Wafer processing method

The thermocompression bonding of a flexible sheet to wafers with annular convex and circular concave portions addresses the gap-related issues in existing methods, ensuring a larger effective area and improved productivity in chip production.

JP2024162645APending Publication Date: 2024-11-21DISCO CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023078368
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-11
Publication Date
2024-11-21

AI Technical Summary

Technical Problem

The existing methods for processing wafers with annular convex and circular concave portions face issues such as chipping or cracking due to gaps created by adhesive tapes, leading to reduced effective wafer area and decreased productivity.

Method used

A thermocompression bonding method using a flexible sheet without adhesive, which is thermally bonded to the wafer, allowing it to conform to the convex and concave portions without sticking, thereby minimizing gaps and enabling precise dividing groove formation.

Benefits of technology

This method secures a larger effective wafer area for device formation, enhances productivity by reducing stress-induced gaps, and maintains the sheet's adherence over time, facilitating efficient chip production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024162645000001_ABST
    Figure 2024162645000001_ABST
Patent Text Reader

Abstract

To provide a sheet replacing adhesive tape that can be placed on one side (back side) of a wafer having a circular concave portion without creating a large gap, and can suppress the expansion of the gap over time.SOLUTION: Provided is a processing method in which a wafer having one surface with an annular convex portion on its outer periphery and a circular concave portion formed in an area surrounded by the annular convex portion is processed using a thermocompression device including an upper chamber with a first concave portion, a lower chamber with a second concave portion, and a holding table disposed in the second concave portion and holding the wafer, and the wafer with one surface facing upward is held from below by the holding table, a sheet is sandwiched between the first and second concave portions, the first and second concave portions are closed, the first and second concave portions are depressurized, the second concave portion is depressurized, the pressure in the first concave portion is increased, the sheet is brought into contact with the one surface of the wafer to bring the sheet into contact with the annular convex portion and the circular concave portion, and the sheet is heated to thermocompress the sheet to one surface of the wafer.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for processing a wafer having a surface with an annular protrusion on its outer periphery and a circular recess formed in an area surrounded by the annular protrusion. [Background technology]

[0002] Device chips are mounted on electronic devices such as mobile phones and personal computers. Device chips are usually manufactured by thinning a wafer, which has multiple devices such as ICs (Integrated Circuits) formed on its front side, by grinding it from its back side, and then dividing the wafer into individual devices.

[0003] The grinded and thinned wafer has a reduced rigidity and is prone to cracking. Therefore, a circular recess is formed by grinding an area of ​​the back surface of the wafer corresponding to a device formation area where multiple devices are formed, and the surrounding area is left as an annular protrusion. This annular protrusion functions to reinforce the thinned circular recess while the wafer is being transported (see, for example, Patent Document 1).

[0004] On the other hand, when dividing the wafer into individual chips, the annular convex portion becomes an obstacle to division, and therefore it is necessary to remove the annular convex portion from the wafer in advance. When removing the annular convex portion, an adhesive tape is applied to the entire back surface of the wafer, including the circular concave portion and the annular convex portion, and the wafer is held by a holding table via the adhesive tape. The holding table has a convex shape corresponding to the circular concave portion of the wafer, and the circular concave portion is aligned with this convex shape. Then, an annular dividing groove is formed in the wafer held by the holding table, and the annular convex portion is removed (see, for example, Patent Document 2). [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2007-173487 A [Patent Document 2] JP 2011-61137 A Summary of the Invention [Problem to be solved by the invention]

[0006] When the adhesive tape is applied to one surface (rear surface) of the wafer, a gap is generated between the adhesive tape and the wafer at the outer periphery of the circular recess due to the step between the circular recess and the annular protrusion. Since the wafer is not supported by the adhesive tape in the area overlapping with this gap, processing this area to form a dividing groove causes unacceptable chipping or cracks in the wafer.

[0007] For this reason, it is necessary to form the dividing trenches in regions that do not overlap with the gaps. However, since devices cannot be formed on the wafer at the positions where the dividing trenches are formed, forming the dividing trenches while avoiding the large gaps reduces the effective area of ​​the wafer, resulting in a problem of reduced productivity of device chips.

[0008] In addition, when the adhesive tape is applied to one surface (rear surface) of the wafer, the adhesive tape is first applied to the annular convex portion, and then the adhesive tape is stretched inside the annular convex portion, and the adhesive tape is applied to the circular concave portion under a large stress. As a result, there is a problem that the gap between the adhesive tape and the wafer widens from the outer periphery of the circular concave portion as time passes after the adhesive tape is applied to the wafer.

[0009] The present invention has been made in consideration of these problems, and aims to provide a wafer processing method that can arrange a sheet in place of adhesive tape without creating a large gap on one side (back side) of a wafer having a circular recess, and that can suppress the expansion of the gap over time. [Means for solving the problem]

[0010] According to one aspect of the present invention, a method for processing a wafer having one surface with an annular convex portion on the outer periphery and a circular concave portion formed in an area surrounded by the annular convex portion, in a thermocompression bonding apparatus comprising an upper chamber connected to a first decompression unit and having a first concave portion with a first opening, a lower chamber connected to a second decompression unit and having a second concave portion with a second opening, and a holding table disposed in the second concave portion and holding the wafer, the upper chamber and the lower chamber being closed by aligning the first opening and the second opening, the method comprising the steps of: holding the wafer with the one surface facing upward from below with the holding table of the thermocompression bonding apparatus; an annular frame having an opening in the center capable of accommodating the wafer; a sealing step of sandwiching the sheet of a frame unit having a frame member and a sheet fixed to a peripheral portion between the first opening of the first recess and the second opening of the second recess inside the opening, to close the first recess and the second recess; a depressurizing step of depressurizing the first recess with the first depressurizing unit and depressurizing the second recess with the second depressurizing unit after the sealing step; a contacting step of increasing the pressure in the first recess and bringing the sheet into contact with the one surface of the wafer, thereby bringing the sheet into contact with the annular convex portion and the circular concave portion; and a thermocompression step of heating the sheet to thermocompression bond the sheet to the one surface of the wafer after the contacting step.

