Wiring board, manufacturing method for wiring board, and semiconductor device

The wiring board design with a laminated reinforcing structure and penetrating connections balances thermal expansion stresses, preventing delamination and improving structural integrity.

JP2024152487AInactive Publication Date: 2024-10-25TOPPAN HOLDINGS INC
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023066712
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-14
Publication Date
2024-10-25
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing wiring boards in multilayer structures face issues with delamination due to differences in thermal expansion coefficients and rigidity between reinforcing members and resins, leading to stress and warpage, which are not adequately addressed by current technologies.

Method used

A wiring board design incorporating a laminated structure with a first and second reinforcing layer, a penetrating structure connecting both layers, and pad portions at both ends of the penetrating portion, which balances stress and prevents delamination by distributing thermal expansion forces.

Benefits of technology

The design effectively reduces stress and prevents delamination across the interface of the wiring board, enhancing its structural integrity and reliability under temperature changes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024152487000001_ABST
    Figure 2024152487000001_ABST
Patent Text Reader

Abstract

To provide a multilayer wiring board in which the stress on the board can be relaxed regardless of the inside or the outside of the wiring board.SOLUTION: One of typical wiring boards according to the present invention is a wiring board including a wiring layer having a first surface and a second surface, a first reinforcement layer having a third surface and a fourth surface, and a second reinforcement layer having a fifth surface and a sixth surface. In the wiring board, the fourth surface of the first reinforcement layer and the first surface of the wiring layer are in contact with each other, and the fifth surface of the second reinforcement layer and the second surface of the wiring layer are in contact with each other to form a multilayer structure. The wiring board has a penetration structure ranging from above the fourth surface of the first reinforcement layer to below the sixth surface of the second reinforcement layer. The penetration structure includes a penetration part ranging from the fourth surface of the first reinforcement layer to the sixth surface of the second reinforcement layer, a first pad part connected to the penetration part and extending onto the third surface of the first reinforcement layer, and a second pad part connected to the penetration part and extending onto the sixth surface of the second reinforcement layer.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a wiring board, a method for manufacturing a wiring board, and a semiconductor device. [Background technology]

[0002] In recent years, the SiP (System In Package) has been put to practical use, in which multiple different semiconductor devices (semiconductor chips) are mounted on an interposer to form a single semiconductor device. This makes it possible to obtain a "package substrate" that is a highly functional semiconductor device without increasing process costs.

[0003] For example, in the packaging of high-performance semiconductors, the mainstream technology is to integrate semiconductor devices such as three-dimensional stacked memory and logic on a silicon interposer, and to mount the silicon interposer equipped with multiple different semiconductor device chips on a package substrate.

[0004] Furthermore, development is underway for FOWLP (Fan-out Wafer Level Package) substrates in which, instead of silicon interposers, semiconductor chips are fixed with a sealing resin called EMC (Electric Molding Compound) and fine wiring is formed on the EMC using a photosensitive insulating resin called a redistribution layer.

[0005] In such FOWLP and normal package substrates, the thermal expansion coefficients of the substrate and the semiconductor chip are different, and a resin with low rigidity is used, and furthermore, the multi-layer structure makes it easy for interface destruction to occur due to the difference in thermal expansion coefficients when bonding the chip. For this reason, a structure has been devised in which a reinforcing member is formed on the peripheral edge of the wiring substrate, reinforcing the wiring substrate with the reinforcing member even in areas other than the bonding area between the semiconductor element and the wiring substrate, thereby suppressing warping of the wiring substrate.

[0006] For example, Patent Document 1 discloses a technology in which "a method for manufacturing a semiconductor package (1) includes the steps of preparing a laminate (20) having a plate-shaped first reinforcing member (5A), a laminate (2A) for a first conductor pattern wiring board, and a plate-shaped second reinforcing member (4A) arranged on a second conductor pattern (224), heating the laminate (20) to thermally harden the insulating layer, selectively removing a portion of the first reinforcing member (5A) to form an opening for exposing the first conductor pattern (224), selectively removing a portion of the second reinforcing member (4A) to form an opening 41 for exposing the second conductor pattern (221), and connecting a semiconductor element (3) to the second conductor pattern (221) exposed from the opening of the second reinforcing member (4A)."

[0007] However, in the case of Patent Document 1, the difference in rigidity and thermal expansion coefficient between the reinforcing member and the resin of the wiring board is not taken into consideration, and if there is a large difference in rigidity and thermal expansion coefficient between the reinforcing member and the resin of the wiring board, there is a risk that delamination will occur at the interface between the reinforcing member and the resin of the wiring board due to stress. In order to alleviate such stress within the board, a structure has been devised in which the filler for the penetrating structure in the core board is made of a plurality of types of material with different thermal expansion coefficients, thereby alleviating the stress.

