Display device, and manufacturing method for display device

A display device with a rib and partition wall structure, along with chemical treatment, addresses the issue of display characteristic deterioration in OLED devices by protecting electrode surfaces and maintaining luminous efficiency.

JP2024158890AInactive Publication Date: 2024-11-08JAPAN DISPLAY INC
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2023074508
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-28
Publication Date
2024-11-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Display devices using organic light emitting diodes (OLEDs) face deterioration of display characteristics during manufacturing.

Method used

The display device incorporates a lower electrode with varying thickness portions, a rib structure, and a partition wall with specific overhang shapes to protect the electrode surfaces, combined with chemical treatment to repair etching damage, ensuring consistent display quality.

Benefits of technology

The solution effectively reduces the impact of etching damage on electrode surfaces, maintaining optimal display characteristics and luminous efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024158890000001_ABST
    Figure 2024158890000001_ABST
Patent Text Reader

Abstract

To provide a display device capable of suppressing deterioration of a display characteristic, and a video method for the display device.SOLUTION: A display device according to an embodiment includes: a lower electrode; a rib covering a first part of the lower electrode and including a pixel opening overlapping with a second part of the lower electrode; a partition wall including a bottom part disposed on the rib, a shaft part disposed on the bottom part, and a top part disposed on the shaft part and protruding from a side surface of the shaft part; an organic layer covering the lower electrode through the pixel opening; and an upper electrode covering the organic layer and disposed in contact with the bottom part. A thickness of a first part of the lower electrode is different from a thickness of a second part of the lower electrode.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] FIELD An embodiment of the present invention relates to a display device and a method for manufacturing a display device. [Background technology]

[0002] In recent years, display devices that use organic light-emitting diodes (OLEDs) as display elements have been put to practical use.

[0003] During the process of manufacturing the above-mentioned display device, there is a possibility that the display characteristics of the display device may deteriorate. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2000-195677 A [Patent Document 2] JP 2004-207217 A [Patent Document 3] JP 2008-135325 A [Patent Document 4] JP 2009-32673 A [Patent Document 5] JP 2010-118191 A [Patent Document 6] International Publication No. 2018 / 179308 [Patent Document 7] US Patent Application Publication No. 2022 / 0077251 [Patent Document 8] JP 2013-213733 A Summary of the Invention [Problem to be solved by the invention]

[0005] Therefore, an object of the present invention is to provide a display device capable of suppressing deterioration of display characteristics and a method for manufacturing the display device. [Means for solving the problem]

[0006] A display device according to an embodiment includes a lower electrode, a rib covering a first portion of the lower electrode and having a pixel opening overlapping a second portion of the lower electrode, a partition including a bottom portion disposed on the rib, an axis portion disposed on the bottom portion, and a top portion disposed on the axis portion and protruding from a side surface of the axis portion, an organic layer covering the lower electrode through the pixel opening, and an upper electrode covering the organic layer and in contact with the bottom portion. The thickness of the first portion of the lower electrode is different from the thickness of the second portion of the lower electrode. [Brief description of the drawings]

[0007] [Figure 1] FIG. 1 is a diagram showing an example of the configuration of a display device according to an embodiment. [Diagram 2] FIG. 4 is a schematic plan view showing an example of a layout of sub-pixels. [Diagram 3] FIG. 3 is a schematic cross-sectional view of the display device taken along line III-III in FIG. [Figure 4] FIG. 11 is a schematic cross-sectional view showing an example of a configuration that can be applied to a partition wall. [Diagram 5] 11 is a flowchart showing an example of a manufacturing method of a display device. [Figure 6] 5A to 5C are schematic cross-sectional views showing an example of a process for forming ribs and partition walls. [Figure 7] 7 is a schematic cross-sectional view showing a step following FIG. 6. [Figure 8] 8 is a schematic cross-sectional view showing a step following FIG. 7. [Figure 9] 9 is a schematic cross-sectional view showing a step following FIG. 8. [Figure 10] 10 is a schematic cross-sectional view showing a step following FIG. 9 . [Figure 11] 11 is a schematic cross-sectional view showing a step subsequent to FIG. 10 . [Figure 12] 1A to 1C are schematic cross-sectional views showing an example of a process for forming a display element. [Figure 13] 13 is a schematic cross-sectional view showing a step following FIG. 12. [Figure 14] 14 is a schematic cross-sectional view showing a step following FIG. 13. [Figure 15] 15 is a schematic cross-sectional view showing a step following FIG. 14. [Figure 16] 16 is a schematic cross-sectional view showing a step following FIG. 15 . [Figure 17] 17 is a schematic cross-sectional view showing a step following FIG. 16. [Figure 18] FIG. 4 is a diagram for explaining a chemical solution treatment. [Figure 19] 11 is a schematic cross-sectional view including an end portion of a pixel opening after a chemical liquid treatment is performed. [Figure 20] 11 is a schematic cross-sectional view including an end portion of a pixel opening after a chemical liquid treatment is performed. [Figure 21] 10 is a flowchart showing another example of a method for manufacturing a display device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] An embodiment will be described with reference to the drawings. The disclosure is merely an example, and those who are skilled in the art can easily conceive of appropriate modifications that maintain the spirit of the invention are naturally included in the scope of the present invention. In addition, the drawings may be schematic in terms of width, thickness, shape, etc., of each part compared to the actual embodiment in order to make the explanation clearer, but they are merely examples and do not limit the interpretation of the present invention. In this specification and each figure, components that perform the same or similar functions as those described above with respect to the previous figures are given the same reference numerals, and duplicate detailed explanations may be omitted as appropriate.

[0009] In addition, in the drawings, an X-axis, a Y-axis, and a Z-axis that are perpendicular to each other are shown as necessary to facilitate understanding. The direction along the X-axis is called the first direction X, the direction along the Y-axis is called the second direction Y, and the direction along the Z-axis is called the third direction Z. The third direction Z is a normal direction to a plane that includes the first direction X and the second direction Y. Also, viewing various elements parallel to the third direction Z is called planar view.

[0010] The display device according to this embodiment is an organic electroluminescence display device having an organic light-emitting diode (OLED) as a display element, and can be mounted in various electronic devices such as televisions, personal computers, in-vehicle devices, tablet terminals, smartphones, mobile phone terminals, and wearable terminals.

[0011] 1 is a diagram showing an example of the configuration of a display device DSP according to this embodiment. The display device DSP has a display area DA for displaying an image and a peripheral area SA around the display area DA, on an insulating substrate 10. The substrate 10 may be glass or a flexible resin film.

