Method for processing lithium-ion battery waste

By employing ammonia or amine compounds and solid-liquid separation, the method effectively addresses the inefficiencies in removing aluminum and iron from lithium-ion battery waste, enabling high recovery rates of cobalt and nickel.

JP2024164376AActive Publication Date: 2024-11-27MEC CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2023079806
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-15
Publication Date
2024-11-27
Estimated Expiration
2043-05-15

AI Technical Summary

Technical Problem

Existing methods struggle to efficiently remove aluminum and iron from lithium-ion battery waste leachate, hindering effective recovery of desired valuable metals like cobalt and nickel.

Method used

A method involving wet processing of lithium-ion battery waste with ammonia or amine compounds, followed by a solid-liquid separation step to remove undesired metals, using specific acids to enhance the recovery of cobalt and nickel.

Benefits of technology

The method achieves a high recovery rate of cobalt and nickel while significantly reducing the presence of aluminum, iron, and manganese in the leachate, allowing for selective recovery of these valuable metals.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024164376000001
    Figure 2024164376000001
  • Figure 2024164376000002
    Figure 2024164376000002
  • Figure 2024164376000003
    Figure 2024164376000003
Patent Text Reader

Abstract

To provide a method for treating lithium-ion battery waste excellent in a recovery rate of desired valuable metals such as nickel and cobalt.SOLUTION: A method for treating lithium-ion battery waste to obtain a leachate containing at least cobalt and nickel dissolved therein through a wet treatment of the lithium-ion battery waste, comprises: a wet treatment step of adding, to the lithium-ion battery waste, at least one compound (1) selected from a group consisting of ammonia and salts thereof, and an amine compound and a salt thereof, and mixing them to obtain the leachate containing at least cobalt and nickel dissolved therein; and a solid-liquid separation step of, after the wet treatment step, removing, through the solid liquid separation, at least a part of the metal that is not dissolved in the leachate.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for treating lithium ion battery waste. [Background technology]

[0002] From the perspective of the SDGs, recovery and reuse of valuable metals such as cobalt and nickel from lithium-ion battery waste is being widely considered.

[0003] When recovering valuable metals such as cobalt and nickel from lithium-ion battery waste, the lithium-ion battery waste is roasted, crushed, and other processes, and the resulting lithium-ion battery powder is added to an acidic solution to obtain a leachate in which lithium, copper, cobalt, nickel, iron, aluminum, manganese, and other metals are dissolved. Next, solid-liquid separation and solvent extraction are repeated to obtain a solution in which the desired valuable metals, such as cobalt and nickel, are dissolved. Finally, nickel and cobalt are recovered from each solution by performing electrolysis, etc.

[0004] For example, Patent Document 1 listed below describes a method for treating lithium ion battery waste, which includes a first neutralization step in which an acidic solution obtained by subjecting lithium ion battery waste to a wet treatment and in which at least cobalt, nickel, manganese and aluminum are dissolved is neutralized to a pH of 4.0 to 6.0, a portion of the aluminum is precipitated, and the portion of the aluminum is removed by solid-liquid separation; and a second neutralization step in which, after the first neutralization step, the pH is neutralized to 11.0 or higher, the remainder of the aluminum is left in the liquid, and a neutralization residue containing cobalt, nickel and manganese is obtained by solid-liquid separation. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2020-180362 A Summary of the Invention [Problem to be solved by the invention]

[0006] As a result of extensive research by the present inventors into the treatment method described in Patent Document 1, it was found that it was difficult to efficiently remove the target elements, aluminum and iron, from the leachate, and that there was room for further improvement in order to leach desired valuable metals such as nickel and cobalt at a high leaching rate.

[0007] In view of the above, an object of the present invention is to provide a method for treating lithium ion battery waste that has an excellent recovery rate of desired valuable metals such as nickel and cobalt. [Means for solving the problem]

[0008] The above problem can be solved by the following configuration. That is, the present invention relates to a method for treating lithium-ion battery waste by wet treating the lithium-ion battery waste to obtain a leachate in which at least cobalt and nickel are dissolved, the method comprising: a wet treatment step of adding at least one compound (1) selected from the group consisting of ammonia and its salt, and amine compounds and its salt to the lithium-ion battery waste and mixing the mixture to obtain the leachate in which at least the cobalt and the nickel are dissolved; and a solid-liquid separation step of removing at least a portion of the metal that is not dissolved in the leachate by solid-liquid separation after the wet treatment step.

