Method for manufacturing scale
The use of a water-based paint to create a magnetic scale with a high magnetic powder content and thickness addresses the environmental concerns of traditional solvent-based methods, achieving high magnetic properties and accurate position detection.
Patent Information
- Application Number
- JP2024017065
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-19
- Filing Date
- 2024-02-07
- Publication Date
- 2024-10-31
Smart Images

Figure 2024155728000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a water-based paint, scale produced by using the water-based paint, and a method for producing scale. [Background technology]
[0002] The spindle and table of a machine tool are controlled to move to a target position by driving the saddle that supports them along a guide rail. In order to achieve this movement control with high precision, some machines have a displacement detection device disposed between the saddle and the guide rail. Such a displacement detection device includes a magnetic sensor provided on the saddle side and a scale provided on the guide rail side. The position of the spindle, etc. can be detected by measuring the relative position of the magnetic sensor with respect to the scale.
[0003] A magnetic pattern made of a magnetic material is recorded on the scale. The magnetic sensor is equipped with a detection head for reading the magnetic field of the magnetic pattern. The detection head is composed of a sensor capable of detecting the direction and strength of a magnetic field, such as an MR element (Magneto Resistive Sensor). The detection head detects the magnetic pattern and converts the detection value into an electrical signal, making it possible to measure precise positions on the order of micrometers.
[0004] Conventionally, scales have been produced by coating a non-magnetic support with a magnetic paint made by kneading and dispersing magnetic powder, a binder, a dispersant, a hardener, etc. in an organic solvent (see Patent Document 1). [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2010-49731 A Summary of the Invention [Problem to be solved by the invention]
[0006] However, with the recent rise in environmental awareness, there has been a demand for scale manufacturing that uses as few chemical substances that have an adverse effect on the environment as possible.
[0007] Therefore, the present invention provides a method for manufacturing a scale having a magnetic pattern for detecting relative displacement with an opposing sensor head, comprising the steps of: applying an aqueous paint containing magnetic powder once onto a support to form a wet coating film with a thickness of 200 μm or more; drying the wet coating to form a magnetic layer having a magnetic powder content of 70% or more and a thickness of 200 μm or more; and forming a magnetic pattern in the magnetic layer that can detect relative displacement with a sensor head, wherein the aqueous paint contains water as the main solvent.
[0008] The present invention also provides water-based paints, scales, and the like. Effect of the Invention
[0009] According to the present invention, it is possible to produce scale using as few chemical substances that have an adverse effect on the environment as possible. [Brief description of the drawings]
[0010] [Figure 1] 1 is a perspective view illustrating an appearance of a displacement detection device according to an embodiment. [Diagram 2] FIG. 2 is a cross-sectional view taken along the line AA in FIG. [Diagram 3] FIG. [Figure 4] FIG. [Diagram 5] FIG. 5 is a BB cross-sectional view of the rail shown in FIG. [Figure 6] 1A and 1B are schematic diagrams for explaining an interpolation processing technique for achieving high resolution of a magnetic sensor. [Figure 7] 5 is a cross-sectional view showing a structure of a modified example of the bottom surface of the rail shown in FIG. [Figure 8] 8 is a cross-sectional view showing a state in which a magnetic layer and a cover are disposed on the bottom surface of the rail shown in FIG. 7. [Figure 9] FIG. 2 is a schematic diagram for explaining a die coating. [Figure 10] FIG. 2 is an enlarged cross-sectional view of a main part of the slit die. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Hereinafter, an embodiment of the present invention will be described in detail with reference to the drawings. For convenience of explanation, the X-axis and Y-axis are set in the horizontal direction, and the Z-axis is set in the vertical direction, and the positional relationship of each structure may be expressed based on the illustrated state. In addition, in the following embodiments and their modified examples, substantially the same components are given the same reference numerals, and their explanation will be omitted as appropriate.
