Method for manufacturing golf ball
The golf ball manufacturing process addresses low spin challenges by heat-treating the intermediate layer-coated core to control crystallinity and hardness, improving flight distance and spin rates for both full shots and short games.
Patent Information
- Application Number
- JP2023083711
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-22
- Publication Date
- 2024-12-04
Smart Images

Figure 2024167554000001 
Figure 2024167554000002 
Figure 2024167554000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a golf ball having a rubber core, at least one resin intermediate layer, and a urethane resin cover. [Background technology]
[0002] It has been known that a good flight can be obtained by designing a ball structure that reduces the spin rate of the ball during a full shot such as with a driver (W#1). In recent years, in order to improve short game performance, balls that can obtain a high level of spin rate during an approach have been developed and researched. As an example, the golf balls described in Patent Documents 1 and 2 have been proposed. These golf balls have a so-called hard inner / soft outer layer structure in which an intermediate layer is interposed between the core and the outermost layer, and the hardness of the inner intermediate layer is set higher than that of the outer cover. That is, by providing a resin material harder than the cover between the rubber elastic core and the soft cover material, the goals of reducing the spin rate during a full shot and maintaining a high level of approach controllability in a short game are simultaneously achieved.
[0003] However, in recent years, in addition to drivers (W#1), there is a demand for low spin on the ball during full shots, in order to obtain a desired flight distance by reducing the spin on the ball during full shots with middle or larger irons. Therefore, a new challenge has arisen to increase the level of low spin on full shots with irons. However, as described above, in a three-piece or larger multi-layer golf ball having a layer structure of a hard inner layer and a soft outer layer, further increasing the number of layers increases the number of steps in the manufacturing process of the golf ball, resulting in high costs. In addition, the more layers there are, the more likely the inner layer structure of the ball centered on the core will become eccentric, which may make it difficult to manufacture a high-quality ball. In addition, there is a limit to the hardness gradient (hardness distribution) between the inner and outer layers of the rubber core, the type of material of the intermediate layer and the cover, the material hardness, and the thickness of each layer, and this has already been proposed in many patent publications.
[0004] Therefore, rather than focusing on the selection and adjustment of the materials, thickness, and hardness of the core, intermediate layer, and cover that have been used in the past, there is room for improvement in the manufacturing process in order to improve the physical properties of the ball, that is, to reduce the spin rate of the ball on driver shots, to increase the spin rate of the ball in short games, and even to increase the flight distance by reducing the spin rate of the ball on full shots with an iron.
[0005] For example, Patent Documents 3 to 6 are cited as prior arts for subjecting cores and balls to heat treatment. Patent Documents 3 and 4 disclose a method for reducing volatile substances contained in a core by heat-treating a core made by vulcanizing a rubber material under certain conditions. Patent Document 5 proposes that a golf ball with excellent resilience performance can be manufactured without impairing the appearance such as deformation of dimples by heat-treating an intermediate-layer-covered sphere formed around the core at 40 to 80°C. Patent Document 6 describes a method for customizing a golf ball by heating the ball to a preselected temperature to change the physical properties of the ball. However, among Patent Documents 3 to 6, Patent Documents 3 and 4 disclose heat treatment of a core to reduce volatile substances contained in the core, while Patent Document 6 discloses heat treatment of a golf ball already covered with a completed cover. Patent Document 5 discloses that the object of heat treatment is an intermediate-layer-covered sphere, but the heat treatment temperature is low at 40 to 80°C. The golf balls described in Patent Documents 3 to 6 all have different features that address the issues of reducing the spin rate of the ball on driver shots, increasing the amount of spin on the ball in short games, and reducing the spin rate of the ball on full shots with an iron, and there is room to explore and consider methods other than these heat treatments. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] Japanese Patent Application Publication No. 09-239068 [Patent Document 2] JP 2002-765 A [Patent Document 3] JP 2017-225686 A [Patent Document 4] JP 2017-225682 A [Patent Document 5] JP 2004-159840 A [Patent Document 6] JP 2011-167508 A Summary of the Invention [Problem to be solved by the invention]
[0007] The present invention has been made in consideration of the above circumstances, and aims to provide a method for producing a golf ball that can improve flight performance by fully demonstrating the low spin characteristics when hitting the golf ball not only with a driver (W#1) but also on full shots with an iron. [Means for solving the problem]
[0008] As a result of extensive research into achieving the above-mentioned object, the inventors have found that in the manufacturing process of a golf ball having a core, intermediate layer, and cover, a core is coated with an intermediate layer to form an intermediate layer-coated sphere, and then the intermediate layer-coated sphere is subjected to a heat treatment at a temperature above the melting point of the base resin of the resin composition of the intermediate layer and below 160°C. When the surface hardness of the intermediate layer-coated sphere was then measured, it was unexpectedly found that the surface hardness increased and that the completed golf ball produced a low spin rate when hit with a full shot with an iron, which led to the creation of the present invention.
[0009] That is, the present invention is characterized in that, unlike the above-mentioned Patent Document 6, a predetermined heat treatment is not performed on a completed golf ball, but rather, in the manufacturing process of a golf ball, a predetermined heat treatment is performed on the intermediate layer-covered sphere after obtaining an intermediate layer-covered sphere having an intermediate layer formed around a core. This method controls the crystallinity of the crystal phase of the intermediate layer (resin layer) in the intermediate layer-covered sphere, and increases the surface hardness of the intermediate layer-covered sphere, thereby reducing the spin rate during a full shot with an iron. When a golf ball is heat-treated after completion as in Patent Document 6, the degree of control of the crystallinity of the crystal phase in the intermediate layer (resin layer) becomes smaller than that of the present invention in which the intermediate layer-covered sphere is directly heat-treated, and it is presumed that the low spin effect during a full shot is insufficient. In addition, when a golf ball is heat-treated after completion, the dimples may change in shape due to the heat treatment, and the desired aerodynamic characteristics may not be obtained. In contrast, in the case of the present invention in which the intermediate layer-covered sphere is directly heat-treated, there is no risk of dimple damage due to the heat treatment.
[0010] Accordingly, the present invention provides a method for producing a golf ball as follows: 1. A method for manufacturing a golf ball having a core, at least one intermediate layer, and a cover, the core being made of a rubber material, the intermediate layer being made of a resin composition, and the cover being made of a urethane resin material, comprising the steps of: (1) coating the core with at least one intermediate layer to form an intermediate-layer-coated sphere; (2) subjecting the intermediate layer-coated sphere to a heat treatment at a temperature equal to or higher than the melting point of the base resin of the intermediate layer and lower than 160°C; and Then, a step (3) of coating the intermediate layer-coated sphere with the cover to form a covered sphere. 2. A method for manufacturing a golf ball comprising the steps of: 2. The method according to claim 1, wherein in step (2), the intermediate layer-coated spheres are heated at a temperature of 90 to 150°C. 3. The method according to 1 or 2 above, wherein in step (2), the intermediate layer-coated spheres are heat-treated for 3 to 60 minutes. 4. The method according to 1 or 2 above, wherein in the step (1), the resin composition for the intermediate layer is injection molded around the core to form an intermediate layer-coated sphere. 5. The manufacturing method according to 1 or 2 above, wherein in the step (3), a urethane resin material for the cover is injection molded around the intermediate layer-covered sphere to form a cover-covered sphere. 6. The method according to 1 or 2 above, wherein the base resin of the resin composition for the intermediate layer is an ionomer resin. Effect of the Invention
[0011] The golf ball of the present invention not only reduces the spin rate of the ball on driver shots, but also increases the flight distance by reducing the spin rate of the ball on full shots with an iron, and further maintains a high level of spin on the ball in short games, improving approach controllability. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] The present invention will now be described in further detail. The method for producing a golf ball of the present invention is a method for producing a golf ball having a core, at least one intermediate layer, and a cover.
[0013] The core is made of a rubber material. The core rubber material used in the present invention is preferably one that does not lose basic performance such as hardness and resilience even when exposed to a temperature equal to or higher than the melting point of the resin material of the intermediate layer described below. In addition, the core rubber material used in the present invention is preferably one that can fully secure the resilience required for a golf ball. Furthermore, a core having a predetermined hardness gradient (hardness distribution) inside can be obtained by selecting the composition of the rubber material and the vulcanization conditions. Specifically, the composition of such a core is preferably formed by hot molding a rubber composition containing at least the following components (A) to (D). (A) Base rubber (B) Organic peroxide (C)Water (D) Sulfur
[0014] The base rubber of the component (A) is not particularly limited, but it is particularly preferable to use polybutadiene. As the type of polybutadiene, commercially available products can be used, for example, trade names "BR 01", "BR 51", "BR 730", "BR T700" (manufactured by ENEOS Materials Co., Ltd.). The proportion of polybutadiene in the base rubber is preferably 60% by mass or more, more preferably 80% by mass or more. In addition to the polybutadiene, other rubber components can be blended into the base rubber within a range that does not impair the effects of the present invention. Examples of rubber components other than the polybutadiene include polybutadienes other than the polybutadienes, and other diene rubbers, such as styrene butadiene rubber, natural rubber, isoprene rubber, and ethylene propylene diene rubber.
[0015] (B) Organic peroxide is used as a crosslinking initiator. Specifically, it is preferable to use an organic peroxide with a relatively high thermal decomposition temperature, specifically, a high-temperature organic peroxide with a 1-minute half-life temperature of about 165 to 185°C is used, and for example, dialkyl peroxides can be mentioned. Examples of dialkyl peroxides include dicumyl peroxide (NOF Corp.'s "Percumyl D"), 2,5-dimethyl-2,5-di(t-butylperoxy)hexane (NOF Corp.'s "Perhexa 25B"), di(2-t-butylperoxyisopropyl)benzene (NOF Corp.'s "Perbutyl P"), etc., and dicumyl peroxide can be preferably used. These may be used alone or in combination of two or more. The half-life is one of the indicators of the degree of decomposition speed of an organic peroxide, and is indicated by the time required for the original organic peroxide to decompose and the amount of active oxygen to be reduced to 1 / 2. The vulcanization temperature of the rubber composition for the core is usually within the range of 120 to 190° C., and within this range, organic peroxides with a high one-minute half-life temperature of about 165 to 185° C. undergo thermal decomposition relatively slowly. According to the rubber composition of the present invention, the amount of free radicals produced, which increases with the passage of vulcanization time, is adjusted to obtain a core, which is a cross-linked rubber product having a specific internal hardness profile.
[0016] The water (C) is not particularly limited and may be distilled water or tap water, but it is particularly preferred to use distilled water that does not contain impurities. The amount of water blended is preferably 0.1 part by mass or more, more preferably 0.3 part by mass or more, per 100 parts by mass of the base rubber, and the upper limit is preferably 5 parts by mass or less, more preferably 4 parts by mass or less.
[0017] By directly blending water (materials containing water) into the core material, the decomposition of organic peroxide during core blending can be promoted. In addition, it is known that the decomposition efficiency of organic peroxide in the rubber composition for the core changes depending on the temperature, and the higher the temperature, the higher the decomposition efficiency. If the temperature is too high, the amount of decomposed radicals becomes too large, and the radicals recombine with each other or become inactivated. As a result, the radicals that work effectively for crosslinking decrease. Here, when the organic peroxide decomposes during core vulcanization and generates decomposition heat, the temperature near the core surface remains almost the same as that of the vulcanization mold, but the temperature near the core center becomes much higher than the mold temperature because the decomposition heat of the organic peroxide that decomposed from the outside accumulates. When water is directly blended into the core, water acts to promote the decomposition of the organic peroxide, so the above-mentioned radical reaction can be changed between the core center and the core surface. In other words, the decomposition of the organic peroxide is further promoted near the center of the core, and the inactivation of radicals is further promoted, further reducing the amount of available radicals, making it possible to obtain a core having a significantly different crosslink density between the core center and the core surface, and also a core having different dynamic viscoelastic properties in the center of the core.
[0018] (D) By using sulfur, the difference in hardness between the inside and outside of the core can be increased. Specific examples of (D) sulfur include products under the trade names "Sunmix S-80N" (Sanshin Chemical Industry Co., Ltd.) and "Sulfax-5" (Tsurumi Chemical Industry Co., Ltd.). The amount of sulfur may be more than 0, preferably 0.005 parts by mass or more, and more preferably 0.01 parts by mass or more, per 100 parts by mass of the base rubber. There is no particular upper limit to the amount of sulfur, but it is preferably 0.1 parts by mass or less, more preferably 0.05 parts by mass or less, and even more preferably 0.03 parts by mass or less. If the amount of sulfur is too large, the resilience may be significantly reduced, or durability against repeated impact may be reduced.
[0019] Regarding the blending ratio of the above (C) component and (D) component, the mass ratio of (D) / (C) is preferably 0.02 or more, more preferably 0.03 or more, and even more preferably 0.04 or more, and the upper limit is preferably 0.20 or less, more preferably 0.16 or less, and even more preferably 0.12 or less. If the above numerical range is exceeded, it becomes difficult to achieve the desired core hardness distribution, and it may become impossible to achieve both the advantageous flight distance due to the low spin rate at the time of full shot and good durability against repeated impacts. Note that the above (D) component refers to the mass of the sulfur component contained in the product, not the mass of the sulfur product itself.
[0020] In the above rubber composition, in addition to the above-mentioned components (A) to (D), a co-crosslinking agent (E) and an inert filler (F) can be blended, and an antioxidant and an organic sulfur compound can be blended as necessary. These components are described in detail below.
[0021] (E) Co-crosslinking agent includes, for example, unsaturated carboxylic acid, metal salt of unsaturated carboxylic acid, etc. Specific examples of unsaturated carboxylic acid include acrylic acid, methacrylic acid, maleic acid, fumaric acid, etc., and acrylic acid and methacrylic acid are particularly preferably used. Metal salt of unsaturated carboxylic acid is not particularly limited, but includes, for example, the above unsaturated carboxylic acid neutralized with a desired metal ion. Specific examples include zinc salt and magnesium salt of methacrylic acid, acrylic acid, etc., and zinc acrylate is particularly preferably used.
[0022] The unsaturated carboxylic acid and / or metal salt thereof is blended in an amount of usually at least 5 parts by weight, preferably at least 9 parts by weight, and more preferably at least 13 parts by weight, with the upper limit usually not exceeding 60 parts by weight, preferably not exceeding 50 parts by weight, and more preferably not exceeding 40 parts by weight, per 100 parts by weight of the base rubber. If the blended amount is too high, the ball may become too hard, resulting in an unbearable feel on impact, whereas if the blended amount is too low, the resilience may decrease.
[0023] As the (F) inert filler, for example, zinc oxide, barium sulfate, calcium carbonate, etc. can be suitably used. These may be used alone or in combination of two or more. The amount of the inert filler is preferably 1 part by mass or more, more preferably 5 parts by mass or more, and preferably 30 parts by mass or less, more preferably 25 parts by mass or less, and even more preferably 20 parts by mass or less, per 100 parts by mass of the base rubber. The amount of the inert filler is adjusted to adjust the specific gravity of the core, and if the amount is too small, it may not be possible to obtain the appropriate mass and suitable resilience.
[0024] Furthermore, an anti-aging agent can be added as necessary, and examples of commercially available products include Nocrac MB, Nocrac NS-6, Nocrac NS-30 (manufactured by Ouchi Shinko Chemical Industry Co., Ltd.), Yoshinox 425 (manufactured by Yoshitomi Pharmaceutical Co., Ltd.), etc. These may be used alone or in combination of two or more kinds.
[0025] The amount of the antioxidant blended per 100 parts by mass of the base rubber is preferably at least 0 part by mass, more preferably at least 0.05 parts by mass, and particularly preferably at least 0.1 parts by mass, with the upper limit being preferably no more than 3 parts by mass, more preferably no more than 2 parts by mass, particularly preferably no more than 1 part by mass, and most preferably no more than 0.5 parts by mass. If the blended amount is too high or too low, suitable resilience and durability may not be obtained.
[0026] In addition, the core may contain an organic sulfur compound to provide good resilience. The organic sulfur compound is not particularly limited as long as it can improve the resilience of the golf ball, and examples thereof include thiophenols, thionaphthols, halogenated thiophenols, and metal salts thereof. More specifically, pentachlorothiophenol, pentafluorothiophenol, pentabromothiophenol, parachlorothiophenol, zinc salt of pentachlorothiophenol, zinc salt of pentafluorothiophenol, zinc salt of pentabromothiophenol, zinc salt of parachlorothiophenol, diphenyl polysulfide with 2 to 4 sulfur, dibenzyl polysulfide, dibenzoyl polysulfide, dibenzothiazoyl polysulfide, dithiobenzoyl polysulfide, and the like are included, and the zinc salt of pentachlorothiophenol is particularly preferably used. The amount of the organic sulfur compound is preferably 0 parts by weight or more, more preferably 0.05 parts by weight or more, and even more preferably 0.1 parts by weight or more, with the upper limit being preferably 5 parts by weight or less, more preferably 3 parts by weight or less, and even more preferably 2.5 parts by weight or less, per 100 parts by weight of the base rubber. If the amount is too large, the effect of improving resilience (especially when hitting with W#1) cannot be expected any more, the core may become too soft, or the feeling of hitting may become poor. On the other hand, if the amount is too small, the effect of improving resilience cannot be expected.
[0027] The core can be produced by vulcanizing and curing a rubber composition containing the above-mentioned components. For example, the rubber composition is kneaded using a kneading machine such as a Banbury mixer or a roll, compression molded or injection molded using a core mold, and the molded body is appropriately heated at a temperature sufficient for the organic peroxide and co-crosslinking agent to act, that is, 100 to 200°C, preferably 140 to 180°C, for 10 to 40 minutes, to cure the molded body.
[0028] In the present invention, the core may be formed as a single layer or a multi-layer rubber core, but in the case of a multi-layer core, peeling may occur at the interface when the core is repeatedly struck, resulting in poor durability.
[0029] The diameter of the core is not particularly limited, but is preferably 35.5 mm or more, more preferably 37.5 mm or more, and even more preferably 38.3 mm or more, and the upper limit is preferably 39.5 mm or less, more preferably 39.2 mm or less, and even more preferably 38.8 mm or less. If the core diameter is too small, the actual initial velocity of a full shot is low, and the target flight distance cannot be obtained, or the hitting feeling may be too hard. On the other hand, if the core diameter is too large, the durability against repeated hitting may be deteriorated.
[0030] The deflection (mm) of the core when subjected to an initial load of 98N (10kgf) to a final load of 1,275N (130kgf) is not particularly limited, but is preferably 2.5mm or more, more preferably 2.7mm or more, and even more preferably 2.9mm or more, with the upper limit being preferably 3.5mm or less, more preferably 3.4mm or less, and even more preferably 3.3mm or less. If the deflection of the core is too small, i.e., if the core is too hard, the ball may have too much spin and may not fly, or the feel on impact may be too hard. On the other hand, if the deflection of the core is too large, i.e., if the core is too soft, the resilience of the ball may be too low, and the ball may not fly, or the feel on impact may be too soft, or the durability against cracking during repeated impact may be poor.
[0031] Next, the hardness distribution of the core will be described. Note that the hardness of the core described below refers to Shore C hardness. This Shore C hardness is a hardness value measured using a Shore C hardness tester conforming to the ASTM D2240 standard.
[0032] The center hardness (Cc) of the core is preferably 58 or more, more preferably 60 or more, and even more preferably 62 or more, with the upper limit being preferably 70 or less, more preferably 68 or less, and even more preferably 66 or less. If this value is too large, the shot feeling may be hard, or the amount of spin may increase on a full shot, making it difficult to achieve the desired flight distance. On the other hand, if this value is too small, the resilience may be reduced, resulting in a poor flight distance, or the durability to cracking when repeatedly hit may be poor.
[0033] The cross-sectional hardness (Cm) of the core at the middle position M is not particularly limited, but is preferably at least 61, more preferably at least 64, and even more preferably at least 67. There is also no particular upper limit, but it is preferably at most 73, more preferably at most 71, and even more preferably at most 69. Any deviation from these hardness limits may result in the same adverse effects as those described for the center hardness (Cc) of the core.
[0034] Furthermore, the cross-sectional hardness (Cp) at the midpoint between the center of the core and the intermediate position M is not particularly limited, but is preferably at least 61, more preferably at least 63, and even more preferably at least 65. The upper limit is also not particularly limited, but is preferably at most 72, more preferably at most 70, and even more preferably at most 68. Any deviation from these hardness limits may result in the same adverse effects as those described for the center hardness (Cc) of the core.
[0035] The surface hardness (Cs) of the core is preferably 82 or more, more preferably 84 or more, and even more preferably 86 or more, with the upper limit being preferably 92 or less, more preferably 90 or less, and even more preferably 88 or less. If this value is too large, the durability against cracking when repeatedly hit may be poor, or the hitting feel may be too hard. On the other hand, if this value is too small, the spin rate at the time of a full shot may be too high, and the target flight distance may not be obtained.
[0036] Furthermore, the cross-sectional hardness (Cq) at the midpoint between the surface of the core and the middle position M is not particularly limited, but is preferably at least 75, more preferably at least 77, and even more preferably at least 79. The upper limit is also not particularly limited, but is preferably at most 85, more preferably at most 83, and even more preferably at most 81. If the hardness deviates from these limits, the same disadvantageous results as those described for the surface hardness (Cs) of the core may occur.
[0037] The difference (Cs-Cc) between the surface hardness and the center hardness of the core is not particularly limited, but is preferably 18 or more, more preferably 19 or more, and even more preferably 20 or more. On the other hand, the upper limit is not particularly limited, and can be preferably 35 or less, more preferably 30 or less, and even more preferably 25 or less. If this value is too small, the ball may not have a low spin rate when it is full shot. On the other hand, if this value is too large, the initial velocity when it is full shot may be too low, or the durability against cracking when it is repeatedly hit may be poor.
[0038] In addition, it is preferable to optimize the value of (Cs-Cc) / (Cm-Cc) for the hardness distribution of the core. The value of (Cs-Cc) / (Cm-Cc) is an index value of the hardness difference from the surface to the center of the core relative to the hardness difference from the center to the middle position M of the core. The value of (Cs-Cc) / (Cm-Cc) is preferably 4 or more, more preferably 6 or more, and even more preferably 7 or more, and the upper limit is preferably 20 or less, more preferably 15 or less, and even more preferably 11 or less. If this value is too small, the ball may not have a low spin rate when it is full shot. On the other hand, if this value is too large, the initial velocity of the actual shot when it is full shot may be too low, or the durability against cracking when it is repeatedly hit may be deteriorated.
[0039] The present invention includes a step (1) of coating the above-mentioned core with at least one intermediate layer to form an intermediate layer-coated sphere.
[0040] The intermediate layer is made of a resin material, and although there are no particular limitations on the resin material, any of the thermoplastic resin materials used in golf balls can be used. In the present invention, it is particularly preferable to use an ionomer resin as the main material (base resin).
[0041] The ionomer resin material preferably contains a high-acid content ionomer resin having an unsaturated carboxylic acid content (also referred to as "acid content") of 16% by mass or more.
[0042] The content of the high acid content ionomer resin is preferably 20% by mass or more, more preferably 50% by mass or more, and even more preferably 60% by mass or more, with the upper limit being preferably 100% by mass or less, more preferably 90% by mass or less, and even more preferably 85% by mass or less, based on 100% by mass of the resin material. If the amount of the high acid content ionomer resin is too small, the ball may have a large spin rate upon full shot, resulting in a loss of flight distance. On the other hand, if the amount of the high acid content ionomer resin is too large, the durability against repeated impacts may be poor.
[0043] When an ionomer resin is used as the base resin, a preferred embodiment is to use a mixture of zinc-neutralized ionomer resin and sodium-neutralized ionomer resin as the base resin. The blending ratio of zinc-neutralized / sodium-neutralized (mass ratio) is 5 / 95 to 95 / 5, preferably 10 / 90 to 90 / 10, and more preferably 15 / 85 to 85 / 15. If the Zn-neutralized ionomer and the Na-neutralized ionomer are not included in this ratio, the hardness will not be high and the resilience of the intermediate layer-covered sphere will not be high, resulting in a failure to achieve low spin rate when the ball is shot full and poor durability against cracking when hit repeatedly.
[0044] Any additives can be added to the intermediate layer material depending on the application. For example, various additives such as pigments, dispersants, antioxidants, UV absorbers, and light stabilizers can be added. When these additives are added, the amount of the additives is preferably 0.1 parts by mass or more, more preferably 0.5 parts by mass or more, and preferably 10 parts by mass or less, more preferably 4 parts by mass or less, relative to 100 parts by mass of the base resin.
[0045] The material hardness of the intermediate layer is preferably 62 or more, more preferably 64 or more, and even more preferably 66 or more in Shore D hardness. The upper limit is not particularly limited, but is preferably 72 or less, more preferably 70 or less, and even more preferably 68 or less. Note that the material hardness of this intermediate layer is the Shore D hardness value measured by molding the resin material alone into a sheet of 2 mm thickness and leaving it for 2 weeks, and does not mean the hardness of the intermediate layer after the heat treatment in step (2) described later.
[0046] As a method for covering the core with the resin material for the intermediate layer, for example, the intermediate layer material may be injected around the core using an injection mold to obtain a covered sphere, or the core may be wrapped with two half cups previously molded into a semi-shelled sphere as the intermediate layer material, and heated and pressurized to produce an intermediate layer-covered sphere surrounding the core. In the present invention, the method of injection molding the intermediate layer around the core using an injection mold is preferably adopted because it has a short molding cycle and is excellent in mass productivity.
[0047] Next, the present invention includes a step (2) of subjecting the intermediate layer-coated sphere to a heat treatment at a temperature equal to or higher than the melting point of the base resin of the intermediate layer resin composition but lower than 160°C. The "melting point" refers to the temperature at which the base resin melts and changes from a solid to a liquid. By subjecting the intermediate layer-coated sphere to a heat treatment within the above-mentioned predetermined temperature range and then leaving the intermediate layer-coated sphere at room temperature, the degree of crystallinity of the crystalline phase of the intermediate layer (resin layer) that coats the core can be controlled, thereby increasing the surface hardness of the intermediate layer-coated sphere.
