Method for manufacturing display device
By controlling the orientation of liquid crystal molecules through a polymer network and directed electric fields, the method addresses inconsistent scattering in display devices, improving display quality and reliability.
Patent Information
- Application Number
- JP2023085547
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-24
- Publication Date
- 2024-12-05
AI Technical Summary
In existing display devices, the scattering characteristics of liquid crystal molecules vary depending on the applied voltage, leading to inconsistent display quality due to differences in initial alignment of liquid crystal molecules within the liquid crystal layer.
A method for manufacturing a display device involving the formation of a polymer network within a liquid crystal layer by applying a voltage between electrodes and irradiating with ultraviolet rays, while using alignment films to control the orientation of liquid crystal molecules, and incorporating protrusions or slits in the electrodes to direct the electric field for consistent scattering.
This method improves display quality by ensuring consistent scattering characteristics across pixels, enhancing impact resistance and reliability of the display device.
Smart Images

Figure 2024168673000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a method for manufacturing a display device. [Background technology]
[0002] Patent Document 1 describes a display device including a first light-transmitting substrate, a second light-transmitting substrate arranged opposite the first light-transmitting substrate, a liquid crystal layer having a polymer-dispersed liquid crystal sealed between the first light-transmitting substrate and the second light-transmitting substrate, and at least one light-emitting unit arranged opposite at least one side surface of the first light-transmitting substrate and the second light-transmitting substrate. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2018-021974 A Summary of the Invention [Problem to be solved by the invention]
[0004] In the display device described in Patent Document 1, a polymer network is formed by polymerizing a monomer, and this polymer network and liquid crystal molecules are mixed in the liquid crystal layer.
[0005] The behavior of liquid crystal molecules near the alignment film may differ from that of liquid crystal molecules in the center of the liquid crystal layer. Specifically, the initial alignment of the liquid crystal molecules in the center of the liquid crystal layer varies, so that when a voltage is applied to the pixel electrode, the liquid crystal molecules may be driven in random directions. This may cause the scattering characteristics of the liquid crystal molecules in response to the applied voltage to differ for each pixel. If the scattering characteristics of the liquid crystal molecules in response to the applied voltage differ for each pixel, this may cause unintended degradation of display quality.
[0006] An object of the present disclosure is to provide a manufacturing method for a display device that improves display quality. [Means for solving the problem]
[0007] A method for manufacturing a display device according to one embodiment of the present disclosure includes the steps of: preparing an array substrate having a plurality of first electrodes formed on a first light-transmissive substrate; preparing an opposing substrate having a second electrode formed on a second light-transmissive substrate opposed to the first light-transmissive substrate; forming a seal portion on either the array substrate or the opposing substrate; dripping polymer dispersed liquid crystal containing a photo-crosslinkable monomer inside the seal portion and liquid crystal molecules in gaps between the monomers; bonding the array substrate and the opposing substrate to form a liquid crystal layer in which the polymer dispersed liquid crystal has been dropped; and irradiating the liquid crystal layer with ultraviolet light while applying a voltage to the first electrode and the second electrode so that a potential difference is generated between the first electrode and the second electrode to harden the polymer dispersed liquid crystal layer. In the step of preparing the opposing substrate, a protrusion of the second electrode protruding from the second electrode toward the first electrode is formed.
[0008] A method for manufacturing a display device according to another aspect of the present disclosure includes the steps of: preparing an array substrate having a plurality of first electrodes formed on a first light-transmissive substrate; preparing an opposing substrate having a second electrode formed on a second light-transmissive substrate opposed to the first light-transmissive substrate; forming a seal portion on either the array substrate or the opposing substrate; dispensing a polymer dispersed liquid crystal containing a photo-crosslinkable monomer inside the seal portion and liquid crystal molecules in gaps between the monomers; bonding the array substrate and the opposing substrate to form a liquid crystal layer into which the polymer dispersed liquid crystal has been dispensed; and irradiating the liquid crystal layer with ultraviolet light while applying a voltage to the first electrode and the second electrode such that a potential difference is generated between the first electrode and the second electrode to harden the polymer dispersed liquid crystal layer. In the step of preparing the opposing substrate, a plurality of slits are formed in the second electrode for each pixel at predetermined intervals in a first direction in a plane parallel to a surface of the second light-transmissive substrate, toward a second direction intersecting the first direction. [Brief description of the drawings]
[0009] [Figure 1] FIG. 1 is a perspective view illustrating an example of a display device according to the present embodiment. [Diagram 2] FIG. 2 is a block diagram showing the display device of the first embodiment. [Diagram 3] FIG. 3 is a timing chart for explaining the timing at which the light source emits light in the field sequential method of the first embodiment. [Figure 4] FIG. 4 is an explanatory diagram showing the relationship between the voltage applied to the pixel electrode and the scattering state of the pixel. [Diagram 5] FIG. 5 is a cross-sectional view showing an example of a cross section of the display device of FIG. [Figure 6] FIG. 6 is a plan view showing the plane of the display device of FIG. [Figure 7] FIG. 7 is a plan view showing scanning lines, signal lines, and switching elements in a pixel. [Figure 8] FIG. 8 is a plan view showing a storage capacitor layer in a pixel. [Figure 9] FIG. 9 is a plan view showing an auxiliary metal layer and an opening region in a pixel. [Figure 10] FIG. 10 is a plan view illustrating a common electrode in a pixel. [Figure 11] FIG. 11 is a plan view for explaining a pixel electrode in a pixel. [Figure 12] FIG. 12 is a cross-sectional view taken along line XII-XII' in FIGS. [Figure 13] FIG. 13 is a cross-sectional view for explaining a scattering state in the liquid crystal layer. [Figure 14] FIG. 14 is a flowchart showing an example of a method for manufacturing the display device according to the first embodiment. [Figure 15] FIG. 15 is a cross-sectional view showing a state before the monomer is polymerized in the liquid crystal layer. [Figure 16] FIG. 16 is a cross-sectional view showing a state in which a liquid crystal layer is irradiated with ultraviolet light while a voltage is being applied thereto. [Figure 17]FIG. 17 is a layout diagram showing a display panel arranged on a motherboard according to the first embodiment. [Figure 18] FIG. 18 is a cross-sectional view for explaining a scattering state in a liquid crystal layer according to a comparative example. [Figure 19] FIG. 19 is a cross-sectional view showing a state in which the liquid crystal layer according to the second embodiment is irradiated with ultraviolet light while a voltage is being applied thereto. [Figure 20] FIG. 20 is a cross-sectional view showing a state in which the liquid crystal layer according to the second embodiment has been cured. [Figure 21] FIG. 21 is a plan view illustrating a common electrode according to the third embodiment. [Figure 22] FIG. 22 is a cross-sectional view taken along line XXII-XXII' of FIG. [Diagram 23] FIG. 23 is a cross-sectional view showing a state in which the liquid crystal layer according to the third embodiment has been cured. [Figure 24] FIG. 24 is a cross-sectional view showing a state in which the liquid crystal layer according to the fourth embodiment is irradiated with ultraviolet light while a voltage is being applied thereto. [Diagram 25] FIG. 25 is a cross-sectional view showing a state in which the liquid crystal layer according to the fourth embodiment has been cured. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] The form (embodiment) for carrying out the present disclosure will be described in detail with reference to the drawings. The present disclosure is not limited by the contents described in the following embodiments. The components described below include those that a person skilled in the art can easily imagine and those that are substantially the same. Furthermore, the components described below can be appropriately combined. Note that the disclosure is merely an example, and those that a person skilled in the art can easily imagine appropriate modifications while maintaining the gist of the disclosure are naturally included in the scope of the present disclosure. In addition, in order to make the explanation clearer, the drawings may be schematic in terms of the width, thickness, shape, etc. of each part compared to the actual embodiment, but they are merely examples and do not limit the interpretation of the present disclosure. In addition, in this specification and each figure, elements similar to those described above with respect to the previously mentioned figures may be given the same reference numerals, and detailed explanations may be omitted as appropriate.