[0012] FIG. 1 is a perspective view showing the appearance of a displacement detection device according to an embodiment. The displacement detection device 1 includes a metal rail 4 that guides the movement of a moving body 2, a magnetic layer 5 formed at a predetermined position of the rail 4, and a sensor unit 8 that is provided integrally with the moving body 2. In this embodiment, the displacement detection device 1 detects the position of a movement control target in a machine tool. The movement control target includes, for example, a spindle and a table. Note that the displacement detection device 1 only needs to detect displacement, and does not need to be a target for movement control. For example, it may be a device that detects a displacement of a shape, such as a shape contraction.
[0013] The rail 4 is long and is installed on a machine tool to form a drive mechanism. A saddle (not shown) of the machine tool is fixed to the moving body 2, and the saddle supports an object to be subjected to movement control. In the illustrated example, one moving body 2 is arranged on the rail 4, but multiple moving bodies 2 may be arranged in series along the rail 4 and support the saddle. Here, the longitudinal direction of the rail 4 is defined as the X direction, the width direction as the Y direction, and the height direction as the Z direction.
[0014] A sensor unit 8 is provided at one end of the movable body 2 in the X direction. The sensor unit 8 includes a holder 9 fixed to the movable body 2, and a magnetic sensor 10 assembled to the holder 9. The movable body 2 and the holder 9 are provided to straddle the rail 4 in the width direction (Y direction). The magnetic sensor 10 is disposed on one side of the holder 9 in the width direction. A cable 12 for extracting a detection signal extends from the magnetic sensor 10.
[0015] The rail 4 has a shape in which both sides are cut out in a tapered shape (V-shaped cross section), and the tapered surfaces form upper and lower guide surfaces 14a, 14b (when there is no particular distinction between them, they are simply referred to as "guide surfaces 14"). On the other hand, although not shown, a plurality of rolling elements made of rollers or balls are disposed on the inner surface of the movable body 2. The movable body 2 moves in the longitudinal direction of the rail 4 while these rolling elements roll along the guide surfaces 14.
[0016] A bottom surface 16 (the surface that serves as the base end of the upper and lower tapered surfaces) is provided between the upper and lower guide surfaces 14a, 14b on one side of the rail 4, and a magnetic layer 5 is formed on the surface of the bottom surface 16. Furthermore, a cover 20 is attached to the rail 4 so as to cover the magnetic layer 5, thereby protecting the magnetic layer 5 and preventing contamination. The magnetic layer 5 and its surrounding structure will be described in detail later.
[0017] A plurality of screw holes 22 that penetrate the rail 4 vertically are provided at predetermined intervals in the longitudinal direction of the rail 4. The rail 4 is fixed to a predetermined position in the machine tool by inserting bolts into these screw holes.
[0018] 2 is a cross-sectional view taken along the line AA in FIG. 1. The magnetic sensor 10 has a sensor head 30 at a position facing the magnetic layer 5 with the cover 20 sandwiched therebetween. In other words, the sensor head 30 faces the cover 20 disposed on the magnetic layer 5. The sensor head 30 includes an MR element. The sensor head 30 may be configured by sealing the MR element mounted on a substrate with resin to prevent contamination by coolant or the like. The magnetic sensor 10 is disposed facing the magnetic layer 5 by being attached to a holder 9 with screws (not shown).
[0019] Fig. 3 is an exploded perspective view of the rail 4. Fig. 4 is an assembled perspective view of the rail 4. Fig. 5 is a BB cross-sectional view of the rail 4 shown in Fig. 4. The left side of Fig. 5 is a cross-sectional view, and the right side is an enlarged view of part F. For convenience of explanation, in each drawing, the structural elements shown in Fig. 1 are shown shortened in the longitudinal direction of the rail 4.
[0020] As shown in FIG. 3, the magnetic layer 5 is formed by applying a water-based paint containing magnetic powder onto the bottom surface 16 of the rail 4, which is the support, and then drying it. After drying, the magnetic layer 5 is subjected to a surface smoothing treatment (surface treatment process). Therefore, if a final thickness of 200 μm is required as the magnetic layer of the magnetic scale of the product, a magnetic layer of about 250 μm in dry thickness is required. Furthermore, by arranging a non-magnetic cover 20 on the surface-treated side of the magnetic layer 5, as shown in FIG. 4, the magnetic layer 5 is arranged inside the cover 20 on the side surface of the rail 4, preventing the adhesion of foreign matter from the outside.