[0008] For example, Patent Document 2 discloses a technology in which "the wiring board 1 of the embodiment has a laminate 100 including a first conductor layer 102a formed on a first surface 100F and a second conductor layer 102b formed on a second surface 100S, a through-hole conductor 30 penetrating the laminate 100 and connecting the first conductor layer 102a and the second conductor layer 102b, a first build-up portion 110 on the first surface 100F, and a second build-up portion 120 on the second surface 100S. The through-hole conductor 30 includes a conductor film 31 covering an inner wall surface of a through hole TH penetrating the laminate 100, and a filler 32 filling the through hole TH, the filler 32 including at least one set of fillers 32a, 32b filling different regions of the through hole TH in the thickness direction of the laminate 100, the set of fillers 32a, 32b having different thermal expansion coefficients."

[0009] However, in the case of Patent Document 2, although the influence of stress inside the core substrate is considered, the influence of stress at the interface between the core substrate and the wiring layer is not considered. [Prior art documents] [Patent documents]

[0010] [Patent Document 1] International Publication No. 2013 / 065287 [Patent Document 2] JP 2022-114157 A Summary of the Invention [Problem to be solved by the invention]

[0011] SUMMARY OF THE PRESENT DISCLOSURE An object of the present invention is to provide a laminated wiring board capable of reducing stress applied to the board, regardless of whether it is inside or outside the board. [Means for solving the problem]

[0012] A representative wiring board of the present invention is a wiring layer board comprising a wiring layer having a first side and a second side, a first reinforcing layer having a third side and a fourth side, and a second reinforcing layer having a fifth side and a sixth side, wherein the wiring board has a laminated structure in which the fourth side of the first reinforcing layer is in contact with the first side of the wiring layer, and the fifth side of the second reinforcing layer is in contact with the second side of the wiring layer, and the wiring board has a through structure extending from above the fourth side of the first reinforcing layer to below the sixth side of the second reinforcing layer, and the through structure has a through portion extending from the fourth side of the first reinforcing layer to below the sixth side of the second reinforcing layer, a first pad portion connected to the through portion and extending onto the third side of the first reinforcing layer, and a second pad portion connected to the through portion and extending onto the sixth side of the second reinforcing layer. Effect of the Invention

[0013] According to the present invention, it is possible to provide a wiring board capable of reducing stress applied to the board regardless of whether it is inside or outside the laminated wiring board. Objects, configurations and effects other than those described above will become apparent from the following description of the preferred embodiment of the invention. [Brief description of the drawings]

[0014] [Figure 1] FIG. 1 is a cross-sectional view that illustrates a schematic configuration of a semiconductor device. [Diagram 2] FIG. 2 is a diagram showing stress applied to a conventional package substrate. [Diagram 3] FIG. 3 is a diagram showing the stress applied to the package substrate. [Figure 4] FIG. 4 is a diagram showing a process (pre-process) of forming a first reinforcing layer, a second reinforcing layer, and a connection electrode on a fine wiring layer. [Diagram 5] FIG. 5 is a diagram showing a step (first step) of forming a through hole. [Figure 6] FIG. 6 is a diagram showing a step (second step) of forming a seed layer. [Figure 7] FIG. 7 is a diagram showing a step (third step) of forming a resist layer. [Figure 8] FIG. 8 is a diagram showing a step (fourth step) of forming a penetrating structure. [Figure 9] FIG. 9 is a diagram showing a step (fifth step) of forming a resist layer. [Figure 10] FIG. 10 is a diagram showing a step (sixth step) of forming solder. [Figure 11] FIG. 11 is a diagram illustrating a step (seventh step) of removing the resist layer. [Figure 12] FIG. 12 is a diagram showing a step (eighth step) of bonding the semiconductor element to a package substrate. [Figure 13] FIG. 13 is a schematic plan view of FIG. [Figure 14] FIG. 14 is a cross-sectional view that illustrates a package substrate according to the first modification. [Figure 15] FIG. 15 is a cross-sectional view that illustrates a package substrate according to the second modification. [Figure 16] FIG. 16 is a cross-sectional view that illustrates a package substrate according to the third modification. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. The embodiment shown below shows an example in which the technical idea of ​​the present invention is embodied, and the technical idea of ​​the present invention is not limited to the material, shape, structure, arrangement, etc. of the components described below. Various modifications can be made to the technical idea of ​​the present invention within the technical scope defined by the claims described in the claims.

[0016] <Embodiments of the present invention> Next, a semiconductor device 22 according to an embodiment of the present invention will be described with reference to FIG. FIG. 1 is a cross-sectional view that diagrammatically illustrates a semiconductor device 22. As shown in FIG. The semiconductor device 22 mainly includes a package substrate 1, a semiconductor element 15, a third metal post 21, a bonding electrode 5, and an underfill 16. In this embodiment, the case where the semiconductor device 22 includes only one semiconductor element 15 will be described, but a plurality of semiconductor elements 15 may be included.

[0017] <Package substrate> The package substrate 1 protects the delicate IC chip from the external environment and provides an external connection wiring terminal when the IC chip is mounted on a printed wiring board. The package substrate 1 is directly bonded to the bonding electrode 5, and is bonded to the semiconductor element 15 via the third metal post 21. The space between the package substrate 1 and the semiconductor element 15 is filled with an underfill 16 . The package substrate 1 mainly includes a fine wiring layer 2, a first reinforcing layer 4, a second reinforcing layer 9, a through structure 23, a seed layer 12, a first metal post 3, and a second metal post 20.

