Method for manufacturing electrode

The dry film forming method for forming a carbon coat layer on electrodes reduces contact area between carbon and binder, addressing resistance issues and improving electrode conductivity.

JP2024166679AInactive Publication Date: 2024-11-29TOYOTA JIDOSHA KK
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023082926
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-19
Publication Date
2024-11-29
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing electrode manufacturing methods result in increased resistance due to the large contact area between carbon materials and binders when using a wet film forming method, obstructing the conductive path.

Method used

A dry film forming method is employed to form a carbon coat layer using a composite material of carbon and binder in powder form, reducing the contact area to point contacts and maintaining a good conductive path.

Benefits of technology

This method effectively suppresses resistance in the electrode, enhancing its performance by ensuring effective conductive pathways.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024166679000001_ABST
    Figure 2024166679000001_ABST
Patent Text Reader

Abstract

To provide a method for manufacturing an electrode of which resistance is suppressed.SOLUTION: A method for manufacturing an electrode having a collector, a carbon coat layer, and an active material layer in that order in a thickness direction according to the present disclosure includes: a preparation step of preparing a composite material including a carbon material and a binder; a carbon coat layer formation step of forming the carbon coat layer on the collector by a dry deposition method using the composition material; and an active material layer formation step of forming the active material on the surface of the carbon coat layer which is on the opposite side of the side where the collector is formed in the thickness direction.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a method for manufacturing an electrode. [Background technology]

[0002] In the field of batteries, an electrode having a carbon coating layer provided on a current collector is known.

[0003] For example, Patent Document 1 discloses providing a concave-convex pattern on the surface of a carbon coating layer facing an active material layer. In particular, Patent Document 1 discloses a method for manufacturing an electrode in which a carbon coating layer is formed using a paint (slurry) containing a solvent, a binder, and a carbon material. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2019-087489 A Summary of the Invention [Problem to be solved by the invention]

[0005] In order to improve the performance of a battery, an electrode having reduced resistance is required. The present disclosure has been made in view of the above-mentioned circumstances, and has as its main object to provide a method for manufacturing an electrode having reduced resistance. [Means for solving the problem]

[0006] [1] A method for manufacturing an electrode having a current collector, a carbon coating layer, and an active material layer in this order in a thickness direction, the method comprising: a preparation step of preparing a composite material containing a carbon material and a binder; a carbon coating layer formation step of forming the carbon coating layer on the current collector by a dry film formation method using the composite material; and an active material layer formation step of forming the active material layer on a surface of the carbon coating layer opposite to the current collector in the thickness direction. Effect of the Invention

[0007] The present disclosure provides an advantage in that an electrode with reduced resistance can be manufactured. [Brief description of the drawings]

[0008] [Figure 1] FIG. 1 is a flow diagram illustrating a method for manufacturing an electrode in the present disclosure. [Diagram 2] 1 is a schematic cross-sectional view illustrating an electrode according to the present disclosure. [Diagram 3] 1 is a graph showing the results of an example and a comparative example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] The method for producing an electrode according to the present disclosure will be described in detail below. Fig. 1 is a flow diagram illustrating the method for producing an electrode according to the present disclosure. First, a composite material containing a carbon material and a binder is prepared (preparation step). Next, a carbon coat layer is formed on the current collector by a dry film formation method using the composite material (carbon coat layer formation step). Then, the active material layer is formed on the surface of the carbon coat layer opposite to the current collector in the thickness direction (active material layer formation step).

[0010] According to the present disclosure, since the carbon coating layer is formed by a dry film formation method, an electrode with reduced resistance can be manufactured.

[0011] As disclosed in the above-mentioned Patent Document 1, it is known that a carbon coating layer is formed by applying a slurry onto a current collector, that is, by a so-called wet coating method. On the other hand, when a carbon material (conductive assistant) is present in a dissolved binder, as in a slurry, the contact area between the carbon material and the binder increases, and the conductive path between the conductive assistants is inhibited, and there is a risk of an increase in resistance. In contrast, in the manufacturing method of an electrode in the present disclosure, a carbon coating layer is formed by a dry coating method. That is, the carbon coating layer is formed when the binder is in a powder state. Therefore, the contact between the carbon material and the binder can be a point contact, and the contact area between the carbon material and the binder can be reduced. As a result, it is possible to suppress the conductive path from being inhibited, and the resistance can be suppressed.

[0012] 1. Preparation process The preparation step in the present disclosure is a step of preparing a composite material containing a carbon material and a binder.

[0013] The carbon material functions as a conductive assistant in the carbon coating layer. The carbon material is not particularly limited as long as it functions as a conductive assistant in the field of batteries. Examples of the carbon material include particulate carbon materials such as acetylene black (AB) and ketjen black (KB), and fibrous carbon materials such as carbon fibers, carbon nanotubes (CNT), and carbon nanofibers (CNF).

