The servo accelerometer addresses the issue of Au thin film wiring melting and poor contact by using a Ni layer to enhance bonding strength with solder, ensuring stable electrical connections and improved sensor accuracy.
Patent Information
- Application Number
- JP2023080886
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-16
- Publication Date
- 2024-11-28
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing servo accelerometers face issues with Au thin film wiring melting into solder and poor contact due to low bonding strength between Au thin film wiring and solder, leading to disconnection and poor electrical connections.
A servo accelerometer design that balances inertial force with Lorentz force using a Ni layer for thin film wiring, where the conductive wire is fixed with solder containing Sn, and a Ni layer is used to enhance bonding strength and reduce disconnection.
The design reduces the likelihood of solder and thin film wiring disconnection, maintaining stable electrical connections and improving sensor accuracy by minimizing thermal stress and oxidation effects.
Smart Images

Figure 2024165058000001_ABST
Abstract
Description
[Technical field]
[0001] This paper concerns a force-balanced servo accelerometer using a pendulum. [Background technology]
[0002] A conventional servo accelerometer is equipped with a pendulum with an electrode film formed between an upper yoke unit and a lower yoke unit that form a magnetic circuit. A torque cup is fixed to the surface of the pendulum, and a coil is wound around the torque cup. To detect acceleration, the displacement of the pendulum caused by acceleration is detected by the electrostatic capacitance generated between the yoke unit and the electrode film, which is converted and amplified into a voltage and applied to the coil. The magnetic field in the magnetic gap of the yoke unit and the Lorentz force (restoring force) generated by the current flowing through the coil control the displacement of the pendulum to zero. Since the restoring force at this time is equal to the force of inertia, acceleration can be detected from the coil current.
[0003] In a servo-type accelerometer having such a configuration, the circuit that controls the restoring force, the coil, the electrode film, etc. are electrically connected via the gold (Au) thin film wiring formed on the surface of the pendulum. Solder containing tin (Sn) is used as a joining material to fix and electrically connect the conductor that constitutes the coil to the thin film wiring. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Japanese Patent Application Publication No. 58-014024 Summary of the Invention [Problem to be solved by the invention]
[0005] In the configuration of the cited document 1, when the Au thin film wiring on the surface of the pendulum is joined to the conductor using solder containing Sn, the Au thin film wiring is easily broken by melting the solder. In addition, since the joining strength between the Au thin film wiring and the solder is low, contact failure is likely to occur. [Means for solving the problem]
[0006] In order to solve the above problems, the servo accelerometer of the present invention is a servo accelerometer in which the inertial force generated in the pendulum is balanced with the Lorentz force generated by the current flowing in a coil wound around a torque cup and the magnetic field passing through the pole piece, and is characterized in that it has thin-film wiring formed on the surface of the pendulum as an Au layer through which the current generated by the inertial force flows, and a conductor made of a metal material that conducts the current flowing in the thin-film wiring, wherein a Ni layer is formed on the path of the current flowing through the thin-film wiring and the conductor, and the conductor is fixed to the Ni layer with solder containing Sn that contacts the Ni layer. Effect of the Invention
[0007] It is possible to provide a servo accelerometer in which the solder and thin film wiring are less likely to break or cause poor contact. [Brief description of the drawings]
[0008] [Figure 1] Exploded perspective view of a servo accelerometer [Diagram 2] Cross-section of a servo accelerometer [Diagram 3] FIG. 1 is a diagram of a pendulum according to an embodiment of the present invention. [Figure 4] Plan view of the base of the pendulum [Diagram 5] 1 is a schematic cross-sectional view of a thin-film wiring according to an embodiment of the present invention; [Figure 6] Schematic cross-sectional view showing a method for producing a Ni layer and an Au layer according to an embodiment of the present invention. [Figure 7] 1 is a schematic cross-sectional view of a thin-film wiring according to an embodiment of the present invention; [Figure 8] Schematic cross-sectional view showing a method for producing a Ni layer and an Au layer according to an embodiment of the present invention. [Figure 9] 1 is a schematic cross-sectional view of a thin-film wiring according to an embodiment of the present invention; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] An embodiment of the present invention will be described below. Fig. 1 shows an exploded perspective view of a servo accelerometer of this embodiment. Fig. 2 shows a cross-sectional view of the servo accelerometer. The servo accelerometer is a device in which disk- or cylindrical-shaped parts are stacked. The central axes of these parts are aligned. Fig. 3 shows a perspective view of the pendulum 1.