[0011] (Display device 1) Fig. 1 is a perspective view showing an example of a display device according to the present embodiment. Fig. 2 is a block diagram showing the display device of Fig. 1. Fig. 3 is a timing chart explaining the timing at which a light source emits light in a field sequential system.
[0012] 1, the display device 1 includes a display panel 2, a light source 3, and a drive circuit 4. Here, one direction in the plane of the display panel 2 is a first direction PX, a direction perpendicular to the first direction PX is a second direction PY, and a direction perpendicular to the PX-PY plane is a third direction PZ.
[0013] The display panel 2 includes an array substrate 10, a counter substrate 20, and a liquid crystal layer 50 (see FIG. 5). The counter substrate 20 faces the array substrate 10 in a direction perpendicular to the surface of the array substrate 10 (the PZ direction shown in FIG. 1). In the liquid crystal layer 50, polymer-dispersed liquid crystal LC is sealed between the array substrate 10, the counter substrate 20, and a seal portion 18.
[0014] As shown in FIG. 1, the display panel 2 has a display area AA capable of displaying an image, and a peripheral area FR outside the display area AA. In the display area AA, a plurality of pixels Pix are arranged in a matrix. In this disclosure, a row refers to a pixel row having m pixels Pix arranged in one direction. Also, a column refers to a pixel column having n pixels Pix arranged in a direction perpendicular to the direction in which the rows are arranged. The values of m and n are determined according to the display resolution in the vertical direction and the display resolution in the horizontal direction. Also, a plurality of scanning lines GL are wired for each row, and a plurality of signal lines SL are wired for each column.
[0015] The light source 3 includes a plurality of light-emitting units 31. As shown in Fig. 2, the light source control unit 32 is included in the drive circuit 4. The light source control unit 32 may be a circuit separate from the drive circuit 4. The light-emitting units 31 and the light source control unit 32 are electrically connected by wiring in the array substrate 10.
[0016] 1, the driving circuit 4 is fixed to the surface of the array substrate 10. As shown in Fig. 2, the driving circuit 4 includes a signal processing circuit 41, a pixel control circuit 42, a gate driving circuit 43, a source driving circuit 44, and a common potential driving circuit 45. The array substrate 10 has a larger area in the XY plane than the counter substrate 20, and the driving circuit 4 is provided on the protruding portion of the array substrate 10 exposed from the counter substrate 20.
[0017] An input signal (such as an RGB signal) VS is input to the signal processing circuit 41 from an image output unit 91 of an external upper level control unit 9 via a flexible substrate 92.
[0018] The signal processing circuit 41 includes an input signal analysis unit 411, a storage unit 412, and a signal adjustment unit 413. The input signal analysis unit 411 generates a second input signal VCS based on a first input signal VS input from the outside.
[0019] The second input signal VCS is a signal that determines, based on the first input signal VS, what gradation value is to be given to each pixel Pix of the display panel 2. In other words, the second input signal VCS is a signal that includes gradation information related to the gradation value of each pixel Pix.
[0020] The signal adjustment unit 413 generates a third input signal VCSA from the second input signal VCS. The signal adjustment unit 413 sends the third input signal VCSA to the pixel control circuit 42, and sends a light source control signal LCSA to the light source control unit 32. The light source control signal LCSA is, for example, a signal including information on the amount of light of the light-emitting unit 31 that is set according to the input gradation value to the pixel Pix. For example, when a dark image is displayed, the amount of light of the light-emitting unit 31 is set to be small. When a bright image is displayed, the amount of light of the light-emitting unit 31 is set to be large.
[0021] The pixel control circuit 42 generates a horizontal drive signal HDS and a vertical drive signal VDS based on the third input signal VCSA. In this embodiment, since the pixel is driven by the field sequential method, the horizontal drive signal HDS and the vertical drive signal VDS are generated for each color that the light emitting unit 31 can emit.
[0022] The gate drive circuit 43 sequentially selects the scanning lines GL of the display panel 2 within one vertical scanning period based on the horizontal drive signal HDS. The order in which the scanning lines GL are selected is arbitrary.
[0023] The source drive circuit 44 supplies a gray scale signal corresponding to the output gray scale value of each pixel Pix to each signal line SL of the display panel 2 within one horizontal scanning period based on the vertical drive signal VDS.
[0024] In this embodiment, the display panel 2 is an active matrix panel, which has signal (source) lines SL extending in the second direction PY and scanning (gate) lines GL extending in the first direction PX in a plan view, and has switching elements Tr at the intersections of the signal lines SL and the scanning lines GL.
[0025] A thin film transistor is used as the switching element Tr. A bottom gate type transistor or a top gate type transistor may be used as an example of the thin film transistor. Although a single gate thin film transistor is illustrated as the switching element Tr, a double gate transistor may be used. One of the source electrode and the drain electrode of the switching element Tr is connected to the signal line SL, the gate electrode is connected to the scanning line GL, and the other of the source electrode and the drain electrode is connected to one end of the capacitance of the polymer dispersion type liquid crystal LC. One end of the capacitance of the polymer dispersion type liquid crystal LC is connected to the switching element Tr via the pixel electrode PE, and the other end is connected to the common potential wiring COML via the common electrode CE. In addition, a storage capacitance HC is generated between the pixel electrode PE and the storage capacitance electrode IO electrically connected to the common potential wiring COML. The pixel electrode PE is a first electrode, and the common electrode CE is a second electrode. The common potential wiring COML is supplied from a common potential driving circuit 45.
[0026] The light-emitting unit 31 includes a first color (e.g., red) light-emitting body 33R, a second color (e.g., green) light-emitting body 33G, and a third color (e.g., blue) light-emitting body 33B. The light source control unit 32 controls the first color light-emitting body 33R, the second color light-emitting body 33G, and the third color light-emitting body 33B to emit light in a time-division manner based on a light source control signal LCSA. In this manner, the first color light-emitting body 33R, the second color light-emitting body 33G, and the third color light-emitting body 33B are driven by a field sequential method.
[0027] 3, in the first subframe (first predetermined time) RF, the first color light emitter 33R emits light in the first color light emission period RON, and the pixels Pix selected in one vertical scanning period GateScan scatter the light to display. In the entire display panel 2, if the gradation signals corresponding to the output gradation values of the pixels Pix are supplied to the signal lines SL described above to the pixels Pix selected in one vertical scanning period GateScan, only the first color is lit in the first color light emission period RON.
[0028] Next, in a second subframe (second predetermined time) GF, the second color light emitter 33G emits light in a second color light emission period GON, and the pixels Pix selected within one vertical scanning period GateScan scatter the light to display. In the entire display panel 2, if the pixels Pix selected within one vertical scanning period GateScan are supplied with grayscale signals corresponding to the output grayscale values of the pixels Pix to the above-mentioned signal lines SL, only the second color is lit during the second color light emission period GON.
[0029] Furthermore, in a third subframe (third predetermined time) BF, the third color light emitter 33B emits light in the third color light emission period BON, and the pixels Pix selected within one vertical scanning period GateScan scatter the light to display. In the entire display panel 2, if the pixels Pix selected within one vertical scanning period GateScan are supplied with gradation signals corresponding to the output gradation values of the pixels Pix to the above-mentioned signal lines SL, then only the third color is lit during the third color light emission period BON.
[0030] The human eye has a limited temporal resolution and an afterimage occurs, so that a composite image of three colors is recognized during one frame (1F). The field sequential method does not require a color filter and reduces absorption loss in the color filter, so that a high transmittance can be achieved. In the color filter method, one pixel is created by dividing the pixel Pix into sub-pixels for the first, second, and third colors, whereas the field sequential method does not require such sub-pixel division. It is also possible to further include a fourth sub-frame and emit a fourth color different from the first, second, and third colors.
