Machining tool
The processing tool efficiently removes the chamfered portion of a wafer using a configured grinding and polishing wheel setup, enhancing productivity and preventing damage, addressing the inefficiencies and safety concerns of existing methods.
Patent Information
- Application Number
- JP2023081472
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-17
- Publication Date
- 2024-11-28
AI Technical Summary
Existing methods for removing the chamfered portion of a wafer are time-consuming, reducing productivity and potentially causing damage to devices and operators due to the formation of cracks and chips.
A processing tool with a specific configuration of grinding and polishing wheels, where the width of the grinding wheel plus polishing wheel exceeds the length of the chamfered portion to be removed, and the polishing wheel's width is between one-third and one-hundredth of the length, combined with diamond abrasive grains of varying sizes, is used to efficiently remove the chamfered portion.
The tool efficiently removes the chamfered portion, improving productivity by smoothing the outer surface and preventing damage to devices and operators.
Smart Images

Figure 2024165347000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a processing tool for removing a chamfer from a wafer having a central region, a peripheral surplus region surrounding the central region, and a chamfer formed in the peripheral surplus region. [Background technology]
[0002] A wafer has a number of devices such as ICs and LSIs formed on its front surface, separated by planned dividing lines. The back surface is ground by a grinding device to form the wafer into a specified thickness, and the wafer is then divided into individual device chips by a cutting device for use in electrical devices such as mobile phones and personal computers.
[0003] The grinding device includes a chuck table for holding a wafer, a grinding means having a rotatable grinding wheel with grinding stones arranged in a ring shape for grinding the wafer held on the chuck table, a feeding means for feeding the grinding means for grinding, and a measuring means for measuring the thickness of the wafer, and can grind the back surface of the wafer to the desired thickness.
[0004] However, because a chamfer is formed on the outer periphery of the wafer, when the back surface of the wafer is ground to thin it, the chamfer on the outer periphery of the wafer becomes a sharp knife edge, which causes cracks to form from the outer periphery and progress into the device region, damaging the device and posing a risk of injury to the operator.
[0005] Therefore, the present applicant has proposed a technique for removing the chamfered portion formed at the outer peripheral end of the outer peripheral excess region before grinding the back surface of the wafer (see, for example, Patent Document 1).
[0006] Furthermore, cutting the above-mentioned chamfered portion with a cutting wheel causes chipping on the outer periphery of the wafer, resulting in a decrease in quality. Therefore, the applicant has proposed a technology to improve the quality before grinding the back surface of the wafer by roughly removing the chamfered portion with a coarse grinding wheel and then removing the chipping with a fine grinding wheel (see Patent Document 2). [Prior art documents] [Patent documents]
[0007] [Patent Document 1] JP 2010-225976 A [Patent Document 2] Patent No. 2014-003198 Summary of the Invention [Problem to be solved by the invention]
[0008] However, a process that involves a removal step in which the chamfered portion is roughly removed using a coarse grindstone surface, followed by a finishing step in which the chamfered portion is finished using a fine grindstone surface, has problems in that it takes a long time to remove the chamfered portion, resulting in poor productivity and being an unbearable hassle.
[0009] The present invention has been made in consideration of the above circumstances, and a main technical object of the present invention is to provide a processing tool capable of efficiently removing the chamfered portion of a wafer. [Means for solving the problem]
[0010] In order to solve the above-mentioned main technical problem, according to the present invention, there is provided a processing tool for removing a chamfer from a wafer having a central region, a peripheral surplus region surrounding the central region, and a chamfer formed in the peripheral surplus region, the processing tool including an annular grinding wheel having an opening for insertion into a rotating shaft and a first side surface and a second side surface, and a polishing wheel formed on at least one of the first side surface or the second side surface, wherein L is the radial length from the peripheral end of the chamfer to be removed, H is the width of the grinding wheel, and h is the width of the polishing wheel, H+h>L (1) L / 3>h>L / 100···(2) The present invention provides a machining tool formed so as to satisfy both conditions (1) and (2) set forth above.