[0011] Preferably, the method further includes a dividing groove forming step of forming a dividing groove in the wafer to cut out the annular convex portion after the thermocompression bonding step, and a removing step of removing the annular convex portion from the sheet after the dividing groove forming step. Effect of the Invention

[0012] In a wafer processing method according to one aspect of the present invention, a sheet is brought into contact with the annular convex portion and the circular concave portion of the wafer, and the sheet is heated to thermocompression bond the sheet to the wafer. Even when the sheet comes into contact with the annular convex portion of the wafer, it does not stick to the annular convex portion. Therefore, the sheet is drawn into the circular concave portion from outside the annular convex portion until the sheet subsequently comes into contact with the circular concave portion. In this case, the stress applied to the sheet is dispersed, and the sheet comes into contact with the circular concave portion without being subjected to a large localized stress. The sheet is then thermocompression bonded to the wafer.

[0013] This allows the sheet to be fixed to the wafer with an extremely small gap between the wafer and the sheet, and therefore, compared to when adhesive tape is fixed to the wafer, there is no need to significantly reduce the device formation area to take this gap into account. In other words, the effective area of ​​the wafer can be secured relatively large, improving the productivity of device chips. In addition, because the sheet thermocompression-bonded to the wafer is not subject to large stress, the expansion of the gap between the sheet and the wafer over time is also extremely limited.

[0014] Therefore, one aspect of the present invention provides a wafer processing method that can arrange a sheet in place of adhesive tape on one side (back side) of a wafer having a circular recess without creating a large gap, and that can suppress the expansion of the gap over time. [Brief description of the drawings]

[0015] [Figure 1] FIG. 1(A) is a perspective view that typically shows the back surface (one surface) side of a wafer, and FIG. 1(B) is a perspective view that typically shows the front surface side of the wafer. [Diagram 2] FIG. 2(A) is a cross-sectional view that typically shows a thermocompression bonding apparatus, and FIG. 2(B) is a cross-sectional view that typically shows the thermocompression bonding apparatus in a holding step. [Diagram 3] FIG. 3(A) is a cross-sectional view that typically shows the thermocompression bonding apparatus in a sealing step, and FIG. 3(B) is a cross-sectional view that typically shows the thermocompression bonding apparatus in a depressurizing step. [Figure 4]FIG. 4 is a cross-sectional view showing a schematic diagram of a thermocompression bonding apparatus in a contacting step. [Diagram 5] FIG. 5(A) is a cross-sectional view showing a schematic diagram of a sheet contacting an annular convex portion of a wafer, and FIG. 5(B) is a cross-sectional view showing a schematic diagram of a sheet contacting a circular concave portion of a wafer. [Figure 6] Figure 6(A) is a cross-sectional view that shows a schematic of an adhesive tape contacting an annular convex portion of a wafer, and Figure 6(B) is a cross-sectional view that shows a schematic of a protective sheet contacting a circular concave portion of a wafer. [Figure 7] FIG. 7(A) is a cross-sectional view showing a schematic state in which the sheet is integrated with the wafer and the annular frame, and FIG. 7(B) is a cross-sectional view showing a schematic state in which the annular convex portion is separated from the wafer in the removal step. [Figure 8] 10 is a cross-sectional view showing a schematic diagram of a cutting device in a dividing groove forming step. FIG. [Figure 9] 1 is a flowchart showing the flow of each step of a wafer processing method. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0016] An embodiment according to one aspect of the present invention will be described with reference to the accompanying drawings. Fig. 1(A) is a perspective view showing the back surface (one surface) of a wafer, and Fig. 1(B) is a perspective view showing the front surface of the wafer. First, a wafer to be processed by the wafer processing method according to this embodiment will be described.

[0017] The wafer 11 is a disk-shaped single crystal substrate made of a semiconductor material such as silicon (Si) or silicon carbide (SiC). However, there is no limitation on the shape, structure, size, etc. of the wafer 11. As shown in Fig. 1(B) , a plurality of planned division lines 19 are set in a lattice pattern on the front surface 11a side of the wafer 11. Devices 21 such as ICs and LSIs are formed in each of the areas partitioned by the plurality of planned division lines 19.

[0018] An outer peripheral region surrounding the region on the front surface 11a of the wafer 11 in which the multiple devices 21 are formed is called an outer peripheral surplus region 23. In addition, an outer peripheral surplus region 23 on the front surface 11a of the wafer 11 in which the multiple devices 21 are formed is called a device formation region 25.

[0019] When the wafer 11 on which a plurality of devices 21 are formed is ground from the back surface 11b side to be thinned, and the wafer 11 is divided along the intended division lines 19, a plurality of thin device chips each having a device 21 are obtained. The wafer 11 is divided, for example, by a cutting device equipped with an annular cutting blade. However, the wafer 11 which has been ground and thinned has a reduced rigidity and is easily broken, and is difficult to handle, such as transport.

[0020] 1(A), a region of the back surface 11b of the wafer 11 corresponding to a device formation region 25 in which a plurality of devices 21 are formed is ground to form a circular recess 15, and its periphery is left as an annular protrusion 13. This annular protrusion 13 functions to reinforce the thinned circular recess 15 while the wafer 11 is being transported, etc. This maintains the rigidity of the wafer 11, making it less susceptible to warping or cracking, and facilitating handling.

[0021] However, when attempting to divide the wafer 11 having the annular protrusion 13 on the back surface 11b side by a cutting device along the intended division lines 19, the division grooves formed in the wafer 11 to divide the thin circular recesses 15 cannot cut the thick annular protrusion 13. In other words, the annular protrusion 13 becomes an obstacle to division when dividing the wafer 11 into individual chips.

