Manufacturing method for semiconductor device
By bonding semiconductor chips and wiring chips to a substrate with a cushioning material and using a tapered sealing method, the method addresses dust and moisture issues, ensuring electrode exposure without grinding, thus reducing costs and maintaining electrode integrity.
Patent Information
- Application Number
- JP2024141026
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2041-03-19
AI Technical Summary
The existing methods for manufacturing semiconductor devices face issues such as dust generation during grinding, moisture ingress, material wastage, and high processing costs due to uneven electrode member heights, making it difficult to reliably expose electrode members from the sealing material.
A method involving bonding semiconductor chips and wiring chips to a substrate, using a cushioning material to fill gaps between electrode members and a mold, and injecting a sealing material with a tapered shape to ensure electrode members protrude from the sealing surface without grinding, thereby reducing manufacturing costs.
The method allows reliable exposure of electrode members without additional processing, preventing moisture ingress and reducing costs by eliminating the need for grinding, while maintaining electrode integrity and preventing stress-related issues.
Smart Images

Figure 2024152939000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a method for manufacturing a semiconductor device. [Background technology]
[0002] Since it is difficult to increase the area of SiC MOSFETs, modules using SiC MOSFETs require multiple chips to be connected in parallel to increase the current capacity. A semiconductor device has been proposed in which multiple semiconductor chips and a wiring chip are bonded to a substrate, and the control electrodes of each semiconductor chip are connected in parallel by the circuit pattern of the wiring chip (see, for example, Patent Document 1). A main electrode member is bonded to the main electrodes of the multiple semiconductor chips, and a control electrode member is bonded to the circuit pattern of the wiring chip, and then the devices are sealed with resin. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] International Publication No. 2020 / 110170 Summary of the Invention [Problem to be solved by the invention]
[0004] In conventional technology, the sealing material is ground to expose the electrode members from the sealing material. However, there are problems with dust being generated during the grinding process, and with wet grinding, moisture can seep in from the ground surface. In addition, there are problems with the electrode members being ground more than necessary due to variations in height, resulting in waste of material and processing time, and making it difficult to detect the end. Furthermore, the grinding process itself is costly.
[0005] The present disclosure has been made to solve the above-mentioned problems, and its purpose is to provide a manufacturing method for a semiconductor device that can reliably remove electrode members from the top surface of the device while reducing manufacturing costs. [Means for solving the problem]
[0006] a step of bonding a semiconductor chip having a main electrode and a control electrode to a substrate; a step of bonding a wiring chip having a first electrode, a second electrode, and wiring connecting the first electrode and the second electrode to the substrate; a step of bonding a main electrode member to the main electrode via a bonding material; a step of connecting the control electrode and the first electrode with a connecting material; a step of placing the bonded semiconductor chip, the substrate, the wiring chip, the main electrode member, and the connecting member into a mold, and injecting a sealing material into the mold while pressing a tip end surface of the main electrode member against a buffer material provided between the main electrode member and the mold, to seal the semiconductor chip, the substrate, the wiring chip, the main electrode member, and the connecting member with the sealing material, wherein a tip end of the main electrode member protrudes from an upper surface of the sealing material, and the sealing material provided on a side surface of the tip end has a tapered shape in which the thickness becomes thinner toward the tip end surface. Effect of the Invention
[0007] In the present disclosure, even if the height of the main electrode member varies and a gap occurs between the main electrode member and the mold, the buffer material fills the gap. Therefore, since the tip surface of the main electrode member is exposed and not covered with the sealing material during the sealing process, the sealing material is not ground after the sealing process. Therefore, the electrode member can be reliably removed from the top surface of the device while keeping manufacturing costs down. [Brief description of the drawings]
