Method for manufacturing heat exchanger
The described method for assembling flat tubes with fin groups in heat exchangers addresses the inefficiencies in existing manufacturing processes by ensuring accurate alignment and reducing fin damage, resulting in a more reliable and efficient production process.
Patent Information
- Application Number
- JP2023058570
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-31
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2043-03-31
AI Technical Summary
Existing methods for manufacturing heat exchangers with flat tubes and fin groups have not been sufficiently developed, particularly in terms of efficient assembly and alignment to prevent damage to fins during the manufacturing process.
A method involving the assembly of flat tubes with fin groups, including steps of combining the first fin group and flat tubes, reversing the assembly, and using a pressing member to align and correct deflections before inserting the flat tubes into slots of the second fin group, ensuring accurate and damage-free assembly.
The method ensures precise alignment and minimizes the risk of fin damage during assembly, allowing for efficient and reliable production of heat exchangers with improved structural integrity.
Smart Images

Figure 2024148180000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a method for manufacturing a heat exchanger. [Background technology]
[0002] Patent Document 1 discloses a heat exchanger equipped with flat heat transfer tubes (flat tubes) and plate-like fins. In this heat exchanger, the windward portion of each of the heat transfer tubes arranged vertically is inserted into the flat grooves of the upstream plate fins, and the leeward portion is inserted into the flat grooves of the downstream plate fins. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Japanese Patent Application Publication No. 03-128167 Summary of the Invention [Problem to be solved by the invention]
[0004] As described above, Patent Document 1 discloses a heat exchanger having a structure in which fin groups are individually arranged on the upwind side and the downwind side of flat tubes. However, a specific method for manufacturing a heat exchanger having such a structure has not been fully considered.
[0005] The objective of the present disclosure is to manufacture a heat exchanger having flat tubes and two groups of fins. [Means for solving the problem]
[0006] A first aspect of the present disclosure is directed to a method for manufacturing a heat exchanger (10) comprising a plurality of flat tubes (20), and a first fin group (41) and a second fin group (42), each of which is composed of a plurality of plate-shaped fins (30), wherein each of the plurality of fins (30) has a plurality of slots (32) having an open end (33) formed on an outer edge of the fin (30), and each of the plurality of flat tubes (20) is inserted into the slots (32) of each of the fins (30) constituting the first fin group (41) and the slots (32) of each of the fins (30) constituting the second fin group (42). A manufacturing method for the heat exchanger (10) of this embodiment includes a first step of inserting the flat tubes (20) into the slots (32) of the fins (30) constituting the first fin group (41) to form an assembly (50) consisting of the first fin group (41) and a plurality of the flat tubes (20), and a second step of positioning the second fin group (42) in an orientation in which the opening ends (33) of the slots (32) of the fins (30) constituting the second fin group (42) are located on the upper side, positioning the assembly (50) in an orientation in which the flat tubes (20) are located on the lower side, and inserting the flat tubes (20) of the assembly (50) from above into the slots (32) of the fins (30) constituting the second fin group (42).
[0007] In the manufacturing method of the first aspect, a first step and a second step are performed. In the first step, the first fin group (41) and the flat tube (20) are combined to form an assembly (50). In the second step, the second fin group (42) is arranged in a position where the open end (33) of the slot (32) faces upward, and the assembly (50) is arranged in a position where the flat tube (20) is located on the lower side. In the second step, the flat tube (20) of the assembly (50) is inserted from above into the slot (32) of the fin (30) that constitutes the second fin group (42). As a result, the flat tube (20), the first fin group (41), and the second fin group (42) are combined.
[0008] A second aspect of the present disclosure is a method of performing an inversion process before the second step in which, in the first step, the first fin group (41) is positioned in a position in which the opening ends (33) of the slots (32) of the fins (30) constituting the first fin group (41) are positioned at the upper side, the flat tubes (20) are inserted from above into the slots (32) of the fins (30) constituting the first fin group (41), and the assembly (50) formed in the first step is inverted from a position in which the flat tubes (20) are positioned at the upper side to a position in which the flat tubes (20) are positioned at the lower side.
[0009] In the first step of the second embodiment, the flat tubes (20) are inserted from above into the slots (32) of the fins (30) that constitute the first fin group (41). In this embodiment, an inversion step is performed between the first and second steps. In the inversion step, the assembly (50) formed in the first step is inverted from a position in which the flat tubes (20) are located on the upper side to a position in which the flat tubes (20) are located on the lower side.
[0010] A third aspect of the present disclosure is a method for forming a second fin group (50) in a second step in which a pressing member (65) having a flat pressing surface (66) on the lower surface is used, and the pressing surface (66) of the pressing member (65) is brought into contact with the upper outer edge of the fin (30) of the assembly (50) arranged in a position in which the flat tube (20) is positioned on the lower side, and the assembly (50) is pressed down by the pressing member (65), thereby inserting the flat tube (20) of the assembly (50) from above into the slot (32) of the fin (30) constituting the second fin group (42).
[0011] In the second step of the third embodiment, the assembly (50) is pressed down with a pressing member (65) so that the flat tubes (20) of the assembly (50) are inserted into the slots (32) of the fins (30) that constitute the second fin group (42).