[0022] Therefore, it is necessary to remove the annular convex portion 13 from the wafer 11 before dividing the wafer 11. In the wafer processing method according to this embodiment, a sheet is thermocompression-bonded to the entire area of ​​one surface (rear surface 11b) of the wafer 11, including the circular concave portion 15 and the annular convex portion 13. The wafer 11 is held by a holding table of the dividing device via the sheet.

[0023] Next, the sheet to be thermocompression bonded to the wafer 11 will be described. FIG. 3(A) and other figures include a cross-sectional view showing a schematic diagram of the sheet 27. The sheet 27 has a diameter larger than the outer diameter of the wafer 11 and does not have a glue layer. The sheet 27 is a thermoplastic sheet. The outer periphery of the sheet 27 is disposed on a metal annular frame 39 (see FIGS. 7(A), 7(B), and 8). The sheet 27 is a flexible resin-based sheet such as a polyolefin-based sheet or a polyester-based sheet, but the material of the sheet 27 is not limited thereto.

[0024] Here, the polyolefin sheet is a sheet of a polymer synthesized using an alkene as a monomer. The polyolefin sheet used for the sheet 27 is, for example, a polyethylene sheet, a polypropylene sheet, or a polystyrene sheet, which is transparent or semi-transparent to visible light.

[0025] The polyester-based sheet is a polymer sheet 27 synthesized using dicarboxylic acid (a compound having two carboxyl groups) and diol (a compound having two hydroxyl groups) as monomers. The polyester-based sheet used for the sheet 27 is, for example, a polyethylene terephthalate sheet or a polyethylene naphthalate sheet 27 that is transparent or semi-transparent to visible light.

[0026] Since sheet 27 does not have a glue layer (adhesive layer) and does not have sufficient adhesiveness, it cannot be attached to wafer 11. Sheet 27 has thermoplastic properties, and when it is heated to a temperature near its melting point while being joined to wafer 11 under application of a predetermined pressure, it partially melts and can be fixed to wafer 11. In other words, sheet 27 can be thermocompression bonded to wafer 11.

[0027] 7(A), 7(B), and 8, the outer periphery of the sheet 27 is preliminarily disposed on a metal annular frame 39. The annular frame 39 has an opening (through hole) 39a having a diameter larger than that of the wafer 11. For example, the sheet 27 is preliminarily thermocompression bonded to the annular frame 39. Alternatively, the sheet 27 is preliminarily attached to the annular frame 39 with an adhesive or the like.

[0028] Finally, when the wafer 11, sheet 27, and annular frame 39 are integrated, a frame unit 41 (see Figures 7(A), 7(B), etc.) is formed. When the frame unit 41 is formed, the wafer 11 can be handled via the sheet 27, making it easy to handle the wafer 11. Furthermore, when the wafer 11 that is part of the frame unit 41 is divided, each formed device chip continues to be supported by the sheet 27, making it easy to handle the device chip.

[0029] Next, a description will be given of a thermocompression bonding apparatus 2 that thermocompresses the sheet 27 to the wafer 11 in the wafer processing method according to this embodiment. 2(A) to 4 each include a cross-sectional view that typically shows the thermocompression bonding apparatus 2.

[0030] 2(A) is a cross-sectional view showing a schematic example of a thermocompression bonding apparatus 2. The thermocompression bonding apparatus 2 is, for example, a chamber-like unit having a space capable of accommodating a wafer 11 therein, and has a function of thermocompression bonding a sheet 27 to the rear surface 11b of the wafer 11. The thermocompression bonding apparatus 2 has a concave lower chamber 6 that opens upward, and a concave upper chamber 4 that is disposed above the lower chamber 6 and opens downward.

[0031] The upper chamber 4 of the thermocompression bonding apparatus 2 includes a first recess 8 connected to a first decompression unit 20 and having a first opening 12. The lower chamber 6 includes a second recess 10 connected to a second decompression unit 22 and having a second opening 14. The first decompression unit 20 and the second decompression unit 22 are, for example, vacuum pumps such as rotary pumps. However, the first decompression unit 20 and the second decompression unit are not limited thereto.

[0032] The thermocompression bonding apparatus 2 also includes a holding table 32 that is disposed in the second recess 10 and holds the wafer 11. The upper chamber 4 and the lower chamber 6 can be closed by aligning the first opening 12 of the upper chamber 4 and the second opening 14 of the lower chamber 6.

[0033] The thermocompression bonding apparatus 2 will be described in more detail. The first opening 12 of the upper chamber 4 and the second opening 14 of the lower chamber 6 have an inner diameter larger than the diameter of the wafer 11. In addition, the first recess 8 of the upper chamber 4 and the second recess 10 of the lower chamber 6 have an outer diameter smaller than the inner diameter of the annular frame 39 disposed on the outer periphery of the sheet 27.

[0034] For example, the upper chamber 4 can be raised and lowered. The second opening 14 of the lower chamber 6 and the first opening 12 of the upper chamber 4 have the same shape, and when the upper chamber 4 is lowered into the lower chamber 6 so that the first opening 12 overlaps with the second opening 14, a space that is isolated from the outside can be formed inside the upper chamber 4 and the lower chamber 6.

[0035] The lower chamber 6 is provided with a table-shaped holding table 32 that supports the wafer 11. The upper surface of the holding table 32 is a flat holding surface 34 that supports and holds the wafer 11. The holding table 32 may be provided with a suction path (not shown) that communicates with the holding surface 34, and a suction source (not shown) connected to the suction path. In this case, when a suction force generated by the suction source is applied to the wafer 11 placed on the holding surface 34 of the holding table 32 through the suction path, the wafer 11 can be suction-held by the holding table 32.