[0008] [Figure 1] 1 is a cross-sectional view showing a semiconductor device according to a first embodiment. [Diagram 2] 1A to 1C are cross-sectional views showing a method for manufacturing a semiconductor device according to a first embodiment. [Diagram 3] 1A to 1C are cross-sectional views showing a method for manufacturing a semiconductor device according to a first embodiment. [Figure 4] 1A to 1C are cross-sectional views showing a method for manufacturing a semiconductor device according to a first embodiment. [Diagram 5] 1A to 1C are cross-sectional views showing a method for manufacturing a semiconductor device according to a first embodiment. [Figure 6]1A to 1C are cross-sectional views showing a method for manufacturing a semiconductor device according to a first embodiment. [Figure 7] 1A to 1C are cross-sectional views showing a method for manufacturing a semiconductor device according to a first embodiment. [Figure 8] 10A to 10C are cross-sectional views showing a method for manufacturing a semiconductor device according to a comparative example. [Figure 9] 10A to 10C are cross-sectional views showing a method for manufacturing a semiconductor device according to a comparative example. [Figure 10] 10A to 10C are cross-sectional views showing a method for manufacturing a semiconductor device according to a comparative example. [Figure 11] FIG. 4 is a cross-sectional view showing the tip portion of the main electrode member after sealing. [Figure 12] 5A to 5C are cross-sectional views showing a modified example of the method for manufacturing the semiconductor device according to the first embodiment. [Figure 13] FIG. 11 is a cross-sectional view showing a semiconductor device according to a second embodiment. [Figure 14] 10A to 10C are cross-sectional views showing a method for manufacturing a semiconductor device according to a second embodiment. [Figure 15] 10A to 10C are cross-sectional views showing a method for manufacturing a semiconductor device according to a second embodiment. [Figure 16] 10A to 10C are cross-sectional views showing a method for manufacturing a semiconductor device according to a second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] A method for manufacturing a semiconductor device according to an embodiment will be described with reference to the drawings. The same or corresponding components are designated by the same reference numerals, and repeated description may be omitted.
[0010] Embodiment 1 1 is a cross-sectional view showing a semiconductor device according to a first embodiment. A plurality of semiconductor chips 1 and one wiring chip 2 are bonded to a substrate 3. The semiconductor chip 1 has a back electrode 4 on its back side, and a main electrode 5 and a control electrode 6 on its front side. The semiconductor chip 1 is, for example, a MOSFET. The control electrode 6 is, for example, a gate electrode or a Kelvin source electrode. If the semiconductor chip 1 has a built-in temperature sensing element or current sensing element, it further has a control electrode corresponding to each of them.
[0011] The back electrode 4 is, for example, a metal film formed by laminating a silicide layer / titanium layer / nickel layer / titanium layer / gold or silver layer from the semiconductor chip 1 side by a sputtering method. The main electrode 5 and the control electrode 6 are, for example, metal films formed by forming an aluminum layer on the semiconductor chip 1 by a sputtering method, and laminating a nickel layer / palladium layer / gold layer thereon by a plating method. Alternatively, the main electrode 5 and the control electrode 6 may be, for example, a metal film formed by laminating an aluminum layer / titanium layer / nickel layer / titanium layer / gold or silver layer by a sputtering method. Other laminated films having similar functions may be selected.
[0012] The wiring chip 2 has a bonding layer 7 on the back side, and a first electrode 8, a second electrode 9, and a wiring 10 connecting the first electrode 8 and the second electrode 9 on the front side. The wiring chip 2 is an element made of, for example, silicon, and an insulating film such as an oxide film is formed on the Si surface, and the first electrode 8, the second electrode 9, and the wiring 10 are formed on the insulating film. The first electrode 8, the second electrode 9, and the wiring 10 are wiring patterns made of, for example, aluminum. At least the second electrode 9 is provided with a bondable metal layer. A similar metal layer may also be provided on the first electrode 8. The bondable metal layer is, for example, a laminated metal film similar to the main electrode 5 of the semiconductor chip 1. The bonding layer 7 is, for example, a metal film similar to the back electrode 4 of the semiconductor chip. The back electrode 4 of the semiconductor chip 1 and the bonding layer 7 of the wiring chip 2 are each bonded to the substrate 3 via a bonding material 11.