[0014] Average particle size of conductive additive (D 50 ) is, for example, 1 nm or more and 500 nm or less. The average particle size is the average particle size (D 50 ) refers to the cumulative 50% particle size in the volume-based particle size distribution measured with a laser diffraction particle size analyzer.

[0015] The proportion of the carbon material in the composite material is, for example, 50% by weight or more and 80% by weight or less.

[0016] The binder may be a known material conventionally used in the field of batteries, such as rubber-based binders such as butylene rubber (BR) and styrene butadiene rubber (SBR), and fluoride-based binders such as polyvinylidene fluoride (PVdF).

[0017] The proportion of the binder in the carbon material is, for example, 20% by weight or more and 50% by weight or less.

[0018] Examples of methods for obtaining a composite material include conventional methods using a particle composite device, etc. The conditions of the device (composite conditions) can be appropriately set.

[0019] In the carbon coating layer forming step described below, the carbon coating layer is formed by a dry film forming method, so the composite material is usually a powder and does not contain a liquid component such as a solvent.

[0020] 2. Carbon coat layer formation process The carbon coating layer forming step in the present disclosure is a step of forming a carbon coating layer on the current collector by a dry film forming method using the composite material.

[0021] The dry film-forming method is not particularly limited as long as it is possible to form a carbon coating layer using the composite material in a powder state, and an example of the dry film-forming method is an electrostatic screen film-forming method.

[0022] The thickness of the carbon coating layer is not particularly limited, but is, for example, not less than 0.1 μm and not more than 100 μm.

[0023] The material of the current collector is not particularly limited, and can be any conventional material used as a positive electrode current collector or a negative electrode current collector. The material of the positive electrode current collector can be, for example, Al, SUS, or Ni. The material of the negative electrode current collector can be, for example, Cu, SUS, or Ni. The thickness of the current collector is not particularly limited.

[0024] 3. Active material layer formation process The active material layer forming step in the present disclosure is a step of forming an active material layer on the surface of the carbon coating layer opposite to the current collector.

[0025] The active material layer forming step may be, for example, a wet film-forming method using a slurry containing at least an active material and a solvent, or a dry film-forming method using a composite material containing at least an active material, but the latter is preferred because the solvent contained in the slurry may cause peeling of the carbon coat. An example of the dry film-forming method is the electrostatic screen method described above.

[0026] The active material layer may be a positive electrode active material layer or a negative electrode active material layer. When the active material layer is a positive electrode active material layer, the active material in the composite is a positive electrode active material. A typical example of the positive electrode active material is an oxide active material. For example, LiNi 1 / 3 Co 1 / 3 Mn 1 / 3 O2, etc., rock salt layered active material, Li(Ni 0.5 Mn 1.5 )O4 and other spinel-type active materials, and LiFePO4 and other olivine-type active materials.

[0027] Examples of the negative electrode active material include carbon active materials such as mesocarbon microbeads (MCMB), Li4Ti5O 12 Examples of the active material include oxide active materials such as SiO and metal active materials such as Si. Examples of the active material include highly oriented graphite (HOPG), hard carbon, and soft carbon. Examples of the active material include oxide active materials such as Nb2O5. Examples of the active material include metal active materials such as In, Al, Si, and Sn.

[0028] The composite may contain at least one of a binder, a conductive assistant, and an electrolyte, as necessary. The binder and the conductive assistant are as described above. The electrolyte in the composite is preferably a solid electrolyte.

[0029] In the active material layer forming step, a fixing process may be performed in which the binder in the composite is softened or melted by a hot press and fixed to the carbon coating layer. In addition, the electrode manufacturing method according to the present disclosure may include a densification process in which the current collector, the carbon coating layer, and the active material layer are pressed in a thickness direction to densify them, after the active material layer forming step.

[0030] 4. Electrode Fig. 2 is a schematic cross-sectional view illustrating an electrode according to the present disclosure. As shown in Fig. 2, the electrode 10 has, in the thickness direction z, a current collector 1, a carbon coating layer 2, and an active material layer 3. The electrode 10 may be a positive electrode or a negative electrode.

[0031] The electrode in the present disclosure is generally used in a battery. The battery is typically a Li-ion battery. The battery may be an all-solid-state battery using a solid electrolyte as the electrolyte, or a liquid-based battery using a liquid electrolyte (electrolytic solution) as the electrolyte.

[0032] Examples of applications of the battery include power sources for vehicles such as hybrid electric vehicles (HEVs), plug-in hybrid electric vehicles (PHEVs), electric vehicles (BEVs), gasoline-powered vehicles, and diesel-powered vehicles. In particular, the battery is preferably used as a driving power source for hybrid electric vehicles (HEVs), plug-in hybrid electric vehicles (PHEVs), or electric vehicles (BEVs). The battery of the present disclosure may also be used as a power source for moving objects other than vehicles (e.g., railways, ships, and aircraft), and may also be used as a power source for electrical appliances such as information processing devices.