[0009] In the above-mentioned method (1) for treating lithium ion battery waste, a method (2) for treating lithium ion battery waste is preferred, in which an acid is added in addition to the compound (1) and mixed in the wet treatment step.

[0010] In the above-mentioned method (2) for treating lithium ion battery waste, a method (3) for treating lithium ion battery waste is preferred, in which the acid is at least one compound (2) selected from the group consisting of monocarboxylic acid-based organic acids and inorganic acids.

[0011] In any of the above-mentioned methods for treating lithium ion battery waste (1) to (3), a method for treating lithium ion battery waste (4) is preferred, in which the compound (1) is at least one compound selected from the group consisting of amine compounds having an amino group and salts thereof.

[0012] In any of the above-mentioned methods for treating lithium ion battery waste (1) to (4), a method for treating lithium ion battery waste (5) is preferred, in which the compound (1) is at least one compound selected from the group consisting of chelating amine compounds having two or more amino groups and salts thereof.

[0013] In any one of the above-mentioned methods for treating lithium-ion battery waste (1) to (5), the lithium-ion battery waste contains aluminum, and in the solid-liquid separation step, at least a part of the aluminum is removed. This is a preferred method for treating lithium-ion battery waste (6).

[0014] In any of the above-mentioned methods for treating lithium-ion battery waste (1) to (6), the lithium-ion battery waste contains iron, and in the solid-liquid separation step, at least a part of the iron is removed in the method for treating lithium-ion battery waste (7).

[0015] In any one of the above-mentioned methods for treating lithium-ion battery waste (1) to (7), the lithium-ion battery waste contains manganese, and in the solid-liquid separation step, at least a part of the manganese is removed. Effect of the Invention

[0016] According to the method for treating lithium ion battery waste of the present invention, a wet treatment process is provided in which at least one compound selected from the group consisting of ammonia and its salts, and amine compounds and their salts is added and mixed to obtain a leachate in which at least cobalt and nickel are dissolved. This makes it possible to remove aluminum, iron, manganese, and other elements other than at least cobalt and nickel that are not the subject of recovery by a simple operation such as solid-liquid separation, and therefore makes it possible to recover desired valuable metals such as nickel and cobalt at a high recovery rate. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0017] The present invention relates to a method for treating lithium ion battery waste, which involves wet treating the lithium ion battery waste to obtain a leachate in which at least cobalt and nickel are dissolved, and which includes at least a wet treatment step and a solid-liquid separation step.

[0018] Lithium-ion battery waste is waste from lithium-ion batteries used in various devices such as electric vehicles, mobile phones, and personal computers. Lithium-ion batteries are usually made up of a positive electrode with lithium cobalt oxide as the main active material, a negative electrode with special carbon as the main active material, and a separator, which are layered or spirally wound together while containing an electrolyte, and are further placed inside an exterior material such as aluminum.

[0019] Lithium ion battery waste is usually subjected to pretreatment such as roasting and crushing before the wet treatment process. In the roasting process, the lithium ion battery is heated and held for several hours at a temperature in the range of, for example, 500 to 1000°C. The heating and holding may be performed in a furnace or in the air. In the crushing process, a crusher such as a sample mill, a hammer mill, or a hammer crusher is used. In the present invention, a pretreatment other than roasting and crushing may be performed before the wet treatment process as necessary. For example, after the lithium ion battery waste is subjected to pretreatment such as roasting and crushing to turn it into a fine powder of lithium ion battery powder, a certain amount of lithium may be recovered from the lithium ion battery powder by contacting it with, for example, ion-exchanged water.

[0020] Lithium ion battery waste contains lithium, copper, cobalt, nickel, iron, aluminum, manganese, and the like. The concentration of each metal contained in the lithium ion battery waste can be measured, for example, by the following method. Specifically, after pretreatment such as roasting and crushing, the lithium ion battery waste is made into a fine powder of lithium ion battery powder, and then the lithium ion battery powder is added to, for example, aqua regia (hydrochloric acid / nitric acid = 3 / 1 solution) to obtain a leachate in which lithium, copper, cobalt, nickel, iron, aluminum, manganese, and the like are dissolved. The leachate is preferably one obtained by leaching lithium ion battery powder with an acidic solution such as aqua regia. The pH of the leachate after the addition of aqua regia is preferably, for example, 0.0 to 1.0. The conditions for obtaining the leachate can be exemplified by adding 1.0 to 10.0 g of lithium ion battery powder per 50.0 to 500.0 g of aqua regia, and leaching at 25 to 80°C for 1 to 72 hours at a stirring speed of 250 to 1500 rpm. After leaching, solid-liquid separation is performed using a suction filter or the like, and the concentration of each metal in the obtained filtrate is measured. The concentration of each metal in the leachate can be measured, for example, by an ICP optical emission spectrometer (ICP-OES). In the present invention, the recovery rate of cobalt, nickel, etc. is calculated based on the leachate (filtrate) after adding aqua regia to the lithium ion battery waste. This point will be described later.