[0011] The grain size of the diamond abrasive grains constituting the polishing wheel is selected according to the material of the workpiece, and the grain size of the diamond abrasive grains constituting the grinding wheel is preferably selected within a range of 1.5 to 5 times the grain size of the diamond abrasive grains constituting the polishing wheel.The bond material constituting the polishing wheel and the grinding wheel is preferably selected from among resin bond, vitrified bond, and metal bond.Furthermore, the central region is preferably a semiconductor wafer having a device region in which a plurality of devices are partitioned by a division line. Effect of the Invention
[0012] The processing tool of the present invention is a processing tool for removing a chamfered portion of a wafer having a central region, an outer circumferential surplus region surrounding the central region, and the chamfered portion formed in the outer circumferential surplus region, and includes an annular grinding wheel having an opening for insertion into a rotating shaft and a first side surface and a second side surface, and a polishing wheel formed on at least one of the first side surface or the second side surface, wherein the radial length from the outer circumferential end of the chamfered portion to be removed is L, the width of the grinding wheel is H, and the width of the polishing wheel is h, H+h>L (1) L / 3>h>L / 100···(2) Since the chamfered portion is formed so as to satisfy both of the conditions (1) and (2) specified in the above, it becomes possible to efficiently roughly remove the region of the radial length L from the outer peripheral end of the wafer that is to be removed, using a grinding wheel, while smoothly finishing the outer peripheral surface that forms the removed region at the chamfered portion, thereby improving productivity. [Brief description of the drawings]
[0013] [Figure 1] 1 is an overall perspective view of a cutting device to which a machining tool according to an embodiment of the present invention is attached; [Diagram 2] FIG. 2(a) is a partially enlarged perspective view of a cutting means of the cutting device shown in FIG. 1, and FIG. [Diagram 3] FIG. 13 is a perspective view showing an aspect of a wafer holding step for holding a wafer. [Figure 4]FIG. 13 is a perspective view showing a mode of detecting a position to be machined in a chamfered portion. [Diagram 5] 5 is a side view showing the wafer in which the chamfered portion is detected in FIG. 4. [Figure 6] FIG. 13 is a perspective view showing how a grinding tool is positioned above a wafer when performing a chamfer removing step. [Figure 7] FIG. 11 is a perspective view showing an aspect in which the chamfered portion is removed in a chamfered portion removing step. [Figure 8] 1A is a partially enlarged side view showing an aspect in which a grinding wheel is cut into a chamfered portion of a wafer, and FIG. 1B is a partially enlarged side view showing an aspect in which a part of the chamfered portion has been removed by a chamfered portion removing step. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, embodiments of a machining tool configured based on the present invention will be described in detail with reference to the accompanying drawings.
[0015] 1 shows a cutting device 1 equipped with cutting means 8 to which a grindstone 9, which is a processing tool of this embodiment, is attached. The cutting device 1 includes a housing 2 having a substantially rectangular parallelepiped shape, a cassette 4 (shown by a two-dot chain line) placed on a cassette table 4a of the housing 2, a carry-in / out means 3 for carrying a wafer 20 out of the cassette 4 to a temporary placement table 5, a transport means 6 having a swivel arm for transporting the wafer 20 carried out to the temporary placement table 5 to a chuck table 7, cutting means 8 including a grindstone cover 81 and a rotary shaft housing 82 to which a grindstone 9 of this embodiment for processing the wafer 20 held on the chuck table 7 is rotatably attached, and an upper The system is provided with an alignment means 10 for imaging the processing area of the wafer 20 held on the chuck table 7 and detecting the area to be processed by the cutting means 8, a height detection means 11 arranged adjacent to the alignment means 10 in the Y-axis direction and for detecting the thickness of the wafer 20 held on the chuck table 7, a cleaning and unloading means 13 for transporting the wafer 20 from the loading / unloading position where the chuck table 7 is positioned in Figure 1 to a cleaning device 12, and a display means 14 arranged on the upper part of the housing 2.