[0013] A main electrode member 12 is bonded to the main electrode 5 of the semiconductor chip 1 via a first bonding material 13. The main electrode member 12 is made of copper, for example. When the main electrode member 12 spans the main electrodes 5 of multiple semiconductor chips 1, the portion bonded to the main electrode 5 protrudes, and the portion connecting them is thinner than the portion bonded to the main electrode 5. This makes it possible to connect the main electrodes 5 of multiple semiconductor chips 1 to the same potential, avoiding the peripheral voltage-resistant structure of the semiconductor chip 1. Alternatively, the main electrodes 5 of multiple semiconductor chips 1 may be independent of each other and have the same potential when connected to an external electrode.
[0014] A control electrode member 14 is bonded to the second electrode 9 of the wiring chip 2 via a second bonding material 15. The control electrode member 14 is a plurality of blocks made of copper, for example.
[0015] The control electrodes 6 of the multiple semiconductor chips 1 and the first electrodes 8 of the wiring chip 2 are connected by connection members 16. The connection members 16 are wires made of, for example, gold, silver, or aluminum. If thin wires made of gold or silver are used, the dimensions of the control electrodes 6 of the semiconductor chips 1 can be reduced. This allows the effective area to be made larger, and the manufacturing costs of the semiconductor chips 1 to be reduced.
[0016] The semiconductor chip 1, the upper surface of the substrate 3, the wiring chip 2, the main electrode member 12, the control electrode member 14, and the connection member 16 are sealed with a sealing material 17. The sealing material 17 is, for example, an epoxy resin mixed with a filler. The tips of the main electrode member 12 and the control electrode member 14 protrude from the upper surface of the sealing material 17, and their tip faces are exposed from the sealing material 17.
[0017] Next, a method for manufacturing a semiconductor device according to the present embodiment will be described. FIGS. 2 to 7 are cross-sectional views showing a method for manufacturing a semiconductor device according to the first embodiment. First, as shown in FIG. 2, a semiconductor chip 1 is bonded to a substrate 3. Next, as shown in FIG. 3, a wiring chip 2 is bonded to a substrate 3. At this time, the back electrode 4 of the semiconductor chip 1 and the bonding layer 7 of the wiring chip 2 are bonded to the substrate 3 via a bonding material 11. The bonding material 11 may be, for example, solder, or a bonding material made of silver or copper may be used for sinter bonding. The sinter bonding may be pressure bonding in which the semiconductor chip 1 and the wiring chip 2 are heated while applying pressure to the electrodes from above, or non-pressure bonding without applying pressure. Alternatively, the wiring chip 2 may be bonded using an adhesive or the like that can obtain thermal and mechanical stability by heating. However, when a wiring chip 2 made of silicon is used, the wiring chip 2 may crack, so a bonding method without applying pressure is preferable.
[0018] Next, as shown in Fig. 4, the main electrode member 12 is joined to the main electrode 5 via a first bonding material 13. Next, as shown in Fig. 5, the control electrode member 14 is joined to the second electrode 9 via a second bonding material 15. The first bonding material 13 and the second bonding material 15 may be, for example, solder, or may be bonded by sinter bonding using a bonding material made of silver or copper. The sinter bonding may be pressure bonding in which the electrodes are heated while being pressed against each other by applying pressure from above, but non-pressure bonding in which no pressure is applied is preferable.
[0019] The main electrode member 12 and the control electrode member 14 have different thicknesses due to manufacturing tolerances. Also, the first bonding material 13 and the second bonding material 15 have different thicknesses. Therefore, the heights of the tip surfaces of the joined main electrode member 12 and control electrode member 14 are different.