[0048] The lower limit of the temperature for the heat treatment of the intermediate layer-covered sphere is equal to or higher than the melting point of the base resin of the intermediate layer resin composition, preferably 90°C or higher, more preferably 100°C or higher. On the other hand, the upper limit of the temperature for the heat treatment is usually less than 160°C, preferably 150°C or lower, more preferably 140°C or lower. If the temperature is too low, the effect of reducing the ball's spin rate due to a full shot may not be obtained. If the temperature is too high, the ball may have a higher spin rate or a lower resilience. When two or more types of resins are blended into the intermediate layer resin composition, the resin with the largest blending amount is designated as the base resin.
[0049] The above-mentioned heat treatment can be carried out, for example, by using a known dryer such as an air circulation type dryer (air constant temperature incubator) and placing the intermediate layer-coated spheres inside the device, but is not particularly limited to this means.
[0050] In the above step (2), the time for the heat treatment of the intermediate layer-coated sphere is preferably 3 minutes or more, more preferably 10 minutes or more, and even more preferably 20 minutes or more. The upper limit of the heating time is preferably 60 minutes or less, more preferably 45 minutes or less, and even more preferably 30 minutes or less. If the heating time is too short, the low spin effect of the ball due to a full shot may not be obtained. If the heating time is too long, the resilience of the ball may be reduced.
[0051] The surface hardness of the intermediate layer-covered sphere after the above step (2) is preferably 68 or more, more preferably 70 or more, and even more preferably 71 or more, with the upper limit being preferably 79 or less, more preferably 77 or less, and even more preferably 75 or less. If the surface hardness of this intermediate layer-covered sphere is too soft, the amount of spin on a full shot with an iron may increase too much, resulting in a loss of distance, or the initial velocity of the ball may decrease, resulting in a loss of distance on a full shot with an iron. Also, if the intermediate layer-covered sphere is too hard, the durability to cracking due to repeated impacts may be poor, and the hitting feel may be poor.
[0052] The thickness of the intermediate layer is preferably 0.90 mm or more, more preferably 1.10 mm or more, and even more preferably 1.15 mm or more, while the upper limit is preferably 1.50 mm or less, more preferably 1.35 mm or less, and even more preferably 1.25 mm or less. If the intermediate layer is too thin, the durability against cracking due to repeated impacts may be poor, and the spin rate may be too high during full shots with an iron. On the other hand, if the intermediate layer is too thick, the initial velocity of the ball may be low, and the hitting feeling may be poor.
[0053] Next, the present invention includes a step (3) of covering the intermediate layer-covered sphere with a cover (outermost layer) to form a covered sphere.
[0054] The method for obtaining the covered sphere in the present invention is not particularly limited, but for example, the covered sphere can be obtained by injecting the cover material around the intermediate layer-covered sphere using an injection molding die, or the covered sphere can be produced by preparing two half cups molded into a semi-shelled spherical shape in advance, wrapping the intermediate layer-covered sphere in them, and molding them under heat and pressure. In the present invention, the method of injection molding the cover material around the intermediate layer-covered sphere using an injection molding die is preferably used because it has a short molding cycle and is excellent in mass productivity.
[0055] A resin composition mainly made of urethane resin can be used as the cover material. In general, ionomer resin materials are widely used as cover materials for golf balls, but they are inferior in abrasion resistance and may have a poorer spin rate when approaching with the same hardness as urethane resin. Among urethane resin materials, thermoplastic urethane resin materials are preferably used because they are excellent in mass production. The softening temperature of a typical thermoplastic urethane resin material to which isocyanate is added is about 140 to 175°C. If a heat treatment of 140°C or higher is performed after molding of the ball, the shape of the dimples may change, and the desired aerodynamic characteristics may not be obtained.
[0056] The material hardness of the cover is not particularly limited, but in Shore D hardness, it is preferably 35 or more, more preferably 40 or more, and even more preferably 45 or more, and the upper limit is preferably 60 or less, more preferably 55 or less, and even more preferably 50 or less. If the material hardness is too soft, the spin rate may be too high on a full shot. On the other hand, if the material hardness is too hard, the spin rate may not be applied on an approach shot, and the abrasion resistance may be poor.
[0057] The thickness of the cover is preferably 0.3 mm or more, more preferably 0.45 mm or more, and even more preferably 0.6 mm or more. On the other hand, the upper limit of the cover thickness is preferably 1.2 mm or less, more preferably 1.15 mm or less, and even more preferably 1.0 mm or less. If the cover is too thick, the resilience of the ball may be insufficient or the amount of spin may be too high on a full shot. On the other hand, if the cover is too thin, the abrasion resistance may be poor, or the spin may not be applied on an approach shot, resulting in insufficient controllability.
[0058] A large number of dimples are usually formed on the surface of the outermost layer of the cover, and the cover may further be subjected to various treatments such as priming, stamping, painting, etc.
[0059] The deflection (mm) of the manufactured golf ball (finished product) when an initial load of 98N (10kgf) to a final load of 1,275N (130kgf) is applied is preferably 2.1mm or more, more preferably 2.2mm or more, and even more preferably 2.4mm or more. On the other hand, the upper limit of the deflection is preferably 2.8mm or less, more preferably 2.7mm or less, and even more preferably 2.6mm or less. If the deflection of the golf ball is too small, i.e., if the ball is too hard, the spin rate may increase too much during a full shot with an iron, or the hitting feel may be too hard. On the other hand, if the deflection is too large, i.e., if the ball is too soft, the durability against cracking during repeated impacts may be poor. EXAMPLES
[0060] The present invention will be specifically described below with reference to examples and comparative examples, but the present invention is not limited to the following examples.