[0036] The height of the holding table 32 is adjusted so that when the wafer 11 is placed on the holding surface 34, the back surface 11b of the wafer 11 and the second opening 14 of the lower chamber 6 are at approximately the same height. Alternatively, the height of the holding table 32 is adjusted so that the second opening 14 of the lower chamber 6 is higher than the back surface 11b of the wafer 11.

[0037] An exhaust unit 24 is connected to the ceiling or side wall of the upper chamber 4. The exhaust unit 24 is an exhaust path having one end connected to the first recess 8 of the upper chamber 4 and the other end connected to the first decompression unit 20. A first solenoid valve 28 (e.g., a solenoid valve) that switches the connection state of the upper chamber 4 and the first decompression unit 20 is provided in the exhaust path of the exhaust unit 24. That is, when the first solenoid valve 28 is operated, the upper chamber 4 and the first decompression unit 20 can be switched between a connected state in which they are connected and a disconnected state in which they are disconnected from each other.

[0038] An exhaust unit 26 is connected to the bottom wall or side wall of the lower chamber 6. The exhaust unit 26 is an exhaust path having one end connected to the second recess 10 of the lower chamber 6 and the other end connected to the second decompression unit 22. A second solenoid valve 30 (e.g., a solenoid valve) that switches the connection state of the lower chamber 6 and the second decompression unit 22 is provided in the exhaust path of the exhaust unit 26. That is, when the second solenoid valve 30 is operated, the lower chamber 6 and the second decompression unit 22 can be switched between a connected state in which they are connected and a disconnected state in which they are disconnected from each other.

[0039] When the first solenoid valve 28 is operated to connect the first decompression unit 20 and the upper chamber 4, the internal space 16 of the upper chamber 4 can be decompressed. When the second solenoid valve 30 is operated to connect the second decompression unit 22 and the lower chamber 6, the internal space 18 of the lower chamber 6 can be decompressed.

[0040] The thermocompression bonding apparatus 2 includes a heating unit that heats the wafer 11 placed on the holding table 32 and the sheet 27 placed on the wafer 11. For example, a heater 36 that can function as a heating unit is disposed inside the holding table 32. The heater 36 is, for example, an electric heating wire. When the heater 36 is operated, the wafer 11 is heated and the sheet 27 is heated through the wafer 11.

[0041] However, the heating unit provided in the thermocompression bonding apparatus 2 is not limited to this. For example, a heating unit (not shown) that supplies hot air to the internal space 16 of the upper chamber 4 may be provided in the first recess 8 of the upper chamber 4. The heating unit includes, for example, a blower that generates an air flow and a heater that can heat the air. The sheet 27 can be heated by placing the wafer 11 on the holding table 32, disposing the sheet 27 on the wafer 11, and supplying hot air to the sheet 27 from the heating unit.

[0042] Next, a wafer processing method according to this embodiment, which is carried out using the thermocompression bonding apparatus 2, will be described. The wafer processing method according to this embodiment is carried out, for example, as part of a device chip manufacturing method in which the wafer 11 is divided to form device chips. FIG. 9 is a flowchart showing the flow of each step of the wafer processing method (device chip manufacturing method). The wafer processing method according to this embodiment will be described below, but the following description also describes each step of the device chip manufacturing method.

[0043] In the wafer processing method according to this embodiment, first, a holding step S10 is performed in which the wafer 11 with one surface (rear surface 11b) facing upward is held from below by the holding table 32 of the thermocompression bonding apparatus 2. Fig. 2(B) is a cross-sectional view that typically shows the thermocompression bonding apparatus 2 and the wafer 11 in the holding step S10.

[0044] In the holding step S10, the wafer 11 is moved above the holding table 32 with the front surface 11a of the wafer 11 facing downward, so that the front surface 11a of the wafer 11 faces the holding surface 34 of the holding table 32. The wafer 11 is then placed on the holding surface 34 of the holding table 32, and the suction source of the holding table 32 is operated to suction-hold the wafer 11 on the holding table 32. At this time, one surface (back surface 11b) to which the sheet 27 is thermocompression-bonded is exposed upward.

[0045] Next, a sealing step S20 is performed in which the sheet 27 fixed to the annular frame 39 is sandwiched between the upper chamber 4 and the lower chamber 6 of the thermocompression bonding apparatus 2 to seal the internal space 16 of the upper chamber 4 and the internal space 18 of the lower chamber 6. Fig. 3(A) is a cross-sectional view that shows a schematic view of the thermocompression bonding apparatus 2 in the sealing step S20.

[0046] In the sealing step S20, a frame unit 41 (see FIG. 7(A) etc.) having an annular frame 39 (see FIG. 7(A) etc.) with an opening 39a in the center capable of accommodating a wafer 11, and a sheet 27 fixed to the outer periphery of the annular frame 39 is placed on the lower chamber 6. At this time, the second opening 14 of the lower chamber 6 is blocked by the sheet 27. The position of the annular frame 39 is adjusted so that the annular frame 39 does not overlap with the first opening 12 and the second opening 14.

[0047] Then, the upper chamber 4 is lowered, and the sheet 27 of the frame unit 41 is sandwiched between the first opening 12 of the first recess 8 and the second opening 14 of the second recess 10 inside the opening 39a of the annular frame 39, closing the first recess 8 and the second recess 10. At this time, the internal space 16 of the upper chamber 4 is sealed by the sheet 27 and the first recess 8. In addition, the internal space 18 of the lower chamber 6 is sealed by the sheet 27 and the second recess 10.

[0048] In the wafer processing method according to this embodiment, after the sealing step S20, a depressurization step S30 is performed in which the first recess 8 is depressurized by the first depressurization unit 20 and the second recess 10 is depressurized by the second depressurization unit 22. Fig. 3(B) is a cross-sectional view that typically shows the thermocompression bonding apparatus 2 in the depressurization step S30.