[0010] The pendulum 1 has torque cups 13 and 14, with coils 11 and 12 wound around them, fixed to the surface of the base 10 of the pendulum. Fixing methods include bonding with an epoxy adhesive, mechanical fixing using screws, and joining using welding. The torque cups 13 and 14 are preferably made of a non-magnetic and lightweight material, such as an aluminum alloy, titanium alloy, or resin material. The coils 11 and 12 are made of a wire 41 made of a metal material. The wire 41 must have high conductivity, so copper, copper alloy, aluminum, or aluminum alloy is suitable. The insulating layer on the outer periphery of the wire 41 must have insulation and heat resistance, so the insulating layer is made of polyurethane, polyester, polyesterimide, or the like. The coils 11 and 12 are made by winding the wire 41 around the torque cups 13 and 14. The insulating layer of the wire 41 has a fusion layer on the outer periphery, and the fusion layers are bonded together to fix the shape after winding. Adhesion methods include applying a solvent and softening / melting by heating. The adhesive layer is required to be easy to process and heat resistant, so it is mainly made of polyvinyl butyral, polyamide, polyester, etc.
[0011] Figure 4 shows a plan view of the base 10 of the pendulum 1. The tongue-shaped pendulum weight 10a is located within the support part 10b, which is a cylindrical frame. Weight 10a is connected to hinge 10c and supported by support part 10b. When acceleration is generated in the pendulum 1, the thin-walled hinge 10c elastically deforms relative to the pendulum support part 10b, causing weight 10a to move in the direction of acceleration detection axis 30. Conductive wires 41 drawn from coils 11 and 12 are fixed to thin-film wiring 10e on the surface of the pendulum base 10 by solder 40 made of an alloy material. The coils 11 and 12 are then electrically connected to the thin-film wiring 10e.
[0012] The pendulum 1 is sandwiched between a pair of yokes 15 and 16. The pendulum 1 has three mounting pads 10f on both sides of the support part 10b that contact each yoke. The support part 10b and the yokes 15 and 16 can be fixed to each other by using the static friction between the mounting pads 10f and the yokes 15 and 16, or by using metallic bonding or diffusion bonding at the contact surfaces between the mounting pads 10f and the yokes 15 and 16.
[0013] The method of manufacturing the weight part 10a, support part 10b, and hinge 10c of the pendulum 1 will be explained. A plate is cut out from a base material such as metal or glass, and polished to produce a substrate with the desired thickness and surface accuracy. The surface of the pendulum 10 serves as the reference for the positions of the torque cups 11, 12 and the yokes 15, 16. Therefore, the higher the surface accuracy of the pendulum surface, the higher the assembly accuracy of each part. Next, part of the base material is removed by cutting, wet etching, laser, etc. to produce the shapes of the weight part 10a, support part 10b, and hinge 10c of the pendulum.
[0014] One end of each of the yokes 15 and 16 is closed by a circular yoke 17 or 18, and the other open end face is in contact with the support portion 10b. Pole pieces 19 or 20 and cylindrical permanent magnets 21 or 22 are housed inside the yokes 15 and 16, respectively. With this configuration, annular magnetic gaps are formed between the inner peripheral surfaces of the open ends of the yokes 15 and 16 and the outer peripheral surfaces of the pole pieces 19 and 20, respectively. The seal band 23 is fixed to the outer periphery of the yokes 15 and 16 using an adhesive or the like. The pendulum 1 is thereby fixed to the yokes 15 and 16.
[0015] The permanent magnets 21 and 22 are made of neodymium, samarium cobalt, or alnico magnets magnetized in the thickness direction, and the yokes 15 and 16, the circular yokes 17 and 18, and the pole pieces 19 and 20 are made of soft magnetic materials. The permanent magnets 21 and 22, the circular yokes 17 and 18, and the pole pieces 19 and 20 are fixed with adhesive, and the yokes 15 and 16 and the circular yokes 17 and 18 are joined by laser welding.
