Joint body and method for producing the same
A joined body with a Sn-Bi layer and Sn-Bi-In layer on flexible base materials addresses the challenges of bonding electronic components on wearable devices, ensuring reliable connections and improved wetting and spreading, thereby enhancing the reliability of wearable devices.
Patent Information
- Application Number
- JP2023067726
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-18
- Publication Date
- 2024-10-30
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing low-temperature solder pastes, such as Sn-Bi eutectic solder paste with a melting point of 139°C, fail to melt during reflow at 120°C, preventing the mounting of electronic components on flexible and stretchable base materials used in wearable devices, while adding In to Sn-Bi solder paste causes oxidation and increased viscosity, reducing wetting and spreading, leading to reduced connection areas and increased crack likelihood.
A joined body comprising a base material with a Sn-Bi layer and a Sn-Bi-In layer that covers the entire surface of the Sn-Bi layer, supported by the base material, ensuring reliable bonding at a lower melting point and improved wetting and spreading.
The solution expands the connection area and enhances reliability by using a Sn-Bi-In layer with a melting point of 120°C or lower, preventing cracks during temperature cycles and maintaining strength.
Smart Images

Figure 2024154098000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a bonded body for bonding a substrate and an electrode land and a manufacturing method thereof, and in particular to a bonded body for low-temperature mounting of Sn-Bi-In solder paste and component electrode lands with Ni plating / Au flash plating, and a manufacturing method thereof. [Background technology]
[0002] In recent years, the need to acquire daily biometric information and manage health in daily life is increasing due to the health consciousness of people. These biometric devices are changing from wearable devices that are worn consciously to wearable devices that are attached unconsciously.
[0003] Currently, most circuit boards are generally made of resin substrates such as FR-4 or polyimide, and the electrode lands of electronic components are joined to the circuit board at a reflow temperature of 260°C using Sn-Ag-Cu solder paste with a melting point of 227°C.
[0004] On the other hand, to construct wearable devices, the circuit substrate needs to be flexible and stretchable. However, the heat resistance of flexible and stretchable substrates (such as PET and urethane) is around 130°C, and so solder paste materials with a reflow temperature of 130°C or less, which is lower than the heat resistance of the substrate, are required in the reflow process for mounting electronic components. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Patent No. 5090349 Summary of the Invention [Problem to be solved by the invention]
[0006] A typical low-temperature solder paste used when mounting heat-resistant components is a Sn-Bi eutectic solder paste with a melting point of 139°C, which is bonded at a reflow temperature of 160°C. However, the melting point of the Sn-Bi eutectic solder paste is 139°C, which is higher than the melting point of the elastic base material, which is around 120°C. As a result, the Sn-Bi eutectic solder paste does not melt during reflow at 120°C, making mounting impossible. To lower the melting point, a low-temperature solder paste material has been developed in which In is added to Sn-Bi to lower the melting point to 96°C (see, for example, Patent Document 1).
[0007] On the other hand, electronic components used in wearable devices need to be mounted in LGA type packages, which are denser and have a lower profile than conventional QFP, SOP, and BGA packages.Generally, unlike BGA, the electrode lands of LGA packages, which do not have solder balls, have a structure where Au is flashed to prevent oxidation of Ni after Ni plating.
[0008] However, adding In to Sn-Bi solder paste causes the In to oxidize and viscosity to increase during reflow. The increase in viscosity during mounting significantly reduces the amount of wettability and spread to the electrode land of the component, and the Ni and Au plating on the electrode land of electronic components has a high melting point, so wettability and spread is small. As a result, the solder wettability decreases and the connection area decreases. The reduced connection area can make cracks more likely to occur during reliability tests (such as temperature cycle tests) after component mounting, which can reduce product reliability.