[0018] <<Fine wiring layer>> The fine wiring layer 2 is provided with fine wiring by embedding the wiring 2B in the insulating resin 8. The insulating resin 8 has a first surface 111 and a second surface 112, with the first surface 111 being in contact with the fourth surface 114 of the first reinforcing layer 4, and the second surface 112 being in contact with the fifth surface 115 of the second reinforcing layer 9. In the fine wiring layer 2 of this embodiment, the wiring 2B is embedded in the first surface 111 and the second surface 112 of the insulating resin 8, but it is also possible to embed the wiring 2B in only one of the surfaces. In this embodiment, the fine wiring layer 2 is described as having a single layer structure in which the fine wiring layer 2 is embedded in one insulating resin 8, but it may also have a multilayer structure in which at least two or more wirings 2B and at least two or more insulating resins 8 are alternately stacked in the positive direction of the Z axis, and different wirings 2B are electrically connected to each other. In this embodiment, the wiring 2B is made of a metal such as copper or an alloy thereof, but may be made of other metals.

[0019] The insulating resin 8 is mainly made of epoxy resin or polyimide resin, and blocks the flow of electricity through the embedded wiring 2B, thereby preventing leakage current. Moreover, the insulating resin 8 may be a thermosetting resin or a photosensitive resin. Furthermore, the insulating resin 8 may contain a filler such as silica (SiO2).

[0020] <<First reinforcing layer>> The first reinforcing layer 4 has a third surface 113 and a fourth surface 114, the fourth surface 114 being provided in contact with the first surface 111 of the fine wiring layer 2, and is an upper reinforcing layer among the reinforcing layers that prevent deformation of the fine wiring layer 2. The first reinforcing layer 4 is a thermosetting resin that is not easily affected by thermal deformation due to temperature changes, for example, an epoxy resin or a glass cloth-impregnated epoxy resin, but may be other resins. Furthermore, the first reinforcing layer 4 may be made of a material other than resin, for example, a metal such as copper or an alloy.

[0021] <<Second reinforcing layer>> The second reinforcing layer 9 has a fifth surface 115 and a sixth surface 116, and the fifth surface 115 is provided in contact with the second surface 112 of the fine wiring layer 2, and is the lower reinforcing layer among the reinforcing layers that prevent deformation of the fine wiring layer 2. The second reinforcing layer 9 is a thermosetting resin that is not easily affected by thermal deformation due to temperature changes, for example, epoxy resin or glass cloth-impregnated epoxy resin, but may be other resins. Furthermore, the first reinforcing layer 4 may be made of a material other than resin, for example, a metal such as copper or an alloy. Moreover, the first reinforcing layer 4 and the second reinforcing layer 9 may be made of different materials.

[0022] <<Penetrating structure>> The penetrating structure 23 is a structure that extends from above the third surface 113 of the first reinforcing layer 4 to below the sixth surface 116 of the second reinforcing layer 9 . The penetrating structure 23 may be made of a material having a different thermal expansion coefficient, elastic modulus, etc. from the first reinforcing layer 4 and the second reinforcing layer 9. The penetrating structure 23 is made of, for example, copper, epoxy resin, or polyimide resin. Furthermore, the penetrating structure 23 may be made of a thermosetting resin, or may be made of a photosensitive resin, a metal such as aluminum, nickel, platinum, or gold, or an alloy containing these metals.

[0023] The through structure 23 has a first pad portion 180 and a second pad portion 190 on both ends of a through portion 231 that extends from the third surface 113 of the first reinforcing layer 4 to the sixth surface 116 of the second reinforcing layer. In this embodiment, the through structure 23 is formed by integral molding, but it may be formed by other methods. For example, a component corresponding to the first pad portion 180 and a component corresponding to the second pad portion 190 may be joined to both ends of the through portion 231.

[0024] The through portion 231 is formed by filling the through hole 14 extending from the third surface 113 of the first reinforcing layer 4 to the sixth surface 116 of the second reinforcing layer. The diameter of the first pad portion 180 is larger than the diameter of the through-hole 14, and similarly, the diameter of the second pad portion 190 is also larger than the diameter of the through-hole 14.

[0025] In the package substrate 1, the through hole 231 is formed on the outer periphery of the first metal post 3 and is provided so as to penetrate the first reinforcing layer 4, the insulating resin 8, and the second reinforcing layer 9, and has an electrode pad structure in the first reinforcing layer 4 and the second reinforcing layer 9 that is larger in diameter than the through hole.

[0026] <<Seed layer>> The seed layer 12 is a thin film containing copper that is formed on the side surface of the through hole 14 and on the surfaces of the first reinforcing layer 4 and the second reinforcing layer 9 . Moreover, the seed layer 12 functions as a power supply layer in the film formation by electrolytic plating.

