Analysis device and electrolyte concentration measuring method

The analytical device with separate hydrophilic and hydrophobic channel regions in microanalytical chips addresses chloride ion diffusion issues, ensuring stable potential measurements for accurate electrolyte concentration determination.

JP2024163046APending Publication Date: 2024-11-21CANON KK

Patent Information

Application Number
JP2024073960
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-10
Filing Date
2024-04-30
Publication Date
2024-11-21

AI Technical Summary

Technical Problem

The challenge in microanalytical chips for electrochemical analysis is the diffusion of chloride ions from the reference electrode to the working electrode, affecting the accuracy of potential difference measurements due to the interconnected flow paths, which is exacerbated by the need for conditioning solutions that further disrupt the ion concentration.

Method used

The analytical device features separate hydrophilic or porous channel regions surrounded by a hydrophobic channel wall, with the reference electrode in one region and the working electrode in another, preventing backflow of chloride ions and ensuring stable potential measurements by maintaining electrical continuity through controlled sample introduction.

Benefits of technology

This configuration stabilizes the potential difference measurement by preventing chloride ion backflow, allowing for accurate electrolyte concentration determination without extending measurement time or device size, enhancing the device's usability in resource-limited settings.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024163046000001_ABST
    Figure 2024163046000001_ABST
Patent Text Reader

Abstract

To solve the problem in which: during conditioning of an electrode and in potential difference ion concentration measurement, CI ion crystals arranged to stabilize the electric potential of a reference electrode flow back to a working electrode, which affects the electric potential of the working electrode.SOLUTION: An analysis device has a hydrophilic or porous flow channel area surrounded by a hydrophobic flow channel wall provided inside or on a base material, and has a first flow channel area and a working electrode. The first flow channel area has a reference electrode provided on the base material. The working electrode is outside the first flow channel area.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an analytical device and a method for measuring the concentration of an electrolyte using the analytical device. [Background technology]

[0002] In recent years, microanalysis chips that utilize micro-sized fine flow channels to efficiently perform biochemical analysis within a single chip have been attracting attention in a wide range of fields, including biochemistry research, medicine, drug discovery, healthcare, the environment, and food.

[0003] In the early 1990s, photolithography and molds were used to form micron-sized fine flow channels on glass or silicon, and microanalysis chips were developed that could perform sample pretreatment, stirring, mixing, reaction, and detection on a single chip. As a result, the miniaturization of testing systems, rapid analysis, and reduction in specimens and waste liquids were achieved.

[0004] Electrochemical analysis measures the potential between electrodes immersed in a sample to be analyzed, and is widely used in the fields of medicine and the environment. Traditionally, electrochemical analysis is performed by engineers using advanced equipment. Therefore, the fields and resources in which measurements can be performed are somewhat limited in order to use electrochemical analysis. Therefore, there is a need for inexpensive, easy-to-use, disposable microanalysis chips for electrochemical analysis, for use in medical activities in developing countries and remote areas with poor medical facilities, as well as in disaster sites, and in airports where the spread of infectious diseases must be stopped at the border.

[0005] In electrochemical analysis, such as quantifying electrolyte ions in a solution, a stable reference electrode capable of maintaining a constant potential is required. Conventional glass reference electrodes are expensive and cannot be miniaturized because they require an internal liquid. They are also difficult to handle, as they require storage in a concentrated ion solution.

[0006] Patent Document 1 proposes a system including a microanalysis chip capable of measuring potential differences using a porous substrate, enabling electrochemical measurements that are low-cost, easy to handle, and easy to dispose of. This microanalysis chip includes one or more working electrodes and one reference electrode on a porous substrate. In such a microanalysis chip, both electrodes must be electrically connected by a fluid during measurement. Patent Document 1 describes that in order to obtain a stable potential at the reference electrode during measurement, a highly concentrated aqueous solution of KCl is used as the reference solution, and the reference solution is introduced into a reference region including the reference electrode.

[0007] In addition, Non-Patent Document 1 proposes a filter paper-based Na ion and K ion concentration measurement device. This device has an inlet for introducing a sample, and the introduced sample permeates from the inlet into the working electrode and the reference electrode. Furthermore, Non-Patent Document 1 proposes a device in which KCl ion crystals are deposited on the reference electrode to stabilize the potential of the reference electrode. During measurement, KCl dissolves into the sample, thereby maintaining a high concentration of Cl ions in the reference electrode area, and a stable reference electrode potential can be obtained. [Prior art documents] [Patent documents]

[0008] [Patent Document 1] US Patent Application Publication No. 2016033438 [Non-patent literature]

[0009] [Non-Patent Document 1] Nipapan Ruecha, Orawon Chailapakul, Koji Suzuki and Daniel Citterio “Fully Inkjet-Printed Paper-Based Potentiometric Ion-Sensing Devices” Analytical chemistry August 29, 2017 Published, 89, pp.10608-10616 Summary of the Invention [Problem to be solved by the invention]

[0010] During measurement, the reference electrode and working electrode need to be electrically connected by the sample. However, during this process, Cl ion crystals on the reference electrode dissolve and diffuse into the working electrode area through the sample, affecting the potential of the working electrode and reducing the accuracy of the potential difference measurement.

[0011] In order to perform measurements with higher accuracy, it is preferable to condition the working electrode and the reference electrode with an aqueous electrolyte solution before performing electrolyte measurements. Ion exchange resins are generally conditioned before use for the purpose of removing impurities, etc. It is also considered that the detection accuracy can be improved for working electrodes having an ion selective membrane by introducing a conditioning solution containing ions that pass through the ion selective membrane in advance and passing the ions through the ion selective membrane. Conditioning the reference electrode also dissolves ion crystals containing Cl, making them easier to reach the reference electrode during measurement.

