Manufacturing method for lithium ion battery, and lithium ion battery
The novel manufacturing method for lithium ion batteries using a Li alloying potential of 0.5V (vs Li/Li+) positive electrode precursor layer addresses the capacity loss issue by reducing Li consumption during initial charging, enhancing battery performance.
Patent Information
- Application Number
- JP2023070325
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-21
- Publication Date
- 2024-10-31
- Estimated Expiration
- 2043-04-21
AI Technical Summary
Conventional lithium ion batteries experience a significant decrease in capacity after initial charging due to Li consumption during the formation of the Solid Electrolyte Interphase (SEI) in the negative electrode.
A novel manufacturing method involving a positive electrode precursor layer with a Li alloying potential of 0.5V (vs Li/Li+) or more, which includes a positive electrode active material, is used to suppress Li consumption by releasing it during the first charge, forming a positive electrode active material layer.
This method effectively prevents the decrease in capacity by minimizing Li consumption for SEI formation, resulting in improved battery performance.
Smart Images

Figure 2024155534000002 
Figure 2024155534000001
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a method for manufacturing a lithium-ion battery, and to a lithium-ion battery. [Background technology]
[0002] Conventionally, in order to increase the capacity of lithium ion batteries, the active materials have been improved.
[0003] Patent Document 1 discloses an electrode for use in a non-aqueous electrolyte secondary battery. The specific surface area of the negative electrode active material of this electrode, measured by the N2 adsorption method, is 3.3 m 2 / g or more and 4.4m 2 / g or less. The positive electrode active material of this electrode has a DBP oil absorption of 30 ml / 100 g or more and 47 ml / 100 g or less. The positive electrode density is 1.8 g / cm 3 More than 2.2g / cm 3 The details are as follows: Patent Document 1 discloses that the capacity of the negative electrode is increased by using a lithium (Li) alloy as an active material.
[0004] In addition, nickel-cobalt-manganese (NCM) lithium oxide is widely used as a positive electrode active material, and improvements to its composition are also being considered. Specifically, Non-Patent Document 1 discloses that the capacity of the positive electrode can be increased by increasing the ratio of nickel (Ni) in NCM lithium oxide as a positive electrode active material. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2014-010991 A Summary of the Invention [Problem to be solved by the invention]
[0006] When conventional electrodes such as the electrode of Patent Document 1 were used, a significant decrease in capacity was sometimes observed after the initial charge.
[0007] The present disclosure provides a novel method for producing a lithium ion battery, which can suppress a decrease in capacity after an initial charge, and a lithium ion battery. [Means for solving the problem]
[0008] As a result of intensive research, the present inventors have found that the above problems can be solved by the following means, and have completed the present disclosure. That is, the present disclosure is as follows: <Mode 1> Lithium alloying potential is 0.5V (vs Li / Li + and a positive electrode precursor layer containing at least a lithium alloy having a positive electrode active material and a positive electrode active material. providing a lithium ion battery precursor having the positive electrode precursor layer, a separator layer, and a negative electrode active material layer in this order and impregnated with an electrolyte; and performing an initial charge on the lithium ion battery precursor to convert the positive electrode precursor layer into a positive electrode active material layer; A method for producing a lithium ion battery, comprising: Aspect 2: The method of aspect 1, wherein the lithium alloy is selected from the group consisting of Li3Bi, Li3Sb, and NiSn. Aspect 3: The method according to aspect 1 or 2, wherein the positive electrode active material is an NCM lithium oxide. Aspect 4: A positive electrode active material layer, a separator layer, and a negative electrode active material layer in this order, The positive electrode active material layer contains a positive electrode active material, and at least one of bismuth element and antimony element. Lithium-ion battery. Effect of the Invention
[0009] According to the present disclosure, it is possible to provide a novel method for manufacturing a lithium ion battery, and a novel lithium ion battery, which can suppress a decrease in capacity after an initial charge. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a schematic diagram of a lithium ion battery of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] <<How lithium-ion batteries are manufactured>> The disclosed method of producing a lithium ion battery includes: Lithium alloying potential (Li alloying potential) is 0.5V (vs Li / Li + ) or more, and a positive electrode precursor layer containing at least a positive electrode active material; Obtaining a lithium ion battery precursor having the positive electrode precursor layer, a separator layer, and a negative electrode active material layer in this order and impregnated with an electrolytic solution; and performing an initial charge on the lithium ion battery precursor to convert the positive electrode precursor layer into a positive electrode active material layer; Includes.
