Structural wall, house and sauna room

The use of lightweight panels with fitting portions and bonding material, along with inner and outer coating layers, addresses installation difficulties and improves durability in structural walls.

JP2024158161AActive Publication Date: 2024-11-08松岡洋良

Patent Information

Application Number
JP2023073123
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-27
Publication Date
2024-11-08
Estimated Expiration
2043-04-27

AI Technical Summary

Technical Problem

Conventional structural walls are difficult to install due to the use of heavy materials such as metal and wood for fastening parts, leading to installation challenges.

Method used

A structural wall composed of lightweight panels with fitting portions and a bonding material, along with inner and outer coating layers, allowing easy assembly and enhanced durability.

Benefits of technology

The solution enables easy installation and improved durability of the structural wall, with the coating layers accommodating thermal expansion and vibrations, enhancing the overall structure's longevity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024158161000001_ABST
    Figure 2024158161000001_ABST
Patent Text Reader

Abstract

To provide a structural wall that can be easily installed.SOLUTION: A structural wall 1 has a body of a plurality of lightweight panels 10 arranged as partitions separating the inside of a house from the outside. The lightweight panel 10 is joined to another lightweight panel 10 arranged adjacently on the partition. The lightweight panels 10 are provided with fitting parts 12 along butt surfaces 11 at each of the butt surfaces 11 to be joined. A joining material 20 for joining the two lightweight panels 10 is filled into a joint 16 where the fitting parts 12 are fitted. An inner coating layer 21 is formed on an inner side of the lightweight panel, and durability is imparted to the lightweight panel 10 as the structural wall 1. The joining material 20 is filled into the joint 16 where the lightweight panels 10 are in contact, and the inner coating layer 21 is provided on the inner side of the lightweight panel 10, thereby forming the structural wall 1. For this reason, the structural wall 1 according to the embodiment can be easily installed.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The technical field of this specification relates to a structural wall that can be easily installed, a house formed from this structural wall, and a sauna room as a house. [Background technology]

[0002] As examples of houses that have used structural walls in the past, Patent Document 1 describes a house formed by connecting multiple foam panels via fastening parts. Patent Document 2 describes a sauna room formed by connecting side panels that are made up of an interior panel, a side panel, and a foamed resin layer between them. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2018-123493 A [Patent Document 2] Utility Model Registration No. 3233199 Summary of the Invention [Problem to be solved by the invention]

[0004] Conventional structural walls have the problem that they are difficult to install because they are constructed of heavy materials, with metal members and wood used for the fastening parts, interior panels, and side panels.

[0005] The problem to be solved by the technology of this specification has been made in consideration of the above-mentioned points, and an object of the technology is to provide a structural wall that can be easily installed. [Means for solving the problem]

[0006] The structural wall according to the embodiment of the present specification is a structural wall arranged as a partition separating the inside of a house from the outside, The structure is made up of multiple lightweight panels. The lightweight panel is joined to an adjacent lightweight panel in the partition of the house; Each of the butt surfaces of the two lightweight panels is provided with a fitting portion along the butt surface, The joint where the butt surfaces of the two lightweight panels are butted together and the fitting portions are fitted together is joined by a joining material that joins the two lightweight panels, The method is characterized in that an inner coating layer is formed on the side of the lightweight panel that faces the interior of the house.

[0007] According to the structural wall of the embodiment of the present specification, a plurality of lightweight panels arranged as partitions separating the inside of a house from the outside are used as a framework, and a joint where abutting surfaces of a lightweight panel and an adjacent lightweight panel are butted together and a fitting portion is fitted is joined with a joining material to form a structural wall of the house. Also, in the structural wall, an inner coating layer is formed on the side of the lightweight panel that faces the inside of the house, giving durability to the lightweight panel as a structural wall. In the structural wall, joints where the lightweight panels come into contact are joined with a joining material, and an inner coating layer is formed on the inner side of the lightweight panel. Therefore, the structural wall of the embodiment can be easily installed.

[0008] Here, the structural wall may be configured such that an outer coating layer is formed on the side of the lightweight panel that faces the exterior of the house.

[0009] According to this, since an outer coating layer is formed on the side of the lightweight panel that faces the exterior of the house, durability can be imparted from the outside to the lightweight panel as a structural wall.

[0010] In the structural wall, the inner coating layer and the outer coating layer may each have an elongation percentage (ASTM D-412) of 100% or more.

[0011] This allows the inner covering layer and the outer covering layer to follow deformations caused by thermal expansion of the lightweight panel as a structural wall and by vibrations caused by external factors, thereby further increasing the durability of the structural wall.

[0012] Here, in the house according to the embodiment, the partition may be the structural wall described above.

[0013] This allows the house of the embodiment to have increased durability.

[0014] In addition, the sauna room according to the embodiment is a sauna room in the above-mentioned house, The interior may be provided with a heater for heating the interior, and an interior protection layer may be provided on the surface of the inner coating layer.

[0015] According to this, the sauna room of the embodiment can improve the heat resistance of the inner coating layer by the interior protective layer.

[0016] In addition, in the sauna room, an exterior protective layer may be provided on the surface of the outer coating layer.