[0027] <First metal post> The first metal post 3 is a base portion of the bonding electrode 5 and is electrically connected to the wiring 2 B of the fine wiring layer 2 , thereby electrically connecting the semiconductor element 15 and the fine wiring layer 2 . The first metal post 3 is disposed inside a through hole 13 that extends from the third surface 113 to the fourth surface 114 of the first reinforcing layer 4 . The first metal post 3 is made of a conductive metal such as copper, or a metal such as copper or an alloy. Furthermore, the material of the first metal post 3 has a higher melting point than the material of the joining electrode 5, and therefore has a lower thermal expansion coefficient than the joining electrode 5 and is highly stable in shape at high temperatures, making it less likely to deform. If the melting point of the first metal post 3 is equal to or lower than the melting point of the bonding electrode 5, the first metal post 3 will also melt at the same time during solder bonding. This makes it difficult to maintain an appropriate gap (standoff) between the semiconductor element 15 and the semiconductor package substrate 1. If the standoff becomes narrow, voids will occur in the filling step of the underfill 16, which will be described later, causing a decrease in reliability. For this reason, it is desirable for the first metal post 3 to have a higher melting point than the bonding electrode 5. The material of the first metal post 3 is preferably a multi-layer of Cu, Ag, Au, Ni, Sn, or Ti, or an alloy thereof, but the present invention is not limited to this. Also, the height of the first metal post 3 is preferably within a range that allows the underfill 16 to be appropriately filled, but the present invention is not limited to this. Specifically, it is preferably within a range of 5 μm or more and 100 μm or less.

[0028] <Second metal post> The second metal post 20 is a base for an electrode when the package substrate 1 is connected to another substrate, and electrically connects to the wiring 2B of the fine wiring layer 2, thereby electrically connecting the other substrate to the fine wiring layer 2. The second metal post 20 is disposed inside a through hole extending from the sixth surface 116 to the fifth surface 115 of the second reinforcing layer 9 . The second metal post 20 is made of a conductive metal such as copper, or a metal such as copper or an alloy. Furthermore, the material of the second metal post 20 has a higher melting point than the material of the joining electrode 5, and therefore has a lower thermal expansion coefficient than the joining electrode 5 and is highly stable in shape at high temperatures, making it less likely to deform.

[0029] <Semiconductor element> The semiconductor element 15 is an element that has a function of operating when supplied with at least one of electric power and an electrical signal, a function of outputting at least one of electric power and an electrical signal in response to an external stimulus, or a function of operating when supplied with at least one of electric power and an electrical signal and outputting at least one of electric power and an electrical signal in response to an external stimulus. The semiconductor element 15 is directly bonded to the third metal post 21 , and is bonded to the package substrate 1 via the bonding electrode 5 .

[0030] The semiconductor element 15 is, for example, a semiconductor chip, or a chip in which circuits and elements are formed on a substrate made of a material other than a semiconductor, such as a glass substrate, and may include one or more elements of a large-scale integrated circuit (LSI), a memory, an imaging element, a light-emitting element, and a MEMS (Micro Electro Mechanical System). Here, the MEMS includes at least one of a pressure sensor, an acceleration sensor, a gyro sensor, a tilt sensor, a microphone, and an acoustic sensor.

[0031] In this embodiment, the semiconductor element 15 is a semiconductor chip and is bonded to the package substrate 1 via the bonding electrode 5 and the first metal post 3, but it may be another type of chip and may be bonded to the package substrate 1 by another method.

[0032] <Third metal post> The third metal post 21 is a base portion that connects the semiconductor element 15 to the bonding electrode 5, and electrically connects the semiconductor element 15 to the fine wiring layer 2 by electrically connecting to the wiring 2B of the fine wiring layer 2 via the bonding electrode 5 or the like, thereby electrically connecting the semiconductor element 15 to the fine wiring layer 2. The third metal post 21 is disposed on the eighth surface 118 of the semiconductor element 15 and is bonded to the bonding electrode 5 . The third metal post 21 is made of a conductive metal such as copper, or a metal such as copper or an alloy. Furthermore, the material of the third metal post 21 has a higher melting point than the material of the joining electrode 5, and therefore has a lower thermal expansion coefficient than the joining electrode 5 and has high shape stability at high temperatures, making it less likely to deform.

[0033] <Joining electrode> The bonding electrode 5 is provided between the first metal post 3 and the third metal post 21 and electrically bonds the first metal post 3 and the third metal post 21 together. As a result, the bonding electrode 5 electrically bonds the fine wiring layer 2 and the semiconductor element 15 to each other. In this embodiment, the joining electrode 5 is an electrode to which a gold electrode is soldered. Here, the solder is, for example, Sn, Sn-Pb, Sn-Ag, Sn-Cu, Sn-Ag-Cu, or Sn-Bi.

[0034] <Underfill> The underfill 16 is an insulating resin used to seal integrated circuits. In this embodiment, underfill 16 fills the space between semiconductor element 15 and package substrate 1, and mechanically reinforces the bond between semiconductor element 15 and package substrate 1 with bonding electrodes 5, thereby strengthening the bond between semiconductor element 15 and package substrate 1.

[0035] <Occurrence of delamination> FIG. 2 is a diagram showing the stress applied to a typical package substrate. Hereinafter, the delamination of the package substrate 1 will be described with reference to FIGS.