[0012] The present inventors have found that the cause of the decrease in battery capacity described in Patent Document 1 is that Li supplied in the initial positive electrode active material is consumed due to the formation of a solid electrolyte interphase (SEI) in the negative electrode during the first charge.
[0013] In response to this, the present inventors have found that the capacity can be improved by obtaining a lithium ion battery using the above-mentioned positive electrode precursor layer. Although not wishing to be bound by theory, this is believed to be because Li from the Li alloy in the positive electrode precursor layer is released during the first charge and becomes Li consumed for SEI formation in the negative electrode, thereby suppressing the consumption of Li in the positive electrode active material for SEI formation. In addition, when the Li alloying potential of the Li alloy is 0.5 V (vs Li / Li + ) or more, it is believed that the occurrence of an electrochemical reaction inside the positive electrode precursor before the first charge can be suppressed.
[0014] Each component of the present disclosure will be described below.
[0015] <Preparation of Positive Electrode Precursor Layer> The positive electrode precursor layer is a Li alloying layer with a Li alloying potential of 0.5 V (vs Li / Li + ) or more, and a positive electrode active material. The positive electrode precursor layer may contain other optional substances. Examples of the other substances include a conductive assistant and a binder.
[0016] The positive electrode precursor layer can be prepared by mixing the respective materials constituting the layer and applying the mixture.
[0017] (Li alloy) Li alloys have a Li alloying potential of 0.5V (vs Li / Li + ) or higher. This Li alloying potential is 0.6V (vs Li / Li + ) or more, 0.7V(vs Li / Li + ) or more, or 0.8V(vs Li / Li + ) or more, and 1.5V (vs Li / Li + ) or less, 1.4V (vs Li / Li + ) or less, 1.3V (vs Li / Li + ) or less, 1.2V (vs Li / Li + ) or less, 1.1V (vs Li / Li + ) or less, 1.0V (vs Li / Li + ) or less.
[0018] Here, the Li alloying potential (vs Li / Li + ) is the electrode potential of the electrode reaction of formula (1) and is expressed based on the electrode potential of lithium of the following formula (2): xLi + +M+xe - ←→ Li x M (1) Li + +e - ←→ Li (2)
[0019] This Li alloying potential (vs Li / Li + ) can be measured as the monopolar potential obtained when the alloy is immersed in a salt solution of Li.
[0020] As such Li alloys, for example, Li3Bi, Li3Sb, NiSn, etc. can be used.
[0021] (Cathode active material) As the cathode active material, any arbitrary cathode active material can be used, and it is not particularly limited. For example, a lithium-containing oxide can be used.
[0022] The lithium-containing oxide as the cathode active material is not particularly limited, and for example, it may contain at least Li, at least one transition metal element selected from Co, Ni, and Mn, and O. As such lithium-containing oxides, for example, lithium cobalt oxide (LiCoO2), lithium nickel oxide (LiNiO2), lithium manganate (LiMn2O4), nickel-cobalt-manganese (NCM) lithium oxide in which some of these elements are substituted with other elements can be used. The NCM lithium oxide is generally represented by the general formula Li a Mn x Ni y Co z O 2±δ (0 < a ≦ 1.5, 0 ≦ x ≦ 1.5, 0 ≦ y ≦ 1.5, 0 ≦ z ≦ 1.5, 0 < δ(=x + y + z) < 1.5). The lithium-containing oxide as the cathode active material may have, for example, an O2-type structure, an O3-type structure, or a crystal structure other than these. As the cathode active material, only one type may be used alone, or two or more types may be used in combination.
[0023] (Conductive assistant) The conductive assistant optionally contained in the positive electrode precursor layer may be a known conductive assistant used in lithium ion batteries. Specifically, carbon materials such as Ketjen Black (KB), vapor grown carbon fiber (VGCF), acetylene black (AB), carbon nanotube (CNT), carbon nanofiber (CNF), carbon black, coke, graphite, etc. may be used. Alternatively, metal materials capable of withstanding the environment during use of the battery may be used. As the conductive assistant, only one type may be used alone, or two or more types may be used in combination. The conductive assistant may be in various forms such as powder and fiber. The amount of the conductive assistant contained in the positive electrode active material layer is not particularly limited.
[0024] (binder) The binder optionally contained in the positive electrode precursor layer may be any binder known to be used in lithium ion batteries. For example, styrene butadiene rubber (SBR)-based binder, carboxymethyl cellulose (CMC)-based binder, acrylonitrile butadiene rubber (ABR)-based binder, butadiene rubber (BR)-based binder, polyvinylidene fluoride (PVDF)-based binder, polytetrafluoroethylene (PTFE)-based binder, etc. may be used. Only one type of binder may be used alone, or two or more types may be used in combination. The amount of binder contained in the positive electrode active material layer is not particularly limited.