[0049] In the depressurization step S30, the first solenoid valve 28 is operated to connect the first depressurization unit 20 and the upper chamber 4. Then, the first depressurization unit 20 evacuates the internal space 16 of the first recess 8 of the upper chamber 4 through the exhaust part 24, and the internal space 16 is depressurized. Also, in the depressurization step S30, the second solenoid valve 30 is operated to connect the second depressurization unit 22 and the lower chamber 6. Then, the second depressurization unit 22 evacuates the internal space 18 of the second recess 10 of the lower chamber 6 through the exhaust part 26, and the internal space 18 is depressurized.

[0050] In the wafer processing method according to this embodiment, after the depressurization step S30, a contact step S40 is performed in which the pressure in the first recessed portion 8 is increased and the sheet 27 is brought into contact with one surface (rear surface 11b) of the wafer 11, thereby bringing the sheet 27 into contact with the annular protrusion 13 and the circular recessed portion 15. Fig. 4 is a cross-sectional view that shows a schematic view of the thermocompression bonding apparatus 2 in the contact step S40.

[0051] In the contact step S40, first, the decompression of the upper chamber 4 by the first decompression unit 20 is stopped. That is, the first solenoid valve 28 is operated to disconnect the first decompression unit 20 from the upper chamber 4. At this time, the second solenoid valve 30 is not operated, and the connection between the second decompression unit 22 and the lower chamber 6 is maintained.

[0052] In this case, the pressure in the internal space 16 of the upper chamber 4 gradually increases. Alternatively, the thermocompression bonding apparatus 2 may be capable of connecting the upper chamber 4 to the outside air through the exhaust unit 24 or the like. In this case, when the upper chamber 4 is connected to the outside air, air flows into the internal space 16 rapidly, and the pressure in the internal space 16 of the upper chamber 4 rapidly increases.

[0053] When the pressure in the internal space 16 of the upper chamber 4 becomes higher than the pressure in the internal space 18 of the lower chamber 6, a downward force is applied to the sheet 27 that separates the internal space 16 and the internal space 18. As a result, the sheet 27 is pressed toward one surface (rear surface 11b) of the wafer 11, and is deformed to fit the shape of the one surface (rear surface 11b) of the wafer 11.

[0054] In the contact step S40, the sheet 27 first comes into contact with the annular convex portion 13 on one surface (rear surface 11b) of the wafer 11. Alternatively, the sheet 27 is already in contact with the annular convex portion 13 at the start of the contact step S40. At this time, unlike an adhesive tape having a glue layer and adhesive strength, the sheet 27 does not stick to the annular convex portion 13. The sheet 27 can slide freely relative to the annular convex portion 13.

[0055] As the contact step S40 progresses, the sheet 27 moves toward the circular recess 15 while deforming so as to bite into the circular recess 15 inside the annular protrusion 13, and finally the sheet 27 comes into contact with the circular recess 15. When the sheet 27 comes into contact with a major portion of one surface (rear surface 11b) of the wafer 11 including the annular protrusion 13 and the circular recess 15, the contact step S40 is completed.

[0056] When the contact step S40 is completed, there is no force acting between the sheet 27 and the wafer 11 that is large enough to fix them together. Therefore, in order to fix the sheet 27 to the wafer 11, after the contact step S40, a thermocompression step S50 is performed in which the sheet 27 is heated and thermocompressed to one surface (rear surface 11b) of the wafer 11.

[0057] In the thermocompression bonding step S50, the heating unit of the thermocompression bonding apparatus 2 is operated to heat the sheet 27. For example, if the thermocompression bonding apparatus 2 has a heater 36 as a heating unit, the heater 36 is operated to heat the sheet 27 together with the wafer 11.

[0058] When sheet 27 is heated to a temperature near its melting point in a state in which sheet 27 is pressed toward wafer 11 due to the pressure difference between internal space 16 of first recess 8 and internal space 18 of second recess 10, sheet 27 is thermocompression-bonded to wafer 11. After sheet 27 is thermocompression-bonded, the heating unit (heater 36) is stopped, and heating of sheet 27 is stopped.

[0059] When performing thermocompression bonding, sheet 27 is preferably heated to a temperature equal to or lower than its melting point. If the heating temperature exceeds the melting point, sheet 27 may melt and become unable to maintain its shape. Furthermore, sheet 27 is preferably heated to a temperature equal to or higher than its softening point. If the heating temperature does not reach the softening point, thermocompression bonding cannot be performed appropriately. In other words, sheet 27 is preferably heated to a temperature equal to or higher than its softening point and equal to or lower than its melting point.

[0060] Furthermore, some sheets 27 may not have a clear softening point. Therefore, when performing the thermocompression bonding, the sheet 27 is preferably heated to a temperature that is at least 20° C. lower than its melting point and is at most its melting point.

[0061] For example, when the polyolefin sheet used as sheet 27 is a polyethylene sheet, the heating temperature is preferably 120° C. to 140° C. When the polyolefin sheet is a polypropylene sheet, the heating temperature is preferably 160° C. to 180° C. When the polyolefin sheet is a polystyrene sheet, the heating temperature is preferably 220° C. to 240° C.

[0062] Furthermore, for example, when the polyester-based sheet used as sheet 27 is a polyethylene terephthalate sheet, the heating temperature is set to 250° C. to 270° C. When the polyester-based sheet is a polyethylene naphthalate sheet, the heating temperature is set to 160° C. to 180° C. However, the heating temperature of sheet 27 is not limited to these.

[0063] The heating unit is stopped to stop heating the sheet 27, the second solenoid valve 30 is operated to disconnect the second decompression unit 22 and the lower chamber 6, the pressure in the internal space 18 of the lower chamber 6 is returned to atmospheric pressure, and then the upper chamber 4 is raised. Then, as shown in Fig. 7(A), a frame unit 41 is obtained in which the sheet 27, the wafer 11, and the annular frame 39 are integrated together.