[0012] In this embodiment, the shape of the substrate 10 in a plan view is rectangular. However, the shape of the substrate 10 in a plan view is not limited to a rectangle, and may be other shapes such as a square, a circle, or an ellipse.

[0013] The display area DA includes a plurality of pixels PX arranged in a matrix in the first direction X and the second direction Y. The pixels PX include a plurality of subpixels SP. In one example, the pixel PX includes a blue subpixel SP1, a green subpixel SP2, and a red subpixel SP3. The pixel PX may include subpixels SP of other colors, such as white, in addition to the subpixels SP1, SP2, and SP3. The pixel PX may also include subpixels SP of other colors instead of any of the subpixels SP1, SP2, and SP3.

[0014] The subpixel SP includes a pixel circuit 1 and a display element DE driven by the pixel circuit 1. The pixel circuit 1 includes a pixel switch 2, a drive transistor 3, and a capacitor 4. The pixel switch 2 and the drive transistor 3 are switching elements constituted by, for example, thin film transistors.

[0015] The gate electrode of the pixel switch 2 is connected to the scanning line GL. One of the source electrode and drain electrode of the pixel switch 2 is connected to the signal line SL, and the other is connected to the gate electrode of the drive transistor 3 and a capacitor 4. In the drive transistor 3, one of the source electrode and drain electrode is connected to the power line PL and the capacitor 4, and the other is connected to the display element DE.

[0016] It should be noted that the configuration of the pixel circuit 1 is not limited to the example shown in the drawing. For example, the pixel circuit 1 may include more thin film transistors and capacitors.

[0017] Fig. 2 is a schematic plan view showing an example of the layout of subpixels SP1, SP2, and SP3. In the example shown in Fig. 2, subpixels SP2 and SP3 are aligned with subpixel SP1 in a first direction X. Furthermore, subpixels SP2 and SP3 are aligned with subpixel SP1 in a second direction Y.

[0018] When the subpixels SP1, SP2, and SP3 are laid out in this manner, a column in which a plurality of subpixels SP1 are repeatedly arranged in the second direction Y, and a column in which the subpixels SP2 and SP3 are alternately arranged in the second direction Y are formed in the display area DA. These columns are arranged alternately in the first direction X. Note that the layout of the subpixels SP1, SP2, and SP3 is not limited to the example shown in FIG.

[0019] In the display area DA, ribs 5 and partition walls 6 are arranged. The rib 5 has pixel apertures AP1, AP2, and AP3 in the subpixels SP1, SP2, and SP3, respectively. In the example shown in Fig. 2, the pixel aperture AP1 is larger than the pixel aperture AP2, and the pixel aperture AP2 is larger than the pixel aperture AP3.

[0020] The partition 6 is disposed at the boundary between adjacent sub-pixels SP and overlaps with the rib 5 in a plan view. The partition 6 has a plurality of first partitions 6x extending in the first direction X and a plurality of second partitions 6y extending in the second direction Y. The first partition 6x is disposed between two pixel openings AP1 adjacent to each other in the second direction Y. The first partition 6x is disposed between pixel openings AP2 and AP3 adjacent to each other in the second direction Y. The second partition 6y is disposed between pixel openings AP1 and AP2 adjacent to each other in the first direction X. The second partition 6y is disposed between pixel openings AP1 and AP3 adjacent to each other in the first direction X.

[0021] 2, the first partition 6x and the second partition 6y are connected to each other. As a result, the partition 6 as a whole has a lattice shape surrounding the pixel openings AP1, AP2, and AP3. It can also be said that the partition 6 has openings in the subpixels SP1, SP2, and SP3, similar to the rib 5.

[0022] The subpixel SP1 includes a lower electrode LE1, an upper electrode UE1, and an organic layer OR1 that overlap the pixel aperture AP1. The subpixel SP2 includes a lower electrode LE2, an upper electrode UE2, and an organic layer OR2 that overlap the pixel aperture AP2. The subpixel SP3 includes a lower electrode LE3, an upper electrode UE3, and an organic layer OR3 that overlap the pixel aperture AP3.

[0023] The lower electrode LE1, the upper electrode UE1, and the organic layer OR1 overlapping with the pixel aperture AP1 constitute the display element DE1 of the subpixel SP1. The lower electrode LE2, the upper electrode UE2, and the organic layer OR2 overlapping with the pixel aperture AP2 constitute the display element DE2 of the subpixel SP2. The lower electrode LE3, the upper electrode UE3, and the organic layer OR3 overlapping with the pixel aperture AP3 constitute the display element DE3 of the subpixel SP3. The display elements DE1, DE2, and DE3 may further include a cap layer, which will be described later. The ribs 5 and the partition walls 6 surround each of these display elements DE1, DE2, and DE3.

[0024] The lower electrode LE1 is connected to the pixel circuit 1 of the subpixel SP1 (see FIG. 1) through a contact hole CH1. The lower electrode LE2 is connected to the pixel circuit 1 of the subpixel SP2 through a contact hole CH2. The lower electrode LE3 is connected to the pixel circuit 1 of the subpixel SP3 through a contact hole CH3. In the example shown in FIG. 2, the contact holes CH1, CH2, and CH3 entirely overlap with the rib 5 and the partition wall 6, but this is not limiting.

[0025] Fig. 3 is a schematic cross-sectional view of the display device DSP taken along line III-III in Fig. 2. A circuit layer 11 is disposed on the above-mentioned substrate 10. The circuit layer 11 includes various circuits and wiring such as the pixel circuits 1, scanning lines GL, signal lines SL, and power lines PL shown in Fig. 1.

[0026] The circuit layer 11 is covered with an insulating layer 12. The insulating layer 12 functions as a planarizing film that flattens unevenness caused by the circuit layer 11. Although not shown in the cross section of FIG. 3, the above-mentioned contact holes CH1, CH2, and CH3 are provided in the insulating layer 12.

[0027] The lower electrodes LE1, LE2, and LE3 are disposed on the insulating layer 12. The rib 5 is disposed on the insulating layer 12 and the lower electrodes LE1, LE2, and LE3. Ends of the lower electrodes LE1, LE2, and LE3 are covered by the rib 5.

[0028] The partition 6 includes a bottom portion 61 disposed on the rib 5, a shaft portion 62 disposed on the bottom portion 61, and a top portion 63 disposed on the shaft portion 62. The top portion 63 has a width greater than that of the shaft portion 62. As a result, both ends of the top portion 63 protrude beyond the side surfaces of the shaft portion 62 in FIG. 3. Such a shape of the partition 6 is called an overhang shape.