[0016] Capacitive electrodes 10d are formed on the upper and lower surfaces of mass 10a and function as two capacitor plates. Electrode surfaces 15e and 16e of yokes 15 and 16 formed opposite to capacitance electrode 10d are at a common potential, and detection signals of capacitance electrodes 10d on both plate surfaces of mass 10a are differentially amplified by a servo amplifier (not shown) via thin-film wiring 10e formed on the surfaces of hinge 10c and support portion 10b, conductor 24 electrically connected thereto, and terminal 25. Then, a servo current based on the capacitance difference flows through a pair of coils 11 and 12 via another terminal and thin-film wiring 10e.
[0017] When acceleration is applied in a direction perpendicular to the plane of the pendulum 10 (acceleration detection axis 30), the weight section 10a that receives the acceleration is displaced, but the displacement returns to the neutral point due to the torque current and the Lorentz force generated by the magnetic field in the magnetic gap, and the force generated by the acceleration and the Lorentz force are balanced. At this time, the magnitude of the torque current directly corresponds to the magnitude of the acceleration along the acceleration detection axis, so acceleration can be detected.
[0018] Conductive wire 24 is made of the same material as conductive wire 41. Terminal 25 is mainly made of a highly conductive material, for example, a single metal such as copper, aluminum, or iron, or an alloy thereof. Copper is particularly suitable because of its high electrical conductivity. However, since copper is easily oxidized, it is preferable to form a thin Au film on its surface to prevent oxidation. Methods for fixing terminal 25 and conductive wire 24 include wire bonding, soldering, and laser welding.
[0019] Example 1 Fig. 5 shows a schematic cross-sectional view of solder 40, conductive wire 41, and thin-film wiring 10e used in the servo-type accelerometer of the present invention. This cross-sectional view is taken from A to B in Fig. 4, with the surface shown in Fig. 4 facing up. Thin-film wiring 10e is made of Au layer 43 on the surface of pendulum 1, and Ni layer 42 is formed between thin-film wiring 10e and conductive wire 41, and conductive wire 41 is fixed to Ni layer 42 by solder 40 containing Sn that contacts Ni layer 42. Conductor 41 is covered with solder 40, and the bottom surface of Ni layer 42 contacts weight part 10a of the pendulum.
[0020] The Ni layer 42 and the Au layer 43 are a thin film structure. The thin film structure can be manufactured by film formation and shape processing. Examples of film formation methods include physical vapor deposition, chemical vapor deposition, electroplating, and chemical plating. Shape processing includes a method of forming a thin film only on the intended part in the film formation process, i.e., a selective film formation method, and a method of removing the intended part after film formation, i.e., a selective removal method. In the selective film formation method, a metal mask with an opening, a photoresist pattern, masking tape, etc. (hereinafter, mask parts) are formed and fixed in advance on the surface of the base part 10 of the pendulum, so that a thin film structure is formed only on the surface of the base part 10 of the pendulum exposed to the opening. In the selective removal method, a mask part is formed and fixed on the surface of the formed thin film to protect the part to be left as the thin film structure. Next, the unprotected part of the thin film is removed by physical energy, an etching solution, etc. When the mask part is removed, a thin film structure is formed on the surface of the base part 10 of the pendulum.
[0021] In order to suppress the phenomenon in which the solder 40 peels off from the thin film wiring 10e, it is necessary to improve the bonding strength between the solder 40 and the Ni layer 42, as well as the bonding strength (adhesion) between the Au layer 43 and the Ni layer 42, the adhesion between the Au layer 43 and the base 10 of the pendulum, and the strength of each thin film structure. In other words, it is preferable to use a method for manufacturing these thin film structures that can obtain good adhesion and strength. The sputtering method, which is one of the physical vapor deposition methods, is advantageous compared to other physical vapor deposition methods. In the sputtering method, Ar gas is introduced in a vacuum, and a voltage is applied to turn the Ar gas into plasma, and Ar ions are accelerated in the plasma and collide with the raw material. Then, particles on the surface of the raw material are repelled (sputtering phenomenon) and adhere to the surface of the base material facing the raw material. Since the particles flying in due to the sputtering phenomenon have high energy, the surface energy of the deposition surface becomes high. Therefore, a high adhesion force can be obtained to the surface on which the material is deposited. In addition, since the flying particles tend to agglomerate on the deposition surface, it is easy to obtain a high-strength thin film in which the elements are in a denser state.