[0021] (Wet processing process) In the wet treatment process, at least one compound (1) selected from the group consisting of ammonia and its salts, and amine compounds and their salts is added to and mixed with lithium-ion battery waste to obtain a leachate in which at least cobalt and nickel are dissolved.

[0022] Compound (1) is at least one compound selected from the group consisting of ammonia and its salts, and amine compounds and their salts. Examples of salts of ammonia (ammonium salts) include ammonium chloride. Examples of amine compounds include ethylenediamine, tris(2-ethylamino)amine, imidazole, 2-piperazine, triethanolamine, L-lysine, and aminoguanidine. Examples of salts of amine compounds include ethylenediamine dihydrochloride, 2-piperazine hydrochloride, 2-piperazine hydrochloride monohydrate, cysteamine hydrochloride, triethanolamine hydrochloride, L-lysine hydrochloride, and aminoguanidine hydrochloride. Ammonia and its salts, and amine compounds and their salts may be used alone or in combination. For example, an ammonium salt may be combined with ammonia, or an amine compound salt may be combined with ammonia. More specifically, for example, a combination of ammonium chloride and ammonia, a combination of 2-piperazine hydrochloride monohydrate and ammonia, a combination of cysteamine hydrochloride and ammonia, a combination of ethylenediamine dihydrochloride and ammonia, a combination of triethanolamine hydrochloride and ammonia, a combination of L-lysine hydrochloride and ammonia, or a combination of aminoguanidine hydrochloride and ammonia may be used.

[0023] In the present invention, among the compounds (1), at least one compound selected from the group consisting of amine compounds having an amino group and their salts is preferred, and at least one compound selected from the group consisting of chelating amine compounds having two or more amino groups and their salts is more preferred. Specifically, for example, ethylenediamine, tris(2-ethylamino)amine, 2-piperazine hydrochloride monohydrate, ethylenediamine dihydrochloride, and L-lysine hydrochloride are preferred because they can further increase the recovery rate of desired valuable metals such as nickel and cobalt.

[0024] In order to increase the recovery rate of desired valuable metals such as nickel and cobalt, in the wet treatment step, it is preferable to add an acid to the lithium ion battery waste in addition to the compound (1) and mix it to remove at least a part of the metals other than cobalt and nickel, and it is even more preferable to add at least one compound (2) selected from the group consisting of monocarboxylic organic acids and inorganic acids as the acid and mix it to remove at least a part of the metals other than cobalt and nickel. Examples of the monocarboxylic organic acid include formic acid and acetic acid. Examples of the inorganic acid include hydrochloric acid and hydrobromic acid.

[0025] In the wet treatment step, when compound (2) is added in addition to compound (1), the molar ratio of compound (2):compound (1) is preferably 1:1 to 1:6, more preferably 1:1 to 1:2. By setting the ratio within this range, the recovery rate of desired valuable metals such as nickel and cobalt can be further increased.

[0026] In order to increase the recovery rate of desired valuable metals such as nickel and cobalt, the pH of the leachate after adding only compound (1) or the leachate after adding compound (1) and compound (2) in the wet treatment step is preferably adjusted to 3.0 to 12.5, more preferably 9.5 to 11.0. In addition, it is preferable to set the temperature of the leachate at 25 to 80°C and stir the leachate at a stirring speed of 500 to 1000 rpm for 8 to 24 hours.

