Method of manufacturing GSR element
Adjusting slit widths and resist thickness ratios on the mask and substrate allows for precise formation of narrow-pitch coils on grooved substrates, addressing diffraction issues and achieving high sensitivity and miniaturization in GSR sensors.
Patent Information
- Application Number
- JP2023084281
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-23
- Publication Date
- 2024-12-05
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing methods struggle to form narrow-pitch coils for magnetic field detection elements like GSR sensors due to light diffraction issues and uneven photoresist thickness on grooved substrates, leading to difficulties in achieving both high sensitivity and miniaturization.
By adjusting the slit width and photoresist thickness ratios on the mask and substrate, and using a spin coating method to ensure uniform resist application, the process forms narrow-pitch coils with equal space widths on flat and grooved areas, allowing for precise coil patterns with pitches of 2 to 5 μm.
This method enables the production of highly sensitive and miniaturized GSR elements with improved coil patterns, enhancing their performance and enabling applications in ultra-compact devices.
Smart Images

Figure 2024167943000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a narrow-pitch microcoil having a detection coil with a coil pitch of 2 μm to 5 μm in a manufacturing process for a GSR element consisting of a magnetic wire, a detection coil consisting of a lower coil and an upper coil wound around the magnetic wire, and electrode wiring. [Background technology]
[0002] High-sensitivity magnetic sensors include Hall sensors, GMR sensors, TMR sensors, high-frequency carrier sensors, FG sensors, MI sensors, GSR sensors, etc. Of these sensors, Hall sensors, GMR sensors, TMR sensors, and carrier sensors have been made smaller and thinner by integrating the element with an ASIC, but improving detection sensitivity remains an issue. On the other hand, FG sensors, MI sensors, and GSR sensors have high sensitivity, but the element and ASIC are arranged separately and joined by wire bonding, making it difficult to make the sensors thinner and smaller.
[0003] One method for solving this problem is to reduce the coil pitch of the magnetic field detection element to increase sensitivity and reduce the size. As a result of the inventors' efforts in technological development, they have succeeded in making a sensor that is smaller and more sensitive (Patent Document 1). Patent Document 1 discloses an MI element with a coil pitch of 14 μm. Furthermore, Patent Document 2 discloses a process for producing a GSR element as a magnetic field detection element on a Si substrate. Patent Document 2 discloses a coil pitch of 10 μm or less.
[0004] Furthermore, since alignment of the lower coil and the upper coil becomes an issue when forming a fine pitch coil, the inventors have investigated a manufacturing method for a highly visible alignment mark and have achieved a coil pitch of 5.5 μm (Patent Document 3, Patent Document 4). However, in order to further reduce the coil pitch, a coil pitch of 3 μm remains a challenge, but no concrete solution has been presented.
[0005] Furthermore, a method is being considered in which a narrow-pitch coil pattern is formed on a flat surface in advance using a film mask consisting of a photoresist layer and a film, and then pasted into the groove. However, this method has not yet been put to practical use due to the difficulty in ensuring high quality and low productivity. (Patent Document 5) [Prior art documents] [Patent documents]
[0006] [Patent Document 1] Patent No. 5747294 [Patent Document 2] Patent No. 6924453 [Patent Document 3] Patent No. 7203400 [Patent Document 4] Patent No. 7207676 [Patent Document 5] Published Patent Publication 2018-148189 Summary of the Invention [Problem to be solved by the invention]
[0007] When a grooved substrate is exposed using a mask with slits, the light diffraction phenomenon occurs, and the bottom of the groove cannot be printed on the resist with a slit of the same width as the slit width of the mask. However, since parallel light is generally incident on the exposure device, it was thought that when the groove is shallow as in this invention, the pattern width is not affected by the slit width (d) or wavelength (λ) and the width is the same. In other words, it was thought that in principle the diffraction width would be judged to be small. In fact, when the slit width of the mask was set to 3 μm and a coil with a pitch of 5.5 μm was formed, the coil pattern could be formed without any problems. However, in order to form a narrower-pitch coil with a coil pitch of 2 μm to 5 μm, it is necessary to narrow the mask slit width (space) and line width (resist). Therefore, when we started to study a narrower-pitch coil with a mask slit width of 1.5 μm, we found that the pattern width inside the grooves, which was not a problem with a 5.5 μm pitch (slit width of 3 μm), became wider compared to the flat part.
