li2S, CuS, Li-Cu-S compounds, TiS2, FeS, MoS2, and Li-Mo-S compounds, mixtures of sulfur and carbon, etc. The positive electrode active material may be composed of one kind of the above materials alone, or may be composed of two or more kinds.

[0028] The positive electrode active material layer 12 may contain a conductive assistant from the viewpoint of improving the conductivity of the positive electrode 10. As the conductive assistant, a conductive assistant that can be generally used in all-solid-state lithium ion batteries can be used. For example, carbon black such as acetylene black and ketjen black; carbon fiber; vapor-grown carbon fiber; graphite powder; carbon materials such as carbon nanotubes can be mentioned. The conductive assistant may be composed of one kind of the above materials alone or two or more kinds.

[0029] The positive electrode active material layer 12 may also contain a binder that serves to bind the positive electrode active materials together and between the positive electrode active material and the positive electrode current collector 11.

[0030] In this embodiment, the positive electrode active material layer 12 is formed on one main surface 11a of the positive electrode current collector 11, but is not limited thereto, and the positive electrode active material layer 12 may be formed on both main surfaces of the positive electrode current collector 11. In addition, when the positive electrode active material layer 12 has a three-dimensional porous structure such as a mesh, nonwoven fabric, or foam, the positive electrode active material layer 12 may be provided integrally with the positive electrode current collector 11.

[0031] The insulating material forming the insulating member 13 is not particularly limited, but examples thereof include insulating oxides such as alumina, resins such as polyvinylidene fluoride (PVDF), and rubbers such as styrene-butadiene rubber (SBR).

[0032] (Solid electrolyte layer) The solid electrolyte layer 20 is disposed between the positive electrode active material layer 12 and the negative electrode active material layer 32 .

[0033] The solid electrolyte is not particularly limited as long as it has lithium ion conductivity and insulation, and materials generally used in all-solid-state lithium ion batteries can be used. For example, inorganic solid electrolytes such as sulfide solid electrolyte materials, oxide solid electrolyte materials, halide solid electrolytes, and lithium-containing salts, polymer-based solid electrolytes such as polyethylene oxide, and gel-based solid electrolytes containing lithium-containing salts and lithium ion conductive ionic liquids can be mentioned. Among these, sulfide solid electrolyte materials are preferable from the viewpoint of high lithium ion conductivity and good structural formability and interface bonding properties by pressing. The form of the solid electrolyte material is not particularly limited, but may be, for example, in the form of particles.

[0034] The solid electrolyte layer 20 may contain an adhesive to impart mechanical strength and flexibility.

[0035] The solid electrolyte layer 20 may be in the form of a sheet having a porous substrate and a solid electrolyte held by the porous substrate. The form of the porous substrate is not particularly limited, and examples thereof include woven fabric, nonwoven fabric, mesh cloth, porous membrane, expanded sheet, and punched sheet. Among these forms, nonwoven fabric is preferred from the viewpoint of handling, which allows the amount of solid electrolyte to be further increased.

[0036] The porous substrate is preferably made of an insulating material. This can improve the insulating properties of the solid electrolyte layer 20. Examples of insulating materials include resin materials such as nylon, polyester, polyethylene, polypropylene, polytetrafluoroethylene, ethylene-tetrafluoroethylene copolymer, polyvinylidene fluoride, polyvinylidene chloride, polyvinyl chloride, polyurethane, vinylon, polybenzimidazole, polyimide, polyphenylene sulfite, polyether ether ketone, cellulose, and acrylic resin; natural fibers such as hemp, wood pulp, and cotton linters; and glass.

[0037] (Negative electrode) The negative electrode current collector 31 is preferably made of at least one material having high electrical conductivity, similar to the positive electrode current collector 11. Examples of the material having high electrical conductivity include metals or alloys containing at least one metal element selected from silver (Ag), palladium (Pd), gold (Au), platinum (Pt), aluminum (Al), copper (Cu), chromium (Cr), and nickel (Ni), and nonmetals such as carbon (C). Considering the manufacturing cost in addition to high electrical conductivity, copper, nickel, or stainless steel is preferable. Furthermore, stainless steel is unlikely to react with the positive electrode active material, the negative electrode active material, and the solid electrolyte. Therefore, when stainless steel is used for the negative electrode current collector 31, the internal resistance of the all-solid-state battery can be reduced.

[0038] Examples of the shape of the negative electrode current collector 31 include a foil shape, a plate shape, a mesh shape, a nonwoven fabric shape, a foam shape, etc. In order to improve the adhesion with the negative electrode active material layer 32, carbon or the like may be disposed on the surface of the negative electrode current collector 31, or the surface may be roughened.