[0016] The chuck table 7 is composed of an adsorption chuck 71 that is formed of an air-permeable porous member and that constitutes a holding surface, and a frame 72 that surrounds the adsorption chuck 71, and is connected to suction means (not shown) via the frame 72. By operating the suction means, negative pressure is generated on the upper surface of the adsorption chuck 71, making it possible to suck and hold the workpiece.
[0017] The housing 2 is provided therein with an X-axis feed means for feeding the chuck table 7 in the X-axis direction for processing, a Y-axis feed means for indexing and feeding the cutting means 8 in the Y-axis direction perpendicular to the X-axis direction, a Z-axis feed means for moving in the Z-axis direction (up and down direction) perpendicular to the X-axis and Y-axis directions for cutting, and a rotation drive means for rotating the chuck table 7, as well as a control means (not shown) for controlling each operating part of the cutting device 1.
[0018] 2(a) is an enlarged perspective view of the main part of the cutting means 8 arranged in the cutting device 1 shown in FIG. 1, and FIG. 2(b) is an exploded perspective view of the configuration of FIG. 2(a). For convenience of explanation, the grindstone cover 81 that covers the grindstone 9 is omitted in FIG. 2. The cutting means 8 includes a rotating shaft housing 82, a rotating shaft 83 rotatably held in the rotating shaft housing 82, and a grindstone 9 that is attached to a tip end 83a of the rotating shaft 83 and is selected so as to satisfy conditions that will be described later in detail. A rotary drive source such as a motor (not shown) is accommodated on the other end side of the rotating shaft housing 82, and the rotary drive source rotates the rotating shaft 83 to rotate the grindstone 9 at high speed.
[0019] 2(b), the cutting means 8 includes a fixed flange 86 formed on the tip 83a side of the rotating shaft 83, a boss portion 86a protruding in the axial direction from the center of the fixed flange 86, a detachable flange 87 that engages with the boss portion 86a and cooperates with the fixed flange 86 to clamp the grindstone 9, and a nut 88 that screws into a male thread 86b formed on the side of the boss portion 86a to fasten the detachable flange 87. The opening 9a of the grindstone 9 is formed to correspond to the diameter of the boss portion 86a, and the boss portion 86a is inserted into the opening 9a of the grindstone 9, the detachable flange 87 is attached to the boss portion 86a, and the nut 88 is screwed into the male thread 86b and fastened, whereby the grindstone 9 is clamped between the fixed flange 86 and the detachable flange 87 and firmly fixed.
[0020] As shown in FIG. 2(b), the grinding wheel 9 includes an annular grinding wheel 91 and an annular polishing wheel 92 formed integrally with the grinding wheel 91. As shown in a partially enlarged cross-sectional view in the upper left of FIG. 2(b), the grinding wheel 91 is a flat grinding wheel having a first side surface 91a and a second side surface 91b, and the polishing wheel 92 is formed on at least one of the first side surface 91a or the second side surface 91b, and in the illustrated embodiment, is formed on the first side surface 91a side. As described above, the grinding wheel 9 constituting the processing tool of the present invention is not limited to forming the polishing wheel 92 on only one side surface of the grinding wheel 91, but may be formed on both the first side surface 91a and the second side surface 91b. The abrasive grains constituting the polishing wheel 92 and the grinding wheel 91 are, for example, diamond abrasive grains, and the bond material is preferably selected from, for example, a resin bond, a bidrified bond, and a metal bond. The polishing wheel 92 is a fine grindstone that smoothly finishes the surface that comes into contact with the workpiece, and the average grain size (hereinafter referred to as "grain size") of the diamond abrasive grains that make up the polishing wheel 92 is appropriately selected depending on the material of the workpiece, and is set to be smaller than the grain size of the diamond abrasive grains that make up the grinding wheel 91. The width (thickness) of the grinding wheel 91 and the width (thickness) of the polishing wheel 92 in this invention are required to satisfy certain conditions, and details will be described later.
[0021] With reference to FIGS. 3 to 8, a processing method for removing a chamfered portion of a wafer using the grindstone 9 of the processing tool of this embodiment, and conditions for the grinding wheel 91 and polishing wheel 92 that constitute the grindstone 9 will be described below.
