Boxing joint with excellent fatigue life and boxing method

The rotary welding method stabilizes weld joints by ensuring a minimum 5 mm overlap and 5-50 mm tip distance, addressing stress concentration and enhancing fatigue strength in steel structures.

JP2024151810AActive Publication Date: 2024-10-25JFE STEEL CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023065532
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-13
Publication Date
2024-10-25
Estimated Expiration
2043-04-13

AI Technical Summary

Technical Problem

Existing rotary welding techniques for steel structures, such as steel bridges and ships, suffer from fatigue cracks due to stress concentration at weld toes, which are exacerbated by welding gaps and variations in weld bead lengths, leading to reduced fatigue strength and potential structural failure.

Method used

A rotary welding method where the short side weld bead starts from the long side, overlaps, and extends onto the main plate, ensuring a minimum overlap length of 5 mm and a distance of 5 mm to 50 mm between the weld toe tips, with a spacing of 2 mm or more between extended portions, to stabilize the weld joint.

Benefits of technology

This method enhances fatigue strength by reducing stress concentration, even with variations in weld bead lengths, providing a stable and cost-effective solution for improving the durability of steel structures.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024151810000001_ABST
    Figure 2024151810000001_ABST
Patent Text Reader

Abstract

To provide a boxing joint having fatigue strength which can be stably and inexpensively improved even if short bead occurs, considering actual welding work, and a boxing method.SOLUTION: A boxing joint is provided which is obtained by boxing a gusset 2 to a main plate 1, the boxing joint has a first weld bead 3 and a second weld bead 4. The first weld bead is formed along the other long side via from one long side to a short side of a rectangular contact surface 2a where the gusset contacts the main plate, and the second weld bead has a long side weld portion 9, an overlapped portion 5 and an extending portion 6. The long side weld portion is formed along the long side of the rectangular contact surface, the overlapped portion is formed by covering a weld portion of the first weld bead, and the extending portion is formed by being drawn from the overlapped portion onto the main plate. A length L from a distal end of the first weld bead to the short side of the rectangular contact surface is 5 mm or more.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a boxing welding technique between a main plate and a gusset, which is widely adopted when constructing steel structures, and in particular to a boxing welded joint and a boxing welding method suitable for steel structures (e.g., steel bridges, ships, etc.) that require excellent fatigue properties. [Background technology]

[0002] Generally, in steel structures, there are many boxing welded joints in which the periphery of the gusset is welded to the main plate (so-called "boxing weld"). In boxing welded joints, the weld bead surrounds the gusset, and if the weld bead has a defect (e.g., a crack, etc.) and the shape of the weld toe is not smoothly formed, stress concentration is likely to occur at the weld toe. As a result, the welding residual stress caused by the boxing weld and the repeated stress caused by the external force are superimposed to generate fatigue cracks, which further propagate and cause fatigue failure. Note that the external force is a load that repeatedly acts on the steel structure from the outside. For example, if the steel structure is a steel bridge, it is a load that repeatedly occurs due to natural weather conditions (e.g., wind, etc.) and vehicle traffic, and if the steel structure is a ship, it is a load that repeatedly occurs due to wind and waves.

[0003] In recent years, reports of fatigue-induced damage have been increasing as steel structures age. To prevent such damage, it is necessary to inspect steel structures periodically to manage the progress of the damage and to take measures according to the progress of the damage. In particular, when fatigue-induced damage occurs in steel bridges, it is possible to reduce the external forces acting on the steel bridge by restricting vehicle traffic, but this causes traffic congestion and delays in logistics, which has a significant negative impact on social activities. Therefore, technology to improve the fatigue properties of boxing welded joints in steel structures is being studied.

[0004] For example, Patent Document 1 discloses a technique for stably increasing joint fatigue strength by fillet-welding the long side of a rectangular abutment surface (hereinafter also referred to as a "rectangular abutment surface") where a gusset abuts against a main plate to the main plate, cooling to room temperature, and then turning and welding the short side from the corner of the rectangular abutment surface. In this technique, a weld bead formed along the short side of the rectangular abutment surface (hereinafter also referred to as a "short side weld bead") is placed over a weld bead formed along the long side (hereinafter also referred to as a "long side weld bead"), and the short side weld bead extends over the long side weld bead onto the main plate. In this way, if the long side weld bead is first welded and then the short side weld bead is placed over it and welded, a gap (i.e., a space surrounded by the main plate, the long side weld bead, and the short side weld bead) is likely to occur at the location where the weld beads overlap. As a result, fatigue cracks due to stress concentration easily occur, and it is difficult to prevent the fatigue cracks from propagating. In other words, with the technology disclosed in Patent Document 1, a significant improvement in the fatigue strength of boxing welded joints cannot be expected.