[0025] Preparation of Lithium-Ion Battery Precursor The lithium ion battery precursor has a positive electrode precursor layer, a separator layer, and a negative electrode active material layer in this order, and is impregnated with a non-aqueous electrolyte solution. This lithium ion battery precursor may be produced by a known method.
[0026] The lithium ion battery precursor may further include a positive electrode current collector layer and a negative electrode current collector layer.
[0027] Each component of the lithium ion battery precursor will now be described.
[0028] (Positive electrode current collector layer) The positive electrode current collector layer may be made of a known metal that can be used as a positive electrode current collector for a lithium ion battery. Examples of such metals include metal materials containing at least one element selected from the group consisting of Cu, Ni, Al, V, Au, Pt, Mg, Fe, Ti, Pb, Co, Cr, Zn, Ge, In, Sn, and Zr. The form of the positive electrode current collector is not particularly limited. It may take various forms such as a foil, a mesh, or a porous form. The above metal may be vapor-deposited or plated on the surface of a substrate.
[0029] (Separator) The separator may be a known separator used in lithium ion batteries. For example, the separator may be made of a resin such as polyethylene (PE), polypropylene (PP), polyester, or polyamide. The separator may have a single layer structure or a multi-layer structure. As the multi-layer separator, for example, a multi-layer separator made of the above resin, for example, a separator with a two-layer structure of PE / PP, or a separator with a three-layer structure of PP / PE / PP or PE / PP / PE, etc. may be used. The separator may be made of a nonwoven fabric such as a cellulose nonwoven fabric, a resin nonwoven fabric, or a glass fiber nonwoven fabric. The thickness of the separator is not particularly limited, and may be, for example, 5 μm or more and 1 mm or less.
[0030] (Negative electrode active material layer) The negative electrode active material layer contains a negative electrode active material. The negative electrode active material layer may contain other optional components. Examples of the other components include a conductive assistant and a binder. For the conductive assistant and the binder, the description of the positive electrode active material layer can be referred to.
[0031] (Negative electrode active material layer: negative electrode active material) As the negative electrode active material, various materials having a potential (charge / discharge potential) for absorbing and releasing ions that is lower than the above-mentioned positive electrode active material may be used. As the negative electrode active material, for example, silicon-based active materials such as Si, Si alloys, and silicon oxide; carbon-based active materials such as graphite, graphite, and hard carbon; various oxide-based active materials such as lithium titanate; metallic lithium, lithium alloys, and the like may be used. As the negative electrode active material, only one type may be used alone, or two or more types may be used in combination.
[0032] (Negative electrode current collector layer) The negative electrode current collector layer may be made of a known metal that can be used as a negative electrode current collector for a lithium ion battery. Such a metal may be, for example, a metal material containing at least one element selected from the group consisting of Cu, Ni, Al, V, Au, Pt, Mg, Fe, Ti, Pb, Co, Cr, Zn, Ge, In, Sn, and Zr. The form of the negative electrode current collector layer is not particularly limited, and may be in various forms such as a foil, a mesh, or a porous form. The negative electrode current collector layer may be a layer in which the above-mentioned metal is plated or vapor-deposited on the surface of a substrate made of any material. The surface of the negative electrode current collector layer may be coated with a carbon material or the like.
[0033] (Non-aqueous electrolyte) The non-aqueous electrolyte may contain a non-aqueous solvent and an electrolyte. The electrolyte may contain alkali metal ions, such as lithium ions, as carrier ions.
[0034] The non-aqueous solvent may be a solvent other than water, for example, an organic solvent. As the organic solvent, for example, a carbonate solvent such as ethylene carbonate (EC), dimethyl carbonate (DMC), ethyl methyl carbonate (EMC), fluoroethylene carbonate (FEC) or the like may be used. These organic solvents may be used alone or in combination.
[0035] The electrolyte is not particularly limited and may be, for example, a lithium salt. As the lithium salt, for example, LiPF6 or the like can be used.
[0036] <Preparation of Positive Electrode Active Material Layer> The positive electrode active material layer is produced by initially charging the lithium ion battery precursor to convert the positive electrode precursor layer into a positive electrode active material layer.
[0037] By initially charging the lithium ion battery precursor having the positive electrode layer precursor layer, the Li of the Li alloy is consumed for the formation of SEI in the negative electrode. As a result, when the Li alloy contains at least one of Li3Bi and Li3Sb, the resulting positive electrode active material layer contains at least one of bismuth element and antimony element.