[0017] According to this, the exterior protective layer can improve the heat retention of the sauna room. Effect of the Invention

[0018] The structural walls described herein can be easily installed. [Brief description of the drawings]

[0019] [Figure 1] This is a side view of a sauna room as a house equipped with the structural wall of the first embodiment. [Diagram 2] This is a front view of the sauna room. [Diagram 3] FIG. 2 is a cross-sectional view taken along line III-III in FIG. [Figure 4] An enlarged view (A) of the joint between the floor panel and the side panel, and an enlarged view (B) of the joint between the upper side panel and the top panel. [Diagram 5] 13A and 13B are a front view and a side view of a box-type store as a house equipped with a structural wall according to a second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0020] Hereinafter, a structural wall 1 and a house including the structural wall 1 according to an embodiment of the present specification will be described. The structural wall 1 of the embodiment is used as a wall as a structure arranged as a partition that separates the inside of the house from the outside. The house of the embodiment is installed outdoors, indoors, on the loading platform of a vehicle, on the deck of a ship, etc., and can be used as a sauna room 100 for steam and hot air bathing, a box-type store 100A selling food, beverages, and goods, a shelter for evacuation during an earthquake disaster, a temporary residence after an earthquake disaster, etc. Note that the house in the embodiment refers to a room, a shed, or a house consisting of one room. In the embodiment, the sauna room 100 for steam and hot air bathing will be described as an example of the first embodiment, and the box-type store 100A selling food, beverages, and goods will be described as an example of the second embodiment.

[0021] (First embodiment) As shown in Figs. 1 to 3, the sauna room 100 as a house equipped with the structural wall 1 of the first embodiment has a cylindrical body, the axial direction of the cylindrical shape is arranged horizontally, and the side is formed by a peripheral wall 110 consisting of a continuous structural wall 1 that goes around the circumference of the cylindrical shape, and the front and rear faces are closed by a front wall 120 and a rear wall 130 consisting of the structural wall 1. The front wall 120 is provided with a hinged door 101 that serves as an entrance and exit for people, and the peripheral wall 110 is provided with a light window 102 that lets in sunlight. Here, as shown in Figs. 1 and 2, when the sauna room 100 is installed, the axial direction of the cylindrical shape is the front-to-rear direction, the side (front wall 120) on which the hinged door 101 is provided is the front, and up, down, left, and right are the up, down, left, and right when the sauna room 100 is viewed from the front, and as used in the drawings, F indicates the front, B indicates the back, U indicates the top, D indicates the bottom, L indicates the left, and R indicates the right. In addition, the sauna room 100 may be referred to as the inside (side) or outside (side) based on the structural wall 1, and the circumferential direction (such as a clockwise direction) of the cylindrical sauna room 100 is the direction when the sauna room 100 is viewed from the front.

[0022] As shown in Figure 1, the structural wall 1, which is arranged as a partition separating the interior of the sauna room 100 from the outside, is composed of a cylindrical peripheral wall 110 with its axial direction being in the front-to-back direction, and a front wall 120 and a rear wall 130 which respectively cover the front and rear surfaces surrounded by the peripheral wall 110.

[0023] As shown in Figures 2 and 3, the peripheral wall 110 is cylindrically formed as a structural wall 1 arranged along the outer periphery in the up-down, left-right directions, with approximately rectangular lightweight panels 10 with an arc-shaped cross section arranged with their long sides in the front-to-back direction and their short sides in the circumferential direction, and which are arranged as a partition separating the inside of the sauna room 100 from the outside.

[0024] The lightweight panels 10 that constitute the peripheral wall 110 as the structural wall 1 use a floor panel 111 that is placed below the peripheral wall 110, a side panel 112 that is placed on the side, a top panel 113 that is placed above, and upper side panels 114 that are placed on each side of the top panel 113, due to differences in the placement position and the shape of the fitting portion 12 provided at the butt surface 11.

[0025] The floor panel 111 is disposed below the peripheral wall 110, and abutting surfaces 11 at both left and right ends are each formed with a cutout recess 13 cut out in a rectangular cross section as a fitting portion 12 along the front-rear direction.

[0026] The side panels 112 are arranged on the left and right side surfaces of the peripheral wall 110, and a protruding convex portion 14 with the center of the cross section protruding is formed as a fitting portion 12 on the abutting surface 11 of the lower end, and the protruding convex portion 14 fits into a notched recess 13 of the panel (floor panel 111 or side panel 112) arranged below. The abutting surface 11 of the upper end is formed as a fitting portion 12 with a notched recess 13 cut out in a rectangular cross section.

[0027] The top panel 113 is disposed above the peripheral wall 110, and abutting surfaces 11 at both left and right ends are formed with mating portions 12 along the front-to-rear direction, each of which has a notch 15 cut out on the inner side of the peripheral wall 110.

[0028] The upper side panels 114 are disposed on the left and right sides of the top panel 113, and a protruding convex portion 14 is formed as a fitting portion 12 on the abutting surface 11 at the lower end, and the protruding convex portion 14 fits into the notched recess 13 of the side panel 112. The abutting surface 11 at the upper end is formed as a fitting portion 12 with a notched portion 15 formed by cutting out the outer side of the peripheral wall 110, and the notched portion 15 fits into the notched portion 15 of the top panel 113.