[0009] The present disclosure is intended to solve the above-mentioned problems in the conventional art, and has an object to provide a highly reliable bonded body using a substrate for device mounting that requires flexibility and stretchability. [Means for solving the problem]
[0010] The bonded structure according to the present disclosure is a bonded structure including a substrate, an electrode land disposed opposite the substrate, and a bonding portion bonding the substrate and the electrode land, the bonding portion including a Sn—Bi layer provided on the electrode land, and a Sn—Bi-In layer covering the entire surface of the Sn—Bi layer and supported by the substrate. A method for producing a joint according to the present disclosure includes the steps of forming a Sn-Bi layer on an electrode land of an electronic component, providing a Sn-Bi-In solder paste on a substrate having a circuit formed thereon, and melting the Sn-Bi-In solder paste so as to cover the Sn-Bi layer in a plan view from the substrate toward the electrode land, thereby joining the electrode land and the substrate, and mounting the electronic component on the substrate. Effect of the Invention
[0011] According to the bonded structure of the present disclosure, a circuit board for device mounting, which requires flexibility, and an electrode land are bonded at a bonded portion including a Sn—Bi layer and a Sn—Bi—In layer, thereby making it possible to increase the connection area and improve reliability. [Brief description of the drawings]
[0012] [Figure 1] FIG. 2(a) is a planar perspective view transparently showing the planar configuration of a bonded body according to the first embodiment, and FIG. 2(b) is a schematic cross-sectional view showing the cross-sectional configuration of the bonded body of FIG. [Figure 2A] FIG. 2 is a schematic cross-sectional view showing a cross-sectional configuration of a Sn—Bi layer before preforming onto an electrode land of an electronic component. [Figure 2B] 2B is a schematic cross-sectional view showing a cross-sectional configuration after a Sn—Bi layer is preformed on the electrode land in FIG. 2A. [Diagram 3] 4 is a flowchart of a method for manufacturing a bonded body according to the first embodiment. [Figure 4] FIG. 13 is a diagram showing the wet spread rate of the wet area after bonding and the reliability results with and without the Sn—Bi layer preform. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] The bonded body according to the first aspect is a bonded body comprising a substrate, an electrode land arranged opposite the substrate, and a bonding portion bonding the substrate and the electrode land, the bonding portion having a Sn-Bi layer provided on the electrode land, and a Sn-Bi-In layer covering the entire surface of the Sn-Bi layer and supported by the substrate.
[0014] A bonded structure according to a second aspect is the bonded structure according to the first aspect, wherein the electrode land has a Ni plating layer.
[0015] A bonded body according to a third aspect may be configured such that, in a plan view from the substrate toward the electrode land, the outer diameter of the Sn—Bi—In layer includes the outer diameter of the Sn—Bi layer and extends outward.
[0016] A bonded body according to a fourth aspect may be such that in the first aspect, the Sn—Bi layer has a protrusion along a direction from the electrode land toward the substrate, and the height of the protrusion along the direction is 15 μm to 50 μm.
[0017] A bonded body according to a fifth aspect may be the same as that of the first aspect, wherein the Sn-Bi layer has a Bi content of 44 to 61 atm%, and the Sn-Bi-In layer has a Sn content of 1 to 40 atm%, a Bi content of 10 to 70 atm%, and an In content of 15 to 75 atm%.
[0018] A bonded body according to a sixth aspect is the bonded body according to the first aspect, wherein the electrode land is provided on the electronic component, and the electronic component and the substrate are bonded together by the bonded body.
[0019] A bonded structure according to a seventh aspect is the same as that of the first aspect, in which the base material has stretchability.
[0020] A method for producing a joint body according to an eighth aspect includes the steps of forming a Sn-Bi layer on an electrode land of an electronic component, providing a Sn-Bi-In solder paste on a substrate having a circuit formed thereon, and melting the Sn-Bi-In solder paste so as to cover the Sn-Bi layer in a plan view from the substrate toward the electrode land, thereby joining the electrode land and the substrate, and mounting the electronic component on the substrate.
[0021] Hereinafter, a bonded body and a manufacturing method thereof according to embodiments of the present disclosure will be described with reference to the accompanying drawings.
[0022] (Embodiment 1) 1(a) is a planar perspective view transparently showing the planar configuration of the bonded body according to embodiment 1, and (b) is a schematic cross-sectional view showing the cross-sectional configuration of the bonded body of (a). For convenience, the direction from the substrate 101 toward the electrode land 102 is shown as the Z direction (vertically upward), and the in-plane of the substrate 101 and the in-plane of the electrode land 102 are shown as the XY plane. The bonded body 110 according to the first embodiment includes an elastic substrate 101 on which a circuit is formed, an electrode land 102 of an electronic component 100 disposed opposite the substrate 101, and a bonding portion 109 bonding the substrate 101 and the electrode land 102. The electrode land 102 has a Ni plating 106 / Au flash plating 107 on its surface. The bonding portion 109 has a Sn-Bi layer 103 preformed on the electrode land 102, and a Sn-Bi-In layer 104 covering the entire surface of the Sn-Bi layer. In this joint 110, the Sn-Bi-In layer 104, which is a low-temperature solder material, covers the entire surface of the Sn-Bi layer 103 preformed on the electrode land, and also spreads widely over the surface of the Ni plating 106 of the electrode land 102, thereby increasing the connection area and improving reliability. Also, the melting point of the Sn-Bi layer 102 preformed on the electrode land is higher than that of the Sn-Bi-In layer 104, and therefore, even when subjected to a temperature cycle, it is difficult to melt, which is expected to have the effect of delaying the progress of cracks, and the strength can be maintained.