[0064] Conventionally, when an adhesive tape having adhesiveness was applied to a wafer 11 having an annular convex portion 13 and a circular concave portion 15 on one surface (rear surface 11b), a relatively large gap occurred between the adhesive tape and the one surface of the wafer 11. In contrast, when the sheet 27 is thermocompression-bonded to the wafer 11 by the wafer processing method according to this embodiment, the gap generated between the sheet 27 and the one surface of the wafer 11 becomes relatively small. One of the effects achieved by the wafer processing method according to this embodiment will be described in detail.

[0065] 5(A) is a cross-sectional view showing a state in which sheet 27 is in contact with annular protrusion 13 on one surface (rear surface 11b) of wafer 11 in contact step S40. At this point, sheet 27 is not thermocompression bonded to wafer 11 and is not fixed thereto. Here, attention is paid to points 29a and 29b of sheet 27 that overlap step 17 connecting annular protrusion 13 and circular recess 15.

[0066] As the contact step S40 progresses, the sheet 27 is pressed toward the circular recess 15 and deformed. Fig. 5(B) is a cross-sectional view that shows a schematic state in which the sheet 27 is in contact with the circular recess 15 on one surface (rear surface 11b) of the wafer 11 in the contact step S40. Even at this point in time, the sheet 27 is not thermocompression bonded to the wafer 11 and is not fixed thereto.

[0067] Here, before the sheet 27 comes into contact with the circular recess 15, the sheet 27 is drawn toward the circular recess 15 from the outside of the annular protrusion 13 as well. Therefore, points 29a and 29b of the sheet 27 also move, as shown in Fig. 5(B). That is, the sheet 27 comes into contact with the circular recess 15 while each point of the sheet 27 moves significantly. Therefore, the stress acting on the sheet 27 is dispersed, and the sheet 27 is not subjected to a locally large stress in the vicinity of the circular recess 15.

[0068] Then, since a sufficient amount of the sheet 27 is drawn toward the circular recess 15, the gap 31 between the sheet 27 and the wafer 11 becomes extremely small. In addition, since no significant stress remains in the sheet 27 that is thermocompression-bonded to the wafer 11, peeling of the sheet 27 from the wafer 11 over time is extremely limited.

[0069] For comparison, a case in which an adhesive tape is attached to a wafer 11 by a conventional method, unlike the wafer processing method according to this embodiment, will be considered. Fig. 6(A) is a cross-sectional view that shows a state in which the adhesive tape 33 is in contact with the annular convex portion 13 on one surface (rear surface 11b) of the wafer 11. When the adhesive tape 33 comes into contact with the annular convex portion 13 of the wafer 11, the adhesive tape 33 is fixed to the annular convex portion 13. Here, attention is paid to points 35a and 35b of the adhesive tape 33 that overlap with the step 17 that connects the annular convex portion 13 and the circular concave portion 15.

[0070] The adhesive tape 33 is pressed toward the circular recess 15 and deformed. Fig. 6(B) is a cross-sectional view that shows a schematic state in which the adhesive tape 33 is in contact with the circular recess 15 on one surface (rear surface 11b) of the wafer 11. At this point, the adhesive tape 33 is attached and fixed to the circular recess 15 of the wafer 11. Here, since the adhesive tape 33 is fixed to the annular protrusion 13, the adhesive tape 33 is not drawn into the circular recess 15 from the outside of the annular protrusion 13 until the adhesive tape 33 comes into contact with the circular recess 15.

[0071] 6(B), points 35a and 35b of adhesive tape 33 do not move. That is, deformation of adhesive tape 33 occurs only in the region inside annular convex portion 13, and adhesive tape 33 is attached to circular concave portion 15. In this process, adhesive tape 33 is locally greatly deformed, and therefore adhesive tape 33 is locally subjected to large stress. If adhesive tape 33 is fixed to circular concave portion 15 in a state where large stress is applied, adhesive tape 33 becomes easily peeled off from wafer 11 over time.

[0072] Furthermore, because the adhesive tape 33 is not drawn toward the circular recess 15, a large gap 37 is formed between the adhesive tape 33 and the wafer 11. As described below, when cutting the annular protrusion 13 from the wafer 11, a cutting blade is made to cut into the outer periphery of the circular recess 15. However, since the circular recess 15 is not sufficiently supported in the portion overlapping with the gap 37, processing with a cutting blade is inappropriate.

[0073] Therefore, when removing the annular convex portion 13, the cutting blade must cut into the wafer 11 at a position significantly inside the outer periphery of the circular concave portion 15. In this case, devices 21 (see FIG. 1(B)) cannot be formed in the region cut by the cutting blade, and the effective area of ​​the wafer 11 decreases, decreasing the number of device chips manufactured from the wafer 11, thereby reducing the manufacturing efficiency of the device chips.

[0074] In contrast, according to the wafer processing method of the present embodiment, the sheet 27 and the wafer 1 is relatively small. Therefore, the wafer 11 can be cut by the cutting blade at a position closer to the outer periphery of the circular recess 15, so that the effective area of ​​the wafer 11 can be relatively large. In other words, the number of device chips that can be manufactured from the wafer 11 can be increased, and the manufacturing efficiency of the device chips is improved. In addition, since the gap 31 is unlikely to expand over time, the frame unit 41 has good storability after the sheet 27 is thermocompression bonded to the wafer 11.

[0075] In the wafer processing method according to this embodiment, after the thermocompression bonding step S50, a dividing groove forming step S60 is performed in which a dividing groove for cutting out the annular convex portion 13 is formed in the wafer 11. Fig. 8 is a cross-sectional view partially showing a cutting device 38 that performs the dividing groove forming step S60.