[0027] (solid-liquid separation process) As a method for removing at least a part of the undissolved metals from the leachate obtained in the wet treatment step, for example, a method for separating the leachate in which at least cobalt and nickel are dissolved from the precipitates of aluminum and iron to be removed by solid-liquid separation can be mentioned. In the method for treating lithium ion battery waste according to the present invention, it is possible to recover desired valuable metals such as nickel and cobalt at a high recovery rate. Specifically, for example, when a solid-liquid separation step is carried out after the wet treatment step, the recovery rate of cobalt and nickel obtained thereafter is 50% or more, and more preferably 70% or more. In the present invention, the recovery rate of cobalt, nickel, etc. can be calculated by the following formula (1). (Recovery rate of each metal (%)) = (Metal concentration in the leachate (filtrate) obtained after the wet treatment process) / (Metal concentration in the leachate (filtrate) after adding aqua regia to lithium-ion battery waste) × 100 Equation (1)

[0028] In the method for treating lithium ion battery waste according to the present invention, the lithium ion battery waste contains aluminum, and in the solid-liquid separation step, removing at least a portion of the aluminum is preferable because the aluminum recovery rate calculated by formula (1) is low, that is, the amount of remaining aluminum is small. Specifically, for example, the aluminum remaining rate after the wet treatment step is 30% or less, and more preferably 10% or less.

[0029] In the method for treating lithium ion battery waste according to the present invention, the lithium ion battery waste contains iron, and in the solid-liquid separation step, removing at least a portion of the iron is preferable because the iron recovery rate calculated by formula (1) is low, that is, the residual iron rate is low. Specifically, for example, the residual iron rate after the wet treatment step is 30% or less, and more preferably 10% or less.

[0030] In the method for treating lithium ion battery waste according to the present invention, the lithium ion battery waste contains manganese, and in the solid-liquid separation step, removing at least a portion of the manganese is preferable because the manganese recovery rate calculated by formula (1) is low, that is, the manganese residual rate is low. Specifically, for example, the manganese residual rate after the wet treatment step is 30% or less, and more preferably 10% or less.

[0031] In the method for treating lithium ion battery waste according to the present invention, even if the lithium ion battery waste contains lithium, the recovery rate of lithium calculated by the formula (1) is relatively high in the solid-liquid separation step, which is preferable. Specifically, for example, the recovery rate of lithium after the wet treatment step is 10% or more, and more preferably 35% or more.

[0032] In the method for treating lithium ion battery waste according to the present invention, even if the lithium ion battery waste contains copper, the recovery rate of copper calculated by the formula (1) is relatively high in the solid-liquid separation step, which is preferable. Specifically, for example, the recovery rate of copper after the wet treatment step is 10% or more, and more preferably 35% or more.

[0033] In the method for treating lithium ion battery waste according to the present invention, when a solid-liquid separation process is carried out after the wet treatment process, the recovery rate of cobalt and nickel is high among the metals contained in the leachate (filtrate) obtained thereafter, and the remaining rate of unnecessary metals, particularly aluminum and iron, is low. Therefore, the method for treating lithium ion battery waste according to the present invention is particularly useful as a method for recovering cobalt and nickel from lithium ion battery waste. For example, by carrying out the extraction operation using an extractant known to those skilled in the art, only cobalt or only nickel can be recovered from the filtrate finally obtained after the wet treatment process. EXAMPLES

[0034] An example of an embodiment of the present invention will be described below, but the present invention is not limited to this description in any way.

[0035] (Measurement of the concentration of each metal in lithium-ion battery waste) Lithium-ion battery waste was roasted and crushed to obtain lithium-ion battery powder (1.0 g), which was added to 50.0 g of aqua regia (hydrochloric acid / nitric acid = 3 / 1), and mixed at 25°C for 24 hours at a stirring speed of 500 to 750 rpm to obtain a leachate. The leachate was subjected to solid-liquid separation using a suction filter, and the metal concentration of the obtained filtrate was measured. Note that ICP was used to measure the metal concentration. The results are shown in Table 1.

[0036] [Table 1]

[0037] (Wet processing process / solid-liquid separation process) 1.0 g of lithium ion battery powder was added to and mixed with 50.0 g of treated water. The treated water used was either ion-exchanged water and compound (1) alone, or ion-exchanged water, compound (1) and compound (2) adjusted in the ratios shown in Tables 2 and 3. The lithium battery powder and treated water were mixed at 25°C for 24 hours at a stirring speed of 500 to 750 rpm (wet treatment process), and then solid-liquid separation was performed using a suction filter (solid-liquid separation process), and the metal concentration of the obtained filtrate was measured. ICP was used to measure the concentration. The results are shown in Tables 2 and 3. The recovery rates of each metal in Tables 2 and 3 were calculated using the above formula (1) and evaluated according to the following criteria.