[0023] The components of this bonded body 110 will now be described.
[0024] <Stretch base material 101> The stretchable substrate 101 is an anisotropic sheet that can stretch in one or more directions. Hereinafter, it may be referred to as "stretchable substrate". The stretchability of the stretchable substrate 101 is preferably 10% to 60%, assuming that the stretchability is 100% when no tensile force is applied. In stretching the surface of the human body, a maximum of 50% stretch occurs during bending and straightening of the knee. Since it is necessary to function even at this stretchability, the stretchability is set to 60%. The stretchability of the stretchable substrate 101 is a stretchability that allows elastic deformation. The material of the elastic base material 101 may be, for example, a urethane-based elastomer, a silicone-based elastomer, nitrile rubber, latex rubber, a thermosetting elastic resin, etc. The thickness of the elastic base material 101 is determined by the required elongation rate of the part where it is used. For example, when used on the chest as a wearable electrocardiogram sensor, if the skin on the chest stretches by 20%, the elastic base material 101 is made of a material having an elongation rate of 20% or more.
[0025] <Electronic components> The electronic component 100 is, for example, a quad flat non-leaded package (QFN), a ceramic LGA, a plastic LGA, or the like. <Electronic component electrode land 102> 2A is a schematic cross-sectional view showing a cross-sectional configuration of an Sn-Bi layer before preforming on an electrode land 102 of an electronic component 100. The electrode land 102 is, for example, a Ni plating 106, and may have an Au flash plating 107 on its surface. The Ni plating 106 is obtained, for example, by applying a Ni plating 106 treatment to a thickness of 0.2 to 1 μm by electrolytic or electroless plating on a copper or iron component electrode. In addition, an Au flash plating 107 treatment to a thickness of 0.005 μm or less may be applied on the Ni plating 106 by electrolytic or electroless plating. In addition, in order to reduce the amount of Au used, a Pd plating to a thickness of 0.05 μm or less may be applied between the Ni plating 106 and the Au flash plating layer.
[0026] <Sn-Bi layer 103> FIG. 2B is a schematic cross-sectional view showing a cross-sectional configuration after preforming the Sn-Bi layer 103 on the electrode land 102 of FIG. 2A. The Sn-Bi layer may have, for example, a Bi content of 44 to 61 atm%. It may also be Bi 58 atm% which is an eutectic composition. The composition of the Sn-Bi solder paste has a melting point of 120° C. or higher and preferably 160° C. or lower. Further, a solder paste with a melting point of 138° C. with 58 wt% Bi and the balance being Sn is preferred. That is, it is to prevent the Sn-Bi layer 103 from being melted by the heat during mounting at the time of reflow mounting of the stretchable base material 101 and the electronic component (temperature of 120° C. or lower). Also, the shape of the Sn-Bi layer preferably has a convex portion with a convex shape along the normal direction (vertical direction) of the surface of the electrode land 102. As shown in FIGS. 1(b) and 2B, the Sn-Bi layer 103 has a convex portion with a convex shape vertically downward. Due to this convex portion, the Sn-Bi-In solder paste during mounting easily spreads around the Sn-Bi layer. Also, the Au flash plating 107 of the electrode land 102 diffuses to the Sn-Bi layer 103 when the Sn-Bi layer is formed on its surface, and forms a Ni-Sn alloy layer with the Sn of the Sn-Bi layer 103 and the Ni plating of the electrode land 102. The Sn-Bi layer 103 may be formed, for example, by using an Sn-Bi solder paste on the electrode land 102 to form the Sn-Bi layer 103.
[0027] <Sn-Bi-In layer 104> The Sn-Bi-In layer 104 has a basic composition including Sn, Bi, and In, for example, 1 to 40 atm% Sn, 10 to 70 atm% Bi, and 15 to 75 atm% In. When the above composition range is expressed by a ternary phase diagram of (Sn, Bi, In), it is each side and the inside of a hexagon with vertices of (Sn40, Bi45, In15), (Sn15, Bi70, In15), (Sn1, Bi70, In29), (Sn1, Bi24, In75), (Sn15, Bi10, In75), and (Sn40, Bi10, In50). In the above composition range, the Sn-Bi-In layer 104 has a melting point of 120° C. or less. Alternatively, when expressed on a weight basis, it may contain 50 to 70 wt % Bi, 10 to 24.5 wt % In, and the balance Sn. Specifically, for example, the Sn-Bi-In layer 104 may be made of 55% by weight Bi, 20% by weight In, and the remainder Sn, with a melting point of 96° C. In a plan view from the substrate 101 toward the electrode land 102, the outer diameter of the Sn-Bi-In layer 104 may include the outer diameter of the Sn-Bi layer 103 and may extend outward. In FIG. 1, the Sn—Bi—In layer 104 is shown to have the same outer diameter as the electrode land 102 (106), but is not limited to this and may extend larger than the outer diameter of the electrode land 102 (106). The Sn—Bi—In layer 104 may be mounted by applying an Sn—Bi—In solder paste to the base material 101, heating and melting it in a reflow furnace, and covering the entire surface of the Sn—Bi layer 103.