[0012] For this reason, it is important to condition the working and reference electrodes before measuring the sample in order to improve the measurement accuracy. However, in the above-mentioned device, the reference and working electrodes are connected by a flow path, so the conditioning solution used and Cl ion crystals such as KCl on the reference electrode dissolved by the conditioning solution may diffuse into the working electrode area and recrystallize around the working electrode. Therefore, during measurement, the crystals around the working electrode that are backflowed may dissolve in the sample, resulting in a higher electrolyte concentration than the actual concentration of the sample, which reduces the accuracy of the potential difference measurement.

[0013] The present invention aims to provide a microanalysis chip that can suppress the influence on the working electrode of backflow of Cl ion crystals arranged around the reference electrode and of the conditioning solution itself that occurs during measurement and conditioning, without changing the size of the device or extending the measurement time, thereby enabling stable ion concentration measurement. [Means for solving the problem]

[0014] An analytical device having a hydrophilic or porous flow region surrounded by a hydrophobic flow wall disposed in or on a substrate, the analytical device having a first flow region and a working electrode; the first flow region has a reference electrode disposed on the substrate; The working electrode is outside the first flow region. An analytical device is provided. Effect of the Invention

[0015] During electrolyte measurement, before the ion-selective membrane of the working electrode stabilizes and the measurement is completed, the solution introduced onto the reference electrode, or the saturated ionic liquid created by placing Cl ion crystals or the like on the reference electrode, may flow back to the working electrode. In the analytical device according to the embodiment of the present invention, the regions where the reference electrode and the working electrode are provided are separated by a flow path wall. Therefore, it is possible to perform conditioning by permeating the solution only into each of them. During measurement, the working electrode and the reference electrode can be electrically connected by introducing a sample. As a result, a stable potential value can be obtained before the crystals placed in the region where the reference electrode is provided flow back to the working electrode, or before the conditioning solution for the reference electrode reaches the working electrode. [Brief description of the drawings]

[0016] [Figure 1] FIG. 2 is a top view of the analytical device in Example 1. [Diagram 2] FIG. 2 is a cross-sectional view taken along the dashed line in FIG. [Diagram 3] Schematic diagram of the shape of a droplet of liquid dropped onto a channel wall. [Figure 4] FIG. 2 is an image diagram of conditioning in Example 1. [Diagram 5] FIG. 2 is an image diagram of pre-measurement sample introduction in Example 1. [Figure 6] FIG. 2 is an image diagram of a method for introducing a sample into an introduction portion during measurement in Example 1. [Figure 7] FIG. 2 is a top view of an analytical device in Comparative Example 1. [Figure 8] FIG. 1 is an image diagram of conditioning in Comparative Example 1. [Figure 9] FIG. 1 is an image diagram of a sample introduction method in Comparative Example 1. [Figure 10] FIG. 4 is a sequence diagram of potential difference measurement in Comparative Example 1. [Figure 11] FIG. 4 is a sequence diagram of potential difference measurement in the first embodiment. [Figure 12A] FIG. 11 is a top view of the analytical device in Example 2 with a restriction member 30 removed. [Figure 12B]FIG. 11 is a top view of the analytical device in Example 2. [Figure 13] FIG. 13 is an image diagram of conditioning in Example 2. [Figure 14] FIG. 11 is an image diagram of sample introduction into an introduction portion during measurement in Example 2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0017] The analytical device according to the present invention for solving the above-mentioned problems will be described below with reference to the drawings. Note that the following embodiments are merely examples, and the present invention is not limited to the contents of the embodiments. In addition, in the following drawings, components that are not necessary for the description of the embodiments may be omitted.

[0018] The first embodiment of the present invention is An analytical device having a hydrophilic or porous flow region surrounded by a hydrophobic flow wall disposed in or on a substrate, the analytical device having a first flow region and a working electrode; the first flow region has a reference electrode disposed on the substrate; The working electrode is outside the first flow region. It is an analytical device.

[0019] In this embodiment, one of the first flow path regions may include two or more of the working electrodes.

[0020] A second embodiment of the present invention is An analytical device having a hydrophilic or porous flow region surrounded by a hydrophobic flow wall disposed in or on a substrate, the analytical device having a first flow region and a working electrode; the first flow region has a reference electrode disposed on the substrate; The working electrode is outside the first flow region. 1. An analytical device comprising: A second flow region; the second flow region includes the working electrode disposed on the substrate; The first flow path region and the second flow path region are separated from each other by the flow path wall. The aforementioned analytical device.

[0021] In this embodiment, two or more second flow path regions can be included for one first flow path region.

[0022] In this embodiment, a portion of each of the first flow path region and the second flow path region is within a distance L from each other, and L can be equal to or less than the diameter of a droplet of the sample to be introduced. Furthermore, a region including a circle having a diameter L including a part of each of the first and second flow path regions and a part of the flow path wall separating them can be used as a measurement introduction section for introducing a specimen during measurement. Alternatively, each of the first and second flow path regions can further have an introduction section. This introduction section can be used to introduce a conditioning solution or a specimen before measurement.

[0023] In order to enable the tester to know that the measurement introduction part is where the sample is introduced during measurement, and that the introduction parts are where the conditioning solution or sample is introduced before measurement, it is possible to mark the relevant parts or to attach a device cover with holes to the relevant parts.

[0024] A third embodiment of the present invention is a method for measuring an electrolyte concentration using the analytical device according to the second embodiment, This is an electrolyte concentration measurement method in which a sample is introduced into the measurement introduction section, thereby establishing electrical continuity between the first flow path region and the second flow path region, and measuring the potential difference generated between the first and second electrodes due to the difference between a reference ion concentration in the first region and an ion concentration derived from the sample in the second region.