[0012] A fourth aspect of the present disclosure is that, in the third aspect, the pressing member (65) used in the second step includes a plurality of pressing blocks (67), each of whose lower surface constitutes the pressing surface (66).
[0013] In the second step of the fourth embodiment, the assembly (50) is pressed down by a pressing member (65) having a plurality of pressing blocks (67).
[0014] A fifth aspect of the present disclosure is that in the first or second aspect, the second step includes a straightening step of straightening the deflection of the assembly (50) arranged in a position in which the flat tube (20) is located on the lower side, and in the second step, the flat tube (20) of the assembly (50) in a state in which the deflection has been straightened is inserted from above into the slot (32) of the fin (30) that constitutes the second fin group (42).
[0015] In the second step of the fifth embodiment, the assembly (50) in a state where the deflection has been corrected is combined with the second fin group (42). Therefore, in the process of inserting the flat tubes (20) of the assembly (50) into the slots (32) of the fins (30) constituting the second fin group (42), it is possible to reduce the possibility that the fins (30) will be crushed by the flat tubes (20).
[0016] A sixth aspect of the present disclosure is the fifth aspect, wherein the straightening step includes a first straightening step of straightening horizontal deflection of the assembly (50) by clamping the assembly (50) from the horizontal direction.
[0017] In the first straightening step of the sixth embodiment, horizontal deflection of the assembly (50) arranged in a position in which the flat tubes (20) are located on the lower side is straightened.
[0018] A seventh aspect of the present disclosure is the sixth aspect, wherein in the first straightening process, the assembly (50) is clamped from both sides in the arrangement direction of the flat tubes (20) and also from both sides in the arrangement direction of the fins (30).
[0019] In the first straightening step of the seventh embodiment, the assembly (50) is sandwiched from both sides in the arrangement direction of the flat tubes (20) and from both sides in the arrangement direction of the fins (30). As a result, horizontal deflection of the assembly (50) arranged in an orientation in which the flat tubes (20) are located on the lower side is straightened.
[0020] An eighth aspect of the present disclosure is a step in which, in the second step, a pressing member (65) having a flat pressing surface (66) on the lower surface is used, and the pressing surface (66) of the pressing member (65) is brought into contact with the upper outer edge of the fins (30) of the assembly (50) arranged in an orientation in which the flat tubes (20) are located on the lower side, and the assembly (50) is pressed down by the pressing member (65), thereby inserting the flat tubes (20) of the assembly (50) from above into the slots (32) of the fins (30) that constitute the second fin group (42), and the straightening step includes a second straightening step in which the assembly (50) is pressed against the pressing surface (66) of the pressing member (65) to straighten the vertical deflection of the assembly (50).
[0021] In the second step of the eighth aspect, the assembly (50) is pressed down by a pressing member (65), so that the flat tubes (20) of the assembly (50) are inserted into the slots (32) of the fins (30) constituting the second fin group (42). In the second straightening step, the assembly (50) is pressed against a pressing surface (66) of the pressing member (65). As a result, the bending in the vertical direction of the assembly (50) arranged in a position in which the flat tubes (20) are located on the lower side is straightened.
[0022] A ninth aspect of the present disclosure is the eighth aspect, wherein in the second straightening step, both ends of the flat tube (20) in the assembly (50) are lifted to press the assembly (50) against the pressing surface (66) of the pressing member (65).
[0023] In the second straightening step of the ninth embodiment, both ends of the flat tubes 20 of the assembly 50 are lifted. As a result, the assembly 50 is pressed against the pressing surface 66 of the pressing member 65, and the bending of the assembly 50 in the vertical direction is straightened.
[0024] A tenth aspect of the present disclosure is the eighth aspect, wherein in the second straightening process, both ends of the flat tube (20) in the assembly (50) and the middle part of the flat tube (20) in the extension direction are lifted, thereby pressing the assembly (50) against the pressing surface (66) of the pressing member (65).
[0025] In the second straightening step of the tenth embodiment, both ends of the flat tubes 20 and a middle portion in the extension direction of the flat tubes 20 of the assembly 50 are lifted. As a result, the assembly 50 is pressed against the pressing surface 66 of the pressing member 65, and the bending of the assembly 50 in the up-down direction is straightened. [Brief description of the drawings]
[0026] [Figure 1] FIG. 1 is a front view of the heat exchanger. [Diagram 2] FIG. 2 is a cross-sectional view of the heat exchanger taken along line AA of FIG. [Diagram 3] FIG. 3 is a plan view of the fin. [Figure 4] FIG. 4 is a process diagram showing a method for manufacturing a heat exchanger. [Diagram 5] FIG. 5 is a schematic perspective view showing the first fin group in the first step. [Figure 6] FIG. 6 is a front view of the first fin group and the flat tubes in the first step. [Figure 7] FIG. 7 is a schematic perspective view of the assembly formed in the first step. [Figure 8] FIG. 8 is a front view of the assembly formed in the first step. [Figure 9] FIG. 9 is a front view of the assembly showing the inversion process in the inversion step. [Figure 10] FIG. 10 is a cross-sectional view showing the CC cross section of FIG. 14 in the second step. [Figure 11] FIG. 11 is a plan view of the assembly and the pressing member in the second step. [Figure 12] FIG. 12 is a plan view of the assembly and the clamping member in the second step. [Figure 13] FIG. 13 is a plan view of the assembly and the clamping member in the first straightening step. [Figure 14] FIG. 14 is a cross-sectional view showing the cross section BB of FIG. 13 in the first straightening step. [Figure 15] FIG. 15 is a cross-sectional view showing the cross section BB of FIG. 13 in the second straightening step. [Figure 16] FIG. 16 is a cross-sectional view corresponding to FIG. 10, illustrating the process of moving the assembly downward in the second step. [Figure 17] FIG. 17 is a cross-sectional view corresponding to FIG. 10, showing the assembly and the second fin group during the second step. [Figure 18] FIG. 18 is a cross-sectional view corresponding to FIG. 10, illustrating a state in which the combination of the assembly and the second fin group is completed in the second step. [Figure 19] FIG. 19 is a plan view of the first modified example of the embodiment, which corresponds to FIG. [Figure 20] FIG. 20 is a cross-sectional view of a second modified example of the embodiment, which corresponds to FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0027] An embodiment will be described below. The embodiment is a method for manufacturing a heat exchanger (10).
[0028] -Heat exchanger- A heat exchanger (10) manufactured by the manufacturing method of the present embodiment will be described. The heat exchanger (10) is provided in a refrigerant circuit of an air conditioner that operates in a refrigeration cycle, and exchanges heat between the refrigerant flowing through the refrigerant circuit and air.
[0029] 1 and 2, the heat exchanger (10) includes a core (15) and two first header collecting pipes (16, 17). The core (15) includes a plurality of flat tubes (20) and a plurality of fins (30). The flat tubes (20), the fins (30), and the header collecting pipes (16, 17) are all made of aluminum or an aluminum alloy.
[0030] <Header collector pipe> Each of the two header collecting pipes (16, 17) is a long, thin cylindrical member. Note that the shape and structure of the header collecting pipes (16, 17) shown here are merely examples. In the heat exchanger (10) shown in Fig. 1, the first header collecting pipe (16) is disposed on the left side of the core (15), and the second header collecting pipe (17) is disposed on the right side of the core (15).
[0031] <Flat tube> 2, the flat tube 20 is a flat tube whose width is greater than its thickness. The cross section of the flat tube 20 perpendicular to its elongation direction is a rectangle with rounded corners or an oval shape with arcs at both ends.
[0032] 1, in the core 15, the flat tubes 20 are arranged such that their extension directions (axial directions) are substantially horizontal and their widthwise sides face each other. The flat tubes 20 are arranged vertically at regular intervals.
[0033] One end of each of the flat tubes (20) constituting the core (15) is inserted into the first header collector pipe (16), and the other end is inserted into the second header collector pipe (17). Each of the header collector pipes (16, 17) is joined to the flat tubes (20) by brazing.
[0034] As shown in Fig. 2, the flat tube (20) has a plurality of flow paths (21). Each flow path (21) is a straight flow path extending along the elongation direction of the flat tube (20). In the flat tube (20), the plurality of flow paths (21) are arranged side by side in the width direction of the flat tube (20). Each flow path (21) opens at both end faces of the flat tube (20). Each flow path (21) communicates with the internal space of the header collecting pipe (16, 17).
[0035] <fin> 3, the fin 30 is a long, thin plate-like member. One long side of the fin 30 is a linear continuous edge 31 that continues from one end of the fin to the other end in the longitudinal direction.
[0036] A plurality of slots 32 are formed in the fin 30. The slots 32 are elongated notches into which the flat tubes 20 are inserted. Each slot 32 extends in the direction of the short side of the fin 30 (in a direction perpendicular to the continuous edge portion 31). Each slot 32 opens to the outer edge of the fin 30. In other words, each slot 32 has an opening end 33 at the outer edge of the fin 30. Specifically, each slot 32 opens to the other long side of the fin 30 (in other words, the long side opposite to the continuous edge portion 31).
[0037] In the fin 30, a plurality of slots 32 are formed at regular intervals from one another in the long side direction (the direction parallel to the continuous edge portion 31) of the fin 30. The number of slots 32 formed in one fin 30 is the same as the number of flat tubes 20 constituting the core 15.
[0038] Each slot (32) is divided into a tube introduction portion (32a) and a tube holding portion (32b). The tube introduction portion (32a) is a portion that continues to the open end (33). The width (length in a direction parallel to the continuous edge portion (31)) of the tube introduction portion (32a) gradually increases toward the open end (33). The tube holding portion (32b) is a long and narrow portion that extends in the direction of the short side of the fin (30). The width (length in a direction parallel to the continuous edge portion (31)) of the tube holding portion (32b) is substantially constant. In addition, the width of the tube holding portion (32b) is slightly narrower than the thickness of the flat tube (20).
[0039] The fin (30) has raised portions (34) formed between adjacent slots (32) for promoting heat transfer.
[0040] The shape of the fins (30) constituting the first fin group (41) and the shape of the fins (30) constituting the second fin group (42) may be the same as or different from each other. For example, the shapes of the cut-and-raised portions (34) of the fins (30) constituting the first fin group (41) and the fins (30) constituting the second fin group (42) may be different from each other.
[0041] <core> As shown in FIGS. 1 and 2, the core (15) includes a flat tube (20), a first group of fins (41), and a second group of fins (42).
[0042] Each of the first fin group (41) and the second fin group (42) is composed of a plurality of fins (30). The number of fins (30) constituting each of the fin groups (41, 42) is preferably the same, but may be different. In each of the fin groups (41, 42), the plurality of fins (30) are arranged facing each other and spaced apart from each other at regular intervals. In each of the fin groups (41, 42), the corresponding slots (32) of each fin (30) are aligned in a row in the arrangement direction of the fins (30).
[0043] The first fin group (41) is disposed in front of the flat tube (20) in Fig. 2. Each fin (30) constituting the first fin group (41) is disposed in such a manner that its continuous edge portion (31) faces the front and the open end (33) of its slot (32) faces the rear. The front portion of the flat tube (20) fits into the slot (32) of the fin (30) constituting the first fin group (41). The fins (30) constituting the first fin group (41) are joined to the flat tube (20) by brazing.
[0044] The second fin group (42) is disposed on the rear side of the flat tube (20) in Fig. 2. Each fin (30) constituting the second fin group (42) is disposed in such a manner that the open end (33) of the slot (32) faces forward and the continuous edge portion (31) faces rearward. The rear portion of the flat tube (20) fits into the slot (32) of the fin (30) constituting the second fin group (42). The fins (30) constituting the second fin group (42) are joined to the flat tube (20) by brazing.
[0045] -Heat exchanger manufacturing method- A method for manufacturing the heat exchanger 10 having the above-described structure will be described below. In the method for manufacturing the heat exchanger 10 of this embodiment, a core assembly step, a header attachment step, and a joining step are carried out in this order.
[0046] The core assembling step is a step of combining the flat tubes 20, the first fin group 41, and the second fin group 42 to form the core 15. The core assembling step will be described in detail later.
[0047] The header attachment process is a process of attaching a first header collector pipe (16) and a second header collector pipe (17) to the core (15) formed in the core assembly process. In the header attachment process, one end of each of the flat tubes (20) constituting the core (15) is inserted into the first header collector pipe (16), and the other end of each of the flat tubes (20) constituting the core (15) is inserted into the second header collector pipe (17).
[0048] The joining process is a process of joining the fins (30) and the header collector pipes (16, 17) to the flat tubes (20) by brazing. In the joining process, the core (15) to which the header collector pipes (16, 17) are attached is placed in a heating furnace or the like and heated. As a result, the brazing material melts, and the fins (30) and the header collector pipes (16, 17) are joined to the flat tubes (20).
[0049] -Core assembly process- As shown in Fig. 4, the core assembling process includes a first step, an inversion step, and a second step, which are carried out in this order. The second step includes a straightening step. The straightening step includes a first straightening step and a second straightening step.
[0050] <1st process> The first step is a step of combining the first fin group (41) and the flat tubes (20) to form an assembly (50). In the first step, all of the flat tubes (20) constituting the core (15) are combined with the first fin group (41). Thus, in the first step, all of the flat tubes (20) constituting the heat exchanger (10), which is a finished product, are combined with the first fin group (41).
[0051] As shown in Fig. 5, in the first step, all the fins (30) constituting the first fin group (41) are arranged facing each other at regular intervals. Note that in Fig. 5, the cut-and-raised portions (34) of the fins (30) are not shown. Each fin (30) is arranged with its continuous edge portion (31) facing downward and the open end (33) of the slot (32) facing upward. The multiple fins (30) are arranged such that their corresponding slots (32) are aligned in a row in the arrangement direction of the fins (30). The fins (30) constituting the first fin group (41) are surrounded by a frame-shaped or tray-shaped member to maintain the orientation shown in Fig. 5.
[0052] 5, the slots (32) of each fin (30) arranged in a row form a slot row (35). In this state, the first fin group (41) has the same number of slot rows (35) as the number of slots (32) formed in one fin (30).
[0053] 6, in the first step, the flat tubes (20) are inserted one by one into each slot row (35) of the first fin group (41). The flat tubes (20) are inserted from top to bottom with respect to the slots (32) that form the corresponding slot row (35) such that the width direction of the flat tubes (20) is substantially vertical and the extension direction of the flat tubes (20) is aligned along the arrangement direction of the fins (30).
[0054] As a result, an assembly 50 is formed in which the first fin group 41 and the flat tubes 20 are combined, as shown in Figures 7 and 8. At the end of the first step, the assembly 50 is in a position in which the continuous edge 31 of the fin 30 is located on the lower side and the flat tubes 20 are located on the upper side. Note that the cut-and-raised portions 34 of the fins 30 are not shown in Figure 7.
[0055] <Inversion process> The inversion step is a step of inverting the position of the assembly (50) formed in the first step.
[0056] As described above, at the end of the first step, the assembly (50) is in a position in which the flat tubes (20) are located on the upper side. As shown in Fig. 9, in the inversion step, the assembly (50) is inverted from a position in which the flat tubes (20) are located on the upper side to a position in which the flat tubes (20) are located on the lower side. In the inversion step, the assembly (50) is held by an arm-shaped member (not shown), and the position of the assembly (50) is inverted by rotating this arm-shaped member by 180 degrees.
[0057] <2nd process> The second step is a step of combining the assembly (50) and the second fin group (42) to form the core (15). In the second step, a straightening step is performed to straighten the deflection of the assembly (50), and the assembly (50) in a straightened state is combined with the second fin group (42).