[0029] As shown in Figures 2 and 3, the floor panel 111 is positioned at the bottom of a cylindrical peripheral wall 110, and side panels 112 are positioned on the circumference of the cylinder on each of the left and right sides of the floor panel 111, and the protruding convex portions 14 of the side panels 112 fit into the cutout recesses 13 at both left and right ends of the floor panel 111.

[0030] The side panels 112 are arranged on the circumference of the cylinder, and their lower ends are joined to the floor panel 111 or to a side panel 112 joined to the floor panel 111. The side panels 112 are stacked according to the size of the peripheral wall 110, and the protruding convex portions 14 of the side panels 112 fit into the cutout recesses 13 of the floor panel 111 or the side panels 112.

[0031] The upper side panels 114 are disposed on the upper left and right sides of the circumference of the cylinder, with their lower ends joined to the side panels 112, and the protruding convex portions 14 on the lower sides of the upper side panels 114 fitting into the notched recessed portions 13 of the side panels 112. The upper sides of the upper side panels 114 disposed on the left and right sides each have a notched joint portion 15 with the outer side cut out.

[0032] The top panel 113 has notches 15 on both left and right ends, which fit into notches 15 on the outside of the upper side panels 114 arranged on the left and right. This closes the circumference, forming a cylindrical peripheral wall 110.

[0033] As shown in Fig. 1, the front and back of the cylindrical peripheral wall 110 are closed by fitting a front wall 120 and a rear wall 130 made of lightweight panels 10 formed to the shape of the inner circumference of the peripheral wall 110, forming a structural wall 1 that serves as a partition separating the inside of the sauna room 100 from the outside. As shown in Figs. 1 to 3, the cylindrical sauna room 100 is placed on a pedestal 106 that fits the shape of the peripheral wall 110 so that it can be installed stably, and is installed outdoors, etc.

[0034] The lightweight panel 10 can be made of expandable polystyrene beads (EPS), which are easy to mold by bead foaming, and has a thickness of 150 to 500 mm and a bulk density of 17 to 33 kg / m 3 For example, a foaming ratio of 30 to 60 can be used. The lightweight panel 10 can be easily cut with a cutter knife or the like, so that the fitting portions 12 (notched recesses 13, protruding protrusions 14, and joint portions 15) can be easily formed on the butting surfaces 11, and the size of the lightweight panel 10 can be easily adjusted. Therefore, the size of the sauna room 100 as a house can be freely set.

[0035] When EPS as the lightweight panel 10 is used in the structural wall 1 arranged as a partition separating the inside of the sauna room 100 from the outside, it allows the structural wall 1 (sauna room 100) to stand on its own without the need for reinforcing materials such as metal members. Therefore, the sauna room 100 formed from EPS is lightweight, and is easy to install and move. In addition, since EPS as the lightweight panel 10 has plasticity, when a user in the sauna room 100 hits his / her head or other part against the structural wall 1, the impact on the head or other part is reduced due to the plasticity, and the head or other part is protected.

[0036] The joint 16 between the protruding convex portion 14 and the notched recess 13 of the fitting portion 12 of the lightweight panel 10, the joint 16 between the joint portion 15 cut out on the inside and the joint portion 15 cut out on the outside, and the fitting portion 17 where the front wall 120 or the rear wall 130 is fitted into the peripheral wall 110 are each bonded together by caulking material as a bonding material 20.

[0037] The caulking material as the joining material 20 is a material that bonds the joints 16 between the lightweight panels 10 forming the peripheral wall 110 and the fitting parts 17 between the peripheral wall 110 and the front wall 120 or the rear wall 130. The caulking material may be made of a moisture-curing silicone caulking material, a urethane caulking material, a dry-curing acrylic caulking material, a butyl rubber caulking material, or the like. In another embodiment, a moisture-curing caulking material that shrinks less when cured may be used, and in yet another embodiment, a silicone caulking material may be used.

[0038] The caulking material as the bonding material 20 can be replenished by pressing into the joints 16 where the lightweight panels 10 come into contact with each other and into the fitting parts 17 between the peripheral wall 110 and the front wall 120 or the rear wall 130 from both inside and outside the sauna room 100 as a house. This allows the joints 16 and fitting parts 17 of the lightweight panels 10 to be filled with the caulking material as the bonding material 20 without leaving any gaps, improving the adhesion between the joints 16 and the fitting parts 17. Note that pressing is a method of applying the caulking material as the bonding material 20 thinly and smoothly into the joints 16 by rubbing it with a plastering trowel.

[0039] Resin is applied to the inside surface of the lightweight panel 10, which is the interior side of the sauna room 100 serving as a house, to form an inner coating layer 21 that provides durability, and an interior topcoat material is applied to the surface of the inner coating layer 21 made of resin to form an interior protective layer 22. Also, resin is applied to the outside surface of the lightweight panel 10, which is the exterior of the sauna room 100, to form an outer coating layer 26 that provides durability, and an exterior topcoat material is applied to the surface of the outer coating layer 26 made of resin to form an exterior protective layer 27.