[0020] Next, as shown in Fig. 6, the control electrode 6 and the first electrode 8 are connected by a connection member 16. Next, as shown in Fig. 7, the semi-finished product having the joined semiconductor chip 1, substrate 3, wiring chip 2, main electrode member 12, control electrode member 14, and connection member 16 is placed into a mold 18. At this time, a buffer material 19 is provided between the mold 18 and the main electrode member 12 and control electrode member 14.
[0021] When the tip faces of the main electrode member 12 and the control electrode member 14 are pressed against the cushioning material 19, the thickness of the cushioning material 19 at the contact points of the main electrode member 12 and the control electrode member 14 becomes thinner due to the pressing force. If the tip faces of the main electrode member 12 and the control electrode member 14 are at different heights, the thickness of the cushioning material 19 will differ at the contact points with the main electrode member 12 and the contact points with the control electrode member 14. In this state, the transfer mold sealing method is used to inject the sealing material 17 into the mold 18, and the semiconductor chip 1, the upper surface of the substrate 3, the wiring chip 2, the main electrode member 12, the control electrode member 14, and the connection member 16 are sealed with the sealing material 17.
[0022] When the semiconductor device is removed from the mold 18 after sealing, the cushioning material 19 is also removed from the upper surface of the semiconductor device. Through the above steps, a semiconductor device is manufactured in which the tip surfaces of the main electrode member 12 and the control electrode member 14 are exposed from the sealing material 17 without grinding the sealing material 17.
[0023] Furthermore, by using a plurality of manufactured semiconductor devices, a higher-level semiconductor device such as a half-bridge circuit or a full-bridge circuit can be constructed. In this case, the substrate 3 is electrically and thermally connected to the drain circuit pattern by solder bonding or sinter bonding. The main electrode member 12 is electrically connected to the source circuit pattern by wire bonding, ribbon bonding, or lead frame solder bonding. The periphery of the semiconductor device and the circuit pattern are then covered with a secondary sealing material such as gel to manufacture the higher-level semiconductor device. When solder is used as a bonding material for the semiconductor chip 1, it is desirable to use a high-melting-point solder having a melting point higher than the bonding process temperature when assembling the higher-level semiconductor device.
[0024] Next, the effect of this embodiment will be described in comparison with a comparative example. Figures 8 to 10 are cross-sectional views showing a manufacturing method of a semiconductor device according to the comparative example. In the comparative example, as shown in Figure 8, a buffer material 19 is not used in the resin sealing process. Therefore, a gap is generated between the mold 18 and the main electrode member 12 and the control electrode member 14, and the sealant 17 wraps around the gap. Therefore, as shown in Figure 9, there are cases where the main electrode member 12 or the control electrode member 14 cannot be exposed from the surface of the sealant 17. Therefore, as shown in Figure 10, it is necessary to grind away the excess sealant 17 and parts of the main electrode member 12 and the control electrode member 14 to expose the main electrode member 12 and the control electrode member 14.
[0025] In contrast, in this embodiment, even if the heights of the control electrode member 14 and the main electrode member 12 vary and gaps occur between the main electrode member 12 and the control electrode member 14 and the mold 18, the buffer material 19 fills the gap. Therefore, since the tip faces of the main electrode member 12 and the control electrode member 14 are exposed and not covered with the sealant 17 in the sealing process, the sealant 17 is not ground after the sealing process. Therefore, the electrode members can be reliably removed from the top surface of the device while keeping manufacturing costs down.
[0026] 11 is a cross-sectional view showing the tip of the main electrode member after sealing. When the tip faces of the main electrode member 12 and the control electrode member 14 are pressed against the cushioning material 19, the part of the cushioning material 19 that is in contact with the control electrode member 14 and the main electrode member 12 becomes thinner than the part that is not in contact. The cushioning material 19 gradually becomes thinner from the part that is not in contact toward the part that is in contact. Since resin sealing is performed in this state, the shape of the sealing material 17 follows the shape of the cushioning material 19. Therefore, the sealing material 17 provided on the side of the tip of the main electrode member 12 and the control electrode member 14 has a tapered shape in which the film thickness in the horizontal direction of the drawing becomes thinner toward the tip faces of the main electrode member 12 and the control electrode member 14.