[0008] As is well known, due to the phenomenon of diffraction, the light passing through the slit will be slightly spread out by diffraction. On the other hand, the diffraction intensity of light is expressed as follows, where the center position of the slit is the origin and the distance from it is x: I(x)=I(0)(sin(αx) / αx) 2 (where h>>d) is known to be the case. α=πD / λh (D: slit width, λ: wavelength of light, h: distance between mask and substrate) Using this formula, the position where the light intensity is attenuated to 70% is taken as the effective diffraction width x, and the relationship with the gap L is graphed as shown in Figure 1. When creating a narrow pitch of 3 μm or less with a slit width of 1.5 μm, if the effective diffraction width x expands by 0.75 μm or more on one side, a coil cannot be formed, but when h = 7 μm, the effective diffraction width is calculated to be 0.4 μm, meaning that a coil pattern can be formed. However, when considering a narrow-pitch coil, a photoresist film is essential, so when the resist film thickness was 1 μm, the slit width was 1.5 μm, and h=7 μm, the effective diffraction width became large at 0.75 μm, and it was found that a slit could not be formed at the bottom of the groove. In other words, it was found that the pattern width inside the groove was wider than that of the flat part. The cause of the broadening is unclear, but the inventors believe that this is because, in an actual substrate, a photosensitive resin film (resist film) exists between the slit, mask, and substrate, and the refraction of light also occurs on the resist surface, thereby increasing the diffraction intensity of the light. In this way, when the coil pattern becomes finer and the slit width d becomes narrower, that is, when the ratio of the slit width d to the distance h between the mask and the substrate (d / h) becomes sufficiently small, detailed consideration is required taking into account the effects of diffraction.
[0009] Furthermore, in order to increase productivity, spin coating is commonly used as a method for applying photoresist. However, when applied to a substrate having grooves such as those of the present invention, the photoresist film thickness differs between the flat and stepped portions. Therefore, when the flat and stepped portions are exposed simultaneously, it is expected that the diffraction width at the bottom of the groove will become even wider, causing a change in the space width between the flat and groove portions. [Means for solving the problem]
[0010] As mentioned above, in a substrate having grooves, the diffraction width at the grooves becomes large. To address this issue, we found that it would be sufficient to make the slit width at the grooves slightly narrower than that of the substrate surface. In addition, since it is strongly dependent on the thickness of the resist, we tried to make the resist film thickness on the bottom of the groove and the flat part of the substrate as similar as possible. Also, when applying resist by spin coating, the resist film thickness on the bottom of the groove tends to be thick, so we decided to make it as thin as possible. First, we started to study the lower coil, which is affected by the grooves for wire placement. Figure 2 shows the relationship between the distance from the slit mask to the photoresist surface and the space width when the resist is uniformly applied to the flat and grooved parts. The photoresist film thickness is 1.0 μm, the coil pitch is 3 μm, the slit width is 1.1 μm, and the exposure dose is 160 mJ / cm2. This shows that for a mask slit width of 1.1 μm, the deeper the groove, the wider the space width of the formed photoresist becomes. Under these conditions, when the resist film thickness is 1 μm, if the groove is 7.0 μm, the space width becomes wider and the resist width becomes narrower, so that it is not possible to form a pattern. Figure 3 shows the relationship between the space width and the groove depth when the photoresist film thickness is 1 μm and 3 μm. The coil pitch is 3 μm, the mask slit width is 1.1 μm, and the exposure dose is 160 mJ / cm2. For both film thicknesses, the deeper the groove, the larger the space width. Here, the space width when the groove depth is 0 μm corresponds to the space width of the flat portion, and the space width in each groove corresponds to the space width inside the groove. Therefore, by developing the difference between the lines and spaces on the flat portion and inside the groove on the mask, taking into account the groove depth, the space widths of the flat portion and inside the groove can be made equal. When this ratio is calculated, if the coil pitch of the mask with slits is the flat portion (A) and the groove bottom portion (B), the space widths of the flat portion and inside the groove can be made equal by setting the ratio of A to B to 1:0.8 to 0.995.
[0011] Next, when considering the case where a magnetic wire is placed in a groove for wire placement and an upper coil is created on top of it, the shape becomes convex upwards, the opposite of the lower coil. In other words, the relationship between the flat part and the groove part is the opposite of that in the case of the lower coil, and the space width above the wire becomes narrower compared to the flat part. This ratio is due to the groove depth, so it is the same as the ratio when considering the lower coil. If the coil pitch of the mask with slits is the flat part (A) and the upper part of the magnetic wire (C), the space width of the flat part and the space width above the wire can be made equal by setting the ratio of A to C to 1:1.00 to 1.25.
[0012] On the other hand, in order to form a narrow pitch coil, it is necessary to narrow not only the slit width (space) of the mask but also the line width (photoresist width). Figure 4 shows the photoresist width and photoresist film thickness ratio (aspect ratio). In the case of a coil pitch of 5.5 μm where a coil pattern can be formed, the slit width is 2.0 μm, the line width is 3.5 μm, the resist film thickness is 5 μm, and the aspect ratio is 1.43. In the case of a coil pitch of 3 μm, a slit width of 1 μm, and a resist film thickness of 5 μm, the aspect ratio is 2.5, The resist collapsed, and it was not possible to form a pattern. For this reason, it is desirable for the photoresist film thickness to be 3.5 μm or less, which results in an aspect ratio of 1.5 or less, in order to form a narrow-pitch coil.
[0013] So far, we have considered the case where the photoresist is uniformly applied to the flat and grooved parts, but in order to increase productivity, it is common to use a spin coat method. When the photoresist is applied to a substrate with grooves such as the present invention by spin coat method, it can be seen that the resist film thickness inside the groove increases along with the groove depth as shown in FIG. 5. When the photoresist film thickness on the flat part is 1 μm, the resist film thickness inside the groove can be thinned to 3 μm. From FIG. 3, the space width of the photoresist film thickness of 1 μm and groove 0 corresponds to the flat part, and the space width of the photoresist film thickness of 3 μm and groove depth of 7 μm corresponds to the inside of the groove. Therefore, when the coil pitch is the flat part (A) and the groove bottom part (B), the ratio of A to B can be set to 1:0.8 to 0.995, so that the space width of the flat part and the inside of the groove can be made equal, as in the case where the resist film thickness is uniformly applied. Effect of the Invention
[0014] According to the present invention, in a manufacturing process for a magnetic field detection element in which a GSR element consisting of a magnetic wire, a detection coil consisting of a lower coil and an upper coil surrounding the magnetic wire, and electrode wiring is fabricated on a substrate, it is possible to form a GSR element having a detection coil with a narrow coil pitch of 2 to 5 μm or less. [Brief description of the drawings]
[0015] [Figure 1] FIG. 1 is a diagram showing the relationship between the diffraction width (width at 70% intensity) due to light diffraction and the gap. [Diagram 2] FIG. 13 is a diagram showing the relationship between a step and a space width. [Diagram 3] FIG. 13 is a diagram showing the relationship between the step and the space width when the resist is uniformly applied. [Figure 4] FIG. 13 is a diagram showing the relationship between the resist width and the aspect ratio. [Diagram 5]FIG. 13 is a diagram showing the relationship between the groove depth and the photoresist film thickness inside the groove. [Figure 6a] FIG. 1 shows a substrate on which grooves for placing magnetic wires are formed. [Figure 6b] FIG. 13 is a diagram showing a substrate on which a groove bottom is smoothed with a photosensitive resin and a metal film is formed. [Figure 6c] FIG. 1 is a diagram showing a substrate on which a photoresist film is applied by spin coating. [Figure 6d] FIG. 13 shows a lower coil pattern exposed using a mask with slits and developed. [Figure 6e] FIG. 2 is a diagram showing a coil with a 3 μm coil pitch formed in a first embodiment of the present invention. [Figure 7a] FIG. 1 is a diagram showing a substrate on which magnetic wires are arranged and fixed. [Figure 7b] This is a diagram showing a substrate on which a photosensitive resin is used to smooth the space between the magnetic wires and the grooves, a metal film is formed, and then a photoresist film is applied by spin coating. [Figure 7c] 13A and 13B are diagrams showing a process of forming an upper coil pattern by plating the coil pattern that has been exposed using a mask having slits and developed, and then etching the metal film. [Figure 8a] FIG. 13 is a cross-sectional view of a lower coil pattern in which resist is uniformly applied to flat portions and step portions. [Figure 8b] FIG. 13 is a cross-sectional view of an upper coil pattern in which resist is uniformly applied to flat and stepped portions. BEST MODE FOR CARRYING OUT THEINVENTION
[0016] In the method for producing a GSR element of the present invention, In a method for manufacturing a GSR element having a lower coil, an upper coil, and electrode wiring on a substrate having an inverted trapezoidal groove, (1) forming a metal film on the entire surface of a substrate, and then applying a photosensitive resin film thereon; (2) In the mask material having slits formed of lines and spaces (hereinafter referred to as L / S) in the photosensitive resin coating, the slit width of the mask is set to a flat portion (A) and a groove bottom portion (B), and the ratio of A to B is less than 1:1.0, (3) using the mask, a flat portion and a groove portion are simultaneously exposed to light, and then developed to form a pattern of the lower coil along a groove surface of the inverted trapezoidal groove; A method for manufacturing a GSR element comprising the steps of:
[0017] In addition, in a method for manufacturing a GSR element having a lower coil, an upper coil, and electrode wiring on a substrate having an inverted trapezoidal groove, (1) placing a magnetic wire inside a groove and fixing the magnetic wire with an adhesive resin, forming a metal film on the adhesive resin, and then applying a photosensitive resin film; (2) In the mask material having slits formed of lines and spaces (hereinafter referred to as L / S) in the photosensitive resin film, the slit width of the mask is set to a flat portion (A) and an upper portion of the magnetic wire (C), and the ratio of A to C exceeds 1:1.0; (3) using the mask to simultaneously expose the flat portion and the upper portion of the magnetic wire, and then developing the mask to form a pattern of the upper coil along the magnetic wire; A method for manufacturing a GSR element comprising the steps of:
[0018] Furthermore, in a method for manufacturing a GSR element having a magnetic wire with a diameter of 5 μm to 15 μm and a detection coil with a coil pitch of 2 μm to 5 μm wound around the magnetic wire on a substrate having a groove with a depth of 2 μm to 10 μm, (1) The groove for disposing the magnetic wire has an inverted trapezoidal shape with a groove depth of 2 to 10 μm and a groove width of 10 to 18 μm, (2) forming a metal film on the entire surface of the substrate on which the grooves for arranging the magnetic wires are formed; (3) In the mask having slits formed of lines and spaces (hereinafter referred to as L / S) in the photosensitive resin coating, the slit width of the mask is set to a flat portion (A) and a groove bottom portion (B), and the ratio of A to B is less than 1:1.0, (4) using the mask, a process of simultaneously exposing a flat portion and a groove portion of a lower coil pattern shape to light, and then developing the mask to form the lower coil pattern along the groove surface of the inverted trapezoid groove; (5) forming the lower coil along a groove surface of the inverted trapezoidal groove by plating the space portion of the lower coil pattern, peeling off the photoresist, and etching the metal film in the unplated portion; (6) arranging the magnetic wire in the inverted trapezoid groove in which the lower coil is formed and fixing it with resin, and then forming a metal film on the entire surface of the substrate; (7) In the mask having slits formed of lines and spaces (hereinafter referred to as L / S) in the photosensitive resin film, the slit width of the mask is set to a flat portion (A) and an upper portion of the magnetic wire (C), and the ratio of A to C exceeds 1:1.0; (8) using the mask, a flat portion and an upper portion of the magnetic wire are simultaneously exposed to light to form an upper coil pattern shape, and then developed to form the upper coil pattern along the magnetic wire; (9) forming the upper coil and electrode wiring along the magnetic wire disposed in the groove by plating the coil pattern, removing the photoresist, and etching the metal film in the unplated portion; A method for manufacturing a GSR element comprising the steps of:
[0019] In addition, in a method for manufacturing a GSR element comprising a lower coil, an upper coil, and electrode wiring on a substrate having a groove, A method for manufacturing a GSR element, characterized in that a photoresist film is formed uniformly on the flat portion and groove portion when the lower coil is formed, and on the flat portion and magnetic wire when the upper coil is formed, and the film thickness is 0.2 μm or more and 3.5 μm or less.