[0028] <Method of manufacturing the bonded body> 3 is a flowchart showing the method for producing the bonded body according to embodiment 1. The method for producing the bonded body will be described below. (1) An electronic component 100 having an electrode land 102 made of Ni plating 106 / Au flash plating 107 is prepared. (2) A Sn-Bi layer 103 is preformed on the Ni plating 106 / Au flash plating 107 of the electrode lands 102 of the electronic component 100. Specifically, a Sn-Bi solder paste is printed on the Ni plating 106 / Au flash plating 107 of the electrode lands 102 of the electronic component using a printing mask with openings having the same diameter as the electrode lands 102 or smaller than the electrode lands 102. (3) Next, the electronic components on which the Sn—Bi solder paste is printed on the electrode lands 102 are melted by heating (reflow) to form a Sn—Bi layer on the electrode lands 102 . (4) Next, a stretchable base material 101 is placed opposite the electrode lands. (5) After that, Sn-Bi-In solder 104 is applied onto base material 101 and heated in a reflow furnace to melt the Sn-Bi-In solder 104 so as to cover the Sn-Bi layer 103 on electrode lands 102, and mounting is performed. In this way, electrode lands 102 and base material 101 are joined by a joint consisting of Sn-Bi layer 103 and Sn-Bi-In layer 104. In this manner, a bonded body 110 including the electrode land 102, the base material 101, and the bonded portion can be obtained. The Au flash plating 107 of the electrode land 102 is diffused into the Sn-Bi solder paste, and a Ni-Sn alloy layer is formed at the bonded interface by the Ni plating 106 and the Sn of the Sn-Bi-In solder 104.
[0029] <Example> A bonded body and a manufacturing method thereof according to an embodiment of the present disclosure will be described. (1) As the electronic component, an LGA 228-pin package 101 (manufactured by Amkor) with an electrode land diameter of 0.3 mmΦ and an electrode configuration of the electrode land 102 with Ni plating 106 / Au flash plating 107 was used. (2) Next, a Sn-Bi solder paste (manufactured by Koki Co., Ltd.) with a melting point of 138° C. and 58% by weight of Bi with the remainder being Sn was applied using a printing mask with the same diameter as the electrode land 102 and a thickness of 80 μm. (3) After that, the electronic component to which the Sn-Bi solder paste was supplied was placed in a reflow furnace (made by Senju Metal Co., Ltd.) to melt the Sn-Bi solder paste at a temperature of 160°C, forming a Sn-Bi layer 103 having a convex portion in a normal direction (vertical direction) of the surface of the electrode land. The height of the convex portion of the formed Sn-Bi layer 103 was about 30 μm, and the solder paste was supplied so that the height of the convex portion was in the range of 15 μm to 90 μm. It is preferable that the height of the convex portion is 15 μm to 50 μm. If the height of the convex portion is less than 15 μm, the Sn-Bi-In solder paste 104 does not wet and spread around the Sn-Bi layer 103 formed on the electrode land 102, so that the connection area after mounting is reduced. Also, if the height of the convex portion is more than 90 μm, the connection height after mounting is increased, so that a decrease in strength occurs.
[0030] The formation of the Sn--Bi layer 103 on the protrusions is preferably carried out using a solder paste, since using electrolytic or electroless processing increases processing costs and causes problems such as infiltration of plating solution into the package. Furthermore, when supplying the solder paste using a printing mask, the shape of the printing mask is the same as the land diameter of the electrode lands 102 or the diameter of the printing mask is smaller than the land diameter of the electrode lands 102, which makes it easier to form the convex portions. The amount of solder paste required to form the convex Sn-Bi layer 103 varies depending on the area of the electrode land 102 of the electronic component, so the amount of solder paste is adjusted according to the thickness of the printing mask and the area of the mask opening. If the diameter of the electrode land is small, it is recommended to supply the solder paste by dispenser or solder ball.