[0005] In response to this, Patent Document 2 discloses a technique for preventing the occurrence of the above-mentioned gap by using a normal welding device and welding material in order to suppress an increase in the construction cost of box welding. In this technique, first, a short side weld bead (first weld bead) is welded in a straight line parallel to the short side, and then long side weld beads (second and third weld beads) are welded to cover the short side weld bead with a long side weld bead. At this time, welding is performed so that the long side weld bead extends beyond the short side weld bead already welded. This prevents the occurrence of the above-mentioned gap, and thus prevents the occurrence of fatigue cracks regardless of the shape of the weld toe. Furthermore, it is described that the occurrence of the above-mentioned gap is more significantly prevented by welding the short side weld bead so that it does not exceed the long side weld bead. Here, the reason for welding the short side weld bead so that it does not exceed the long side weld bead is that if the short side weld bead is too long and extends from the underside of the two long side weld beads onto the main plate, the above-mentioned gap is likely to occur, and fatigue cracks are likely to occur. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] Japanese Patent Application Publication No. 8-19860 [Patent Document 2] JP 2018-158380 A Summary of the Invention [Problem to be solved by the invention]

[0007] However, when considering actual welding, performing welding so that the short side weld bead does not exceed the long side weld bead according to the technique of Patent Document 2 may cause problems in welding management. In other words, in actual welding, the end position of the short side weld bead formed in a straight line parallel to the short side may vary due to differences in the skills of the worker and the performance of the welding machine, resulting in a phenomenon in which the actual length of the short side weld bead is shorter than the target length by about 5 mm to 10 mm. This phenomenon is called a short bead of the short side weld bead. In this case, if a gap (a gap of 10% or more compared to the bead width of the long side weld bead) occurs in the portion where the short side weld bead overlaps with the long side weld bead, there is a problem that stress concentration occurs due to bead discontinuity, and fatigue strength decreases.

[0008] In view of the above circumstances, the present invention takes into consideration actual welding construction and has an object to provide a boxing welded joint and a boxing welding method that can inexpensively and stably improve fatigue strength even if short beads occur. [Means for solving the problem]

[0009] The present inventors have conducted extensive research to solve the above problems. As a result, they have found that if the short side weld bead is not formed in a straight line parallel to the short side, but starts from the long side, passes through the short side, and ends on the opposite long side, excellent fatigue strength can be obtained regardless of whether or not short beads are generated in the short side weld bead. Furthermore, they have found that if the length of the overlapping portion between the long side weld bead that covers the long side of the short side weld bead and the short side weld bead is 5 mm or more, it is effective in improving fatigue strength.

[0010] The present invention was made based on the above findings and further studies, and the gist of the present invention is as follows. [1] A boxing welded joint obtained by joining a gusset to a main plate by boxing welding, The weld joint has a first weld bead and a second weld bead; The first weld bead is formed along one long side, via one short side, and along the other long side of a rectangular abutment surface where the gusset abuts against the main plate, The second weld bead has a long side weld portion, an overlap portion, and an extension portion; The long side weld is formed along a long side of the rectangular abutment surface, The overlapping portion is formed by covering a welded portion of the first weld bead, The extension portion is formed by extending from the overlap portion onto the main plate, The length L1 from the welding start end of the first weld bead to the short side of the rectangular abutment surface is 5 mm or more, The length L2 from the short side of the rectangular contact surface to the welding end portion of the first weld bead is 5 mm or more. A turn weld joint characterized by: [2] The box weld joint according to [1], characterized in that the first weld beads and the second weld beads each have two. [3] In the above [1] or [2], The length N (N1, N2) between the tip of the extension and the short side toe of the rectangular abutment surface of the first weld bead is 5 mm to 50 mm, The distance M between the ends of the extension is 2 mm or more. A turn weld joint characterized by: [4] In any one of [1] to [3], the plate thickness T of the main plate S A box welded joint, characterized in that the gap is 5mm to 20mm. [5] In any one of [1] to [4], the length T of the short side of the rectangular contact surface G A box welded joint, characterized in that the gap is 5mm to 20mm. [6] In a turn welding method for joining a gusset to a main plate by turn welding, a first weld bead is formed along one long side, via one short side, and along the other long side of a rectangular abutment surface where the gusset abuts against the main plate; Next, a second weld bead is formed, the second weld bead having a long side weld portion formed along a long side of the rectangular abutment surface, an overlap portion formed by covering the weld portion of the first weld bead, and an extension portion formed by extending from the overlap portion onto the main plate; A length L1 from a welding start end of the first weld bead to a short side of the rectangular abutment surface is set to 5 mm or more, The length L2 from the short side of the rectangular contact surface to the welding end portion of the first weld bead is set to 5 mm or more. A method of turning welding. [7] The method of turning welding according to [6], characterized in that the first weld beads are formed in two on both short side sides of the rectangular abutment surface, and then the second weld beads are formed in two on both long side sides of the rectangular abutment surface. [8] In the above [6] or [7], the length N (N1, N2) between the tip of the extension and the short side toe of the rectangular abutment surface of the first weld bead is set to 5 mm to 50 mm, The distance M between the ends of the extension is 2 mm or more. A method of turning welding. [9] In any one of [6] to [8], the plate thickness T of the main plate S The present invention relates to a turn welding method, and