[0027] When there is a difference between the linear expansion coefficients of the main electrode member 12 and the control electrode member 14 and the sealing material 17, stress is generated between them due to a thermal cycle or the like. If the stress causes cracks in the sealing material 17 or the sealing material 17 to peel off, moisture will penetrate during a moisture resistance test or the like and reach the semiconductor chip 1, etc., shortening the life of the semiconductor device. In contrast, in this embodiment, the thickness of the sealing material 17 gradually decreases toward the tip faces of the main electrode member 12 and the control electrode member 14 as described above. Therefore, since the stress decreases toward the end faces of the main electrode member 12 and the control electrode member 14, it is possible to prevent the sealing material 17 from peeling off from the control electrode member 14 and the main electrode member 12.
[0028] Furthermore, when a temperature sensing element or a current sensing element is built into the semiconductor chip 1, these elements are often more vulnerable to static electricity than the main portion. Therefore, it is preferable that the surface of the buffer material 19 with which the tip faces of the main electrode member 12 and the control electrode member 14 come into contact is conductive. This prevents a potential difference from occurring between the terminals during and after sealing, thereby preventing overvoltage breakdown of the semiconductor chip 1 due to static electricity.
[0029] FIG. 12 is a cross-sectional view showing a modified example of the manufacturing method of the semiconductor device according to the first embodiment. The buffer material 19 has a sealing material 17 that has no electrical conductivity, and a conductive thin film 20 such as a carbon sheet or metal foil provided between the sealing material 17 and the main electrode member 12 and the control electrode member 14. The tip surfaces of the main electrode member 12 and the control electrode member 14 contact the conductive thin film 20, and no potential difference occurs between the terminals, so that the semiconductor chip 1 can be prevented from being destroyed by overvoltage due to static electricity. In addition, by using the conductive thin film 20, an inexpensive sealing material 17 such as Teflon (registered trademark) can be used. Alternatively, the main component of the buffer material 19 may be carbon. Since such a buffer material 19 has electrical conductivity, the buffer material 19 can be formed of a single material without using the conductive thin film 20. Therefore, the processing cost can be reduced.
[0030] Embodiment 2 13 is a cross-sectional view showing a semiconductor device according to embodiment 2. In this embodiment, there is no wiring chip 2 and no connection member 16, and a control electrode member 14 is bonded to a control electrode 6 of a semiconductor chip 1 via a second bonding material 15. The other configurations are the same as those of embodiment 1.
[0031] Next, a method for manufacturing a semiconductor device according to the present embodiment will be described. Figures 14 to 16 are cross-sectional views showing a method for manufacturing a semiconductor device according to embodiment 2. First, as shown in Figure 14, a semiconductor chip 1 is bonded to a substrate 3. Next, as shown in Figure 15, a main electrode member 12 is bonded to a main electrode 5 via a first bonding material 13. A control electrode member 14 is bonded to a control electrode 6 via a second bonding material 15.
[0032] 16, the semi-finished product having the bonded semiconductor chip 1, substrate 3, main electrode member 12, and control electrode member 14 is placed in a mold 18. At this time, a buffer material 19 is provided between the mold 18 and the main electrode member 12 and control electrode member 14. With the tip faces of the main electrode member 12 and control electrode member 14 pressed against the buffer material 19, a sealant 17 is injected into the mold 18, and the semiconductor chip 1, substrate 3, main electrode member 12, and control electrode member 14 are sealed with the sealant 17.