[0021] An example of the surface smoothing treatment is smoothing (flattening) the surface of the magnetic layer 5 by scraping it. The surface of the magnetic layer may also be smoothed by calendaring. By smoothing the surface of the magnetic layer 5 in this way, the cover 20 can be placed on the magnetic layer 5 with the gap between the magnetic layer 5 and the cover 20 being within a desired constant range (for example, 10 μm to 100 μm). In other words, the smoothing treatment using a scale such as that according to this embodiment allows the cover 20 to be placed in a stable position relative to the surface of the magnetic layer 5.
[0022] In the magnetic layer 5, a magnetic pattern is formed by N poles and S poles. The water-based paint containing the magnetic powder contains water as a main solvent. The water-based paint contains a water-dispersible acrylic resin and a water-soluble polyvinyl alcohol resin as a water-based binder. The water-based paint may contain 20 to 30 parts by weight of the water-based binder per 100 parts by weight of the magnetic powder in terms of solid content weight. The water-based paint may contain a dispersant. The dispersant may be contained in an amount of 2 to 4 parts by weight per 100 parts by weight of the magnetic powder in terms of solid content weight. The water-based paint may contain water as a main solvent, and may also contain a trace amount of an organic solvent (e.g., methanol, methyl acetate, etc.).
[0023] The magnetic powder may contain an acicular ferromagnetic alloy material with a major axis to minor axis ratio of 3 to 8. More specifically, the magnetic powder of this embodiment is an acicular ferromagnetic powder (magnetic powder in the examples described later) that is an iron oxide-based particle containing Co-iron alloy with Al solid solution Y clad therein, with a major axis length of 0.08 to 0.30 μm and a major axis ratio of 3 to 8, and is made up of an iron 92% Co 8% alloy: iron oxide: aluminum oxide: yttrium oxide: water = 56: 34: 6: 3: 1. Although not shown in the figure, an absolute pattern is formed as a magnetic pattern in the center of the width direction (Z direction) of the magnetic layer 5, and incremental patterns are formed on both sides of the width direction.
[0024] The cover 20 is a rectangular plate-like member having a thickness of 20 to 250 μm and made of a non-magnetic metal (e.g., stainless steel). The cover 20 has a length substantially equal to that of the rail 4, and extends from one end of the rail 4 to the other end. The cover 20 is attached to one side (bottom surface 16) of the rail 4 so as to cover the magnetic layer 5 from the outside. The magnetic flux due to the magnetization pattern of the magnetic layer 5 passes through the cover 20. Therefore, even if the cover 20 is interposed between the sensor head 30 and the magnetic layer 5, it does not affect the detection of the magnetic flux.
[0025] The position of the magnetic sensor 10, and therefore the position of the moving object 2, can be detected by placing the sensor head 30 opposite the magnetic layer 5 and reading the magnetized magnetic pattern. The magnetic sensor 10 transmits the detected position information to an external device via a cable 12.
[0026] Next, the water-based paint used when forming the magnetic layer will be described. By using the water-based paint according to this embodiment in the manufacture of scale, it is possible to provide a magnetic scale with a high magnetic powder content and thick coating, and the magnetic properties of the formed magnetic layer are excellent. In this embodiment, when manufacturing the magnetic scale by applying the water-based magnetic paint to the rail 4, which is a non-magnetic support, a combination of a water-dispersible acrylic resin and a water-soluble polyvinyl alcohol resin is contained in the water-based magnetic paint as the water-based binder.