[0022] A method for producing the thin-film wiring 10e, Ni layer 42, and Au layer 43 will be described with reference to Figure 6. Ni layer 42, which serves as a base for solder 40, is produced as a thin-film structure on the surface of weight portion 10a of the pendulum. Next, Au layer 43 is produced in the same manner, covering Ni layer 42. Au layer 43 is deposited not only on the portion where Ni layer 42 is formed, but also on the surfaces of hinge portion 10c and support portion 10b of the pendulum. Au layer 43 occupies most of the thin-film wiring 10e.
[0023] A method for manufacturing the solder 40 will be described. First, the Au layer 43 on the upper surface of the Ni layer 42 shown in FIG. 6 is removed. In this method, molten solder is attached to a heated soldering iron or the like, and then the molten solder and the soldering iron are brought into contact with the Au layer 43 on the upper surface of the Ni layer 42. The Au layer 43 on the surface of the Ni layer is dissolved in the molten solder, and the soldering iron is then removed from the processing area. At this time, the Au layer 43 on the surface of the Ni layer is removed together with the molten solder. Then, a compound layer of elements contained in the solder and Ni is formed on the surface of the Ni layer. Then, the conductor 41 drawn out from the coils 11 and 12 is fixed to the Ni layer 42 by soldering. At this time, flux for removing the oxide film formed on the surface of the Ni layer is applied to the processing area as necessary. Next, the conductor 41 and the surface of the Ni layer 42 are covered with the molten solder. Then, the solder 40 is coagulated and solidified by natural cooling, and is fixed to the surface of the Ni layer 42. At this time, the solder 40 forms an intermetallic compound layer at the interface with the conductive wire 41 and the thin film wiring 10e, thereby firmly fixing these components. As a post-processing step, the remaining flux may be removed with a solvent or the like.
[0024] In order to reduce the thermal effects on the pendulum 1 and to facilitate processing, it is preferable that the solder be a low melting point material. For this reason, the solder is made of an alloy containing tin (Sn). In particular, an alloy of 37% Sn and 63% Pb called eutectic solder has a melting point of 183°C, is inexpensive compared to precious metal solder, and has good wettability with the main thin film wiring materials, making it suitable for the solder 40, which requires economy and reliability.
[0025] In soldering, the surface of Ni dissolves into the molten solder, forming an intermetallic compound mainly of Sn and Ni. If the dissolution rate is fast, the amount of dissolution increases, making the conductor 41 and thin-film wiring 10e more susceptible to breakage. The Au used in the thin-film wiring in Reference 1 melts into solder at a rate of about 10 μm / s at 300° C. Because soldering takes several seconds to process, the thickness of the Au needs to be about several tens of μm in order to prevent breakage due to melting. Because Au is expensive, the cost of the accelerometer increases significantly when Au thin-film wiring is used.
[0026] By lowering the temperature of the molten solder and Au thin-film wiring during soldering, it is possible to suppress breakage even in thin Au thin-film wiring. However, if the temperature of the molten solder is low, the wettability with the Au thin-film wiring decreases, resulting in a state commonly known as potato solder, and the contact area between the Au thin-film wiring and the solder becomes smaller, so the overall bonding strength of the joint tends to decrease. In addition, even if the joint is joined, the bonding strength per unit area cannot be secured. This is because AuSn4, an intermetallic compound of Sn and Au, has a volume several times larger than that of the solder material. When the solder is formed, internal stress is generated in the solder due to the expansion of the intermetallic compound, and if the stress is large, microcracks occur around the intermetallic compound. This is a major cause of solder breakage. In other words, with such a configuration, the accelerometer becomes more susceptible to failure due to impact.
[0027] Compared to Au, Ni dissolves in Sn at about 1 / 1000 the rate. Therefore, thin film wiring is less likely to break when soldered. The intermetallic compound formed by soldering is mostly Ni3Sn4. The molar volume of AuSn4 is 75.0×10 -6 m 3 mol -1 In contrast, Ni3Sn4 is 11.32 x 10 -6 m 3 mol -1 , which is relatively small. The molar volume of Au is 10.21 × 10 -6 m 3 mol -1 And Ni is 6.6×10 -6 m 3 mol -1Therefore, the expansion coefficient from the base elements is 7.4 times for AuSn4 and 1.7 times for Ni3Sn4. Thus, Ni intermetallic compounds have a smaller volume and expansion coefficient than Au. In other words, compared to Au, the internal stress is smaller at the interface between the Ni layer and the solder, and microcracks are less likely to occur. In addition, since the Au layer, which is the thin-film wiring 10e, can be made thin, the accelerometer according to this embodiment can be manufactured at low cost.