[0039] The negative electrode active material layer 32 contains a negative electrode active material that gives and receives lithium ions and electrons. The negative electrode active material is not particularly limited as long as it is a material that can reversibly release and absorb lithium ions and transport electrons, and known negative electrode active materials that can be applied to the negative electrode of an all-solid-state lithium ion battery can be used. For example, carbonaceous materials such as natural graphite, artificial graphite, resin carbon, carbon fiber, activated carbon, hard carbon, and soft carbon; alloy-based materials mainly composed of tin, tin alloys, silicon, silicon alloys, gallium, gallium alloys, indium, indium alloys, aluminum, and aluminum alloys; conductive polymers such as polyacene, polyacetylene, and polypyrrole; metallic lithium, lithium alloys; lithium titanium composite oxides (for example, Li4Ti5O 12 The negative electrode active material may be composed of one kind of the above materials alone, or may be composed of two or more kinds of the above materials.

[0040] The negative electrode active material layer 32 may contain a conductive assistant, a binder, etc. There are no particular limitations on the materials used for these, and for example, the same materials as those used for the positive electrode active material layer 12 described above can be used.

[0041] As described above, according to the all-solid-state battery 1 of this embodiment, the positive electrode active material layer 12 of the positive electrode 10 has the first inclined portion 12a that is inclined so as to widen in the direction away from one main surface 11a of the positive electrode current collector 11, and therefore it is possible to suppress current concentration at the boundary between the positive electrode active material layer 12 and the insulating member 13. As a result, it is possible to suppress localized precipitation of lithium on the side of the negative electrode 30 containing metallic lithium or a lithium alloy.

[0042] Here, the results of simulating the current density of the all-solid-state battery 1 are shown in Fig. 2. In Fig. 2, the upper dashed line indicates the total current density (magnitude), the lower dashed line indicates the current density in the y direction, and the solid line indicates the current density in the x direction. As shown in Fig. 2, no current concentration is observed in the all-solid-state battery 1. As shown in Fig. 1, the insulating member 13 has a second inclined portion 13a that is inclined so as to widen toward one main surface 11a of the positive electrode current collector 11. Therefore, in the all-solid-state battery 1, localized precipitation of lithium on the side of the negative electrode 30 containing metallic lithium or a lithium alloy can be suppressed.

[0043] A cross-sectional view of an example of a conventional all-solid-state battery is shown in Fig. 3. In Fig. 3, the same components as those shown in Fig. 1 are denoted by the same reference numerals, and the description thereof will be omitted. In the all-solid-state battery 200, the positive electrode active material layer 12 has a first inclined portion 12a that is inclined so as to narrow in a direction away from one main surface 11a of the positive electrode current collector 11. The insulating member 13 has a second inclined portion 13a that is inclined so as to narrow toward one main surface 11a of the positive electrode current collector 11.

[0044] Here, the results of simulating the current density of the all-solid-state battery 200 are shown in Fig. 4. In Fig. 4, the upper dashed line indicates the total current density (magnitude), the lower dashed line indicates the current density in the y direction, and the solid line indicates the current density in the x direction. 4, current concentration was observed in the all-solid-state battery 200. Therefore, in the all-solid-state battery 200, lithium is locally deposited on the negative electrode 30 side containing metallic lithium or a lithium alloy.

[0045] [Manufacturing method of all-solid-state batteries] Fig. 5 is a cross-sectional view showing a method for manufacturing an all-solid-state battery according to an embodiment of the present invention. Fig. 6 is a plan view showing a method for manufacturing an all-solid-state battery according to an embodiment of the present invention. In Fig. 5 and Fig. 6, the same components as those shown in Fig. 1 are denoted by the same reference numerals, and the description thereof will be omitted. In addition, the drawings used in the following explanation may show characteristic parts in an enlarged manner for convenience in order to make the features easier to understand, and the dimensional ratios of each component are not limited to those shown in the drawings.

[0046] The method for producing an all-solid-state battery of this embodiment includes a step of forming, at intervals, a plurality of insulating members, each having an inclined portion that inclines so as to widen toward the positive electrode current collector, on a positive electrode current collector (hereinafter referred to as an "insulating member forming step"); a step of forming a positive electrode active material layer between adjacent insulating members on the positive electrode current collector to obtain a positive electrode for an all-solid-state battery (hereinafter referred to as a "positive electrode forming step"); and a step of stacking the positive electrode for an all-solid-state battery and the negative electrode for an all-solid-state battery with a solid electrolyte layer interposed therebetween (hereinafter referred to as a "stacking step").