[0029] The organic layer OR1 covers the lower electrode LE1 through the pixel opening AP1. The upper electrode UE1 covers the organic layer OR1 and faces the lower electrode LE1. The organic layer OR2 covers the lower electrode LE2 through the pixel opening AP2. The upper electrode UE2 covers the organic layer OR2 and faces the lower electrode LE2. The organic layer OR3 covers the lower electrode LE3 through the pixel opening AP3. The upper electrode UE3 covers the organic layer OR3 and faces the lower electrode LE3.

[0030] 3, a cap layer CP1 is disposed on the upper electrode UE1, a cap layer CP2 is disposed on the upper electrode UE2, and a cap layer CP3 is disposed on the upper electrode UE3. The cap layers CP1, CP2, and CP3 serve as optical adjustment layers that improve the extraction efficiency of light emitted from the organic layers OR1, OR2, and OR3, respectively.

[0031] In the following description, a laminate including an organic layer OR1, an upper electrode UE1, and a cap layer CP1 is referred to as a thin film FL1, a laminate including an organic layer OR2, an upper electrode UE2, and a cap layer CP2 is referred to as a thin film FL2, and a laminate including an organic layer OR3, an upper electrode UE3, and a cap layer CP3 is referred to as a thin film FL3.

[0032] A part of the thin film FL1 is located on the top portion 63. A part of the thin film FL1 is separated from a part of the thin film FL1 located below the partition wall 6 (a part that constitutes the display element DE1). Similarly, a part of the thin film FL2 is located on the top portion 63, and this part is separated from a part of the thin film FL2 located below the partition wall 6 (a part that constitutes the display element DE2). Furthermore, a part of the thin film FL3 is located on the top portion 63, and this part is separated from a part of the thin film FL3 located below the partition wall 6 (a part that constitutes the display element DE3).

[0033] Sealing layers SE1, SE2, and SE3 are disposed in the subpixels SP1, SP2, and SP3, respectively. The sealing layer SE1 continuously covers the thin film FL1 and the partition wall around the subpixel SP1. The sealing layer SE2 continuously covers the thin film FL2 and the partition wall 6 around the subpixel SP2. The sealing layer SE3 continuously covers the thin film FL3 and the partition wall 6 around the subpixel SP3.

[0034] 3, the thin film FL1 and the sealing layer SE1 on the partition wall 6 between the subpixels SP1 and SP2 are separated from the thin film FL2 and the sealing layer SE2 on the partition wall 6. In addition, the thin film FL1 and the sealing layer SE1 on the partition wall 6 between the subpixels SP1 and SP3 are separated from the thin film FL3 and the sealing layer SE3 on the partition wall 6.

[0035] The sealing layers SE1, SE2, and SE3 are covered with a resin layer 13. The resin layer 13 is covered with a sealing layer 14. The sealing layer 14 is covered with a resin layer 15. The resin layers 13 and 15 and the sealing layer 14 are provided continuously at least throughout the entire display area DA, and a part of them extends into the peripheral area SA.

[0036] A cover member such as a polarizing plate, a touch panel, a protective film, or a cover glass may be further disposed above the resin layer 15. Such a cover member may be adhered to the resin layer 15 via an adhesive layer such as OCA (Optikcal Clear Adhesive).

[0037] The insulating layer 12 is formed of an organic insulating material. The rib 5, the sealing layer 14, SE1, SE2, and SE3 can be formed of an inorganic insulating material such as silicon nitride (SiN), silicon oxide (SiO), silicon oxynitride (SiON), or aluminum oxide (Al2O3). The rib 5, the sealing layer 14, SE1, SE2, and SE3 may have a single-layer structure of any inorganic insulating material, or may have a laminated structure in which layers of two or more types of inorganic insulating materials are stacked. The inorganic insulating materials forming the rib 5, the sealing layer 14, SE1, SE2, and SE3 may be the same or different. In one example, the rib 5 is formed of silicon oxynitride, and the sealing layer 14, SE1, SE2, and SE3 are formed of silicon nitride.

[0038] The resin layers 13 and 15 are made of a resin material (organic insulating material) such as epoxy resin or acrylic resin. The lower electrodes LE1, LE2, and LE3 each have a reflective layer made of silver (Ag), and a pair of conductive oxide layers covering the upper and lower surfaces of the reflective layer. Each conductive oxide layer can be made of a transparent conductive oxide such as ITO (Indium Tin Oxide), IZO (Indium Zinc Oxide), or IGZO (Indium Gallium Zinc Oxide).

[0039] The upper electrodes UE1, UE2, and UE3 are formed of a metal material such as an alloy of magnesium and silver (MgAg), etc. For example, the lower electrodes LE1, LE2, and LE3 correspond to anodes, and the upper electrodes UE1, UE2, and UE3 correspond to cathodes.

[0040] The organic layers OR1, OR2, and OR3 each have a stacked structure of, for example, a hole injection layer, a hole transport layer, an electron blocking layer, a light emitting layer, a hole blocking layer, an electron transport layer, and an electron injection layer. The organic layers OR1, OR2, and OR3 may each have a so-called tandem structure including a plurality of light emitting layers.

[0041] The cap layers CP1, CP2, and CP3 are formed, for example, by a multilayer body of a plurality of transparent thin films. The multilayer body may include a thin film formed of an inorganic material and a thin film formed of an organic material as the plurality of thin films. Moreover, the plurality of thin films have different refractive indices. The material of the thin films constituting the multilayer body is different from the material of the upper electrodes UE1, UE2, and UE3, and also different from the material of the sealing layers SE1, SE2, and SE3. At least one of the cap layers CP1, CP2, and CP3 may be omitted.

[0042] In this embodiment, the bottom portion 61 is formed of, for example, titanium nitride (TiN) or molybdenum-tungsten alloy (MoW). The shaft portion 62 can be formed of, for example, aluminum (Al). The shaft portion 62 may be formed of an aluminum alloy. Examples of the aluminum alloy that can be used include an aluminum-neodymium alloy (AlNd), an aluminum-yttrium alloy (AlY), and an aluminum-silicon alloy (AlSi). The shaft portion 62 may have a single-layer structure of aluminum or an aluminum alloy, or may have a layered structure including multiple layers formed of different materials. The shaft portion 62 may also include a layer formed of an insulating material such as silicon nitride, silicon oxide, and silicon oxynitride.

[0043] The top portion 63 may be made of a conductive material such as titanium, titanium nitride, molybdenum, tungsten, molybdenum-tungsten alloy, molybdenum-niobium alloy, ITO, and IZO. The top portion 63 may have a single layer structure of any of these materials, or a laminate structure including multiple layers made of different materials. The top portion 63 may also include a layer made of an insulating material such as silicon nitride, silicon oxide, and silicon nitride.