[0036] The semiconductor package substrate 1 generally has a structure in which different materials, such as insulating materials and metal wiring, are laminated together, and therefore it is practically difficult to avoid that each layer has a different thermal expansion coefficient and elastic modulus. FIG. 2(a) is a schematic diagram of a typical semiconductor package substrate 1 made of three different materials. When the thermal expansion coefficient of the second reinforcement layer 9 is smaller than that of the first reinforcement layer 4, that is, when the thermal expansion coefficient of the second reinforcement layer 9 is smaller than that of the first reinforcement layer 4, as the temperature rises, the stress 311 applied to the thermal expansion of the second reinforcement layer 9 becomes relatively greater than the stress 310 applied to the thermal expansion of the first reinforcement layer 4. In other words, stress occurs due to the difference in thermal expansion coefficient and elastic modulus for each constituent layer material, and when the stress of the constituent materials of each constituent layer is balanced, the phenomenon of "warping" is observed in the semiconductor package substrate 1. As a result of the warping of the semiconductor package substrate 1, that is, as a result of bending of the constituent materials of the constituent layers, stresses 330 and 331 are generated in the peeling direction, which are restored according to the bending elastic modulus of each constituent layer. Here, the stress in the peeling direction occurs at a magnitude that is balanced with the adhesive strength of each interface. In other words, when warping occurs, it means that stress that peels off each bonded interface is applied. Furthermore, even if the thermal expansion coefficient of the first reinforcement layer 4 is smaller than that of the second reinforcement layer 9, that is, if the thermal expansion coefficient of the first reinforcement layer 4 is smaller than that of the second reinforcement layer 9, the direction of the stress 330 in the warping and peeling directions will be reversed, but a stress that peels off each of the joined interfaces will be applied. For this reason, when warping of the semiconductor package substrate 1 occurs, it is difficult to eliminate the occurrence of stress in the peeling direction.

[0037] FIG. 2( b ) is an enlarged schematic view of the interface where the first reinforcing layer 4 and the fine wiring layer 2 are joined. If the first reinforcing layer 4 and the fine wiring layer 2 are made of different materials, they have different thermal expansion coefficients 310 and 312. Also at the adhesive interface 321, a stress 340 occurs in the direction parallel to the adhesive plane (x-axis), i.e., in the shear direction, due to the difference in the relative thermal expansion coefficients. FIG. 2(b) shows an example of a combination of thermal expansion coefficients in which the magnitude of the thermal expansion coefficient is “first reinforcing layer 4” > “fine wiring layer 2”. However, regardless of this magnitude relationship, if there is a difference in the thermal expansion coefficients of the materials of the constituent layers, stress 340 will be generated.

[0038] In an actual semiconductor package substrate 1, repeated cooling and heating during temperature cycles such as turning on and off the semiconductor device or during reliability testing causes stress 330 in the warping and peeling directions and stress 340 in the shearing direction to continue to apply load to the adhesive interface while reversing their directions as shown in Figures 2(a) and 2(b). As a result of this repeated load, microscopic peeling occurs at the adhesive interface, and the microscopic peeling propagates and becomes continuous, causing delamination as shown in Figure 2(c).

[0039] 3 is a diagram showing stress applied to the semiconductor package substrate 1 of this embodiment. In the package substrate 1 of this embodiment, the first reinforcing layer 4 and the second reinforcing layer 9 have a thermal expansion coefficient of about 4 to 10 ppm / k and an elastic modulus of about 5 to 40 MPa. In contrast, the insulating resin 8 constituting the fine wiring layer 2 has a thermal expansion coefficient of about 50 ppm / k and an elastic modulus of 1 to 5 Pa, which are higher than those of the first reinforcing layer 4 and the second reinforcing layer 9, and lower than those of the second reinforcing layer 9. Therefore, the insulating resin 8 is forced to follow the deformation of the first reinforcing layer 4 and the second reinforcing layer 9. As a result, warping occurs due to the difference in thermal expansion coefficient between the first reinforcing layer 4 and the second reinforcing layer 9. When the semiconductor package substrate 1 is heated or generates heat by passing electricity through it, causing a temperature rise, if the thermal expansion coefficient of the second reinforcing layer 9 is greater than that of the first reinforcing layer 4, as shown in Figure 3, repeated loads are applied to the adhesion at the bonding interfaces due to stresses 330 and 310 in the peel direction and strains 320, 321 in the shear direction applied to each bonding interface.

[0040] In the present invention, the through structure 23 is provided which communicates the first pad portion 180 to the second pad portion 190 and integrally forms the first pad portion 180 and the second pad portion 190. The stress 330 in the peeling direction related to the first reinforcing layer 4 is balanced with the resistance 332 from the first pad portion 180, so deformation can be prevented. Similarly, the stress 331 in the peeling direction related to the second reinforcing layer 9 is balanced with the resistance 333 from the second pad portion 190, so deformation can be prevented. Even if a stress 340 in the shear direction related to the first reinforcing layer 4 and a stress 341 in the shear direction related to the second reinforcing layer 9 occur, they can be suppressed by the resistance 342 by the communicating through structure 23. By resisting the stresses 330 and 331 in the peeling direction and suppressing the stresses 340 and 341 in the shear direction, delamination can be prevented.