[0047] (Insulating member forming process) In the insulating member formation process, an insulating material applicator 110 applies an insulating material 53 to one main surface 11a of the positive electrode current collector 11, and hardens the insulating material 53 to form a plurality of spaced apart insulating members 13 having second inclined portions 13a that are inclined so as to widen toward the one main surface 11a of the positive electrode current collector 11.

[0048] (Positive electrode formation process) In the positive electrode formation process, a positive electrode mixture coating device 120 coats a positive electrode mixture containing a positive electrode active material between adjacent insulating members 13 on one main surface 11a of the positive electrode current collector 11 to form a positive electrode active material layer 12, thereby obtaining a positive electrode 10.

[0049] (Pressure process) The positive electrode forming step preferably includes a pressurizing step of pressing the positive electrode collector 11, the positive electrode active material layer 12, and the insulating member 13 with a pressurizing roller 130 after forming the positive electrode active material layer 12. The pressurizing step makes it possible to easily form the positive electrode active material layer 12 having the first inclined portion 12a inclined so as to widen in a direction away from one main surface 11a of the positive electrode collector 11 between adjacent insulating members 13.

[0050] (cutting process) In the positive electrode formation step, it is preferable to have a cutting step of cutting the insulating member 13 and the positive electrode current collector 11 after the pressing step. By the cutting step, an all-solid-state battery 1 of a predetermined size is obtained.

[0051] According to the method for producing an all-solid-state battery of this embodiment, the all-solid-state battery of the above embodiment can be obtained.

[0052] Although the embodiments of the present invention have been described in detail above, the present invention is not limited to the above-described embodiments, and various modifications and variations are possible within the scope of the gist of the present invention as described in the claims. [Explanation of symbols]

[0053] 1 All-solid-state battery 10 Positive electrode for solid-state batteries (positive electrode) 11 Positive electrode current collector 12 Cathode active material layer 13 Insulating materials 20 Solid electrolyte layer 30 Anode for all-solid-state batteries (anode) 31 Negative electrode current collector 32 Negative electrode active material layer

Claims

1. a positive electrode for an all-solid-state battery in which a positive electrode active material layer is formed on a positive electrode current collector; a negative electrode for an all-solid-state battery in which a negative electrode active material layer is formed on a negative electrode current collector; a solid electrolyte layer disposed between the all-solid-state battery positive electrode and the all-solid-state battery negative electrode, The positive electrode for an all-solid-state battery includes a positive electrode current collector, a positive electrode active material layer formed on the positive electrode current collector, and an insulating member provided on an outer periphery of the positive electrode active material layer, the positive electrode active material layer has a first inclined portion that is inclined so as to widen in a direction away from the positive electrode current collector, The negative electrode active material layer comprises metallic lithium or a lithium alloy.

2. The all-solid-state battery according to claim 1 , wherein the insulating member has a second inclined portion that is inclined so as to widen toward the positive electrode current collector.

3. A method for producing the all-solid-state battery according to claim 1 or 2, forming, at intervals on a positive electrode current collector, a plurality of insulating members each having an inclined portion inclined so as to widen toward the positive electrode current collector; forming a positive electrode active material layer between adjacent insulating members on the positive electrode current collector to obtain a positive electrode for an all-solid-state battery; laminating the all-solid-state battery positive electrode and the all-solid-state battery negative electrode with a solid electrolyte layer interposed therebetween; The method for producing an all-solid-state battery comprising the steps of:

4. The method for producing an all-solid-state battery according to claim 3 , further comprising a pressurizing step of pressing the positive electrode current collector, the positive electrode active material layer, and the insulating member after forming the positive electrode active material layer.

5. The method for producing an all-solid-state battery according to claim 4 , further comprising, after the pressing step, a cutting step of cutting the insulating member and the positive electrode current collector.

Citation Information

Patent Citations

  • Nonaqueous electrolyte secondary battery

    JP2021026852A

  • All-solid battery

    JP2021027013A

  • All-solid battery and manufacturing method thereof

    JP2022062579A

  • Laminated battery

    WO2020183795A1

  • Positive electrode for all-solid-state battery and all-solid-state battery

    JP2020173954A

Cited By

  • All-solid-state battery and method for manufacturing all-solid-state battery

    CN122868616A

  • All-solid-state battery and method for manufacturing an all-solid-state battery

    JP2026165950A

  • Colored glass articles having improved mechanical durability