[0076] Here, a description will be given of the cutting device 38. The cutting device 38 includes a chuck table 40 that holds the wafer 11 (frame unit 41), and a cutting unit 58 that cuts the wafer 11 held by the chuck table 40.

[0077] The chuck table 40 includes a porous member 44 having a planar upper surface that fits into the circular recess 15, and a frame 42 that houses the porous member 44 and exposes it upward. The frame 42 includes a circular protrusion 48 that mainly supports the circular recess 15 of the wafer 11, and an annular support portion 50 that is disposed on the outer periphery of the circular protrusion 48 and mainly supports the annular protrusion 13 of the wafer 11.

[0078] The circular protrusion 48 of the frame 42 has an accommodating recess on its upper surface for accommodating the porous member 44. The planar shape of the upper surface of the circular protrusion 48 is a shape that fits into the circular recess 15 of the wafer 11, and is slightly smaller than the circular recess 15. The annular support 50 of the frame 42 has a width (distance between the inner and outer peripheries) that is larger than the width (distance between the inner and outer peripheries) of the annular protrusion 13 of the wafer 11. The difference in height between the upper surface of the annular support 50 and the upper surface of the circular protrusion 48 corresponds to the difference in height between the circular recess 15 of the wafer 11 and the annular protrusion 13.

[0079] A suction passage 54 is formed inside the frame 42, one end of which is connected to the porous member 44 and the other end of which is connected to a suction source 52 such as an ejector. For ease of explanation, the suction passage 54 is represented by a line in FIG. 8.

[0080] When the wafer 11 (frame unit 41) is placed on the chuck table 40 and the suction source 52 is operated, negative pressure acts on the wafer 11 (particularly the main part of the circular recess 15) through the suction path 54 and the porous member 44. That is, the wafer 11 is held by suction on the chuck table 40. The upper surface of the circular protrusion 48 of the frame 42 becomes the holding surface 46 that holds the wafer 11 by suction.

[0081] A spacer 56 is disposed on the upper surface of the annular support portion 50. The spacer 56 is formed of an elastic material such as a resin layer, and its thickness varies in accordance with the variation in the difference in height between the circular recess 15 and the annular protrusion 13 of the wafer 11. The suction path 54 formed inside the frame 42 may be branched, and the branch of the suction path 54 is connected to the spacer 56. When the suction source 52 is operated, a negative pressure is applied to the wafer 11 (particularly the annular protrusion 13) through the branch of the suction path 54 and the spacer 56. In this case, the wafer 11 is more firmly held by suction.

[0082] A rotation drive source (not shown) such as a motor is connected to the chuck table 40, and the rotation drive source rotates the chuck table 40 around a rotation axis that is approximately parallel to the holding surface 46. Furthermore, a plurality of clamps (not shown) that grip and fix the annular frame 39 that supports the wafer 11 via the sheet 27 may be provided around the periphery of the chuck table 40.

[0083] A cutting unit 58 that cuts the wafer 11 is disposed above the chuck table 40. The cutting unit 58 includes a cylindrical spindle 60 disposed along a direction generally parallel to the holding surface 46 of the chuck table 40. An annular cutting blade 64 that cuts the wafer 11 is attached to the tip (one end side) of the spindle 60.

[0084] Further, the base end (the other end side) of the spindle 60 is rotatably accommodated in a spindle housing 62. A rotation drive source (not shown) such as a motor is accommodated in the spindle housing 62, and this rotation drive source (not shown) is connected to the base end of the spindle 60. The cutting blade 64 rotates due to the power transmitted from the rotation drive source via the spindle 60.

[0085] For example, a hub-type cutting blade (hub blade) is used as the cutting blade 64 attached to the tip of the spindle 60. The hub blade is composed of an annular base made of metal or the like and an annular cutting edge 66 formed along the outer periphery of the base, which is integrated together. The cutting edge 66 of the hub-type cutting blade is composed of an electroformed grinding wheel in which abrasive grains made of diamond or the like are fixed by a bonding material such as a nickel plating layer.

[0086] However, a washer-type cutting blade (washer blade) can also be used as the cutting blade 64. The washer blade is composed of an annular cutting edge 66 in which abrasive grains are fixed by a binder made of metal, ceramics, resin, etc. In any case, the cutting blade 64 can cut the wafer 11 with the annular cutting edge 66.

[0087] The cutting unit 58 is connected to a moving unit (not shown) so that the position at which the cutting blade 64 cuts into the wafer 11 can be adjusted. In addition, the cutting unit 58 is connected to a lifting unit (not shown) so that the height position of the lower end of the annular cutting blade 66 can be changed.

[0088] When cutting the wafer 11 with the cutting device 38 to remove the annular protrusion 13, first, the frame unit 41 is placed on the chuck table 40. At this time, the position of the wafer 11 is adjusted so that one surface (back surface 11b) of the wafer 11 faces the holding surface 46 and the center of the holding surface 46 overlaps with the center of the one surface of the wafer 11. Thereafter, the suction source 52 is operated to suction-hold the wafer 11 on the chuck table 40 via the sheet 27.

[0089] The position where the dividing groove of the wafer 11 is to be formed is set in a circular area centered on the center of the circular recess 15. According to the wafer processing method of this embodiment, the gap 31 between the wafer 11 and the sheet 27 is sufficiently small, so that the area where the dividing groove is to be formed can be set relatively outside the circular recess 15. By moving the cutting unit 58, the cutting edge 66 of the cutting blade 64 is positioned above the area where the dividing groove is to be formed.

[0090] Next, the rotary drive source provided inside the spindle housing 62 is operated to start rotation of the cutting blade 64, and the cutting unit 58 is lowered to cause the cutting edge 66 to cut into the wafer 11. Then, the cutting unit 58 is lowered to a height position where the lower end of the cutting edge 66 reaches the sheet 27, and rotation of the chuck table 40 is started. Then, when the chuck table 40 rotates once or more, a circular dividing groove is formed in the wafer 11, and the annular protrusion 13 is separated from the wafer 11.