[0040] The inner coating layer 21 and the outer coating layer 26 are made of the same type of resin and are formed on the inside and outside of the sauna room 100 to impart durability to the sauna room 100. A resin with an elongation rate (ASTM D-412) of 100 to 1000% can be used. With an elongation rate of 100 to 1000%, the inner coating layer 21 and the outer coating layer 26 can follow deformation caused by thermal expansion of the sauna room 100 and vibrations caused by external factors, ensuring the durability of the house. If the elongation rate of the inner coating layer 21 and the outer coating layer 26 is less than 100%, they will not be able to follow deformation of the sauna room 100, and cracks may occur in the inner coating layer 21 and the outer coating layer 26, making it difficult to ensure durability. On the other hand, if the elongation rate of the inner covering layer 21 and the outer covering layer 26 exceeds 1000%, durability can be ensured, but the inner covering layer 21 and the outer covering layer 26 will become flexible and soft, causing a sticky feeling and making them more susceptible to dirt adhesion, and there is a risk of causing discomfort to users of the sauna room 100. In another embodiment, the elongation rate of the inner covering layer 21 and the outer covering layer 26 is 150 to 800%, and in yet another embodiment, the elongation rate is 200 to 600%.

[0041] As the resin forming the inner coating layer 21 and the outer coating layer 26, general-purpose resins such as urea resin, urethane resin, silicone resin, and acrylic resin can be used. As another embodiment, urea resin or urethane resin that can be instantly cured can be used, and as a further embodiment, urea resin that is difficult to hydrolyze can be used. Urea resin (polyurea) is a resin generated by mixing an isocyanate component and an amine component at the tip of a spray gun. Urethane resin (polyurethane) is a resin generated by mixing an isocyanate component and a polyol component at the tip of a spray gun. In addition, a mixture of urea resin and urethane resin can also be used as the resin forming the inner coating layer 21 and the outer coating layer 26. In addition, the resin forming the inner coating layer 21 and the outer coating layer 26 can also be colored with a pigment or a colored aggregate.

[0042] The coating weight of the inner coating layer 21 and the outer coating layer 26 is 0.5 to 5 kg / m 2 (film thickness: about 0.5 to 5 mm). This is because sufficient durability can be exhibited. The coating amount of the inner coating layer 21 and the outer coating layer 26 is 0.5 kg / m 2 If the coating amount is less than 5 kg / m, the coating thickness is too thin, and when an impact is received from an external factor, the inner coating layer 21 and the outer coating layer 26 may crack or peel off, and durability may not be maintained. 2 If the thickness exceeds 100 μm, durability is ensured, but the thickness becomes excessively thick, which may be uneconomical. In another embodiment, the coating amount of the inner coating layer 21 and the outer coating layer 26 is 1 to 4 kg / m 2 (film thickness: about 1 to 4 mm), and in another embodiment, 2 to 3 kg / m 2 (film thickness: about 2 to 3 mm).

[0043] In addition, in the embodiments, the "amount applied" and the "parts by mass (%)" when expressing the amount or ratio of resin or topcoat material mean the "amount applied of non-volatile matter" excluding volatile matter, and "parts by mass (%) of non-volatile matter", unless otherwise specified.

[0044] The interior protective layer 22 is applied to improve the heat resistance of the inner coating layer 21. The interior topcoat material forming the interior protective layer 22 is applied to the inside of the sauna room 100 as a house, so a general-purpose emulsion paint with excellent heat resistance can be used. The resin emulsion of the interior topcoat material forming the interior protective layer 22 can be a vinyl acetate emulsion, an ethylene vinyl acetate emulsion, an acrylic emulsion, an acrylic styrene emulsion, an acrylic silicone emulsion, an acrylic urethane emulsion, or the like, depending on its resin composition. As another embodiment, an acrylic emulsion, an acrylic styrene emulsion, an acrylic silicone emulsion, or an acrylic urethane emulsion, which are excellent in heat resistance, can be used. As yet another embodiment, an acrylic emulsion, an acrylic silicone emulsion, or an acrylic urethane emulsion, which are excellent in water resistance in addition to heat resistance, can be used.

[0045] The interior coating material forming the interior protective layer 22 can contain a metallic pigment. The metallic pigment has excellent heat insulating properties and reflects the heat of the sauna room 100, so that the heat resistance of the inner coating layer 21 can be further improved. As the metallic pigment, titanium oxynitride powder, titanium-manganese composite oxide powder, titanium dioxide powder, aluminum powder, etc. can be used.

[0046] The metallic pigment can be contained in the interior topcoat material forming the interior protective layer 22 in an amount of 1 to 50% by mass. This is because the interior protective layer 22 can maintain heat-shielding properties and the heat resistance of the inner coating layer 21 can be improved. If the content of the metallic pigment is less than 1% by mass, the interior protective layer 22 may not maintain sufficient heat-shielding properties. On the other hand, if the content of the metallic pigment exceeds 50% by mass, the resin component becomes relatively small, and the movement of the inner coating layer 21 may not be followed, which may cause cracking or peeling. In another embodiment, the metallic pigment can be contained in the interior topcoat material forming the interior protective layer 22 in an amount of 3 to 25% by mass, and in yet another embodiment, it can be contained in an amount of 5 to 15% by mass.

