Partial plating device and partial plating method

The partial plating apparatus and method using a backup belt with specific elastic properties prevents unintended plating on non-plated areas, reducing precious metal deposition and optimizing plating efficiency.

JP2024162760APending Publication Date: 2024-11-21DOWA METALTECH CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023078628
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-11
Publication Date
2024-11-21

AI Technical Summary

Technical Problem

Conventional partial plating methods using drum-shaped jigs result in unintended plating on areas that do not require plating, leading to increased costs due to unnecessary deposition of precious metals like Au and Ag.

Method used

A partial plating apparatus and method utilizing a backup belt with a soft elastic body (Asker C hardness of 0.5° to 25°) and a hard elastic body (hardness of 35° or more) to press the material against a drum-shaped jig, preventing plating solution contact with non-plated areas by using a backup belt with a soft elastic body (0.5° to 25° Asker C hardness) and a hard elastic body (35° or more) on a base material, ensuring precise plating only on required surfaces.

Benefits of technology

The solution effectively reduces unnecessary plating on non-plated areas, minimizing the deposition of precious metals on side and back surfaces, thereby reducing material costs and ensuring targeted plating adherence.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024162760000001_ABST
    Figure 2024162760000001_ABST
Patent Text Reader

Abstract

To prevent an unnecessary plating solution from coming into contact with a plating unnecessary area of a material to be plated when performing partial plating using a drum-type jig, thereby reducing the amount of plating that adheres to the plating unnecessary area.SOLUTION: A partial plating device 1 using a drum-shaped jig 11 comprises a backup belt 31 for pressing a material to be plated, which comprises a terminal member 21, against a cylindrical surface 11a of the drum-shaped jig 11, wherein: the cylindrical surface 11a of the drum-shaped jig 11 includes an opening 13 for supplying a plating solution to a surface 23a to be plated of the terminal member 21; the backup belt 31 has a substrate 32 and a soft elastic body 33 arranged on one side of the substrate 32 to press a terminal part 23 of the terminal member 21 from the back side 23b, which is opposite to the plating surface 23a, to the cylindrical surface 11a of the drum-shaped jig 11; and the Asker C hardness of the soft elastic body 33 is 0.5° to 25°.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a selective plating apparatus and a selective plating method using a drum-type jig. [Background technology]

[0002] Terminal members are plated to provide electrical conductivity and corrosion resistance. Usually, a base plating of Ni, Cu, etc. is first applied, and then a precious metal plating of Au, Ag, etc. is applied on the surface of the base plating. The base plating is applied to improve the adhesion of the precious metal plating and provide corrosion resistance, etc., while the surface precious metal plating is applied to provide electrical conductivity, corrosion resistance, etc.

[0003] Precious metals such as Au and Ag used for surface plating are expensive, and in order to reduce the raw material cost for plating, it is desirable to form the surface plating on the minimum necessary range (part, area) of the terminal member. In the case of a terminal member, which is an intermediate product of a terminal formed by pressing a metal plate material into a terminal shape, the minimum necessary range is the part used as a contact point, for example, the terminal tip part on one (front) plate surface (non-fractured surface). Furthermore, plating is not formed on the side surface, which is a fractured surface caused by pressing, or the other plate surface (back surface).

[0004] A conventional method for performing partial plating only on the areas that require plating is the plating method using a drum-type jig, in which the material to be plated is wrapped around the drum-type jig and plating solution is sprayed from the inside of the drum-type jig through a nozzle to perform continuous plating.

[0005] Conventionally, when plating is performed using a drum-type jig, plating is performed in a state where the workpiece is pressed against the drum-type jig from the outside by a backup belt.

[0006] For example, Patent Document 1 discloses that in a rotary drum type selective plating device, a masking belt is provided with a convex portion that fits into a concave portion on the circumferential surface of the rotary drum, thereby suppressing positional fluctuation of the masking belt.

[0007] Patent Document 2 discloses that in a rotating drum type partial plating device, a backup member that is pressed against the outer periphery of the rotating drum to make tight contact therewith is formed with an opening for draining plating solution that corresponds to the plating holes in the rotating drum, thereby solving the problems of plating loss and bleeding.

[0008] Patent Document 3 discloses that when plating terminal members using a rotating drum-type jig, adhesion of plating to the side surfaces of the terminals is suppressed by providing sidewall members made of an insulating material around the opening of the drum-type jig and along the side surfaces of the terminals.

[0009] Patent Document 4 discloses that when forming a plating layer on a protruding portion of a base to be partially plated, the protruding portion is sandwiched between insulators in the width direction of the base, and the top portion of the protruding portion is immersed in a flowing plating solution, thereby preventing the formation of a plating layer in unnecessary portions. [Prior art documents] [Patent documents]

[0010] [Patent Document 1] Japanese Patent Application Publication No. 11-131284 [Patent Document 2] JP 2013-216937 A [Patent Document 3] JP 2015-108186 A [Patent Document 4] Japanese Patent Application Publication No. 2-97692 Summary of the Invention [Problem to be solved by the invention]

[0011] However, with either method, in the case of the plated material such as a terminal member, the plating solution will come into contact with parts that do not require plating by design (parts not requiring plating), such as the press-fractured surface (side surface of the terminal) or the plate surface opposite the surface to be plated, and it is unavoidable that the plating will adhere to the parts not requiring plating, resulting in increased costs.

[0012] The object of the present invention is to prevent unnecessary plating solution from coming into contact with parts of a workpiece that do not need to be plated when performing selective plating using a drum-type jig, and to reduce the amount of plating adhering to the parts that do not need to be plated. [Means for solving the problem]

[0013] In order to solve the above problems, the present invention provides a selective plating apparatus that uses a drum-type jig, comprising a backup belt for pressing a workpiece to be plated consisting of a terminal member against the cylindrical surface of the drum-type jig, the cylindrical surface of the drum-type jig having an opening for supplying a plating solution to the surface to be plated of the terminal member, the backup belt having a base material and a soft elastic body that is disposed on one surface of the base material and presses the terminal portion of the terminal member against the cylindrical surface of the drum-type jig from the back surface side that is opposite the surface to be plated, and the soft elastic body has an Asker C hardness of 0.5° to 25°.

[0014] A hard elastic body having a higher Asker C hardness and a smaller thickness than the soft elastic body may be provided in an area where the soft elastic body is not disposed on one surface of the substrate. The hard elastic body preferably has an Asker C hardness of 35° or more. The soft elastic body may be a synthetic rubber. The soft elastic body may be mainly composed of one or more synthetic rubbers selected from the group consisting of silicone rubber, ethylene-propylene-diene rubber, and nitrile rubber.

[0015] It is preferable that the difference between the thickness of the soft elastic body and the thickness of the hard elastic body is equal to or greater than the plate thickness of the workpiece. It is preferable that the soft elastic body has a width sufficient to cover the entire terminal portion of the terminal member.

[0016] Further, according to the present invention, there is provided a partial plating method for a terminal member, in which a plated material consisting of a terminal member is pressed against the cylindrical surface of a drum-type jig by a backup belt to bring the material into close contact with the cylindrical surface of the drum-type jig, and a plating solution is supplied to a terminal portion of the terminal member through an opening formed in the drum-type jig to form a plating on the plated surface of the terminal portion, characterized in that the backup belt has a base material and a soft elastic body having an Asker C hardness of 0.5° to 25° and arranged on one surface of the base material, and the soft elastic body presses at least the terminal portion of the terminal member from the back surface side opposite to the plated surface of the terminal member on which plating is to be formed, and the terminal member is brought into close contact with the cylindrical surface of the drum-type jig to perform plating.

[0017] A hard elastic body having a higher Asker C hardness and a smaller thickness than the soft elastic body may be provided in an area where the soft elastic body is not disposed on one surface of the substrate. The hard elastic body preferably has an Asker C hardness of 35° or more. The soft elastic body may be a synthetic rubber. The soft elastic body may be mainly composed of one or more synthetic rubbers selected from the group consisting of silicone rubber, ethylene-propylene-diene rubber, and nitrile rubber.

[0018] It is preferable that the difference between the thickness of the soft elastic body and the thickness of the hard elastic body is equal to or greater than the sheet thickness of the plated material. It is preferable that the soft elastic body presses the entire terminal portion of the terminal member from the back surface side of the terminal member. Effect of the Invention

[0019] According to the present invention, when performing partial plating of Au or the like using a drum-type jig, it is possible to provide a partial plating apparatus and a partial plating method which prevent the plating solution from coming into contact with parts of the workpiece that do not require partial plating, thereby reducing the amount of plating adhering to the parts that do not require plating. [Brief description of the drawings]

[0020] [Figure 1] FIG. 1 is a top view showing an outline of a selective plating device using a drum-type jig. [Diagram 2] 1A and 1B are side views of a drum-type jig, in which FIG. 1A shows the cylindrical surface of the drum-type jig and FIG. 1B shows the state of the cylindrical surface of the drum-type jig during spot plating. [Diagram 3] 1A and 1B show an example of a backup belt according to an embodiment of the present invention, where FIG. 1A is a plan view and FIG. [Figure 4] 1A and 1B are cross-sectional views of backup belts in examples and comparative examples of the present invention, and a front view showing the positional relationship between a terminal member and the backup belt, where (a) is Example 1 of the present invention, and (b) is Comparative Example 1. [Diagram 5] 1A is a cross-sectional view of a backup belt in an embodiment of the present invention and a comparative example, and a front view showing the positional relationship between a terminal member and the backup belt, where (a) is an embodiment 2 of the present invention, (b) is an embodiment 3, and (c) is a comparative example 2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0021] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In this specification and the drawings, elements having substantially the same functional configurations are denoted by the same reference numerals, and duplicated explanations will be omitted.

[0022] FIG. 1 shows an outline of a partial plating apparatus 1 equipped with a backup belt according to an embodiment of the present invention. The partial plating apparatus 1 to which the present invention is directed is equipped with a belt-shaped backup belt 31 for pressing a plated material consisting of a belt-shaped terminal member 21 against a cylindrical surface 11a of a drum-type jig 11. As shown in FIGS. 2(a) and 2(b), the cylindrical surface 11a of the drum-type jig 11 is equipped with an opening 13 for supplying a plating solution to a plated surface 23a of a terminal portion 23 of the terminal member 21. The terminal member 21 has an upper support portion 22 having a guide hole 22h and a terminal portion 23 extending from the upper support portion 22. In this specification, the region on the plated surface 23a side of the terminal portion 23 where partial plating is performed facing the opening 13 is referred to as a plated region. As shown in Fig. 3(b), the backup belt 31 is characterized in that it comprises a substrate 32, a band-shaped soft elastic body 33 provided on one surface of the substrate 32 for contacting the terminal portion 23 of the terminal member 21 and pressing the terminal portion 23 against the cylindrical surface 11a of the drum-type jig 11 from the back surface 23b side opposite to the surface 23a to be plated, and the Asker C hardness of the soft elastic body 33 is 0.5° to 25°. Furthermore, as shown in Fig. 3(b), it is preferable that a hard elastic body 34 having a higher Asker C hardness and a smaller thickness than the soft elastic body 33 is provided on one surface of the substrate 32 at a position where the soft elastic body 33 is not provided.

[0023] Here, pressing the terminal portion 23 means pressing at least a part of the terminal portion 23. The area where the soft elastic body 33 contacts the terminal portion 23 may be a part or the whole of the terminal portion 23. The area to be plated may be a part or the whole of the plated surface 23a side of the terminal portion 23.

[0024] The Asker C hardness is a value obtained by the spring hardness test (type C) method specified in JIS K7312, and may be measured using a hardness tester conforming to JIS K7312.

[0025] The selective plating apparatus 1 is also provided with a member transport roll 2 for transporting a terminal member 21 which is a material to be plated, and a backup belt transport roll 3 for transporting a backup belt 31.

[0026] In this embodiment, an example will be described in which Au plating is performed on a terminal member 21 as a material to be plated, using a backup belt 31 having a soft elastic body 33 and a hard elastic body 34 provided on a substrate 32 in a (continuous) partial plating apparatus 1 using such a drum-type jig 11.

[0027] The drum-type jig 11 has a cylindrical shape formed of, for example, an insulating resin such as PVC, and is a jig that partially plates a terminal member 21 as a material to be plated while being conveyed along the outer periphery in close contact with the cylindrical surface 11a of the drum-type jig 11. The drum-type jig 11 rotates as the terminal member 21 is sent out by the member conveying roll 2. The cylindrical surface 11a of the drum-type jig 11 is provided with a positioning pin 12 as shown in FIG. 2(a), and the positioning pin 12 is fitted into a guide hole 22h formed in the terminal member 21 as shown in FIG. 2(b), thereby fixing the position of the terminal member 21 in the conveying direction and the up-down direction (perpendicular to the conveying direction) on the drum-type jig 11. A plurality of openings 13 are formed in the cylindrical surface 11a of the drum-type jig 11 so that when the position of the terminal member 21 is fixed, the region to be plated on the plated surface 23a of the terminal portion 23 of the terminal member 21 and the openings 13 of the drum-type jig 11, which are the supply region of the plating solution, overlap at the same position. The terminal member 21 may be a terminal member 21 made of a material punched by pressing, and is not limited to the shape shown in FIG. 2(b). For example, the terminal member 21 may have a shape in which an upper support portion 22 including a guide hole 22h is provided above the punched portion of the belt-shaped terminal member 21, a lower support portion 25 (see FIGS. 4 and 5) is provided below the punched portion, and portions called tie bars that connect the upper support portion 22 and the lower support portion 25 are provided on the left and right of the punched portion.

[0028] An Au plating solution jetting device 14 is provided inside the drum-type jig 11. Au plating solution is supplied to the Au plating solution jetting device 14 from a plating solution tank (not shown), and the Au plating solution is supplied to the space between the metal plate 15 on the surface of the Au plating solution jetting device 14 and the drum-type jig 11. The Au plating solution is then jetted toward the terminal portion 23 of the terminal member 21 from an opening 13 provided in the cylindrical surface 11a of the drum-type jig 11, and the Au plating solution is supplied to the plating area. With the metal plate 15 as the anode and the terminal member 21 as the cathode, a current is passed through the Au plating solution supplied to the plating area, whereby partial plating is continuously performed on the plating surface 23a of the terminal portion 23 of the terminal member 21. When partial plating is performed continuously, the terminal member 21 is pressed against the cylindrical surface 11a of the drum-type jig 11 by a backup belt 31 from the outside (the back surface 23b side of the terminal member 21 opposite the surface 23a to be plated).

[0029] 3 is a plan view and a cross-sectional view of the backup belt 31. The belt-shaped backup belt 31 is composed of a base material 32 and two types of soft elastic bodies 33 and hard elastic bodies 34, such as synthetic rubber, having different hardness, which are provided on one surface of the base material 32 by, for example, adhesion.

[0030] The substrate 32 is preferably a band-shaped member with no permeability. "Non-permeable" means that even if a plating solution comes into contact with one side of the substrate 32, the plating solution does not seep out from the other side. The substrate 32 may be made of any material that is flexible enough to withstand tensile stress and can be used as the backup belt 31, and may be, for example, a material with a core of polyester canvas, one side of which is silicone-coated and the other side is silicone-impregnated.

[0031] A band-shaped soft elastic body 33 having an Asker C hardness of 0.5° to 25° is provided by adhesion or the like on a part or the whole of the area on the surface of the base material 32 that may come into contact with the terminal portion 23. In an area where the soft elastic body 33 is not provided, a band-shaped hard elastic body 34 having an Asker C hardness of 35° or more and thinner than the soft elastic body 33 is preferably provided by adhesion or the like. In this case, when the terminal member 21 is pressed against the cylindrical surface 11a of the drum-type jig 11 by the backup belt 31 to be in close contact with the terminal member 21, the soft elastic body 33 on the base material 32 protrudes toward the terminal member 21 side (drum-type jig 11 side) more than the hard elastic body 34. The thickness of the soft elastic body 33 and the hard elastic body 34 is preferably, for example, 0.1 to 10 mm.

[0032] The present invention is characterized in that at least the terminal portion 23 (and between the terminal portions) of the terminal member 21 is pressed by the soft elastic body 33 of the backup belt 31 from the back surface 23b side opposite to the plated surface 23a of the terminal member 21 on which plating is to be formed, and the terminal member 21 is brought into close contact with the cylindrical surface 11a of the drum-type jig 11 for plating. A plating solution is supplied from an opening 13 formed in the drum-type jig 11, and plating is formed on the plated surface 23a of the terminal portion 23 of the terminal member 21. The area on the plated surface 23a of the terminal portion 23 on which plating is formed is the plated area.

[0033] The soft elastic body 33 is deformed by pressing to fill the space between the terminals, and covers the back surface 23b and the side surface of the terminals 23, suppressing the contact and adhesion of the plating solution to the back surface 23b and the side surface (for example, the fracture surface caused by the press working) of the terminals 23. If the hardness of the soft elastic body 33 is 0.5° to 25° in Asker C hardness, it can be deformed along the side surface of the terminals 23, but if it exceeds 25°, it will not be deformed sufficiently, and there is a risk that it will not be possible to suppress the contact and adhesion of the Au plating solution to the side surface of the terminals 23. In other words, when pressing with a hard elastic body such as the hard elastic body 34 described later, it is difficult to suppress the contact of the plating solution. Therefore, the hardness of the soft elastic body 33 is set to 25° or less. Also, if the Asker C hardness of the soft elastic body 33 is less than 0.5°, the terminals 23 may sink into the backup belt 31 and cover a part of the plated surface 23a, which may result in poor plating. Therefore, the Asker C hardness of the soft elastic body 33 is set to 0.5° to 25°, and more preferably 1° to 20°.

[0034] The soft elastic body 33 and the hard elastic body 34 arranged on the surface of the substrate 32 may have various shapes depending on the shape of the terminal portion 23 and the shape of the region to be plated, and from the viewpoint of cost, a strip shape is preferable. Moreover, the region on one surface of the substrate 32 where the soft elastic body 33 is arranged includes at least a part of the region that may come into contact with the terminal portion 23. The soft elastic body 33 may be in the shape of a strip having a specific width, and is preferably a width that covers at least the tip portion of the terminal portion 23, and more preferably a width that covers the entire terminal portion 23 in order to prevent excess Au plating solution from adhering.

[0035] In addition, a hard elastic body 34 having a higher hardness and a smaller thickness than the soft elastic body 33 may be provided in an area on one side of the substrate 32 where the soft elastic body 33 is not provided. In this case, it is preferable that the area on one side of the substrate 32 where the hard elastic body 34 is provided is an area including an area where the guide hole 22h in the upper support part 22 of the terminal member 21 may come into contact. By using the hard elastic body 34 in this area, it is possible to effectively suppress changes in the inclination of the terminal member 21 relative to the cylindrical surface 11a of the drum-type jig 11. If the soft elastic body 33 is provided up to the area where the guide hole 22h may come into contact, there is a risk that the angle of the terminal member 21 relative to the cylindrical surface 11a of the drum-type jig 11 may vary, causing a variation in the plating thickness of the plated area.

[0036] The material of the soft elastic body 33 is preferably made mainly of synthetic rubber, and preferably made mainly of one or more synthetic rubbers selected from the group consisting of silicone rubber, ethylene-propylene-diene rubber, and nitrile rubber. It may also be a foam of these synthetic rubbers.

[0037] The hard elastic body 34 can be made of synthetic rubber such as silicone rubber having an Asker C hardness of 35° or more. If the hard elastic body 34 has the same thickness as the soft elastic body 33, the soft elastic body 33 is less likely to deform to cover the side surface of the terminal portion 23. Therefore, it is preferable that the thickness of the soft elastic body 33 is greater than the thickness of the hard elastic body 34 so that the soft elastic body 33 protrudes from the surface of the hard elastic body 34 in a state where no pressure is applied. Furthermore, it is more preferable that the protruding dimension of the soft elastic body 33 (the difference in thickness between the soft elastic body 33 and the hard elastic body 34) is equal to or greater than the plate thickness of the plated material in a state where no pressure is applied. Depending on the Asker C hardness of the soft elastic body 33, the protruding dimension can be 1 to 5 times the plate thickness of the plated material. For example, when the plated material has a plate thickness of 0.64 mm, the protruding dimension can be about 1 to 3 mm. By making the protruding dimension equal to or greater than the plate thickness of the material to be plated, the side surface of the terminal can be sufficiently covered, which increases the effect of reducing the amount of Au attached to the side surface of the terminal. Note that in this specification, the thickness of each of the soft elastic body 33 and the hard elastic body 34 is the average thickness in the width direction of the strip.

[0038] By configuring the backup belt 31 as described above, it is possible to prevent the plating solution from coming into contact with the back side (back surface 23b) and side surfaces (fractured surfaces by pressing, etched surfaces, etc.) of the plated surface 23a of the terminal member 21, which is the material to be plated. In addition, by making the part that presses the terminal portion 23 a soft elastic body 33, the soft elastic body 33 deforms and enters the punched portion (space between terminals) of the terminal member 21 made of material punched by pressing, for example, and it is possible to reduce the plating solution coming into contact with the portion not requiring plating. Furthermore, the current is shielded by the soft elastic body 33, thereby reducing the amount of unnecessary plating adhering to the fractured surfaces and surrounding areas of the punched portion.

[0039] Furthermore, the partial plating method of the present invention is a method for partial plating of a terminal member 21, in which a (strip-shaped) terminal member 21 is pressed against the cylindrical surface 11a of a drum-type jig 11 by a (strip-shaped) backup belt 31 to bring the material to be plated into intimate contact with the cylindrical surface 11a, and a plating solution is supplied to the terminal portion of the terminal member 21 through an opening 13 formed in the drum-type jig 11 to form a plating on the plated surface 23a of the terminal portion 23, and the backup belt 31 has a base material 32 and a band-shaped soft elastic body 33 having an Asker C hardness of 0.5° to 25° and arranged on one surface of the base material 32, and is characterized in that the soft elastic body 33 presses at least the terminal portion 23 of the terminal member 21 from the back surface 23b side opposite to the plated surface 23a of the terminal member 21 on which plating is to be formed, and the terminal member 21 is brought into intimate contact with the cylindrical surface 11a of the drum-type jig 11 to perform plating. On one surface of the base material 32, a hard elastic body 34 having a higher Asker C hardness and a smaller thickness than the soft elastic body 33 is preferably provided at a position where the soft elastic body 33 is not provided.

[0040] Hereinafter, a procedure for a partial plating method using a backup belt 31 having a soft elastic body 33 and a hard elastic body 34 provided on a base material 32 according to an embodiment of the present invention will be described. In this embodiment, too, an example is described in which Au plating is performed on a terminal member 21 as a material to be plated. When plating the terminal member 21, it is preferable to perform pre-treatment, undercoat plating (Ni plating, Cu plating, etc.), finish plating (also called surface plating or main plating), and post-treatment in that order.

[0041] First, as pretreatment, degreasing is performed to remove oil from the surface of the terminal member 21, pickling is performed to remove an oxide film on the surface, and water rinsing is performed to remove chemicals, etc. The pretreatment is generally performed in the order of water rinsing, degreasing, water rinsing, pickling, and water rinsing.

[0042] After the pretreatment is completed, the terminal member 21 is entirely immersed in a Ni sulfamate plating solution to perform electric Ni plating as the underplating, for example, in order to improve the adhesion between the finish plating and the underplating, and to prevent corrosion deterioration of the terminal member 21 itself and diffusion of metal elements in the terminal member 21. The method of underplating is not limited to this, and it is sufficient that Ni is uniformly attached to the necessary parts of the terminal member 21. Cu plating may also be performed as the underplating.

[0043] It is preferable that the pretreatment, base plating, and further the post-treatment described below are carried out in a continuous plating apparatus (not shown) using, for example, a reel-to-reel plating method, and it is preferable that the selective plating apparatus of the present invention is incorporated into this continuous plating apparatus.

[0044] After the underplating, the plated surface 23a of the terminal portion 23 of the terminal member 21, for example, at the terminal tip, is plated as a finishing plating. The main plating is performed to satisfy the corrosion resistance, electrical conductivity, wear resistance, and other properties required for the parts, and in addition to Au plating, for example, Ag, Sn, etc. are plated. The terminal member 21 is transported by the member transport roll 2 and pressed against the cylindrical surface 11a of the drum-type jig 11 by the backup belt 31. The backup belt 31 is a base material 32 on which a soft elastic body 33 is provided, and the soft elastic body 33 presses the terminal portion 23 of the terminal member 21 from the back side. Alternatively, the backup belt 31 may be a base material 32 on which a soft elastic body 33 and a hard elastic body 34 are provided, for example, as in the above-mentioned embodiment. The Au plating solution is supplied to the outside through a plurality of openings 13 formed in the cylindrical surface 11a of the drum-type jig 11 as described above. In this manner, the Au plating solution is sprayed while the terminal member 21 is being transported, and an Au plating film is formed on the plated surface 23a of the terminal portion 23 at the terminal tip of the terminal member 21. The back surface 23b of the terminal portion 23 is pressed by the soft elastic body 33 of the backup belt 31, and the soft elastic body 33 is deformed to cover the back surface 23b and side surface of the terminal portion 23, thereby preventing the Au plating solution from spilling out from the plated surface 23a of the terminal portion 23 and adhering thereto.

[0045] After the Au plating, the terminal member 21 is washed with water and dried with hot air as post-treatment, completing a series of continuous plating processes. The plated terminal member 21 is processed and divided into a required shape by, for example, pressing, etc., and used as a terminal.

[0046] Although the preferred embodiment of the present invention has been described above, the present invention is not limited to such an example. For example, the cylindrical surface 11a of the drum-shaped jig 11 may not be provided with the positioning pin 12, and the positioning may be performed by another method that does not use the positioning pin 12 and the guide hole 22h. It is clear that a person skilled in the art can think of various modified or revised examples within the scope of the technical ideas described in the claims, and it is understood that these also naturally fall within the technical scope of the present invention.

[0047] In addition, the effects described in this specification are merely explanatory or exemplary and are not limiting. In other words, the technology according to the present disclosure may achieve other effects that are apparent to a person skilled in the art from the description of this specification in addition to or in place of the above effects.

[0048] Note that the following configuration examples also fall within the technical scope of the present disclosure. (1) A selective plating device using a drum-type jig, a backup belt for pressing a workpiece made of a terminal member against the cylindrical surface of the drum-type jig; the cylindrical surface of the drum-type jig is provided with an opening for supplying a plating solution to the surface to be plated of the terminal member; the backup belt has a base material and a soft elastic body disposed on one surface of the base material for pressing the terminal portion of the terminal member from a back surface side opposite to a surface to be plated against the cylindrical surface of the drum-type jig; The selective plating apparatus is characterized in that the soft elastic body has an Asker C hardness of 0.5° to 25°. (2) The selective plating apparatus described in (1) above, characterized in that, on one surface of the base material, in an area where the soft elastomer is not arranged, a hard elastomer having a higher Asker C hardness and a smaller thickness than the soft elastomer is provided. (3) The selective plating apparatus according to (2) above, characterized in that the hard elastic body has an Asker C hardness of 35° or more. (4) The selective plating apparatus according to any one of (1) to (3), wherein the soft elastic body is made of synthetic rubber. (5) The selective plating apparatus according to any one of (1) to (4), wherein the soft elastomer is mainly composed of one or more synthetic rubbers selected from the group consisting of silicone rubber, ethylene-propylene-diene rubber, and nitrile rubber. (6) The selective plating apparatus according to any one of (2) to (5), characterized in that the difference between the thickness of the soft elastic body and the thickness of the hard elastic body is equal to or greater than the plate thickness of the material to be plated. (7) The continuous selective plating apparatus according to any one of (1) to (6), wherein the soft elastic body has a width sufficient to cover the entire terminal portion of the terminal member. (8) A method for partial plating of a terminal member, comprising pressing a workpiece to be plated, which is a terminal member, against a cylindrical surface of a drum-type jig by a backup belt to bring the workpiece into intimate contact with the cylindrical surface, and supplying a plating solution to a terminal portion of the terminal member through an opening formed in the drum-type jig to form a plating on the surface to be plated of the terminal portion, comprising the steps of: The backup belt has a base material and a soft elastic body having an Asker C hardness of 0.5° to 25° arranged on one surface of the base material, A selective plating method, characterized in that at least the terminal portion of the terminal member is pressed from the back surface side opposite the plated surface on which plating is formed of the terminal member by the soft elastic body, and the terminal member is closely attached to the cylindrical surface of the drum-shaped jig for plating. (9) The selective plating method according to (8) above, characterized in that, on one surface of the base material, in an area where the soft elastomer is not disposed, a hard elastomer having a higher Asker C hardness and a smaller thickness than the soft elastomer is disposed. (10) The selective plating method according to (9) above, wherein the hard elastic body has an Asker C hardness of 35° or more. (11) The selective plating method according to any one of (8) to (10), wherein the soft elastic body is a synthetic rubber. (12) The continuous selective plating method according to any one of (8) to (11), wherein the soft elastomer is mainly composed of one or more synthetic rubbers selected from the group consisting of silicone rubber, ethylene-propylene-diene rubber, and nitrile rubber. (13) The continuous selective plating method according to any one of (9) to (12), characterized in that the difference between the thickness of the soft elastomer and the thickness of the hard elastomer is equal to or greater than the sheet thickness of the material to be plated. (14) The continuous selective plating method according to any one of (8) to (13), characterized in that the entire terminal portion of the terminal member is pressed from a back surface side of the terminal member by the soft elastic body. EXAMPLES

[0049] [Example 1], [Comparative Example 1] A test was conducted on the terminal member 21, which was formed by pressing a rolled brass material (C2600R-H) to form a terminal portion 23, by using a continuous plating processing device equipped with the partial plating device described above, in which the pre-treatment, Ni plating as the under-plating, Au plating as the main plating, and post-treatment were performed. The soft elastic body 33a and the hard elastic body 34a of the backup belt 31a were strip-shaped.

[0050] 4(a), in the backup belt 31a of Example 1, a soft elastic body 33a is arranged in an area that may come into contact with the terminal portion 23, with a width that covers the entire terminal portion 23 from the back surface side opposite to the plated surface of the terminal member 21, and a hard elastic body 34a is arranged in an area where the soft elastic body 33a is not arranged. The terminal member 21 has an upper support portion 22 having a guide hole 22h, and a lower support portion 25, and the hard elastic body 34a is arranged in an area including an area that comes into contact with the guide hole 22h in the upper support portion 22 and an area that comes into contact with the lower support portion 25. The base material 32 of the backup belt 31a has a core material of polyester canvas, one side of which is silicone-coated and the other side is silicone-impregnated, with a thickness of 2 mm. Then, a soft elastomer 33a made of ethylene-propylene-diene rubber (EPDM) foam with an Asker C hardness of 1° and a thickness of 7 mm, and a hard elastomer 34a made of silicone rubber with an Asker C hardness of 35° and a thickness of 5 mm were adhered to the base material 32.

[0051] The thickness of the terminal member 21 is 0.64 mm, and the thickness 2 mm obtained by subtracting the thickness of the hard elastic body 34a from the thickness of the soft elastic body 33a when no pressure is applied is 3.1 times the plate thickness of the terminal member 21.

[0052] 4(b), the backup belt 31b of Comparative Example 1 was configured such that the entire back surface side of the terminal member 21 was covered with a hard elastic body 34b made of silicone rubber having an Asker C hardness of 35°. That is, the backup belt 31b used was configured such that the hard elastic body 34b made of silicone rubber having an Asker C hardness of 35° was bonded to the entire surface of the same base material 32 as in Example 1.

[0053] In both Example 1 and Comparative Example 1, the plating conditions were adjusted so that the thickness of the Au plating film on the terminal portion 23 of the plating surface, which is the portion requiring plating, was the same, and a partially plated product was produced by forming the Au plating film.

[0054] When the thickness of the Au plating film on the side surface of the punched portion by press working (cross section of terminal portion 23) and the back surface of terminal portion 23 of the partially plated product of Example 1 was measured with a fluorescent X-ray thickness meter, it was found that only a small amount of plating had adhered to the side surface of terminal portion 23, and no Au plating had adhered to the back surface of terminal portion 23. Similarly, when the thickness of the Au plating film of the partially plated product of Comparative Example 1 was measured, it was found that the same amount of Au plating had adhered to almost the entire surface of the side surface of terminal portion 23 as to the front surface of terminal portion 23, and a small amount of Au plating had adhered to the back surface of terminal portion 23. In other words, it was confirmed that the present invention can significantly reduce the amount of Au adhesion to the parts where Au plating is not required.

[0055] [Example 2, Example 3, Comparative Example 2] Except for changing the width of the band-shaped soft elastomer 33 and hard elastomer 34 of the backup belt 31 and the portion covering the terminal portion 23 from the back side of the terminal member 21, a test was conducted in the same manner as in Example 1, in which Ni plating was applied as the base plating and Au plating was applied as the main plating to the terminal member 21 in which the terminal portion 23 was formed by pressing a rolled brass material (C2600R-H).

[0056] The backup belt 31c of Example 2 was the same as that of Example 1, except that the width of the soft elastic body 33c was changed to a width that covered the entire terminal portion 23 and the lower support portion 25, as shown in FIG. 5(a), and the remaining portions were made of a hard elastic body 34c.

[0057] The backup belt 31d of Example 3 was the same as that of Example 1, except that the width of the soft elastomer 33d was changed to a width that covered only the tip portion, which is a part of the terminal portion 23, as shown in Figure 5 (b), and the other areas where the soft elastomer 33d is not located were made of a hard elastomer 34d.

[0058] The backup belt 31e of Comparative Example 2 was similar to that of Example 1, except that, as shown in FIG. 5(c), the soft elastic body 33e was not placed in the area that may come into contact with the terminal portion 23, but was placed only in the area that comes into contact with the lower support portion 25 from the rear surface side of the terminal member 21, and the other areas were made of hard elastic body 34e.

[0059] When the partially plated product of Example 2 was observed in the same manner as in Example 1, it was found that only a small amount of plating had adhered to the side surface of terminal portion 23, and no Au plating had been observed on the back surface of terminal portion 23. Furthermore, when the partially plated product of Example 3 was observed, it was found that only a small amount of plating had adhered to the side surface at the tip portion of terminal portion 23, and no Au plating had been observed on the back surface at the tip portion of terminal portion 23. Similarly, when the partially plated product of Comparative Example 2 was observed, it was found that Au plating had adhered to almost the entire surface of the side surface and back surface of terminal portion 23.