[0028] The current flowing through the coil heats the accelerometer from the inside, so the temperature of the pendulum 1 tends to rise. The rise in temperature promotes metal diffusion at the interface between the solder and the underlying metal thin film. Au easily diffuses into Sn, so even a small change in temperature will generate new AuSn4. In other words, accelerometers that use an Au layer as the solder base are prone to failure due to temperature changes. On the other hand, Ni does not easily diffuse into Sn, so it is difficult for new intermetallic compounds to be generated by temperature increases. Compared to those that use Au, accelerometers that use a Ni layer as the solder base are less likely to fail due to temperature changes.
[0029] Ni easily forms an oxide film on its surface, which reduces wettability with molten solder and makes the solder more likely to become a potato solder. In addition, the oxide film prevents the formation of an intermetallic compound between Ni and solder, which reduces the strength of the joint between the Ni layer and the solder. In the present invention, the formation of an oxide film is suppressed by forming an Au layer on the surface of the Ni layer in advance. Then, by removing the Au layer on the surface of the Ni layer, the amount of Au mixed into the solder can be reduced, and the amount of intermetallic compounds of Au and Sn contained in the solder 40 can be reduced. This makes it possible to obtain a solder 40 with high strength.
[0030] The bottom surface of the solder 40 is within the region of the upper surface of the Ni layer 42 and does not protrude beyond it. If the bottom surface of the solder 40 protrudes beyond the surface of the Ni layer 42, the molten solder will come into contact with the thin-film wiring 10e during soldering, melting the constituent Au layer 43 and disconnecting the thin-film wiring 10e, or causing poor contact between the Ni layer 42 and the Au layer 43 or increasing the electrical resistance value at the interface.
[0031] When a temperature change occurs in the accelerometer, the components that make up the servo accelerometer change shape due to thermal expansion and contraction. This causes a change in the shape of the pendulum 10, which changes the behavior of the pendulum that reflects acceleration, resulting in a decrease in sensor accuracy. To reduce this, it is necessary to use materials for the components that have as low a linear expansion coefficient as possible. In particular, it is required that the pendulum 1, which is the oscillator itself and serves as the reference for the position of each component, deform as little as possible. Quartz glass has a linear expansion coefficient of 0.5×10 -6 / K. Compared to common commercial metals, the linear expansion coefficient is about 1 / 10. Also, because it is an insulating material, it is not conductive to the thin film wiring 10e formed on the surface of the pendulum. Furthermore, because it is a non-magnetic material, it does not affect the magnetic field in the magnetic gap formed by the yokes 15, 16, the circular yokes 17, 18, the magnets 19, 20, and the pole pieces 17, 18. Quartz glass is a suitable material for the pendulum 10.
[0032] The adhesion between glass materials and metal thin films tends to be low. In addition, the Ni layer is easily peeled off from the pendulum base 10b, which is quartz glass, due to thermal stress caused by soldering. The adhesion layer of titanium (Ti) or chromium (Cr) produced by the above-mentioned film formation method can form a chemically stable and high-strength mixed layer at the interface with the quartz glass, which is the pendulum material. For example, titanium bonds with oxygen atoms or silicon atoms of the quartz glass to form an amorphous Si-Ti mixed layer or an amorphous Si-O-Ti mixed layer at the interface. These are in a metastable state and have high strength, so titanium and quartz glass can obtain strong adhesion. In addition, titanium and chromium can form a good mixed layer for the Au layer and Ni layer that constitute the thin film wiring 10e. In other words, the use of an adhesion layer of titanium or chromium can suppress peeling between the Ni layer 42 and the pendulum base 10 and peeling between the Au layer 43 and the pendulum base 10.
[0033] Example 2 Example 2 is shown in Fig. 7. In the servo acceleration according to this example, the surface of the Au layer 43 that faces the surface of the pendulum is in contact with the Ni layer 42. The Au layer 43 is not present on a portion of the upper surface of the Ni layer 42, and the conductor 41 is fixed to the Ni layer 42 by solder 40. In other words, the Ni layer 42 is present on the bottom surface of the Au layer 43 except for the portion where the solder 40 is formed, and the Ni layer on the bottom surface of the Au layer can be laminated continuously with the Au layer.