[0020] Furthermore, in a method for manufacturing a GSR element having a lower coil, an upper coil, and electrode wiring on a substrate having a groove, A method for manufacturing a GSR element, characterized in that the photoresist film is thicker on the flat and grooved portions when the lower coil is formed, and is thicker on the flat and magnetic wires when the upper coil is formed, the thickness of the thickly applied film being 1.5 to 5 times that of the flat portion and 3.5 μm or less, and the aspect ratio of the line width to the thickness of the resist film (=resist film thickness / line width) being 1.5 or less.
[0021] Also, a method for manufacturing a GSR element is characterized in that a lower coil or an upper coil is formed by etching using a coil pattern formed using the mask with slits. EXAMPLES
[0022] The manufacturing flow for the lower coil is shown in Figs. 6a to 6e for forming fine coils with a pitch of 2 to 5 µm or less on a substrate with a groove of 5 to 8 µm flatly and inside the groove at once. FIG. 6a: A substrate 6 has grooves 61 with a depth of 7 μm formed for placement of magnetic wires. The grooves are formed by digging into the silicon substrate or by curing a positive photosensitive resin with a heat treatment. FIG. 6b: In order to make the bottom of the groove have a gentle R shape 601, a negative photosensitive resin 62 is embedded in the bottom of the groove, and after a curing heat treatment, a metal film 63 is formed to a thickness of 100 nm over the entire surface of the substrate. Figure 6c: Next, photoresist 64 with a viscosity of 10 CP is dropped onto the substrate and applied to the entire substrate by spin coating at a coating rotation speed of 2000 rpm and a coating rotation time of 10 seconds. At this time, the film thickness on the flat part is 1 μm, and the film thickness inside the groove is 3 μm. Figure 6d: Then, using a mask with a coil pitch of 3 μm (line width:space width = 1.9:1.1 μm) on the flat part, the flat part and the inside of the groove are exposed at once with an exposure dose of 200 mJ / cm2, and developed for 90 seconds with the oscillation direction set to the longitudinal direction of the coil pattern. The narrow pitch coil pattern thus formed has a line width:space width=1.44:1.56 μm. At this time, the mask in the groove is designed with a coil pitch of 2.959 μm (line width:space width=1.874:1.085 μm), and the finished dimensions are line width:space width=1.43:1.53 μm. Figure 6e: This 3 μm coil pitch pattern is plated, the resist pattern is removed by peeling, and the deposited metal film is then removed by etching. Figure 6e shows a photograph of the lower coil after removal. A lower coil of approximately the same width was formed inside the 7 μm deep groove and on the flat surface. It is of course also possible to form the lower coil by etching the metal film after the coil pattern has been formed, without plating. In this case, the slits in the mask that will form the coil by plating and the line parts of the mask are reversed.
[0023] Next, the flow of forming the upper coil will be described with reference to FIGS. 7a to 7c. Figure 7a: A magnetic wire 73 is placed in a groove 71 of a substrate 70 in which a lower coil 72 with a 3 μm pitch has been formed by pseudo-three-dimensional photolithography technology, and fixed with a photosensitive resin 701. Then, after removing the SiO2 around the magnetic wire, a positive photosensitive resin 704 is formed on the magnetic wire and a curing heat treatment is performed to smooth the step between the magnetic wire and the groove, and then a metal film 74 is formed over the entire surface of the substrate. 7b: Next, photoresist 702 with a viscosity of 220 CP is dropped onto the substrate 70 and applied to the entire substrate at a coating rotation speed of 3500 rpm for a coating rotation time of 5 seconds. At this time, the film thickness on the flat part is 3 μm, and the film thickness above the wire is 1.4 μm. Then, using a mask with a coil pitch of 3 μm (line width: space width = 1.9:1.1 μm) on the flat part, the flat part and the top of the wire are exposed at once with an exposure dose of 400 mJ / cm2, and developed for 180 seconds with the oscillation direction as the longitudinal direction of the coil pattern. The narrow pitch coil pattern formed in this way has a line width: space width = 1.54:1.46 μm on the flat part. Figure 7c: After plating this pattern, the resist is removed by peeling, and the metal film formed over the entire substrate is etched. After etching, the coil pattern was formed with approximately the same width, 1.76 μm on the flat portion and 1.74 μm above the wire. It is of course also possible to form the upper coil by etching the metal film after forming the coil pattern, without plating. In this case, the slits in the mask that form the coil by plating and the line portions of the mask are reversed.
[0024] Figure 8a shows a cross-sectional view of the lower coil pattern when a fine coil with a pitch of 3 μm or less is formed on a substrate with a 7 μm groove and photoresist is applied to the flat part and inside the groove by spray coating, and Figure 8b shows an upper coil pattern when a fine coil with a pitch of 3 μm or less is formed on a substrate with a magnetic wire arranged in a groove and photoresist is applied to the flat part and above the magnetic wire. The step is 7 μm. The film thickness of the flat part and the step part (inside the groove and above the magnetic wire) is about 3 μm, and it can be applied almost uniformly. The relationship between the space width y and the step x for a resist film thickness of 3 μm in Figure 3 can be expressed as y = 0.0392x + 1.3697, and from this, the space width for a step of 7 μm is 1.644. Therefore, when the ratio of A to B is 1:0.949 for the flat portion (A) and bottom of the groove (B) of the mask with slits in the lower coil, and when the ratio of A to C is 1:1.054 for the flat portion (A) and top of the magnetic wire (C) of the mask with slits in the upper coil, the width of the coil pattern formed by exposing the flat portion and step portion at once can be made equivalent.
[0025] As described above, a magnetic wire was placed on a substrate with a 7 μm groove, and a coil with a 3 μm pitch was formed around the magnetic wire. [Industrial Applicability]
[0026] The present invention makes it possible to form a GSR element with a narrow-pitch coil, which enables the GSR sensor to have high sensitivity. Furthermore, by integrating it with a circuit board, it is possible to realize an ultra-thin and ultra-compact device, which is expected to be used in applications that require ultra-compactness and high performance, such as motion devices in living organisms. It can also be applied to small, high-performance GSR sensors for automobiles or wearable computers. [Explanation of symbols]
[0027] 60:Si substrate 61: Groove 62: Resin coating 63: Metal film 601: R shape of the groove bottom 64: Photoresist 65: Space 66: Line 67: Lower coil 80:Si substrate 81: Groove 82: Lower coil 83: Magnetic wire 801: Photosensitive resin to fix magnetic wire 802: Photoresist
Claims
1. A method for manufacturing a GSR element having a lower coil, an upper coil, and electrode wiring on a substrate having an inverted trapezoidal groove, comprising the steps of: (1) forming a metal film on the entire surface of a substrate, and then applying a photosensitive resin film thereon; (2) In the mask having slits formed of lines and spaces (hereinafter referred to as L / S) in the photosensitive resin film, the slit width of the mask is set to a flat portion (A) and a groove bottom portion (B), and the ratio of A to B is less than 1:1.0, (3) using the mask, a flat portion and a groove portion are simultaneously exposed to light, and then developed to form a pattern of the lower coil along a groove surface of the inverted trapezoidal groove; A method for manufacturing a GSR element comprising the steps of:
2. A method for manufacturing a GSR element having a lower coil, an upper coil, and electrode wiring on a substrate having an inverted trapezoidal groove, comprising the steps of: (1) placing a magnetic wire inside a groove and fixing the magnetic wire with an adhesive resin, forming a metal film on the adhesive resin, and then applying a photosensitive resin film; (2) In the mask having slits formed of lines and spaces (hereinafter referred to as L / S) in the photosensitive resin film, the slit width of the mask is set to a flat portion (A) and an upper portion of the magnetic wire (C), and the ratio of A to C exceeds 1:1.0; (3) using the mask to simultaneously expose the flat portion and the upper portion of the magnetic wire, and then developing the mask to form a pattern of the upper coil along the magnetic wire; A method for manufacturing a GSR element comprising the steps of:
3. A method for manufacturing a GSR element having a magnetic wire with a diameter of 5 μm to 15 μm and a detection coil with a coil pitch of 2 μm to 5 μm surrounding the magnetic wire on a substrate having a groove with a depth of 2 μm to 10 μm, comprising the steps of: (1) The groove for disposing the magnetic wire has an inverted trapezoid shape with a groove depth of 2 μm to 10 μm and a groove width of 10 to 18 μm; (2) forming a metal film on the entire surface of the substrate in which the grooves for arranging the magnetic wires are formed; (3) In the mask material having slits formed of lines and spaces (hereinafter referred to as L / S) in the photosensitive resin coating, the coil pitch of the mask having the slits is set such that the ratio of A to B is less than 1:1.0 when the coil pitch is set to a flat portion (A) and a groove bottom portion (B), (4) using the mask, a flat portion and a groove portion of a lower coil pattern are simultaneously exposed to light, and then developed to form the lower coil pattern along a groove surface of the inverted trapezoid groove; (5) forming the lower coil along a groove surface of the inverted trapezoidal groove by plating the space portion of the lower coil pattern, peeling off the photoresist, and etching the metal film in the unplated portion; (6) arranging the magnetic wire in the inverted trapezoidal groove in which the lower coil is formed and fixing it with resin, and then forming a metal film on the entire surface of the substrate; (7) In the mask material having slits formed of lines and spaces (hereinafter referred to as L / S) in the photosensitive resin film, the coil pitch of the mask having the slits is such that the ratio of A to C exceeds 1:1.0 when the coil pitch of the mask having the slits is a flat portion (A) and an upper portion of the magnetic wire (C), (8) using the mask, a flat portion and an upper portion of the magnetic wire are simultaneously exposed to light to form an upper coil pattern shape, and then developed to form the upper coil pattern along the magnetic wire; (9) A method for manufacturing a GSR element, characterized in that after plating the coil pattern, the photoresist is peeled off and the metal film in the unplated portion is etched, thereby forming the metal film in the groove, and the film thickness is 0.2 μm to 3.5 μm.
4. A method for manufacturing a GSR element comprising a lower coil, an upper coil, and electrode wiring on a substrate having a groove according to any one of claims 1 to 3, A method for manufacturing a GSR element, comprising the steps of: forming a photoresist film on flat portions and groove portions when forming a lower coil; and forming the upper coil and electrode wiring uniformly along the magnetic wire on the flat portions and magnetic wire when forming an upper coil.
5. A method for manufacturing a GSR element comprising a lower coil, an upper coil, and electrode wiring on a substrate having a groove according to any one of claims 1 to 3, A method for manufacturing a GSR element, characterized in that when the lower coil is formed, the photoresist film is thicker in the grooves and flat portions, and when the upper coil is formed, the photoresist film is thicker on the flat portions and magnetic wires, the thickness of the thickly applied film being 1.5 to 5 times that of the flat portions and 3.5 μm or less, and the aspect ratio of the thickness of the resist film (= resist film thickness / line width) is 1.5 or less.
6. 3. A method for manufacturing a GSR element according to claim 3, further comprising the step of forming a lower coil or an upper coil by etching using a coil pattern formed using the mask with a slit.
Citation Information
Patent Citations
Photomask and pattern forming method
JP1991137647A
Pattern forming method, pattern forming program and manufacturing method for semiconductor device
JP2004077824A
Method for manufacturing nanocoil type GSR sensor element
JP2018148189A
Magnetic Impedance Sensor Element with Electromagnetic Coil and Magnetic Impedance Sensor with Electromagnetic Coil
JP5747294B1
Manufacturing method for GSR sensor element
JP6924453B1