[0061] [Examples 1 to 4, Comparative Examples 1 and 2] For each example, a core composition was prepared using a rubber compound containing polybutadiene as a main component as shown in Table 1 below, which was common to all of the examples, and then vulcanized at 150° C. for 19 minutes to produce a core having a diameter of 38.7 mm.
[0062] [Table 1]
[0063] Details of the above formulation are as follows: Polybutadiene rubber: Product name "BR T700" manufactured by ENEOS Materials Co., Ltd. Zinc acrylate: Product name "ZN-DA85S" (manufactured by Nippon Shokubai Co., Ltd.) Organic peroxide: Dicumyl peroxide, trade name "Percumyl D" (manufactured by NOF Corporation) Sulfur: Trade name "Sunmix S-80N" (Sanshin Chemical Industry), sulfur masterbatch containing 80% powdered sulfur for rubber Water: Pure water (Seiki Pharmaceutical Co., Ltd.) Zinc stearate: Product name "Zinc Stearate GP" (manufactured by NOF Corporation) Anti-aging agent: 2,2-methylenebis(4-methyl-6-butylphenol), product name "Nocrac NS-6" (manufactured by Ouchi Shinko Chemical Industry Co., Ltd.) Zinc oxide: Product name "Zinc oxide type 3" (manufactured by Sakai Chemical Industry Co., Ltd.) Pentachlorothiophenol zinc salt: Fujifilm Wako Pure Chemical Industries, Ltd.
[0064] Formation of the intermediate layer and cover (outermost layer) Next, for each example, an intermediate layer was formed around the core obtained above by injection molding using intermediate layer material No. 1 with the composition shown in Table 2, to produce intermediate layer-coated spheres. The intermediate layer-coated spheres were then heat-treated under the temperature and time conditions shown in Table 3 below, and the surface hardness of the intermediate layer-coated spheres after heat treatment is also shown in the same table. The heat treatment was performed using a dry air-blowing constant temperature incubator manufactured by Yamato Scientific Co., Ltd., with the product name "DNF610," and 20 of the intermediate layer-coated spheres were placed side by side in the dryer and heat-treated. Next, a cover (outermost layer) was formed by injection molding around the intermediate layer-covered sphere obtained above using cover material No. 2 having the composition shown in Table 2, to produce a golf ball. At this time, predetermined dimples common to each example were formed on the surface of the cover.
[0065] [Table 2]
[0066] The trade names of the main materials listed in the table are as follows: "Himilan 1706" Ionomer manufactured by Mitsui Dow Polychemicals "AM7318" Ionomer manufactured by Mitsui Dow Polychemicals "Trimethylolpropane" (TMP) manufactured by Tokyo Chemical Industry Co., Ltd. "Titanium oxide" manufactured by Sakai Chemical Industry Co., Ltd. "TPU" is a product name "Pandex" manufactured by DIC Covestro Polymer, an ether type thermoplastic polyurethane, material hardness (Shore D) "47"
[0067] For each of the resulting golf balls, various physical properties such as the internal hardness at each position of the core, the outer diameter of the core and each coated sphere, the thickness of each layer and material hardness were evaluated by the methods described below. The results are shown in Table 3.
[0068] The outer diameter of each sphere of the core and the intermediate layer-coated sphere The sphere to be measured is placed in a thermostatic chamber adjusted to 23.9±1°C for at least 3 hours, and then measured in a room at 23.9±2°C. Five randomly selected points on the surface are measured, and the average value is taken as the measurement value for each sphere, and the average value for 10 measurements is calculated.
[0069] Ball diameter The ball to be measured is placed in a thermostatic bath adjusted to 23.9±1°C for at least three hours and then measured in a room at 23.9±2°C. 15 randomly selected non-dimpled areas are measured and the average value is taken as the measurement value for one ball, and the average value for 10 balls is calculated.
[0070] Core hardness distribution The surface of the core is spherical, and the needle of the hardness tester is set almost perpendicular to the spherical surface, and the surface hardness is measured in Shore C hardness according to ASTM D2240. For the center and specified positions of the core, the core is cut into a hemisphere to make the cross section flat, and the needle of the hardness tester is pressed perpendicularly against the center part and the specified positions shown in Table 3 to measure the hardness, and the hardness at the center and each position is shown as a Shore C hardness value. To measure the hardness, an automatic rubber hardness tester "P2" made by Kobunshi Keiki Co., Ltd. equipped with a Shore C type hardness tester is used. The hardness value is read as the maximum value. All measurements are performed in an environment of 23±2°C. The values in Table 3 are Shore C hardness values.
[0071] Amount of deformation (deflection) of the core, the intermediate layer-covered sphere and the ball Each target sphere is compressed at a speed of 10 mm / s at a temperature of 23±1°C, and the amount of compressive deformation (mm) of the target sphere is measured from the state in which an initial load of 98 N (10 kgf) is applied to the state in which a final load of 1275 N (130 kgf) is applied, and the average value of 10 measurements is calculated.