[0034] In the first embodiment, the Ni layer 42 and the Au layer 43 are only partially laminated, so that each layer must be subjected to different film formation and shape processing. Therefore, after the Ni layer 42 is formed, there is a time until the Au layer 43 is laminated, and an oxide film and impurities are likely to adhere to the surface of the Ni layer exposed during the process. The passivation film formed on the surface of Ni or Ni alloy is chemically stable, so it cannot be sufficiently removed by the flux used in soldering. Although it is possible to chemically remove (etch) the oxide film using a strong acidic chemical solution immediately before forming the Au layer 43, the oxide film will adhere again in a subsequent process such as a cleaning process. Furthermore, the material remaining after etching may reduce the adhesion between the Ni layer 42 and the Au layer 42. If all the processes are performed in a vacuum or in an inert gas, the surface of the Ni layer 42 can be kept clean, but the number of processes and the number of materials used make the manufacturing equipment more complex and large-scale, and the manufacturing cost of the accelerometer significantly increases.
[0035] In this embodiment, since the Ni layer 42 and the Au layer 43 are laminated, they can be deposited continuously in the film formation. Furthermore, no oxide film or residue is attached to the surface of the Ni layer 42, or the amount of residue is less than that of the first embodiment. Therefore, it is possible to obtain good wettability between the molten solder and the Ni layer 42, and the bonding area between the solder 40 and the Ni layer 42 is large. Furthermore, since the amount of impurities mixed into the solder 40 is small, the solder 40 has high strength. Thus, in the accelerometer according to this embodiment, the bonding strength between the solder 40 and the Ni layer is high, and the strength of the solder 40 is also high, compared to the first embodiment.
[0036] A method for producing the thin film wiring 10e will be described with reference to FIG. 8. In the selective removal method, a thin Ni film and a thin Au film are continuously deposited on the surface of the base 10 of the pendulum 1 using physical vapor deposition, chemical vapor deposition, electroplating, or chemical plating. Next, a mask component is formed and fixed so as to leave the shape of the thin film wiring 10e, and the part to be left as the thin film wiring 10e is protected. Next, the unprotected parts of the thin Ni film and the thin Au film are removed using physical energy, an etching solution, or the like. In the selective deposition method, a metal mask, a photoresist pattern, a masking tape, or the like (hereinafter, mask component) having an opening is fixed on the surface of the pendulum 1, and a Ni layer 42 and a Au layer 43 are continuously deposited on the surface of the base 10 of the pendulum exposed to the opening. Since the planar shapes of the Ni layer 42 and the Au layer 43 are the same, the selective deposition method and the selective removal method make it possible to process the shape at once. In either method, the Ni layer 42 and the Au layer 43 can be deposited successively on the pendulum base 10.
[0037] The method of manufacturing the solder 40 is the same as in Example 1. A part of the Au layer 43 is removed using a soldering iron and molten solder, and the conductive wire 41 is fixed with the solder 40 to the upper surface of the exposed Ni layer 42.
[0038] The permanent magnets 19 and 20 are composed of neodymium, samarium cobalt, alnico magnets, etc. magnetized in the thickness direction, and their residual magnetic flux density is about 1T. The magnetic flux density of the magnetic gap controlled by the closed magnetic circuit of the yoke units 2 and 3 (yokes 15 and 16, circular yokes 17 and 18, pole pieces 19-20, magnets 21-22) is a value that is reduced to a certain extent from the residual magnetic flux density of the permanent magnets. If there is a magnetic body in the vicinity of the yoke units 2 and 3, the magnetic body affects the magnetic flux of the magnetic gap, and the magnetic flux density of the magnetic gap changes. For example, a Ni thin film produced by electroplating has a saturation magnetic flux density of about 0.6T, and the residual magnetic flux density increases by the amount of its thickness. On the other hand, in order to prevent the Ni layer from disappearing due to molten solder, the Ni layer must have a certain thickness. Thus, it is difficult to reduce the thickness of the Ni layer and reduce the effect on the magnetic gap. This phenomenon can be ignored if the accelerometer is large and its component permanent magnets are large, but in small, thin accelerometers, its effect on the magnetic gap cannot be ignored. Also, in Ni, hysteresis occurs in the residual magnetization caused by an external magnetic field. The increase or decrease in the magnetic field caused by an increase or decrease in the coil current causes the residual magnetization of the Ni thin film to change nonlinearly, affecting the coil current and the magnetic flux density of the magnetic gap. This effect appears as mechanical noise in response to the displacement of the pendulum, or electrical noise in the coil current.