[0058] [Arrangement of second fin group] In the second step, the fins (30) constituting the second fin group (42) are arranged in the same manner as the fins (30) of the first fin group (41) in the first step (see FIG. 5). Specifically, in the second step, all the fins (30) constituting the second fin group (42) are arranged facing each other at regular intervals. Each fin (30) is arranged with its continuous edge portion (31) facing downward and with the open end (33) of its slot (32) facing upward. The multiple fins (30) are also arranged such that their corresponding slots (32) are aligned in a row in the arrangement direction of the fins (30).
[0059] As shown in Fig. 10, the second fin group (42) is placed on a flat base member (60). The fins (30) constituting the second fin group (42) are surrounded by a frame- or tray-shaped member to maintain the position shown in Fig. 5. In this state of the second fin group (42), the slots (32) of each fin (30) lined up in a row form a slot row (35). In this state of the second fin group (42), the same number of slot rows (35) are formed as the number of slots (32) formed in one fin (30).
[0060] [Layout of Assembly] 10, in the second step, the assembly (50) that has been subjected to the inversion step is disposed above the second fin group (42). The assembly (50) is disposed above the second fin group (42) with the flat tubes (20) positioned on the lower side. In this state, each flat tube (20) of the assembly (50) faces the slot row (35) of the corresponding second fin group (42).
[0061] [Pressing member] In the second step, the assembly (50) is placed below the pressing member (65). As shown in Fig. 11, the pressing member (65) is a flat member that covers the entire assembly (50) when viewed from above. The lower surface of the pressing member (65) is a flat pressing surface (66). The pressing surface (66) faces the continuous edge portions (31) of the fins (30) that constitute the first fin group (41) of the assembly (50) (see Fig. 10).
[0062] [Holding member] 12, in the second step, the assembly (50) is surrounded by four clamping members (71-74). In the assembly (50), one end of each of the fins (30) constituting the first fin group (41) faces the first clamping member (71), and the other end of each fin (30) faces the second clamping member (72). In the assembly (50), one end face of each of the flat tubes (20) faces the third clamping member (73), and the other end face of each of the flat tubes (20) faces the fourth clamping member (74).
[0063] Each of the first clamping member (71) and the second clamping member (72) is an elongated member extending horizontally. The surface of each of the first clamping member (71) and the second clamping member (72) facing the assembly (50) is a substantially vertical surface.
[0064] 10 and 12, the first clamping member (71) is disposed on the left side of the assembly (50) and faces the left end of the fin (30) that constitutes the first fin group (41). In addition, in Fig. 10 and 12, the second clamping member (72) is disposed on the right side of the assembly (50) and faces the right end of the fin (30) that constitutes the first fin group (41).
[0065] Each of the third clamping member (73) and the fourth clamping member (74) is an elongated member extending in the horizontal direction. As shown in Fig. 14, each of the third clamping member (73) and the fourth clamping member (74) includes a clamping portion (73a, 74a) and a support portion (73b, 74b). The surface of the clamping portion (73a, 74a) facing the assembly (50) is a substantially vertical surface. The support portion (73b, 74b) is a portion that protrudes from the clamping portion (73a, 74a) toward the assembly (50). The upper surface of the support portion (73b, 74b) is a substantially horizontal surface.
[0066] In Fig. 12, the third clamping member (73) is disposed on the front side of the assembly (50). The third clamping member (73) has a clamping portion (73a) facing the end face of the flat tube (20) and a support portion (73b) positioned below the end of the flat tube (20) (see Fig. 14). Also, in Fig. 12, the fourth clamping member (74) is disposed on the rear side of the assembly (50). The fourth clamping member (74) has a clamping portion (74a) facing the end face of the flat tube (20) and a support portion (74b) positioned below the end of the flat tube (20) (see Fig. 14).
[0067] [First straightening process] The first straightening step is a step of straightening horizontal deflection of the assembly (50) arranged in a position in which the flat tubes (20) are located on the lower side.
[0068] Here, in the assembly (50), the flat tubes (20) inserted into the slot rows (35) of the first fin group (41) are held by the first fin group (41) by frictional force. Therefore, the assembly (50) may bend in the horizontal direction due to relative displacement between the first fin group (41) and the flat tubes (20). Therefore, in the first straightening process, the horizontal bending of the assembly (50) is straightened.
[0069] As shown in Fig. 12, in the first straightening step, the second clamping member (72) is pressed against the assembly (50). As a result, as shown in Fig. 13, the assembly (50) is sandwiched from both the left and right sides in Fig. 13 by the first clamping member (71) and the second clamping member (72). In this manner, the assembly (50) is sandwiched from both sides in the arrangement direction of the flat tubes (20) (in other words, the longitudinal direction of the fins (30)) by the first clamping member (71) and the second clamping member (72). Note that the pressing member (65) is not shown in Figs. 12 and 13.
[0070] Furthermore, in the first straightening step, as shown in Fig. 12, the third clamping member (73) and the fourth clamping member (74) are each pressed against the assembly (50). As a result, as shown in Fig. 13, the assembly (50) is sandwiched by the third clamping member (73) and the fourth clamping member (74) from both the front and rear sides in Fig. 13. In this manner, the assembly (50) is sandwiched by the third clamping member (73) and the fourth clamping member (74) from both sides in the arrangement direction of the fins (30) (in other words, the extension direction of the flat tubes (20)).