[0044] The upper electrodes UE1, UE2, and UE3 are in contact with the bottom portion 61. A common voltage is supplied to the bottom portion 61. This common voltage is supplied to the upper electrodes UE1, UE2, and UE3, respectively. A pixel voltage is supplied to the lower electrodes LE1, LE2, and LE3 through the pixel circuits 1 included in the sub-pixels SP1, SP2, and SP3, respectively.

[0045] The organic layers OR1, OR2, and OR3 emit light in response to the application of a voltage. Specifically, when a potential difference is formed between the lower electrode LE1 and the upper electrode UE1, the light-emitting layer of the organic layer OR1 emits light in the blue wavelength region. When a potential difference is formed between the lower electrode LE2 and the upper electrode UE2, the light-emitting layer of the organic layer OR2 emits light in the green wavelength region. When a potential difference is formed between the lower electrode LE3 and the upper electrode UE3, the light-emitting layer of the organic layer OR3 emits light in the red wavelength region.

[0046] As another example, the light-emitting layers of the organic layers OR1, OR2, and OR3 may emit light of the same color (e.g., white). In this case, the display device DSP may include color filters that convert the light emitted by the light-emitting layers into light of the colors corresponding to the subpixels SP1, SP2, and SP3. The display device DSP may also include a layer including quantum dots that are excited by the light emitted by the light-emitting layers to generate light of the colors corresponding to the subpixels SP1, SP2, and SP3.

[0047] 4 is a schematic cross-sectional view showing an example of a configuration applicable to the partition 6. Here, a portion of the partition 6 located between the subpixels SP1 and SP2 is illustrated. A structure similar to that shown in FIG. 4 can also be applied to a portion of the partition 6 located between the subpixels SP1 and SP3 and a portion located between the subpixels SP2 and SP3.

[0048] 4, the bottom portion 61 and the shaft portion 62 have a single-layer structure. The top portion 63 has a first top layer 631 and a second top layer 632 disposed on the first top layer 631. Materials for the first top layer 631 and the second top layer 632 can be appropriately selected from the materials mentioned above as the material for the top portion 63. The bottom portion 61 and the top portion 63 are formed thinner than the shaft portion 62.

[0049] The bottom portion 61 has a side surface F11 on the subpixel SP1 side and a side surface F12 on the subpixel SP2 side. The stem portion 62 has a side surface F21 on the subpixel SP1 side and a side surface F22 on the subpixel SP2 side.

[0050] In the example shown in Fig. 4, the side faces F11 and F12 are aligned and form a flat surface without any steps. Similarly, the side faces F12 and F22 are aligned and form a flat surface without any steps. From another perspective, Fig. 4 shows an example in which the width of the bottom portion 61 and the width of the shaft portion 62 are equal.

[0051] As another example, the side surface F11 may be slightly recessed from the side surface F21. Also, the side surface F11 may protrude from the side surface F21. Similarly, the side surface F12 may be slightly recessed from the side surface F22. Also, the side surface F12 may protrude from the side surface F22. Also, in FIG. 4, the side surfaces F11, F12, F21, and F22 are parallel to the third direction Z, but this is not limited to the example. For example, the side surfaces F11, F12, F21, and F22 may be inclined so that the width of the bottom portion 61 and the shaft portion 62 narrows as they approach the top portion 63.

[0052] The top portion 63 protrudes from the side surfaces F21 and F22. Specifically, the top portion 63 has an end portion E1 protruding from the side surface F21 and an end portion E2 protruding from the side surface F22.

[0053] The organic layer OR1 is spaced apart from the side surfaces F11 and F21. The upper electrode UE1 is in contact with at least a portion of the side surface F11. In the example shown in Fig. 4, the upper electrode UE1 covers the entire side surface F11 and is also in contact with a portion of the side surface F21. This example is not limited thereto, and the upper electrode UE1 does not have to be in contact with the side surface F21.

[0054] Similarly, the organic layer OR2 is spaced apart from the side surfaces F12 and F22. The upper electrode UE2 is in contact with at least a portion of the side surface F12. In the example shown in Fig. 4, the upper electrode UE2 covers the entire side surface F12 and is also in contact with a portion of the side surface F22. This example is not limited thereto, and the upper electrode UE2 does not necessarily have to be in contact with the side surface F22.

[0055] The sealing layer SE1 covers the thin film FL1, and also covers a portion of the side surface F21 that is not covered by the upper electrode UE1 and the lower surface of the end E1. Similarly, the sealing layer SE2 covers the thin film FL2, and also covers a portion of the side surface F22 that is not covered by the upper electrode UE2 and the lower surface of the end E2.

[0056] 4 is merely an example. The bottom portion 61 and the shaft portion 62 may have a laminated structure of two or more layers. The top portion 63 may have a single layer structure or a laminated structure of three or more layers.

[0057] Next, a manufacturing method of the display device DSP will be described taking as an example the case where the partition 6 has the configuration shown in Fig. 4. As an example, it is assumed here that the rib 5 is made of silicon oxynitride, the bottom portion 61 is made of titanium nitride, the shaft portion 62 is made of aluminum, the first top layer 631 is made of titanium, the second top layer 632 is made of ITO, and the sealing layers SE1, SE2, and SE3 are made of silicon nitride.

[0058] 5 is a flowchart showing an example of a method for manufacturing the display device DSP. In manufacturing the display device DSP, first, a circuit layer 11, an insulating layer 12, and lower electrodes LE1, LE2, and LE3 are formed on a substrate 10 (step PR1). Furthermore, a rib 5 and a partition wall 6 are formed (step PR2).

[0059] 6 to 11 are schematic cross-sectional views showing an example of a step PR2 for forming the ribs 5 and the partition walls 6. In these drawings, the substrate 10, the circuit layer 11, and the insulating layer 12 are omitted.

[0060] 6, in process PR2, an insulating layer 5a to be processed into the rib 5 is formed, a first layer L1 to be processed into the bottom portion 61 is formed on the insulating layer 5a, a second layer L2 to be processed into the shaft portion 62 is formed on the first layer L1, and a third layer L3 to be processed into the top portion 63 is formed on the second layer L2. Furthermore, a resist R1 patterned into the planar shape of the partition wall 6 is formed on the third layer L3. The third layer L3 includes a first top layer 631a and a second top layer 632a covering the first top layer 631a.

[0061] In this embodiment, the insulating layer 5a is made of silicon oxynitride and has a thickness of, for example, 400 nm. The first layer L1 is made of titanium nitride and has a thickness of, for example, 20 nm. The second layer L2 is made of aluminum and has a thickness of, for example, 800 nm. The first top layer 631a is made of titanium and has a thickness of, for example, 100 nm. The second top layer 632a is made of ITO and has a thickness of, for example, 50 nm.

[0062] The insulating layer 5a is formed by, for example, chemical vapor deposition (CVD). The first layer L1, the second layer L2, the first top layer 631a, and the second top layer 632a are formed by, for example, sputtering.

[0063] 7, the portion of the second top layer 632a exposed from the resist R1 is removed by wet etching. Furthermore, the portion of the first top layer 631a exposed from the resist R1 is removed by anisotropic dry etching. By these etching steps, the top portion 63 including the first top layer 631 and the second top layer 632 is formed.

[0064] In the above-mentioned anisotropic dry etching, the thickness of the portion of the second layer L2 exposed from the resist R1 and the top portion 63 is also reduced. This example is not limited to this, and the portion of the second layer L2 exposed from the resist R1 may be entirely removed. In addition, the first top layer 631a and the second layer L2 may be processed by different etching methods as shown in FIG.

[0065] After the step of Fig. 7, the second layer L2 is processed by isotropic wet etching as shown in Fig. 8. In this wet etching, the portion of the second layer L2 whose thickness has been reduced in the step of Fig. 7 is removed. Furthermore, the width of the second layer L2 remaining below the top portion 63 is reduced below the width of the top portion 63. As a result, the shaft portion 62 is formed.

[0066] After the step of Fig. 8, as shown in Fig. 9, the portion of the first layer L1 exposed from the shaft portion 62 is removed by dry etching, thereby forming the bottom portion 61. After the partition wall 6 is formed by the steps of Figs. 6 to 9 above, the resist R1 is removed.

[0067] Next, as shown in Fig. 10, a resist R2 patterned into the planar shape of the rib 5 is disposed. Furthermore, as shown in Fig. 11, the portion of the insulating layer 5a exposed from the resist R2 is removed by dry etching. As a result, the rib 5 having pixel openings AP1, AP2, and AP3 is formed. After this dry etching, the resist R2 is removed.

[0068] 6 to 11, the pixel openings AP1, AP2, and AP3 of the rib 5 are formed after the partition wall 6 is formed, but as another example, the partition wall 6 may be formed after the pixel openings AP1, AP2, and AP3 of the rib 5 are formed. Furthermore, the steps for processing the first layer L1, the second layer L2, the third layer L3, and the rib 5, such as wet etching and dry etching exemplified here, may be appropriately changed depending on the materials from which they are formed.

[0069] Although not shown, for example, in the rib 5 in the peripheral area SA, a contact hole or the like is formed for supplying a common voltage to the bottom portion 61 (that is, connecting the bottom portion 61 to the backplane).

[0070] Incidentally, when the portions of the insulating layer 5a exposed from the resist R2 are removed by dry etching to form the rib 5 as described above, the surfaces of the lower electrodes LE1, LE2, and LE3 overlapping with the pixel openings AP1, AP2, and AP3 are exposed to dry etching, and therefore the surfaces of the lower electrodes LE1, LE2, and LE3 may be damaged.

[0071] Such damage to the surfaces of the lower electrodes LE1, LE2, and LE3 may affect the surface characteristics of the lower electrodes LE1, LE2, and LE3, and may affect the display characteristics of the display device DSP.

[0072] For this reason, in this embodiment, after step PR2, a chemical treatment is performed (step PR3) to reduce the influence of damage to the surfaces of the lower electrodes LE1, LE2, and LE3 on the display characteristics of the display device DSP. The chemical treatment in step PR3 will be described later.

[0073] After the ribs 5 and the partition walls 6 are formed and the chemical treatment is performed as described above, a process for forming the display elements DE1, DE2, and DE3 is performed. In this embodiment, it is assumed that the display element DE1 is formed first, the display element DE2 is formed next, and the display element DE3 is formed last. However, the order in which the display elements DE1, DE2, and DE3 are formed is not limited to this example.

[0074] 12 to 17 are schematic cross-sectional views showing an example of a process for forming display elements DE1, DE2, and DE3. In forming display element DE1, first, as shown in Fig. 12, an organic layer OR1 covering the lower electrode LE1 through the pixel aperture AP1, an upper electrode UE1 covering the organic layer OR1 and in contact with the bottom portion 61, and a cap layer CP1 covering the upper electrode UE1 are formed in this order by vapor deposition, and a sealing layer SE1 continuously covering the cap layer CP1 and the partition wall 6 is formed by CVD (step PR4).

[0075] The thin film FL1 including the organic layer OR1, the upper electrode UE1 and the cap layer CP1 is formed over at least the entire display area DA and is disposed not only on the subpixel SP1 but also on the subpixels SP2 and SP3 and the partition wall 6. The thin film FL1 is divided by the overhanging partition wall 6. The sealing layer SE1 is formed over the entire display area DA and continuously covers the thin film FL1 and the partition wall 6 without being divided by the partition wall 6.

[0076] After step PR4, the thin film FL1 and the sealing layer SE1 are patterned (step PR5). In this patterning, a resist R3 is disposed on the sealing layer SE1 as shown in Fig. 13. The resist R3 is located above the subpixel SP1 and a part of the partition wall 6 around it.

[0077] Thereafter, by etching using the resist R3 as a mask, the thin film FL1 and the sealing layer SE1 are removed in portions exposed from the resist R3 as shown in Fig. 14. For example, this etching includes wet etching or dry etching performed in sequence on the sealing layer SE1, the cap layer CP1, the upper electrode UE1, and the organic layer OR1. Specifically, for example, the sealing layer SE1 is removed by dry etching, the cap layer CP1 (multilayer body) is removed by wet etching and dry etching, the upper electrode UE1 is removed by wet etching, and the organic layer OR1 is removed by dry etching (for example, ashing).

[0078] After the step of Fig. 14, the resist R3 is removed. As a result, a substrate can be obtained in which the display element DE1 and the sealing layer SE1 are formed in the subpixel SP1, and no display element or sealing layer is formed in the subpixels SP2 and SP3, as shown in Fig. 15.

[0079] The display element DE2 is formed in the same manner as the display element DE1. That is, after step PR5, the organic layer OR2 covering the lower electrode LE2 through the pixel opening AP2, the upper electrode UE2 covering the organic layer OR2, and the cap layer CP2 covering the upper electrode UE2 are formed in this order by vapor deposition, and the sealing layer SE2 continuously covering the cap layer CP2 and the partition wall 6 is formed by CVD (step PR6).

[0080] The thin film FL2 including the organic layer OR2, the upper electrode UE2 and the cap layer CP2 is formed over at least the entire display area DA, and is disposed not only on the subpixel SP2 but also on the subpixels SP1 and SP3 and the partition wall 6. The thin film FL2 is divided by the overhanging partition wall 6. The sealing layer SE2 is formed over the entire display area DA, and continuously covers the thin film FL2 and the partition wall 6 without being divided by the partition wall 6.

[0081] After step PR6, the thin film FL2 and the sealing layer SE2 are patterned by wet etching or dry etching (step PR7). The flow of this patterning is similar to that of step PR5.

[0082] After step PR7, as shown in Figure 16, a substrate can be obtained in which a display element DE1 and a sealing layer SE1 are formed in subpixel SP1, a display element DE2 and a sealing layer SE2 are formed in subpixel SP2, and no display element or sealing layer is formed in subpixel SP3.

[0083] The display element DE3 is formed in the same manner as the display elements DE1 and DE2. That is, after step PR7, an organic layer OR3 covering the lower electrode LE3 through the pixel opening AP3, an upper electrode UE3 covering the organic layer OR3, and a cap layer CP3 covering the upper electrode UE3 are formed in this order by vapor deposition, and a sealing layer SE3 continuously covering the cap layer CP3 and the partition wall 6 is formed by CVD (step PR8).

[0084] The thin film FL3 including the organic layer OR3, the upper electrode UE3 and the cap layer CP3 is formed over at least the entire display region DA and is disposed not only on the subpixel SP3 but also on the subpixels SP1 and SP2 and the partition wall 6. The thin film FL3 is divided by the overhanging partition wall 6. The sealing layer SE3 is formed over the entire display region DA and continuously covers the thin film FL3 and the partition wall 6 without being divided by the partition wall 6.

[0085] After step PR8, the thin film FL3 and the sealing layer SE3 are patterned by wet etching or dry etching (step PR9). The patterning process is similar to that of step PR5.

[0086] After step PR9, a substrate can be obtained in which a display element DE1 and a sealing layer SE1 are formed in subpixel SP1, a display element DE2 and a sealing layer SE2 are formed in subpixel SP2, and a display element DE3 and a sealing layer SE3 are formed in subpixel SP3, as shown in Figure 17.

[0087] After the display elements DE1, DE2, and DE3 and the sealing layers SE1, SE2, and SE3 are formed, the resin layer 13, the sealing layer 14, and the resin layer 15 shown in Fig. 3 are successively formed (step PR10), thereby completing the display device DSP.

[0088] Hereinafter, the chemical treatment carried out in the above-mentioned step PR3 shown in Fig. 5 will be described with reference to Fig. 18. Fig. 18 is a schematic cross-sectional view including an end of a pixel opening of the rib 5 formed in the step PR2 shown in Fig. 5.

[0089] Note that the pixel aperture AP shown in Fig. 18 is intended to be any one of the pixel apertures AP1, AP2, and AP3 described above. Similarly, the lower electrode LE shown in Fig. 18 is intended to be any one of the lower electrodes LE1, LE2, and LE3 disposed below the pixel aperture AP.

[0090] In the following description, a portion LEa of the lower electrode LE that is covered by the rib 5 is referred to as a first portion LEa, and a portion LEb of the lower electrode LE that overlaps with the pixel aperture AP1 is referred to as a second portion LEb.

[0091] For convenience of explanation, only the insulating layer 12, the lower electrode LE, and the rib 5 are shown in FIG.

[0092] Here, as shown in FIG. 18, the lower electrode LE has a laminated structure including a first conductive oxide layer LEc arranged on an insulating layer 12, a reflective layer LEd arranged on the first conductive oxide layer LEc, and a second conductive oxide layer LEe arranged on the reflective layer LEd.

[0093] The first conductive oxide layer LEc is made of, for example, ITO, the reflective layer LEd is made of, for example, silver, and the second conductive oxide layer LEe is made of, for example, ITO.

[0094] In this case, the lower electrode LE is formed by sequentially forming, by a sputtering method, a layer made of ITO to be processed into the first conductive oxide layer LEc, a layer made of silver to be processed into the reflective layer LEd, and a layer made of ITO to be processed into the second conductive oxide layer LEe, and then sequentially performing wet etching on these layers on which resist has been formed.

[0095] The second portion LEb of the lower electrode LE thus formed is exposed at the pixel opening AP by dry etching for forming the rib 5 as described above, but as shown in FIG. 18, the surface of the second conductive oxide layer LEe disposed on the side on which the organic layer OR1 is formed is damaged by the dry etching.

[0096] The display device DSP is manufactured by forming an organic layer on the second conductive oxide layer LEe, and if the surface of the second conductive oxide layer LEe is damaged, the display characteristics of the display device DSP may deteriorate. Specifically, damage to the surface of the second conductive oxide layer LEe may affect the injection efficiency of holes in the organic layer covering the second conductive oxide layer LEe, and may reduce the luminous efficiency of the organic layer.

[0097] For this reason, in this embodiment, the chemical treatment is performed after the formation of the rib 5. Note that the chemical treatment in this embodiment is performed using a chemical that acts on the lower electrode LE (the second conductive oxide layer LEe).

[0098] Here, the chemical solution used in the above-mentioned chemical treatment includes, for example, an acidic solution (hereinafter, referred to as an acid solution). One example of the acid solution is a mixed acid obtained by mixing phosphoric acid, nitric acid, and acetic acid. In the chemical treatment using such an acid solution, the acid solution acts on the second conductive oxide layer LEe by contacting the second conductive oxide layer LEe, and the surface layer (i.e., the damaged layer) of the second conductive oxide layer LEe can be removed.

[0099] In other words, the chemical solution treatment in this embodiment corresponds to a treatment for removing a damaged layer of the second portion LEb of the lower electrode LE and exposing an undamaged layer.

[0100] In addition, since the chemical treatment (the chemical used in the chemical treatment) may affect, for example, the partition 6 (the bottom portion 61, the axis portion 62, and the top portion 63), it is preferable that the chemical treatment be performed in a state in which the partition 6 is covered with resist R2, as shown in, for example, FIG. 11.

[0101] However, the chemical treatment may be performed after the resist R2 is removed (peeled off). Specifically, for example, a part of the top portion 63 included in the partition 6 may be removed (shaved off) by the chemical treatment performed after the resist R2 is removed. However, it is considered that the extent (thickness) of the undamaged top portion 63 removed by the chemical treatment is small compared to the damaged second conductive oxide layer LEe. Furthermore, the top portion 63 has a thickness of about 150 nm. That is, when the chemical treatment has a small effect on the top portion 63, a configuration in which the chemical treatment is performed after the resist R2 is removed may be adopted. Furthermore, when the shaft portion 62 provided on the partition 6 is made of aluminum, when the chemical treatment is performed after the resist R2 is removed, for example, oxalic acid, which has a small effect on the aluminum, may be used as the chemical. Furthermore, when a mixed acid of phosphoric acid / nitric acid / acetic acid is used as the chemical, a mixed acid with a lower phosphoric acid ratio may be used.

[0102] Further, although the chemical solution used in the chemical treatment has been mainly described here as an acid solution, the chemical solution may be an alkaline solution (hereinafter, referred to as an alkaline solution). In addition, an amine-based alkaline stripper may be used to remove (peel off) the resist R2 shown in FIG. 11, and the amine-based alkaline stripper may be used as the chemical solution in the chemical treatment. This makes it possible to simultaneously perform the removal of the resist R2 and the chemical treatment (removal of the surface layer of the second conductive oxide layer LEe), which may enable efficient manufacturing of the display device DSP.

[0103] The chemical liquid used in the chemical treatment in this embodiment can be appropriately selected depending on the materials forming the lower electrode LE and other components.

[0104] Here, FIG. 19 is a schematic cross-sectional view including the edge of the pixel aperture AP after the chemical liquid treatment has been carried out.

[0105] When the chemical treatment is performed as described above, the surface layer of the second conductive oxide layer LEe overlapping the second portion LEb of the lower electrode LE is removed as shown in Fig. 19. That is, in the display device DSP manufactured by the manufacturing method according to the present embodiment, the surface of the second conductive oxide layer LEe is scraped off by the chemical treatment, so that the thickness T1 of the first portion LEa of the lower electrode LE is different from the thickness T2 of the second portion LEb of the lower electrode.

[0106] Specifically, a thickness T1 of the first portion LEa of the lower electrode LE is thicker than a thickness T2 of the second portion LEb of the lower electrode LE. In this case, the thicknesses of the first conductive oxide layer LEc and the reflective layer LEd (i.e., layers other than the second conductive oxide layer LEe) are the same in the first portion LEa of the lower electrode LE and the second portion LEb of the lower electrode LE, but the thickness of the second conductive oxide layer LEe overlapping the first portion LEa of the lower electrode LE is thicker than the thickness of the second conductive oxide layer LEe overlapping the second portion LEb of the lower electrode LE.

[0107] In this embodiment, the thickness of the surface layer of the second portion LEb (second conductive oxide layer LEe) of the lower electrode LE removed by the chemical solution treatment is assumed to be, for example, about 3 to 5 nm. That is, in the above-described step PR1 shown in Fig. 5, it is preferable to form the lower electrode LE (second conductive oxide layer LEe) having a thickness taking into consideration the removal of the surface layer by the chemical solution treatment.

[0108] Here, in FIG. 19, the thickness T1 of the first portion LEa of the lower electrode LE is constant, and the thickness T2 of the second portion LEb of the lower electrode LE is constant, that is, the end 51 of the rib 5 (pixel opening AP) and the end LEf of the recess formed in the lower electrode LE (second conductive oxide layer LEe) by the chemical solution treatment are aligned in a plan view. However, the display device DSP according to this embodiment may be configured such that the thickness of the portion of the second portion LEb of the lower electrode LE close to the rib 5 (end of the pixel opening AP) is thicker than the thickness of the portion of the second portion LEb of the lower electrode LE away from the rib 5, as shown in FIG. 20, for example. In other words, the recess formed in the lower electrode LE in this embodiment may have an inclined surface LEg. In this case, the display device DSP is configured such that the width W of the thinnest portion of the second portion LEb of the lower electrode LE is shorter than the width of the pixel opening AP1.

[0109] In this embodiment, an organic layer is formed on the lower electrode LE, but the lower electrode LE (second conductive oxide layer LEe) in this embodiment is formed in a shape such that at least the organic layer does not extend below the rib 5 in a plan view. In this case, for example, the thickness of the first portion LEa of the lower electrode LE may be constant, or the end of the rib 5 forming the pixel aperture AP may be in contact with the lower electrode LE (second conductive oxide layer LEe).

[0110] As described above, in this embodiment, the display device DSP is manufactured by forming the lower electrode LE (LE1, LE2, and LE3), forming the rib 5 having the pixel opening AP (AP1, AP2, and AP3) that covers the first portion LEa of the lower electrode LE and overlaps with the LE second portion LEb of the lower electrode LE, and removing the surface layer of the second portion LEb of the lower electrode LE (the second conductive oxide layer LEe) using a chemical solution that acts on the second portion LEb of the lower electrode LE. Note that the display device DSP manufactured as described above has a structure in which the thickness T1 of the first portion LEa of the lower electrode LE is different from the thickness T2 of the second portion LEb of the lower electrode LE.

[0111] As a result, in this embodiment, the influence of damage to the lower electrode LE (second conductive oxide layer LEe) caused by dry etching for forming the rib 5 can be mitigated, and deterioration of the display characteristics (reduction in the luminous efficiency in the organic layers OR1, OR2, and OR3) in the display device DSP can be suppressed.

[0112] The chemical treatment in this embodiment can be performed using an acid solution or an alkaline solution as the chemical solution. The chemical treatment in this embodiment may be performed before the resist R2 covering the partition wall 6 is removed to form the rib 5, or may be performed after the resist R2 is removed.

[0113] Furthermore, in this embodiment, when an amine-based alkaline stripping solution is used as the chemical solution, removal (stripping) of the resist R2 and chemical solution treatment (removal of the surface layer of the lower electrode LE) may be performed simultaneously.

[0114] As described above, in this embodiment, several manufacturing methods of the display device DSP have been described, but these manufacturing methods of the display device DSP may be combined. Specifically, for example, after removing the resist R2 and carrying out a chemical treatment using an amine-based alkaline stripping solution, a further chemical treatment may be carried out using an acid solution. With this configuration, it is possible to improve the reliability of suppressing the deterioration of the display characteristics of the display device DSP.

[0115] 5, in consideration of damage to the surfaces of the lower electrodes LE (LE1, LE2, and LE3) caused by dry etching for forming the rib 5, the chemical treatment is performed, but, for example, the etching performed in the patterning in step PR5 may damage the surfaces of the lower electrodes LE2 and LE3 that overlap with the pixel openings AP2 and AP3. Furthermore, the etching performed in the patterning in step PR7 shown in FIG. 5 may damage the surface of the lower electrode LE3 that overlaps with the pixel opening AP3.