[0022] (Whetstone preparation process) When the cutting device 1 shown in FIG. 1 is used to remove the chamfered portion 26c of the wafer 20 shown in FIG. 3, a grindstone preparation step is performed. The wafer 20 processed in this embodiment is a semiconductor (e.g., silicon) wafer in which a plurality of devices 22 are formed on the surface 20a by dividing the device 22 by the dividing lines 24, and includes a central region 26a in which the devices 22 are formed, an outer circumferential surplus region 26b surrounding the central region 26a, and a chamfered portion 26c in which the outer circumferential surplus region 26b is chamfered at its outer circumferential end. In FIG. 3, a circular dividing line 28 (shown by a broken line) dividing the central region 26a and the outer circumferential surplus region 26b is shown, but this is added for convenience of explanation and is not actually formed on the surface 20a of the wafer 20. Here, the wafer 20 has a thickness of, for example, 700 μm, and the radial length L from the outer circumferential end to be removed at the chamfered portion 26c is preset to 3.0 mm. Then, assuming that the width of the grinding wheel 91 is H and the width of the polishing wheel 92 is h, based on the radial length L (=3.0 mm) from the outer peripheral end to be removed, H+h>L (1) L / 3>h>L / 100···(2) The grindstone 9 is formed so as to satisfy both of the conditions (1) and (2). In this embodiment, the radial length L from the outer peripheral end to be removed in the chamfered portion 26c is 3.0 mm, while the width H of the grinding grindstone 91 is 3.0 mm, and the width h of the polishing grindstone 92 is 0.3 mm, so that the grindstone 9 is prepared to have a total width of 3.3 mm and a diameter of 58 mm.
[0023] Regarding the condition (2) of the grindstone 9 prepared by the grindstone preparation step described above, it is more preferable that the width h of the polishing grindstone 92 is set in a range of dimensions smaller than L / 20 and larger than L / 60. The grain size of the diamond grains constituting the polishing grindstone 92 is selected according to the physical properties of the silicon constituting the wafer 20, but it is preferable to select the grain size of the diamond grains constituting the grinding grindstone 91 in a range of 1.5 to 5 times the grain size of the diamond grains constituting the polishing grindstone 92. More specifically, when the grain size of the diamond grains constituting the polishing grindstone 92 is selected as 3 to 10 μm, the grain size of the diamond grains constituting the grinding grindstone 91 is set in a range of 15 to 50 μm, which is 1.5 to 5 times the grain size of the diamond grains constituting the grinding grindstone 91. If the grindstone 9 satisfying the above conditions is prepared in the grindstone preparation step, it is attached to the cutting means 8 as described based on FIG. 2(b). In this embodiment, the polishing wheel 92 is disposed on the tip end 83a side of the rotating shaft 83, and the grinding wheel 91 is disposed on the rotating shaft housing 82 side.
[0024] (Wafer holding process) After the grindstone preparation step has been carried out, the wafer 20 is carried out by the carry-in / out means 3 from the cassette 4 of the cutting device 1 described based on Fig. 1 and temporarily placed on the temporary placement table 5, and the transport means 6 is operated to suck the wafer 20 from the temporary placement table 5 and transport it to the chuck table 7. At this time, as shown in Fig. 3, the back surface 20b of the wafer 20 is placed on the chuck table 7 with its back surface 20b facing downward, and a suction means (not shown) is operated to generate negative pressure in the suction chuck 71 to hold the wafer by suction.
[0025] (Processing position detection process) After the wafer holding step is performed as described above, the X-axis feed means is operated to position the wafer 20 together with the chuck table 7 directly under the alignment means 10, and the wafer 20 is imaged to detect the center of the wafer 20 and the position of the region in the peripheral excess region 26b that is a radial length L (3.0 mm) from the peripheral end of the chamfered portion 26c to be removed. Furthermore, as shown in Fig. 4, the height detection means 11 detects the thickness of the region of the chamfered portion 26c to be removed, more specifically, the height Z0 of the surface of the chuck table 7 and the height Z1 of the surface 20a of the chamfered portion 26c of the wafer 20 as shown in Fig. 5, and the difference (Z0-Z1) is calculated as the thickness of the wafer 20, and information on these detected processing regions is stored in a control means (not shown).