[0071] In the first straightening step, the assembly (50) in a position in which the flat tubes (20) are located on the lower side is clamped from both sides in the arrangement direction of the flat tubes (20) by the first clamping member (71) and the second clamping member (72), and is also clamped from both sides in the arrangement direction of the fins (30) by the third clamping member (73) and the fourth clamping member (74). As a result, the horizontal deflection of the assembly (50) arranged in a position in which the flat tubes (20) are located on the lower side is straightened.
[0072] [Second straightening process] The second straightening step is a step of straightening out any bending in the vertical direction of the assembly (50) arranged in a position in which the flat tubes (20) are located on the lower side.
[0073] Here, the assembly 50 arranged with the flat tubes 20 positioned on the lower side may bend downward near the center in the arrangement direction of the flat tubes 20 (left-right direction in FIG. 10) due to elastic deformation of the fins 30. Also, the assembly 50 arranged with the flat tubes 20 positioned on the lower side may be curved upward.
[0074] When the assembly 50 is curved, the width direction of each flat tube 20 is tilted with respect to the vertical direction. Therefore, the flat tube 20 cannot be inserted straight from above into the slot row 35 of the second fin group 42, and as a result, the fins 30 of the second fin group 42 may be crushed. Therefore, in the second straightening process, the bending of the assembly 50 in the vertical direction is straightened.
[0075] As shown in FIG. 14, in the second straightening step, the third clamping member (73) and the fourth clamping member (74) move upward, and the upper surfaces of the support portions (73b, 74b) come into contact with the ends of the flat tubes (20). As shown in FIG. 15, the assembly (50) that is horizontally sandwiched by the four clamping members (71-74) is lifted by the third clamping member (73) and the fourth clamping member (74) and pressed against the pressing surface (66) of the pressing member (65). The pressing surface (66) of the pressing member (65) is a flat horizontal surface. Therefore, when the assembly (50) is pressed against the pressing member (65), the continuous edge portions (31) of the fins (30) that constitute the first fin group (41) are straightened along the pressing surface (66), and the bending of the assembly (50) in the vertical direction is straightened.
[0076] [Combination of assembly and second fin group] The assembly (50) is combined with the second fin group (42) in a state where deflections in the horizontal and vertical directions are corrected.
[0077] As shown in FIG. 16, the assembly (50) is sandwiched horizontally by the four clamping members (71-74) and moves downward while being pressed against the pressing surface (66) of the pressing member (65).
[0078] When the assembly (50) moves downward, as shown in Fig. 17, the lower portion of each flat tube (20) of the assembly (50) enters into the corresponding slot row (35) of the second fin group (42). The assembly (50) is then pressed further downward by the pressing member (65). As a result, as shown in Fig. 18, each flat tube (20) of the assembly (50) enters into the corresponding slot row (35) of the second fin group (42), and the assembly (50) is combined with the second fin group (42). In this way, a core (15) is formed that is composed of the flat tube (20), the first fin group (41), and the second fin group.
[0079] -Features of the embodiment (1)- In the manufacturing method of the heat exchanger (10) of this embodiment, a first step and a second step are performed. In the first step, the first fin group (41) and the flat tubes (20) are combined to form an assembly (50). In the second step, the second fin group (42) is arranged in a position where the open ends (33) of the slots (32) face upward, and the assembly (50) is arranged in a position where the flat tubes (20) are located on the lower side. In the second step, the flat tubes (20) of the assembly (50) are inserted from above into the slots (32) of the fins (30) that constitute the second fin group (42). As a result, the flat tubes (20), the first fin group (41), and the second fin group (42) are combined.
[0080] In the first step of the manufacturing method of this embodiment, the flat tubes (20) are inserted from above into the slots (32) of the fins (30) constituting the first fin group (41). Therefore, the fins (30) of the first fin group (41) arranged as shown in Fig. 5 can be placed on a stable platform member, for example, and the flat tubes (20) can be inserted into each slot row (35) of the first fin group (41) in that state. Therefore, when combining the first fin group (41) and the flat tubes (20), the fins (30) of the first fin group (41) can be reliably kept in an aligned position, and the flat tubes (20) can be easily inserted into each slot row (35) of the first fin group (41).
[0081] -Features of the embodiment (2)- The assembled body 50 formed in the first step of the manufacturing method of this embodiment is in an orientation in which the flat tubes 20 are located on the upper side. In the manufacturing method of this embodiment, an inversion step is performed to invert the assembled body 50 to an orientation in which the flat tubes 20 are located on the lower side, and then a second step is performed.
[0082] In the second step, the assembly (50) in an orientation in which the flat tubes (20) are located on the lower side is pressed down by a pressing member (65), thereby inserting the flat tubes (20) of the assembly (50) into the slot row (35) of the second fin group (42). In this second step, the fins (30) of the second fin group (42) arranged as shown in Fig. 5 are placed on a stable base member (60), and the flat tubes (20) of the assembly (50) are inserted from above into the slot row (35) of the second fin group (42) in this state.
[0083] Therefore, when combining the assembly (50) and the second fin group (42), each fin (30) of the second fin group (42) can be reliably maintained in an aligned position, and the flat tube (20) can be easily inserted into each slot row (35) of the second fin group (42).