[0047] The coating amount of the interior protection layer 22 is 0.05 to 0.5 kg / m 2 (film thickness: about 0.05 to 0.5 mm). This is because sufficient heat resistance can be exhibited. The coating amount of the interior protection layer 22 is 0.05 kg / m 2 If the coating weight is less than 0.5 kg / m, the thickness of the interior protective layer 22 is too thin to follow the movement of the inner coating layer 21, which may cause cracking or peeling. 2 If the coating amount of the interior protective layer 22 exceeds 0.06 to 0.2 kg / m, the heat resistance is ensured, but the coating thickness becomes excessively thick, which may be uneconomical. 2 (film thickness: about 0.06 to 0.2 mm), and in yet another embodiment, 0.07 to 0.1 kg / m 2 (film thickness: about 0.07 to 0.1 mm).

[0048] The inner coating layer 21 and the interior protection layer 22 formed on the inner surface of the lightweight panel 10 are flexible. Therefore, when a user in a sauna room 100 having the lightweight panel 10 as a body hits his / her head or other part against the lightweight panel 10 (structural wall 1) on which the inner coating layer 21 and the interior protection layer 22 are formed, the flexibility reduces the impact on the head and other parts, thereby protecting the head and other parts.

[0049] The exterior protective layer 27 is applied to improve the weather resistance of the outer covering layer 26 and thus the heat retention of the sauna room 100. The exterior protective layer 27 also adds design to the exterior of the sauna room 100. For this reason, the exterior protective layer 27 contains 30 to 50 mass % of a filler (aggregate).

[0050] The exterior topcoat material forming the exterior protective layer 27 is applied to the outside of the sauna room 100 as a house, so a general-purpose emulsion paint with excellent weather resistance can be used. The resin emulsion of the topcoat material forming the exterior protective layer 27 can be a vinyl acetate emulsion, an ethylene vinyl acetate emulsion, an acrylic emulsion, an acrylic styrene emulsion, an acrylic silicone emulsion, an acrylic urethane emulsion, or the like, depending on its resin composition. As another embodiment, an acrylic emulsion, an acrylic styrene emulsion, an acrylic silicone emulsion, or an acrylic urethane emulsion, which are excellent in weather resistance, can be used. As yet another embodiment, an acrylic emulsion, an acrylic silicone emulsion, or an acrylic urethane emulsion, which are excellent in weather resistance and water resistance, can be used.

[0051] Calcium carbonate, silica sand, glass beads, etc. are used as fillers (aggregates) contained in the exterior topcoat material that forms the exterior protective layer 27. In order to impart design to the exterior protective layer 27, these fillers (aggregates) have a particle diameter (d50 (cumulative 50 vol% diameter)) of 0.1 to 2.0 mm.

[0052] The exterior topcoat material forming the exterior protective layer 27 can contain inorganic pigments. This is because inorganic pigments have excellent heat absorption properties for sunlight and can improve the heat retention of the sauna room 100. Carbon black, iron black, yellow iron oxide, red iron oxide, etc. can be used as inorganic pigments.

[0053] The coating amount of the exterior protective layer 27 is 0.5 to 3.0 kg / m 2 (film thickness: about 0.5 to 3.0 mm). This is because sufficient weather resistance and heat retention can be achieved. The coating amount of the exterior protective layer 27 is 0.5 kg / m 2 If the coating weight of the exterior protective layer 27 is less than 3.0 kg / m, the thickness of the exterior protective layer 27 is too thin to follow the movement of the inner coating layer 21, which may cause cracking or peeling. 2If the coating amount of the exterior protective layer 27 exceeds 0.8 to 2.0 kg / m, the weather resistance and heat retention are ensured, but the coating thickness becomes excessively thick, which may be uneconomical. 2 (film thickness: about 0.8 to 2.0 mm), and in yet another embodiment, 1.0 to 1.5 kg / m 2 (film thickness: about 1.0 to 1.5 mm).

[0054] Next, a method for installing a sauna room 100 using the structural wall 1 of the first embodiment will be described. The method for installing the sauna room 100 of the embodiment includes an assembly process for joining the lightweight panel 10 and assembling it to the cylindrical structural wall 1, a fixture installation process for attaching the front wall 120 and the rear wall 130 and installing fixtures such as a hinged door 101 in the sauna room 100, a coating layer formation process for forming an inner coating layer 21 and an outer coating layer 26 on the inner and outer sides of the sauna room 100, an interior protective layer formation process for forming an interior protective layer 22 on the surface of the inner coating layer 21, and an exterior protective layer formation process for forming an exterior protective layer 27 on the surface of the outer coating layer 26, in that order.

[0055] The lightweight panel 10 that forms the framework of the structural wall 1 of the sauna room 100 has a foaming ratio of 50 times and a bulk density of 20 kg / m 3 We used polystyrene foam (EPS) with a thickness of 120 mm, a length in the front-to-rear direction of 3,500 mm, and a length in the circumferential direction of 600 to 800 mm.