[0060] As described above, in all of Examples 1, 2, and 3, it was possible to reduce contact of the Au plating solution with the unnecessary parts (side and back surfaces of terminal portion 23) that are not the surfaces to be plated, and to reduce the amount of Au plating adhesion, compared to Comparative Examples 1 and 2. In particular, Example 2 was able to reduce the amount of Au adhesion the most. In Comparative Examples 1 and 2, the part that presses terminal portion 23 is hard elastic body 34c, so adhesion of Au plating solution to the side surfaces of terminal portion 23 was unavoidable.

[0061] [Examples 4, 5, and 6] Partially plated products were produced in the same manner as in Example 1, except that the soft elastic bodies 33 used had Asker C hardnesses of 5° (Example 4), 10° (Example 5), and 15° (Example 6).

[0062] The partially plated products of Examples 4, 5, and 6 were observed in the same manner as in Example 1. As a result, in all of the partially plated products, the adhesion of Au plating to the side surface of terminal portion 23 was slight, and the amount of adhesion to the side surface was reduced compared to Comparative Examples 1 and 2, and no Au plating adhesion was observed on the back surface of terminal portion 23. In other words, it was confirmed that the amount of Au adhesion can be significantly reduced by the present invention. [Industrial Applicability]

[0063] The present invention can be applied to continuous partial plating using a drum-type jig. [Explanation of symbols]

[0064] 1 Partial plating equipment 2. Material transport roll 3 Backup belt transport roll 11 Drum-type jig 13 Opening 14 Au plating solution jetting device 21 Terminal material 23 Terminal section 23a Plated surface 23b Back side 31 Backup Belt 32 Base material 33 Soft elastic body 34 Hard elastic body

Claims

1. A selective plating apparatus using a drum-type jig, a backup belt for pressing a workpiece made of a terminal member against the cylindrical surface of the drum-type jig; the cylindrical surface of the drum-type jig is provided with an opening for supplying a plating solution to the surface to be plated of the terminal member; the backup belt has a base material and a soft elastic body disposed on one surface of the base material for pressing the terminal portion of the terminal member from a back surface side opposite to a surface to be plated against the cylindrical surface of the drum-type jig; The selective plating apparatus is characterized in that the soft elastic body has an Asker C hardness of 0.5° to 25°.

2. 2. The selective plating apparatus according to claim 1, further comprising a hard elastic body having a higher Asker C hardness and a smaller thickness than the soft elastic body in an area on one surface of the base material where the soft elastic body is not disposed.

3. 3. The selective plating apparatus according to claim 2, wherein the hard elastic body has an Asker C hardness of 35 degrees or more.

4. 3. The selective plating apparatus according to claim 1, wherein the soft elastic body is made of synthetic rubber.

5. 3. The selective plating apparatus according to claim 1, wherein the soft elastic body is mainly composed of one or more synthetic rubbers selected from the group consisting of silicone rubber, ethylene propylene diene rubber, and nitrile rubber.

6. 4. The selective plating apparatus according to claim 2, wherein the difference between the thickness of said soft elastic body and the thickness of said hard elastic body is equal to or greater than the plate thickness of said workpiece.

7. 3. The selective plating apparatus according to claim 1, wherein the soft elastic body has a width sufficient to cover the entire terminal portion of the terminal member.

8. A method for partial plating of a terminal member, comprising the steps of pressing a workpiece to be plated, which is a terminal member, against a cylindrical surface of a drum-type jig by a backup belt to bring the workpiece into intimate contact with the cylindrical surface, and supplying a plating solution to a terminal portion of the terminal member through an opening formed in the drum-type jig to form a plating on the surface to be plated of the terminal portion, The backup belt has a base material and a soft elastic body having an Asker C hardness of 0.5° to 25° and disposed on one surface of the base material, A selective plating method, characterized in that at least the terminal portion of the terminal member is pressed from the back surface side opposite the plated surface on which plating is formed of the terminal member by the soft elastic body, and the terminal member is closely attached to the cylindrical surface of the drum-shaped jig for plating.

9. 9. The selective plating method according to claim 8, wherein a hard elastic body having a higher Asker C hardness and a smaller thickness than the soft elastomer is provided in an area on one surface of the base material where the soft elastomer is not provided.

10. 10. The selective plating method according to claim 9, wherein the hard elastic body has an Asker C hardness of 35° or more.

11. 10. The selective plating method according to claim 8, wherein the soft elastic body is a synthetic rubber.

12. 10. The selective plating method according to claim 8, wherein the soft elastic body is mainly composed of one or more synthetic rubbers selected from the group consisting of silicone rubber, ethylene propylene diene rubber, and nitrile rubber.

13. 11. The selective plating method according to claim 9, wherein a difference between a thickness of the soft elastic body and a thickness of the hard elastic body is equal to or greater than a plate thickness of the workpiece.

14. 10. The selective plating method according to claim 8, wherein the entire terminal portion of the terminal member is pressed from a rear surface side of the terminal member by the soft elastic body.

Citation Information

Patent Citations

  • Partially plating method

    JP1990097692A

  • Rotary drum type radial plating device

    JP1999131284A

  • Spot plating device

    JP2013216937A

  • Method and apparatus for plating terminal member, and terminal member

    JP2015108186A