[0091] Note that the dividing groove forming step S60 is not limited to this. For example, the height of the cutting unit 58 is adjusted in advance so that the height of the lower end of the cutting blade 66 outside the wafer 11 is lower than the height of the upper surface of the sheet 27, and the cutting blade 66 is caused to cut from the outer periphery of the wafer 11. That is, the cutting unit 58 and the chuck table 40 are moved in a direction parallel to the holding surface 46, and the cutting blade 66 is caused to cut into the area where the dividing groove is to be formed. In this state, when the chuck table 40 is rotated once, a circular dividing groove is formed in the wafer 11.

[0092] After the dividing groove forming step S60, a removing step S70 is performed in which the annular convex portion 13 separated from the wafer 11 is removed from the sheet 27. Fig. 7(B) includes a cross-sectional view showing a schematic view of the annular convex portion 13 when it is removed from the sheet 27 in the removing step S70. After the annular convex portion 13 is separated from the wafer 11, when the frame unit 41 is carried out from the chuck table 40, the portion of the wafer 11 that was the circular recess 15 and the annular convex portion 13 remain on the sheet 27.

[0093] In this state, the annular protrusion 13 is pulled up and peeled off from the sheet 27. This results in a frame unit 41 in which the wafer 11 from which the annular protrusion 13 has been removed, the sheet 27, and the annular frame 39 are integrated together. Thereafter, the wafer 11 is divided along the intended division lines 19 (see FIG. 1(B)), to obtain individual device chips each including a device 21.

[0094] As described above, the wafer processing method of this embodiment makes it possible to arrange a sheet 27 in place of adhesive tape 33 on one side (back side 11b) of a wafer 11 having a circular recess 15 without creating a large gap 31, and also makes it possible to suppress the expansion of the gap 31 over time.

[0095] In the above embodiment, a case has been described in which a dividing groove is formed in the wafer 11 using the cutting device 38 equipped with the cutting blade 64 in the dividing groove forming step S60, but one aspect of the present invention is not limited to this. That is, in the dividing groove forming step S60, a laser processing device (not shown) capable of irradiating the wafer 11 with a laser beam to laser process the wafer 11 may be used.

[0096] For example, a laser beam including a wavelength component absorbed by the wafer 11 is irradiated onto an area of ​​the wafer 11 where a dividing groove is to be formed, and the wafer 11 is ablated. Alternatively, a laser beam including a wavelength component that transmits through the wafer 11 is focused onto an area of ​​the wafer 11 where a dividing groove is to be formed, a modified layer is formed on the wafer 11 along that area, and the wafer 11 is divided using the modified layer as a dividing starting point. Even in this case, according to the wafer processing method according to one aspect of the present invention, a dividing groove can be formed at a position relatively close to the outer periphery of the circular recess 15 of the wafer 11.

[0097] In addition, the structures, methods, and the like according to the above-described embodiments and modifications may be modified as appropriate without departing from the scope of the present invention. The above-described embodiments and modifications may be combined as appropriate. [Explanation of symbols]

[0098] 11 Wafers 11a surface 11b Back side 13 Annular protrusion 15 Circular recess 17 Steps 19 Division line 21 Devices 23 Surplus outer area 25 Device Formation Area 27 sheets 29a,29b points 31 Gap 33 Adhesive Tape 35a,35b points 37 Gap 39 Annular Frame 39a opening 41 Frame unit 2 Thermocompression bonding equipment 4 Upper chamber 6 Lower Chamber 8 First recess 10 Second recess 12 First opening 14 Second opening 16,18 Interior space 20 First decompression unit 22 Second decompression unit 24,26 Exhaust section 28 First solenoid valve 30 Second solenoid valve 32 Holding Table 34 Holding surface 36 Heater 38 Cutting equipment 40 Chuck table 42 Frame 44 Porous Materials 46 Holding surface 48 Circular protrusion 50 Annular support 52 Suction source 54 Suction path 56 Spacer 58 Cutting unit 60 Spindle 62 Spindle housing 64 Cutting Blade 66 Cutting edge

Claims

1. A processing method for processing a wafer having one surface with an annular convex portion on an outer periphery and a circular concave portion formed in an area surrounded by the annular convex portion, in a thermocompression bonding apparatus comprising an upper chamber connected to a first decompression unit and having a first concave portion with a first opening, a lower chamber connected to a second decompression unit and having a second concave portion with a second opening, and a holding table disposed in the second concave portion and holding the wafer, the upper chamber and the lower chamber being closed by aligning the first opening and the second opening, a holding step of holding the wafer with the one surface facing upward from below by the holding table of the thermocompression bonding apparatus; a sealing step of sandwiching the sheet of a frame unit, the frame unit having an annular frame having an opening in the center capable of accommodating the wafer, between the first opening of the first recess and the second opening of the second recess inside the opening, and closing the first recess and the second recess; a depressurizing step of depressurizing the first recess by the first depressurizing unit and depressurizing the second recess by the second depressurizing unit after the sealing step; a contacting step of increasing the pressure in the first recess after the depressurizing step and contacting the sheet with the annular protrusion and the circular recess by contacting the sheet with the one surface of the wafer; a thermocompression bonding step after the contacting step of heating the sheet to thermocompress the sheet to the one surface of the wafer.

2. a dividing groove forming step of forming a dividing groove in the wafer by cutting out the annular protrusion after the thermocompression bonding step; 2. The wafer processing method according to claim 1, further comprising a removing step of removing the annular convex portion from the sheet after the dividing groove forming step.

Citation Information

Patent Citations

  • Method of processing wafer and device

    JP2007173487A

  • Method of processing wafer, and apparatus for removing annular projection

    JP2011061137A