[0072] Hardness of mid layer and cover materials The resin material for each layer is formed into a 2 mm thick sheet and left to stand for 2 weeks. The Shore D hardness and Shore C hardness are then measured in accordance with the ASTM D2240 standard. The hardness is measured using an automatic rubber hardness tester "P2" manufactured by Kobunshi Keiki Co., Ltd. Attachments for Shore D hardness and Shore C hardness are attached and the respective hardness is measured. The maximum hardness value is read. All measurements are performed in an environment of 23±2°C.
[0073] Surface hardness of intermediate layer coated spheres The measurement is made by pressing a needle perpendicularly against the surface of the intermediate layer-coated sphere. Shore D hardness is measured in accordance with the ASTM D2240 standard. The hardness is measured using an automatic rubber hardness tester "P2" manufactured by Kobunshi Keiki Co., Ltd. An attachment for the Shore D hardness is attached and each hardness is measured. The maximum hardness value is read. All measurements are made in an environment of 23±2°C.
[0074] [Table 3]
[0075] The flight (I#6, HS40m / s), (I#6, HS35m / s) and controllability at the time of approach of each golf ball were evaluated by the following method. The results are shown in Table 4.
[0076] Flight rating (I#6, HS40m / s) A No. 6 iron (I#6) was attached to the golf hitting robot, and the amount of spin was measured when hitting the ball at a head speed (HS) of 40 m / s, and judged according to the following criteria. The amount of spin was measured by an initial condition measuring device on the ball immediately after hitting. The club used was the "TourStage X-BLADE CB (2008 model)" manufactured by Bridgestone Sports Co., Ltd. 〔Judgment criteria〕 ○: The spin rate is less than -25 rpm compared to Comparative Example 1. △: Spin rate is -25 to +25 rpm compared to Comparative Example 1 × The spin rate is greater than +25 rpm compared to Comparative Example 1
[0077] Flight rating (I#6, HS35m / s) The golf hitting robot was fitted with a No. 6 iron (I#6), and the amount of spin was measured in the same manner as above when hitting the ball with a head speed (HS) of 35 m / s, and the results were judged according to the following criteria. The club used was the Bridgestone Sports TourStage X-BLADE CB (2008 model). 〔Judgment criteria〕 ○: The spin rate is less than -25 rpm compared to Comparative Example 1. △: Spin rate is -25 to +25 rpm compared to Comparative Example 1 × The spin rate is greater than +25 rpm compared to Comparative Example 1
[0078] Evaluating the amount of spin when approaching The amount of spin was determined by attaching a sand wedge (SW) to a golf hitting robot and hitting the ball at a head speed (HS) of 14 m / s. The amount of spin was measured by an initial condition measuring device on the ball immediately after hitting. The sand wedge (SW) used was the "TourStage TW-03 (loft angle 57°) 2002 model" manufactured by Bridgestone Sports. 〔Judgment criteria〕 ○: The spin rate is -25 rpm or more compared to Comparative Example 1 × Spin rate compared to Comparative Example 1 is less than -25 rpm
[0079] [Table 4]
[0080] As shown in Table 4, the golf balls of Examples 1 to 4 were produced by subjecting the intermediate layer-covered sphere to heat treatment at a specified temperature range, and it was found that the spin rate on a full shot with a No. 6 iron was reduced, improving flight performance. On the other hand, Comparative Example 1 is a ball in which the intermediate layer-covered sphere was not subjected to heat treatment, but was covered by injection molding, and the spin rate on a full shot with a 6 iron was greater than those of the Examples. In Comparative Example 2, a ball covered with an intermediate layer was subjected to a heat treatment at 160°C for 10 minutes, and then a cover was injection molded to cover the ball. The spin rate on a full shot with a 6 iron was greater than that of each of the Examples.
Claims
1. 1. A method for manufacturing a golf ball having a core, at least one intermediate layer, and a cover, the core being made of a rubber material, the intermediate layer being made of a resin composition, and the cover being made of a urethane resin material, the method comprising the steps of: (1) forming an intermediate-layer-coated sphere by coating the core with at least one intermediate layer; A step (2) of subjecting the intermediate layer-coated sphere to a heat treatment at a temperature equal to or higher than the melting point of the base resin of the intermediate layer and lower than 160° C.; and Then, a step (3) of covering the intermediate layer-covered sphere with the cover to form a covered sphere.
2. A method for manufacturing a golf ball comprising the steps of:
2. 2. The method according to claim 1, wherein in the step (2), the intermediate layer-coated spheres are heated at a temperature of 90 to 150°C.
3. 3. The method according to claim 1, wherein in the step (2), the intermediate layer-coated spheres are heated for a period of 3 to 60 minutes.
4. 3. The method according to claim 1, wherein in the step (1), the intermediate layer-covered sphere is formed by injection molding the resin composition for the intermediate layer around the core.
5. 3. The method according to claim 1, wherein in the step (3), the urethane resin material of the cover is injection molded around the intermediate layer covered sphere to form the covered sphere.
6. 3. The method according to claim 1, wherein the base resin of the resin composition for the intermediate layer is an ionomer resin.
Citation Information
Patent Citations
Three-pieces solid golf ball
JP1997239068A
Golf ball
JP2002000765A
Method of manufacturing golf ball
JP2004159840A
Method and system for customizing golf ball
JP2011167508A
Production method of golf ball
JP2017225682A