[0056] In the lightweight panel 10 that will become the floor panel 111, a notched recess 13 cut out in a rectangular cross section is formed along the front-rear direction on the butt surfaces 11 at both left and right ends in the circumferential direction as a fitting portion 12. In the lightweight panel 10 that will become the side panel 112, a protruding convex portion 14 protruding from the center of the cross section is formed as a fitting portion 12 on the butt surface 11 at the lower end, and a notched recess 13 cut out in a rectangular cross section is formed as a fitting portion 12 on the butt surface 11 at the upper end. In the lightweight panel 10 that will become the top panel 113, a notched portion 15 cut out on the inside is formed as a fitting portion 12 along the front-rear direction on the butt surfaces 11 at both left and right ends in the circumferential direction. In the lightweight panel 10 which becomes the upper side panel 114, a protruding convex portion 14 is formed as a fitting portion 12 on the butt surface 11 of the lower end, and a joint portion 15 with an outer side cut out is formed as the fitting portion 12 on the butt surface 11 of the upper end.

[0057] In the assembly process, the lightweight panels 10 were arranged along the outer periphery of the cylindrical sauna room 100, and adhesive 20 was applied to each fitting portion 12 of the joints 16 of the butt surfaces 11 of the lightweight panels 10, and the butt surfaces 11 of the lightweight panels 10 were joined together while being assembled.

[0058] The procedure of the assembly process is as follows: the floor panel 111 is placed on the placement surface on which the sauna room 100 is placed, the protruding convex parts 14 of the side panel 112 are joined from the left and right to the left and right notched recesses 13 of the floor panel 111, and the protruding convex parts 14 of the side panel 112 are joined from the left and right to the notched recesses 13 of the left and right side panels 112, respectively, to gradually form a cylindrical shape. Then, the protruding convex parts 14 of the upper side panel 114 are joined from the left and right to the notched recesses 13 of the left and right side panels 112, respectively, to the left and right, and the joint parts 15 with the outer side cut out as the fitting parts 12 appear at the opposing ends of the left and right upper side panels 114. The top panel 113 with the joint parts 15 with the inner side cut out on the left and right sides is fitted so as to connect the joint parts 15 with the outer side cut out on the left and right sides, and the peripheral wall 110 of the sauna room 100 is closed in the circumferential direction to form a cylindrical shape.

[0059] In the assembly process, a bonding material 20 made of a silicone-based caulking material is applied to the fitting parts 12 that form the joints 16 of the butt surfaces 11 that form the joints of the lightweight panels 10, bonding the lightweight panels 10 together. In addition, the bonding material 20 is replenished by pressing and applying the bonding material 20 to the butt surfaces 11 that form the joints of the lightweight panels 10 from both the inside and outside of the sauna room 100, thereby improving the adhesion of the joints 16.

[0060] The equipment installation process is a process of attaching a front wall 120 to the front side and a rear wall 130 to the rear side of the peripheral wall 110 of the sauna room 100, and attaching a hinged door 101 to the front wall 120 and a light window 102 to the peripheral wall 110. The front wall 120 and the rear wall 130 are attached to the peripheral wall 110 by bonding them with a bonding material 20 made of a silicone-based caulking material, and by driving fixing nails (not shown) into the front wall 120 and the rear wall 130 from the outside of the peripheral wall 110. The hinged door 101 is attached by fitting an outer frame (not shown) of the hinged door 101 into the front wall 120, and the light window 102 is attached by fitting an outer frame (not shown) of the light window 102 into the peripheral wall 110. Since there is a risk that resin or the like will adhere to and contaminate the hinged door 101 and the skylight window 102 in the next coating layer forming process and thereafter, both the inside and outside are masked with masking tape.

[0061] In the coating layer forming process, resin is applied to the inner and outer surfaces of the lightweight panel 10, which will form the inside and outside of the sauna room 100 as a house, to form the inner coating layer 21 and the outer coating layer 26. In this embodiment, a commercially available urea resin is used for the resin that forms the inner coating layer 21 and the outer coating layer 26, which is formed by mixing an isocyanate component and an amine component at the tip of a spray gun. The inner coating layer 21 and the outer coating layer 26 made of urea resin in this embodiment have an elongation rate (ASTM D-412) of 300%, and the coating amount is 2.0 kg / m 2 (film thickness: approximately 2.0 mm).

[0062] The interior protection layer forming step is a step of applying an interior topcoat material that forms the interior protection layer 22 to the surface of the inner coating layer 21 formed from resin. In the embodiment, the interior topcoat material is a general-purpose acrylic emulsion paint (JIS K 5660 glossy synthetic resin emulsion paint), and the application amount is 0.08 kg / m 2 (Film thickness: about 0.08 mm). The acrylic emulsion paint used as the interior topcoat contains about 10% by mass of titanium dioxide powder to reflect the heat from the sauna room 100 due to its heat-shielding properties.

[0063] The exterior protective layer forming step is a step of applying a topcoat material that forms an exterior protective layer 27 to the surface of the outer coating layer 26 formed from a resin. In the embodiment, the exterior topcoat material is a general-purpose acrylic emulsion paint (JIS A 6909 Exterior Thin Coating Material E), and the application amount is 1.2 kg / m 2 (Film thickness: about 1.2 mm). The acrylic emulsion paint used for the exterior topcoat is colored black by incorporating about 3% by mass of carbon black in order to absorb the heat of sunlight and improve the heat retention of the sauna room 100.