[0031] Fig. 4 is an explanatory diagram showing the relationship between a voltage applied to a pixel electrode and the scattering state of a pixel. Fig. 5 is a cross-sectional view showing an example of a cross section of the display device of Fig. 1. Fig. 6 is a plan view showing the plane of the display device of Fig. 1. Fig. 5 is a V-V' cross section of Fig. 6.
[0032] If a grayscale signal corresponding to the output grayscale value of each pixel Pix selected within one vertical scanning period GateScan is supplied to each of the signal lines SL described above, the voltage applied to the pixel electrode PE changes according to the grayscale signal. When the voltage applied to the pixel electrode PE changes, the voltage between the pixel electrode PE and the common electrode CE changes. Then, as shown in FIG. 4, the scattering state of the liquid crystal layer 50 for each pixel Pix is controlled according to the voltage applied to the pixel electrode PE, and the scattering ratio within the pixel Pix changes.
[0033] 4, when the voltage applied to the pixel electrode PE becomes equal to or higher than the saturation voltage Vsat, the change in the scattering ratio in the pixel Pix becomes small. Therefore, the drive circuit 4 changes the voltage applied to the pixel electrode PE in accordance with the vertical drive signal VDS in a voltage range Vdr lower than the saturation voltage Vsat.
[0034] 5, the display device 1 includes a light-transmitting first base material 25, a display panel 2, and a light-transmitting second base material 27. A protective layer 75 is provided on one surface of the light-transmitting first base material 25. A protective layer 76 is provided on one surface of the light-transmitting second base material 27.
[0035] The display panel 2 includes an array substrate 10, a counter substrate 20, and a liquid crystal layer 50. The counter substrate 20 faces the array substrate 10 in a direction perpendicular to the surface of the array substrate 10 (the PZ direction shown in FIG. 1). The liquid crystal layer 50 is made by sealing a polymer-dispersed liquid crystal, which will be described later, between the array substrate 10, the counter substrate 20, and a seal portion 18.
[0036] 5 and 6, the array substrate 10 has a first main surface 10A, a second main surface 10B, a first side surface 10C, a second side surface 10D, a third side surface 10E, and a fourth side surface 10F. The first main surface 10A and the second main surface 10B are parallel planes. The first side surface 10C and the second side surface 10D are parallel planes. The third side surface 10E and the fourth side surface 10F are parallel planes.
[0037] 5 and 6, the counter substrate 20 has a first main surface 20A, a second main surface 20B, a first side surface 20C, a second side surface 20D, a third side surface 20E, and a fourth side surface 20F. The first main surface 20A and the second main surface 20B are parallel planes. The first side surface 20C and the second side surface 20D are parallel planes. The third side surface 20E and the fourth side surface 20F are parallel planes.
[0038] 5 and 6, the first base material 25 has a first main surface 25A, a second main surface 25B, a first side surface 25C, a second side surface 25D, a third side surface 25E, and a fourth side surface 25F. The first main surface 25A and the second main surface 25B are parallel planes. The first side surface 25C and the second side surface 25D are parallel planes. The third side surface 25E and the fourth side surface 25F are parallel planes.
[0039] The first base material 25 is bonded to the first main surface 20A of the counter substrate 20 via an optical resin 23. The first base material 25 is a protective substrate for the counter substrate 20, and is formed, for example, from glass or a light-transmitting resin. When the first base material 25 is formed from a glass base material, it is also called a cover glass. When the first base material 25 is formed from a light-transmitting resin, it may be flexible. Note that the same base material as the first base material 25 may be bonded to the first main surface 10A of the array substrate 10 via an optical resin.
[0040] 5 and 6, the second base material 27 has a first main surface 27A, a second main surface 27B, a first side surface 27C, a second side surface 27D, a third side surface 27E, and a fourth side surface 27F. The first main surface 27A and the second main surface 27B are parallel planes. The first side surface 27C and the second side surface 27D are parallel planes. The third side surface 27E and the fourth side surface 27F are parallel planes.
[0041] The second base material 27 is attached to the first main surface 10A of the array substrate 10 via an optical resin 26. The second base material 27 is a protective substrate for the array substrate 10, and is made of, for example, glass or a light-transmitting resin. When the second base material 27 is made of a glass base material, it is also called a cover glass. When the second base material 27 is made of a light-transmitting resin, it may be flexible.
[0042] As shown in Fig. 5 and Fig. 6, the light source 3 faces the second side surface 25D of the first base material 25. The light source 3 is sometimes called a side light source. As shown in Fig. 5, the light source 3 irradiates the second side surface 25D of the first base material 25 with light from the light source. The second side surface 25D of the first base material 25 facing the light source 3 serves as a light incident surface. The light incident surface facing the light source 3 may be the second side surface 20D of the counter substrate 20 or the second side surface 27D of the second base material 27.
[0043] The light source 3 includes a light emitting section 31 and a light guide 33L. The light emitting section 31 includes a first color (e.g., red) light emitting body 33R, a second color (e.g., green) light emitting body 33G, and a third color (e.g., blue) light emitting body 33B. The light guide 33L irradiates the light emitted by the first color light emitting body 33R, the second color light emitting body 33G, and the third color light emitting body 33B to the second side surface 25D of the first base material 25. The light guide 33L simultaneously receives the light of the multiple light emitting sections 31, diffuses it internally, and releases it to the display panel 2. As a result, the distribution of light per unit area irradiated to the second side surface 25D of the first base material 25 is uniformed.
[0044] Furthermore, the light guide 33L is a single light guide 33L integrally formed from the third side surface 25E to the fourth side surface 25F. The light guide 33L may be configured by arranging a plurality of divided light guides from the third side surface 25E to the fourth side surface 25F. The light guide 33L may be configured by arranging a plurality of divided light guides from the third side surface 25E to the fourth side surface 25F and connecting adjacent light guides to each other.
[0045] The light emitting unit 31 and the light guide 33L are fixed with an adhesive or the like, and assembled to the support 33M to form a light source module. The support 33M is mounted so as to overlap the first main surface 25A of the first base material 25, and is fixed to the first base material 25 with an adhesive or the like.
[0046] The wiring board 93 (flexible printed circuit board or PCB board) has an integrated circuit of the light source control unit 32 mounted thereon, and the light source control unit 32 is connected to the light source 3 via the wiring board 93 (flexible printed circuit board or PCB board). The wiring board 93 is fixed to the support body 33M with an adhesive or the like.
[0047] As shown in Figure 5, the light source light L emitted from the light source 3 propagates in a direction away from the second side surface 20D (second direction PY) while being reflected by either the first substrate 25, the array substrate 10, the counter substrate 20 or the second substrate 27.
[0048] 5, the light source light L propagated inside any of the first base material 25, the array substrate 10, the counter substrate 20, or the second base material 27 is scattered by the pixel Pix having the liquid crystal in a scattering state, and the incident angle of the scattered light becomes smaller than the critical angle, so that the emitted light 68, 68A is radiated to the outside from the first main surface 20A of the counter substrate 20 (the first main surface 25A of the first base material 25) and the first main surface 10A of the array substrate 10, respectively. The emitted light 68, 68A radiated to the outside from the first main surface 20A of the counter substrate 20 and the first main surface 10A of the array substrate 10, respectively, is observed by an observer.
[0049] For this reason, as shown in FIG. 6, a plurality of light emitting sections 31 are arranged at a predetermined pitch in an area of the display area AA corresponding to the second direction PY.
[0050] As shown in FIG. 6, the drive circuit 4 includes a plurality of integrated circuits for the gate drive circuit 43 and a plurality of integrated circuits for the source drive circuit 44.
[0051] FIG. 7 is a plan view showing a scanning line, a signal line, and a switching element in a pixel. FIG. 8 is a plan view showing a storage capacitance layer in a pixel. FIG. 9 is a plan view showing an auxiliary metal layer and an opening region in a pixel. FIG. 10 is a plan view for explaining a common electrode in a pixel. FIG. 11 is a plan view for explaining a pixel electrode overlapping the common electrode shown in FIG. 10. As shown in FIGS. 1, 2, 10, and 11, a plurality of signal lines SL and a plurality of scanning lines GL are provided in a lattice shape in a plan view on the array substrate 10. In other words, one surface of the array substrate 10 includes a plurality of signal lines arranged at intervals in the first direction PX and a plurality of scanning lines arranged at intervals in the second direction PY.
[0052] As shown in Fig. 7, a region surrounded by adjacent scanning lines GL and adjacent signal lines SL is a pixel Pix. The pixel Pix is provided with a pixel electrode PE and a switching element Tr. In this embodiment, the switching element Tr is a bottom-gate type thin film transistor. The switching element Tr has a semiconductor layer SC that overlaps, in a plan view, with a gate electrode GE that is electrically connected to the scanning line GL.
[0053] 7, the scanning lines GL are wirings made of a metal such as molybdenum (Mo) or aluminum (Al), a laminate of these, or an alloy of these, while the signal lines SL are wirings made of a metal such as aluminum or an alloy.
[0054] 7, the semiconductor layer SC is provided so as not to protrude from the gate electrode GE in a plan view, whereby the light source light L directed from the gate electrode GE side toward the semiconductor layer SC is reflected, making it difficult for light leakage to occur in the semiconductor layer SC.
[0055] As shown in Fig. 5, the light source light L emitted from the light source 3 is incident in the second direction PY. The incident direction is the direction from the second side surface 20D closest to the light source 3 to the first side surface 20C which is the opposing surface of the second side surface 20D. When the incident direction of the light source light L is the second direction PY, the length of the semiconductor layer SC in the first direction PX is smaller than the length of the semiconductor layer SC in the second direction PY. This reduces the length of the light source light L in the direction intersecting the incident direction, thereby reducing the effect of light leakage.
[0056] 7, the source electrode SE has two conductors, the same as those of the signal line SL, which are in the same layer as the signal line SL and extend from the signal line SL in a direction intersecting the signal line SL. As a result, the source electrode SE electrically connected to the signal line SL overlaps one end of the semiconductor layer SC in a plan view.
[0057] 7, the drain electrode DE is provided between the conductors of the adjacent source electrodes SE in a plan view. The drain electrode DE overlaps with the semiconductor layer SC in a plan view. The portion that does not overlap with the source electrode SE and the drain electrode DE functions as a channel of the switching element Tr.
[0058] As shown in FIG. 8, the storage capacitance electrode IO has an area IOX that is free of translucent conductive material in an area surrounded by the scanning line GL and the signal line SL. The storage capacitance electrode IO is formed of a translucent conductive material such as ITO (Indium Tin Oxide). The storage capacitance electrode IO is also called a third translucent electrode. The storage capacitance electrode IO is provided across a plurality of pixels Pix, straddling adjacent pixels Pix. The storage capacitance electrode IO has an area with translucent conductive material that overlaps the scanning line GL or the signal line SL and extends to the adjacent pixel Pix.
[0059] The storage capacitance electrode IO is in a lattice shape that covers the scanning lines GL and the signal lines SL along the scanning lines GL and the signal lines SL. This reduces the storage capacitance HC between the region IOX without the translucent conductive material and the pixel electrode PE, so that the storage capacitance HC is adjusted by the size of the region IOX without the translucent conductive material.
[0060] 9, a switching element Tr is provided that is connected to a scanning line GL and a signal line SL, and at least the switching element Tr is covered with a third insulating layer 13 that is an organic insulating layer, and a metal layer TM having an area larger than that of the switching element Tr is provided above the third insulating layer 13. This makes it possible to suppress light leakage from the switching element Tr.
[0061] More specifically, the array substrate 10 includes a third insulating layer 13, which is an organic insulating layer that covers at least the switching element Tr, and a metal layer TM that is provided above the third insulating layer 13 and has an area larger than that of the switching element Tr. In the region surrounded by the scanning line GL and the signal line SL, there is a region that is thinner than the third insulating layer 13 that overlaps the scanning line GL and the signal line SL in a plan view. Therefore, a slope is formed in which the thickness of the third insulating layer 13 changes on the side closer to the light source 3 than the switching element Tr in a plan view. As shown in FIG. 5, the light source light L irradiated from the light source 3 is incident in the second direction PY.
[0062] As shown in FIG. 9, in a plan view, the width of the metal layer TM overlapping the signal line SL is greater than the width of the signal line SL. This prevents light reflected at the edge of the signal line SL from being emitted from the display panel 2. Here, the width of the metal layer TM and the width of the signal line SL are lengths in a direction intersecting the direction in which the signal line SL extends. In addition, the width of the metal layer TM overlapping the scanning line GL is greater than the width of the scanning line GL. Here, the width of the metal layer TM and the width of the scanning line GL are lengths in a direction intersecting the direction in which the scanning line GL extends.
[0063] As shown in FIG. 10, a plurality of protrusions 61 are arranged on the common electrode CE at predetermined intervals in the first direction PX, straddling the pixels Pix, and the protrusions 61 extend in a second direction PY that intersects with the first direction PX.
[0064] 11, the pixel electrode PE is partitioned for each pixel Pix. The contact electrode DEA electrically connected to the drain electrode DE is electrically connected to the pixel electrode PE through a contact hole CH.
[0065] Next, the array substrate 10, the counter substrate 20, and the liquid crystal layer 50 that constitute the display panel 2 will be described. Fig. 12 is a cross-sectional view taken along line XII-XII' in Figs. 10 and 11. Fig. 12 shows the liquid crystal layer in a state after the monomer has been polymerized. Fig. 12 also shows the liquid crystal layer in a non-scattering state. Fig. 13 is a cross-sectional view for explaining the scattering state in the liquid crystal layer.
[0066] As shown in FIG. 12, the array substrate 10 has a first light-transmitting base material 19, a pixel electrode PE, and a first alignment film (alignment film) AL1. The first alignment film AL1 is provided on the pixel electrode PE. The counter substrate 20 has a second light-transmitting base material 29, a common electrode CE, and a second alignment film (alignment film) AL2. A plurality of protrusions 61 protruding from the counter substrate 20 side toward the array substrate 10 side are provided on the surface of the common electrode CE, and the second alignment film AL2 is provided so as to cover the entire common electrode CE and the protrusions 61. The liquid crystal layer 50 is sealed between the first alignment film AL1 and the second alignment film AL2. The array substrate 10 may have a protective member (not shown) made of, for example, glass on the surface of the first light-transmitting base material 19 opposite to the surface on which the pixel electrode PE and the first alignment film (alignment film) AL1 are provided. The protective member may be made of resin as long as it has light-transmitting properties. The counter substrate 20 may have a protective member (not shown) made of, for example, glass on the surface of the second light-transmitting base material 29 opposite to the surface on which the common electrode CE and the second alignment film (alignment film) AL2 are provided. The protective member may be made of resin as long as it is light-transmitting.
[0067] The first light-transmitting substrate 19 and the second light-transmitting substrate 29 are made of a light-transmitting material such as glass or polyethylene terephthalate. The pixel electrode PE and the common electrode CE are made of a light-transmitting conductive material such as ITO (Indium Tin Oxide). The first alignment film AL1 and the second alignment film AL2 align the liquid crystal molecules 52 in the liquid crystal layer 50 in a predetermined direction, and are made of a light-transmitting alignment film material such as polyimide.
[0068] 12, a photo-crosslinkable monomer 51A and a plurality of liquid crystal molecules 52 are contained between the first alignment film AL1 and the second alignment film AL2. The monomers 51A undergo a photo-crosslinking (polymerization) reaction when irradiated with ultraviolet light of a predetermined wavelength to form a three-dimensional mesh-like polymer network 51. As a result, a liquid crystal layer 50 is formed having a reverse mode polymer dispersed liquid crystal LC in which the liquid crystal molecules 52 are dispersed in the gaps in the polymer network 51.
[0069] As the monomer 51A, a photo-crosslinkable acrylate-based material shown in formula (1) can be used. The monomer of formula (1) has an acrylate group that functions as a photo-crosslinkable group at each of the left and right ends. Note that the monomer 51A is not limited to the one shown in formula (1), and various materials having photo-crosslinkability such as acrylate groups shown in formulas (2-1) to (2-4) and maleimide groups shown in formulas (2-5) to (2-8) can be used.
[0070] [ka]
[0071] [ka]
[0072] However, when a polymer network is formed by polymerizing a monomer, the polymer network is usually not fixed and floats in the liquid crystal layer. For this reason, for example, due to a point press on the screen of the display panel or a drop impact, the polymer network in the liquid crystal layer may move irreversibly, causing a disturbance in the alignment of the liquid crystal molecules. This causes unevenness and a decrease in contrast in each pixel of the display panel, and there is a demand for improving the impact resistance of display devices (display panels).
[0073] In this embodiment, an end (a part) of the polymer network 51 is connected to the first alignment film AL1 and the second alignment film AL2. Therefore, the polymer network 51 is fixed to the array substrate 10 and the counter substrate 20 via the first alignment film AL1 and the second alignment film AL2. This improves the impact resistance of the display panel 2 including the liquid crystal layer 50, and improves the reliability. Note that an end (a part) of the polymer network 51 may be connected only to the first alignment film AL1.
[0074] Next, the first alignment film AL1 and the second alignment film AL2 will be described. In this embodiment, the first alignment film AL1 and the second alignment film AL2 are preferably alignment films transparent in the visible region and are formed of polyimide. Polyimide can be obtained by heating polyamic acid (including polyamic acid compounds) to imidize it. For this reason, liquid polyamic acid is applied to the surfaces of the pixel electrode PE and the common electrode CE by spin coating or the like, and the liquid is imidized to form the first alignment film AL1 and the second alignment film AL2. Polyamic acid can be synthesized by reacting a tetracarboxylic acid compound (tetracarboxylic dianhydride) with a diamine compound. For this reason, polyimide is formed having a skeleton derived from tetracarboxylic dianhydride and a skeleton derived from a diamine compound, as shown in formula (3).
[0075] [ka]
[0076] In this formula (3), R1 of the skeleton derived from the tetracarboxylic dianhydride can be, for example, a cyclobutane skeleton, an alicyclic skeleton other than a cyclobutane skeleton, or a chain skeleton. R2 of the skeleton derived from the diamine compound can be, for example, an alicyclic skeleton other than a cyclobutane skeleton, or a chain skeleton. Here, examples of the alicyclic skeleton other than a cyclobutane skeleton include a cycloheptane skeleton and a cyclohexane skeleton. On the other hand, an aromatic compound can also be used as the alicyclic skeleton, but it is preferable to use one that causes little coloring of the polyimide.
[0077] In this embodiment, the polyimide, which is the material (alignment film material) of the first alignment film AL1 and the second alignment film AL2, has a photocrosslinking group X in the side chain of the polyimide. Specifically, the photocrosslinking group X is provided via an ether bond to the above-mentioned R2 forming the skeleton derived from the diamine compound. The photocrosslinking group X may be provided via an ester bond instead of an ether bond. That is, the diamine compound constituting the polyimide has the photocrosslinking group X. This photocrosslinking group X reacts with the monomer 51A during the photocrosslinking (polymerization) reaction of the monomer 51A described above, and connects the first alignment film AL1 and the second alignment film AL2 to the polymer network 51 (polymer fiber), respectively. As a result, the first alignment film AL1 and the second alignment film AL2 are firmly connected to the polymer network 51, and thus the impact resistance of the display panel 2 including the liquid crystal layer 50 is improved, and the reliability is improved.
[0078] The photocrosslinking group X can have, for example, an acrylate group as shown in formula (4). In this case, R in formula (4) means a group to which the photocrosslinking group is linked, and includes the above-mentioned ether bond or ester bond.
[0079] [ka]
[0080] In this configuration, by providing a photocrosslinking group X via an ether bond or an ester bond to R2 of the skeleton derived from the diamine compound, it is possible to easily form a first alignment film AL1 and a second alignment film AL2 made of a polyimide containing the photocrosslinking group X, and it is possible to easily link the first alignment film AL1 and the second alignment film AL2 with the polymer network 51. In addition, since the photocrosslinking group X is provided on the side chain of the polyimide, the degree of freedom of orientation is higher than when the photocrosslinking group X is provided on the polymer main chain, and it is possible to increase the efficiency of the photocrosslinking (polymerization) reaction between the photocrosslinking group X and the photocrosslinkable monomer 51A when the polymer network 51 is formed.
[0081] The photocrosslinking group X is not limited to an acrylate group, and may be at least one of a methacrylate group, a cinnamic acid group, a maleimide group, a phenyldiazirine group, and a phenylazide group on the side chain of the polyimide, as shown in formulas (5-1) to (5-5). These photocrosslinking groups X may be provided on the main chain of the polyimide, or on the terminal of the side chain or the main chain.
[0082] [ka]
[0083] Next, polyimides having other structures will be described. Although the structure of the polyimide having a photocrosslinking group X in the side chain has been described above, a structure having a photocrosslinking group in the main chain of the polyimide can also be adopted. Specifically, a polyimide having a diazo group shown in formula (6-1) or a polyimide having a benzophenone group shown in formula (6-2) can be adopted as a photocrosslinking group in R1 of the skeleton derived from tetracarboxylic dianhydride in formula (3). In these formulas (6-1) and (6-2), Et represents an ethyl group. Moreover, the structural formulas shown in formulas (6-1) and (6-2) are merely examples, and other structures may be used as long as the polyimide has a diazo group or a benzophenone group.
[0084] [ka]
[0085] In this configuration, since the polyimide originally has a functional group that functions as a photocrosslinking group, it is possible to easily link the first alignment film AL1 and the second alignment film AL2 to the polymer network 51. In addition, since the photocrosslinking group is provided in the main chain of the polyimide, when the polymer network 51 is linked to the polymer network 51, the polymer network 51 becomes less mobile and can be fixed.
[0086] In the above-mentioned configuration, the polymer network 51 and the liquid crystal molecules 52 each have optical anisotropy. The orientation of the liquid crystal molecules 52 is controlled by the voltage difference between the pixel electrode PE and the common electrode CE. For example, as shown in FIG. 12, when no voltage is applied between the pixel electrode PE and the common electrode CE, the optical axis Ax1 of the polymer network 51 and the optical axis Ax2 of the liquid crystal molecules 52 are generally aligned with each other. The optical axis Ax2 of the liquid crystal molecules 52 is parallel to the PZ direction (FIG. 5) of the liquid crystal layer 50. The optical axis Ax1 of the polymer network 51 is parallel to the PZ direction of the liquid crystal layer 50 regardless of the presence or absence of voltage. The orientation of the liquid crystal molecules 52 changes depending on the voltage applied to the pixel electrode PE. The change in the orientation of the liquid crystal molecules 52 changes the degree of scattering of light passing through the pixel Pix (the region on the pixel electrode PE).
[0087] In this embodiment, it is preferable to use a polyimide represented by formula (7) in consideration that the first alignment film AL1 and the second alignment film AL2 are vertical alignment films. The polyimide of formula (7) has an acrylate group, which is a photo-crosslinking group X, at the end of the side chain, and this acrylate group is connected to an ether group via R3, which is a chain skeleton. This R3 is a long-chain alkyl group ((CH2)n; n=1 to 12), and particularly when n=6 to 12 and the density of the long-chain alkyl group is higher, the pretilt angle of the liquid crystal molecules 52 tends to become larger, which is effective for use as a vertical alignment film.
[0088] [ka]
[0089] When no voltage is applied between the pixel electrode PE and the common electrode CE, the refractive index difference between the polymer network 51 and the liquid crystal molecules 52 is zero in all directions. Therefore, the liquid crystal layer 50 is in a non-scattering state in which it does not scatter the light source light L (FIG. 5). When the liquid crystal layer 50 is in a non-scattering state in which it does not scatter the light source light L, the background on the first main surface 20A side of the counter substrate 20 is visible from the first main surface 10A of the array substrate 10, and the background on the first main surface 10A side of the array substrate 10 is visible from the first main surface 20A of the counter substrate 20.
[0090] 13, between the pixel electrode PE and the common electrode CE to which a voltage is applied, the optical axis Ax2 of the liquid crystal molecules 52 is tilted by the electric field E generated between the pixel electrode PE and the protrusion 61 of the common electrode CE. Since the optical axis Ax1 of the polymer network 51 does not change due to the electric field E, the optical axis Ax1 of the polymer network 51 and the optical axis Ax2 of the liquid crystal molecules 52 are oriented in different directions. In the pixel Pix having the pixel electrode PE to which a voltage is applied, the light source light L is scattered. As described above, a part of the scattered light source light L is emitted to the outside from the first main surface 10A of the array substrate 10 or the first main surface 20A of the counter substrate 20, and the light is observed by the observer.
[0091] In a pixel Pix having a pixel electrode PE to which no voltage is applied, the background on the first main surface 20A side of the counter substrate 20 is visible from the first main surface 10A of the array substrate 10, and the background on the first main surface 10A side of the array substrate 10 is visible from the first main surface 20A of the counter substrate 20. When the display device 1 of this embodiment receives a first input signal VS from the image output unit 91, a voltage is applied to the pixel electrode PE of the pixel Pix where an image is displayed, and an image based on the third input signal VCSA is visible together with the background. In this way, when the polymer dispersed liquid crystal LC is in a scattering state, an image is displayed in the display region.
[0092] An image displayed by light emitted to the outside after scattering the light source light L in a pixel Pix having a pixel electrode PE to which a voltage is applied is superimposed on the background. In other words, the display device 1 of this embodiment can display an image superimposed on the background by combining the emitted light 68 or 68A with the background.
[0093] The electric field E generated between the pixel electrode PE and the common electrode CE is applied in an oblique direction toward the protrusion 61 because the electric potential is higher at the protrusion 61 than at the flat surface of the common electrode CE. This allows the electric field E to control the alignment direction of the liquid crystal molecules 52.
[0094] (Manufacturing method of display device 1) Next, a method for manufacturing the display device 1 will be described. Fig. 14 is a flow chart showing an example of a method for manufacturing the display device in embodiment 1. Fig. 15 is a cross-sectional view showing a state before monomers are polymerized in the liquid crystal layer. Fig. 16 is a cross-sectional view showing a state in which the liquid crystal layer is irradiated with ultraviolet light while a voltage is applied thereto. Fig. 17 is a layout diagram showing a display panel arranged on a mother substrate in embodiment 1.
[0095] 14, first, an array substrate 10 having a plurality of pixel electrodes PE formed on a first light-transmissive base material 19 is fabricated (S1). A first alignment film AL1 is laminated on the entire surface of the pixel electrodes PE. In addition, a counter substrate 20 having a common electrode CE formed thereon is fabricated on a second light-transmissive base material 29 (S2). A second alignment film AL2 is laminated on the entire surface of the common electrode CE.
[0096] In manufacturing process S2, a plurality of protrusions 61 are formed on the common electrode CE at predetermined intervals in the first direction PX, protruding from the common electrode CE to the pixel electrode PE so as to extend in the second direction PY. The protrusions 61 have, for example, a triangular cross-sectional shape. The shape of the protrusions 61 is not particularly limited, and may be a semicircular cross-sectional shape or a trapezoidal cross-sectional shape.
[0097] Next, a method for injecting the solution LC' into the inside of the seal portion 18 in the manufacturing steps S3 to S5 will be described. There are two methods: a vacuum injection method and a drop injection (ODF) method. In the vacuum injection method, an injection port is formed in the seal portion 18, and the solution LC' is injected from the injection port after the seal portion 18 is hardened. In the ODF method, the seal portion 18 is formed on either the array substrate or the counter substrate, and the solution LC' is dripped inside the seal portion 18. In this embodiment, a manufacturing method of the display device 1 using the ODF method will be described.
[0098] After manufacturing steps S1 and S2, an uncured seal portion 18 is formed on either the array substrate 10 or the counter substrate 20 (S3). The seal portion 18 can be formed in a ring shape, for example, using a dispenser. In the ODF method, since no injection port is formed in the seal portion 18, the seal portion 18 is a continuous ring shape without any breaks.
[0099] After the manufacturing process S3, a solution LC' is dropped inside the seal portion 18 (S4). Then, the array substrate 10, the counter substrate 20, and the seal portion 18 are bonded together in a vacuum (S5). As a result, a liquid crystal layer 50 is formed in the space surrounded by the array substrate 10, the counter substrate 20, and the seal portion 18 (see FIG. 5).
[0100] After the manufacturing step S5, the sealed portion 18 is cured (S6). First, heat is applied to the sealed portion 18 at a temperature at which the uncured acrylic resin contained in the sealed portion 18 cures. Radical polymerization proceeds in the acrylic resin due to the action of the thermal radical polymerization initiator contained in the sealed portion 18. Because the reaction rate of radical polymerization is fast, the acrylic resin can be cured in a short time.
[0101] Next, heat is applied to the sealing portion 18 at a temperature at which the uncured epoxy resin contained in the sealing portion 18 cures. Addition polymerization proceeds in the epoxy resin due to the action of the heat curing agent contained in the sealing portion 18. Because the reaction rate of addition polymerization is slower than that of radical polymerization, it is possible to cure the epoxy resin over a longer period of time than in the process of curing the acrylic resin.
[0102] At this time, as shown in FIG. 15, the surfaces of the first alignment film AL1 and the second alignment film AL2 (the surfaces in contact with the liquid crystal layer 50) have not been subjected to an alignment treatment, so that before the monomer 51A is polymerized, the alignment states of the monomer 51A and the liquid crystal molecules 52 are each tilted in random directions.
[0103] As shown in FIG. 15, between the array substrate 10, the counter substrate 20, and the seal portion 18, a solution LC′ containing a plurality of photo-crosslinkable monomers 51A, liquid crystal molecules 52, and a photopolymerization initiator 53 is injected.
[0104] The photopolymerization initiator 53 absorbs light when irradiated with ultraviolet light of a predetermined wavelength, generates radicals, and initiates polymerization of the monomer 51A in the solution LC'. The photopolymerization initiator 53 can be selected from those suitable for the ultraviolet wavelength to be used, and for example, one of the following can be used.
[0105] (±)-Camphorquinone, acetophenone, benzophenone, 4-benzoylbenzoic acid, 2-benzoylbenzoic acid, 2-benzoylbenzoic acid methyl, 4,4´-bis(dimethylamino)benzophenone, 4,4´-bis(diethylamino)benzophenone, 4,4´-dichlorobenzophenone, 1,4-dibenzoylbenzene, benzyl, p-anisyl, 2-benzoyl-2-propanol, 2-hydroxy-4´-(2-hydroxyethoxy)-2-methylpropiophenone, 1-benzylcyclohexanol, benzoin, benzoin methyl ether, benzoin ethyl ether, benzoin isopropyl ether, benzoin butyl ether, o-tosylbenzoin, 2,2-di Ethoxyacetophenone, benzil dimethyl ketal, 2-methyl-4´-(methylthio)-2-morpholinopropiophenone, 2-benzyl-2-(dimethylamino)-4´-monofolinobutyrophenone, 2-isonitrosopropiophenone, 2-chlorothioxanthone, 2-isopropylthioxanthone, 2,4-diethylthioxanthen-9-one, 2,2´-bis(2-chlorophenyl)-4,4,5,5´-tetraphenyl-1,2´-biimidazole, diphenyl(2,4,6-trimethylbenzoyl)phosphine oxide, phenylbis(2,4,6-trimethylbenzoyl)phosphine oxide, lithium phenyl(2,4,6-trimethylbenzoyl)phosphinate.
[0106] After the manufacturing process S6, ultraviolet rays UV are irradiated onto the entire surface of the liquid crystal layer 50 while applying a voltage to the common electrode CE and the pixel electrode PE (S7). First, as shown in Fig. 16, a voltage is applied to the common electrode CE and the pixel electrode PE, and an electric field is applied in an oblique direction from the pixel electrode PE to the multiple protrusions 61 of the common electrode CE. As a result, the inclination of the monomers 51A and the liquid crystal molecules 52 is influenced by the oblique electric field direction and tilts, resulting in a pretilt angle of 85 degrees to 88 degrees with respect to the surface of the counter substrate 20. The magnitude of the voltage is a low voltage at which light begins to scatter within the pixels.
[0107] 16, while a voltage is applied to the common electrode CE and the pixel electrodes PE, the entire surface of the liquid crystal layer 50 is irradiated with ultraviolet light UV. As a result, the monomers 51A undergo a photocrosslinking (polymerization) reaction to form a three-dimensional mesh-like polymer network 51, and the liquid crystal LC is hardened (see FIG. 12).
[0108] Here, in the manufacturing process S7, as shown in FIG. 17, the multiple display panels 2 are arranged in a matrix on a mother glass 1000. The mother glass 1000 includes the multiple display panels 2, a power supply unit 101, and a cutting line 120. The power supply unit 101 includes a pixel potential supply unit 102 and a common potential supply unit 103. The power supply unit 101 is connected to each display panel 2 by wiring drawn from a terminal unit 110 of each display panel 2. By applying a voltage to each display panel 2, a pixel potential is supplied from the pixel potential supply unit 102 to the pixel electrode PE of each display panel 2. In addition, a common potential is supplied from the common potential supply unit 103 to the common electrode CE of each display panel 2.
[0109] After the manufacturing process S7, the display panels 2 are each cut away from the mother glass 1000 along the cutting lines 120 on the mother glass 1000.
[0110] When the solution LC' is injected into the seal portion 18 using the vacuum injection method, the manufacturing process S7 is performed for each display panel 2 after the display panel 2 is separated from the mother glass 1000. Methods for applying a voltage to each display panel 2 include a method of attaching the panel to a test pad or test jig, and a method of connecting the panel to an external power source with lead wires.
[0111] Fig. 18 is a cross-sectional view for explaining a scattering state in a liquid crystal layer according to a comparative example. In a display panel 2A according to the comparative example shown in Fig. 18, unlike the display panel 2 shown in Fig. 14, a protrusion 61 is not formed on the common electrode CE.
[0112] 18, in the display panel 2A according to the comparative example, between the pixel electrode PE and the common electrode CE to which a voltage is applied, the optical axis Ax2 of the liquid crystal molecules 52 is tilted by the electric field generated between the pixel electrode PE and the common electrode CE. Since the optical axis Ax1 of the polymer network 51 does not change due to the electric field, the orientations of the optical axis Ax1 of the polymer network 51 and the optical axis Ax2 of the liquid crystal molecules 52 are different from each other. However, since the initial orientation of the liquid crystal molecules 52 in the central portion of the liquid crystal layer 50 varies, the orientations of the optical axes Ax2 of the liquid crystal molecules 52 may differ from each other. This may cause light to be scattered in the liquid crystal layer 50.
[0113] In contrast, in the display panel 2 according to the first embodiment, during the manufacture of the display panel 2, a plurality of protrusions 61 are formed on the common electrode CE, and while a voltage is applied to the pixel electrodes PE and the common electrode CE, the entire surface of the liquid crystal layer 50 is irradiated with ultraviolet light to harden the liquid crystal layer 50. Therefore, the electric field E generated between the pixel electrodes PE and the common electrode CE is applied in an oblique direction toward the protrusions 61, so that the electric field E can control the orientation of the optical axis Ax2 of the liquid crystal molecules 52 to an intended orientation.
[0114] As a result, the liquid crystal molecules 52 are affected by the electric field E applied obliquely with respect to the third direction PZ, and the orientation of the optical axis Ax2 of the entire liquid crystal molecule 52 rotates due to the electric field E with random behavior suppressed, and a pretilt angle of 85 degrees to 88 degrees is imparted with respect to the surface of the array substrate 10, thereby suppressing variation in the scattering characteristics of the liquid crystal molecules according to the applied voltage.
[0115] (Embodiment 2) Fig. 19 is a cross-sectional view showing a state in which the liquid crystal layer according to embodiment 2 is irradiated with ultraviolet light while a voltage is applied thereto. Fig. 20 is a cross-sectional view showing a state in which the liquid crystal layer according to embodiment 2 is hardened. Note that the same components as those described in embodiment 1 above are denoted by the same reference numerals, and duplicated descriptions will be omitted.
[0116] 19, in the process of producing the counter substrate 20 of the display panel 2B according to the second embodiment, a plurality of resin materials 62, a common electrode CE, and a second alignment film AL2 are laminated in this order on a second light-transmissive substrate 29. A plurality of protrusions 63 are formed on the common electrode CE. The resin materials 62 are formed so as to overlap with the protrusions 63 in the third direction PZ. The resin materials 62 are formed between the second light-transmissive substrate 29 and the protrusions 63 so as to protrude toward the array substrate 10 side beyond the second light-transmissive substrate 29.
[0117] The resin material 62 is made of a flexible resin, such as polyimide. The resin material 62 is provided as a base for the protrusion 63. The resin material 62 has, for example, a semicircular cross-sectional shape. This causes the protrusion 63 of the common electrode CE to curve, making it easier for the electric field E to gather at the protrusion 63. The shape of the resin material 62 is not particularly limited, and may be a triangular cross-sectional shape, a trapezoidal cross-sectional shape, or the like.
[0118] 19, in a process of irradiating the liquid crystal layer 50 with ultraviolet light to harden the liquid crystal layer 50 while applying voltages to the pixel electrode PE and the common electrode CE so as to generate a potential difference between the pixel electrode PE and the common electrode CE, an electric field E is applied obliquely from the pixel electrode PE to the protrusion 63 with respect to the third direction PZ. As a result, as shown in Fig. 20, the liquid crystal molecules 52 are affected by the electric field E applied obliquely with respect to the third direction PZ, and the orientation of the optical axis Ax2 of the entire liquid crystal molecules 52 rotates due to the electric field E with random behavior suppressed, and a pretilt angle of 85 degrees to 88 degrees is given with respect to the surface of the array substrate 10, thereby suppressing variation in the scattering characteristics of the liquid crystal molecules according to the applied voltage.
[0119] (Embodiment 3) Fig. 21 is a plan view for explaining a common electrode according to embodiment 3. Fig. 22 is a cross-sectional view showing a state in which the liquid crystal layer according to embodiment 3 is irradiated with ultraviolet light while a voltage is applied thereto. Fig. 23 is a cross-sectional view showing a state in which the liquid crystal layer according to embodiment 3 is hardened. Note that the same components as those explained in the above-mentioned embodiment 1 are given the same reference numerals and overlapping explanations will be omitted.
[0120] As shown in Fig. 21, a plurality of slits 64 are formed on the common electrode CE according to the third embodiment for each pixel Pix. The slits 64 are arranged at predetermined intervals in the first direction PX, and each slit 64 extends in a second direction PY intersecting the first direction PX. Ends of the slits 64 are connected to the scanning lines GL. The ends of the slits 64 are closed by the translucent conductive material of the common electrode CE at positions overlapping the scanning lines GL. The width of the slits 64 is, for example, 10 µm. The width of the slits 64 is preferably between 3 µm and 20 µm.
[0121] 22, in the process of producing the counter substrate 20 of the display panel 2C according to embodiment 3, a common electrode CE and a second alignment film AL2 are laminated in this order on a second light-transmissive base material 29. A plurality of slits 64 are formed between the common electrodes CE. The second alignment film AL2 is formed to cover the surfaces of the common electrode CE and the slits 64.
[0122] As shown in Figure 22, in the process of irradiating the liquid crystal layer 50 with ultraviolet light to harden the liquid crystal layer 50 while applying voltage to the pixel electrode PE and the common electrode CE so that a potential difference is generated between the pixel electrode PE and the common electrode CE, when an electric field E is generated from the pixel electrode PE to the common electrode CE, the electric field E is not applied to the slit 64 because the common electrode CE is not provided at the slit 64.
[0123] Therefore, the electric field E is applied obliquely from the pixel electrode PE toward the common electrodes CE on both sides of the slit 64. As a result, as shown in Fig. 23, the liquid crystal molecules 52 are affected by the electric field E applied obliquely with respect to the third direction PZ, and the orientation of the optical axis Ax2 of the entire liquid crystal molecules 52 rotates due to the electric field E with random behavior suppressed, and a pretilt angle of 85 degrees to 88 degrees is imparted with respect to the surface of the array substrate 10, thereby suppressing variations in the scattering characteristics of the liquid crystal molecules according to the applied voltage.
[0124] (Embodiment 4) Fig. 24 is a cross-sectional view showing a state in which the liquid crystal layer according to embodiment 4 is irradiated with ultraviolet light while a voltage is applied thereto. Fig. 25 is a cross-sectional view showing a state in which the liquid crystal layer according to embodiment 4 has been cured. Note that the same components as those described in the above-mentioned present embodiment are given the same reference numerals, and duplicated descriptions will be omitted.
[0125] 24, in the process of producing the counter substrate 20 of the display panel 2D according to the fourth embodiment, a third electrode CE1, a light-transmitting insulating film 65, a common electrode CE, and a second alignment film AL2 are laminated in this order on a second light-transmitting base material 29. A plurality of slits 64 are formed between the common electrodes CE. The third electrode CE1 has the same potential as the common electrode CE.
[0126] The insulating film 65 is a light-transmitting organic insulating film made of an organic insulating material.
[0127] As shown in Figure 24, in the process of irradiating ultraviolet light to the liquid crystal layer 50 to harden the liquid crystal layer 50 while applying voltage to the pixel electrode PE and the common electrode CE so that a potential difference is generated between the pixel electrode PE and the common electrode CE, when an electric field E is generated from the pixel electrode PE to the common electrode CE, the electric field E is not easily applied to the slit 64 due to the insulating film 65 covering the third electrode CE1 in the portion overlapping with the slit 64, and therefore a larger electric field is more likely to be applied to the common electrode CE than to the third electrode CE1.
[0128] Therefore, the electric field E is applied obliquely from the pixel electrode PE toward the common electrodes CE on both sides of the slit 64. As a result, as shown in Fig. 25, the liquid crystal molecules 52 are affected by the electric field E applied obliquely with respect to the third direction PZ, and the orientation of the optical axis Ax2 of the entire liquid crystal molecules 52 rotates due to the electric field E while suppressing random behavior, and a pretilt angle of 85 degrees to 88 degrees is given with respect to the surface of the array substrate 10, suppressing variation in the scattering characteristics of the liquid crystal molecules according to the applied voltage. When driving the display device 1, a voltage may also be supplied to the third electrode CE1 to drive it.
[0129] Although the preferred embodiment has been described above, the present disclosure is not limited to such an embodiment. The contents disclosed in the embodiment are merely examples, and various modifications are possible within the scope of the present disclosure. Appropriate modifications made within the scope of the present disclosure also naturally belong to the technical scope of the present disclosure. [Explanation of symbols]
[0130] 1 Display device 2 Display Panel 3 light source 10 Array substrate (first light-transmitting substrate) 18 Seal part 19 First translucent base material 20 Opposite substrate (second transparent substrate) 29 Second translucent base material 50 Liquid crystal layer 51 Polymer Network 51A Monomer 52 Liquid crystal molecules AL1 First alignment layer (alignment layer) AL2 Second alignment layer (alignment layer) CE common electrode (second electrode) CE1 3rd electrode PE Pixel electrode (first electrode) LC Polymer dispersed liquid crystal 61, 63 Protrusion 62 Resin material 64 Slit 65 Insulating Film
Claims
1. A step of producing an array substrate having a plurality of first electrodes formed on a first light-transmitting base material; preparing an opposing substrate having a second electrode formed on a second light-transmissive substrate opposed to the first light-transmissive substrate; forming a seal portion on either the array substrate or the counter substrate; a step of dropping a polymer dispersed liquid crystal containing a monomer having photocrosslinkability inside the sealing portion and liquid crystal molecules in gaps between the monomers; a step of bonding the array substrate and the counter substrate together to form a liquid crystal layer in which the polymer dispersed liquid crystal is dropped; and applying a voltage to the first electrode and the second electrode to generate a potential difference between the first electrode and the second electrode, and curing the liquid crystal layer by irradiating the liquid crystal layer with ultraviolet light, In the step of fabricating the counter substrate, a protrusion of the second electrode is formed, the protrusion protruding from the second electrode toward the first electrode. A method for manufacturing a display device.
2. In the step of fabricating the counter substrate, the plurality of protrusions are arranged at predetermined intervals in a first direction on a plane parallel to a surface of the second light-transmitting base material, and the protrusions are formed to extend in a second direction intersecting the first direction. The method for manufacturing the display device according to claim 1 .
3. In the step of fabricating the counter substrate, a resin material is formed between the protrusion and the second light-transmitting base material, the resin material protruding toward the array substrate side beyond the second light-transmitting base material. The method for manufacturing the display device according to claim 1 or 2.
4. A step of producing an array substrate having a plurality of first electrodes formed on a first light-transmitting base material; preparing an opposing substrate having a second electrode formed on a second light-transmissive substrate opposed to the first light-transmissive substrate; forming a seal portion on either the array substrate or the counter substrate; a step of dropping a polymer dispersed liquid crystal containing a monomer having photocrosslinkability inside the sealing portion and liquid crystal molecules in gaps between the monomers; a step of bonding the array substrate and the counter substrate together to form a liquid crystal layer in which the polymer dispersed liquid crystal is dropped; and applying a voltage to the first electrode and the second electrode to generate a potential difference between the first electrode and the second electrode, and curing the liquid crystal layer by irradiating the liquid crystal layer with ultraviolet light, In the step of fabricating the counter substrate, a plurality of slits are formed in the second electrode for each pixel at predetermined intervals in a first direction in a plane parallel to a surface of the second light-transmitting base material, the slits being oriented in a second direction intersecting the first direction. A method for manufacturing a display device.
5. In the step of fabricating the counter substrate, a third electrode, a light-transmitting insulating film, and the second electrode are laminated in this order on the second light-transmitting base material, the third electrode overlaps the second electrode and the slit and has the same potential as the second electrode; The method for manufacturing the display device according to claim 4 .
6. In the process of fabricating the array substrate and the process of fabricating the counter substrate, an alignment film in contact with the liquid crystal layer is formed on the first electrode and the second electrode; In the step of hardening the liquid crystal layer, the monomer is polymerized to form a polymer network in a mesh-like shape, The alignment film is connected to the polymer network. The method for manufacturing the display device according to claim 1 .
Citation Information
Patent Citations
Liquid crystal display panel and image display applying apparatus
JP2002244137A
Liquid crystal display device
JP2002303869A
Liquid crystal display and its manufacturing method
JP2008122871A
Liquid crystal display
JP2018200453A
Orientation film material and liquid crystal display device
JP2022154781A