[0084] -Features of the embodiment (3)- In a second step of the manufacturing method of this embodiment, a straightening step is performed to straighten the deflection of the assembly (50), and the assembly (50) in a straightened state is combined with the second fin group (42).
[0085] Here, when the assembly 50 is bent, the relative positions of the flat tubes 20 constituting the assembly 50 change from the correct positions when the assembly 50 is not bent. Therefore, when the assembly 50 is bent, the flat tubes 20 of the assembly 50 cannot be accurately positioned above the corresponding slot rows 35 of the second fin group 42. Therefore, when the bent assembly 50 is combined with the second fin group 42, the flat tubes 20 of the assembly 50 are not inserted straight from above into the corresponding slot rows 35 of the second fin group 42, and the fins 30 of the second fin group 42 may be crushed by the flat tubes 20.
[0086] In contrast, in the second step of the manufacturing method of this embodiment, the assembly (50) in a state where the deflection has been corrected is combined with the second fin group (42). Therefore, the flat tubes (20) of the assembly (50) can be inserted straight from above into the corresponding slot rows (35) of the second fin group (42). Therefore, according to the manufacturing method of this embodiment, it is possible to reduce the possibility that the fins (30) of the second fin group (42) will be crushed by the flat tubes (20) when combining the assembly (50) with the second fin group (42).
[0087] In particular, in the straightening step of the manufacturing method of this embodiment, the horizontal deflection of the assembly (50) in the position where the flat tubes (20) are located on the lower side is straightened in the first straightening step, and the vertical deflection of the assembly (50) in the position where the flat tubes (20) are located on the lower side is straightened in the second straightening step. Therefore, in the second step of the manufacturing method of this embodiment, the assembly (50) in which both the horizontal deflection and the vertical deflection have been corrected can be combined with the second fin group (42). Therefore, according to this embodiment, it is possible to reliably reduce the possibility that the fins (30) of the second fin group (42) will be crushed by the flat tubes (20) when combining the assembly (50) with the second fin group (42).
[0088] -Modifications of the embodiment- The manufacturing method of the heat exchanger (10) of this embodiment can be modified as follows.
[0089] First Modified Example As shown in Fig. 19, the pressing member (65) used in the second step may include a plurality of pressing blocks (67). The pressing member (65) shown in Fig. 19 includes two pressing blocks (67). The lower surface of each of the two pressing blocks (67) forms a flat pressing surface (66). The two pressing blocks (67) are arranged side by side in the arrangement direction of the flat tubes (20) in the assembly (50) (the left-right direction in Fig. 19).
[0090] The pressing surface (66) of the pressing member (65) is larger than the heat exchanger (10) to be manufactured. Therefore, when a pressing member (65) made of a single member is used to manufacture a large heat exchanger (10), the rigidity of the large pressing member (65) needs to be ensured, which may increase the weight of the pressing member (65). Therefore, by forming the pressing member (65) from a plurality of pressing blocks (67) as in this modified example, the rigidity of each pressing block (67) can be ensured while the weight of each pressing block (67) can be reduced, thereby reducing the weight of the entire pressing member (65).
[0091] <Second Modification> As shown in Fig. 20, in the second straightening step, the assembly (50) may be pressed against the pressing member (65) by a third clamping member (73), a fourth clamping member (74), and an intermediate support member (75). The intermediate support member (75) is a member extending in a direction perpendicular to the extension direction (front-rear direction in Fig. 20) of the flat tubes (20) constituting the assembly (50). The intermediate support member (75) abuts against the center of the extension direction of the flat tubes (20) constituting the assembly (50). The intermediate support member (75) moves upward in conjunction with the third clamping member (73) and the fourth clamping member (74), and lifts the assembly (50) together with the third clamping member (73) and the fourth clamping member (74).
[0092] When the flat tubes (20) are long, there is a risk that the flat tubes (20) will bend to a non-negligible extent when the assembly (50) is arranged with the flat tubes (20) positioned on the lower side. In this case, if the ends of the flat tubes (20) are supported by the third clamping member (73) and the fourth clamping member (74) and the central portion of the flat tubes (20) in the extension direction is supported by the intermediate support member (75), the flat tubes (20) can be straightened in the second straightening step. As a result, even when the flat tubes (20) are long, the bending in the vertical direction of the assembly (50) arranged with the flat tubes (20) positioned on the lower side can be reliably straightened.
[0093] <Third Modification> In the second step, the second fin group (42) arranged below the assembly (50) may be moved upward to insert the flat tube (20) of the assembly (50) into the slot row (35) of the second fin group (42). In the second step, the assembly (50) may be moved downward and the second fin group (42) may be moved upward at the same time to insert the flat tube (20) of the assembly (50) into the slot row (35) of the second fin group (42). In this manner, in the second step of the present embodiment, the assembly (50) and the second fin group (42) arranged below the assembly (50) are brought relatively close to each other, so that the flat tube (20) of the assembly (50) is inserted into the slot row (35) of the second fin group (42).