[0033] When the semiconductor device is removed from the mold 18 after sealing, the cushioning material 19 is also removed from the top surface of the semiconductor device. Through the above steps, a semiconductor device is manufactured in which the tip surfaces of the main electrode member 12 and the control electrode member 14 are exposed from the sealing material 17 without grinding the sealing material 17. As a result, as in the first embodiment, the electrode members can be reliably removed from the top surface of the device while keeping manufacturing costs down. In the case of a small number of semiconductor chips to be connected in parallel, such as a small-capacity semiconductor product, this embodiment in which electrodes are individually taken out from the semiconductor chip 1 without using the wiring chip 2 and connected to an external circuit may be preferable because it keeps manufacturing costs down.
[0034] The semiconductor chip 1 is not limited to being made of silicon, but may be made of a wide band gap semiconductor having a larger band gap than silicon. The wide band gap semiconductor is, for example, silicon carbide, gallium nitride-based material, or diamond. A semiconductor chip made of such a wide band gap semiconductor has high voltage resistance and allowable current density, and can be miniaturized. By using this miniaturized semiconductor chip, a semiconductor device incorporating this semiconductor chip can also be miniaturized and highly integrated. In addition, since the semiconductor chip has high heat resistance, the heat dissipation fins of the heat sink can be miniaturized, and the water-cooled part can be air-cooled, so the semiconductor device can be further miniaturized. In addition, since the power loss of the semiconductor chip is low and highly efficient, the efficiency of the semiconductor device can be increased. [Explanation of symbols]
[0035] REFERENCE SIGNS LIST 1 semiconductor chip, 2 wiring chip, 3 substrate, 5 main electrode, 6 control electrode, 8 first electrode, 9 second electrode, 10 wiring, 13 first bonding material, 15 second bonding material, 16 connection member, 17 sealing material, 18 mold, 19 buffer material, 20 conductive thin film
Claims
1. bonding a semiconductor chip having a main electrode and a control electrode to a substrate; a step of bonding a wiring chip having a first electrode, a second electrode, and wiring connecting the first electrode and the second electrode to the substrate; a step of joining a main electrode member to the main electrode via a joining material; connecting the control electrode and the first electrode with a connecting member; and placing the joined semiconductor chip, the substrate, the wiring chip, the main electrode member, and the connection member into a metal mold, and injecting a sealing material into the metal mold while pressing a tip end surface of the main electrode member against a buffer material provided between the main electrode member and the metal mold, thereby sealing the semiconductor chip, the substrate, the wiring chip, the main electrode member, and the connection member with the sealing material. a tip portion of the main electrode member protrudes from an upper surface of the sealing material, 4. A method for manufacturing a semiconductor device, comprising the steps of: forming a sealing material on a side surface of the tip portion; forming a sealing material having a tapered shape whose thickness becomes thinner toward the tip surface;
2. bonding a semiconductor chip having a main electrode and a control electrode to a substrate; a step of joining a main electrode member to the main electrode via a joining material; and placing the joined semiconductor chip, the substrate, and the main electrode member in a mold, and injecting a sealing material into the mold while pressing a tip end surface of the main electrode member against a buffer material provided between the main electrode member and the mold, thereby sealing the semiconductor chip, the substrate, and the main electrode member with the sealing material. a tip portion of the main electrode member protrudes from an upper surface of the sealing material, 4. A method for manufacturing a semiconductor device, comprising the steps of: forming a sealing material on a side surface of the tip portion; forming a sealing material having a tapered shape whose thickness becomes thinner toward the tip surface;
3. 3. The method for manufacturing a semiconductor device according to claim 1, wherein the sealing material is not ground.
Citation Information
Patent Citations
Chip-type semiconductor device
JP2002252318A
Method for resin-sealing semiconductor chip and film for releasing semiconductor chip resin-sealing mold
JP2002280403A
Electronic component and manufacturing method therefor
JP2002343917A
Power semiconductor unit, power module, and their production process
JP2012028595A
Power converter
WO2010147202A1