[0025] In this embodiment, before introducing the specimen into the measurement introduction section, a first conditioning solution containing chloride ions can be introduced into the first flow path region, a second conditioning solution containing ions to be detected by the working electrode can be introduced into the second flow path region, or the specimen can be introduced into the second region. A combination of these may be performed.

[0026] A fourth embodiment of the present invention is An analytical device having a hydrophilic or porous flow region surrounded by a hydrophobic flow wall disposed in or on a substrate, the analytical device having a first flow region and a working electrode; the first flow region has a reference electrode disposed on the substrate; The working electrode is outside the first flow region. 1. An analytical device comprising: The first flow region and a portion of the working electrode are within a distance L of each other, where L is less than or equal to the diameter of a droplet of analyte to be introduced into the analytical device.

[0027] In this embodiment, a region including a circle having a diameter L including a part of each of the first flow path region and the coating membrane and a part of the flow path wall separating them can be used as a measurement introduction part for introducing a specimen during measurement, and each of the first flow path region and the working electrode can further have an introduction part. This introduction part can be used to introduce a conditioning solution or a specimen before measurement.

[0028] A fifth embodiment of the present invention is a method for measuring an electrolyte concentration using the analytical device according to the fourth embodiment, This is an electrolyte concentration measurement method in which a sample is introduced into the measurement introduction section, thereby establishing electrical continuity between the first flow path region and the working electrode, and measuring the potential difference between the reference electrode and the working electrode, which is caused by the difference between the reference ion concentration in the first region and the ion concentration derived from the sample at the working electrode.

[0029] In this embodiment, before introducing the sample into the measurement introduction section, a first conditioning solution containing chloride ions can be introduced into the first flow path region, a second conditioning solution containing ions to be detected by the working electrode can be introduced into the working electrode, or the sample can be introduced into the working electrode. A combination of these may be performed. EXAMPLES

[0030] [Example 1] <Flow path configuration> The analytical device P1 of Example 1 will be described with reference to FIGS. 1 and 2, which are schematic diagrams. FIG. 1 is a simplified top view of an analytical device P1, and FIG. 2 is a simplified cross-sectional view of the analytical device P1 taken along a dashed dotted line in FIG.

[0031] The analytical device P1 of this embodiment uses a porous substrate as a substrate, and is an analytical device having a flow region surrounded by a flow wall 5 made of a hydrophobic resin inside the porous substrate, and has a first flow region 1 and a working electrode 9 including a base electrode 9a as a working electrode and a coating film (ion-selective 8 in this embodiment) containing a compound having ion selectivity covering the base electrode 9a, the first flow region 1 has a reference electrode 7 provided on the porous substrate, and the working electrode 9 is outside the first flow region 1. Furthermore, the analytical device of this embodiment has a second flow region 2, the second flow region has the above-mentioned working electrode 9 provided on the porous substrate, and the first flow region 1 and the second flow region 2 are separated from each other by a flow wall 5.

[0032] In this embodiment, a hydrophobic resin was placed on a paper porous substrate S1 having a thickness T1 = 0.1 mm and a porosity of 50%, and then thermally fixed to form a flow path pattern as a flow path wall 5 that is impermeable to samples.

[0033] The flow pattern includes a first flow region 1 containing a reference electrode 7 and a second flow region 2 containing a working electrode 9 .

[0034] In the figure, the first flow path region includes a flow path chamber 1a including a reference electrode 7 and an ion crystal 6, a flow path 1b, and a proximity portion 1c, but the shape of the first flow path region is not limited to this. In this embodiment, the first flow path region 1 further includes a flow path chamber 3 including a contact portion of the reference electrode 7, but the flow path chamber 3 may be omitted.

[0035] Similarly, the second flow path region 2 includes a flow path chamber 2a including the working electrode 9, and a flow path 2b and a nearby portion 2c, but the shape of the second flow path region is not limited to this. In this embodiment, the second flow path region 2 further includes a flow path chamber 4 including a contact portion of the base electrode 9a of the working electrode 9, but the flow path chamber 4 may be omitted.

[0036] In this embodiment, adjacent portion 1c, which is the region of first flow path region 1 closest to second flow path region 2, and adjacent portion 2c, which is the region of second flow path region 1 closest to first flow path region 1, are adjacent to each other at a distance L1. L1 is preferably a distance at which a sample introduced into the introduction portion during measurement touches both adjacent portion 1c and adjacent portion 2c, and in this embodiment, L1 was set to 1 mm.

[0037] It is preferable that the distance L1 between adjacent portions 1c and 2c is equal to or less than the diameter of the droplet of the specimen to be introduced. Figure 3 shows a simplified diagram of a droplet of the specimen dropped onto a channel wall 5. The diameter of the droplet of the specimen dropped onto the channel wall 5 is 2r1, its height is h1, its volume is V1, and its contact angle is θ1. If we assume that the droplet is a part of a sphere, then equation (1) can be obtained from the A half-angle method, which is generally used to measure contact angles.

number

number

number

number

[0038] In this embodiment, θ1=89.4°, V1=10 μL, and therefore 2r1=7.29 mm, and therefore L1 was set to 1 mm. In addition, in this embodiment, a paper-made material is used as the porous substrate, but the present invention is not limited thereto. The porous substrate may have a suitable porosity and generate a capillary phenomenon in the liquid, and may have a porous structure such as a mesh-like structure, such as open bubbles and nanofibers, inside, and may be made of resin, glass, an inorganic substrate, fabric, metal paper, or the like. The porosity may be appropriately selected depending on the purpose, but is preferably 20% to 90%. If the porosity exceeds 90%, the substrate may not be able to maintain its strength, and if it is less than 20%, the permeability of the sample liquid may be deteriorated.

[0039] Porosity (%) is Porosity (%) = (true density - apparent density) / true density x 100 It is calculated as follows.

[0040] Apparent density (g / cm 3 )teeth, Apparent density (g / cm 3 ) = basis weight (g / m 2 ) / thickness(mm)×1000 It is calculated from:

[0041] The hydrophobic resin forming the flow path wall is not particularly limited, and examples thereof include polyester resin, vinyl resin, acrylic resin, styrene-acrylic resin, polyethylene, polypropylene, polyolefin, ethylene-vinyl acetate copolymer resin, and ethylene-acrylic acid copolymer resin.

[0042] As a method for disposing the hydrophobic resin, a thermoplastic hydrophobic resin is applied to the surface of the porous substrate using an electrophotographic device to form a flow path pattern, and is melted by heat to penetrate into the porous substrate. In this case, a preferred example of the thermoplastic resin is toner particles. For this method, refer to JP-A-2021-37612. The hydrophobic resin may be disposed by a method such as forming it with an inkjet printer or a wax printer, in addition to using an electrophotographic device.

[0043] In this embodiment, the toner particles are arranged as a hydrophobic resin, and then the flow path pattern is formed by thermal fixing.

[0044] In this embodiment, the adjacent portion 1c of the first flow path region 1 is the region closest to the second flow path region 2, but this is not limited to this. The adjacent portion 1c may be within the first flow path region 1 and may be within a range in which the electrolyte concentration measurement function of the reference electrode 7 is not lost, and the adjacent portion 2c may be within the second flow path region 2 and may be within a range in which the electrolyte concentration measurement function of the working electrode 9 is not lost. In addition, the distance between adjacent portions 1c and 2c is 1 mm, but this is not limited to this and may be within a range in which measurement is possible using the electrolyte concentration measurement method described later.

[0045] <Electrode formulation> The formulation of the electrodes used in this example will be described. The first flow path region 1 has a reference electrode 7 using Ag / AgCl. In this embodiment, an example is shown in which the reference electrode 7 is composed only of a base electrode. The reference electrode 7 has a shape in which the electrode extends continuously from the first flow path region 1 onto the flow path wall 5 as a contact point during measurement. In addition, 2.5 mg of NaCl ion crystals 6 were placed upstream of the reference electrode 7 in the first flow path region 1.

[0046] On the other hand, the second flow path region 2 was provided with a base electrode 9a of the working electrode 9 using PEDOT:PSS (a dispersion of polyethylenedioxythiophene and polystyrenesulfonic acid). The base electrode 9a was formed so that the electrode extended continuously from within the second flow path region 2 onto the flow path wall 5. In addition, within the second flow path region 2, an ion-selective membrane 8 that selects Na was formed as a coating material containing a compound having ion selectivity so as to cover the base electrode 9a. The ion-selective membrane 8 contained 3 wt% of Bis(12-crown-4) as a compound having ion selectivity, and potassium tetrakis(4-chlorophenyl)borate as an anion rejector. The ion selective membrane 8 was formed from a composition containing 3 wt% of the above Bis(12-crown-4), 0.5 wt% of potassium tetrakis(4-chlorophenyl)borate, 64 wt% of O-nitrophenyl octyl ether, and 32.5 wt% of polyvinyl chloride. In this manner, a working electrode including a base electrode 9a and the ion selective membrane 8 covering the base electrode was produced.

[0047] In this embodiment, the reference electrode 7 and the working electrode 9 are formed with the above-mentioned shapes and materials, but are not limited thereto. The reference electrode 7 only needs to receive a solution of a constant concentration at the time of measurement, and the ion crystals 6 do not need to be arranged if a saturated ion liquid is introduced into the second flow path region 2 during measurement. The material of the ion crystals 6 only needs to contain Cl ions, and is not limited to NaCl. The mass of the ion crystals 60 to be arranged is not limited to the above, and only needs to be in a range that results in a saturated solution when the Cl ion crystals are dissolved in pure water having a volume equivalent to the volume of the first flow path region 1. In this embodiment, the location of the ion crystals is formed upstream of the reference electrode in the flow path A, but is not limited thereto, and may be covered on the top of the reference electrode.

[0048] The base electrode may be made of Ag / AgCl, PEDOT / PSS, or carbon, without any particular limitation. For the preparation of an electrode using Ag / AgCl or carbon, see, for example, Patent Document 1. For the preparation of an electrode using PEDOT / PSS, see, for example, Non-Patent Document 1. For the base electrode, an electrode that matches the required characteristics of the device, such as cost and performance, may be selected.

[0049] The coating material containing a compound having ion selectivity may be any commonly used coating material that has sensitivity to the target ion and sufficient selectivity to interfering ions. The coating material containing a compound having ion selectivity is specifically an ion-selective membrane. The compound having ion selectivity is not particularly limited, but preferably includes ionophores and anion removers that show ion selectivity. An example of the ionophore is 12-crown 4-ether having a crown ether structure, and an example of the anion remover is sodium tetraphenylborate (NaTPB). Any known material can be used for the ion-selective membrane, and for such materials, see pages 138 to 140 of "I want to measure ion concentration with an electrode" by Dojindo Laboratories, Ltd.

[0050] The ion-selective membrane may contain a polymeric compound to maintain its structure. Examples of the polymeric compound include polyvinyl chloride (abbreviation: PVC) and a copolymer of vinyl chloride and vinyl acetate. The ion-selective membrane may contain a plasticizer to make the ionophore operable. Although known plasticizers can be used, lipophilic ion exchange materials that act as lipophilic ion exchange in the ion-selective membrane are more preferable. Examples of known materials include 2-nitrophenyl octyl ether (abbreviation: NPOE), bis(2-ethylhexyl) sebacate (abbreviation: DOS), bis(2-ethylhexyl) adipate (abbreviation: DOA), and di-n-octylphenyl phosphonate (abbreviation: DOPP).

[0051] The above-mentioned components are mixed in appropriate amounts, dissolved or dispersed in a solvent such as THF or cyclohexanone, and the resulting liquid is applied, for example, by an inkjet method, onto a base electrode (Ag / AgCl electrode) on which an intermediate layer such as NaCl is laminated. The ion selective membrane 8 can be produced by this method. Note that the method for applying the ion selective membrane 8 is not limited to the inkjet method, and a dispenser, screen printing, or the like can also be used as appropriate. The viscosity of the solution can be adjusted according to each application method, and then the ion selective membrane can be laminated on the base electrode.

[0052] <Conditioning> The conditioning refers to a process of permeating the first flow path region and the second flow path region with an appropriate solution before measuring a sample, for the purpose of increasing the measurement accuracy. The conditioning carried out in this example will be described with reference to FIG.

[0053] Conditioning was performed prior to the measurement. In this example, the inlet portion was an inlet portion 10 in the first flow path region 1 and an inlet portion 11 in the second flow path region 2. The inlet portion 10 and the inlet portion 11 may be located within the first flow path region 1 and the second flow path region 2, respectively. The inlet portion 10 may be located above the reference electrode 7 or above the ion crystal 6 as long as it does not contact the second flow path region 2, and the inlet portion 11 may be located above the ion selective membrane 8 as long as it does not contact the first flow path region 1.

[0054] 10 μL of a 3 mol / L aqueous solution of NaCl was used as the conditioning liquid S2 to be introduced into the first flow path region 1. Also, 10 μL of a 1 mmol / L aqueous solution of NaCl was used as the conditioning liquid S3 to be introduced into the second flow path region 2. After being introduced into each introduction part, the conditioning liquid permeated into the flow paths of the first flow path region 1 and the second flow path region 2.

[0055] In this embodiment, the conditioning liquid S3 used was a solution of the above composition, but is not limited to this as long as it is a material containing ions that pass through the ion selective membrane 8 used. Also, in this embodiment, the conditioning liquid S2 used was the above solution, but is not limited to this as long as it is measurable.

[0056] An example of conditioning the first region including the reference electrode is to introduce an aqueous solution containing Cl ions, more specifically, an aqueous solution containing NaCl or KCl, which dissolves ionic crystals containing Cl, making them easier to reach the reference electrode during measurement.

[0057] An example of conditioning the second region comprising the working electrode is to preliminarily introduce a conditioning solution containing ions that pass through the ion selective membrane. Also, the sample itself can be introduced prior to the measurement (pre-measurement sample introduction), which is also an aspect of conditioning. In this example, as described below, a specimen was introduced into the second region equipped with the working electrode 9 before measurement (pre-measurement specimen introduction). At this time, introduction section 12 in the second flow path region 2 shown in Fig. 5 was used. Note that pre-measurement specimen introduction is also an aspect of conditioning.

[0058] In this embodiment, both the conditioning and the pre-measurement sample introduction were performed twice for the second region, but both may be performed, or only one of them may be performed. Also, for each, different introduction parts may be provided (i.e., introduction part 11 and introduction part 12 may be different), or a common introduction part may be used (i.e., introduction part 11 and introduction part 12 may be the same or overlap).

[0059] That is, in this embodiment, in addition to the above-mentioned conditioning, 30 μL of the specimen was dropped into the introduction section 12 as a pre-measurement specimen introduction. After introduction, the specimen spreads in the second flow path region 2 by capillary action and reaches the ion selective membrane 8. When the specimen reaches the ion selective membrane 8, the ions in the specimen are taken into the ion selective membrane and react with the working electrode 9. However, at this point, the first flow path region 1 and the second flow path region 2 were not electrically connected.

[0060] <Measurement> Thirty seconds after the introduction of the first sample, 10 μL of the sample was dropped into the measurement introduction section 13 (introduction of the second sample). Since the measurement introduction section includes a part of the first flow path region 1 and a part of the second flow path region 2, after the second sample was introduced into the measurement introduction section 13, the sample spreads in the first flow path region 1 by capillary action, and the first flow path region 1 and the second flow path region 2 were electrically connected by the sample dropped into the measurement introduction section 13. While the sample dropped at the time of the second sample introduction permeates the first flow path region 1, the ions contained in the sample dropped at the time of the first sample introduction are selected by the ion selective membrane 8, and the measurement potential of the working electrode required for electrolyte concentration measurement is stabilized. After that, when the sample dropped into the measurement introduction section dissolves the ion crystal 6 and reaches the reference electrode 7, the concentration of the sample can be measured, and the measurement of the sample is completed at the specified measurement time.

[0061] In this embodiment, by delaying the timing of the introduction of the second specimen compared to the introduction of the first specimen, the specimen penetrates into the reference electrode 7 after it reaches the ion selective membrane and is ion-selected. This makes it easier to achieve a stable state of the potential of the working electrode when the specimen dropped in the second specimen introduction reaches the reference electrode 7.

[0062] [Comparative Example 1] In order to explain the effect of Example 1 in more detail, Comparative Example 1 will be given. <Flow path configuration> 7 shows a schematic diagram of the analytical device according to Comparative Example 1. In this comparative example, the configuration of the analytical device is the same as that of Example 1, except that the first and second flow path regions are not provided, and the reference electrode 7 and the working electrode 9 are provided in a single flow path region 14.

[0063] <Conditioning method> The conditioning method performed in this comparative example will be described with reference to FIG. As in Example 1, conditioning was performed before the measurement of the electrolytic concentration. In this comparative example, as in Example 1, two inlet parts, an inlet part 15 and an inlet part 16, were provided. As the conditioning liquid S2 acting on the reference electrode and the ion crystals, 10 μL of a 3 mol / L aqueous solution of NaCl was used and dropped into the inlet part 15. As the conditioning liquid S3 acting on the ion selective membrane, 10 μL of a 1 mmol / L aqueous solution of NaCl was used and dropped into the inlet part 16. At this time, both conditioning liquids permeated the single flow path region 14 and were mixed in the single flow path region 14. In addition, when the conditioning liquid reached the ion crystals 6, not only the conditioning liquid in contact with the reference electrode 7, but also ions derived from the ion crystals may flow back through the conditioning liquid to the region of the working electrode 9.

[0064] <Measurement of sample concentration> The measurement of the specimen concentration performed in this comparative example will be described with reference to FIG. In this comparative example, since there is only one flow path region, there is no measurement introduction section (including a part of each of the first flow path region and the second flow path region, and a part of the flow path wall separating them).

[0065] The specimen was introduced from introduction portion 17 and introduction portion 18. The specimen introduced into introduction portion 17 permeated into reference electrode 7 and introduction portion 18 in flow path chamber 1a, and the specimen introduced into introduction portion 18 permeated into working electrode 9 and introduction portion 17 in flow path chamber 2a at the same time, and after a certain time, reached reference electrode 7 and working electrode 9. The specimen that permeated into reference electrode 7 dissolves ion crystals 6 containing Cl, as in Example 1, and becomes a Cl ion solution of saturated concentration, which reacts with reference electrode 7. On the other hand, when the specimen reaches the working electrode 9, ions contained in the specimen are selected by the ion selective membrane 8. However, the specimen fills the entire flow path chamber 1a, leaving no area for the specimen to permeate, and so a flow occurs from the reference electrode side to the introduction part 18 side where the specimen has already permeated. As a result, the saturated concentration Cl solution (NaCl solution in this comparative example) flows back toward the working electrode side.

[0066] <Effects of Example 1 when measuring specimen concentration> Regarding the time advantage of sample measurement, an image diagram showing the behavior of the sample after introduction in Comparative Example 1 is used in FIG. 10, and an image diagram showing the behavior of the sample after introduction in Example 1 is used in FIG. 11.

[0067] In Comparative Example 1, the specimen was introduced into the introduction section 17 and then reached the reference electrode 7 or the working electrode 9. After the specimen reached both electrodes, the potential on the measurement working electrode side stabilized, and it took a certain amount of time from the start of potential difference measurement to the completion of the measurement. In addition, after the specimen reached the reference electrode, it dissolved the NaCl crystals provided on the upper part of the reference electrode, became a saturated NaCl solution, and proceeded to permeate into the unpermeated area in the first flow path area, filling the flow path chamber 1a. After that, the flow to the unpermeated area became gentle, and the specimen that became a saturated NaCl solution began to flow back toward the working electrode side, and a high concentration of the specimen reached the working electrode. In this Comparative Example, the measurement target was K ions, but some Na ions also passed through the K ion-selective selective membrane, and the presence of high concentrations of Na affected the measurement.

[0068] In Example 1, the specimen introduced into the introduction section 12 as the pre-measurement specimen introduction reached the working electrode 9. After the specimen reached the working electrode 9, the specimen was dripped into the measurement introduction section at the timing when the potential on the measurement working electrode side became stable. Since the specimen had already reached the working electrode 9, the measurement could be started at the timing when the specimen dripped into the measurement introduction section reached the reference electrode 7. Thereafter, the flow to the unpermeated part of the reference electrode region became gentle, and the specimen that had become a saturated NaCl solution began to flow back toward the working electrode side. However, since the measurement could be started in a stable state of the working electrode 9, the measurement could be completed before the backflowing specimen reached the working electrode 9.

[0069] [Example 2] <Analysis device configuration> The analytical device P2 in Example 2 will be described with reference to Figures 12A and 12B. Figure 12A is a top view of the analytical device P2, and Figure 12B is a top view of the regulating member 30. As shown in Figure 12A, the analytical device P2 in this example is an analytical device having a flow region surrounded by a flow wall 5 formed of a hydrophobic resin inside a porous substrate, and has a first flow region 19 and a working electrode 9 covered with a coating film (ion selective membrane 8 in this example) containing a compound having ion selectivity, and the first flow region 1 has a reference electrode 7 provided on the porous substrate, and the working electrode 9 is outside the first flow region 19. The working electrode 9 is formed on the flow wall 5, and does not have a second flow region. A regulating member 30 (shown in dark gray) is arranged so as to cover the flow region except for the inlet portion of the conditioning liquid and the sample inlet portion.

[0070] In this embodiment, the first flow region 19 and the working electrode 9 are arranged so that the distance L4 between the adjacent portion 20, which is the region in the first flow region 19 that is closest to the working electrode 9, and the adjacent portion 21, which includes the ion selective membrane 8 that is closest to the first flow region 19, is 1 mm. The method for forming the porous substrate and the flow path walls was the same as in the first embodiment. In this embodiment, a restricting member 30 shown in Fig. 12B is placed on the upper part of the porous substrate 5. The restricting member 30 is a polyethylene terephthalate sheet with a thickness of 0.1 mm that is impermeable to specimens and the like, and is placed so as to cover the flow path region excluding the conditioning liquid inlet and specimen inlet. This makes it possible to prevent the specimens and the like from evaporating from the flow path region.

[0071] <Conditioning> The conditioning carried out in this example will be described with reference to FIG. Conditioning was performed before measuring the electrolyte concentration. In this embodiment, the inlet for conditioning includes a conditioning inlet 22 in the flow channel region 19 and an inlet 23 for conditioning which is above the ion selective membrane 8. However, the inlet for conditioning is not limited to the above as long as it is above the flow channel region 19 and the ion selective membrane 8, respectively, and the inlet 22 may be above the reference electrode 7 or above the ion crystal 6 as long as it does not contact the ion selective membrane 8, and the inlet 23 may not contact the flow channel 19.

[0072] As conditioning liquid S4, 10 μL of a 3 mol / L aqueous solution of NaCl was introduced into introduction portion 22. Also, as conditioning liquid S5, 10 μL of a 1 mmol / L aqueous solution of NaCl was introduced into conditioning introduction portion 23. After being introduced into each introduction portion, the conditioning liquid permeated into flow path region 19.

[0073] <Measurement of sample concentration> The method for measuring the specimen concentration will be described with reference to FIG. In this embodiment, the measurement introduction section 24 includes the adjacent section 20 and the adjacent section 21. At this time, 30 μL of the specimen was dropped into the measurement introduction section 24. Since the specimen was dropped onto the ion selective membrane 8, the ions in the specimen were immediately taken into the ion selective membrane after dropping, reacted with the electrode, and the potential started to stabilize. After that, the specimen dropped into the measurement introduction section 24 dissolved the ion crystal 6 and reached the reference electrode 7, but the working electrode 9 and the reference electrode 7 were electrically connected by the specimen, making it possible to measure the concentration, and the measurement of the specimen was completed at the specified measurement time.

[0074] In the above description, the flow path of the present invention is an example of a flow path surrounded by a flow path wall formed by a hydrophobic resin provided inside a porous substrate, but the flow path may be a flow path in which a hydrophobic sheet such as PET is used as the substrate and the surface is made hydrophilic by plasma treatment, corona discharge treatment, or surface coating treatment with a hydrophilic polymer. The hydrophilic polymer may be, for example, polyethylene glycol (PEG), or a polymer containing a polymer having a phosphorylcholine group. A coating layer may be applied and dried with a blend liquid consisting of hydrophilic inorganic fine particles, polymer fine particles dispersed in an aqueous medium, and a reactive organic fluorine compound. The specimen can move due to the hydrophilicity of the flow path. Furthermore, if a regulating member as in Example 2 is provided on the flow path so as to have a gap between the flow path and the regulating member, the capillary phenomenon due to the gap between the flow path and the regulating member is also added, so that the movement of the specimen can be made faster. A hydrophobic sheet may be used as the substrate and a flow path made of a porous member may be provided on the surface of the sheet. The flow path of the present invention may be a hydrophilic flow path surrounded by a hydrophobic flow path wall. The conditioning liquid to be introduced into the flow path region may be introduced in an amount that corresponds to the size of the flow path region. Furthermore, in this embodiment, the working electrode is described as being covered with a coating film containing a compound having ion selectivity according to the ion to be detected. However, the presence or absence of a coating film may be determined depending on the type of ion to be detected.

[0075] The embodiments of the present invention include the following configurations and methods. [Configuration 1] An analytical device having a hydrophilic or porous flow region surrounded by a hydrophobic flow wall disposed in or on a substrate, the analytical device having a first flow region and a working electrode; the first flow region has a reference electrode disposed on the substrate; The working electrode is outside the first flow region. Analytical devices. [Configuration 2] A second flow region; the second flow region includes the working electrode disposed on the substrate; The first flow path region and the second flow path region are separated from each other by the flow path wall. 2. The analytical device according to configuration 1. [Configuration 3] 3. The analytical device according to configuration 2, comprising two or more second flow path regions for one first flow path region. [Configuration 4] 4. The analytical device of configuration 2 or 3, wherein a portion of each of the first flow path region and the second flow path region is within a distance L of each other, where L is equal to or less than the diameter of a droplet of analyte to be introduced. [Configuration 5] The analytical device according to configuration 4, wherein an area including a circle having a diameter of L including a portion of each of the first flow path region and the second flow path region and a portion of the flow path wall separating them is used as an introduction portion during measurement for introducing a sample during measurement. [Configuration 6] 6. The analytical device according to any one of configurations 2 to 5, wherein each of the first flow path region and the second flow path region further includes an introduction portion. [Method 1] A method for measuring an electrolyte concentration using the analytical device according to any one of configurations 2 to 5, A method for measuring electrolyte concentration, comprising: introducing a specimen into the measurement introduction section to establish electrical continuity between the first flow path region and the second flow path region; and measuring a potential difference between a reference electrode and the working electrode, the potential difference being caused by a difference between a reference ion concentration in the first flow path region and an ion concentration derived from the specimen in the second flow path region. [Method 2] The electrolyte concentration measurement method according to Method 1, wherein a first conditioning solution containing chloride ions is introduced into the first flow path region before the sample is introduced into the measurement introduction portion. [Method 3] The electrolyte concentration measurement method described in Method 2 or 3, in which a second conditioning solution containing ions to be detected by the working electrode is introduced into the second flow path area before introducing a sample into the measurement introduction portion. [Method 4] The electrolyte concentration measurement method according to any one of Methods 1 to 3, wherein the sample is introduced into the second region before being introduced into the measurement introduction section. [Configuration 7] 2. The analytical device according to claim 1, comprising two or more working electrodes for one first flow region. [Configuration 8] 8. The analytical device of any one of configurations 1 to 7, wherein a portion of each of the first flow region and the working electrode are within a distance L of each other, where L is less than or equal to the diameter of a droplet of analyte to be introduced. [Configuration 9] The analytical device according to configuration 8, wherein an area including a circle having a diameter of L including a portion of each of the first flow path region and the working electrode, and a portion of the flow path wall separating them from each other, is used as an introduction portion during measurement for introducing a sample during measurement. [Configuration 10] 10. The analytical device of any one of configurations 1 and 7 to 9, wherein each of the first flow region and the working electrode further comprises an inlet portion. [Method 5] A method for measuring an electrolyte concentration using the analytical device according to any one of configurations 1 and 7 to 9, A method for measuring electrolyte concentration, comprising: introducing a specimen into the measurement introduction portion to electrically connect the first flow path region and the working electrode; and measuring a potential difference between the reference electrode and the working electrode, the potential difference being generated due to a difference between a reference ion concentration in the first flow path region and an ion concentration derived from the specimen at the working electrode. [Method 6] The electrolyte concentration measurement method according to Method 5, wherein a first conditioning solution containing chloride ions is introduced into the first flow path region before the sample is introduced into the measurement introduction portion. [Method 7] The electrolyte concentration measurement method according to Method 5 or 6, wherein a second conditioning solution containing ions to be detected by the working electrode is introduced into the working electrode before the sample is introduced into the measurement introduction portion. [Method 8] The method for measuring an electrolyte concentration according to any one of Methods 5 to 7, wherein the sample is introduced into the working electrode before the sample is introduced into the measurement introduction portion. [Explanation of symbols]