[0039] The Ni layer 42 is preferably non-magnetic, since the presence of a ferromagnetic material on the surface of the base 10 of the pendulum leads to a decrease in sensor accuracy. Its saturation magnetic flux density is preferably 10-3 T or less, which is sufficiently smaller than the residual magnetic flux density of the permanent magnets 19 and 20. In order to meet this requirement and to prevent loss due to soldering, an alloy containing a large amount of Ni is preferable, and examples of such alloys include Ni-Cu, Ni-Sn, Ni-P, Ni-W, Ni-Mo, or alloys containing these and other elements. All of these metals and alloys can be produced by electroplating or physical vapor deposition, and lose ferromagnetism when the Ni content is 80 to 70 wt%. If these alloys are used for the Ni layer, an accelerometer can be obtained in which the adhesion between the solder 40 and the Ni layer 42 is high while maintaining high sensor accuracy.
[0040] Example 3 Example 2 is shown in Figure 9. In the servo acceleration according to this example, the surface of Ni layer 42 facing the surface of pendulum 1 is in contact with Au layer 43, and a second Au layer 44 is provided around solder 40 on the upper surfaces of Ni layer 42 and Au layer 43. That is, Ni layer 42 is laminated on the upper surface of Au layer 43 which is thin-film wiring 10e, and conducting wire 41 is fixed to the upper surface of Ni layer 42 by solder 40. Then, Au layer 44 different from Au layer 43 is laminated around solder 40.
[0041] A method for producing the thin-film wiring 10e will be described. As in the first embodiment, an Au layer 43 is formed on the surface of the base 10 of the pendulum by using a selective film formation method or a selective removal method. Then, as in the second embodiment, an Ni layer 42 and an Au layer 44 are successively formed and laminated. The subsequent soldering is the same as in the first embodiment. A soldering iron and molten solder are used to remove a portion of the Au layer 44, and a conductor 41 is fixed with solder 40 to the top surface of the exposed Ni layer 42.
[0042] Since Au does not form an oxide film, even if the Ni layer 42 is deposited on the upper surface of the Au layer 43, an oxide film or impurities are unlikely to be mixed in at the interface. In the process of depositing the Au layer 44 on the Ni layer 42, the Ni layer 42 and the Au layer 44 can be continuously laminated, so that an oxide film or impurities are unlikely to be mixed in at the interface, as shown in Example 2. In other words, good adhesion can be obtained between the Au layer 43, the Ni layer 42, and the Au layer 44, and it is easy to obtain a solder 40 with high strength.
[0043] In the accelerometer, the Lorentz force generated by the coil current and the magnetic gap and the inertial force received by the pendulum 1 are balanced to detect the accelerometer. However, the spring force generated by the hinge 10c is also added to this balance of forces, and the spring force becomes a factor of error in the sensor accuracy. In other words, the smaller the rigidity of the hinge, the higher the sensor accuracy of the accelerometer. For this reason, the thin film wiring 10e on the hinge surface is also required to have low rigidity. The electrical resistivity of Au at room temperature is 2.44×10-8 Ω·m, and that of Ni is 6.99×10-8 Ω·m. The Young's modulus of Au is about 78 GPa, and that of Ni is about 200 GPa. In other words, the thin film wiring 10e of the accelerometer according to this embodiment can reduce the rigidity of the thin film wiring required to obtain a predetermined conductivity compared to Example 2. And, since the spring force of the hinge 10c of the pendulum including the thin film wiring 10e is reduced, the accelerometer can obtain high sensor accuracy.