[0033] The present disclosure is not limited to the above-described embodiment. The above-described embodiment is merely an example, and any configuration that is substantially the same as the technical idea described in the claims of the present disclosure and that exhibits similar effects is included in the technical scope of the present disclosure. EXAMPLES

[0034] [Example] A positive electrode having a positive electrode current collector, a carbon coating layer, and a positive electrode active material layer was prepared as follows. First, acetylene black (Li-435, manufactured by Denka Co., Ltd.) as a carbon material and PVdF (LBG8200, manufactured by Arkema Co., Ltd.) as a binder were weighed out so that the weight ratio of carbon material:binder was 60:40. The weighed acetylene black and PVdF were introduced into an MP mixer (manufactured by Nippon Coke & Engineering Co., Ltd.) equipped with a spherical tank and composited at 10,000 rpm for 10 minutes. As a result, a composite powder was obtained.

[0035] Next, a carbon coating layer was formed on a positive electrode current collector (Al foil) by a dry film formation method using the composite powder. Specifically, the carbon coating layer was formed using an electrostatic screen duster manufactured by Belc Industrial Co., Ltd. The film formation conditions in the electrostatic screen duster were as follows. Voltage: 0.5kV Distance between collector and screen: 0.5cm Weight: 1mg / cm 2

[0036] Furthermore, a positive electrode active material layer was formed using a positive electrode mixture containing a positive electrode active material. For the positive electrode mixture, nickel cobalt manganese oxide lithium (manufactured by Hunan Ruixiang Co., Ltd.) was used as the positive electrode active material, the above-mentioned acetylene black was used as the conductive additive, and the above-mentioned PVdF was used as the binder. In the positive electrode mixture, the ratio of the positive electrode active material, the conductive additive, and the binder was 97.5:1.5:1 by weight. A positive electrode active material layer was formed on the carbon coat layer by a dry film formation method. Note that, in the dry film formation method, the basis weight was 20 mg / cm. 2 The same procedure was followed as for the formation of the carbon coat layer, except that the above-mentioned conditions were met. A load of 15 t was applied for 1 minute using a flat plate heated to 160°C. This caused the binder to soften and melt, and the positive electrode active material layer was fixed onto the carbon coat layer, thereby obtaining an electrode. The obtained electrode was pressed using a roll press machine (manufactured by Nagano Roll Press Co., Ltd.) until the density reached 3.5 g / cm. 3 The densified electrode was used as an evaluation electrode.

[0037] [Comparative Example 1] An electrode was prepared in the same manner as in the example, except that no carbon coating layer was provided.

[0038] [Comparative Example 2] An electrode was produced in the same manner as in the example, except that a carbon coating layer was formed by a wet film formation method as described below. First, a solvent (N-methyl-2-pyrrolidone) was added to acetylene black and PVdF weighed in the same proportions as in the example. These were introduced into a mixer (manufactured by Thinky Corporation) and composited at 2000 rpm for 5 minutes. This resulted in a composite slurry. The composite slurry obtained was applied onto a positive electrode current collector using a coater and dried using a hot plate. This resulted in a carbon coating layer. The basis weight was 1 mg / cm. 2 It was decided.

[0039] [evaluation] The composite interface resistance was measured for each of the evaluation batteries obtained in the Examples and Comparative Examples. For the measurement, an electrode resistance measurement system (RM2610, manufactured by HIOKI EE Corporation) was used. The results are shown in FIG.

[0040] As shown in FIG. 3, the resistance of Comparative Example 2 and the Example is lower than that of Comparative Example 1, indicating that the resistance can be reduced by the carbon coating layer. In addition, the resistance of the Example is lower than that of Comparative Example 2, indicating that the resistance can be further reduced by forming a carbon coat by the dry film formation method. In the carbon coating layer formed by the wet film formation method, the binder melts and diffuses, so the contact area between the binder and the conductive assistant is large, the contact area between the conductive assistants is reduced, and it is considered that the conductive path is inhibited. On the other hand, in the carbon coating layer formed by the dry film formation method, the binder and the conductive assistant are in contact at points, and the contact area between the conductive assistants is sufficiently secured, and it is considered that a good conductive path is formed. [Explanation of symbols]

[0041] 1...Current collector 2...Carbon coating layer 3...Active material layer 10...electrode

Claims

[Claim 1] A method for producing an electrode having a current collector, a carbon coating layer, and an active material layer in this order in a thickness direction, comprising the steps of: A preparation step of preparing a composite material containing a carbon material and a binder; a carbon coating layer forming step of forming the carbon coating layer on the current collector by a dry film forming method using the composite material; and forming the active material layer on a surface of the carbon coating layer opposite to the current collector in the thickness direction.

Citation Information

Patent Citations

  • Carbon coated layer, paint, current collector, battery, forming method of carbon coated layer, and gravure plate