[0038] The initial charging conditions may be known conditions.
[0039] Lithium-ion battery The lithium ion battery of the present disclosure comprises: A positive electrode active material layer, a separator layer, and a negative electrode active material layer, The positive electrode active material layer contains a positive electrode active material, and at least one of elemental bismuth and elemental antimony.
[0040] FIG. 1 is a schematic diagram showing a configuration of a lithium-ion battery 100 according to one embodiment of the present disclosure. As shown in FIG. 1, the lithium-ion battery 100 may include a positive electrode 10, a separator 20, and a negative electrode 30. The positive electrode 10 may include a positive electrode active material layer 11 and a positive electrode current collector layer 12, and the negative electrode 30 may include a negative electrode active material layer 31 and a negative electrode current collector layer 32. In this case, the positive electrode active material layer 11 may include the above-mentioned positive electrode active material. Although not shown, an electrolyte may be included in the positive electrode active material layer 11 and the negative electrode active material layer 31.
[0041] For each component of the lithium ion battery, the description of the manufacturing method can be referred to. EXAMPLES
[0042] The present disclosure will be specifically described with reference to examples and comparative examples, but the present disclosure is not limited thereto.
[0043] <<Making a lithium-ion battery>> Example 1 92.3 mg of LiNi as the positive electrode active material 0.8 Co 0.1 Mn 0.1 O2, 8.4 mg of Li3Bi as a Li alloy, a conductive additive, and a binder were mixed in NMP to prepare a slurry, which was then applied to an Al foil and dried to obtain a positive electrode precursor layer.
[0044] The obtained positive electrode precursor layer was placed opposite to a negative electrode active material layer containing graphite as an active material via a separator layer, and the layers were dried in a vacuum, and a non-aqueous electrolyte was poured therein to obtain a lithium ion battery precursor.
[0045] Examples 2 to 3 and Comparative Examples 1 to 3 Lithium ion battery precursors of Examples 2 to 3 and Comparative Examples 1 to 3 were obtained in the same manner as in Example 1, except that the content of the positive electrode active material and the type and content of the Li alloy were changed as shown in Table 1.
[0046] "evaluation" Based on the mass of the positive electrode active material contained in the cell, the current value at 210 mA / g is defined as 1C rate, the charge / discharge current value is 0.2C, and the end current value is 0.03C, and CCCV charging and CCCV discharging are performed. The upper limit voltage during charging is 4.25V, and the lower limit voltage during discharging is 2.50V. The obtained CCCV discharge capacity is the capacity of the cell and is the evaluation index of this disclosure.
[0047] Table 1 shows the configurations and evaluation results of the examples and comparative examples.
[0048] [Table 1]
[0049] From Table 1, the Li alloying potential is 0.5 V (vs Li / Li + It can be seen that the lithium ion battery of the present disclosure obtained from the Li alloy and positive electrode active material described above can suppress the decrease in capacity of the positive electrode. [Explanation of symbols]
[0050] 10 positive electrode 11 Cathode active material layer 12 Positive electrode current collector 20 Separator 30 negative electrode 31 Negative electrode active material layer 32 Negative electrode current collector 100 Lithium-ion batteries
Claims
1. Lithium alloying potential is 0.5V (vs Li / Li + ) or more, and a positive electrode precursor layer containing at least a positive electrode active material; providing a lithium ion battery precursor having the positive electrode precursor layer, a separator layer, and a negative electrode active material layer in this order and impregnated with an electrolyte; and performing an initial charge on the lithium ion battery precursor to convert the positive electrode precursor layer into a positive electrode active material layer; A method for producing a lithium ion battery, comprising:
2. The lithium alloy is Li 3 Bi, Li 3 2. The method of claim 1 , wherein the metal is selected from the group consisting of Sb, and NiSn.
3. 3. The method of claim 1 or 2, wherein the positive electrode active material is an NCM lithium oxide.
4. A positive electrode active material layer, a separator layer, and a negative electrode active material layer in this order, The positive electrode active material layer contains a positive electrode active material, and at least one of bismuth element and antimony element. Lithium-ion battery.
Citation Information
Patent Citations
Nonaqueous electrolyte secondary battery
JP1991233859A
Lithium ion secondary battery
JP1997293538A
Power storage device
JP2014049420A
All-solid secondary battery
JP2019117768A
Positive electrode for secondary battery, method for producing same, and lithium secondary battery including same
JP2021520614A