[10] In any one of [6] to [9], the length T of the short side of the rectangular contact surface G The present invention relates to a turn welding method, and Effect of the Invention

[0011] According to the present invention, when a steel structure is newly constructed or an aging steel structure is repaired, even if a short bead of a short side weld bead occurs during boxing, it is possible to inexpensively and stably improve the fatigue strength of a boxing welded joint, which is of great industrial benefit. [Brief description of the drawings]

[0012] [Figure 1] FIG. 1 is a perspective view showing a schematic example of a box welded joint according to the present invention. [Diagram 2] 1 is a plan view showing a schematic example of a procedure for performing a rotation welding method according to the present invention; FIG. [Diagram 3] FIG. 3 is an enlarged schematic plan view of FIG. 2(c). DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] Representative embodiments of the box welded joint and box welding method according to the present invention will be described in detail below with reference to the drawings, but the present invention is not limited to these. In addition, since the drawings are intended to conceptually explain the present invention, the dimensions of each member shown and their ratios may differ from the actual ones.

[0014] Fig. 1 is a perspective view showing an example of a box welded joint according to the present invention, Fig. 2 is a plan view showing an example of a procedure for a box welding method for obtaining the box welded joint, and Fig. 3 is an enlarged view of Fig. 2(c). In Fig. 2, the rectangular contact surface 2a where the gusset 2 contacts the main plate 1 coincides with the shape surrounded by a rectangular line obtained by projecting the gusset 2 onto the main plate 1, and is composed of a long side 2b and a short side 2c. Figs. 2 and 3 show the box welded joint and the procedure for the box welding method on one short side of the rectangular contact surface 2a.

[0015] [Swivel weld joint] The boxing weld joint according to the present invention has a first weld bead 3 and a second weld bead 4. Preferably, it has two first weld beads 3 and 3' and two second weld beads 4a and 4b.

[0016] The first weld bead 3 is formed from one long side, via one short side, to the other long side of the rectangular contact surface 2a where the gusset 2 contacts the main plate 1. The first weld bead 3' is symmetrical to the first weld bead 3, and is formed from one long side, via the other short side, to the other long side of the rectangular contact surface 2a.

[0017] Next, the second weld bead 4 (4a, 4b) is formed along the long side of the rectangular abutment surface 2a, and is continuously covered with the two first weld beads 3 and 3', and is further extended onto the main plate 1. Therefore, it has a long side weld portion 9 (9a, 9b), an overlap portion 5 (5a, 5b), and an extension portion 6 (6a, 6b). The long side weld portion 9 (9a, 9b) is formed along the long side 2b of the rectangular abutment surface 2a. The overlap portion 5 (5a, 5b) is formed by covering the long side 2b portion of the rectangular abutment surface 2a of the first weld beads 3 and 3'. The extension portion 6 (6a, 6b) is formed by extending from the overlap portion 5 (5a, 5b) onto the main plate 1.

[0018] It is preferable that long side welds 9 (9a, 9b) are formed continuously at first weld beads 3 and 3', but they may be interrupted midway. When first weld bead 3 is formed only on one short side of rectangular abutting surface 2a, second weld bead 4a is formed from the middle of the long side of rectangular abutting surface 2a so as to cover weld start end 10a of first weld bead 3. Similarly, second weld bead 4b is formed from the middle of the other long side of rectangular abutting surface 2a so as to cover weld end end 10b of first weld bead 3.

[0019] Here, the length L of the overlapping portion 5 (5a, 5b), that is, the length L1 from the welding start end 10a of the first weld bead 3, 3' to the short side 2c of the rectangular abutting surface 2a and the length L2 from the short side 2c of the rectangular abutting surface 2a to the welding end end 10b of the first weld bead 3, 3', may be 5 mm or more. If the lengths L1 and L2 are less than 5 mm, the fatigue strength may decrease regardless of whether or not a short bead is generated. Note that if the length L exceeds 20 mm, the number of unnecessary welding steps for forming the first weld bead increases, so it is preferable to set it to 5 mm to 20 mm. More preferably, it is 10 mm to 15 mm.

[0020] Furthermore, the length N (N1, N2) between the tip 7 (7a, 7b) of the extension 6 (6a, 6b) of the second weld bead 4 (4a, 4b) and the short side toe 3a of the rectangular abutment surface 2a of the first weld bead 3, 3' is preferably in the range of 5 mm to 50 mm. If it is less than 5 mm, there is no effect of improving fatigue strength, and if it exceeds 50 mm, construction takes a long time. More preferably, it is 10 mm to 20 mm.

[0021] Furthermore, the distance M between the toes of the extensions 6 of the second weld beads 4 (4a, 4b), i.e., the width of the space surrounded by the extensions 6a and 6b, is preferably 2 mm or more. If it is less than 2 mm, the beads are likely to be connected to each other, and the fatigue strength improvement effect is not achieved. More preferably, it is 5 mm to 10 mm.

[0022] Next, the plate thickness T of the main plate in the present invention S Although there is no limitation, it is preferable that the thickness is 5 mm to 20 mm.

[0023] In addition, the thickness of the gusset in the present invention, i.e., the length T of the short side of the rectangular contact surface G is not particularly limited, but is preferably 5 mm to 20 mm from the viewpoint of improving fatigue properties. G If the distance is less than 5 mm, it is difficult to perform the second weld bead construction with a distance M of 0 mm or more, while if the distance exceeds 20 mm, it is disadvantageous in terms of the effect of improving fatigue properties.

[0024] [Wheel welding method (construction procedure)] Next, a procedure for performing the box welding method for obtaining a box welded joint according to the present invention will be described with reference to FIG.

[0025] 2(a), a first weld bead 3 is formed from the middle of one long side 2b of a rectangular contact surface 2a with which a gusset 2 on a main plate 1 contacts, via one short side 2c, along the other long side 2b, using a welding method and welding conditions described below. The long side from which welding begins when forming this first weld bead 3 may be any of the long sides.

[0026] Here, the welding start point of the first weld bead 3 may be a place where the length L1 from the welding start end 10a of the first weld bead 3 to the short side 2c of the rectangular abutting surface 2a is 5 mm or more. Also, the welding end point of the first weld bead 3 may be a place where the length L2 from the short side 2c of the rectangular abutting surface 2a to the welding end end 10b of the first weld bead 3 is 5 mm or more. As described above, if the lengths L1 and L2 are less than 5 mm, the fatigue strength may decrease regardless of whether or not a short bead is generated. If the lengths L1 and L2 exceed 20 mm, the number of unnecessary welding steps for forming the first weld bead increases, so the lengths L1 and L2 are preferably 5 mm to 20 mm. More preferably, they are 10 mm to 15 mm. It is not necessary to make the lengths L1 and L2 the same, and the same effect can be obtained if each length is 5 mm or more.

[0027] Next, when forming a second first weld bead 3' on the other short side that is symmetrical to the short side on which the above-mentioned first weld bead 3 is formed, as shown in FIG. 1, it is preferable to form the first first weld bead 3 and then form the second bead in the same procedure as the first one.

[0028] Next, as shown in Fig. 2(b), a second weld bead 4a is formed along one long side 2b of the rectangular abutting surface 2a, covering the weld bead on the long side 2b side of the first weld bead 3, and further extending onto the main plate. This second weld bead 4a is preferably formed by continuously covering the first first weld bead 3 formed on one short side of the rectangular abutting surface and the second first weld bead 3' formed on the other short side. The formed second weld bead 4a has a long side weld portion 9a that is on the long side of the rectangular abutting surface and does not cover the first weld beads 3 and 3', an overlap portion 5a that covers the first weld bead 3, and an extension portion 6a that extends onto the main plate 1.

[0029] Here, the length N1 between the tip 7a of the extension 6a of the second weld bead 4a and the short side toe 3a of the rectangular abutting surface 2a of the first weld bead 3 is preferably in the range of 5 mm to 50 mm. If it is less than 5 mm, there is no effect of improving fatigue strength, and if it exceeds 50 mm, a long period of time is required for construction. More preferably, it is 10 mm to 20 mm.

[0030] Finally, as shown in FIG. 2(c), the second weld bead 4b is formed along the other long side 2b of the rectangular abutment surface 2a, covering the weld bead on the long side 2b side of the first weld bead 3, and further extending onto the main plate. This second weld bead 4b is also formed with a long side weld portion 9b, an overlap portion 5b, and an extension portion 6b, similar to the first second weld bead 4a. Furthermore, the interval M (the interval between the toes of the extension portions), which is the width of the space surrounded by the extension portions 6a and 6b of the second weld beads 4a and 4b, is preferably 2 mm or more. If it is less than 2 mm, the beads are likely to be connected to each other, and the fatigue strength improvement effect is not achieved. More preferably, it is 5 mm to 10 mm.

[0031] It is preferable that long side welds 9 (9a, 9b) are formed continuously on first weld beads 3 and 3', but they may be interrupted midway. When first weld bead 3 is formed only on one short side of rectangular abutting surface 2a, second weld bead 4a is formed from the middle of the long side of rectangular abutting surface 2a so as to cover weld start end 10a of first weld bead 3. Similarly, second weld bead 4b is formed from the middle of the other long side of rectangular abutting surface 2a so as to cover weld end end 10b of first weld bead 3.

[0032] In the above description, second weld bead 4a is formed first, and then second weld bead 4b is formed, but which is formed first or last is not particularly limited.

[0033] Furthermore, when forming the second weld bead, if two weld beads are formed, it is not necessary for the lengths and shapes of the above-mentioned portions to be the same for both beads.

[0034] [Welding method and welding object] The welding means for performing the rotational welding are mainly the shielded metal arc welding method and the gas metal arc welding method, but other means can also be used as appropriate, and either manual welding or automatic welding can be adopted.

[0035] The present invention can be applied not only to the construction of new steel structures, but also to the reinforcement and repair of deteriorated steel structures.

[0036] [Fatigue resistance properties] The present invention is effective regardless of the material of the main plate and gusset used to construct the steel structure. Examples of the material for the main plate include steel types such as SM400, SM490, SM520, and SM570, and materials with a yield stress of 245 MPa to 560 MPa. EXAMPLES

[0037] The present invention will be further described below with reference to examples. However, the following examples are merely intended to illustrate and explain the present invention in more detail, and are not intended to limit the scope of the present invention.

[0038] Main plate (thickness T S : 14mm, plate width: 80mm, length: 500mm) with gusset (plate thickness T G The test pieces (diameter: 14 mm, plate width: 75 mm, height: 50 mm) were box-welded by gas metal arc welding using a flux-cored wire, and fatigue tests were conducted on the box-welded joints obtained. The procedure is described below.

[0039] For the main plate and gusset, steel plates having the chemical composition (mass%) shown in Table 1 were used. Tensile test pieces (parallel part diameter 6 mmΦ) were taken from the steel plates in accordance with the provisions of JIS Z 2241, and tensile tests were carried out to measure the yield stress (MPa) and tensile strength (MPa).

[0040] [Table 1]

[0041] The flux-cored wire used was MX-Z200 (wire diameter: 1.2 mmφ) manufactured by Kobe Steel, Ltd., a material conforming to JIS Z 3313. The composition of the wire (mass %) was as follows: C: 0.04%, Si: 0.07%, Mn: 1.22%, P: 0.010%, S: 0.011%, the balance being Fe and unavoidable impurities.

[0042] The welding conditions for gas metal arc welding were welding current: 240A, welding voltage: 32V, welding speed: 30cm / min, and the leg length was targeted to be about 8mm for both the first and second weld beads. Note that the gusset was placed in the center of the main plate, so the rectangular contact surface was located in the center of the main plate.

[0043] The fatigue tests were carried out at room temperature and in air under axial load control, stress ratio of 0.1, and frequency of 10 Hz.

[0044] For the obtained boxing welded joints, the measured bead spacing (L1, L2, N1, N2, M), the stress range as the fatigue test conditions, and the fatigue test results are shown in Table 2. Here, the fatigue life is expressed as the number of load repetitions (cycles) until fatigue fracture.

[0045] [Table 2]

[0046] As is clear from Table 2, all of the examples of the present invention had lengths L1 and L2 of 5 mm or more and had good fatigue lives, whereas all of the comparative examples had lengths L1 and L2 of less than 5 mm or both and had fatigue lives that were half or less than those of the examples of the present invention. [Explanation of symbols]

[0047] 1 Main plate 2 Gusset 2a: rectangular contact surface; 2b: long side of rectangular contact surface; 2c: short side of rectangular contact surface 3, 3' First weld bead 3a Toe of the short side of the first weld bead 4(4a, 4b) Second weld bead 5 (5a, 5b) Second weld bead overlap 6 (6a, 6b) Extension of second weld bead 7 (7a, 7b) Tip of extension of second weld bead 9 (9a, 9b) Long side weld of second weld bead 10a Weld start end of first weld bead 10b Weld end of first weld bead L (L1, L2) Length from the tip of the first weld bead to the short side of the rectangular contact surface M Spacing between extensions N (N1, N2) Length from the short side toe of the first weld bead to the tip of the extension

Claims

1. A box weld joint obtained by joining a gusset to a main plate by box welding, The turn weld joint has a first weld bead and a second weld bead; The first weld bead is formed along one long side, via one short side, and along the other long side of a rectangular abutment surface where the gusset abuts against the main plate, the second weld bead has a long side weld portion, an overlap portion, and an extension portion; The long side weld is formed along a long side of the rectangular abutment surface, The overlapping portion is formed to cover a welded portion of the first weld bead, The extension portion is formed by extending from the overlap portion onto the main plate, A length L1 from a welding start end of the first weld bead to a short side of the rectangular abutment surface is 5 mm or more, A length L2 from a short side of the rectangular contact surface to a welding end portion of the first weld bead is 5 mm or more. A turn weld joint characterized by:

2. The weld joint according to claim 1 , wherein each of the first weld beads and the second weld beads has two beads.

3. a length N (N1, N2) between the tip of the extension portion and a short side toe of the rectangular abutment surface of the first weld bead is 5 mm to 50 mm; The distance M between the ends of the extension is 2 mm or more.

3. The box weld joint according to claim 1 or 2.

4. The thickness T of the main plate S The box welded joint according to claim 3, characterized in that the distance is 5 mm to 20 mm.

5. The length T of the short side of the rectangular contact surface G The box welded joint according to claim 4, characterized in that the gap is 5 mm to 20 mm.

6. In a turn welding method for joining a gusset to a main plate by turn welding, a first weld bead is formed along one long side, via one short side, and along the other long side of a rectangular abutment surface where the gusset abuts against the main plate; Next, a second weld bead is formed, the second weld bead having a long side weld portion formed along a long side of the rectangular abutment surface, an overlap portion formed by covering the weld portion of the first weld bead, and an extension portion formed by extending from the overlap portion onto the main plate; A length L1 from a welding start end of the first weld bead to a short side of the rectangular abutment surface is set to 5 mm or more, The length L2 from the short side of the rectangular contact surface to the welding end portion of the first weld bead is set to 5 mm or more. A method of turning welding.

7. The turn welding method according to claim 6, characterized in that after the first weld beads are formed in two on both short side sides of the rectangular abutment surface, the second weld beads are formed in two on both long side sides of the rectangular abutment surface.

8. a length N (N1, N2) between a tip end of the extension portion and a short side toe of the rectangular abutment surface of the first weld bead is set to 5 mm to 50 mm; The distance M between the toes of the extension is 2 mm or more.

8. The box welding method according to claim 6 or 7.

9. The thickness T of the main plate S The method for turning welding according to claim 8, characterized in that the distance is 5 mm to 20 mm.

10. The length T of the short side of the rectangular contact surface G The method for turning welding according to claim 9, characterized in that the distance is 5 mm to 20 mm.

Citation Information

Patent Citations

  • Welding method and weld joint

    JP2013099764A

  • Boxing joint and boxing method excellent in fatigue strength

    JP2018158380A

  • Turning weld joint with excellent fatigue strength and turning welding method

    JP2022188324A

  • Method for welding boxing welding joint of construction steel

    JP1996019860A