[0064] As shown in FIG. 3, the sauna room 100 is equipped with seats 103, a heater (not shown), and other components inside, so that the sauna room 100 can function as a sauna room for steam and hot air bathing.

[0065] According to the structural wall 1 of the embodiment of the present specification, a structural wall 1 of a house can be formed by filling a joint 16 formed by butting abutting surfaces 11 of a lightweight panel 10 and a lightweight panel 10 arranged adjacent to each other and fitting a fitting portion 12 with a bonding material 20. In addition, an inner coating layer 21 is formed on the side of the lightweight panel 10 that faces the inside of the house, and durability is imparted to the lightweight panel 10 as the structural wall 1. The structural wall 1 is formed by filling a bonding material 20 in the joint 16 where the lightweight panels 10 are in contact with each other and providing an inner coating layer 21 on the inside side of the lightweight panel 10. Therefore, the structural wall 1 according to the embodiment can be easily installed.

[0066] Second embodiment Hereinafter, a box-type store 100A as a house equipped with a structural wall 1 according to a second embodiment of the present specification will be described with reference to Fig. 5. In the second embodiment, elements common to the first embodiment will be denoted by the same reference numerals and will not be described.

[0067] As shown in FIG. 5, the box-type store 100A of the second embodiment has a substantially box-shaped shape, and a peripheral wall 110 is formed from a continuous structural wall 1 that goes around the circumference of a cylindrical side. The peripheral wall 110 is formed by filling a joint 16 where abutting surfaces 11 of a lightweight panel 10 and an adjacent lightweight panel 10 are butted against each other and a fitting portion 12 is fitted into the joint 16, with a joining material 20. The front and rear surfaces surrounded by the peripheral wall 110 of the box-type store 100A are closed by a front wall 120 and a rear wall 130 made of the structural wall 1. A sales window 107 for selling food, beverages, and goods to customers is provided in the front wall 120, and a hinged door 101 for employees to enter and exit is provided on the right side of the peripheral wall 110. Since employees perform work and the like inside the box-type store 100A, it is required that the room temperature does not rise excessively, and when food and drink are handled, the inside side is required to be water-resistant.

[0068] Resin (resin) is applied to the inner surface of the lightweight panel 10, which is the inside side of the box-type store 100A, to form an inner coating layer 21 that imparts durability, and an interior topcoat material that forms an interior protective layer 22A is applied to the surface of the inner coating layer 21 formed from resin. Also, resin (resin) is applied to the outer surface of the lightweight panel 10, which is the outside of the box-type store 100A, to form an outer coating layer 26 that imparts durability, and an exterior topcoat material that forms an exterior protective layer 27A is applied to the surface of the outer coating layer 26 formed from resin.

[0069] The interior protection layer 22A is applied to improve the water resistance of the inner coating layer 21. A general-purpose emulsion paint having excellent water resistance can be used as the interior topcoat material forming the interior protection layer 22A. In the embodiment, a glossy synthetic resin emulsion paint (JIS K 5660) is used as the interior topcoat material forming the interior protection layer 22A.

[0070] The coating amount of the interior protective layer 22A is 0.05 to 0.5 kg / m 2 (film thickness: about 0.05 to 0.5 mm). This is because sufficient water resistance can be exhibited. The coating amount of the interior protection layer 22A is 0.05 kg / m 2 If the coating amount of the interior protective layer 22A is less than 0.5 kg / m, the coating thickness is too thin to follow the movement of the inner coating layer 21, which may cause cracking or peeling, resulting in poor water resistance. 2 If the coating amount of the interior protective layer 22 exceeds 0.06 to 0.2 kg / m, the water resistance is ensured, but the coating thickness becomes excessively thick, which may be uneconomical. 2 (film thickness: about 0.06 to 0.2 mm), and in yet another embodiment, 0.07 to 0.1 kg / m 2 (film thickness: about 0.07 to 0.1 mm).

[0071] The exterior protective layer 27A is applied to improve the weather resistance of the outer coating layer 26. The exterior topcoat material forming the exterior protective layer 27A is applied to the outside of the box-type store 100A, so a general-purpose emulsion paint with excellent weather resistance can be used. In the embodiment, a high solar reflectance paint for roofs (JIS K5675) Class 1 LG grade was used for the exterior topcoat material forming the exterior protective layer 27A. The high solar reflectance paint for roofs contains titanium-manganese composite oxide powder as a metal pigment and effectively reflects the radiant heat of the sun, so it has excellent weather resistance and can suppress the rise in room temperature inside the box-type store 100A. In addition, the high solar reflectance paint for roofs as an exterior topcoat material can contain 10 to 30 mass% of hollow filler, which can further suppress the rise in room temperature inside the box-type store 100A.

[0072] The coating amount of the exterior protective layer 27A is 0.1 to 1.0 kg / m 2 (film thickness: about 0.1 to 1.0 mm). This is because sufficient weather resistance can be exhibited. The coating amount of the exterior protective layer 27A is 0.1 kg / m 2 If the coating weight of the exterior protective layer 27A is less than 1.0 kg / m, the coating thickness is too thin to follow the movement of the inner coating layer 21, which may cause cracking or peeling, resulting in poor weather resistance. 2 If the coating amount of the exterior protective layer 27A exceeds 0.2 to 0.8 kg / m, the weather resistance is ensured, but the coating thickness becomes excessively thick, which may be uneconomical. 2 (film thickness: about 0.2 to 0.8 mm), and in yet another embodiment, 0.3 to 0.5 kg / m 2 (film thickness: about 0.3 to 0.5 mm).

[0073] The structural wall 1 as a partition of a house in the embodiment can be modified in its configuration as follows.

[0074] In the structural wall 1 of the embodiment, the lightweight panel 10 uses polystyrene foam (EPS) which is easy to mold by bead foaming, but the lightweight panel 10 can be any lightweight panel. Polymer foam and inorganic foam can be used as the material for the lightweight panel. As the polymer foam, polystyrene foam, polyurethane foam, polyphenol foam, polyolefin foam (polyethylene foam, polypropylene foam), etc. can be used. As the inorganic foam, aluminum hydroxide foam (Talbocel), cement foam (ALC (autoclaved lightweight aerated concrete)), etc. can also be used.

[0075] In the structural wall 1 of the embodiment, the lightweight panel 10 uses EPS with an expansion ratio of 50 times, but any expansion ratio of 30 to 60 times can be used as the EPS of the lightweight panel 10. If the expansion ratio of the EPS is less than 30 times, a large amount of resin (beads) is required, which may be uneconomical. On the other hand, if the expansion ratio of the EPS is more than 60 times, the strength is weak and there is a risk of plastic deformation when impact is received. In another embodiment, the expansion ratio of the EPS can be 40 to 55 times.

[0076] In the embodiment of the lightweight panels 10 of the structural wall 1 of the sauna room 100, the lightweight panels 10 are joined together and the gaps between the lightweight panels 10 are sealed using caulking material as the joining material 20. However, if there are gaps between the lightweight panels 10 to be joined, a panel made of the same material as the lightweight panels 10 can be processed to a size that will fill the gap, thereby sealing the gap between the lightweight panels 10.

[0077] In addition, other technical ideas that can be understood from the structural wall 1 of the embodiment will be described below.

[0078] A sauna room characterized in that an interior protective layer is formed from a glossy synthetic resin emulsion paint (JIS K 5660) containing a metallic pigment, and an exterior protective layer is formed from an acrylic emulsion paint (JIS A 6909 Exterior Thin Coating Material E) containing an inorganic pigment. This can improve the heat retention of the sauna room.

[0079] A box-type store characterized in that the interior protective layer is formed from glossy synthetic resin emulsion paint (JIS K 5660) and the exterior protective layer is formed from high solar reflectance paint for roofs (JIS K 5675). This makes it possible to increase the water resistance inside the store and suppress the rise in room temperature inside the store. [Explanation of symbols]

[0080] 1 structural wall 10 Lightweight Panels 11. Butt Surface 12 Fitting part 13 Notch recess 14 Protruding part 15 Joint part 16 Joint 17 Inset part 20 Bonding material 21 Inner coating layer 22 Interior protection layer 22A Interior protective layer 26 Outer coating layer 27 Exterior protective layer 27A Exterior protective layer 100 Sauna room 100A Box-type store 101 Swing Door 102 Skylight window 103 Seat 107 Sales window 106 Pedestal 110 Peripheral wall 111 Floor Panel 112 Side Panel 113 Top Panel 114 Upper side panel 120 Front wall 130 Rear wall

Claims

1. A structural wall that is arranged as a partition separating the inside of a house from the outside, The structure is made up of multiple lightweight panels. The lightweight panel is joined to an adjacent lightweight panel in the partition of the house; Each of the butt surfaces of the two lightweight panels is provided with a fitting portion along the butt surface, A joint portion where the butt surfaces of the two lightweight panels are butted together and the fitting portions are fitted together is joined by a joining material that joins the two lightweight panels, A structural wall, characterized in that an inner covering layer is formed on the side of the lightweight panel that faces the interior of the house.

2. 2. The structural wall according to claim 1, wherein an outer covering layer is formed on the side of the lightweight panel that faces the exterior of the house.

3. 3. The structural wall of claim 2, wherein the inner and outer coating layers each have an elongation (ASTM D-412) of 100% or greater.

4. A house, characterized in that the partition is a structural wall according to claim 2 or 3.

5. The house according to claim 4 is a sauna room, A sauna room characterized in that a heater for heating the inside is provided inside the sauna room, and an interior protection layer is provided on the surface of the inner coating layer.

6. The sauna room according to claim 5, characterized in that an exterior protective layer is provided on the surface of the outer coating layer.

Citation Information

Patent Citations

  • Modified graphene water-based polyurea resin as well as preparation method and application thereof

    CN111171276A

  • Single-component self-crosslinking polyurethane-polyurea aqueous dispersion as well as preparation method and application thereof

    CN113004493A

  • Professional cabin for wellbeing treatments, such as turkish baths, saunas and the like and a method for making such cabins

    EP2453061A1

  • Foam body panel and assembly type house

    JP2018123493A

  • Sauna room structure

    JP3233199U

Cited By

  • Exterior wall materials and exterior walls of structures constructed using them

    JP2026162310A

  • Exterior wall materials and exterior walls of structures constructed using them

    JP7886055B1