[0116] Therefore, in this embodiment, for example, a manufacturing method of the display device DSP shown in Fig. 21 may be applied. Although detailed description is omitted, steps PR101 to PR105, PR107, PR108, and PR110 to PR112 shown in Fig. 21 correspond to steps PR1 to PR10 shown in Fig. 5. That is, Fig. 21 shows a manufacturing method of the display device DSP in which a chemical liquid treatment is further performed in step PR106 after step PR105 which corresponds to step PR5 shown in Fig. 5, and a chemical liquid treatment is further performed in step PR109 after step PR108 which corresponds to step PR7 shown in Fig. 5.

[0117] In addition, the chemical treatments performed multiple times in the manufacturing process of the display device DSP may be the same treatment or different treatments. Specifically, for example, a chemical treatment using a mixed acid of phosphoric acid, nitric acid, and acetic acid may be performed in step PR103 shown in Fig. 21, and a chemical treatment using an amine-based alkaline stripping solution may be performed in steps PR106 and PR109. Furthermore, the chemical treatment may be performed before the resist R2 is removed in step PR103, and the chemical treatment may be performed after the resist R3 is removed in steps PR106 and PR109.

[0118] In addition, in FIG. 21, the chemical treatment is performed multiple times, but some of the chemical treatments may be omitted.

[0119] In addition, in this embodiment, it is sufficient that the surface layer of the lower electrode LE (second conductive oxide layer LEe) is removed by chemical treatment in order to suppress deterioration of the display characteristics of the display device DSP, and at least a part of the manufacturing method of the display device DSP described in this embodiment may be modified.

[0120] All display devices and display device manufacturing methods that can be implemented by a person skilled in the art through appropriate design modifications based on the display device and display device manufacturing method described above as embodiments of the present invention fall within the scope of the present invention as long as they include the gist of the present invention.

[0121] Within the scope of the concept of the present invention, a person skilled in the art may conceive of various modifications, and such modifications are also understood to fall within the scope of the present invention. For example, those in which a person skilled in the art appropriately adds or removes components or modifies the design of the above-mentioned embodiment, or adds or omits steps or modifies conditions, are also included in the scope of the present invention as long as they include the gist of the present invention.

[0122] Furthermore, with regard to other effects and advantages brought about by the aspects described in the above-mentioned embodiments, those which are obvious from the description in this specification or which can be appropriately thought up by a person skilled in the art are naturally understood to be brought about by the present invention. [Explanation of symbols]

[0123] DSP...display device, DA...display area, SA...peripheral area, PX...pixel, SP1, SP2, SP3...sub-pixel, AP, AP1, AP2, AP3...pixel aperture, LE, LE1, LE2, LE3...lower electrode, LEa...first portion, LEb...second portion, LEc...first conductive oxide layer, LEd...reflective layer, LEe...second conductive oxide layer, OR1, OR2, OR3...organic layer, UE1, UE2, UE3...upper electrode, CP1, CP2, CP3...cap layer, SE1, SE2, SE3...sealing layer, 5...rib, 6...partition, 61...bottom portion, 62...axis portion, 63...top portion.

Claims

1. A lower electrode; a rib covering a first portion of the lower electrode and having a pixel opening overlapping a second portion of the lower electrode; a partition wall including a bottom portion disposed on the rib, a shaft portion disposed on the bottom portion, and a top portion disposed on the shaft portion and protruding from a side surface of the shaft portion; an organic layer covering the lower electrode through the pixel opening; an upper electrode covering the organic layer and in contact with the bottom portion; Equipped with The thickness of the first portion of the lower electrode is different from the thickness of the second portion of the lower electrode. Display device.

2. 2. The display device according to claim 1, wherein the thickness of the first portion of the lower electrode is greater than the thickness of the second portion of the lower electrode.

3. the lower electrode has a laminated structure in which a conductive oxide layer is disposed on the organic layer side, a thickness of the conductive oxide layer in a first portion of the lower electrode is greater than a thickness of the conductive oxide layer in a second portion of the lower electrode; The thickness of the layer other than the conductive oxide layer in the first portion of the lower electrode is the same as the thickness of the layer other than the conductive oxide layer in the second portion of the lower electrode. The display device according to claim 2.

4. 3. The display device according to claim 2, wherein the thickness of the second portion of the lower electrode is constant.

5. 3. The display device according to claim 2, wherein a thickness of the second portion of the lower electrode near the rib is greater than a thickness of a portion of the second portion of the lower electrode away from the rib.

6. 6. The display device according to claim 5, wherein the width of the thinnest part of the second portion of the lower electrode is shorter than the width of the pixel aperture.

7. 3. The display device according to claim 2, wherein the thickness of the first portion of the lower electrode is constant.

8. 3. The display device according to claim 2, wherein an end of the rib that forms the pixel opening is in contact with the lower electrode.

9. The display device according to any one of claims 1 to 8, further comprising a cap layer covering the upper electrode.

10. The display device according to claim 9 , further comprising a sealing layer continuously covering the cap layer and the partition wall.

11. Forming a lower electrode; forming a rib covering a first portion of the lower electrode and having a pixel opening overlapping a second portion of the lower electrode; A surface layer of the second portion of the lower electrode is removed using a chemical solution that acts on the lower electrode. A method for manufacturing a display device.

12. The method for manufacturing a display device according to claim 11, wherein the chemical solution is an acidic solution.

13. The method for manufacturing a display device according to claim 11, wherein the chemical solution is an alkaline solution.

14. The method for manufacturing a display device according to any one of claims 11 to 13, further comprising forming a partition wall on the rib, the partition wall including a bottom portion, an axis portion located on the bottom portion, and a top portion located on the axis portion.

15. forming an organic layer covering the lower electrode through the pixel opening; forming an upper electrode covering the organic layer and in contact with the bottom portion; The method for manufacturing the display device according to claim 14.

16. The method for manufacturing a display device according to claim 15 , further comprising forming a cap layer to cover the upper electrode.

17. The method for manufacturing a display device according to claim 16 , further comprising forming a sealing layer that continuously covers the cap layer and the partition wall.

Citation Information

Patent Citations

  • Organic el display device and its manufacture

    JP2000195677A

  • Display device and manufacturing method of the same

    JP2004207217A

  • Organic el display device, and manufacturing method therefor

    JP2008135325A

  • Organic electroluminescent display device and its manufacturing method

    JP2009032673A

  • Organic electroluminescent display device and its manufacturing method

    JP2010118191A