[0026] (Bevel removal process) Next, based on the information of the processing area to be removed in the chamfered portion 26c detected by the above-mentioned processing position detection step and stored in the control means, the X-axis feed means and Y-axis feed means of the cutting device 1 are operated to position the chamfered portion 26c of the wafer 20 directly below the grindstone 9 attached to the cutting means 8 as shown in FIG. 6. At this time, the position of the polishing grindstone 92 of the grindstone 9 is positioned above the position that coincides with the radial length L from the outer circumferential end to be removed. Then, the grindstone 9 is rotated at a predetermined rotation speed (e.g., 30,000 rpm) in the direction indicated by the arrow R1, and the Z-axis feed means is operated to lower the cutting means 8 in the direction indicated by the arrow R2, so that the grindstone 9 cuts into the chamfered portion 26c of the wafer 20. At the same time, as shown in FIG. 7, the chuck table 7 is rotated at least once in the direction indicated by the arrow R3 at a predetermined rotation speed (e.g., 0.8 to 3 rpm). At this time, as shown in FIG. 8(a), the grindstone 9 removes a region of the radial length L from the outer peripheral end and is fed to a position where the cutting depth DZ (300 μm in this embodiment) is reached. As a result, the chamfered portion 26c forming the outer peripheral end of the outer peripheral excess region 26b of the wafer 20 is removed in an annular shape by the predetermined cutting depth DZ with a width of the radial length L from the outer peripheral end (see FIG. 8(b)), completing the chamfered portion removing process. The above-mentioned cutting depth DZ is set according to the thickness of the wafer 20 to be finished by grinding from the back surface 20b side in a back surface grinding process (details are omitted) performed in a process after the processing method of this embodiment is performed, and in this embodiment, the back surface 20b of the wafer 20 is ground to a thickness of 250 μm in a back surface grinding process performed later, so that the cutting depth DZ in the chamfered portion removing process is sufficient at 300 μm.
[0027] In this embodiment, the dimension of the width H of the grinding wheel 91 plus the width h of the polishing wheel 92 is formed to be larger than the radial length L from the outer peripheral end to be removed in the chamfered portion 26c forming the outer peripheral end of the outer peripheral excess region 26b (condition (1)), and the width h of the polishing wheel 92 is formed to be smaller than L / 3 and larger than L / 100 (condition (2)). As a result, as described above, by positioning the polishing wheel 92 on the center side of the wafer 20 and positioning the grinding wheel 91 on the outside, and rotating the wafer 20 at least once at a predetermined cutting depth, as shown in FIG. 8(b), the chamfered portion 26 can be roughly removed with the dimension of the radial length L from the outer peripheral end to be removed, and at the same time, the outer peripheral surface 20c forming the removed region 26d removed in the chamfered portion 26c can be finished, improving productivity.
[0028] Regarding the above-mentioned condition (2), it is more preferable that the width h of the polishing wheel 92 is set to a dimension smaller than L / 20 and larger than L / 60. For example, when the radial length L from the outer peripheral end to be removed is 3.00 mm (3000 μm), it is preferable to set the width h of the polishing wheel 92 to 50 to 150 μm and adjust the width H of the grinding wheel 91 to a range of 2950 to 3050 μm so that the total width (H+h) of the grinding wheel 9 is 3100 μm. By setting the width H of the grinding wheel 91 and the width h of the polishing wheel 92 in such a range, it becomes possible to roughly remove the region of the radial length L from the outer peripheral end to be removed on the wafer 20 by the grinding wheel 91, while at the same time more efficiently finishing the outer peripheral surface 20c that forms the removed region 26d removed in the chamfered portion 26c.