[0076] 1. First flow area 1a Flow passage chamber 1b Flow path 1c Proximal 2 Second flow area 2a Channel chamber 2b Flow path 2c Proximal part 3. Flow chamber 4 Flow chamber 5 Channel Wall Ionic crystals containing 6 Cl ions 7 Reference electrode 8. Ion-selective membranes 9 Working electrode 9a Base electrode 10 Reference side conditioning introduction 11. Working side conditioning introduction section 12 Introduction 13 Measurement Introduction S1 Porous base material L1 Distance between adjacent parts L4 Distance between adjacent parts 14 Single channel area 15 Introduction 16 Introduction 17 Introduction 18 Introduction 19 First flow area 20 Nearby area 21 Proximal 22 Introduction to conditioning 23 Introduction to conditioning 24 Measurement Introduction 30 Regulatory Materials

Claims

1. An analytical device having a hydrophilic or porous flow region surrounded by a hydrophobic flow wall disposed in or on a substrate, the analytical device having a first flow region and a working electrode; the first flow region has a reference electrode provided on the substrate; The working electrode is outside the first flow region. Analytical devices.

2. A second flow path region; the second flow region includes the working electrode disposed on the substrate; The first flow path region and the second flow path region are separated from each other by the flow path wall. The analytical device according to claim 1 .

3. The analytical device according to claim 2 , comprising two or more second flow path regions for one first flow path region.

4. 4. The analytical device according to claim 2, wherein a portion of each of the first flow path region and the second flow path region is within a distance L from each other, and L is equal to or smaller than a diameter of a droplet of the sample to be introduced.

5. The analytical device according to claim 4, wherein an area including a circle having a diameter of L including a portion of each of the first flow path region and the second flow path region and a portion of the flow path wall separating them is used as a measurement introduction portion for introducing the sample during measurement.

6. The analytical device according to claim 5 , wherein each of the first flow path region and the second flow path region further comprises an inlet portion.

7. A method for measuring an electrolyte concentration using the analytical device according to claim 5, A method for measuring electrolyte concentration, comprising: introducing the specimen into the measurement introduction portion to establish electrical continuity between the first flow path region and the second flow path region; and measuring a potential difference between the reference electrode and the working electrode, the potential difference being caused by a difference between a reference ion concentration in the first flow path region and an ion concentration derived from the specimen in the second flow path region.

8. 8. The method for measuring an electrolyte concentration according to claim 7, further comprising the step of introducing a first conditioning solution containing chloride ions into the first flow path region before introducing the specimen into the measurement introduction portion.

9. 8. The method for measuring an electrolyte concentration according to claim 7, further comprising the step of: introducing a second conditioning solution containing ions to be detected by the working electrode into the second flow path region before introducing the specimen into the measurement introduction portion.

10. The method for measuring an electrolyte concentration according to claim 7 , wherein the specimen is introduced into the second flow path region before being introduced into the measurement introduction portion.

11. The analytical device according to claim 1 , comprising two or more working electrodes for one first flow region.

12. 12. The assay device of claim 1 or 11, wherein a portion of each of the first flow region and the working electrode are within a distance L of each other, L being equal to or less than a diameter of a droplet of analyte to be introduced.

13. The analytical device according to claim 12, wherein a region including a circle having a diameter of L including a portion of each of the first flow path region and the working electrode, and a portion of the flow path wall separating them, is used as a measurement introduction portion for introducing the sample during measurement.

14. The analytical device of claim 13 , wherein each of the first flow region and the working electrode further comprises an inlet.

15. A method for measuring an electrolyte concentration using the analytical device according to claim 13, A method for measuring electrolyte concentration, comprising: introducing the specimen into the measurement introduction portion to electrically connect the first flow path region to the working electrode; and measuring a potential difference between the reference electrode and the working electrode, the potential difference being generated due to a difference between a reference ion concentration in the first flow path region and an ion concentration derived from the specimen at the working electrode.

16. 16. The method for measuring an electrolyte concentration according to claim 15, further comprising the step of introducing a first conditioning solution containing chloride ions into the first flow path region before introducing the specimen into the measurement introduction portion.

17. 16. The method for measuring an electrolyte concentration according to claim 15, further comprising the step of: introducing a second conditioning solution containing ions to be detected by the working electrode into the working electrode before introducing the specimen into the measurement introduction portion.

18. The method for measuring an electrolyte concentration according to claim 15 , wherein the specimen is introduced into the working electrode before being introduced into the measurement introduction portion.

Citation Information

Patent Citations

  • Paper-Based Reference Electrode And Potentiometric Ion Sensing

    US20160033438A1

Cited By

  • Ion analysis device and ion analysis method

    WO2025142287A1