[0044] The Ni layer dissolves into the molten solder due to the heat of soldering. In order for the Ni layer to disappear and for the molten solder not to come into contact with the Au layer, the Ni layer needs to be sufficiently thick. In soldering using Sn-Pb solder, which is a typical example of eutectic solder, a soldering iron temperature of about 250 to 300°C is suitable. At this time, the speed at which Ni melts into eutectic solder is about 0.01 μm / s. That is, in order for the Ni layer not to disappear in soldering for a few seconds, a thickness of several tens of nm is required at the minimum. Considering that the Ni layer also melts or diffuses into the Au layer, it is preferable to ensure a thickness twice that of the Au layer. That is, the thickness of the Ni layer 42 needs to be 100 nm or more. Since the melting speed decreases when the processing temperature is lowered, it is possible to reduce the thickness of the Ni layer. However, this leads to a decrease in wettability and a decrease in bonding strength. In order to obtain good bonding properties, it is required to make the Ni layer 100 nm or more thick and process it at an appropriate processing temperature of 250 to 300°C.
[0045] The Au layer 44 is formed on the upper surface of the Ni layer 42 to suppress oxidation of the Ni layer 42. As in the first embodiment, most of the Au layer 44 is removed during soldering to form the solder 40. At this time, a part of the molten solder remains on the surface of the Ni layer, and therefore a small amount of the dissolved Au layer contained in the molten solder also remains on the surface of the Ni layer. In order to reduce the amount of remaining Au, it is necessary to reduce the volume of the Au layer 44. On the other hand, in order to suppress oxidation of the Ni layer, the thickness of the Au layer 44 needs to be at least 50 nm. Thus, a thickness of about 50 nm is suitable for the Au layer 44.
[0046] Although the preferred embodiment of the present invention has been described above, it goes without saying that the present invention is not limited to such an embodiment. It is clear that a person skilled in the art can come up with various modifications or alterations within the scope of the claims, and it is understood that these naturally fall within the technical scope of the present invention. Specifically, the above embodiment merely shows the joining of the conductor 41 of the coils 11 and 12 to the thin-film wiring 10e on the surface of the pendulum. For example, the present invention is also applicable to the process of joining the thin-film wiring 10e and the conductor 24 using solder and electrically connecting the thin-film wiring 10e to the terminal 25. In this way, the present invention is applicable to all processing parts in which a conductor is fixed to the thin-film wiring 10e using solder. [Explanation of symbols]
[0047] 1 pendulum 10 base 10a Weight 10b Support part 10c Hinge 10d Capacitive Electrode 10e Thin film wiring formed on the hinge, support, and weight surface 10f Mounting Pad 10g hole 10h End of hole 11, 12 Coils 13, 14 Torka Cup 19, 20 Pole pieces 21, 22 Permanent magnets 23 Seal Band 24 Conductor 25 Terminals 30 acceleration sensing axes 40 Solder 41 Conductor 42 Ni layer 43, 44 Au layer
Claims
1. The inertial force generated in the pendulum, A servo accelerometer in which the Lorentz force generated by the current flowing in a coil wound around a torque cup and the magnetic field passing through a pole piece is balanced, A thin film wiring formed on the surface of the pendulum as an Au layer through which a current generated by an inertial force flows; a conductor made of a metal material that conducts a current flowing through the thin film wiring; a Ni layer is formed on a path of a current flowing through the thin film wiring and the conductor; A servo accelerometer, wherein the conducting wire is fixed to the Ni layer by solder containing Sn in contact with the Ni layer.
2. 2. The servo accelerometer according to claim 1, wherein a surface of said Au layer facing said surface of said pendulum is in contact with said Ni layer.
3. 2. The servo accelerometer according to claim 1, wherein the Au layer is an undercoat for the Ni layer.
4. 2. The servo accelerometer according to claim 1, wherein the sides of the Ni layer are covered with the Au layer.
5. 2. The servo accelerometer according to claim 1, further comprising an adhesion layer made of Cr, Ti or an alloy thereof on a bottom surface of the Ni layer or the Au layer.
6. The Ni layer is Ni-Cu, Ni-Sn, Ni-P, Ni-W, Ni-Mo or an alloy thereof containing other elements; The Ni content is 80 to 70 wt %, Saturation magnetic flux density is 10- 3 6. The servo accelerometer according to claim 1, wherein the acceleration is equal to or smaller than T.
Citation Information
Patent Citations
Bending section for power transducer
JP1983014024A
Cited By
Quartz base plane differential type quartz vibrating beam accelerometer and packaging method thereof
CN119827796A