[0094] Although the embodiments and modifications have been described above, it will be understood that various modifications of form and details are possible without departing from the spirit and scope of the claims. In addition, the elements of the above embodiments, modifications, and other embodiments may be appropriately combined or substituted. In addition, the descriptions "first," "second," "third," etc. in the specification and claims are used to distinguish the words to which these descriptions are attached, and do not limit the number or order of the words. [Industrial Applicability]
[0095] INDUSTRIAL APPLICABILITY As described above, the present disclosure is useful for a method for manufacturing a heat exchanger. [Explanation of symbols]
[0096] 10 Heat exchanger 20 flat tube 30 Finn 32 Slots 33 Open end 41 First Fin Group 42 2nd Fin Group 50 assembly 65 Pressing member 66 Pressing surface 67 Pressing block
Claims
1. A method for manufacturing a heat exchanger (10) comprising a plurality of flat tubes (20), and a first fin group (41) and a second fin group (42), each of which is composed of a plurality of plate-like fins (30), wherein a plurality of slots (32) having open ends (33) are formed in each of the plurality of fins (30) at an outer edge of the fin (30), and each of the plurality of flat tubes (20) is inserted into the slots (32) of each of the fins (30) constituting the first fin group (41) and the slots (32) of each of the fins (30) constituting the second fin group (42), a first step of inserting the flat tubes (20) into the slots (32) of the fins (30) constituting the first fin group (41) to form an assembly (50) consisting of the first fin group (41) and a plurality of the flat tubes (20); and a second step of arranging the second fin group (42) in a position where the open ends (33) of the slots (32) of the fins (30) constituting the second fin group (42) are positioned on an upper side, arranging the assembly (50) in a position where the flat tubes (20) are positioned on a lower side, and inserting the flat tubes (20) of the assembly (50) from above into the slots (32) of the fins (30) constituting the second fin group (42). A method for manufacturing a heat exchanger.
2. In the first step, the first fin group (41) is arranged in such a position that the open ends (33) of the slots (32) of the fins (30) constituting the first fin group (41) are positioned on the upper side, and the flat tubes (20) are inserted from above into the slots (32) of the fins (30) constituting the first fin group (41); An inversion step is performed before the second step, in which the assembly (50) formed in the first step is inverted from a position in which the flat tubes (20) are located at the upper side to a position in which the flat tubes (20) are located at the lower side. A method for manufacturing the heat exchanger according to claim 1.
3. In the second step, a pressing member (65) having a flat pressing surface (66) on the lower surface is used, and the pressing surface (66) of the pressing member (65) is brought into contact with the upper outer edges of the fins (30) of the assembly (50) arranged in a position in which the flat tubes (20) are located on the lower side, and the assembly (50) is pressed down by the pressing member (65), thereby inserting the flat tubes (20) of the assembly (50) from above into the slots (32) of the fins (30) that constitute the second fin group (42). A method for manufacturing the heat exchanger according to claim 1 or 2.
4. The pressing member (65) used in the second step includes a plurality of pressing blocks (67), the lower surface of each of which constitutes the pressing surface (66). A method for manufacturing the heat exchanger according to claim 3.
5. The second step includes a straightening step of straightening deflection of the assembly (50) arranged in an orientation in which the flat tube (20) is located on the lower side, In the second step, the flat tubes (20) of the assembly (50) in a state where the deflection has been corrected are inserted from above into the slots (32) of the fins (30) constituting the second fin group (42). A method for manufacturing the heat exchanger according to claim 1 or 2.
6. The straightening step includes a first straightening step of straightening the horizontal deflection of the assembly (50) by clamping the assembly (50) from the horizontal direction. A method for manufacturing the heat exchanger according to claim 5.
7. In the first straightening step, the assembly (50) is sandwiched from both sides in the arrangement direction of the flat tubes (20) and from both sides in the arrangement direction of the fins (30). A method for manufacturing the heat exchanger according to claim 6.
8. In the second step, a pressing member (65) having a flat pressing surface (66) on the lower surface is used, and the pressing surface (66) of the pressing member (65) is brought into contact with the upper outer edges of the fins (30) of the assembly (50) arranged in a position in which the flat tubes (20) are located on the lower side, and the assembly (50) is pressed down by the pressing member (65), thereby inserting the flat tubes (20) of the assembly (50) from above into the slots (32) of the fins (30) that constitute the second fin group (42), The straightening step includes a second straightening step of straightening the deflection of the assembly (50) in the vertical direction by pressing the assembly (50) against the pressing surface (66) of the pressing member (65). A method for manufacturing the heat exchanger according to claim 5.
9. In the second straightening step, both ends of the flat tube (20) in the assembly (50) are lifted to press the assembly (50) against the pressing surface (66) of the pressing member (65). A method for manufacturing the heat exchanger according to claim 8.
10. In the second straightening step, both ends of the flat tube (20) in the assembly (50) and a middle portion of the flat tube (20) in the extension direction are lifted, thereby pressing the assembly (50) against the pressing surface (66) of the pressing member (65). A method for manufacturing the heat exchanger according to claim 8.
Citation Information
Patent Citations
Micro-channel heat exchanger and air conditioner
CN112444146A
A heat transfer component that is arranged in low temperature waste heat from flue gas to retrieve and utilize
CN205748069U
Fin tube type heat exchanger, its manufacturing method, and refrigeration air conditioner
JP2003262485A
Heat exchanger, and heat pump device
JP2013221713A
Heat exchanger core assembly device
JP2020169734A