[0041] <Effects> As described above, according to the package substrate 1 of this embodiment, the stress generated when the first reinforcing layer 4 and the second reinforcing layer 9 are deformed can be countered by the resistance from the first pad portion 180 and the second pad portion 190 and the resistance from the penetrating structure 23. This makes it possible to reduce stress occurring at the interfaces between the layers of the package substrate 1, thereby making it possible to suppress delamination. In addition, it is possible to select an optimum material for the through structure 23 depending on the material of the package substrate 1.

[0042] <Manufacturing method of package substrate> A method for manufacturing the package substrate 1 will now be described with reference to FIGS. FIG. 4 is a diagram showing a process (pre-process) of forming a first reinforcing layer 4, a second reinforcing layer 9 and connection electrodes on a fine wiring layer 2. As shown in FIG. In the previous process, a fine wiring layer 2 having wiring 2B applied to an insulating resin 8 is used, and the fine wiring layer 2 has a first surface 111 and a second surface 112. A first reinforcing layer 4 is bonded to the first surface 111 side of the fine wiring layer 2, and a second reinforcing layer 9 is bonded to the second surface 112 side. After the first reinforcing layer 4 and the second reinforcing layer 9 are bonded together, a hole is formed in a part of the layer using a drill or the like, and a third metal post 21 is provided. The third metal post 21 can be formed by a known method. Specifically, the third metal post 21 can be formed through the following steps: after bonding the first reinforcing layer 4 and the second reinforcing layer 9, a step of forming a via hole penetrating the first reinforcing layer 4 and the second reinforcing layer 9 by laser processing or the like to reach the fine wiring layer 2, a step of desmearing the via hole and forming a seed layer on the entire surface of the first reinforcing layer 4 and the second reinforcing layer 9 by electroless plating, a step of forming a photoresist pattern on the seed layer by photolithography to form an opening pattern that will be a mold for the third metal post 21, a step of passing electricity through the seed layer in the electrolytic plating step to fill and form the third metal post 21 in the opening pattern by electrolytic plating, a step of removing the photoresist pattern that is no longer needed, and a step of removing the seed layer that is no longer needed.

[0043] FIG. 5 is a diagram showing a step (first step) of forming the through-hole 14. As shown in FIG. In a first step, a drill is aligned with the third surface 113 of the first reinforcing layer, and then through holes 14 are formed with a drill aligned with the sixth surface 116 of the second reinforcing layer 9 .

[0044] FIG. 6 is a diagram showing a step (second step) of forming a seed layer 12. As shown in FIG. In a second process, a seed layer 12 is formed on the third surface 113 and the sixth surface 116, the side surfaces of the through holes 14, the side surfaces and top surfaces of the first metal posts 3, and the side surfaces and top surfaces of the second metal posts 20 by electroless plating of copper. Also, the seed layer 12 may be formed by a different technique, for example vacuum deposition, and may be formed from a different material, for example silver.

[0045] FIG. 7 is a diagram showing a step (third step) of forming a resist layer 11. In a third step, a resist layer 11 having an opening pattern with a diameter larger than the diameter of the through hole 14 on the third surface 113 is formed on the seed layer 12 on the surface of the third surface 113 of the first reinforcing layer by photolithography. Next, in a similar manner, a resist layer 11 having an opening pattern with a diameter larger than the diameter of the through hole 14 on the sixth surface 116 of the second reinforcing layer 9 is formed by photolithography on the seed layer 12 on the sixth surface 116 of the second reinforcing layer 9. Similarly, a resist layer 11 is formed on the first metal post 3 and the second metal post 20 by photolithography.

[0046] FIG. 8 is a diagram showing a step (fourth step) of forming the penetrating structure 23. As shown in FIG. In a fourth step, electrolytic plating is performed on the seed layer 12 through the opening pattern of the resist layer 11 to fill the through holes 14 with plating, thereby forming the through structures 23. As a result, a first pad portion 180 having a diameter larger than the diameter of the through hole 14 on the third surface 113 is formed on the surface of the first reinforcement layer 4, and a second pad portion 190 having a diameter larger than the diameter of the through hole 14 on the sixth surface 116 is formed on the surface of the second reinforcement layer 9.

[0047] In this process, the through holes 14 are filled with copper by electrolytic plating, but other metals may be used. For example, metals such as aluminum, nickel, platinum, and gold, and alloys containing these metals may be used. Furthermore, the through holes 14 may be filled with materials other than metals. For example, the through holes 14 may be filled with a thermosetting resin or a photosensitive resin. In either case, by changing the type of metal to suit the physical properties and structure of the substrate material, the fixing force can be changed, the stress can be appropriately attenuated, and delamination can be suppressed. Furthermore, the through holes 14 may be filled by a method other than electrolytic plating, such as by laminating a paste or a resin film, or by screen printing.

[0048] FIG. 9 is a diagram showing a step (fifth step) of forming a resist layer 11B. In the fifth step, the resist layer 11 is removed by an alkaline solvent or solution, and then a resist layer 11B is formed so as to cover the penetrating structure 23 and the seed layer 12. At this time, the resist layer 11B has openings communicating with the first metal post 3 and the second metal post 20. As shown in FIG.

[0049] FIG. 10 is a diagram showing a step (sixth step) of forming solder 10. As shown in FIG. In a sixth step, dome-shaped solder 10 is formed on the first metal post 3 and the second metal post 20 by electrolytic plating.