[0027] The scale according to the embodiment has a magnetic layer with a magnetic powder content of 75% or more and a dry film thickness of 200 μm or more. The aqueous coating composition according to the embodiment contains magnetic powder, an aqueous binder, a dispersant, and the like. The amount of the aqueous binder is preferably 20 to 30 parts by weight per 100 parts by weight of the magnetic powder in terms of solid content. The mixing ratio of the water-dispersible acrylic resin and the water-soluble polyvinyl alcohol resin is preferably 1:1.5 to 2.5 in terms of solid content. Furthermore, it is preferable to use a water-soluble copolymer containing a functional group with high pigment affinity as a dispersant for the aqueous magnetic coating. The amount of the dispersant is preferably 2 to 4 parts by weight per 100 parts by weight of the magnetic powder in terms of solid content.
[0028] The scale manufacturing method according to the embodiment is a method for manufacturing a scale having a magnetic pattern for detecting relative displacement by an opposing sensor head 30, and includes the steps of applying a water-based paint containing magnetic powder onto the rail 4 and drying it to form a magnetic layer 5 having a magnetic powder content of 75% or more and a film thickness of 200 μm or more, and forming (magnetizing) a magnetic pattern on the magnetic layer 5 that allows the sensor head 30 to detect relative displacement. The water-based paint contains water as a main solvent. Note that, other than forming a magnetic layer directly on the rail 4, a magnetic layer may be formed on a resin or glass of a non-magnetic plate-like component, and the plate-like component may be mounted at a predetermined position on the rail 4.
[0029] This makes it possible to manufacture a scale having a magnetic layer with a magnetic powder content of 75% or more and a film thickness of 200 μm or more formed on a support using an aqueous paint whose main solvent is water, which is inexpensive, safe, and has less impact on health and the environment than organic solvents. By using a scale manufactured by this method, a displacement detection device with excellent magnetic properties and high position detection accuracy can be realized. The thickness of the magnetic layer after smoothing treatment that functions as a scale is preferably in the range of 150 to 250 μm (approximately 200 to 300 μm in terms of dry film thickness).
[0030] FIG. 6 is a schematic diagram for explaining an interpolation processing technique that realizes high resolution of a magnetic sensor. The interpolation processing technique is a technique for accurately dividing a signal waveform detected from a magnetic scale to a required pitch (fineness). The magnetic pattern P is magnetized in a pattern with a pitch Px of about 400 μm in the scale direction (longitudinal direction parallel to the X-axis). The sensor is a magnetoresistive sensor, and two sensor heads 30 detect two sine waves S1 and S2 with a phase difference of 90 degrees from the magnetic scale.
[0031] The detected signal is divided electrically, but if the signal contains distortion, accurate position information (true value) cannot be obtained. Therefore, for example, DC components can be removed from the signal detected by the scale, and level and position adjustments can be performed in real time, achieving 80,000 divisions through advanced signal processing. This makes it possible to realize a scale that can obtain position information with a resolution of 5 nm, by dividing a 400 μm sine wave corresponding to the pitch Px by 80,000.
[0032] When the output of the sine wave suitable for this scale was measured, it was found that a layer thickness of around 200 μm was the layer thickness that could detect the sine wave most suitable for signal processing. When the magnetic layer was thinner than 150 μm, the function as a magnetic scale was satisfied, but the output gradually decreased. When the magnetic layer was thicker than 250 μm, it could be used as a scale by adjusting the thickness at which the magnetic pattern of the magnetic layer was magnetized, but the magnetized area would need to be adjusted. If the magnetic pattern was formed by magnetizing the entire layer, the repulsive action of magnetization at the magnetization reversal boundary would occur, resulting in demagnetization.
[0033] The thickness of the magnetic layer after smoothing treatment is preferably in the range of 150 to 250 μm, because the manufacturing process can be simplified by allowing the magnetic pattern to be formed by magnetizing the entire magnetic layer without adjusting the thickness of the magnetic layer to be magnetized.
[0034] A magnetic layer with a dry thickness of 200 μm was created using magnetic organic paint, and then smoothed to produce a magnetic scale with a thickness of 150 μm. In this case, it was confirmed that the magnetic powder content of the magnetic layer when dried before smoothing was 73% and 80%. It was also confirmed that a magnetic scale can be used if the magnetic powder content is between 70% and 90%. In particular, to generate a strong magnetic field, it is best for the magnetic powder content to be 75% or more.
[0035] In addition, by using an aqueous magnetic paint that combines an environmentally friendly water-dispersible acrylic resin and a water-soluble polyvinyl alcohol resin, a wet coating film containing magnetic powder and having a thickness of 200 μm or more can be applied to a support in one go. The reason for this is that when the aqueous paint of this embodiment is a combination of an acrylic resin and a polyvinyl alcohol resin, the reactive groups (e.g., carboxyl groups) of the acrylic resin and the reactive groups (e.g., hydroxyl groups) of the polyvinyl alcohol resin bond together (e.g., ester bonds). By bonding some of the reactive groups together, for example, the peel-resistant property of the acrylic resin and the crack-resistant property of the polyvinyl alcohol resin are combined, and it is thought that coating without coating defects can be achieved. Therefore, it is thought that the aqueous paint of this embodiment can be applied to a support in one go.
[0036] On the other hand, when a paint using only acrylic resin as a binder becomes thick, the paint film is prone to cracking as the film dries, and a single application can only produce a dry film of less than 100 μm. Also, when a paint using only polyvinyl alcohol resin as a binder becomes thick, the paint film is prone to peeling from the substrate after drying, resulting in a coating defect, and a single application can only produce a dry film of less than 100 μm.
[0037] Note that "one-time application" refers to the minimum unit of action required for application by a certain method. For example, when forming a film on a substrate by immersing the substrate in a reservoir of paint, immersing the substrate in the reservoir once is considered as one-time application, and immersing the substrate in the reservoir multiple times is considered as multiple applications.
[0038] As a result, for example, whereas using a paint that can only apply a film about 100 μm thick in one application requires multiple applications, the water-based paint according to this embodiment makes it possible to form a magnetic layer of the desired thickness with fewer applications. In other words, the scale manufacturing method according to this embodiment makes it possible to easily manufacture the desired scale in a short time, thereby reducing manufacturing costs.
[0039] A method that can be applied to the application of the water-based paint of this embodiment includes die coating. FIG. 9 is a schematic diagram for explaining die coating. FIG. 10 is an enlarged cross-sectional view of the main part of a slit die. Die coating can easily form a planarly uniform film by the relative movement of the substrate and the slit die during application. In this embodiment, a method in which the slit die 40 is fixed and the substrate (sheet) 42 moves will be described. Specifically, when applying the paint of this embodiment, a slit die 40 with an opening width D1 of 10 mm and a slit width D2 of 0.5 mm is used, and a coating amount of 0.75 mL / s, a coating speed of 50 mm / s, and a gap width D3 (a gap between the tip of the discharge part and the substrate) of 3 mm are used to apply the paint once, resulting in an undried coating film 44 with a thickness of 2200 μm. By drying this undried coating film 44, a dried coating film as a magnetic layer with a magnetic powder content of 70% or more and a thickness of 200 μm or more can be obtained without cracks or cracks. The thickness of the wet coating film may be 200 μm or more, and may be 500 μm or more, and more preferably 1000 μm or more. The substrate is made of a non-magnetic metal such as stainless steel or aluminum.
[0040] As shown in Fig. 9, in the die coating of this embodiment, paint 48 stored in a tank 46 is supplied to a slit die 40 by a syringe pump 50. A manifold 52 for retaining paint 48 is provided near the tip of the slit die 40 as shown in Fig. 10. The manifold 52 contributes to uniformity of the coating film. The substrate 42 moves in the direction of arrow A while being fixed to an adsorption platen.
[0041] Example 1 A container was charged with 100 parts by weight of magnetic powder (the above-mentioned acicular ferromagnetic powder), 17 parts by weight of acrylic resin (WCP-4, solid content 48% manufactured by Resitex Co., Ltd.), 167 parts by weight of a 10% aqueous solution of polyvinyl alcohol resin (JF-20, manufactured by Japan Vinyl Acetate & Poval Co., Ltd.), 8 parts by weight of dispersant (TEGO Dispers 750W, solid content 40% manufactured by Evonik Tego Chemie GmbH), 287 parts by weight of water, and 600 parts by weight of ceramic beads, and dispersed for 60 minutes with a bead mill to obtain an aqueous magnetic paint. The coating film obtained from this aqueous magnetic paint had a magnetic powder content of 78% and a dry film thickness of 250 μm. After that, the film thickness was made 200 μm by smoothing treatment, and the performance was evaluated as a magnetic scale, and sufficient performance was obtained. In addition, there was no cracking or peeling of the coating film.
[0042] Example 2 A container was charged with 100 parts by weight of magnetic powder (the aforementioned acicular ferromagnetic powder), 52 parts by weight of acrylic resin (WCP-4 manufactured by Resitex Co., Ltd., solid content 48%), 8 parts by weight of dispersant (TEGO Dispers 750W manufactured by Evonik Tego Chemie GmbH, solid content 40%), 418 parts by weight of water, and 600 parts by weight of ceramic beads, and dispersed for 60 minutes using a bead mill to obtain a water-based magnetic paint. The coating film obtained from this water-based magnetic paint functions as a scale. However, cracks have occurred in this coating film, and further improvements in coating conditions, etc. are required to form an optimal magnetic layer as a scale (for example, a dry film thickness of 250 μm) without cracking or peeling.
[0043] Example 3 A container was charged with 100 parts by weight of magnetic powder (the aforementioned acicular ferromagnetic powder), 250 parts by weight of a 10% aqueous solution of polyvinyl alcohol resin (JF-20 manufactured by Japan Vinyl Acetate & Poval Co., Ltd.), 8 parts by weight of a dispersant (TEGO Dispers 750W manufactured by Evonik Tego Chemie GmbH, solid content 40%), 221 parts by weight of water, and 600 parts by weight of ceramic beads, and the mixture was dispersed for 60 minutes using a bead mill to obtain a water-based magnetic paint. The coating film obtained from this water-based magnetic paint functions as a scale. However, peeling occurred in this coating film, and further improvement of coating conditions, etc. is required to form an optimal magnetic layer as a scale (for example, a dry film thickness of 250 μm) without cracking or peeling.
[0044] Example 4 A container was charged with 100 parts by weight of magnetic powder (the aforementioned acicular ferromagnetic powder), 17 parts by weight of acrylic resin (WCP-4, manufactured by Resitex Co., Ltd., solid content 48%), 167 parts by weight of a 10% aqueous solution of polyvinyl alcohol resin (JF-20, manufactured by Nippon Vinyl Acetate & Poval Co., Ltd.), 291 parts by weight of water, and 600 parts by weight of ceramic beads, and the mixture was dispersed for 60 minutes using a bead mill to obtain a water-based magnetic paint. The coating film obtained from this water-based magnetic paint functions as a scale. However, cracks were generated in this coating film, and further improvements in coating conditions, etc. are required to form an optimal magnetic layer as a scale (for example, a dry film thickness of 250 μm) without cracking or peeling.
[0045] Example 5 A container was charged with 100 parts by weight of magnetic powder (the aforementioned acicular ferromagnetic powder), 17 parts by weight of acrylic resin (WCP-4, manufactured by Resitex Co., Ltd., solid content 48%), 167 parts by weight of a 10% aqueous solution of polyvinyl alcohol resin (JF-20, manufactured by Japan Vinyl Acetate & Poval Co., Ltd.), 3 parts by weight of dispersant (DISPARLON AQ-330, manufactured by Kusumoto Chemical Co., Ltd., solid content 100%), 291 parts by weight of water, and 600 parts by weight of ceramic beads, and the mixture was dispersed for 60 minutes using a bead mill to obtain a water-based magnetic paint. The coating film obtained from this water-based magnetic paint functions as a scale. However, cracks were generated in this coating film, and further improvement of coating conditions, etc. is required to form an optimal magnetic layer as a scale (for example, a dry film thickness of 250 μm) without cracking or peeling.
[0046] Example 6 A container was charged with 100 parts by weight of magnetic powder (the aforementioned acicular ferromagnetic powder), 17 parts by weight of acrylic resin (WCP-4, manufactured by Resitex Co., Ltd., solid content 48%), 167 parts by weight of a 10% aqueous solution of polyvinyl alcohol resin (JF-20, manufactured by Nippon Vinyl Acetate & Poval Co., Ltd.), 3 parts by weight of dispersant (citric acid), 291 parts by weight of water, and 600 parts by weight of ceramic beads, and the mixture was dispersed for 60 minutes using a bead mill to obtain a water-based magnetic paint. The coating film obtained from this water-based magnetic paint functions as a scale. However, cracks were generated in this coating film, and further improvement of coating conditions, etc. is required to form an optimal magnetic layer as a scale (for example, a dry film thickness of 250 μm) without cracking or peeling.
[0047] Example 7 A container was charged with 100 parts by weight of magnetic powder (the aforementioned acicular ferromagnetic powder), 17 parts by weight of acrylic resin (WCP-4, manufactured by Resitex Co., Ltd., solid content 48%), 167 parts by weight of a 10% aqueous solution of polyvinyl alcohol resin (CKS-50, manufactured by Mitsubishi Chemical Corporation), 8 parts by weight of dispersant (TEGO Dispers 750W, manufactured by Evonik Tego Chemie GmbH, solid content 40%), 287 parts by weight of water, and 600 parts by weight of ceramic beads, and the mixture was dispersed for 60 minutes using a bead mill to obtain an aqueous magnetic paint. The coating film obtained from this aqueous magnetic paint functions as a scale. However, cracks were generated in this coating film, and further improvement of coating conditions, etc. is required to form an optimal magnetic layer as a scale (for example, a dry film thickness of 250 μm) without cracking or peeling.
[0048] The above results are shown in Table 1. [Table 1]
[0049] Comparing Example 1 and Example 7, the products used as polyvinyl alcohol resins are different. JF-20 used in Example 1 has a degree of polymerization of 2000, a degree of saponification of 98.0 to 99.0 (mol%), and a 4% aqueous solution viscosity of 35 to 45 (mPa·s). On the other hand, although the degree of polymerization of CKS-50 is unknown, the degree of saponification is 99.0 (mol%) or more, and the viscosity of a 4% aqueous solution is 2.5 to 3.0 (mPa·s). The viscosity tends to increase as the degree of polymerization and the degree of saponification increase. Therefore, since the degrees of saponification of both are about the same, it can be inferred that the degree of polymerization of CKS-50 is much lower than that of JF-20. This inference is consistent with the description in International Publication No. 2017 / 056596 that the degree of polymerization of CKS-50 is 300. Therefore, it is considered that the degree of polymerization has a significant effect on film formability, and a high degree of polymerization is necessary for the formation of a thick film without cracking or peeling.
[0050] [Cover fixing structure] Fig. 7 is a cross-sectional view showing a modified structure of the bottom surface of the rail shown in Fig. 4. Fig. 8 is a cross-sectional view showing the state in which a magnetic layer and a cover are arranged on the bottom surface of the rail shown in Fig. 7. The rail 4 shown in Fig. 7 has an uneven bottom 32 formed at the bottom of a V-shaped groove. The bottom 32 has a protrusion 32a that supports the center of the lower surface 5a of the magnetic layer 5. The upper surface 32b of the protrusion 32a is a rectangular flat surface that fits along the groove of the rail 4, and supports the magnetic layer 5 in a fixed position.
[0051] In the bottom 32, the width W1 of the region R1 on which the magnetic layer 5 is placed is wider than the width W2 of the region R2 that becomes the space 32c when the magnetic layer 5 is placed. Therefore, a step 32d is formed at the boundary between the region R1 and the region R2, and the magnetic layer 5 placed on the upper surface 32b is less likely to tilt. The bottom 32 has flat step portions 32e formed on the left and right sides of the groove at a predetermined position above the region R1. The rectangular cover 20 is fixed to the bottom 32 at a constant distance from the smoothed surface of the magnetic layer 5 by being placed on the predetermined step portion 32e. In other words, the surface of the magnetic layer 5 is smoothed in consideration of the height between the upper surface 32b and the step portion 32e, so that the distance between the sensor head and the magnetic layer 5 can be set to a desired value.