[0038] Recovery rate of metals to be recovered (cobalt (Co) and nickel (Ni)); 70% or more was evaluated as "Good", 50% or more but less than 70% was evaluated as "Good", and 50% or less was evaluated as "Poor". Recovery rate of non-recoverable metals (iron (Fe), aluminum (Al) and manganese (Mn)); 10% or less was evaluated as "good", 10% to less than 30% was evaluated as "good", and 30% or more was evaluated as "bad". Note that for non-recoverable metals, the higher the recovery rate, the more likely they are to remain in the filtrate and be recovered together with the target metals, which is undesirable since it means that the target metals are not selectively recovered. Recovery rate of other metals (lithium (Li) and copper (Cu)): 35% or more was evaluated as "Good", 10% to less than 35% was evaluated as "Good", and 10% or less was evaluated as "Poor".

[0039] [Table 2]

[0040] Comparative Example 1-3 is a conventionally known treatment method using an organic acid or inorganic acid, and not only the target metals of recovery, cobalt and nickel, but also the non-target metals of recovery, aluminum, iron and manganese, are simultaneously recovered, and it is understood that cobalt and nickel cannot be selectively recovered. On the other hand, Example 1-9 is a treatment method for lithium-ion battery waste according to the present invention, and it is understood that the target metals of recovery, cobalt and nickel, can be selectively recovered while decreasing the recovery rate of non-target metals of recovery, aluminum, iron and manganese. In particular, in Examples 3, 4, 6 and 8, which used a chelate-based amine compound having two or more amino groups as compound (1) and a monocarboxylic acid-based organic acid or inorganic acid as compound (2), the recovery rate of desired valuable metals such as nickel and cobalt was particularly excellent.

[0041] [Table 3]

[0042] Examples 10-19 are the method for treating lithium ion battery waste according to the present invention, and it can be seen that the recovery rates of the target metals, cobalt and nickel, can be selectively recovered while reducing the recovery rates of the non-target metals, aluminum, iron and manganese. In particular, Example 10, which uses ammonium chloride in combination with ammonia, Example 12, which uses 2-piperazine hydrochloride monohydrate in combination with ammonia, Example 13, which uses cysteamine hydrochloride in combination with ammonia, Example 15, which uses ethylenediamine dihydrochloride in combination with ammonia, and Example 18, which uses L-lysine hydrochloride in combination with ammonia, showed particularly excellent results in the recovery rates of desired valuable metals such as nickel and cobalt.

Claims

1. A method for treating lithium ion battery waste, comprising the steps of: wet treating the lithium ion battery waste to obtain a leachate in which at least cobalt and nickel are dissolved; a wet treatment step of adding at least one compound (1) selected from the group consisting of ammonia and its salt, and amine compounds and their salts to the lithium ion battery waste and mixing the resulting mixture to obtain the leachate in which at least the cobalt and the nickel are dissolved; A method for treating lithium ion battery waste, comprising a solid-liquid separation step of removing at least a portion of the metal that does not dissolve in the leachate by solid-liquid separation after the wet treatment step.

2. The method for treating lithium ion battery waste according to claim 1, wherein in the wet treatment step, an acid is added in addition to the compound (1) and mixed.

3. 3. The method for treating lithium ion battery waste according to claim 2, wherein the acid is at least one compound (2) selected from the group consisting of monocarboxylic organic acids and inorganic acids.

4. 2. The method for treating lithium ion battery waste according to claim 1, wherein the compound (1) is at least one compound selected from the group consisting of amine compounds having an amino group and salts thereof.

5. The method for treating lithium ion battery waste according to claim 1, wherein the compound (1) is at least one compound selected from the group consisting of chelate-type amine compounds having two or more amino groups and salts thereof.

6. The method for treating lithium ion battery waste according to claim 1, wherein the lithium ion battery waste contains aluminum, and at least a portion of the aluminum is removed in the solid-liquid separation step.

7. The method for treating lithium ion battery waste according to claim 1, wherein the lithium ion battery waste contains iron, and at least a portion of the iron is removed in the solid-liquid separation step.

8. The method for treating lithium ion battery waste according to claim 1, wherein the lithium ion battery waste contains manganese, and at least a portion of the manganese is removed in the solid-liquid separation step.

Citation Information

Patent Citations

  • Method for extracting lithium from lithium containing ore

    CN108277367A

  • Method for separating cobalt from material containing cobalt and nickel

    CN109468472A

  • Preparation method of nickel-cobalt binary oxide positive electrode material precursor of lithium-ion battery

    CN111129488A

  • Process for recycling waste lithium batteries

    CN111600090A

  • Method for recovering lithium and other metals from waste ion batteries

    JP2022542879A