[0050] FIG. 11 is a diagram showing a step (seventh step) of removing resist layer 11B in FIG. In the seventh step, the resist layer 11B is removed by an alkaline solvent or solution. The seed layer 12 can be mainly selected from metals. The seed layer can be removed by immersing it in an etching solution that corrodes and dissolves the metal layer. For example, if the seed layer 12 is copper, it can be removed by using an etching solution consisting of an aqueous solution of sulfuric acid and hydrogen peroxide.

[0051] <Method of Manufacturing Semiconductor Device> Hereinafter, a method for manufacturing a semiconductor device 22 using a package substrate 1 will be described with reference to FIGS. FIG. 12 is a diagram showing a step (eighth step) of bonding semiconductor element 15 to package substrate 1. As shown in FIG. In an eighth process, the solder 10 on the first metal post 3 on the third surface 113 of the package substrate 1 is bonded to the third metal post 21 to form a bonding electrode 5, thereby bonding the semiconductor element 15 to the package substrate 1. Next, an underfill material is filled between the package substrate 1 and the semiconductor element 15 to form an underfill 16.

[0052] In this process, the underfill material is a mixture of resin and filler. The resin is, for example, one of epoxy resin, urethane resin, silicone resin, polyester resin, oxetane resin, and maleimide resin, or a mixture of two or more of these resins. The filler is, for example, one of silica, titanium oxide, aluminum oxide, magnesium oxide, and zinc oxide, or a mixture of two or more of these resins.

[0053] FIG. 13 is a schematic plan view of FIG. In the semiconductor device 22 , a through structure 23 is formed so as to surround the periphery of a semiconductor element 15 .

[0054] <Variation 1> Hereinafter, a package substrate according to the first modified example of the present invention will be described with reference to FIGS. FIG. 14 is a cross-sectional view that diagrammatically illustrates a package substrate 1B according to the first modification.

[0055] A package substrate 1B according to another embodiment shown in FIG. 14 differs from the embodiment in that a penetrating structure 23 has a cylindrical shape having a minimum portion 25 in its diameter. Here, the extremely small portion 25 is a portion between the first surface 111 and the second surface 112 of the fine wiring layer 2 where the diameter of the cross section of a surface parallel to the first surface 111 is the smallest. In order to give the through structure 23 a shape having a very small portion 25, the through hole 14 can be formed so as to penetrate from both sides of the package substrate 1B, i.e., the third surface 113 and the sixth surface 116.

[0056] For example, when the through structure 23 is cylindrical as in this embodiment, the through hole 14 is formed by drilling. However, in this method, it takes time to form the through-hole 14, and there is a limit to how small the diameter of the through-hole 14 can be made due to the physical size of the drill. On the other hand, in the penetration structure of this embodiment, the through holes can be formed from the front and back by laser processing, so that the time required to form the through holes 14 can be shortened. Furthermore, the diameter of the through holes 14 can be reduced by laser processing, which can increase the formation density of the through structures 23 and improve the delamination prevention effect.

[0057] This makes it possible to prevent deformation of package substrate 1B due to the force from penetrating structure 23 in addition to first pad portion 180 and second pad portion 190.

[0058] <Variation 2> The package substrate according to the second modification of the present invention will be described below. FIG. 15 is a cross-sectional view that diagrammatically illustrates a package substrate 1C according to the second modification. Modification 2 differs from Modification 1 in that the minimum portion 25 is provided in the first reinforcing layer 4. That is, the minimum portion is provided between the third surface 113 and the fourth surface 114 of the first reinforcing layer 4. In the package substrate 1 of this modification, the first reinforcing layer 4 and the second reinforcing layer 9 have a thermal expansion coefficient of about 4 to 10 ppm / k and an elastic modulus of about 5 to 40 MPa. In contrast, the insulating resin 8 has a thermal expansion coefficient of about 50 ppm / k and an elastic modulus of 1 to 5 Pa, which are higher than those of the reinforcing layers, but lower than those of the reinforcing layers. For this reason, in modification 2, the minimum portion 25, where stress is likely to concentrate, is provided inside the first reinforcing layer 4, which is less susceptible to thermal deformation and has a high elastic modulus. This makes it possible to distribute the stress to the first reinforcing layer 4 while reinforcing the minimum portion with the first reinforcing layer 4, thereby effectively suppressing delamination.

[0059] <Variation 3> The package substrate according to the third modification of the present invention will be described below. FIG. 16 is a cross-sectional view that illustrates a package substrate 1D according to a third modification. Modification 3 differs from Modification 2 in that the minimum portion 25 is provided in the second reinforcing layer 9. That is, the minimum portion 25 is provided between the fifth surface 115 and the sixth surface 116 of the second reinforcing layer 9. At this time, similarly to the second modification, the effect of reducing the stress due to thermal deformation at the minimum portion 25 where the stress is likely to be concentrated is increased, and delamination can be suppressed.