[0029] In addition, it is preferable to form the grain size of the diamond abrasive grains constituting the grinding wheel 91 in the range of 1.5 to 5 times the grain size of the diamond abrasive grains constituting the polishing wheel 92, and more specifically, when the grain size of the diamond abrasive grains constituting the polishing wheel 92 is set to 3 to 10 μm in consideration of the material of the wafer 20, it is preferable to set the grain size of the diamond abrasive grains constituting the grinding wheel 91 in the range of 15 to 50 μm. By doing so, the grinding wheel 91 and the polishing wheel 92 are secured to be in conformity when integrally formed, and the grinding wheel 9 is formed firmly, improving durability, and it is possible to efficiently roughly remove the region of the radial length L from the outer peripheral end to be removed in the wafer 20, while smoothly finishing the outer peripheral surface 20c forming the removed region 26d removed in the chamfered portion 26c.
[0030] In the above embodiment, when the grindstone 9 is attached to the rotating shaft 83 of the grinding means 8, the polishing grindstone 92 is attached to the tip 83a side of the rotating shaft 82 and the grinding grindstone 91 is attached to the rotating shaft housing 82 side, but the present invention is not limited to this, and the chamfered portion removing step of the above processing method can also be performed by attaching the polishing grindstone 92 side to the rotating shaft housing 82 side and the grinding grindstone 91 to the tip 83a side of the rotating shaft 83. In that case, when performing the chamfered portion removing step, the grindstone 9 of the cutting means 8 is positioned so that the polishing grindstone 92 side is on the center side of the wafer 20 in the radial direction, more specifically, for example, the grindstone 9 of the cutting means 8 is positioned on the lower left side in the figure (the area where the notch 25 of the wafer 20 shown in FIG. 7 is positioned) across the wafer 20 shown in FIG. 7, and the chuck table 7 is rotated to perform the chamfered portion removing step. [Explanation of symbols]
[0031] 1:Cutting device 2: Housing 3: Carrying in / out means 4: Cassette 5: Temporary table 6: Means of transportation 7: Chuck table 71: Suction chuck 72:Frame body 8: Cutting means 81:Whetstone cover 82: Rotating shaft housing 83: Rotation axis 83a:Tip 86: Fixed flange 86a: Boss Department 86b: Male thread 87: Detachable flange 88: Nut 9: Grindstone 91: Grinding wheel 91a: First aspect 91b: The second aspect 92: Grinding stone 10: Alignment means 11: Height detection means 12: Cleaning equipment 13: Cleaning and carrying out means 14:Display means 20: Wafer 20a: Surface 20b: Back side 20c: Outer surface 22: Device 24: Planned division line 25: Notch 26a: Central area 26b: Surplus outer area 26c: Chamfered part 26d: Removal area 28: Partition line
Claims
1. A processing tool for removing a chamfered portion of a wafer having a central region, a peripheral excess region surrounding the central region, and a chamfered portion formed in the peripheral excess region, comprising: The grinding wheel has an opening for insertion into a rotating shaft and has a first side surface and a second side surface, and a polishing wheel is formed on at least one of the first side surface or the second side surface, If the radial length from the outer peripheral end of the chamfered portion to be removed is L, the width of the grinding wheel is H, and the width of the polishing wheel is h, then H+h>L...(1) L / 3>h>L / 100...(2) The machining tool is formed so as to satisfy both of the conditions (1) and (2) specified in the above.
2. The machining tool according to claim 1, wherein the particle size of the diamond abrasive grains constituting the polishing stone is selected according to the material of the workpiece, and the particle size of the diamond abrasive grains constituting the grinding stone is selected in the range of 1.5 to 5 times the particle size of the diamond abrasive grains constituting the polishing stone.
3. 3. The machining tool according to claim 2, wherein the bond material constituting said polishing wheel and said grinding wheel is selected from the group consisting of a resin bond, a vitrified bond, and a metal bond.
4. 2. The processing tool according to claim 1, wherein the central region is a semiconductor wafer having a device region in which a plurality of devices are partitioned by planned division lines.
Citation Information
Patent Citations
Method of dividing laminated wafer
JP2010225976A
Wafer processing method
JP2014003198A