[0031] (4) Next, the electrode land 102 of the electronic component and the expandable substrate 101 on which the circuit was formed were bonded in a reflow furnace (made by Senju Metal Co., Ltd.) at a reflow temperature of 120° C. Specifically, Sn-Bi-In solder paste was applied to the electrodes of the urethane sheet (thickness 0.1 mm, elongation rate 600%), which was the expandable substrate 101 on which the circuit was formed, using a printing mask with a thickness of 80 μm. The Sn-Bi-In solder paste used had a melting point of 96° C. and was composed of 55% by weight Bi, 20% by weight In, and the remainder Sn.
[0032] In a cross-sectional observation after mounting, it was confirmed that the Sn—Bi layer 103 was present in a convex shape and was covered with the composition of the Sn—Bi—In solder paste 105 . FIG. 4 is a diagram showing the wet spread rate of the wet area after bonding and the reliability results in relation to the presence or absence of the Sn—Bi layer preform, which was evaluated this time.
[0033] The reliability test was performed in accordance with JIS C 600682-14 (IEC60068). The reliability test was performed at a temperature cycle of -40℃ to +85℃. The temperature cycle was repeated by holding at -40℃ for 15 minutes, increasing the temperature from -40℃ to +85℃, holding at +85℃ for 15 minutes, and decreasing the temperature from +85℃ to -45℃. Specifically, the electronic components and the substrate were connected in a daisy chain so that the stress change of the joints of all the terminals could be confirmed by the resistance value. The evaluation was performed by measuring the total resistance value (initial resistance value: 1.9Ω) of all the daisy chained terminals, and then measuring the resistance value at 100, 250, 500, 750, 1000, and 1500 cycles. If the resistance value was 3.8Ω or more, which is twice the initial resistance value, it was judged as NG. For example, if the evaluation was NG at 1000 cycles, the actual performance was set at 750 cycles. The increase in resistance is believed to occur, for example, when cracks caused by temperature cycles progress from the ends of the joint to the inside, resulting in a reduction in the joint area.
[0034] According to the evaluation results in Figure 4, it can be seen that the wettability of the solder paste is improved when the Sn-Bi layer is provided on the joint and the Sn-Bi-In layer covering the entire surface of the Sn-Bi layer is included, compared to the joint area when there is no Sn-Bi layer on the joint. In other words, the joint area is increased. [Industrial Applicability]
[0035] The bonded body according to the present disclosure can be used for electronic components requiring high reliability by bonding a circuit board for device mounting, which requires flexibility, and an electrode land made of Ni plating / Au flash plating at a recessed portion including a Sn-Bi layer and a Sn-Bi-In layer. [Explanation of symbols]
[0036] 100 Electronic Components 101 Stretchable base material 102 Electrode Land 103 Sn-Bi layer 104 Sn-Bi-In solder paste 105 Sn-Bi eutectic solder paste 106 Ni plating 107 Au flash plating 108 LGA Package 109 Joint 110 Zygote
Claims
1. A substrate; An electrode land disposed opposite the substrate; a joint portion that joins the base material and the electrode land; A joint comprising: The joint is a Sn—Bi layer provided on the electrode land; a Sn—Bi—In layer covering the entire surface of the Sn—Bi layer and supported by the substrate; having zygote.
2. The joined body according to claim 1 , wherein the electrode land has a Ni plating layer.
3. 2. The joined body according to claim 1, wherein, in a plan view from the substrate toward the electrode land, an outer diameter of the Sn--Bi--In layer includes an outer diameter of the Sn--Bi layer and expands outward.
4. 2. The joined body according to claim 1, wherein the Sn—Bi layer has a protrusion along a direction from the electrode land toward the substrate, and the height of the protrusion along the direction is 15 μm to 50 μm.
5. The Sn—Bi layer has a Bi content of 44 to 61 atm %, 2. The joined body according to claim 1, wherein the Sn--Bi--In layer has an Sn content of 1 to 40 atomic %, a Bi content of 10 to 70 atomic %, and an In content of 15 to 75 atomic %.
6. The bonded body according to claim 1 , wherein the electrode land is provided on an electronic component, and the electronic component and the base material are bonded together by the bonded body.
7. The bonded structure according to claim 1 , wherein the substrate has elasticity.
8. forming a Sn—Bi layer on an electrode land of an electronic component; providing a Sn-Bi-In solder paste on the circuitized substrate; a step of melting the Sn—Bi—In solder paste so as to cover the Sn—Bi layer in a plan view from the substrate toward the electrode land, thereby joining the electrode land and the substrate, and mounting the electronic component on the substrate; A method for producing a bonded body, comprising: