Protection facility for converter slag and converter refining method
The integration of a heat-resistant plate and insulating material with specified dimensions addresses thermal stress issues in converter refining, ensuring the smoke-proof shutter's functionality and reducing maintenance needs.
Patent Information
- Application Number
- JP2023071576
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-25
- Publication Date
- 2024-11-07
- Estimated Expiration
- 2043-04-25
AI Technical Summary
Conventional converter refining equipment experiences thermal stress and deformation due to radiant heat and slag collision, leading to cracks and inability to open and close the smoke-proof shutter effectively.
Installation of a heat-resistant plate with a heat insulating material and a shutter body, characterized by specific dimensions and thermal properties, to prevent slag flow and protect the smoke-proof shutter from thermal deformation.
Prevents thermal deformation of the smoke-proof shutter frame, reducing maintenance disruptions and ensuring smooth operation by controlling cracks and deformation, thus maintaining production efficiency.
Smart Images

Figure 2024157295000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a protective equipment used during converter slag drainage in a converter refining process for steelmaking, and to a converter refining method for preventing slag from flowing out onto a work floor in front of the converter during converter slag drainage. [Background technology]
[0002] In conventional converter facilities, a pair of movable walls that can be opened and closed is provided to suppress the diffusion of dust generated during refining and to prevent radiant heat and slag from flowing out to the work floor in front of the furnace when the converter is slag-discharging. These movable walls are called smoke shutters. The smoke shutters are opened when iron sources such as molten pig iron and scrap are charged (hereinafter simply referred to as charging), and are closed during blowing, tapping, and slag-discharging.
[0003] Meanwhile, in converter refining operations, so-called intermediate slag removal has been conventionally performed during blowing, in which slag is removed while leaving molten iron in the converter. In this case, the converter is often tilted vigorously toward the front of the furnace to remove the slag. For this reason, for example, in Patent Document 1, a method is adopted in which the joint part of the smoke shutter is shifted horizontally from the center position of the throat to prevent slag from adhering to the joint part.
[0004] In addition, the smoke shutter is subjected to a large thermal load due to the radiant heat from the furnace throat and the collision of the discharged slag. Therefore, for example, in Patent Documents 2 and 3, the heat-receiving surface of the smoke shutter is made of a heat-resistant plate, and a protective wall is provided in front of the smoke shutter at the slag collision part, which is subject to a particularly large thermal load, to protect the smoke shutter. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2017-57496 A [Patent Document 2] JP 2017-66500 A [Patent Document 3] Patent Publication No. 2021-102795 Summary of the Invention [Problem to be solved by the invention]
[0006] However, the above-mentioned conventional technology has the following problems. That is, the radiant heat from the furnace opening and the heat caused by the collision of the slag are transferred from the heat-resistant plate of the heat-receiving surface to the frame part constituting the smoke shutter. As a result, the frame part is deformed or cracked due to thermal stress, which makes it impossible to open and close the smoke shutter.
[0007] The present invention has an object to solve the above-mentioned conventional problems and to provide a converter slag protection system and a converter refining method in which a smoke shutter can be opened and closed without deformation. [Means for solving the problem]
[0008] The converter slag removal protective equipment of the present invention, which advantageously solves the above-mentioned problems, is protective equipment for preventing slag from flowing out onto the work floor in front of the furnace when slag is removed while molten iron remains in the converter, and is characterized in that a heat-resistant plate, insulation material, and shutter body are installed in that order from the converter side.
[0009] The converter slag protection equipment according to the present invention is as follows: (a) The heat transfer coefficient K of the heat insulating material is 8W / (m 2 ·℃) or less. (b) further comprising a seal plate disposed between the heat-resistant plate and the heat insulating material; (c) the heat-resistant plate is fastened to the shutter body with a screw, and a pipe seat through which the screw passes is embedded in the insulating material; (d) the heat-resistant plate is a rectangular parallelepiped with a side length in the range of 0.3 to 0.9 m and a thickness t in the range of 20 to 30 mm, and the gap between the heat-resistant plates is 6 / 1000 times or more of the side length and 1 / 2 times or less of the thickness t; This may be a preferred solution.
[0010] The converter refining method of the present invention, which advantageously solves the above-mentioned problems, is a converter refining method that uses any of the above-mentioned converter slag removal protective equipment to prevent slag from flowing out onto the front-of-furnace work floor when removing slag while leaving molten iron in the converter, and is characterized by including the steps of attaching a heat-resistant plate with insulating material sandwiched between the shutter body installed in front of the furnace to the converter side, and removing the heat-resistant plate damaged by heat. Effect of the Invention
[0011] According to the converter slag protection equipment and converter refining method of the present invention, the temperature of the smoke shutter frame can be prevented from exceeding a certain value, and it is possible to prevent the smoke shutter from becoming unable to move due to thermal deformation of the frame. In addition, it is possible to manage deformation and cracks of the heat-resistant plate and replace it during regular maintenance, which is extremely useful in industry, as it reduces the impact on production due to problems. [Brief description of the drawings]
[0012] [Figure 1] FIG. 1 is a schematic diagram showing a converter slag protection system according to an embodiment of the present invention. [Diagram 2] 4 is a schematic cross-sectional view showing an example of a method for connecting a heat-resistant plate and a frame according to the embodiment. FIG. [Diagram 3] FIG. 2 is a partial front view illustrating the condition of the heat-resistant plate after the converter slag removal work, where (a) shows the heat-resistant plate of a conventional panel, and (b) shows the heat-resistant plate of a segmented panel. [Figure 4] 4 is a graph showing the relationship between the thickness and thermal conductivity of the insulating material used in the above embodiment. [Diagram 5] 1 is a graph showing an example of a temperature transition of a heat-resistant plate during converter refining. [Figure 6] 1 is a schematic diagram showing temperature distribution by finite element method (FEM) analysis based on actual measurement results, where (a) shows the heat-resistant plate and (b) shows the frame. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] Hereinafter, the embodiments of the present invention will be described in detail. Note that the drawings are schematic and may differ from the actual ones. Furthermore, the following embodiments are merely examples of devices and methods for embodying the technical idea of the present invention, and are not intended to limit the configuration to the following. In other words, the technical idea of the present invention can be modified in various ways within the technical scope described in the claims.
[0014] Fig. 1 is a schematic diagram showing a converter slag removal protection system according to one embodiment of the present invention. The converter system has a converter installation section where a converter 1 is present, and a furnace front section adjacent to the converter installation section where molten iron and the like are charged. A furnace front side work floor 4 is provided in front of the furnace. Fig. 1 shows a state during slag removal, in which slag S on the molten iron L is discharged to the furnace front side. In this embodiment, the converter 1 is tilted to the furnace front side while leaving the molten iron L in the converter 1, and the slag S is discharged, that is, intermediate slag removal is performed.
[0015] A pair of smoke shutters 2 are provided in front of the converter to isolate the front-side work floor 4 from the converter 1 during operation. The smoke shutters 2 are opened and closed by moving on a traveling rail using a traveling device consisting of wheels and an electric motor. In this embodiment, a heat-resistant plate 3 is attached to the frame 2A (shutter body) of the smoke shutter 2.
[0016] The heat-resistant plate 3 according to this embodiment is connected and fixed to the frame 2A via a heat insulating material 5 as shown in FIG. 2. The heat-resistant plate 3 blocks, for example, radiant heat from the throat of the converter 1 toward the front-side working floor 4 and outflowing slag during intermediate slag removal. The heat-resistant plate 3 is preferably made of ductile cast iron or heat-resistant cast steel. If the thickness of the heat-resistant plate 3 is less than 20 mm, it is difficult to cast the plate and the risk of material defects increases, so the thickness is set to 20 mm or more. If the thickness of the heat-resistant plate 3 exceeds 30 mm, the temperature difference between the front and back sides increases, and the risk of cracks occurring due to thermal stress increases, so the thickness is set to 30 mm or less. If the heat-resistant plate 3 is made of ductile cast iron, for example, its thermal expansion coefficient is 10.0×10 -6 / K. If the temperature rise of the heat-resistant plate due to the heat load from the converter is about 600°C, it is preferable to provide a gap of 6 mm or more between adjacent heat-resistant plates 3 for every 1000 mm of side length of the heat-resistant plate 3, taking into consideration thermal expansion. If the gap is too wide, there is a risk of molten slag or sparks leaking out from the gap, so it is preferable to make the gap 1 / 2 times the thickness of the heat-resistant plate or less (10 mm or less if the heat-resistant plate thickness is 20 mm).
[0017] In order to suppress the thermal stress that causes cracks and deformations in the heat-resistant plate 3, it is effective to reduce the temperature difference within the heat-resistant plate 3. In the smoke shutter 2, the main thermal loads are radiant heat and slag collision. In the case of radiant heat, the temperature of the heat-resistant plate 3 rises uniformly, so temperature differences are unlikely to occur. On the other hand, in the case of slag collision, a large temperature difference occurs between the parts with and without slag. This increases the thermal stress generated in the heat-resistant plate 3. Therefore, by dividing the heat-resistant plate into smaller parts in the area that is subjected to slag collision, it is possible to suppress the damage range and the amount of deformation per sheet.
[0018] An example of dividing a panel of a heat-resistant plate 3 is shown in FIG. 3. FIG. 3(a) shows a conventional panel, which is a square panel 3A with side lengths of 0.9 m x 0.9 m. In the example of FIG. 3(a), four panels are partially covered by the impact range D of the slag, that is, four damaged panels 3C are 0.9 m x 0.9 m x 4. FIG. 3(b) shows a divided panel 3B with a size of 0.3 m x 0.9 m. Although the impact range D of the slag is the same as in FIG. 3(a), the damaged panel 3C is 0.3 m x 0.9 m x 6 panels. Therefore, the area of the damaged panel 3C is halved by dividing the heat-resistant plate.
[0019] Therefore, the heat-resistant plate 3 is preferably a rectangular parallelepiped with a side length in the range of 0.3 to 0.9 m and a thickness in the range of 20 to 30 mm. If the side length is below the lower limit, the number of heat-resistant plates 3 to be installed will be too large, which may lead to an increase in the number of work steps.
[0020] The thickness and physical properties of the heat insulating material 5 used in this embodiment must be selected according to the expected thermal load. The mechanical strength of SS400, the material of the frame 2A, drops rapidly when it exceeds 300 to 400°C. For this reason, it is preferable to design the frame so that the temperature is 200°C or less. Figure 4 shows the relationship between the thermal conductivity λ and thickness t of the heat insulating material 5. The inventors' investigations have determined that, based on the results of actual temperature measurements during operation, in order to keep the temperature of the frame 2A below 200°C, the overall heat transfer coefficient K (= λ / t) of the heat insulating material 5 needs to be 8 W / (m 2 It was found that the temperature should be kept below 30°C.
[0021] Insulation material 5 is classified into fixed and irregular insulation materials. When fixed insulation material is used, the heat-resistant plate and the insulation material are not bonded, making replacement easy. A special mold is required to manufacture fixed insulation material, which is costly. In the case of irregular insulation material, construction methods such as pouring and spraying are common. If irregular insulation material is directly installed between the heat-resistant plate 3 and the frame 2A, it will adhere to the heat-resistant plate 3. For this reason, by providing a seal plate 6 between the heat-resistant plate 3 and the insulation material 5 and installing irregular insulation material on the seal plate 6, it becomes possible to replace the heat-resistant plate 3 alone.
[0022] Furthermore, most of the insulation 5 is made of brittle material and may break under the tightening force of the bolt 7. Therefore, the application of tightening force to the insulation can be prevented by fastening the bolt 7 through a pipe seat 9 having a length equal to or greater than the thickness of the insulation. With this method, the insulation will rattle due to vibrations caused when the smoke shutter 2 is in motion, so it is preferable to adhere the insulation to the frame with an adhesive or the like. EXAMPLES
[0023] In order to clarify the heat load on the smoke shutter 2 in a factory with a converter facility as shown in Fig. 1, a heat-resistant plate for temperature measurement was installed on the existing smoke shutter 2 and temperature measurements were performed. The converter operation method during the measurements was the double slag method (WS), which is the method with the highest heat load. In other words, the converter is charged with molten iron, de-Si and de-P blowing is performed as the first blow, de-P slag is discharged as intermediate slag discharge Rm, de-C blowing is performed as the second blow, and then steel is tapped and final slag discharge Rf is performed. The smoke shutter 2 is subjected to heat loads due to radiation from the throat (throat temperature 1600°C) and collision with slag during the intermediate slag discharge Rm (7-10 min) and final slag discharge Rf (3-5 min) processes. The measurement was performed on the panel of the heat-resistant plate 3, which is the part that is hit by the slag and has the highest heat load, in front of the throat where the radiant heat is the largest. Figure 5 shows an example of the temperature measurement results for one cycle. From this result, it can be seen that temperature peaks appear at the time of intermediate slag discharge Rm and final slag discharge Rf. It was found that as the operation continues, heat gradually accumulates in the smoke shutter 2, and when the amount of heat received and released balances, the temperature of the heat-resistant plate 3 reaches a maximum of approximately 600°C. Based on these measurement results, a finite element method (FEM) analysis was performed to select the insulation material 5. Figure 6 shows the analysis results for insulation material 5 with a thermal conductivity λ = 0.2 W / (m°C) and a thickness of 30 mm. The overall overall heat transfer coefficient of this insulation material 5 is 6.67 W / (m 2 The maximum temperature of the heat-resistant plate 5 was 600°C, whereas the maximum temperature of the frame 2A was 150°C, which was a good result.
[0024] The heat-resistant plate 3 must cover an area that is subject to the collision of molten slag and the radiant heat from the furnace opening, so it is preferable that the heat-resistant plate 3 be about twice the diameter of the furnace opening. In this embodiment, the heat-resistant plate area is 9.5m x 10.0m for a furnace opening diameter of 4.6m.
[0025] In addition, if the heat-resistant plate 3 is divided too finely, for example, in the case of a panel of 0.1 m x 0.1 m, the number of bolts required is 4 bolts per panel x 1296 panels, totaling 5184 bolts, which is a significant increase compared to the case of using a heat-resistant plate of 0.9 m x 0.3 m in this embodiment. Increasing the number of bolts not only increases the labor required to install the heat-resistant plate 3, but also increases the bolt area relative to the heat-receiving surface, leading to a deterioration in heat resistance performance.
[0026] Without the insulation material 5, the temperature of frame 2A would reach approximately 550°C, and the rise in temperature would cause the tensile strength of the SS400 material of frame 2A to drop from 400MPa to approximately 150MPa. SS400, the material of frame 2A, has low creep resistance, so it is generally not recommended for use as a structure in environments of 350°C or higher. If heat-resistant steel were used in consideration of creep resistance, the cost would be significantly higher than that of SS400. [Explanation of symbols]
[0027] 1 Converter 2 Smokeproof shutter 2A (Smokeproof shutter) frame 3 Heat-resistant plate 3A (conventional) panel 3B (Subdivided) Panel 3C (Damaged) Panel 4 (Furnace front side) Working floor 5. Insulation 6 Seal plate 7 Flat head bolt 8 Nuts 9 Tube seat L Molten steel S slug D (Slug) Collision Range Rm Intermediate slag Rf final slag
Claims
1. This is a protective equipment to prevent slag from flowing out onto the work floor in front of the converter when removing slag while leaving molten iron in the converter. The converter slag discharge protection equipment is installed in the following order from the converter side: heat-resistant plate, insulation material, and the shutter body.
2. The heat transfer coefficient K of the heat insulating material is 8W / (m 2 2. The converter slag protection system according to claim 1, wherein the temperature is 0.1 ° C. or lower.
3. The converter slag protection system according to claim 1 , further comprising a seal plate disposed between the heat-resistant plate and the heat insulating material.
4. The converter slag protection equipment according to claim 1, wherein the heat-resistant plate is fastened to the shutter body with a screw, and a pipe seat through which the screw passes is embedded in the insulating material.
5. The converter slag protection equipment according to claim 1, wherein the heat-resistant plate is a rectangular parallelepiped having a side length in the range of 0.3 to 0.9 m and a thickness t in the range of 20 to 30 mm, and the gap between the heat-resistant plates is 6 / 1000 times or more of the side length and 1 / 2 times or less of the thickness t.
6. A converter refining method for preventing slag from flowing out to a furnace front side working floor by using a converter slag removal protective equipment according to any one of claims 1 to 5 when removing slag while leaving molten iron in the converter, comprising: A process of attaching a heat-resistant plate to the converter side of the shutter body installed in front of the furnace, sandwiching insulation material between them; and removing the heat-damaged refractory plate.
Citation Information
Patent Citations
Hermetically sealed dusttcollecting and heattprotecting device of moving type in front of converter
JP1979014306A
Steelmaking method in converter
JP1993140627A
Container for transporting molten slag
JP2004131817A
High heat-resistant flexible tube, bearing under high temperature atmosphere and ladle used for this tube
JP2005081354A
Protection member for converter residue, converter facility and converter refining method
JP2017066500A