[0052] Furthermore, by forming the top surface 32b and the step portion 32e by processing the bottom portion 32 of the rail 4, which is a single component, it is possible to suppress dimensional errors in the positional relationship between the top surface 32b and the step portion 32e due to processing accuracy. As a result, in the magnetic sensor 10 according to the modified example, the distance between the surface of the magnetic layer 5 and the surface of the cover 20 is constant, and a stable output (accuracy) as a scale is ensured, thereby improving the detection accuracy of the scale.
[0053] As described above, by applying the water-based paint of this embodiment once, a wet coating film can be formed on the support, which can appropriately form the magnetic pattern used for the scale on the film, has few cracks, high continuity, and a film thickness of 200 μm or more at any point. Furthermore, even if the water-based paint of this embodiment is applied once and then dried, a dry film is formed on the support, which still has a thickness of 200 μm or more, has few cracks, high continuity, and has high adhesion to the support to the extent that it does not cause the film to move in position. Therefore, a dry film suitable as a magnetic layer for scale can be produced.
[0054] The present invention is not limited to the above-mentioned embodiments and examples, and the components can be modified and embodied without departing from the spirit and scope of the invention. Various inventions can be formed by appropriately combining multiple components disclosed in the above-mentioned embodiments and examples. In addition, some components can be deleted from all the components shown in the above-mentioned embodiments and examples. [Explanation of symbols]
[0055] 1 displacement detection device, 2 movable body, 4 rail, 5 magnetic layer, 8 sensor unit, 9 holder, 10 magnetic sensor, 12 cable, 14 guide surface, 16 bottom surface, 20 cover, 22 screw hole, 30 sensor head, 32 bottom portion, 32a convex portion, 32b upper surface, 32c space, 32d step portion, 32e step portion.
Claims
1. A method for manufacturing a scale having a magnetic pattern for detecting relative displacement by opposing sensor heads, comprising the steps of: A step of applying an aqueous coating material containing a magnetic powder once onto a support to form a wet coating film having a thickness of 200 μm or more; a step of drying the wet coating film to form a magnetic layer having a magnetic powder content of 70% or more and a film thickness of 200 μm or more; forming a magnetic pattern on the magnetic layer that allows the sensor head to detect a relative displacement; The method for producing scale, wherein the water-based paint contains water as a main solvent.
2. The method for manufacturing scale according to claim 1, wherein the water-based paint contains 20 to 30 parts by weight of water-based binder per 100 parts by weight of the magnetic powder, in terms of solid content weight.
3. The method for producing scale according to claim 2 , wherein the water-based paint contains a water-dispersible acrylic resin and a water-soluble polyvinyl alcohol resin as the water-based binder.
4. The method for producing scale according to claim 3 , wherein the water-based paint contains a dispersant.
5. The method for producing scale according to claim 4, wherein the dispersant is contained in an amount of 2 to 4 parts by weight based on 100 parts by weight of the magnetic powder in terms of solid content.
6. a step of smoothing the surface of the magnetic layer by scraping; 2. The method of claim 1, further comprising the step of: disposing a rectangular shaped solid cover in spaced relation on the smoothed surface of the magnetic layer.
7. the sensor head faces the solid cover, The method for manufacturing a scale according to claim 6, wherein the solid cover has a thickness of 20 to 250 μm and is made of a non-magnetic metal.
8. The method for producing a scale according to any one of claims 1 to 7, wherein the magnetic powder contains an acicular ferromagnetic alloy material having a ratio of major axis to minor axis of 3 to 8.
9. The method further includes a step of placing the magnetic layer on a bottom of a V-shaped groove formed in a rail, 8. The method for manufacturing a scale according to claim 6, wherein the rail has flat steps formed on the left and right sides of the groove above the bottom.
Citation Information
Patent Citations
Magnetic recording medium and method of manufacturing the same
JP2010049731A