[0060] The present invention can also take the following forms. (Aspect 1) a wiring layer having a first surface and a second surface; a first reinforcing layer having a third surface and a fourth surface; A wiring board including a second reinforcing layer having a fifth surface and a sixth surface, The wiring board includes: the fourth surface of the first reinforcing layer and the first surface of the wiring layer are in contact with each other, the fifth surface of the second reinforcing layer and the second surface of the wiring layer are in contact with each other to form a laminated structure, a through structure extending from above the fourth surface of the first reinforcing layer to below the sixth surface of the second reinforcing layer; The through structure includes a through portion extending from the third surface of the first reinforcing layer to the sixth surface of the second reinforcing layer; a first pad portion connected to the through portion and extending on the third surface of the first reinforcing layer; a second pad portion connected to the through portion and extending on the sixth surface of the second reinforcing layer; have Wiring board. (Aspect 2) In the wiring board according to the first aspect, The through portion has a minimum portion between the third surface of the first reinforcing layer and the sixth surface of the second reinforcing layer, the minimum portion being a cross-sectional diameter of a surface parallel to the first surface. Wiring board. (Aspect 3) In the wiring board according to aspect 2, The minimum portion is present between the third surface and the fourth surface of the first reinforcing layer, or between the fifth surface and the sixth surface of the second reinforcing layer. Wiring board. (Aspect 4) In the wiring board according to any one of aspects 1 to 3, The through structure is filled with metal Wiring board. (Aspect 5) In the wiring board according to any one of aspects 1 to 4, The through structure is filled with resin. Wiring board. (Aspect 6) A method for producing a wiring board according to any one of aspects 1 to 5, comprising the steps of: a first step of forming a through hole penetrating the first reinforcing layer, the wiring layer, and the second reinforcing layer; a second step of forming a seed layer on a side surface of the through hole, the third surface, and the sixth surface; forming a resist opening pattern having a diameter larger than a diameter of the through portion on the third surface of the first reinforcing layer in the seed layer; a third step of forming a resist opening pattern in the seed layer on the sixth surface of the second reinforcing layer, the opening pattern having a diameter larger than a diameter of the penetrating portion on the sixth surface; A fourth step of performing an electrolytic plating process on the seed layer to form a through structure. A method for manufacturing a wiring board. (Aspect 7) A semiconductor device comprising: the wiring board according to any one of the first to sixth aspects; and a semiconductor circuit board electrically connected to the wiring board. [Explanation of symbols]

[0061] 1, 1B, 1C, 1D Package Substrate 15 Semiconductor elements 16 Underfill 21 3rd Metal Post 2 Fine wiring layer 2B wiring 3. First Metal Post 8. Insulating resin 4 First Reinforcement Layer 5 Junction electrode 9 Second Reinforcement Layer 10 Solder 11 Resist layer 12 Seed layer (for metal posts) 14 Through hole 20 Second Metal Post 22 Semiconductor Devices 23 Penetration structure 180 First pad section 190 Second Pad Section

Claims

1. a wiring layer having a first surface and a second surface; a first reinforcing layer having a third surface and a fourth surface; A wiring board including a second reinforcing layer having a fifth surface and a sixth surface, The wiring board includes: the fourth surface of the first reinforcing layer and the first surface of the wiring layer are in contact with each other, the fifth surface of the second reinforcing layer and the second surface of the wiring layer are in contact with each other to form a laminated structure, a through structure extending from above the fourth surface of the first reinforcing layer to below the sixth surface of the second reinforcing layer; The through structure includes a through portion extending from the third surface of the first reinforcing layer to the sixth surface of the second reinforcing layer, a first pad portion connected to the through portion and extending on the third surface of the first reinforcing layer; a second pad portion connected to the through portion and extending on the sixth surface of the second reinforcing layer; have Wiring board.

2. 2. The wiring board according to claim 1, The through portion has a minimum portion between the third surface of the first reinforcing layer and the sixth surface of the second reinforcing layer, the minimum portion having a cross-sectional diameter in a surface parallel to the first surface. Wiring board.

3. 3. The wiring board according to claim 2, The minimum portion is present between the third surface and the fourth surface of the first reinforcing layer, or between the fifth surface and the sixth surface of the second reinforcing layer. Wiring board.

4. 2. The wiring board according to claim 1, The through structure is filled with metal Wiring board.

5. 2. The wiring board according to claim 1, The through structure is filled with resin. Wiring board.

6. 2. A method for manufacturing a wiring board according to claim 1, comprising the steps of: a first step of forming a through hole penetrating the first reinforcing layer, the wiring layer, and the second reinforcing layer; a second step of forming a seed layer on a side surface of the through hole, the third surface, and the sixth surface; forming a resist opening pattern having a diameter larger than a diameter of the through portion on the third surface of the first reinforcing layer in the seed layer; a third step of forming a resist opening pattern in the seed layer on the sixth surface of the second reinforcing layer, the opening pattern having a diameter larger than a diameter of the penetrating portion on the sixth surface; A fourth step of performing an electrolytic plating process on the seed layer to form a through structure. A method for manufacturing a wiring board.

7. A semiconductor device comprising: the wiring board according to claim 1; and a semiconductor circuit board electrically connected to the wiring board.

Citation Information

Patent Citations

  • Wiring board

    JP2022114157A

  • Method for manufacturing semiconductor package

    WO2013065287A1